Three-dimensional lamination shaping device and method for controlling three-dimensional lamination shaping device
The apparatus improves determination accuracy in three-dimensional additive manufacturing by using multiple detection units and arithmetic expressions to process backscattered electron signals, addressing limitations in conventional methods.
Patent Information
- Application Number
- JP2023063588
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-04-10
- Publication Date
- 2024-10-23
- Estimated Expiration
- 2043-04-10
AI Technical Summary
Conventional three-dimensional additive manufacturing apparatuses face limitations in determination accuracy due to the use of a single calculation formula for backscattered electron signals, leading to reduced recognition and processing capabilities.
The apparatus incorporates multiple detection units to capture backscattered electron signals, employing a control section with various arithmetic expressions for processing these signals, allowing for improved determination accuracy through selective arithmetic processing based on the modeling process.
Enhances determination accuracy during the manufacturing process by utilizing multiple backscattered electron signals, expanding their applicability and improving judgment precision.
Smart Images

Figure 2024150258000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a three-dimensional additive manufacturing apparatus and a method for controlling a three-dimensional additive manufacturing apparatus. [Background technology]
[0002] In recent years, 3D additive manufacturing technology, which creates objects by stacking thin layers of powder material one by one, has been attracting attention, and many types of 3D additive manufacturing technologies have been developed based on differences in powder materials and manufacturing methods.
[0003] In a conventional 3D additive manufacturing device, for example, a powder material is spread layer by layer on a base plate installed on the upper surface of a stage. Next, only the two-dimensional structure part corresponding to one cross section of the model is melted from the powder material spread on the base plate by a heating mechanism consisting of an electron beam or laser. Then, the layers of such powder material are stacked one by one in the height direction (Z direction) to form a model (see, for example, Patent Document 1).
[0004] Patent document 1 also describes a technology in which a detection unit is provided to detect reflected electrons generated when an electron beam is irradiated onto a powder material, and the state of the object is determined based on the information detected by this detection unit. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Patent Publication No. 2021-42410 Summary of the Invention [Problem to be solved by the invention]
[0006] In addition, there are multiple judgment factors in the modeling process, such as unevenness and contours of the modeled object. However, in the technology described in Patent Document 1, a single arithmetic formula is used to process the reflected electron signal detected by the detection unit, and only one type of reflected electron image is obtained. Therefore, in the technology described in Patent Document 1, the judgment process using the reflected electron signal is limited. Furthermore, there is a problem in that the judgment process is performed using an image that is difficult to recognize, resulting in a decrease in judgment accuracy.
[0007] In consideration of the above problems, an object of the present invention is to provide a three-dimensional additive manufacturing device and a control method for a three-dimensional additive manufacturing device that can improve the judgment accuracy during the modeling process using reflected electron signals and expand the applications of the reflected electron signals. [Means for solving the problem]
[0008] In order to solve the above problems and achieve the object of the present invention, the three-dimensional additive manufacturing apparatus of the present invention includes a modeling plate, a powder supplying device that supplies a powder material to the modeling plate to form a powder layer, and a beam irradiation device that irradiates the powder layer with an electron beam. The three-dimensional additive manufacturing apparatus also includes a plurality of detection units that detect reflected electrons generated when the powder material is irradiated with the electron beam, and a control unit that acquires a plurality of reflected electron signals detected by the plurality of detection units, performs arithmetic processing on the plurality of reflected electron signals, and calculates an arithmetic signal. The control unit has a plurality of arithmetic expressions. The control unit selects a predetermined arithmetic expression from the plurality of arithmetic expressions in accordance with the modeling process, and performs arithmetic processing on the plurality of reflected electron signals by using the selected arithmetic expression to calculate an arithmetic signal.
