Noodles
Incorporating cellulose nanofibers and alginic acids into rice flour noodles addresses the texture and workability issues, enhancing the noodles' structural integrity during boiling and cooking.
Patent Information
- Application Number
- JP2024039445
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2023-03-31
- Filing Date
- 2024-03-13
- Publication Date
- 2024-10-15
AI Technical Summary
Noodles made with rice flour have reduced texture and workability due to low gluten content, leading to issues such as disintegration during boiling.
Incorporation of cellulose nanofibers, specifically anion-modified cellulose nanofibers like carboxymethylated cellulose nanofibers, and alginic acids, particularly alginate propylene glycol ester, into rice flour noodles to enhance texture and workability.
Improves the texture and workability of rice flour noodles during production and cooking, ensuring they maintain integrity during boiling and cooking processes.
Smart Images

Figure 2024146802000001 
Figure 2024146802000002 
Figure 2024146802000003
Abstract
Description
[Technical field]
[0001] The present invention relates to noodles containing rice flour, such as udon, rice vermicelli, soba, somen, hiyamugi, Chinese noodles, yakisoba, macaroni, spaghetti, pasta, Korean hiyamen, kuzu-kiri, and harusame. [Background technology]
[0002] In recent years, there has been research into the development of foods that use rice flour instead of wheat flour, which is known to cause allergies. The use of rice flour in noodles such as udon and soba has been under consideration.
[0003] Patent Document 1 describes that the texture of rice flour noodles containing rice flour can be improved by adding pregelatinized starch, starch other than pregelatinized starch, and alginic acid ester. Patent Document 2 describes that the noodle production properties and texture of noodles containing rice flour can be improved by adding tara gum and alginic acid ester. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2013-198420 A [Patent Document 2] JP 2019-129823 A Summary of the Invention [Problem to be solved by the invention]
[0005] However, noodles containing rice flour have problems such as a poor texture and poor workability due to the reduced gluten content of the noodles, which tend to break when boiled. The goal is to improve the texture of noodles containing rice flour and the workability during production and cooking. [Means for solving the problem]
[0006] As a result of extensive research to achieve this objective, the inventors discovered that blending cellulose nanofibers (CNF) and alginic acids is effective in noodles containing rice flour, and thus completed the present invention.
[0007] The present invention provides the following: (1) Noodles containing rice flour, cellulose nanofiber, and alginic acids. (2) The noodles according to (1), wherein the cellulose nanofiber is anionically modified cellulose nanofiber. (3) Noodles according to (1) or (2), wherein the anion-modified cellulose nanofibers are cellulose nanofibers having a carboxyl group or cellulose nanofibers having a carboxyalkyl group. (4) The anion-modified cellulose nanofiber is a carboxymethylated cellulose nanofiber having a carboxymethyl substitution degree in the range of 0.01 to 0.50 (3). The noodles described. (5) Noodles according to (1) or (2), wherein the alginic acid is propylene glycol alginate. (6) The noodles according to (1) or (2), further comprising carboxymethyl cellulose. (7) The noodles according to (1) or (2), which are one type selected from the group consisting of udon, rice vermicelli, soba, somen, hiyamugi, Chinese noodles, yakisoba, macaroni, spaghetti, pasta, Korean hiyashi noodles, kuzukiri, and vermicelli. Effect of the Invention
[0008] According to the present invention, the texture of noodles containing rice flour and the workability during production and cooking can be improved. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] The present invention will be described in detail below. In the present invention, "to" includes the end values. That is, "X to Y" includes the values X and Y at both ends.
[0010] The noodles of the present invention contain rice flour, cellulose nanofibers, and alginic acids, and if necessary, other ingredients.
[0011] The noodles in the present invention are foods that are produced using cereal flour as a main ingredient and are generally called noodles, regardless of their form or type. Specific examples include udon, rice vermicelli, soba, somen, hiyamugi, Chinese noodles, yakisoba, macaroni, spaghetti, pasta, Korean hiyamen, kuzukiri, vermicelli, etc. Examples of forms include chilled noodles, dried noodles, instant noodles, etc.
[0012] In the noodles of the present invention, it is essential that rice flour is contained as the main raw material cereal flour. The rice flour is preferably contained in an amount of 50 to 95% by mass based on the bone dry mass of the total of all cereal flours and starch. Rice flour is usually made by polishing and grinding raw non-glutinous rice into powder. Examples of non-glutinous rice include japonica rice, indica rice, and javanica rice. Examples of rice to be ground include polished rice, brown rice, broken rice, and old rice. There is no particular limitation on the particle size after grinding, and it is usually about the particle size of commonly commercially available joshinko.
