Sensor element and gas sensor

By integrating a low porosity region covered by a porous layer and a high porosity region covered by a dense layer, the sensor element addresses cracking issues and water ingress, enhancing reliability and durability.

JP2024145697AInactive Publication Date: 2024-10-15NGK INSULATORS LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023058160
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-03-31
Publication Date
2024-10-15
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Sensor elements used in gas detection, such as those for NOx in automobile exhaust, are prone to cracks due to the presence of a dense layer that inhibits capillary action, leading to water ingress and potential corrosion at connector electrodes.

Method used

The sensor element incorporates a low porosity region covered by a porous layer and a high porosity region covered by a dense layer, with the high porosity region having a higher porosity than the low porosity region, to prevent water migration and reduce stress differences that cause cracking.

Benefits of technology

This configuration effectively suppresses the occurrence of cracks in the sensor element by managing water ingress and stress distribution, ensuring reliable operation and longevity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024145697000001_ABST
    Figure 2024145697000001_ABST
Patent Text Reader

Abstract

To suppress a crack of a sensor element.SOLUTION: A sensor element 20 includes an element main body 60, an external electrode 64, an upper connector electrode 71, an external lead wire 75, a first internal porous layer 83, and a first dense layer 92. The external lead wire 75 is disposed on a first surface 60a of the element main body 60, and electrically connects the external electrode 64 and the upper connector electrode 71(71b). The first dense layer 92 covers a part of the first surface 60a, is disposed on a rear end side of the element main body 60 in a longitudinal direction relative to at least a part of the first internal porous layer 83, is disposed on a front end side in the longitudinal direction relative to the upper connector electrode 71, and is in contact with the first internal porous layer 83 on the front end side and / or the rear end side. The external lead wire 75 includes a low-porosity region 76 covered with the first internal porous layer 83 of the porous layer 80 and a high-porosity region 77 covered with the first dense layer 92 of the dense layer 90, being in contact with the low-porosity region 76, and having higher porosity than the low-porosity region 76.SELECTED DRAWING: Figure 3
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a sensor element and a gas sensor. [Background technology]

[0002] Conventionally, a sensor element for detecting the concentration of a specific gas such as NOx in a measurement gas such as an automobile exhaust gas is known (see, for example, Patent Document 1). The sensor element of Patent Document 1 includes an element body, an outer electrode, a connector electrode, an outer lead portion, a porous layer, and a dense layer. The front end side of the element body is exposed to the measurement gas. The outer electrode is disposed on the front end side of the side surface of the element body. The connector electrode is disposed on the rear end side of the side surface of the element body and is electrically connected to the contact portion of the connector. The outer lead portion is disposed on the side surface of the element body and is electrically connected to the outer electrode and the connector electrode. The porous layer is disposed on the side surface of the element body and covers at least a part of the outer lead portion to protect it. The dense layer is disposed on the side surface of the element body so as to divide the porous layer along the longitudinal direction of the element body or to be located on the rear end side of the porous layer, and is located on the front end side of the connector electrode. When moisture in the measured gas moves through the porous layer toward the rear end of the element body due to capillary action, capillary action is less likely to occur in the dense layer, and the presence of the dense layer prevents water from reaching the connector electrode. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] International Publication No. 2019 / 155865 Summary of the Invention [Problem to be solved by the invention]

[0004] In a sensor element in which the outer lead portion is covered with a dense layer and a porous layer as in Patent Document 1, cracks may occur in the sensor element.

[0005] The present invention has been made to solve such problems, and has as its main object to suppress cracks in the sensor element. [Means for solving the problem]

[0006] In order to achieve the above-mentioned main object, the present invention adopts the following means.

[0007] [1] The sensor element of the present invention comprises: A sensor element for detecting a specific gas concentration in a measurement gas, comprising: an element body having a front end and a rear end which are both ends along a longitudinal direction and a side surface which is a surface along the longitudinal direction, the front end side being exposed to the measurement gas; an outer electrode disposed on the front end side of the side surface; a connector electrode disposed on the rear end side of the side surface for electrical connection to an outside; an outer lead portion disposed on the side surface and electrically connecting the outer electrode and the connector electrode; a porous layer covering a portion of the side surface; a dense layer that covers a portion of the side surface, is disposed closer to the rear end than at least a portion of the porous layer, is disposed closer to the front end than the connector electrode, and is in contact with the porous layer at the front end and / or the rear end; Equipped with the outer lead portion has a low porosity region covered by the porous layer, and a high porosity region covered by the dense layer, in contact with the low porosity region, and having a porosity higher than that of the low porosity region. It is something.

[0008] In this sensor element, the outer lead portion has a low porosity region covered by a porous layer and a high porosity region that is covered by a dense layer and in contact with the low porosity region and has a higher porosity than the low porosity region. This makes it possible to suppress the occurrence of cracks in the sensor element. The inventors have confirmed this through experiments and analyses.

[0009] [2] In the sensor element described above (the sensor element described in [1] above), the high porosity region may have a porosity of 40% or less. This can prevent water from moving inside the high porosity region, going around the dense layer, and moving toward the rear end of the element body. This can prevent water from reaching the connector electrode.

[0010] [3] In the sensor element described above (the sensor element according to [1] or [2] above), the high porosity region may have a porosity of less than 15%. This makes it possible to further prevent water from moving inside the high porosity region, going around the dense layer, and moving toward the rear end side of the element body.

[0011] [4] In the above-mentioned sensor element (the sensor element according to any one of [1] to [3] above), the difference in porosity between the high porosity region and the low porosity region may be 1% or more. In this way, the effect of suppressing the occurrence of cracks in the sensor element by providing the above-mentioned high porosity region and low porosity region can be more reliably obtained.

[0012] [5] In the above-mentioned sensor element (the sensor element according to any one of [1] to [4] above), the high porosity region may have a porosity of 5% or more. In this way, the effect of suppressing the occurrence of cracks in the sensor element by providing the above-mentioned high porosity region and low porosity region can be more reliably obtained.

[0013] [6] In the above-mentioned sensor element (the sensor element according to any one of the above [1] to [5]), the dense layer may have a thickness of 10 μm or less. This can further suppress the occurrence of cracks in the sensor element.

[0014] [7] In the above-mentioned sensor element (the sensor element according to any one of [1] to [6] above), the dense layer may have an overlap portion in a portion in contact with the porous layer that overlaps with the porous layer in a thickness direction of the dense layer, and the dense layer may cover only the high porosity region of the high porosity region and the low porosity region from the front end side to the rear end side of the dense layer, including the overlap portion.

[0015] [8] In the above-mentioned sensor element (the sensor element according to any one of [1] to [7] above), the high porosity region may have a protruding portion protruding beyond the dense layer toward the front end side and / or the rear end side and covered by the porous layer, and the length of the protruding portion in the longitudinal direction may be 0.5 mm or less. In this way, the effect of suppressing the occurrence of cracks in the sensor element by providing the above-mentioned high porosity region and low porosity region can be more reliably obtained.

[0016] [9] In the above-mentioned sensor element (the sensor element according to any one of [1] to [8] above), the outer lead portion may contain zirconia. Here, when the outer lead portion contains zirconia, the zirconia expands due to TM transformation, and the outer lead wire is deformed, which tends to cause cracks in the sensor element. Therefore, when the outer lead portion contains zirconia, it is very meaningful to provide the outer lead portion with a low porosity region and a high porosity region to suppress the occurrence of cracks in the sensor element.

[0017]

[10] A gas sensor of the present invention includes the sensor element according to any one of [1] to [9] above. Therefore, the gas sensor can obtain the same effects as those of the above-mentioned sensor element, such as the effect of suppressing the occurrence of cracks in the sensor element. [Brief description of the drawings]

[0018] [Figure 1] FIG. 4 is a vertical cross-sectional view showing a state in which the gas sensor 10 is attached to a pipe 58. [Diagram 2] FIG. [Diagram 3] FIG. [Figure 4] FIG. [Diagram 5] FIG. 4 is a vertical cross-sectional view showing the periphery of a high porosity region 77 covered with a first dense layer 92. [Figure 6] 13 is a cross-sectional view showing the periphery of a first dense layer 92 and a high porosity region 77 in a modified example. FIG. [Figure 7] 13 is a cross-sectional view showing the periphery of a first dense layer 92 and a high porosity region 77 in a modified example. FIG. [Figure 8] 13 is a cross-sectional view showing the periphery of a first dense layer 92 and a high porosity region 77 in a modified example. FIG. [Figure 9] 13 is a cross-sectional view showing the periphery of a first dense layer 92 and a high porosity region 77 in a modified example. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0019] Next, an embodiment of the present invention will be described with reference to the drawings. FIG. 1 is a vertical cross-sectional view showing a state in which a gas sensor 10 according to an embodiment of the present invention is attached to a pipe 58. FIG. 2 is a perspective view of a sensor element 20 as viewed from the upper right front. FIG. 3 is a vertical cross-sectional view showing a schematic vertical cross-section of the sensor element 20. FIG. 4 is a top view of the sensor element 20. FIG. 5 is a vertical cross-sectional view showing the periphery of a high porosity region 77 of an outer lead wire 75 covered with a first dense layer 92. In this embodiment, as shown in FIGS. 1 to 5, the longitudinal direction of the element body 60 of the sensor element 20 is defined as the front-rear direction (length direction), the stacking direction (thickness direction) of the solid electrolyte layer of the element body 60 is defined as the up-down direction, and the direction perpendicular to the front-rear direction and the up-down direction is defined as the left-right direction (width direction).

