Positive electrode active material, lithium ion secondary battery, and method for identifying positive electrode active material
The positive electrode active material, with a uniformly dispersed transition metal element marker, addresses the challenge of identifying and recycling positive electrodes by enabling accurate material recognition, thus facilitating effective battery recycling.
Patent Information
- Application Number
- JP2023056967
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-03-31
- Publication Date
- 2024-10-15
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing technologies face challenges in appropriately determining the recycling of batteries, particularly positive electrodes, due to difficulties in identifying and distinguishing between different types and sources of positive electrode active materials.
A positive electrode active material is developed, comprising a first component as a metal oxide containing a fourth period transition element and a second component as a transition metal element from the fifth or sixth period, uniformly dispersed within the material, which serves as an identification marker, allowing for accurate identification and recycling judgment through a method involving extraction, analysis, and querying manufacturing profile information.
Enables accurate identification of the type and source of positive electrode active materials even after detachment from the battery, facilitating appropriate recycling by ensuring precise determination of the material's origin and composition.
Smart Images

Figure 2024144829000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a positive electrode active material, a lithium ion secondary battery, and a method for identifying the positive electrode active material. [Background technology]
[0002] In recent years, the demand for batteries that use rare metals has been increasing. Because the manufacturing cost of batteries is high, they are generally reused if possible, and those that are difficult to reuse are generally recycled. Because the cost of recycling is high, optimal recycling implementation decisions are required.
[0003] Patent Document 1 discloses a method for identifying the origin, type, etc. of an electrochemical device in which an organic / inorganic composite is introduced onto the surface of an electrode. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Special Publication No. 2009-544139 Summary of the Invention [Problem to be solved by the invention]
[0005] However, with conventional techniques, there are cases where it is not possible to appropriately determine whether or not to recycle a battery, particularly a positive electrode.
[0006] The present invention has been made in consideration of the above circumstances, and an object of the present invention is to provide a positive electrode active material, a lithium ion secondary battery, and a method for identifying a positive electrode active material that can more appropriately determine and identify the recycling of positive electrodes. [Means for solving the problem]
[0007] The gist of each aspect of the positive electrode active material, the lithium ion secondary battery, and the method for identifying a positive electrode active material according to the present invention is as follows.
[0008] [1] A positive electrode active material according to one embodiment of the present invention is an active material for a positive electrode of a storage battery, a first component which is a metal oxide containing a transition element of the fourth period; A second component including at least one transition metal element belonging to the fifth or sixth period; having The first and second components are mixed. [2] In the positive electrode active material described in the above [1], the content of the second component may be 0.1 to 1000 ppm relative to the content of the first component. [3] In the positive electrode active material according to the above [1] or [2], the second component may contain two or more kinds of transition metal elements belonging to the fifth or sixth period. [4] In the positive electrode active material according to any one of the above [1] to [3], the second component may be uniformly dispersed. [5] A method for identifying a positive electrode active material according to one aspect of the present invention includes a first removal step of removing a positive electrode from a storage battery including the positive electrode active material according to any one of the above items [1] to [4]; a second removal step of removing at least a portion of the positive electrode active material from the positive electrode; an analysis step of identifying information including at least one of the type and content of the constituent elements of the positive electrode active material extracted in the second extraction step; an identification step of comparing manufacturing profile information that records the manufacturing conditions of the storage battery or the positive electrode with the information acquired in the analysis step, and identifying information related to the manufacturing of the positive electrode active material; Includes. [6] A lithium-ion secondary battery according to one embodiment of the present invention comprises: a positive electrode including a positive electrode active material having a lithium transition metal composite oxide, a first component which is a metal oxide containing a transition metal element of the fourth period, and a second component which contains at least one transition metal element belonging to the fifth period or the sixth period, the first component and the second component being mixed together; A negative electrode including non-graphitizable carbon and graphite as a negative electrode active material that absorbs and releases lithium; an electrolyte interposed between the positive electrode and the negative electrode and containing at least a lithium salt; Equipped with. [7] In the lithium ion secondary battery described in [6] above, the second component may be uniformly dispersed in the positive electrode. Effect of the Invention
[0009] According to each aspect of the present invention, even if the positive electrode active material is peeled off from the battery or the positive electrode, it is possible to know the type and source of the material used as the positive electrode active material. In addition, since it is possible to know the type and source of the material used as the positive electrode active material, it is possible to appropriately recycle the battery. [Brief description of the drawings]
[0010] [Figure 1] 1A to 1C are schematic diagrams illustrating an example of a method for producing a positive electrode active material according to an embodiment. [Diagram 2] 5A to 5C are schematic diagrams illustrating another example of the method for producing a positive electrode active material according to the embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Hereinafter, with reference to the drawings as needed, embodiments of the positive electrode active material, the lithium ion secondary battery, and the method for identifying the positive electrode active material of the present invention will be described.