[0013] In the noodles of the present invention, it is essential that rice flour is contained as the cereal flour (main ingredient), but cereal flours such as wheat flour may also be contained. Examples of cereal flours other than rice flour include cereal flours such as wheat flour (strong flour, semi-strong flour, medium strength flour, weak flour, durum wheat flour, whole wheat flour, etc.), buckwheat flour, soy flour, etc., and, if necessary, unprocessed starches such as potato starch, sweet potato starch, tapioca starch, corn starch, waxy corn starch, rice starch, mung bean starch, etc., and processed starches produced by etherifying unprocessed starch, esterifying, oxidizing, bleaching, crosslinking, pregelatinizing, etc., alone or in combination. In addition, salt and kansui may be added as additives. In addition to these, thickening stabilizers such as phosphates, alginic acid, caprobean gum, guar gum, tamarind seed gum, pectin, xanthan gum, carrageenan, and curdlan, emulsifiers, oils and fats, egg white, milk protein, coloring agents, antioxidants, wheat protein, and other physiologically active ingredients such as vitamins, calcium, iron, and other seasonings can also be used as desired.
[0014] (Cellulose nanofiber) In the present invention, cellulose nanofibers (hereinafter sometimes referred to as CNF) are fine fibers with a fiber width of about 1 to 500 nm, which are made by pulp, a cellulose-based raw material, being refined to the nanometer level. The average fiber diameter and average fiber length of cellulose nanofibers can be obtained by averaging the fiber diameters and fiber lengths obtained from the results of observing each fiber using an atomic force microscope (AFM) or a transmission electron microscope (TEM). The average aspect ratio of cellulose nanofibers is usually 50 or more. There is no particular upper limit, but it is usually 1000 or less. The average aspect ratio can be calculated by the following formula. Aspect ratio = average fiber length / average fiber diameter
[0015] Cellulose nanofibers are obtained by applying mechanical force to pulp to make it finer, and can be obtained by defibrating unmodified cellulose or modified cellulose such as carboxylated cellulose (also called oxidized cellulose), carboxymethylated cellulose, anionically modified cellulose such as cellulose with a phosphate ester group introduced therein, or cationized cellulose. The average fiber length and average fiber diameter of the fine fibers can be adjusted by oxidation treatment and defibration treatment. In the present invention, it is preferable to use carboxymethylated (CM) cellulose nanofibers obtained by defibrating carboxymethylated cellulose obtained by carboxymethylation treatment.
[0016] (Cellulose raw material) Examples of cellulose raw materials for producing cellulose nanofibers used in the present invention include those originating from plant materials (e.g., wood, bamboo, hemp, jute, kenaf, agricultural waste, cloth, pulp), animal materials (e.g., sea squirts), algae, and microorganisms (e.g., acetic acid bacteria (Acetobacter)). Pulps include softwood unbleached kraft pulp (NUKP), softwood bleached kraft pulp (NBKP), hardwood unbleached kraft pulp (LUKP), hardwood bleached kraft pulp (LBKP), softwood unbleached sulfite pulp (NUSP), softwood bleached sulfite pulp (NBSP), thermomechanical pulp (TMP), recycled pulp, waste paper, and the like. All of these can be used, but cellulose fibers derived from plants or microorganisms are preferred, and cellulose fibers derived from plants are more preferred.
[0017] (Carboxymethylation) In the present invention, when carboxymethylated cellulose nanofibers are used, the carboxymethylated cellulose may be obtained by carboxymethylating the above-mentioned cellulose raw material by a known method, or a commercially available product may be used. In either case, the degree of carboxymethyl substitution per anhydrous glucose unit of cellulose is preferably 0.01 to 0.50. An example of a method for producing such carboxymethylated cellulose can be mentioned as follows. Cellulose is used as a starting material, and 3 to 20 times by mass of water or a lower alcohol is used as a solvent. Specifically, water, methanol, ethanol, N-propyl alcohol, isopropyl alcohol, N-butanol, isobutanol, tertiary butanol, etc. can be used alone or in combination of two or more kinds. When a mixed solvent of water and a lower alcohol is used, the mixing ratio of the lower alcohol is 60 to 95% by mass. As a mercerizing agent, 0.5 to 20 times by mole of an alkali metal hydroxide per anhydrous glucose residue of the starting material, specifically sodium hydroxide or potassium hydroxide, is used. The starting material, solvent, and mercerizing agent are mixed, and a mercerization treatment is carried out at a reaction temperature of 0 to 70° C., preferably 10 to 60° C., for a reaction time of 15 minutes to 8 hours, preferably 30 minutes to 7 hours. Then, a carboxymethylating agent is added at 0.05 to 10.0 times the moles per glucose residue, and an etherification reaction is carried out at a reaction temperature of 30 to 90° C., preferably 40 to 80° C., for a reaction time of 30 minutes to 10 hours, preferably 1 hour to 4 hours.
[0018] <Carboxymethylated cellulose nanofiber> The carboxymethylated cellulose nanofibers of the present invention maintain at least a part of their fibrous shape even when dispersed in water. That is, when an aqueous dispersion of the carboxymethylated cellulose nanofibers is observed under an electron microscope, a fibrous substance can be observed. Furthermore, when the carboxymethylated cellulose nanofibers are measured by X-ray diffraction, a peak of cellulose type I crystals can be observed.