[0020] As shown in FIG. 1, the gas sensor 10 includes an assembly 15, a nut 47, an outer tube 48, a connector 50, a lead wire 55, and a rubber plug 57. The assembly 15 includes a sensor element 20, a protective cover 30, and an element sealing body 40. The gas sensor 10 is attached to a pipe 58 such as an exhaust gas pipe of a vehicle, and is used to measure the concentration (specific gas concentration) of a specific gas such as NOx or O2 contained in exhaust gas as a measurement gas. In this embodiment, the gas sensor 10 measures the NOx concentration as the specific gas concentration. Of both ends (front end and rear end) along the longitudinal direction of the sensor element 20, the front end side is the side exposed to the measurement gas.

[0021] 1, the protective cover 30 includes a cylindrical inner protective cover 31 with a bottom that covers the front end side of the sensor element 20, and a cylindrical outer protective cover 32 with a bottom that covers the inner protective cover 31. A plurality of holes are formed in each of the inner protective cover 31 and the outer protective cover 32 for passing the measurement gas. An element chamber 33 is formed as a space surrounded by the inner protective cover 31, and a fifth surface 60e (front end surface) of the sensor element 20 is disposed within the element chamber 33.

[0022] The element sealing body 40 is a member that seals and fixes the sensor element 20. The element sealing body 40 includes a cylindrical body 41 having a metal shell 42 and an inner cylinder 43, insulators 44a to 44c (an example of a dense body), powder compacts 45a and 45b, and a metal ring 46. The sensor element 20 is disposed so as to extend along the central axis of the element sealing body 40 (here, an axis extending in the front-rear direction), and penetrates the element sealing body 40 in the axial direction.

[0023] The metal shell 42 is a cylindrical metal member. The metal shell 42 has a thick portion 42a whose inner diameter is smaller at the front side than at the rear side. A protective cover 30 is attached to the metal shell 42 on the same side (front side) as the front end of the sensor element 20. The rear end of the metal shell 42 is welded to a flange portion 43a of the inner cylinder 43. A part of the inner peripheral surface of the thick portion 42a is a bottom surface 42b which is a stepped surface. This bottom surface 42b holds the insulator 44a so that it does not protrude forward. The metal shell 42 has a through hole penetrating the metal shell 42 along the axial direction (here, the front-rear direction), and the sensor element 20 penetrates the inside of this through hole.

[0024] The inner cylinder 43 is a cylindrical metal member and has a flange portion 43a at the front end. The inner cylinder 43 and the metal shell 42 are welded coaxially. The inner cylinder 43 is also formed with a reduced diameter portion 43c for pressing the powder compact 45b in the central axial direction of the inner cylinder 43, and a reduced diameter portion 43d for pressing the insulators 44a to 44c and the powder compacts 45a and 45b forward via the metal ring 46. The inner cylinder 43 has a through hole penetrating the inner cylinder 43 along the axial direction (here, the front-rear direction), and the sensor element 20 passes through the inside of this through hole. The through hole of the metal shell 42 and the through hole of the inner cylinder 43 are in communication with each other in the axial direction, and these constitute the through hole of the cylindrical body 41.

[0025] The insulators 44a to 44c and the powder compacts 45a and 45b are disposed between the inner circumferential surface of the through hole of the cylindrical body 41 and the sensor element 20. The insulators 44a to 44c serve as supporters for the powder compacts 45a and 45b. Examples of materials for the insulators 44a to 44c include ceramics such as alumina, steatite, zirconia, spinel, cordierite, and mullite, and glass. The insulators 44a to 44c are dense members, and the porosity thereof is, for example, less than 1%. Each of the insulators 44a to 44c is a hollow columnar member having a through hole penetrating the insulator along the axial direction (here, the front-rear direction), and the sensor element 20 penetrates through the inside of this through hole. In this embodiment, the through hole of each of the insulators 44a to 44c has a rectangular cross section perpendicular to the axial direction in accordance with the shape of the sensor element 20. The powder compacts 45a and 45b are, for example, formed from powder, and serve as a sealing material. Examples of the material of the powder compacts 45a and 45b include ceramic powder such as alumina powder and boron nitride, in addition to talc, and the powder compacts 45a and 45b may each contain at least one of these. The average particle size of the particles constituting the powder compacts 45a and 45b may be 150 to 300 μm. The powder compact 45a is filled between the insulators 44a and 44b, and is sandwiched and pressed by the insulators 44a and 44b from both sides (front and back) in the axial direction. The powder compact 45b is filled between the insulators 44b and 44c, and is sandwiched and pressed by the insulators 44b and 44c from both sides (front and back) in the axial direction. The insulators 44a to 44c and the powder compacts 45a, 45b are sandwiched and pressed from both sides (front and back) in the axial direction by the bottom surface 42b of the thick portion 42a of the metal shell 42, the reduced diameter portion 43d, and the metal ring 46. The powder compacts 45a, 45b are compressed between the cylindrical body 41 and the sensor element 20 by the pressing forces from the reduced diameter portions 43c, 43d, so that the powder compacts 45a, 45b seal the gap between the element chamber 33 in the protective cover 30 and a space 49 in the outer cylinder 48 and fix the sensor element 20.

[0026] The nut 47 is fixed to the outside of the metallic shell 42 coaxially with the metallic shell 42. A male thread is formed on the outer circumferential surface of the nut 47. This male thread is screwed into a female thread provided on the inner circumferential surface of a fixing member 59 welded to the pipe 58. As a result, the gas sensor 10 is fixed to the pipe 58 such that the front end side of the sensor element 20 and a portion of the protective cover 30 protrude into the pipe 58.

[0027] The outer tube 48 is a cylindrical metal member, and covers the inner tube 43, the rear end side of the sensor element 20, and the connector 50. The rear end of the metal shell 42 is inserted inside the outer tube 48. The front end of the outer tube 48 is welded to the metal shell 42. A plurality of lead wires 55 connected to the connector 50 are drawn out from the rear end of the outer tube 48 to the outside. The connector 50 has housings 51a and 51b, a plurality of contact fittings 52, and a clamp 53. The housings 51a and 51b are members made of ceramics such as alumina, and are arranged above and below the rear end of the sensor element 20. The plurality of contact fittings 52 are all metal members, and are arranged below the housing 51a and above the housing 51b. The clamp 53 is a member formed by bending a plate-shaped metal into a C-shape, and uses elastic force to clamp the housings 51a and 51b from above and below and press them in a direction toward each other. The housings 51a and 51b clamp and fix the rear end of the sensor element 20 via the contact fittings 52 by the elastic force of the clamp 53. The contact fittings 52 are in contact with and electrically connected to the corresponding connector electrodes among the upper connector electrodes 71 and the lower connector electrodes 72 arranged on the surface of the rear end side of the sensor element 20, and are also electrically connected to the corresponding lead wires among the lead wires 55. The lead wires 55 are electrically connected to the connector 50 and to any of the electrodes 64 to 68 and the heater 69 inside the sensor element 20 via any of the upper connector electrodes 71 and the lower connector electrodes 72. The gap between the outer tube 48 and the lead wire 55 is sealed by a rubber plug 57. A space 49 in the outer tube 48 is filled with a reference gas. A sixth surface 60f (rear end surface) of the sensor element 20 is disposed in the space 49.