[0012] <Cathode active material> The positive electrode active material according to this embodiment is an active material for a positive electrode of a storage battery, and has a first component which is a metal oxide containing a transition element of the fourth period, and a second component which contains at least one transition metal element belonging to the fifth or sixth period.
[0013] (1st component) The first component of the positive electrode active material is a metal oxide containing a transition element of the fourth period, for example, an oxide containing at least one of nickel, cobalt, and manganese. Specifically, the first component is preferably a lithium transition metal composite oxide. As the positive electrode active material, for example, lithium manganese composite oxide (Lix Mn2O4 or Li x MnO2), lithium nickel composite oxide (Li x NiO2), lithium cobalt complex oxide (Li x CoO2), lithium nickel cobalt composite oxide (LiNi 1-y Co y O2), lithium manganese cobalt oxide (LiMn y Co 1-y O2), spinel-structure lithium manganese nickel composite oxide (Li x Mn 2-y Ni y O4), olivine-structured lithium phosphate (Li x FePO4, Li x Fe 1-y Mn y PO4, Li x CoPO4), LiNiCoAlO2, Li2MnO3, Li 2-x-y Fe x Mn y O2, Li2Fe 1-x Mn x SiO4, LiNi 1 / 3 Mn 1 / 3 Co 1 / 3 O2 and the like can be used alone or in combination (however, in the above-mentioned compounds, x and y are preferably in the range of more than 0 and 1 or less).
[0014] (2nd component) The second component of the positive electrode active material contains at least one transition metal element belonging to the fifth or sixth period. Specifically, the second component may be, for example, zirconium, niobium, molybdenum, or REM (rare earth element). REM (rare earth element) is a general term for two elements, scandium (Sc) and yttrium (Y), and 15 elements (lanthanoids) from lanthanum (La) to lutetium (Lu).
[0015] The second component may be composed of the above metal element alone or two or more kinds of the above metal element. The second component may also exist as a compound containing the above metal element, for example, as an oxide containing the above metal element.
[0016] In the positive electrode active material of this embodiment, the first component and the second component are mixed. That is, the second component is dispersed throughout the positive electrode active material, and is not present in a layered or film form, for example. In this way, the second component, which is composed of a component completely different from the first component, is mixed with the first component and dispersed throughout the positive electrode active material, so that even if the positive electrode is separated from the battery or the battery is disassembled, the second component can be easily and accurately detected. As a result, the positive electrode active material can be appropriately identified.
[0017] The content of the second component is preferably 0.1 to 1000 ppm relative to the content of the first component. The second component functions as an identification material. In order to stably exert the identification ability, it is preferable to contain a certain amount or more. Specifically, the content of the second component is preferably 0.1 ppm or more relative to the content of the first component. More preferably, it is 10 ppm or more. On the other hand, if the ratio of the second component in the entire positive electrode active material increases excessively, there is a risk that the function as an electrode will be deteriorated, such as a decrease in capacity, an increase in resistance, and a decrease in durability. Therefore, the content of the second component is preferably 1000 ppm or less relative to the content of the first component. More preferably, it is 100 ppm or less.
[0018] In addition, the second component preferably contains two or more of the transition metal elements belonging to the fifth or sixth period. Conventionally, metal oxides containing transition elements of the fourth period have often been used as the main component of the positive electrode active material. Therefore, if one of the transition metal elements belonging to the fifth or sixth period, which does not significantly affect the electrode performance, is used as the second component as the identification material, the identification effect can be obtained. On the other hand, in order to further improve the identification ability, the second component preferably contains two or more of the transition metal elements belonging to the fifth or sixth period. For example, the second component may contain zirconium oxide, niobium oxide, and molybdenum oxide.