[0019] <Crystallization degree of cellulose type I> The crystallinity of cellulose in the carboxymethylated cellulose nanofiber used in the present invention is preferably 40% or more, more preferably 50% or more, for crystalline type I. When the crystallinity of cellulose type I is as high as 40% or more, the proportion of cellulose that does not dissolve in a solvent such as water and maintains its crystalline structure is high, so that the thixotropy is high and it becomes suitable for viscosity adjustment applications such as thickeners. In addition, for example, but not limited to, when added to a gel-like substance (e.g., food, cosmetics, etc.), it has the advantage of being able to impart excellent shape retention. The crystallinity of cellulose can be controlled by the concentration of the mercerizing agent, the temperature during treatment, and the degree of carboxymethylation. Since a high concentration of alkali is used in mercerization and carboxymethylation, cellulose type I crystals are easily converted to type II, but the desired crystallinity can be maintained by adjusting the degree of denaturation by adjusting the amount of alkali (mercerizing agent) used. There is no particular upper limit to the crystallinity of cellulose type I. In reality, it is thought that the upper limit is about 90%.
[0020] Method for measuring the crystallinity of cellulose type I in carboxymethylated cellulose nanofibers is as follows:
[0021] The sample is placed in a glass cell and measured using an X-ray diffraction measuring device (LabX XRD-6000, manufactured by Shimadzu Corporation). The degree of crystallinity is calculated using the method of Segal et al., and is calculated from the diffraction intensity of the 002 plane at 2θ = 22.6° and the diffraction intensity of the amorphous part at 2θ = 18.5° using the diffraction intensity of the X-ray diffraction pattern at 2θ = 10° to 30° as the baseline, according to the following formula.
[0022] Xc = (I002c - Ia) / I002c x 100 Xc = Crystallinity of cellulose type I (%) I002c: 2θ=22.6°, diffraction intensity of 002 plane Ia: 2θ=18.5°, diffraction intensity of the amorphous part.
[0023] The proportion of type I crystals in carboxymethylated cellulose nanofibers is usually the same as that in the carboxymethyl cellulose before it is made into nanofibers.
[0024] <Degree of carboxymethyl substitution> The carboxymethylated cellulose nanofibers used in the present invention preferably have a carboxymethyl substitution degree per anhydrous glucose unit of cellulose of 0.50 or less. If the carboxymethyl substitution degree exceeds 0.50, it is considered that the cellulose dissolves in water and cannot maintain the fiber shape. In consideration of the operability, the substitution degree is preferably 0.01 to 0.50, more preferably 0.02 to 0.50, even more preferably 0.05 to 0.50, and even more preferably 0.10 to 0.50, 0.15 to 0.50, 0.2 to 0.50, or 0.25 to 0.50. By introducing a carboxymethyl group into cellulose, the cellulose particles electrically repel each other, so that the cellulose can be defibrated into nanofibers. However, if the carboxymethyl substitution degree per anhydrous glucose unit is less than 0.01, the defibration becomes insufficient, and cellulose nanofibers with high transparency may not be obtained. In the conventional aqueous medium method, it was difficult to obtain carboxymethylated cellulose nanofibers having a crystallinity of cellulose I type of 60% or more when the degree of carboxymethyl substitution was in the range of 0.20 to 0.40, but the present inventors have found that it is possible to produce carboxymethylated cellulose nanofibers having a degree of carboxymethyl substitution in the range of 0.20 to 0.50 and a crystallinity of cellulose I type of 60% or more, for example, by the method described below. The degree of carboxymethyl substitution can be adjusted by controlling the amount of the carboxymethylating agent to be reacted, the amount of the mercerizing agent, the composition ratio of water to the organic solvent, etc.
[0025] In the present invention, the anhydroglucose unit means each anhydroglucose (glucose residue) constituting cellulose. The degree of carboxymethyl substitution (also called the degree of etherification) indicates the ratio of hydroxyl groups in the glucose residues constituting cellulose that are substituted with carboxymethyl ether groups (the number of carboxymethyl ether groups per glucose residue). The degree of carboxymethyl substitution may be abbreviated as DS.