[0028] As shown in Figs. 2 to 4, the sensor element 20 includes an element body 60, a detection unit 63, a heater 69, a plurality of upper connector electrodes 71, a plurality of lower connector electrodes 72, a porous layer 80, and a dense layer 90. The element body 60 has a laminated body in which a plurality of oxygen ion conductive solid electrolyte layers (six in Fig. 3) such as zirconia (ZrO2) are laminated. The element body 60 has a rectangular parallelepiped shape with the longitudinal direction along the front-rear direction, and has first to sixth faces 60a to 60f as outer surfaces on the top, bottom, left, right, front and rear sides. The first to fourth faces 60a to 60d are surfaces along the longitudinal direction of the element body 60 and correspond to side faces of the element body 60. The fifth face 60e is the front end face of the element body 60, and the sixth face 60f is the rear end face of the element body 60. The dimensions of the element body 60 may be, for example, a length in the front-rear direction of 25 mm to 100 mm, a width in the left-right direction of 2 mm to 10 mm, and a thickness in the up-down direction of 0.5 mm to 5 mm. The element body 60 is formed with a measurement gas inlet 61 that opens to the fifth surface 60e and introduces a measurement gas into itself, and a reference gas inlet 62 that opens to the sixth surface 60f and introduces a reference gas (here, the atmosphere) that serves as a reference for detecting a specific gas concentration into itself.

[0029] The detection section 63 is for detecting the concentration of a specific gas in the measurement gas. The detection section 63 has a plurality of electrodes disposed on the front end side of the element body 60. In this embodiment, the detection section 63 includes an outer electrode 64 disposed on the first surface 60a, and an inner main pump electrode 65, an inner auxiliary pump electrode 66, a measurement electrode 67, and a reference electrode 68 disposed inside the element body 60. The inner main pump electrode 65 and the inner auxiliary pump electrode 66 are disposed on the inner circumferential surface of the space inside the element body 60, and have a tunnel-like structure.

[0030] The principle by which the detection unit 63 detects the concentration of a specific gas in a measurement gas is well known, and therefore a detailed description thereof will be omitted. The detection unit 63 detects the concentration of a specific gas, for example, as follows. The detection unit 63 pumps out or pumps in oxygen in the measurement gas around the inner main pump electrode 65 to the outside (element chamber 33) based on a voltage applied between the outer electrode 64 and the inner main pump electrode 65. The detection unit 63 also pumps out or pumps in oxygen in the measurement gas around the inner auxiliary pump electrode 66 to the outside (element chamber 33) based on a voltage applied between the outer electrode 64 and the inner auxiliary pump electrode 66. As a result, the measurement gas whose oxygen concentration has been adjusted to a predetermined concentration reaches the vicinity of the measurement electrode 67. The measurement electrode 67 functions as a NOx reduction catalyst and reduces the specific gas (NOx) in the measurement gas that has reached it. The detection unit 63 generates, as an electric signal, an electromotive force generated between the measurement electrode 67 and the reference electrode 68 in accordance with the oxygen concentration after reduction, or a current flowing between the measurement electrode 67 and the outer electrode 64 based on the electromotive force. The electric signal thus generated by the detection unit 63 is a signal indicating a value in accordance with the specific gas concentration in the measured gas (a value from which the specific gas concentration can be derived), and corresponds to the detection value detected by the detection unit 63.

[0031] The heater 69 is an electric resistor disposed inside the element body 60. When power is supplied from the outside, the heater 69 generates heat to heat the element body 60. The heater 69 heats and keeps warm the solid electrolyte layer that forms the element body 60, and can adjust the temperature to a temperature (e.g., 800° C.) at which the solid electrolyte layer is activated.

[0032] The upper connector electrodes 71 and the lower connector electrodes 72 are disposed on the rear end side of one of the side surfaces of the element body 60, and are electrodes for electrical conduction with the outside. The upper connector electrodes 71 and the lower connector electrodes 72 are exposed without being covered by the porous layer 80. In this embodiment, the four upper connector electrodes 71 (71a to 71d in FIG. 4) are arranged in the left-right direction and disposed on the rear end side of the first surface 60a (upper surface). The four lower connector electrodes 72 are arranged in the left-right direction and disposed on the rear end side of the second surface 60b (lower surface) facing the first surface 60a (upper surface). The four upper connector electrodes 71 (71a to 71d) and the four lower connector electrodes 72 are electrically connected to the electrodes 64 to 68 and the heater 69 of the detection unit 63, respectively. In this embodiment, the upper connector electrode 71a is electrically connected to the measurement electrode 67, the upper connector electrode 71b is electrically connected to the outer electrode 64, the upper connector electrode 71c is electrically connected to the inner auxiliary pump electrode 66, the upper connector electrode 71d is electrically connected to the inner main pump electrode 65, the three lower connector electrodes 72 are electrically connected to the heaters 69, and one lower connector electrode 72 is electrically connected to the reference electrode 68. The upper connector electrode 71b and the outer electrode 64 are electrically connected via an outer lead wire 75 disposed on the first surface 60a (see FIGS. 3 and 4). The other connector electrodes are electrically connected to the corresponding electrodes or the heater 69 via lead wires or through holes disposed inside the element body 60.

[0033] The outer lead wire 75 is a conductor containing a precious metal such as platinum (Pt) or a high melting point metal such as tungsten (W) or molybdenum (Mo). The outer lead wire 75 is preferably a conductor of a cermet containing a precious metal or a high melting point metal and an oxygen ion conductive solid electrolyte (zirconia in this embodiment) contained in the element body 60. In this embodiment, the outer lead wire 75 is a conductor of a cermet containing platinum and zirconia. As shown in Figs. 3, 4, and 5, the outer lead wire 75 has a low porosity region 76 and a high porosity region 77. In this embodiment, the outer lead wire 75 is configured such that the entire portion other than the high porosity region 77 is the low porosity region 76. The low porosity region 76 is covered with a porous layer 80, more specifically, with a first inner porous layer 83 as shown in Fig. 3. The low porosity region 76 has a front end portion 76a disposed in front of the high porosity region 77 and in contact with the high porosity region 77 from the front to the rear, and a rear end portion 76b disposed behind the high porosity region 77 and in contact with the high porosity region 77 from the front to the rear. The front end portion 76a of the low porosity region 76 is covered by a front end portion 83a of the first inner porous layer 83 of the porous layer 80, and the rear end portion 76b is covered by a rear end portion 83b of the first inner porous layer 83. The high porosity region 77 is covered by a dense layer 90, and more specifically, is covered by a first dense layer 92 as shown in FIG. 3. As shown in FIG. 3 and FIG. 5, the first dense layer 92 and the high porosity region 77 have the same front-to-rear length, and their front end positions and rear end positions are the same. Therefore, the high porosity region 77 does not have a protruding portion protruding further toward the front end side and / or rear end side than the first dense layer 92. The high porosity region 77 has a higher porosity than the low porosity region 76. The porosity of the high porosity region 77 may be 5% or more. The porosity of the high porosity region 77 may be 40% or less, or less than 15%. The porosity of the low porosity region 76 may be lower than the porosity of the high porosity region 77, and the difference in porosity between the high porosity region 77 and the low porosity region 76 may be 1% or more. The porosity of the front end portion 76a and the rear end portion 76b of the low porosity region 76 may be different.The low porosity region 76 and the high porosity region 77 may be made of different materials, but in this embodiment, the low porosity region 76 and the high porosity region 77 are made of the same material but have different porosities. The line width (thickness) of the outer lead wire 75 may be, for example, 0.1 mm or more and 1.0 mm or less. The line thickness (thickness) of the outer lead wire 75 may be, for example, 1 μm or more and 30 μm or less. An insulating layer (not shown) may be disposed between the outer lead wire 75 and the first surface 60a of the element body 60 to insulate the outer lead wire 75 from the solid electrolyte layer of the element body 60.

[0034] The porosity of the low porosity region 76 and the high porosity region 77 of the outer lead wire 75 is a value derived as follows using an image (SEM image) obtained by observation using a scanning electron microscope (SEM). First, the sensor element 20 is cut along the thickness direction of the outer lead wire 75 so that the cross section of the outer lead wire 75 is the observation surface, and the cut surface is filled with resin and polished to obtain an observation sample. Next, the magnification of the SEM is set to 1000 to 10000 times, and an SEM image of the outer lead wire 75 is obtained by photographing the observation surface of the observation sample. Next, the obtained image is analyzed, and a threshold value is determined by a discriminant analysis method (Otsu's binarization) from the brightness distribution of the brightness data of the pixels in the image. After that, each pixel in the image is binarized into an object part and a pore part based on the determined threshold value, and the area of ​​the object part and the area of ​​the pore part are calculated. Then, the ratio of the area of ​​the pore part to the total area (the total area of ​​the object part and the pore part) is derived as the porosity (unit: %). The porosity of the low porosity region 76 is a value measured in a region of the low porosity region 76 near the high porosity region 77, for example, a value measured on a cross section at a position 1 mm away from the high porosity region 77 as an observation surface. The porosity of the high porosity region 77 is a value measured in a region of the high porosity region 77 near the low porosity region 76, for example, a value measured on a cross section at a position 1 mm away from the low porosity region 76 as an observation surface. The porosities of the porous layer 80 and dense layer 90 described below are also values ​​derived in a similar manner.