[0009] A control method for a three-dimensional additive manufacturing apparatus according to the present invention is a control method for use in a three-dimensional additive manufacturing apparatus having the above-mentioned configuration, in which the control unit selects a predetermined arithmetic formula from a plurality of arithmetic formulas according to the modeling process, and performs arithmetic processing on the plurality of reflected electron signals using the selected arithmetic formula to calculate an arithmetic signal. Effect of the Invention
[0010] According to the three-dimensional additive manufacturing apparatus and the control method for the three-dimensional additive manufacturing apparatus of the present invention, it is possible to improve the accuracy of determination during the modeling process using the reflected electron signal and to expand the applications of the reflected electron signal. [Brief description of the drawings]
[0011] [Figure 1] 1 is a schematic cross-sectional view showing a three-dimensional additive manufacturing apparatus according to an embodiment of the present invention. [Diagram 2] FIG. 2 is a block diagram showing an example of the configuration of a control system of a three-dimensional additive manufacturing apparatus according to an embodiment of the present invention. [Diagram 3] FIG. 2 is a plan view showing the position of a detection unit in the three-dimensional additive manufacturing apparatus according to the first embodiment of the present invention. [Figure 4] 1 shows an example of a reflected electron image acquired after powder heating. [Diagram 5] A backscattered electron image taken after a powder heat shows an example of improperly packed powder material. [Figure 6] 1 is a backscattered electron image taken after full melting, showing an example of melted powder material. [Figure 7] FIG. 11 is a plan view showing the position of a detection unit in a three-dimensional additive manufacturing apparatus according to a second embodiment of the present invention. [Figure 8] FIG. 13 is a plan view showing the position of a detection unit in a three-dimensional additive manufacturing apparatus according to a third embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0012] Hereinafter, an embodiment of a three-dimensional additive manufacturing apparatus and a control method for a three-dimensional additive manufacturing apparatus of the present invention will be described with reference to Fig. 1 to Fig. 8. In addition, the same reference numerals are used to designate common members in each drawing.
[0013] 1. First embodiment 1-1. Configuration of 3D additive manufacturing equipment First, a three-dimensional additive manufacturing apparatus according to a first embodiment of the present invention (hereinafter, referred to as "this example") will be described with reference to FIG. Fig. 1 is a schematic cross-sectional view showing a three-dimensional additive manufacturing apparatus of this embodiment. In the following description, in order to clarify the shapes and positional relationships of the various parts of the three-dimensional additive manufacturing apparatus, the left-right direction in Fig. 1 is defined as the X direction, the depth direction in Fig. 1 is defined as the Y direction, and the up-down direction in Fig. 1 is defined as the Z direction. The X direction, Y direction, and Z direction are mutually orthogonal. Moreover, the X direction and Y direction are parallel to the horizontal direction, and the Z direction is parallel to the vertical direction.
[0014] The 3D additive manufacturing device 1 shown in FIG. 1 is a device that irradiates a powder material made of a metal powder such as titanium, aluminum, or iron with an electron beam to melt the powder material, and then stacks layers of the solidified powder material to form a three-dimensional object.
[0015] 1, the 3D additive manufacturing apparatus 1 includes a vacuum chamber 3, a beam irradiation device 2, a powder supplying device 16, a modeling table 18, a modeling box 20, and a collection box 21. The 3D additive manufacturing apparatus 1 also includes a modeling plate 22, an inner base 24, a plate moving device 26, a radiation shield cover 28, a mask cover 30, a camera 42, and a shutter 44. The 3D additive manufacturing apparatus 1 also includes a plurality of detection units 46 that detect reflected electrons.
[0016] The vacuum chamber 3 is a chamber for creating a vacuum state by evacuating the air inside the chamber with a vacuum pump (not shown).
[0017] The beam irradiation device 2 is a device that irradiates the electron beam 15 onto the shaping plate 22 or the shaping surface 32a of the powder layer formed by the powder material 32. The shaping surface 32a corresponds to the upper surface of the powder layer. The state of the powder layer changes as the 3D additive manufacturing process progresses. Although not shown, the beam irradiation device 2 has an electron gun that is a source of the electron beam 15, a focusing lens that focuses the electron beam generated by the electron gun, and a deflection lens that deflects the electron beam 15 focused by the focusing lens. The focusing lens is configured using a focusing coil and focuses the electron beam 15 by the magnetic field generated by the focusing coil. The deflection lens is configured using a deflection coil and deflects the electron beam 15 by the magnetic field generated by the deflection coil.