[0019] In addition, the second component is preferably uniformly dispersed throughout the positive electrode active material. In other words, the second component is preferably mixed with the first component throughout the positive electrode active material without uneven distribution. As described above, the second component has a function as an identification material. Therefore, the second component is preferably not in a layered or film form, and is preferably dispersed throughout the positive electrode active material without uneven distribution. In this way, the second component is uniformly dispersed throughout the positive electrode active material, so that the positive electrode active material can be stably identified. In addition, the second component is uniformly dispersed throughout the positive electrode active material, so that the concentration of the second component in the positive electrode active material changes little regardless of the method of extracting the positive electrode active material. Therefore, a state of a preferred concentration can be maintained, and identification by quantitative analysis is also possible.
[0020] The method for identifying the positive electrode active material will be described in detail later.
[0021] <Method of manufacturing positive electrode active material> Next, a method for producing the above-mentioned positive electrode active material will be described below with reference to the drawings. Fig. 1 is a flow chart showing an example of the method for producing the positive electrode active material according to the present embodiment, and Fig. 2 is a flow chart showing another example of the method for producing the positive electrode active material according to the present embodiment. In the following description, the method for producing the positive electrode active material will be described by taking as an example a case where the positive electrode active material used in a lithium ion secondary battery is produced by a coprecipitation method, but the positive electrode active material of the present embodiment is not limited to this method. Other methods for producing the positive electrode active material include, for example, a solid-phase reaction method, a sol-gel method, a hydrothermal method, and a spray pyrolysis method, and any of these can be applied as the method for producing the positive electrode active material of this embodiment.
[0022] First, as shown in FIG. 1, a precipitant is added to a solution containing a mixture of recycled metal A compound to recycled metal C compound and a metal compound for identification, which is the second component, to precipitate metal A to metal C and the metal ions for identification, which are the second component, as salts. If the timing at which precipitation occurs differs depending on the metal species used, it is advisable to adjust the pH of the solution or the amount of precipitant added. Although FIG. 1 shows three types of metal compounds (recycled metal A compound to recycled metal C compound) as examples, the number of metal compounds used is not limited to this. Two or more types of metal compounds for identification, which are the second component, may also be used.
[0023] Next, the obtained precipitate is heat-treated at a high temperature to obtain a precursor of the positive electrode active material. The heat treatment is preferably drying. The heat treatment step may be performed under known conditions.
[0024] Next, the obtained precursor is mixed with a lithium compound, and then calcined to produce a positive electrode active material. The lithium compound is preferably a transition metal oxide having a layered rock salt crystal structure. The transition metal oxide having a layered rock salt crystal structure is LiNi x Co y Mn z Compounds represented by O2 (x+y+z=1) are preferred.
[0025] In Fig. 1, the second component, the metal compound for identification, is added at a stage before the precipitant is added, but in this embodiment, the timing of adding the second component is not limited to this. For example, as shown in Fig. 2, a precursor containing metals A to C may be prepared in advance by mixing recycled metal A compound to recycled metal C compound, and the second component, the metal compound for identification, may be added when this precursor is mixed with a lithium compound.
[0026] By adding the identifying metal compound at the timing shown in Fig. 1, it becomes easier to mix with the first component (recycled metal A compound to recycled metal C compound in the case of Fig. 1) which is the skeleton of the positive electrode active material, and as a result, the identification ability of the positive electrode active material can be improved. In addition, as shown in Fig. 2, when a precursor is prepared in advance and then the second component is mixed, for example, spray coating method or application method can be suitably applied.
[0027] As described above, by mixing the second component, the identifying metal compound, during the production of the positive electrode active material, it is possible to produce a positive electrode active material in which the first component and the second component are thoroughly mixed.
[0028] In the manufacturing flow shown in Figures 1 and 2, an example using "recycled metal A compound to recycled metal C compound" is shown, but it is of course acceptable that the metal A compound to metal C compound are not recycled materials. For example, when a positive electrode active material is manufactured using recycled metal A compound to metal C compound, the second component is added, and when a positive electrode active material is manufactured using metal A compound to metal C compound that are not recycled materials, the second component is not added. By analyzing each positive electrode and checking whether the second component is detected, it is possible to identify whether the material used in the positive electrode active material is a recycled material or not.