[0035] The porous layer 80 is a porous body that covers part of the side surfaces, i.e., the first and second faces 60a and 60b, of the element body 60 on which the upper and lower connector electrodes 71 and 72 are disposed. In this embodiment, the porous layer 80 covers at least the front end sides of the first and second faces 60a and 60b. The porous layer 80 includes an inner porous layer 81 that covers the first and second faces 60a and 60b, respectively, and an outer porous layer 85 that is disposed on the outside of the inner porous layer 81.

[0036] The inner porous layer 81 includes a first inner porous layer 83 covering the first surface 60a and a second inner porous layer 84 covering the second surface 60b. The first inner porous layer 83 has a front end portion 83a and a rear end portion 83b (see Figs. 2 to 4 and 5). The front end portion 83a covers the area of ​​the first surface 60a from the front end of the first surface 60a to the front end of the first dense layer 92. The rear end portion 83b covers the area of ​​the first surface 60a from the rear end of the first dense layer 92 to the rear end of the first surface 60a, except for the area where the upper connector electrode 71 is present. The widths of the front end portion 83a and the rear end portion 83b of the first inner porous layer 83 are the same as the width of the first surface 60a, and the front end portion 83a and the rear end portion 83b cover the first surface 60a from the left end to the right end of the first surface 60a. The first inner porous layer 83 covers at least a part of the outer electrode 64 and the outer lead wire 75. In this embodiment, as shown in Figs. 3 and 4, the first inner porous layer 83 covers the entire outer electrode 64 and the outer lead wire 75 except for the high porosity region 77 (i.e., the entire low porosity region 76). The first inner porous layer 83 serves as a protective layer that protects the outer electrode 64 and the outer lead wire 75 from components such as sulfuric acid in the measured gas, and suppresses corrosion of these electrodes.

[0037] The second inner porous layer 84 has a front end portion 84a and a rear end portion 84b (see Figs. 2 and 3). The front end portion 84a covers the area of ​​the second surface 60b from the front end of the second surface 60a to the front end of the second dense layer 96. The rear end portion 84b covers the area of ​​the second surface 60b from the rear end of the second dense layer 96 to the rear end of the second surface 60b, except for the area where the lower connector electrode 72 is present. The left-right width of the front end portion 84a and the rear end portion 84b of the second inner porous layer 84 is the same as the left-right width of the second surface 60b, and the front end portion 84a and the rear end portion 84b cover the second surface 60b from the left end to the right end of the second surface 60b.

[0038] The outer porous layer 85 covers at least a part of each of the first to fifth faces 60a to 60e. The outer porous layer 85 covers the first face 60a and the second face 60b by covering the inner porous layer 81. The outer porous layer 85 has a shorter length in the front-rear direction than the inner porous layer 81, and unlike the inner porous layer 81, covers only the front end and the region near the front end of the element body 60. As a result, the outer porous layer 85 covers the peripheral portion of the multiple electrodes 64 to 68 of the detection unit 63 of the element body 60, in other words, the portion of the element body 60 that is disposed in the element chamber 33 and exposed to the measured gas. As a result, the outer porous layer 85 serves as a protective layer that suppresses the occurrence of cracks in the element body 60 due to the adhesion of water or the like in the measured gas.

[0039] The porous layer 80 is made of a ceramic porous body such as a porous alumina body, a porous zirconia body, a porous spinel body, a porous cordierite body, a porous titania body, or a porous magnesia body. In this embodiment, the porous layer 80 is made of a porous alumina body. The thickness of each of the first inner porous layer 83 and the second inner porous layer 84 may be, for example, 5 μm or more and 40 μm or less. The thickness of the outer porous layer 85 may be, for example, 40 μm or more and 800 μm or less. The porosity of the porous layer 80 is 10% or more. The porous layer 80 covers the outer electrode 64 and the measurement gas inlet 61, but if the porosity of the porous layer 80 is 10% or more, the measurement gas can pass through the porous layer 80. The porosity of the inner porous layer 81 may be 10% or more and 50% or less. The porosity of the outer porous layer 85 may be 10% or more and 85% or less. The outer porous layer 85 may have the same porosity as the inner porous layer 81 , or may have a higher porosity than the inner porous layer 81 .

[0040] The dense layer 90 suppresses the capillary phenomenon of water along the longitudinal direction of the element body 60. In this embodiment, the dense layer 90 has a first dense layer 92 and a second dense layer 96. The first dense layer 92 is provided on the first surface 60a on which the upper connector electrode 71 and the first inner porous layer 83 are provided. The first dense layer 92 is provided on the rear end side, i.e., rearward, of the element body 60 from at least a part of the porous layer 80 (here, the outer porous layer 85 and the front end side portion 83a). The first dense layer 92 is provided on the front end side, i.e., forward of the plurality of upper connector electrodes 71, of the element body 60. The first dense layer 92 is provided rearward from the outer electrode 64. The first dense layer 92 is provided rearward from any of the plurality of electrodes 64 to 68 of the detection unit 63 including the outer electrode 64 (see FIG. 3). When water moves backward in the first inner porous layer 83 by capillary action, the first dense layer 92 serves to prevent the water from passing through the first dense layer 92 and thus preventing the water from reaching the upper connector electrode 71. The first dense layer 92 is a dense layer having a porosity of less than 10%. The left-right width of the first dense layer 92 is the same as the left-right width of the first surface 60a, and the first dense layer 92 covers the first surface 60a from the left end to the right end of the first surface 60a. The front end of the first dense layer 92 contacts the rear end of the front end portion 83a of the first inner porous layer 83. The rear end of the first dense layer 92 contacts the front end of the rear end portion 83b of the first inner porous layer 83. The first dense layer 92 covers the high porosity region 77 of the outer lead wire 75, as shown in Figures 3, 4, and 5.

[0041] The second dense layer 96 is provided on the second surface 60b on which the lower connector electrodes 72 and the second inner porous layer 84 are disposed. The second dense layer 96 is provided on the rear end side, i.e., rearward, of the element body 60 from at least a part of the porous layer 80 (here, the outer porous layer 85 and the front end side portion 84a). The second dense layer 96 is provided on the front end side, i.e., forward of the lower connector electrodes 72, of the element body 60 from the lower connector electrodes 72. The second dense layer 96 is provided rearward from all of the electrodes 64 to 68 of the detection unit 63 including the outer electrode 64 (see FIG. 3). When water moves rearward in the second inner porous layer 84 by capillary action, the second dense layer 96 serves to prevent the water from passing through the second dense layer 96 and thus preventing the water from reaching the lower connector electrode 72. The second dense layer 96 is a dense layer with a porosity of less than 10%. The left-right width of the second dense layer 96 is the same as the left-right width of the second surface 60b, and the second dense layer 96 covers the second surface 60b from the left end to the right end of the second surface 60b. The front end of the second dense layer 96 contacts the rear end of the front end portion 84a of the second inner porous layer 84. The rear end of the second dense layer 96 contacts the front end of the rear end portion 84b of the second inner porous layer 84.

[0042] The first dense layer 92 and the second dense layer 96 differ from the porous layer 80 in that the porosity is less than 10%, but ceramics made of the materials exemplified for the porous layer 80 can be used. In this embodiment, the first dense layer 92 and the second dense layer 96 are both made of alumina ceramics. The thickness of the first dense layer 92 may be, for example, 5 μm or more and 40 μm or less. The thickness of the first dense layer 92 may be thinner than the thickness of the first inner porous layer 83. The thickness of the first dense layer 92 may be thinner than the thickness of the outer lead wire 75. The thickness of the first dense layer 92 may be 10 μm or less. The thickness of the first dense layer 92 is measured at a portion of the first dense layer 92 located directly above the outer lead wire 75. The porosity of each of the first dense layer 92 and the second dense layer 96 is preferably 8% or less, more preferably 5% or less. The smaller the porosity, the more the first dense layer 92 and the second dense layer 96 can suppress the capillary phenomenon of water along the longitudinal direction of the element body 60 .

[0043] In the longitudinal direction (here, the front-rear direction) of the element body 60, the length Le1 (see FIG. 4) of the first dense layer 92 may be 0.5 mm or more. The length Le1 may be 5 mm or more. The length Le1 may be 25 mm or less, or 20 mm or less. In this embodiment, the length of the high porosity region 77 of the outer lead wire 75 is equal to the length Le1 of the first dense layer 92.