[0026] The method for measuring the degree of carboxymethyl substitution is as follows: Weigh out approximately 2.0 g of the sample and place it in a 300 mL Erlenmeyer flask with a stopper. Add 100 mL of a solution of 100 mL of concentrated nitric acid in 1000 mL of methanol, shake for 3 hours, and convert the salt of carboxymethylated cellulose nanofiber (CMC) into H-CMC (hydrogen-type carboxymethylated cellulose nanofiber). Weigh out 1.5 to 2.0 g of the bone-dry H-CMC and place it in a 300 mL Erlenmeyer flask with a stopper. Moisten the H-CMC with 15 mL of 80% methanol, add 100 mL of 0.1 N-NaOH, and shake for 3 hours at room temperature. Using phenolphthalein as an indicator, back-titrate the excess NaOH with 0.1 N-H2SO4, and calculate the degree of carboxymethyl substitution (DS value) using the following formula. A = [(100 × F'-0.1N-H2SO4 (mL) × F) × 0.1] / (bone dry mass of H-CMC (g)) Degree of carboxymethyl substitution = 0.162 x A / (1-0.058 x A) F': Factor of 0.1N-H2SO4 F: Factor of 0.1N NaOH.
[0027] The degree of carboxymethyl substitution in the carboxymethyl cellulose nanofibers is usually the same as the degree of carboxymethyl substitution in the carboxymethyl cellulose before it is made into nanofibers.
[0028] <Fiber diameter, aspect ratio> The carboxymethyl cellulose nanofibers used in the present invention have a nanoscale fiber diameter. The average fiber diameter is preferably 3 nm to 500 nm, more preferably 3 nm to 150 nm, more preferably 3 nm to 20 nm, more preferably 5 nm to 19 nm, and even more preferably 5 nm to 15 nm.
[0029] The aspect ratio of the carboxymethylated cellulose nanofiber is not particularly limited, but is preferably 350 or less, more preferably 300 or less, more preferably 200 or less, more preferably 120 or less, more preferably 100 or less, and even more preferably 80 or less. When the aspect ratio is 350 or less, the fibers are not excessively long, and the fibers are less entangled, which reduces the generation of lumps (lumps) of cellulose nanofibers, making it suitable for use as an additive. In addition, since the fluidity is high, it is easy to use even at high concentrations, and there is an advantage that it is easy to use in applications requiring a high solid content. The lower limit of the aspect ratio is not particularly limited, but is preferably 25 or more, more preferably 30 or more. When the aspect ratio is 25 or more, the fibrous shape has an effect of improving thixotropy. The aspect ratio of the carboxymethylated cellulose nanofiber can be controlled by the mixing ratio of the solvent and water during carboxymethylation, the amount of chemicals added, and the degree of carboxymethylation, and can be produced, for example, by the production method described below.
[0030] The average fiber diameter and average fiber length of carboxymethylated cellulose nanofibers can be measured by analyzing 200 randomly selected fibers using an atomic force microscope (AFM) if the diameter is 20 nm or less, or a field emission scanning electron microscope (FE-SEM) if the diameter is 20 nm or more, and calculating the average. The aspect ratio can be calculated using the following formula: Aspect ratio = average fiber length / average fiber diameter.
[0031] (Defibrilization) The defibration of the cellulose raw material may be carried out before or after the denaturation treatment of the cellulose raw material. Furthermore, the defibration may be carried out once or multiple times. If the defibration is carried out multiple times, each defibration may be carried out at any time.
[0032] The device used for defibration is not particularly limited, but examples include devices of high-speed rotation type, colloid mill type, high pressure type, roll mill type, ultrasonic type, etc., and a high-pressure or ultra-high pressure homogenizer is preferable, and a wet high-pressure or ultra-high pressure homogenizer is more preferable. The device is preferably capable of applying a strong shear force to the cellulose raw material or modified cellulose (usually a dispersion liquid). The pressure that the device can apply is preferably 50 MPa or more, more preferably 100 MPa or more, and even more preferably 140 MPa or more. The device is preferably a wet high-pressure or ultra-high pressure homogenizer that can apply the above pressure to the cellulose raw material or modified cellulose (usually a dispersion liquid) and can apply a strong shear force. This allows efficient defibration.
[0033] When defibrating a dispersion of cellulose raw material, the solid content concentration of the cellulose raw material in the dispersion is usually 0.1% by mass or more, preferably 0.2% by mass or more, and more preferably 0.3% by mass or more. This ensures that the amount of liquid relative to the amount of cellulose fiber raw material is appropriate and efficient. The upper limit is usually 10% by mass or less, and preferably 6% by mass or less. This allows fluidity to be maintained.
[0034] Prior to defibration (preferably with a high-pressure homogenizer) or, if necessary, prior to dispersion treatment, a pretreatment may be carried out as necessary. The pretreatment may be carried out using a mixing, stirring, emulsifying or dispersing device such as a high-speed shear mixer.
[0035] (Dry) The cellulose nanofibers used in the present invention can be used in the state of a dispersion obtained after defibration, but can also be dried and redispersed in water as necessary. The drying method is not particularly limited, and known methods such as freeze drying, spray drying, tray drying, drum drying, belt drying, a method of thinly spreading on a glass plate or the like and drying, fluidized bed drying, microwave drying, and heated fan reduced pressure drying can be used. After drying, the cellulose nanofibers may be pulverized using a cutter mill, hammer mill, pin mill, jet mill, or the like as necessary. The method of redispersing in water is also not particularly limited, and known dispersion devices can be used.