[0029] <Lithium-ion secondary battery> Next, a lithium ion secondary battery will be described as an example of a storage battery using the above-described positive electrode active material. The lithium ion secondary battery according to this embodiment is formed by forming a positive electrode, a negative electrode, and a separator containing an electrolyte between the positive electrode and the negative electrode into a long strip shape, and winding these in a stacked state into a coil shape to form a cylindrical power generating element, which is sealed in a cylindrical battery can (not shown). Note that the shape of the lithium ion secondary battery is not limited to a cylindrical shape, and it can also be formed into a square prism shape.
[0030] The positive electrode is formed by laminating a dispersion of the above-mentioned positive electrode active material, an electronic conductive agent, and a binder in a solvent on a conductor such as aluminum foil.
[0031] As the electronic conductive agent, acetylene black, carbon black, ketjen black, graphite, carbon fiber, etc. can be used. As the binder, polyvinylidene fluoride (PVdF), polytetrafluoroethylene (PTFE), fluorine-based rubber, etc. can be used. As the solvent, N-methyl-2-pyrrolidone (NMP), water, or the like can be used.
[0032] The negative electrode is formed by laminating a dispersion of a negative electrode active material, an electronic conductive agent, and a binder in a solvent on a conductor such as copper foil.
[0033] The negative electrode may be any negative electrode active material that absorbs and releases lithium and contains non-graphitizable carbon and graphite.
[0034] Non-graphitizable carbon (hard carbon) refers to a carbon material that is heat-treated at 1000 to 1400° C. and is difficult to graphitize by heat treatment, and refers to a carbon material in which the conversion from a turbostratic structure to a graphite structure does not occur even by heat treatment at about 3000° C., and the development of graphite crystallites is not observed. Examples of such non-graphitizable carbon include polyacene and silicon-containing non-graphitizable carbon.
[0035] The graphite may be any known graphite, including, for example, any graphite based on artificial graphite, mesophase graphite, or natural graphite.
[0036] The electrolyte may contain at least an inorganic or organic lithium salt, and may be prepared by dissolving the lithium salt in a non-aqueous solvent such as an organic electrolyte or an ionic liquid (room temperature molten salt), and may be interposed between the positive electrode and the negative electrode by impregnating the separator. As such an electrolyte, for example, lithium salts such as LiClO4, LiPF6, LiBF4, LiBOB, LiTFSI, LiAsF6, LiCF3SO3, LiN(CF3SO2)2, LiN(CF3CF2SO2)2, LiN(CF3SO2)(C4F9SO2), and LiC(CF3SO2)3 may be used alone or in combination. The electrolyte may contain commonly used solvents and additives as necessary.
[0037] As the organic electrolyte, cyclic esters such as ethylene carbonate, vinylene carbonate, propylene carbonate, butylene carbonate, γ-butyrolactone, etc., and chain esters such as low boiling point solvents such as diethyl carbonate, ethyl methyl carbonate, dimethyl carbonate, methyl ethyl carbonate, etc. These organic electrolytes may be used alone or in combination.
[0038] As the ionic liquid, an ionic liquid having an imidazolium salt as the cation or an ionic liquid having a cyclic quaternary ammonium salt as the cation can be used.
[0039] Examples of ionic liquids in which an imidazolium salt is the cation include ionic liquids in which a dialkylimidazolium salt, such as 1,3-dimethylimidazolium salt, 1-ethyl-3-methylimidazolium salt, 1-methyl-3-ethylimidazolium salt, 1-methyl-3-butylimidazolium salt, and 1-butyl-3-methylimidazolium salt, and ionic liquids in which a trialkylimidazolium salt, such as 1,2,3-trimethylimidazolium salt, 1,2-dimethyl-3-ethylimidazolium salt, 1,2-dimethyl-3-propylimidazolium salt, and 1-butyl-2,3-dimethylimidazolium salt, is the cation.
[0040] Examples of ionic liquids having a cyclic quaternary ammonium salt as a cation include ionic liquids having a tetraalkylammonium salt such as trimethylethylammonium salt, trimethylpropylammonium salt, trimethylhexylammonium salt, and tetrapentylammonium salt as a cation, and ionic liquids having an alkylpyridinium salt such as N-methylpyridinium salt, N-ethylpyridinium salt, N-propylpyridinium salt, N-butylpyridinium salt, 1-ethyl-2-methylpyridinium salt, 1-butyl-4-methylpyridinium salt, and 1-butyl-2,4-dimethylpyridinium salt as a cation. In addition, examples of ionic liquids having a cyclic quaternary ammonium salt as a cation include ionic liquids having a pyrazolium salt, a pyrrolidinium salt, a piperidinium salt, and the like as a cation.