[0044] The first dense layer 92 and the second dense layer 96 are disposed so as to overlap with the inner peripheral surface of any one of the plurality of insulators 44a to 44c in the longitudinal direction of the element body 60. In this embodiment, as shown in Fig. 1, the first dense layer 92 and the second dense layer 96 are disposed so as to overlap with the inner peripheral surface of the insulator 44b among the insulators 44a to 44c in the longitudinal direction of the sensor element 20. The inner peripheral surface of the insulator 44b is a surface of the insulator 44b facing the first dense layer 92 and the second dense layer 96, i.e., a surface exposed toward the first dense layer 92 and the second dense layer 96, and is a surface located on the upper and lower sides of the inner peripheral surface of the insulator 44b having a rectangular cross section.

[0045] Next, a method for manufacturing the gas sensor 10 thus constructed will be described. After the method for manufacturing the sensor element 20 is described, a method for manufacturing the gas sensor 10 incorporating the sensor element 20 will be described.

[0046] A method for manufacturing the sensor element 20 will be described. First, a plurality of (here, six) unfired ceramic green sheets corresponding to the element body 60 are prepared. In each green sheet, notches, through holes, grooves, etc. are provided by punching processing as necessary, and wiring patterns such as electrodes and outer lead wires 75 are screen-printed. In addition, the unfired porous layers that become the first inner porous layer 83 and the second inner porous layer 84 after firing, and the unfired dense layers that become the first dense layer 92 and the second dense layer 96 after firing are also formed on the surfaces of the green sheets that correspond to the first and second surfaces 60a, 60b by screen printing. After that, a plurality of green sheets are stacked. The stacked plurality of green sheets are the unfired element body that becomes the element body after firing, and include the unfired porous layer and the unfired dense layer. Then, this unfired element body is fired to obtain the element body 60 that includes the first inner porous layer 83, the second inner porous layer 84, the first dense layer 92, and the second dense layer 96. Next, the outer porous layer 85 is formed by plasma spraying to obtain the sensor element 20. Note that, in addition to screen printing and plasma spraying, gel casting, dipping, etc. can also be used as a manufacturing method for the porous layer 80, the first dense layer 92, and the second dense layer 96.

[0047] The wiring pattern that becomes the outer lead wire 75 after firing can be formed, for example, by screen printing a slurry made by kneading raw material particles (here, platinum particles and zirconia particles) of the outer lead wire 75, a pore-forming material, and a solvent. The wiring patterns of the low porosity region 76 and the high porosity region 77 of the outer lead wire 75 can be formed, for example, by preparing two types of slurries made of the same material except for the content ratio of the pore-forming material, and screen printing the two types of slurries separately.

[0048] A method for manufacturing the gas sensor 10 incorporating the sensor element 20 will be described. First, the sensor element 20 is inserted axially into the through hole of the cylindrical body 41, and the insulator 44a, the powder compact 45a, the insulator 44b, the powder compact 45b, the insulator 44c, and the metal ring 46 are arranged in this order between the inner circumferential surface of the cylindrical body 41 and the sensor element 20. Next, the metal ring 46 is pressed to compress the powder compacts 45a and 45b, and in this state, the diameter-reduced portions 43c and 43d are formed to manufacture the element sealing body 40, and the gap between the inner circumferential surface of the cylindrical body 41 and the sensor element 20 is sealed. After that, the protective cover 30 is welded to the element sealing body 40, and the nut 47 is attached to obtain the assembly 15. Then, the lead wire 55 passing through the rubber plug 57 and the connector 50 connected thereto are prepared. The prepared connector 50 is connected to the rear end side of the sensor element 20, and the multiple contact metal fittings 52 of the connector 50 are electrically connected to corresponding connector electrodes among the multiple upper connector electrodes 71 and lower connector electrodes 72. Thereafter, the outer cylinder 48 is fixed to the main metal fitting 42 by welding, thereby obtaining the gas sensor 10.

[0049] Next, an example of use of the gas sensor 10 thus constructed will be described. When the gas sensor 10 is attached to the pipe 58 as shown in FIG. 1 and a measurement gas flows through the pipe 58, the measurement gas flows through the protective cover 30 and flows into the element chamber 33, and the front end side of the sensor element 20 is exposed to the measurement gas. When the measurement gas passes through the porous layer 80 and reaches the outer electrode 64 and then reaches the sensor element 20 from the measurement gas inlet 61, the detection unit 63 generates an electric signal corresponding to the NOx concentration in the measurement gas, as described above. This electric signal is extracted through the upper and lower connector electrodes 71 and 72, and the NOx concentration is detected based on the electric signal.

[0050] In the sensor element 20 of the gas sensor 10 thus configured, as described above, the outer lead wire 75 has the low porosity region 76 covered by the first inner porous layer 83 of the porous layer 80, and the high porosity region 77 covered by the first dense layer 92, in contact with the low porosity region 76, and having a higher porosity than the low porosity region 76. This makes it possible to suppress the occurrence of cracks in the sensor element 20. The inventors have confirmed this through experiments and analysis. The reason why such an effect is obtained is considered to be as follows. First, the first dense layer 92 has a lower porosity and is denser than the first inner porous layer 83, and therefore has a higher Young's modulus, so that the internal stress of the first dense layer 92 is likely to be larger than that of the first inner porous layer 83. As a result, when the outer lead wire 75 is deformed, a stress difference is likely to occur between the first dense layer 92 and the first inner porous layer 83 (particularly, between the first dense layer 92 and the rear end of the front end portion 83a, and between the first dense layer 92 and the front end of the rear end portion 83b). If this stress difference becomes too large, cracks may occur in the sensor element 20, for example, in the first dense layer 92 having a high Young's modulus. However, in the sensor element 20 of this embodiment, the high porosity region 77 of the outer lead wire 75 covered with the first dense layer 92 has a higher porosity than the low porosity region 76, and therefore the high porosity region 77 has a lower Young's modulus than the low porosity region 76. Therefore, the high porosity region 77 with a low Young's modulus exists in the portion covered with the first dense layer 92 with a high Young's modulus, and the low porosity region 76 with a high Young's modulus exists in the portion covered with the first inner porous layer 83 with a low Young's modulus, so that when the outer lead wire 75 is deformed, the stress difference between the first dense layer 92 and the first inner porous layer 83 can be reduced. This is thought to suppress the occurrence of cracks in the sensor element 20.

[0051] The deformation of the outer lead wire 75 is considered to occur due to thermal expansion of the outer lead wire 75 caused by heat from the heater 69 or high-temperature gas to be measured when the gas sensor 10 is in use. In this embodiment, since the outer lead wire 75 contains zirconia, it is considered that the heat generated when the gas sensor 10 is in use may cause TM transformation of zirconia (change in crystal structure from T phase (tetragonal) to M phase (monoclinic)), which causes the volume of zirconia to expand, resulting in deformation of the outer lead wire 75. In the sensor element 20 of this embodiment, the occurrence of cracks in the sensor element 20 caused by such deformation of the outer lead wire 75 can be suppressed.

[0052] Furthermore, the measured gas may contain water (water, sulfuric acid dissolved in water, etc.), and this water may move through the porous layer 80 by capillary action. If this water reaches the upper and lower connector electrodes 71, 72, there is a concern that the upper and lower connector electrodes 71, 72 and the contact fittings 52 of the connector 50 that contact the upper and lower connector electrodes 71, 72 may rust or corrode. However, in the gas sensor 10 of this embodiment, even if the water in the measured gas moves through the porous layer 80 (particularly through the first inner porous layer 83 and the second inner porous layer 84) toward the rear end side of the sensor element 20 (element body 60) by capillary action, the water reaches the first and second dense layers 92, 96 before reaching the upper and lower connector electrodes 71, 72. Since the first and second dense layers 92, 96 are denser than the first and second inner porous layers 83, 84, capillary action of water is less likely to occur along the longitudinal direction of the element body 60. As a result, water can be prevented from moving beyond the first and second dense layers 92, 96 toward the rear end of the sensor element 20 and reaching the upper and lower connector electrodes 71, 72.

[0053] At this time, since the porosity of the high porosity region 77 covered by the first dense layer 92 is 40% or less, water can be prevented from moving inside the high porosity region 77, around the first dense layer 92, and moving toward the rear end side of the sensor element 20 beyond the first dense layer 92. This makes it possible to prevent water from reaching the upper connector electrode 71. Furthermore, when the porosity of the high porosity region 77 is less than 15%, water is further prevented from moving inside the high porosity region 77, and therefore water can be further prevented from reaching the upper connector electrode 71.