[0018] The powder supplying device 16 is a device that supplies a powder material 32, which is an example of a powder material that is a raw material of the molded object 38, onto the molding plate 22 to form a powder layer. The powder supplying device 16 has a hopper 16a, a powder dropper 16b, and a squeegee 16c. The hopper 16a is a container for storing metal powder. The powder dropper 16b is a device that drops the powder material 32 stored in the hopper 16a onto the molding table 18. The squeegee 16c is a long, elongated member that is long in the Y direction and has a blade 16d for spreading powder. The squeegee 16c spreads the powder material 32 dropped by the powder dropper 16b onto the molding table 18. The squeegee 16c is provided so as to be movable in the X direction in order to spread the powder material 32 over the entire surface of the molding table 18.
[0019] The modeling table 18 is arranged horizontally inside the vacuum chamber 3. The modeling table 18 is arranged below the powder supplying device 16. The center of the modeling table 18 is open. The shape of the opening of the modeling table 18 is circular or angular (for example, rectangular) when viewed from above.
[0020] The modeling box 20 is a box that forms a space for modeling. An upper end of the modeling box 20 is connected to an edge of the opening of the modeling table 18. A lower end of the modeling box 20 is connected to the bottom wall of the vacuum chamber 3.
[0021] The recovery box 21 is a box for recovering the powder material 32 that has been supplied onto the modeling table 18 by the powder supplying device 16 in an amount greater than necessary.
[0022] The shaping plate 22 is a plate for forming a shaped object 38 using the powder material 32. The shaped object 38 is formed by stacking on the shaping plate 22. The shaping plate 22 is formed to be circular or angular in plan view to match the opening shape of the shaping table 18. The shaping plate 22 is connected (grounded) to the inner base 24 by an earth wire 34 so as not to be in an electrically floating state. The inner base 24 is held at GND (ground) potential. The powder material 32 is spread over the shaping plate 22 and the inner base 24.
[0023] The inner base 24 is provided so as to be movable in the vertical direction (Z direction). The shaping plate 22 moves vertically together with the inner base 24. The inner base 24 has outer dimensions larger than those of the shaping plate 22. The inner base 24 slides vertically along the inner side surface of the shaping box 20. A sealing member 36 is attached to the outer periphery of the inner base 24. The sealing member 36 is a member that maintains slidability and airtightness between the outer periphery of the inner base 24 and the inner side surface of the shaping box 20. The sealing member 36 is made of a material that is heat-resistant and elastic.
[0024] The plate moving device 26 is a device that moves the shaping plate 22 and the inner base 24 in the up-down direction. The plate moving device 26 includes a shaft 26a and a drive mechanism unit 26b. The shaft 26a is connected to the lower surface of the inner base 24. The drive mechanism unit 26b includes a motor and a power transmission mechanism (not shown), and moves the shaping plate 22 and the inner base 24 together with the shaft 26a in the up-down direction by driving the power transmission mechanism using the motor as a drive source. The power transmission mechanism is, for example, configured by a rack-and-pinion mechanism, a ball screw mechanism, or the like.
[0025] The radiation shield cover 28 is disposed between the shaping plate 22 and the beam irradiation device 2 in the Z direction. The radiation shield cover 28 is made of a metal such as stainless steel. The radiation shield cover 28 shields radiant heat generated when the powder material 32 is irradiated with the electron beam 15 by the beam irradiation device 2. When the powder material 32 is irradiated with the electron beam 15 in order to perform the main sintering of the powder material 32, the powder material 32 melts. At this time, if the heat radiated from the shaping surface 32a of the powder layer, i.e., the radiant heat, is widely diffused within the vacuum chamber 3, the thermal efficiency is deteriorated. In contrast, when the radiation shield cover 28 is disposed above the shaping plate 22, the heat radiated from the shaping surface 32a is shielded by the radiation shield cover 28, and the shielded heat is reflected by the radiation shield cover 28 and returned to the shaping plate 22 side. Therefore, the heat generated by the irradiation of the electron beam 15 can be efficiently utilized.