[0036] The cellulose nanofibers used in the present invention may be in the form of a dispersion or powder, but from the viewpoint of excellent workability during the production of confectioneries, it is preferable to use them in the form of a dispersion.
[0037] In the present invention, the blending amount of cellulose nanofibers is preferably 0.01 to 5 mass %, more preferably 0.05 to 3 mass %, and even more preferably 0.1 to 2 mass %, calculated as solid content based on the cereal flour.
[0038] The cellulose nanofiber of the present invention may contain other components as necessary. For example, when producing a powder, it is preferable to add a water-soluble polymer to the cellulose nanofiber dispersion before drying, as this improves redispersibility.
[0039] <Water-soluble polymer> Examples of water-soluble polymers include cellulose derivatives (carboxymethylcellulose, methylcellulose, hydroxypropylcellulose, ethylcellulose), xanthan gum, xyloglucan, dextrin, dextran, carrageenan, locust bean gum, alginic acid, alginates, pullulan, starch, potato starch, kudzu starch, corn starch, gum arabic, locust bean gum, gellan gum, polydextrose, pectin, chitin, water-soluble chitin, chitosan, casein, albumin, soy protein lysate, peptone, tamarind gum, guar gum, etc. Among these, cellulose derivatives are preferred in terms of affinity with carboxymethylated cellulose nanofibers, and carboxymethylcellulose and its salts are particularly preferred. It is believed that water-soluble polymers such as carboxymethylcellulose and its salts penetrate between carboxymethylated cellulose nanofibers and increase the distance between the nanofibers, thereby improving redispersibility.
[0040] When carboxymethylcellulose or a salt thereof is used as the water-soluble polymer, it is preferable to use carboxymethylcellulose with a degree of carboxymethyl group substitution per anhydrous glucose unit of 0.55 to 1.6, more preferably 0.55 to 1.1, and even more preferably 0.65 to 1.1. In addition, a molecule with a long length (high viscosity) is preferable because it has a high effect of widening the distance between nanofibers. In addition, the B-type viscosity of a 1% by mass aqueous solution of carboxymethylcellulose at 25°C and 60 rpm is preferably 3 mPa·s to 14000 mPa·s, more preferably 7 mPa·s to 14000 mPa·s, and even more preferably 1000 mPa·s to 8000 mPa·s. Note that the "carboxymethylcellulose or a salt thereof" as the water-soluble polymer referred to here is completely dissolved in water, and is therefore distinguished from the carboxymethylated cellulose nanofibers whose fiber shape can be confirmed in water.
[0041] The blending amount of the water-soluble polymer is preferably 5% by mass to 300% by mass, more preferably 20% by mass to 300% by mass, even more preferably 25% by mass to 200% by mass, and even more preferably 25% by mass to 60% by mass, relative to the cellulose nanofiber (bone dry solid content). (Alginate ester) The alginic acids used in the present invention include propylene glycol alginate, alginic acid, sodium alginate, potassium alginate, ammonium alginate, calcium alginate, etc., and it is preferable to use propylene glycol alginate. The amount of alginic acids to be blended is preferably 0.05 to 5% by mass, more preferably 0.1 to 3% by mass, and even more preferably 0.2 to 2% by mass, calculated as solid content, relative to the cereal flour.
[0042] The noodles of the present invention can be produced by conventionally known production methods. For example, this can be done as follows. First, a noodle dough containing the ingredients contained in the noodles of the present invention is prepared. Raw noodle strands of the desired shape are produced from this noodle dough by conventionally known methods. The resulting raw noodle strands are subjected to both a step of boiling in hot water or a steaming step and a step of drying using hot air or deep-frying, thereby achieving final starch gelatinization. Starch gelatinization in the steaming step is minimized, that is, the starch granules are brought to a state where they are swollen to the limit without being disintegrated by the heat of the steaming step. The noodles are then dried. The drying step can be, for example, high-temperature drying, such as hot air drying or deep-frying drying. EXAMPLES
[0043] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these examples.