[0054] In addition, the first and second dense layers 92, 96 are arranged so that the inner circumferential surface of the insulator 44b and the sensor element 20 (element body 60) overlap in the longitudinal direction, respectively, thereby preventing water from moving around the first and second dense layers 92, 96 from the outside of the sensor element 20 toward the rear end side of the sensor element 20. For example, as a comparative example, consider a case in which the first and second dense layers 92, 96 are arranged so that the inner circumferential surface of the powder compact 45a in FIG. 1 and the sensor element 20 overlap in the longitudinal direction. The powder compact 45a is formed from powder as described above, and has water absorption properties. Therefore, in the comparative example, water may move around the first and second dense layers 92, 96 from the outside of the sensor element 20 toward the rear end side of the first and second dense layers 92, 96 by moving inside the powder compact 45a. 1, in the sensor element 20 of this embodiment, the first and second dense layers 92, 96 are arranged so that the inner circumferential surface of the insulator 44b overlaps with the position of the sensor element 20 in the longitudinal direction, and the insulator 44b is dense. This makes it possible to prevent water from moving around the multiple first and second dense layers 92, 96 from the outside of the sensor element 20 to the rear end side of the sensor element 20. This makes it possible to prevent water from reaching the upper and lower connector electrodes 71, 72.

[0055] Here, the correspondence between the components of this embodiment and the components of the present invention will be clarified. The sensor element 20 of this embodiment corresponds to the sensor element of the present invention, the element body 60 corresponds to the element body, the first surface 60a corresponds to the side surface, the outer electrode 64 corresponds to the outer electrode, the upper connector electrode 71 (71b) corresponds to the connector electrode, the outer lead wire 75 corresponds to the outer lead portion, the porous layer 80 (particularly the first inner porous layer 83) corresponds to the porous layer, the first dense layer 92 corresponds to the dense layer, the low porosity region 76 corresponds to the low porosity region, and the high porosity region 77 corresponds to the high porosity region.

[0056] According to the sensor element 20 of this embodiment described above in detail, the outer lead wire 75 has the low porosity region 76 covered by the first inner porous layer 83, and the high porosity region 77 covered by the first dense layer 92, in contact with the low porosity region 76, and having a higher porosity than the low porosity region 76. This makes it possible to suppress the occurrence of cracks in the sensor element 20.

[0057] Furthermore, by making the porosity of the high porosity region 77 40% or less, water can be prevented from moving inside the high porosity region 77, around the first dense layer 92, and toward the rear end side of the element body 60. This makes it possible to prevent water from reaching the upper connector electrode 71. Furthermore, by making the porosity of the high porosity region 77 less than 15%, water can be further prevented from reaching the upper connector electrode 71. From this viewpoint, the porosity of the high porosity region 77 is more preferably 10% or less, and even more preferably 7% or less.

[0058] Furthermore, since the difference in porosity between the high porosity region 77 and the low porosity region 76 is 1% or more, the effect of suppressing the occurrence of cracks in the sensor element 20 by providing the above-mentioned high porosity region 77 and low porosity region 76 can be more reliably obtained.

[0059] Furthermore, by setting the porosity of the high porosity region 77 to 5% or more, the effect of suppressing the occurrence of cracks in the sensor element 20 by providing the above-mentioned high porosity region 77 and the low porosity region 76 can be more reliably obtained. The reason for this is considered to be that if the porosity is 5% or more, the Young's modulus of the high porosity region 77 becomes sufficiently low.

[0060] Furthermore, by setting the thickness of the first dense layer 92 to 10 μm or less, it is possible to further suppress the occurrence of cracks in the sensor element 20. The reason for this is considered to be that, by setting the thickness of the first dense layer 92 to a relatively thin thickness of 10 μm or less, the Young's modulus of the first dense layer 92 is reduced, and the stress difference between the first dense layer 92 and the first inner porous layer 83 can be further reduced.

[0061] Furthermore, the outer lead wire 75 contains zirconia. When the outer lead wire 75 contains zirconia, the zirconia expands due to TM transformation, and the outer lead wire 75 is deformed, which tends to cause cracks to easily occur in the sensor element 20. Therefore, it is very meaningful to provide the outer lead wire 75 with the low porosity region 76 and the high porosity region 77 in order to suppress the occurrence of cracks in the sensor element 20.

[0062] It goes without saying that the present invention is not limited to the above-described embodiment, and can be embodied in various forms within the technical scope of the present invention.

[0063] For example, in the contact portion between the first dense layer 92 and the first inner porous layer 83 shown in FIG. 5 in the above-mentioned embodiment, there is no portion where the first dense layer 92 and the first inner porous layer 83 overlap in the thickness direction of the first dense layer 92, i.e., in the vertical direction. However, the present invention is not limited to this, and the first dense layer 92 may have an overlap portion where the first dense layer 92 overlaps with the first inner porous layer 83 in the thickness direction of the first dense layer 92 at the contact portion with the first inner porous layer 83. FIG. 6 is a cross-sectional view showing the first dense layer 92 and the periphery of the high porosity region 77 of the modified example. In FIG. 6, the first dense layer 92 and the first inner porous layer 83 partially overlap with each other in the thickness direction of the first dense layer 92, i.e., in the vertical direction. Therefore, the first dense layer 92 has an overlap portion 92a which is a part of the first dense layer 92 on the front end side, and an overlap portion 92b which is a part of the first dense layer 92 on the rear end side. The overlapping portion 92a is a portion of the first dense layer 92 that overlaps with the rear end of the front end portion 83a of the first inner porous layer 83 in the vertical direction, and the upper surface of the overlapping portion 92a is in contact with the front end portion 83a. The upper surface of the overlapping portion 92a is inclined with respect to the front-rear direction, and the overlapping portion 92a has a shape in which the thickness becomes thinner as it approaches its own front end. The overlapping portion 92b is a portion of the first dense layer 92 that overlaps with the front end of the rear end portion 83b of the first inner porous layer 83 in the vertical direction, and the upper surface of the overlapping portion 92b is in contact with the rear end portion 83b. The upper surface of the overlapping portion 92b is inclined with respect to the front-rear direction, and the overlapping portion 92b has a shape in which the thickness becomes thinner as it approaches its own rear end. In FIG. 6, the low porosity region 76 and the high porosity region 77 also partially overlap each other in the thickness direction of the high porosity region 77, i.e., in the vertical direction. Therefore, the high porosity region 77 has an overlap portion 77a which is a part of the front end side of the high porosity region 77, and an overlap portion 77b which is a part of the rear end side. The overlap portion 77a is a part of the high porosity region 77 which overlaps with the rear end portion of the front end portion 76a of the low porosity region 76 in the up-down direction, and the upper surface of the overlap portion 77a is in contact with the front end portion 76a. The upper surface of the overlap portion 77a is inclined with respect to the front-to-rear direction, and the overlap portion 77a has a shape which becomes thinner as it approaches its front end.The overlapping portion 77b is a portion of the high porosity region 77 that overlaps with the front end of the rear end portion 76b of the low porosity region 76 in the up-down direction, and the upper surface of the overlapping portion 77b is in contact with the rear end portion 76b. The upper surface of the overlapping portion 77b is inclined with respect to the front-rear direction, and the overlapping portion 77b has a shape in which the thickness becomes thinner as it approaches its rear end. Such overlapping portions 77a, 77b, 92a, and 92b may be formed, for example, for reasons related to the manufacture of the sensor element 20. For example, in the above-mentioned method of manufacturing the sensor element 20, when the pattern of the high porosity region 77 of the outer lead wire 75 is formed by screen printing and then the pattern of the low porosity region 76 is formed, as shown in FIG. 6, a part of the front and rear of the high porosity region 77 is covered from the outside (upper side) of the sensor element 20 by the low porosity region 76, and the overlapping portions 77a and 77b are formed. Similarly, when the pattern of the first dense layer 92 is formed by screen printing and then the pattern of the first inner porous layer 83 is formed, overlapping portions 92a and 92b are formed as shown in FIG.