[0026] In addition, the radiation shield cover 28 functions to prevent evaporated material generated when the powder material 32 is irradiated with the electron beam 15 from adhering (evaporating) onto the inner wall of the vacuum chamber 3. When the powder material 32 is irradiated with the electron beam 15, part of the molten metal becomes a mist of evaporated material and rises from the printing surface 32a. The radiation shield cover 28 is disposed to cover the space above the printing surface 32a to prevent the evaporated material from diffusing inside the vacuum chamber 3.
[0027] The mask cover 30 has an opening 30a and a mask portion 30b. When forming the shaped object 38, the mask cover 30 is placed over the upper surface of the powder material 32, i.e., the shaping surface 32a. At this time, the opening 30a exposes the powder material 32 spread on the shaping plate 22, and the mask portion 30b shields the powder material 32 located outside the opening 30a. The shape of the opening 30a is set according to the shape of the shaping plate 22. For example, if the shaping plate 22 is circular in plan view, the shape of the opening 30a in plan view is set to be circular accordingly, and if the shaping plate 22 is angular in plan view, the shape of the opening 30a in plan view is set to be angular accordingly.
[0028] The mask cover 30 is disposed below the radiation shield cover 28. The opening 30a and the mask portion 30b of the mask cover 30 are disposed between the modeling plate 22 and the radiation shield cover 28 in the Z direction. The mask cover 30 has an enclosure portion 30c. The enclosure portion 30c is disposed so as to surround the space above the opening 30a. A part (upper portion) of the enclosure portion 30c overlaps with the radiation shield cover 28 in the Z direction. The enclosure portion 30c serves to shield radiant heat generated from the modeling surface 32a and to suppress the diffusion of evaporated substances generated from the modeling surface 32a. In other words, the enclosure portion 30c serves the same function as the radiation shield cover 28.
[0029] The mask cover 30 is made of a metal having a higher melting point than the powder material 32 used as the raw material of the molded object 38. The mask cover 30 is made of a material having low reactivity with the powder material 32. Titanium can be given as an example of a material for the mask cover 30. The mask cover 30 may be made of the same metal material as the powder material 32 used. The mask cover 30 is electrically grounded to GND. The mask cover 30 serves as an electrical shield when the powder material 32 is pre-sintered by irradiation with the electron beam 15 in a pre-heating step before the main sintering step described later, thereby minimizing the occurrence of powder scattering.
[0030] The camera 42 is a camera capable of photographing the modeling surface 32a of the powder layer. The camera 42 is disposed at a position shifted in the Y direction from the beam irradiation device 2 so as not to interfere with the position of the camera 42 and the beam irradiation device 2. The camera 42 is preferably configured by a visible light camera such as a digital video camera. The camera 42 photographs the modeling surface 32a of the powder layer to generate an image (image data) of the powder layer. Therefore, the image generated by the camera 42 is an image showing the state of the modeling surface 32a of the powder layer. The photographing by the camera 42 is performed in a state where the modeling surface 32a of the powder layer is irradiated with illumination light emitted by an illumination light source (not shown) provided in the 3D additive manufacturing apparatus 1.
[0031] The shutter 44 protects the camera 42 and the observation window so that evaporated substances generated from the forming surface 32a do not adhere to the camera 42 or the observation window when the powder material 32 is melted by irradiation with the electron beam 15. The camera 42 photographs the forming surface 32a with the shutter 44 open. Moreover, in a process in which evaporated substances are likely to be generated or a process in which a large amount of evaporated substances are generated, that is, when the powder material 32 is melted by the electron beam 15, the shutter 44 is closed.