[0044] (Method for measuring degree of carboxymethyl substitution) 1) Accurately weigh out approximately 2.0 g of carboxymethylated cellulose fiber (bone dry) and place it in a 300 mL Erlenmeyer flask with a stopper. 2) Add 100 mL of a solution of 100 mL of special-grade concentrated nitric acid to 1000 mL of nitric acid methanol, shake for 3 hours, and convert the carboxymethyl cellulose salt (carboxymethyl cellulose) into hydrogen-type carboxymethyl cellulose. 3) Accurately weigh out 1.5 to 2.0 g of hydrogenated carboxylated cellulose (bone dry) and place it in a 300 mL Erlenmeyer flask with a stopper. 4) Wet the hydrogenated carboxylated cellulose with 15 mL of 80% methanol, add 100 mL of 0.1 N NaOH, and shake at room temperature for 3 hours. 5) Back-titrate excess NaOH with 0.1N H2SO4 using phenolphthalein as an indicator. 6) The degree of carboxymethyl substitution (DS) is calculated by the following formula: A = [(100 × F'-(0.1N H2SO4) (mL) × F) × 0.1] / (bone-dry mass of hydrogenated carboxylated cellulose (g)) DS = 0.162 x A / (1-0.058 x A) A: The amount of 1N NaOH required to neutralize 1 g of hydrogenated carboxymethyl cellulose (mL) F': Factor of 0.1N H2SO4 F: Factor of 0.1N NaOH
[0045] (Method of measuring average fiber diameter and aspect ratio) The average fiber diameter and average fiber length of CNF were analyzed for 200 randomly selected fibers using an atomic force microscope (AFM). The aspect ratio was calculated using the following formula: Aspect ratio = average fiber length / average fiber diameter
[0046] [Production Example 1] (Preparation of carboxymethylated cellulose nanofibers A) In a 5L twin-shaft kneader with the rotation speed adjusted to 100 rpm, 1089 parts of isopropanol (IPA) and 31 parts of sodium hydroxide dissolved in 121 parts of water were added, and 200 parts of hardwood pulp (LBKP, manufactured by Nippon Paper Industries Co., Ltd.) were added in terms of dry mass when dried at 100 ° C for 60 minutes. The mixture was stirred and mixed at 30 ° C for 60 minutes to prepare mercerized cellulose. 117 parts of sodium monochloroacetate were further added while stirring, and after stirring at 30 ° C for 30 minutes, the mixture was heated to 70 ° C over 30 minutes and carboxymethylation reaction was carried out at 70 ° C for 60 minutes. The proportion of water in the reaction medium during the mercerization reaction and the carboxymethylation reaction was 10 mass%. After the reaction was completed, the mixture was neutralized, washed with 65% water-containing methanol, deliquored, dried, and pulverized to obtain a sodium salt of carboxymethylated cellulose with a carboxymethyl substitution degree of 0.27 and a crystallinity of cellulose I type of 64%. The methods for measuring the degree of carboxymethyl substitution and the crystallinity of cellulose type I are as described above. The obtained sodium salt of carboxymethyl cellulose was dispersed in water to obtain a 1% (w / v) aqueous dispersion. This was treated three times with a high-pressure homogenizer at 150 MPa to obtain a dispersion of carboxymethyl cellulose nanofibers. The obtained carboxymethyl cellulose nanofibers had an average fiber diameter of 3.2 nm and an aspect ratio of 40. The obtained carboxymethylated cellulose nanofibers were dispersed in water to a solid content of 0.7% by mass, and carboxymethyl cellulose (manufactured by Nippon Paper Industries Co., Ltd., product name: F350HC-4, viscosity (1% by mass, 25°C, 60 rpm) approximately 3000 mPa·s, degree of carboxymethyl substitution approximately 0.90) was added at 40% by mass relative to the carboxymethyl cellulose nanofibers (i.e., so that the solid content of carboxymethyl cellulose was 40 parts by mass when the solid content of the carboxymethylated cellulose nanofibers was 100 parts by mass), and the mixture was stirred for 60 minutes with a TK homomixer (12,000 rpm). To this dispersion, 0.5% by mass of sodium hydroxide solution was added to adjust the pH to 9, and then the mixture was applied to the drum surface of a drum dryer D0405 (manufactured by Katsuragi Kogyo Co., Ltd.) and dried at 140°C for 1 minute. The resulting dried product was scraped off and then pulverized using an impact mill at a rate of 10 kg per hour to obtain a dried pulverized product with a moisture content of 5% by mass. The pulverized product was classified using a 30 mesh to obtain a powder containing carboxymethylated cellulose nanofibers and carboxymethyl cellulose (CNF powder A).
[0047] [Example 1] (Udon manufacturing) 90 parts of rice flour, 10 parts of processed starch (manufactured by Nihon Shokuhin Kako Co., Ltd.), 0.5 parts of alginic acid ester (trade name: Kombu Acid 501, manufactured by Kimika Co., Ltd.), 0.5 parts of salt, 1 part of the CNF powder A obtained above, and 60 parts of water were placed in a stainless steel beaker and mixed at 5000 rpm for 5 minutes using a TK homogenizer to prepare udon dough. The udon dough was put into an extrusion noodle machine to produce udon. The udon was transferred to a tray, wrapped in plastic wrap, and stored in a freezer. After thawing the frozen udon, we added 2.5L of water and boiled it for 13 minutes. We evaluated how easily the boiled udon came apart when dipped in soup, and also tasted it.
[0048] [Comparative Example 1] Udon noodles were produced in the same manner as in Example 1, except that CNF powder A was not added, and workability and taste evaluations were performed.