[0064] Even if the overlapping portions 77a, 77b, 92a, and 92b are present as shown in Fig. 6, the outer lead wire 75 has the low porosity region 76 covered by the first inner porous layer 83 and the high porosity region 77 covered by the first dense layer 92, in contact with the low porosity region 76, and has a higher porosity than the low porosity region 76, so that the occurrence of cracks in the sensor element 20 can be suppressed as in the above-mentioned embodiment. In this case, it is preferable that the first dense layer 92 covers only the high porosity region 77 out of the low porosity region 76 and the high porosity region 77 from the front end side to the rear end side of the first dense layer 92 including the overlapping portions 92a and 92b. In other words, it is preferable that the low porosity region 76 does not exist directly below the first dense layer 92 from the front end to the rear end of the first dense layer 92 in Fig. 6. In FIG. 6, the front end position of the overlap portion 92a and the rear end position of the overlap portion 77a (= the rear end position of the front end portion 76a of the low porosity region 76) are at the same position in the front-rear direction, so the front end portion 76a of the low porosity region 76 does not exist directly below the overlap portion 92a. In addition, the front end position of the overlap portion 77b (= the front end position of the rear end portion 76b of the low porosity region 76) is located rearward of the rear end position of the overlap portion 92b, so the rear end portion 76b of the low porosity region 76 does not exist directly below the overlap portion 92b. As a result, the low porosity region 76 does not exist directly below the first dense layer 92 from the front end to the rear end of the first dense layer 92. This more reliably achieves the effect of suppressing the occurrence of cracks in the sensor element 20 by the low porosity region 76 and the high porosity region 77. For example, as shown in Fig. 7, a part of a front end portion 76a of the low porosity region 76 may exist directly below an overlapping portion 92a of the first dense layer 92, that is, the overlapping portion 92a and the overlapping portion 77a may partially overlap in the up-down direction. Rather than the configuration shown in Fig. 7, it is preferable that the low porosity region 76 does not exist directly below the first dense layer 92 from the front end to the rear end of the first dense layer 92, as shown in Fig. 6.

[0065] In FIG. 6, the first dense layer 92 and the first inner porous layer 83 are partially overlapped with each other so that the first inner porous layer 83 is located on the upper side, but the first dense layer 92 may be partially overlapped with each other so that the first dense layer 92 is located on the upper side of the first inner porous layer 83. The same applies to the vertical relationship of the overlap between the low porosity region 76 and the high porosity region 77. For example, FIG. 8 is a cross-sectional view in which the vertical relationship of the overlap between the first dense layer 92 and the first inner porous layer 83 in FIG. 6 is reversed, and the vertical relationship of the overlap between the low porosity region 76 and the high porosity region 77 is reversed. Similarly, FIG. 9 is a cross-sectional view in which the vertical relationship of the overlap in FIG. 7 is reversed. In FIG. 8 and FIG. 9, the same components as those in FIG. 6 and FIG. 7 are denoted by the same reference numerals, and detailed description thereof will be omitted. In FIG. 9, the lower surface of the first dense layer 92 does not overlap with the overlapping portion 77a of the high porosity region 77 in the vertical direction, but the overlapping portion 92a of the first dense layer 92 partially overlaps with the overlapping portion 77a of the high porosity region 77 in the vertical direction. That is, in FIG. 9, like FIG. 7, a part of the front end portion 76a of the low porosity region 76 is present directly below the overlapping portion 92a of the first dense layer 92. In contrast, in FIG. 8, the overlapping portion 92a of the first dense layer 92 does not overlap with the overlapping portion 77a of the high porosity region 77 in the vertical direction. That is, in FIG. 8, like FIG. 6, the front end portion 76a of the low porosity region 76 is not present directly below the overlapping portion 92a. Therefore, in FIG. 8, the low porosity region 76 is not present directly below the first dense layer 92 from the front end to the rear end of the first dense layer 92. Therefore, the configuration of FIG. 8 is preferable to the configuration of FIG.

[0066] In the embodiment described above, the high porosity region 77 shown in FIG. 5 does not have a protruding portion protruding from the first dense layer 92 toward the front end side and / or rear end side, but the high porosity region 77 may have a protruding portion. For example, the high porosity region 77 in FIG. 6 and FIG. 8 has an overlap portion 77a protruding from the first dense layer 92 toward the front end side, and the overlap portion 77a corresponds to the protruding portion. The high porosity region 77 in FIG. 6 and FIG. 8 has a region 77c protruding from the first dense layer 92 toward the rear end side. The region 77c includes the overlap portion 77b and a region between the overlap portion 92b and the overlap portion 77b in the front-rear direction. This region 77c also corresponds to the protruding portion. Even if the high porosity region 77 has the protruding portion (overlap portion 77a, region 77c) in this way, the outer lead wire 75 has the low porosity region 76 covered by the first inner porous layer 83 and the high porosity region 77 covered by the first dense layer 92, in contact with the low porosity region 76, and has a higher porosity than the low porosity region 76, so that the occurrence of cracks in the sensor element 20 can be suppressed as in the above-mentioned embodiment. In this case, it is preferable that the length in the front-rear direction of the protruding portion is 0.5 mm or less. In the case of Figs. 6 and 8, it is preferable that the length in the front-rear direction of the overlap portion 77a and the length in the front-rear direction of the region 77c are each 0.5 mm or less. In this way, the effect of suppressing the occurrence of cracks in the sensor element 20 can be more reliably obtained. From the viewpoint of this effect, it is more preferable that the length in the front-rear direction of the protruding portion is 0.3 mm or less.

[0067] In the above-described embodiment, the first inner porous layer 83 of the sensor element 20 covers the first surface 60a except for the region where the upper connector electrode 71 and the first dense layer 92 are present, but this is not limited thereto. For example, the first inner porous layer 83 may cover the region of the first surface 60a from the front end of the first surface 60a to the front end of the upper connector electrode 71 or a predetermined position further forward than that. In addition, a gap region (a region where neither a porous layer nor a dense layer exists) may be provided between the front end portion 83a of the first inner porous layer 83 and the first dense layer 92, or between the rear end portion 83b of the first inner porous layer 83 and the first dense layer 92. Alternatively, the first inner porous layer 83 may not have the rear end portion 83b, and the region between the first dense layer 92 and the upper connector electrode 71 may be the gap region. The outer lead wire 75 may be exposed where the gap region is provided. The low porosity region of the outer lead wire is disposed so as to be covered by the porous layer in contact with the dense layer, and the high porosity region is disposed so as to be in contact with the low porosity region and covered by the dense layer. Therefore, for example, when a gap region is provided between the rear end portion 83b of the first inner porous layer 83 and the first dense layer 92, or when the rear end portion 83b does not exist, the porous layer in contact with the first dense layer 92 is only the front end portion 83a. In this case, it is sufficient that the front end portion 76a of the outer lead wire 75 covered by the front end portion 83a is the low porosity region, and the rear end portion 76b of the outer lead wire 75 does not have to be the low porosity region. For example, the rear end portion 76b may have the same porosity as the high porosity region 77.

[0068] In the above-described embodiment, the first dense layer 92 overlaps with the insulator 44b in the front-rear direction, but this is not limited thereto. The first dense layer 92 may overlap with, for example, the insulator 44a or the insulator 44c in the front-rear direction.

[0069] In the above-described embodiment, the sensor element 20 includes the outer porous layer 85, but this may not be included.

[0070] In the above embodiment, the element body 60 has a rectangular parallelepiped shape, but is not limited thereto. For example, the element body 60 may have a cylindrical or columnar shape. In this case, the element body 60 has only one side surface.

[0071] In the above-described embodiment, the gas sensor 10 includes two powder compacts 45a, 45b and three insulators 44a to 44c, but may include one or more powder compacts and multiple insulators (dense bodies). For example, the insulator 44b may be removed from the gas sensor 10. In this case, since the powder compacts 45a, 45b are adjacent to each other in the front-rear direction, the powder compacts 45a, 45b may be integrated. EXAMPLES

[0072] Specific examples of sensor elements produced will be described below as examples. Experimental Examples 2 to 4, 6 to 7, 9 to 10, and 12 to 13 correspond to examples of the present invention, and Experimental Examples 1, 5, 8, and 11 correspond to comparative examples. Note that the present invention is not limited to the following examples.

[0073] [Experimental Examples 1-13] The sensor elements were fabricated by the same manufacturing method as the gas sensor 10 in Figs. 1 to 6, and were used as Experimental Examples 1 to 13. The element body 60 of each of these sensor elements 20 had dimensions of 52.5 mm in length, 4.25 mm in width, and 1.45 mm in thickness. The first dense layer 92 had a length Le1 of 5 mm, a thickness of 10 µm, and a porosity of 0%. The outer lead wire 75 had a line width of 0.4 mm and a line thickness of 15 µm. Hereinafter, the region of the outer lead wire 75 that corresponds to the high porosity region 77 may be referred to as the first region, and the region of the outer lead wire 75 that corresponds to the low porosity region 76 may be referred to as the second region. In Experimental Examples 1 to 13, the porosity of the first and second regions of the outer lead wire 75 was changed in various ways as shown in Table 1. In Experimental Examples 2 to 4, 6 to 7, 9 to 10, and 12 to 13, the porosity of the first region of outer lead wire 75 was made higher than the porosity of the second region, so that outer lead wire 75 had low porosity region 76 and high porosity region 77. In Experimental Examples 1, 5, 8, and 11, the porosity of the first region of outer lead wire 75 was made equal to or lower than the porosity of the second region.