[0041] The separator may be, for example, a porous film or nonwoven fabric made of a polyolefin-based synthetic resin such as polyethylene, polypropylene, or polyvinylidene fluoride, or cellulose.
[0042] The power generation element composed of the elements described above is formed into a cylindrical shape and enclosed in a cylindrical battery can. A nonaqueous solvent having an electrolyte dissolved therein is then injected into the power generation element, and a can lid is placed over the opening of the cylindrical battery can and joined by welding or the like to enclose the battery can, thereby producing the lithium ion secondary battery according to this embodiment.
[0043] In the lithium ion secondary battery using the positive electrode active material of this embodiment, the second component, which is an identifying metal compound, is uniformly dispersed in the positive electrode. Therefore, even if the active material is detached or peeled off from the battery or positive electrode due to damage or disassembly, for example, the second component can be detected more accurately, so that the accuracy of identifying the raw material and the source of the positive electrode active material can be improved.
[0044] <How to identify positive electrode active materials> Next, a method for identifying a positive electrode active material according to this embodiment will be described. The method for identifying a positive electrode active material according to the present embodiment includes the steps of: (I) a first removal step of removing a positive electrode from a storage battery including the positive electrode active material; (II) a second removal step of removing at least a portion of the positive electrode active material from the positive electrode; (III) an analysis step of identifying information including at least one of the types and contents of the constituent elements of the positive electrode active material taken out in the second removal step; (IV) an identification step of comparing manufacturing profile information that records the manufacturing conditions of the storage battery or the positive electrode with the information acquired in the analysis step to identify information related to the manufacturing of the positive electrode active material; Includes.
[0045] (I: First removal process) First, the positive electrode is removed from a storage battery (for example, a lithium ion secondary battery). There is no particular limitation on the method of removing the positive electrode, but at least a part of the positive electrode may be removed. In addition, if the storage battery has already been disassembled or damaged, the part including the positive electrode may be removed.
[0046] (II: Second removal process) Next, at least a portion of the positive electrode active material is taken out from the removed positive electrode, and the surface of the positive electrode active material is then washed and subjected to an analysis step described below.
[0047] (III: Analysis process) Next, information including at least one of the types and contents of the constituent elements of the positive electrode active material extracted in the second extraction step is identified. Specifically, a qualitative analysis is performed to identify the types of the constituent elements of the positive electrode active material, or a quantitative analysis is performed to identify the contents of the constituent elements of the positive electrode active material.
[0048] For qualitative analysis, it is recommended to use SEM-EDX (energy dispersive X-ray spectroscopy). Specifically, the surface of the positive electrode active material is analyzed by SEM-EDX, and the constituent elements of the positive electrode active material are investigated by the obtained element mapping. The presence or absence of the second component (identification metal) is determined from the investigation results.
[0049] For quantitative analysis, it is recommended to use ICP-AES (Inductively Coupled Plasma-Atomic Emission Spectrometry). Specifically, an acidic aqueous solution such as sulfuric acid or nitric acid is prepared in advance, and the concentration of the target metal in the aqueous solution is determined using a calibration curve. Then, by performing back calculation, the content of the constituent elements in the positive electrode active material can be determined.
[0050] Both the qualitative and quantitative analyses may be performed.
[0051] (IV:Identification process) Finally, the manufacturing profile information that records the manufacturing conditions of the storage battery or positive electrode and the information acquired in the analysis process (quantitative analysis results, qualitative analysis results) are referenced to identify information related to the manufacturing of the positive electrode active material. The "manufacturing conditions of the storage battery or positive electrode" include, for example, whether recycled materials were used as raw materials for the positive electrode material, and if so, what type of raw materials were used.
[0052] By carrying out this identification process, for example, in a case where the second component is added when a positive electrode active material is manufactured using a recycled metal compound, and the second component is not added when a positive electrode active material is manufactured using a metal compound that is not a recycled material, if the second component is detected by qualitative analysis, it can be determined that the battery is a battery manufactured using recycled materials.
[0053] Hereinafter, specific examples of inquiries about the manufacturing profile information of the positive electrode, the qualitative analysis results or the quantitative analysis results, and an example of a method for identifying information about the manufacturing of the positive electrode active material will be specifically described with reference to Tables 1 and 2.