[0049] [Comparative Example 2] Udon noodles were produced in the same manner as in Example 1, except that the amount of alginate ester (manufactured by Kimika) added was 1.5 parts and CNF powder A was not added, and workability evaluation and taste evaluation were performed.
[0050] [Comparative Example 3] Udon noodles were produced in the same manner as in Example 1, except that no alginic acid ester was added, and workability evaluation and taste evaluation were carried out. Workability rating: The workability of the udon noodle making process (ease of the noodles breaking apart, sticking together) was evaluated on a 10-point scale from excellent: 10 to poor: 1. Conditions for boiling: We evaluated how easily udon noodles break apart when boiled. Tasting rating: The texture (ease of swallowing, ease of disintegration) was evaluated on a 10-point scale from excellent: 10 to poor: 1.
[0051] Table 1 shows the evaluation of workability during the production of udon noodles in Example 1 and Comparative Examples 1 to 3, and Table 2 shows the evaluation of taste.
[0052] [Table 1]
[0053] As shown in Table 1, the udon of Example 1 had better workability in the noodle-making process than the udon of Comparative Examples 1 to 3.
[0054] [Table 2]
[0055] As shown in Table 2, the udon of Example 1 had a better texture than the udon of Comparative Examples 1 to 3.
[0056] [Production Example 2] (Preparation of carboxymethylated cellulose nanofibers B) In a twin-shaft kneader adjusted to a rotation speed of 100 rpm, 130 parts of water and 20 parts of sodium hydroxide dissolved in 100 parts of water were added, and 100 parts of hardwood pulp (manufactured by Nippon Paper Industries Co., Ltd., LBKP) was added in terms of dry mass when dried at 100 ° C for 60 minutes. The mixture was stirred and mixed at 30 ° C for 90 minutes to prepare mercerized cellulose. Further, 230 parts of IPA and 60 parts of sodium monochloroacetate were added while stirring, and after stirring for 30 minutes, the mixture was heated to 70 ° C and subjected to CM reaction for 90 minutes. The concentration of IPA in the reaction medium during the CM reaction was 50%. After the reaction was completed, the mixture was neutralized, deliquored, dried, and pulverized to obtain a sodium salt of CM-modified cellulose with a CM substitution degree of 0.31 and a crystallinity of cellulose I type of 67%. The obtained sodium salt of carboxymethyl cellulose was dispersed in water to obtain a 1% (w / v) aqueous dispersion. This was treated once with a high-pressure homogenizer at 150 MPa to obtain an aqueous dispersion of carboxymethyl cellulose (CNF). The obtained carboxymethyl cellulose (CNF) had an average fiber diameter of 10 nm and an aspect ratio of 50.
[0057] The obtained carboxymethylated cellulose nanofibers were dispersed in water to a solid content of 0.7% by mass, and carboxymethyl cellulose (manufactured by Nippon Paper Industries Co., Ltd., product name: F350HC-4, viscosity (1% by mass, 25°C, 60 rpm) approximately 3000 mPa·s, degree of carboxymethyl substitution approximately 0.90) was added at 40% by mass relative to the carboxymethyl cellulose nanofibers (i.e., so that the solid content of carboxymethyl cellulose was 40 parts by mass when the solid content of the carboxymethylated cellulose nanofibers was 100 parts by mass), and the mixture was stirred for 60 minutes with a TK homomixer (12,000 rpm).
[0058] To this dispersion, 0.5% by mass of sodium hydroxide aqueous solution was added to adjust the pH to 9, and then the mixture was applied to the drum surface of a drum dryer D0405 (manufactured by Katsuragi Kogyo Co., Ltd.) and dried at 140°C for 1 minute. The resulting dried product was scraped off and then pulverized using an impact mill at a rate of 10 kg per hour to obtain a dried pulverized product with a moisture content of 5% by mass. The pulverized product was classified using a 30 mesh to obtain a powder containing carboxymethylated cellulose nanofibers and carboxymethyl cellulose (CNF powder B).
[0059] [Production Example 3] (Preparation of carboxymethylated cellulose nanofibers C) In a twin-shaft kneader adjusted to a rotation speed of 100 rpm, 130 parts of water and 20 parts of sodium hydroxide dissolved in 100 parts of water were added, and 100 parts of hardwood pulp (manufactured by Nippon Paper Industries Co., Ltd., LBKP) was added in terms of dry mass when dried at 100 ° C for 60 minutes. The mixture was stirred and mixed at 30 ° C for 90 minutes to prepare mercerized cellulose. Further, 230 parts of IPA and 60 parts of sodium monochloroacetate were added while stirring, and after stirring for 30 minutes, the mixture was heated to 70 ° C and subjected to CM reaction for 90 minutes. The concentration of IPA in the reaction medium during the CM reaction was 50%. After the reaction was completed, the mixture was neutralized, deliquored, dried, and pulverized to obtain a sodium salt of CM-modified cellulose with a CM substitution degree of 0.31 and a crystallinity of cellulose I type of 67%. The obtained sodium salt of carboxymethyl cellulose was dispersed in water to obtain a 1% (w / v) aqueous dispersion. This was treated once with a high-pressure homogenizer at 150 MPa to obtain an aqueous dispersion of carboxymethyl cellulose (CNF). The obtained carboxymethyl cellulose (CNF) had an average fiber diameter of 10 nm and an aspect ratio of 50.