[0074] [Table 1]

[0075] [Crack test] A test was conducted to evaluate the crack resistance of the sensor elements 20 of Experimental Examples 1 to 13. Specifically, first, 20 sensor elements 20 of Experimental Example 1 were prepared, and these were placed in an autoclave and left for 5 hours under saturated water vapor at a temperature of 180°C. Thereafter, whether or not cracks occurred in each of the 20 sensor elements 20 was visually confirmed using an optical microscope. The ratio of the number of sensor elements 20 in which cracks occurred among the 20 sensor elements 20 was calculated as the crack rate. The crack rates were also calculated in the same manner for the sensor elements 20 of Experimental Examples 2 to 13. The crack rate of Experimental Example 1 was used as a reference value, and when the crack rate in Experimental Examples 1 to 13 was less than the reference value, it was judged as excellent (A), and when it was equal to or greater than the reference value, it was judged as poor (F).

[0076] [Liquid penetration test] A liquid penetration test was carried out on the sensor elements 20 of Experimental Examples 1 to 13 to examine how much liquid penetrates into the rear end side of the element body 60 due to capillary action when the front end side of the element body 60 is immersed in liquid. First, the front end side of the sensor element 20 was downward and the longitudinal direction of the sensor element 20 was aligned vertically, and a portion of the sensor element 20 up to a predetermined position (hereinafter, immersion position) on the rear end side of the front end of the outer lead wire 75 and on the front end side of the first dense layer 92 was immersed in red check liquid. The sensor element was left in this state for 24 hours, and the arrival position indicating how far the red check liquid had reached the rear end side from the immersion position was measured visually. The arrival position was measured as the distance from the front end of the element body 60. When the arrival position after 24 hours was a position forward of the rear end of the first dense layer 92, that is, when the red check liquid did not pass through the first dense layer 92, it was judged as excellent (A). If the reached position was behind the first dense layer 92 but did not pass a predetermined position forward of the front end of the upper connector electrode 71, it was judged as good (B). If the reached position passed the predetermined position, it was judged as bad (F). The red check liquid used was stamp ink (for sol ink pads only) (product number: S-1, color: red) manufactured by Shachihata Co., Ltd. The red check liquid contains 50-60 wt% water, 30-40 wt% glycerin, and 5-15 wt% dye. The ingredients and composition of the red check liquid are listed in the safety data sheet (SDS) manufactured by Shachihata Co., Ltd.

[0077] As can be seen from Table 1, in the crack test, all of Experimental Examples 2 to 4, 6 to 7, 9 to 10, and 12 to 13 in which the porosity of the first region of the outer lead wire 75 was higher than the porosity of the second region, i.e., the outer lead wire 75 had a low porosity region 76 and a high porosity region 77, were evaluated as excellent (A). In contrast, all of Experimental Examples 1, 5, 8, and 11 in which the porosity of the first region of the outer lead wire 75 was lower than the porosity of the second region were evaluated as poor (F). From this, it was confirmed that the occurrence of cracks in the sensor element 20 can be suppressed by the outer lead wire 75 having the low porosity region 76 covered by the first inner porous layer 83 and the high porosity region 77 covered by the first dense layer 92, in contact with the low porosity region 76, and having a porosity higher than that of the low porosity region 76.

[0078] Furthermore, as can be seen from Table 1, when comparing Experimental Examples 2 to 4, 6 to 7, 9 to 10, and 12 to 13, which were evaluated as excellent (A) in the crack test in the liquid penetration test, Experimental Examples 12 and 13, in which the porosity of high porosity region 77 exceeded 40%, were evaluated as poor (F), whereas Experimental Examples 2 to 4, 6 to 7, and 9 to 10, in which the porosity of high porosity region 77 was 40% or less, were evaluated as good (B) or excellent (A). From this, it was confirmed that by having the porosity of high porosity region 77 be 40% or less, it is possible to suppress water from reaching upper connector electrode 71 compared to the case where the porosity exceeds 40%. Furthermore, among experimental examples 2-4, 6-7, and 9-10, experimental examples 6-7 and 9-10 in which the porosity of high porosity region 77 was 15% or more were evaluated as good (B), whereas experimental examples 2-4 in which the porosity of high porosity region 77 was less than 15% were evaluated as excellent (A). From this, it was confirmed that by having the porosity of high porosity region 77 be less than 15%, it is possible to suppress water from reaching upper connector electrode 71, compared to when the porosity is 15% or more and 40% or less. [Industrial Applicability]

[0079] INDUSTRIAL APPLICABILITY The present invention can be used in a gas sensor for detecting the concentration of a specific gas, such as NOx, in a measurement gas, such as an exhaust gas from an automobile. [Explanation of symbols]

[0080] 10 gas sensor, 15 assembly, 20 sensor element, 30 protective cover, 31 inner protective cover, 32 outer protective cover, 33 element chamber, 40 element sealing body, 41 cylindrical body, 42 metal shell, 42a thick portion, 42b bottom surface, 43 inner cylinder, 43a flange portion, 43c, 43d reduced diameter portion, 44a to 44c insulator, 45a, 45b powder compact, 46 metal ring, 47 nut, 48 outer cylinder, 49 space, 50 connector, 51a, 51b housing, 52 contact metal, 53 clamp, 55 lead wire, 57 rubber plug, 58 piping, 59 fixing member, 60 element body, 60a to 60f first surface to sixth surface, 61 measured gas inlet, 62 reference gas inlet, 63 Detection portion, 64 outer electrode, 65 inner main pump electrode, 66 inner auxiliary pump electrode, 67 measurement electrode, 68 reference electrode, 69 heater, 71, 71a to 71d upper connector electrodes, 72 lower connector electrode, 75 outer lead wire, 76 low porosity region, 76a front end portion, 76b rear end portion, 77 high porosity region, 77a, 77b overlap portion, 77c region, 80 porous layer, 81 inner porous layer, 83 first inner porous layer, 83a front end portion, 83b rear end portion, 84 second inner porous layer, 84a front end portion, 84b rear end portion, 85 outer porous layer, 90 dense layer, 92 first dense layer, 92a, 92b overlap portion, 96 second dense layer.

Claims

1. A sensor element for detecting a specific gas concentration in a measurement gas, comprising: an element body having a front end and a rear end which are both ends along a longitudinal direction and a side surface which is a surface along the longitudinal direction, the front end side being exposed to the measurement gas; an outer electrode disposed on the front end side of the side surface; a connector electrode disposed on the rear end side of the side surface for electrical connection to an outside; an outer lead portion disposed on the side surface and electrically connecting the outer electrode and the connector electrode; a porous layer covering a portion of the side surface; a dense layer that covers a portion of the side surface, is disposed on the rear end side of at least a portion of the porous layer, is disposed on the front end side of the connector electrode, and is in contact with the porous layer on the front end side and / or the rear end side; Equipped with the outer lead portion has a low porosity region covered by the porous layer, and a high porosity region covered by the dense layer, in contact with the low porosity region, and having a porosity higher than that of the low porosity region. Sensor element.

2. The high porosity region has a porosity of 40% or less. The sensor element according to claim 1 .

3. The high porosity region has a porosity of less than 15%. The sensor element according to claim 1 or 2.

4. The difference in porosity between the high porosity region and the low porosity region is 1% or more. The sensor element according to claim 1 or 2.

5. The high porosity region has a porosity of 5% or more. The sensor element according to claim 1 or 2.

6. The thickness of the dense layer is 10 μm or less. The sensor element according to claim 1 or 2.

7. the dense layer has an overlap portion that overlaps with the porous layer in a thickness direction of the dense layer at a portion in contact with the porous layer, the dense layer covers only the high porosity region of the high porosity region and the low porosity region from the front end side to the rear end side of the dense layer including the overlap portion; The sensor element according to claim 1 or 2.

8. the high porosity region has a protruding portion protruding beyond the dense layer toward the front end side and / or the rear end side and covered by the porous layer, The length of the protruding portion in the longitudinal direction is 0.5 mm or less. The sensor element according to claim 1 or 2.

9. The outer lead portion includes zirconia. The sensor element according to claim 1 or 2.

10. A gas sensor comprising the sensor element according to claim 1 or 2.

Citation Information

Patent Citations

  • Sensor element and gas sensor

    WO2019155865A1