[0032] A plurality of detectors 46 for detecting reflected electrons are disposed below the beam irradiation device 2. Specifically, the detectors 46 are disposed between the beam irradiation device 2 and the printing surface 32a of the object 38 formed on the printing plate 22.
[0033] FIG. 3 is a plan view showing the position of the detection unit 46. As shown in FIG. 3, the multiple detection units 46a, 46b, 46c, and 46d are disposed so as to surround the periphery of the object 38 and the forming plate 22. The first detection unit 46a is disposed on one side of the object 38 in the X direction, and the second detection unit 46b is disposed on the other side of the object 38 in the X direction. The first detection unit 46a and the second detection unit 46b face each other with the object 38 therebetween. The third detection unit 46c is disposed on one side of the object 38 in the Y direction, and the fourth detection unit 46d is disposed on the other side of the object 38 in the Y direction. The third detection unit 46c and the fourth detection unit 46d face each other with the object 38 therebetween.
[0034] The detector 46 is not limited to a semiconductor detector, but may be a Ti electrode having a low secondary electron emission rate due to electronic excitation. The detector 46 may detect the reflected electrons incident on the electrode as a current using a current detection amplifier, and detect the increase or decrease of the current.
[0035] FIG. 2 is a block diagram showing an example of the configuration of a control system of the three-dimensional additive manufacturing apparatus 1 of this embodiment. As shown in Figure 2, the 3D additive manufacturing device 1 has a polarization amplifier control circuit 101 which is an electron beam control unit, an analog-to-digital conversion circuit (ADC) 102, a preamplifier (Pre-AMP) 103, a personal computer (PC) 104 which is an example of a control unit, and a display unit 105.
[0036] The polarization amplifier control circuit 101 is connected to the beam irradiation device 2 and the PC 104. The polarization amplifier control circuit 101 controls the beam irradiation device 2 based on the set beam scanning information. As a result, the beam irradiation device 2 irradiates a predetermined position with the electron beam 15. The polarization amplifier control circuit 101 also transmits beam irradiation position information indicating the irradiation position of the electron beam 15 to the PC 104.
[0037] The Pre-AMP 103 is connected to the detection unit 46 and the ADC 102. The Pre-AMP 103 converts the reflected electron current detected by the detection unit 46 from a current signal to a voltage signal. The voltage signal converted by the Pre-AMP 103 is transmitted to the ADC 102. The ADC 102 converts the reflected electron signal, which has become a voltage signal, from an analog signal to a digital signal and transmits it to the PC 104.
[0038] PC 104 has an image processing unit and a storage unit (not shown). The image processing unit of PC 104 captures an image generated by camera 42 and performs a predetermined image processing on the captured image. PC 104 outputs the camera image that has been subjected to image processing by the image processing unit to display unit 105.
[0039] The storage unit stores the camera images generated by the image processing unit. Furthermore, the storage unit stores beam irradiation position information transmitted from the polarization amplifier control circuit 101. The storage unit also stores a plurality of arithmetic expressions for performing arithmetic processing on the reflected electron signals obtained from the plurality of detection units 46a, 46b, 46c, and 46d.
[0040] The PC 104 selects a predetermined arithmetic expression from a plurality of arithmetic expressions according to the modeling process. Then, the PC 104 performs arithmetic processing on the reflected electron signal using the selected arithmetic expression to calculate an arithmetic signal. Then, the image processing unit visualizes the arithmetic signal to obtain a reflected electron image (BSE image). The PC 104 outputs the obtained reflected electron image (BSE image) to the display unit 105. In addition, the reflected electron image (BSE image) is stored in the storage unit.
[0041] The display unit 105 is configured with a display such as a liquid crystal display (LCD) or an organic ELD (Electro Luminescence Display), etc. The display unit 105 displays the BSE image and the camera image output from the PC 104 on a display screen 106 (see FIG. 4, etc.).
[0042] 1-2. Example of operation of 3D additive manufacturing device Next, an example of the operation of the three-dimensional additive manufacturing apparatus 1 having the above-mentioned configuration will be described with reference to FIGS.