[0060] The obtained carboxymethylated cellulose nanofibers were dispersed in water to a solid content of 0.7% by mass, and carboxymethyl cellulose (manufactured by Nippon Paper Industries Co., Ltd., product name: F800HC, viscosity (1% by mass, 25°C, 60 rpm) approximately 7000 mPa·s, degree of carboxymethyl substitution approximately 0.85) was added at 30% by mass relative to the carboxymethyl cellulose nanofibers (i.e., so that the solid content of carboxymethyl cellulose was 30 parts by mass when the solid content of the carboxymethylated cellulose nanofibers was 100 parts by mass), and the mixture was stirred for 60 minutes with a TK homomixer (12,000 rpm).
[0061] To this dispersion, 0.5% by mass of sodium hydroxide solution was added to adjust the pH to 9, and then the mixture was applied to the drum surface of a drum dryer D0405 (manufactured by Katsuragi Kogyo Co., Ltd.) and dried at 140°C for 1 minute. The resulting dried product was scraped off and then pulverized using an impact mill at a rate of 10 kg per hour to obtain a dried pulverized product with a moisture content of 5% by mass. The pulverized product was classified using a 30 mesh to obtain a powder containing carboxymethylated cellulose nanofibers and carboxymethyl cellulose (CNF powder C).
[0062] [Example 2] (Pasta noodle manufacturing) (Preparation process) 100 parts by weight of rice flour, 0.5 parts by weight of alginic acid ester (product name: Kombu Acid 501, manufactured by Kimika Co., Ltd.), and 1 part by weight of the CNF powder A obtained above were placed in a small pasta machine (Squeezer II SQZ, manufactured by Fuji Seiki Co., Ltd.), mixing was started, and then 45 parts by weight of boiling water was gradually added. After that, normal mixing (2 minutes) and vacuum mixing (6 minutes) were performed in that order to knead the mixture, and when the noodle dough was sufficiently kneaded, it was extruded to produce noodles. The noodles were cut to a certain length, and then hung to dry and cool, taking care not to let the noodles stick together using chopsticks or other tools, to obtain pasta noodle A.
[0063] (Boiling process) The obtained pasta noodles were put into a bag and frozen for about one day. After frozen storage, the pasta noodles were boiled in boiling water for 3 minutes, and after boiling, they were thoroughly washed with water to obtain boiled pasta noodles.
[0064] [Example 3] Pasta noodles B was obtained in the same manner as in Example 2, except that the CNF powder A used in the preparation process was changed to CNF powder B, and the boiling process was carried out.
[0065] [Example 4] Pasta noodle C was obtained in the same manner as in Example 2, except that the CNF powder A used in the preparation process was changed to CNF powder C, and the boiling process was carried out.
[0066] [Comparative Example 4] Pasta noodles D was obtained and the boiling step was carried out in the same manner as in Example 2, except that CNF powder A was not added in the preparation step.
[0067] (Workability evaluation) The workability in each process was evaluated as shown in Table 3.
[0068] [Table 3]
[0069] (Tasting evaluation) The boiled pasta noodles were evaluated for texture (ease of swallowing, ease of coming apart, etc.) on a 10-point scale (excellent: 10 to poor: 1). The results are shown in Table 4.
[0070] [Table 4]
Claims
1. Noodles containing rice flour, cellulose nanofiber, and alginic acids.
2. The noodles according to claim 1 , wherein the cellulose nanofibers are anionically modified cellulose nanofibers.
3. 3. The noodles according to claim 1 or 2, wherein the anionically modified cellulose nanofiber is a cellulose nanofiber having a carboxyl group or a cellulose nanofiber having a carboxyalkyl group.
4. The noodles according to claim 3, wherein the anionically modified cellulose nanofiber is a carboxymethylated cellulose nanofiber having a degree of carboxymethyl substitution in the range of 0.01 to 0.
50.
5. 2. The noodles according to claim 1, wherein the alginic acid is propylene glycol alginate.
6. The noodles according to claim 1 or 2, further comprising carboxymethyl cellulose.
7. 3. The noodles according to claim 1 or 2, which is one type selected from the group consisting of udon, rice vermicelli, soba, somen, hiyamugi, Chinese noodles, yakisoba, macaroni, spaghetti, pasta, Korean hiyashi noodles, kuzukiri, and vermicelli.
Citation Information
Patent Citations
Rice flour noodle
JP2013198420A
Noodles and method for producing the same
JP2019129823A
Cited By
Dry noodle
JP2023050685A
Dried noodles
JP7725982B2