[0054] <<In the case of qualitative analysis>> Table 1 shows an example of an inquiry in the case of a manufacturing profile in which, when a recycled product is used for the metal A compound, component α is added as the second component for identification when a recycled product is used for the metal B compound, and component γ is added as the second component when a recycled product is used for the metal C compound. As shown in Table 1, by identifying the types of constituent elements of the positive electrode active material through qualitative analysis, it is possible to identify whether the metal compound that constitutes the positive electrode is a recycled material or not. For example, when the two types of components α and β are detected in the positive electrode through qualitative analysis, but component γ is not detected, the manufacturing information is obtained that recycled products are used for the metal A compound and the metal B compound, and that recycled products are not used for the metal C compound.
[0055] [Table 1]
[0056] <<For quantitative analysis>> In the case of quantitative analysis, for example, a combination of the contents of each second component, which is an identifying metal component, can be used as an identification code, and various information related to the production of the positive electrode active material can be identified. Specifically, for example, as shown in Table 2, when "α", "β" and "γ" are added as the second components and the ratio is 10:10:10 (ppm), profile information is prepared in advance that metal A, B and C compounds are all recycled products and produced by production process X. Similarly, when "α", "β" and "γ" are added as the second components and the ratio is 10:20:10 (ppm), profile information is prepared in advance that metal A and B compounds are all recycled products and produced by production process X. In this way, by preparing production profile information such as that shown in Table 2, for example, it is possible to identify information related to production, such as the source of the constituent materials of the positive electrode active material and the production conditions. Note that the quantitative analysis result may be a ratio, not an absolute value as shown in Table 2 (unit ppm in the case of the table). In addition, "Process; X, Y, Z" in Table 2 may include various process information. For example, "Process" may include information such as manufacturing conditions (temperature, pH, etc.), manufacturing location (factory, business establishment, etc.), and manufacturing lot number.
[0057] [Table 2]
[0058] According to the above-described embodiment, even if the positive electrode active material is peeled off from the battery or the positive electrode, it is possible to know the type and source of the material used as the positive electrode active material. In addition, since it is possible to know the type and source of the material used as the positive electrode active material, it is possible to appropriately recycle the battery.
[0059] The above describes the form for carrying out the present invention using an embodiment, but the present invention is not limited to such an embodiment, and various modifications and substitutions can be made within the scope that does not deviate from the gist of the present invention.
Claims
1. An active material for a positive electrode of a storage battery, comprising: a first component which is a metal oxide containing a transition element of the fourth period; A second component including at least one transition metal element belonging to the fifth or sixth period; having The first component and the second component are mixed. Cathode active material.
2. The content of the second component is 0.1 to 1000 ppm relative to the content of the first component. The positive electrode active material according to claim 1 .
3. The second component contains two or more transition metal elements belonging to the fifth or sixth period. The positive electrode active material according to claim 1 or 2.
4. The second component is uniformly dispersed. The positive electrode active material according to any one of claims 1 to 3.
5. A first removal step of removing a positive electrode from a storage battery containing the positive electrode active material according to any one of claims 1 to 4; a second removal step of removing at least a portion of the positive electrode active material from the positive electrode; an analysis step of identifying information including at least one of the type and content of the constituent elements of the positive electrode active material extracted in the second extraction step; an identification step of comparing manufacturing profile information that records the manufacturing conditions of the storage battery or the positive electrode with the information acquired in the analysis step, and identifying information related to the manufacturing of the positive electrode active material; A method for identifying a positive electrode active material, comprising:
6. a positive electrode including a positive electrode active material having a lithium transition metal composite oxide, a first component being a metal oxide containing a transition metal element of the fourth period, and a second component containing at least one transition metal element belonging to the fifth period or the sixth period, the first component and the second component being mixed together; A negative electrode including non-graphitizable carbon and graphite as a negative electrode active material that absorbs and releases lithium; an electrolyte interposed between the positive electrode and the negative electrode and containing at least a lithium salt; A lithium-ion secondary battery comprising:
7. The second component is uniformly dispersed in the positive electrode. The lithium ion secondary battery according to claim 6.
Citation Information
Patent Citations
Electrode into which organic / inorganic composite is introduced and electrochemical device comprising said electrode
JP2009544139A