[0043] First, the beam irradiation device 2 operates based on a control command given from the PC 104 to heat the shaping plate 22. The beam irradiation device 2 irradiates the shaping plate 22 with the electron beam 15 through the opening 30a of the mask cover 30, and scans the shaping plate 22 with the electron beam 15. As a result, the shaping plate 22 is heated to a temperature at which the powder material 32 is provisionally sintered.
[0044] Next, the powder material 32 is spread on the shaping plate 22. The plate moving device 26 operates based on a control command given from the PC 104 to lower the shaping plate 22 by a predetermined amount. The plate moving device 26 lowers the inner base 24 by a predetermined amount so that the upper surface of the shaping plate 22 is slightly lower than the upper surface of the powder material 32 spread on the shaping table 18. At this time, the shaping plate 22 is lowered by the predetermined amount together with the inner base 24.
[0045] Then, the powder supplying device 16 drops the powder material 32 supplied from the hopper 16a to the powder dropper 16b onto the modeling table 18 by the powder dropper 16b, and then moves the squeegee 16c from one end side to the other end side in the X direction to spread the powder material 32 over the inner base 24. At this time, the powder material 32 is spread over the modeling table 18 to a thickness equivalent to ΔZ. In addition, excess powder material 32 is collected in the collection box 21.
[0046] Next, the beam irradiation device 2 operates based on control commands given from the polarization amplifier control circuit 101 and the PC 104 to preheat, or so-called powder heat (PH), the powder layer on the modeling plate 22. The powder layer is preheated in order to pre-sinter the powder material 32. Pre-sintering the powder material 32 can impart electrical conductivity to the powder material 32. This can suppress powder scattering in the main sintering process carried out after the pre-heating process.
[0047] The beam irradiation device 2 irradiates the powder material 32 on the printing plate 22 with the electron beam 15. The beam irradiation device 2 also scans the electron beam 15 over an area wider than the area for forming the model 38 (hereinafter also referred to as the "printing area"). As a result, the powder material 32 present in the printing area and the powder material 32 present around the printing area are both pre-sintered.
[0048] Next, a backscattered electron image (BSE image) is acquired. First, the beam irradiation device 2 scans the electron beam 15 on the pre-sintered region where the pre-sintered powder material 32 exists by operating based on control commands given from the polarization amplifier control circuit 101 and the PC 104. At this time, the beam irradiation device 2 reduces the electron beam current of the electron beam 15 as much as possible and irradiates the electron beam 15 while focusing it on the manufacturing surface 32a. Then, the detection unit 46 detects the backscattered electrons generated by the electron beam 15.
[0049] Furthermore, the detection unit 46 outputs the detected reflected electron signal to the PC 104 via the Pre-AMP 103 and the ADC 102. Here, the PC 104 selects an arithmetic equation capable of emphasizing the contour of the object 38 from among a plurality of arithmetic equations. Then, the PC 104 performs arithmetic processing on the reflected electron signal using the selected arithmetic equation to calculate an arithmetic signal. Then, the image processing unit converts the arithmetic signal into an image to obtain a reflected electron image (BSE image).
[0050] FIG. 4 shows an example of a backscattered electron image acquired after powder heating. The image processing unit performs arithmetic processing on the reflected electron signals acquired from the multiple detection units 46a, 46b, 46c, and 46d to generate a reflected electron image. Here, in the reflected electron image acquired after the powder heat, the image processing unit adds the first reflected electron signal A of the first detection unit 46a and the second reflected electron signal B of the second detection unit 46b, which are arranged opposite to each other. That is, the arithmetic expression is A+B. The third reflected electron signal C of the third detection unit 46c and the fourth reflected electron signal D of the fourth detection unit 46d, which are arranged opposite to each other, may be added (C+D). By using such an arithmetic expression, it is possible to acquire a reflected electron image in which the contour of the model 38 is emphasized. This makes it easier to check whether the powder material 32 has been properly spread, and the PC 104 can accurately perform the process of determining the degree of spreading of the powder material 32. In FIG. 4, the powder is properly spread, so that the image is basically uniformly black all over.
[0051] Next, using the acquired BSE image, the PC 104 judges whether the powder material 32 has been properly spread. If the PC 104 judges that the powder material 32 has not been properly spread, the operation of spreading the powder material 32 is performed again.
[0052] Next, the beam irradiation device 2 operates based on control commands given from the PC 104 and the polarization amplifier control circuit 101 to melt and solidify the powder material 32. The powder material 32 provisionally sintered as described above is irradiated with the electron beam 15 to melt and solidify, thereby finally sintering the powder material 32 as a provisionally sintered body.
[0053] The beam irradiation device 2 specifies a printing region based on two-dimensional data obtained by slicing three-dimensional CAD data of a target object 38 at a certain thickness (a thickness corresponding to ΔZ), and selectively melts the powder material 32 on the printing plate 22 by scanning the electron beam 15 over this printing region. The powder material 32 melted by irradiation with the electron beam 15 solidifies after the electron beam 15 has passed. This forms the first layer of the object.
[0054] Next, a backscattered electron image (BSE image) after the main melting, i.e., a post-melt BSE image, is obtained. First, the beam irradiation device 2 scans the electron beam 15 on the pre-sintered region where the pre-sintered powder material 32 exists, by operating based on control commands given from the polarization amplifier control circuit 101 and the PC 104. At this time, the beam irradiation device 2 makes the electron beam current of the electron beam 15 as small as possible, and focuses and irradiates the electron beam 15 on the manufacturing surface 32a. Then, the detection unit 46 detects the backscattered electrons generated by the electron beam 15.
[0055] The detection unit 46 also outputs the detected reflected electron signal to the PC 104 via the Pre-AMP 103 and the ADC 102. The detection unit 46 also outputs the detected reflected electron signal to the PC 104 via the Pre-AMP 103 and the ADC 102. The PC 104 then selects an arithmetic equation that can emphasize the unevenness of the object 38 from among a plurality of arithmetic equations. The PC 104 then performs arithmetic processing on the reflected electron signal using the selected arithmetic equation to calculate an arithmetic signal. The image processing unit then images the arithmetic signal to obtain a reflected electron image (BSE image).
[0056] FIG. 6 shows an example of a backscattered electron image acquired after the main melting. In the reflected electron image acquired after the main melting, the image processing unit subtracts the first reflected electron signal A from the second reflected electron signal B, or subtracts the third reflected electron signal C from the fourth reflected electron signal D. This makes it possible to acquire a reflected electron image in which the unevenness of the printing surface 32a of the object 38 is emphasized.
[0057] The arithmetic formula may be (AB) / (A+B) or (CD) / (C+D). That is, by dividing the subtraction signal of two reflected electron images by the addition signal of two reflected electron images, it is possible to suppress the influence of fluctuations in the electron beam current and noise. As a result, as shown in FIG. 6, it is possible to obtain a reflected electron image in which the unevenness of the printing surface 32a of the model 38 is emphasized. As a result, it becomes easier to check whether the powder material 32 has been properly melted, and the PC 104 can accurately perform the process of determining the degree of melting of the powder material 32.
[0058] Next, the PC 104 evaluates the post-melt BSE image to determine whether or not the powder material 32 has been properly melted. If the PC 104 determines that the powder material 32 has not been properly melted, the PC 104 performs the main melting operation of the powder material 32 again.
[0059] Next, in preparation for spreading the powder material 32, afterheating (AH) is performed to heat the printing surface 32a. The beam irradiation device 2 operates under the control of the polarization amplifier control circuit 101 and the PC 104 to irradiate the electron beam 15 onto the printing surface 32a through the opening 30a of the mask cover 30. At this time, the polarization amplifier control circuit 101 defocuses the electron beam 15 using an objective lens or the like provided in the beam irradiation device 2. This defocusing causes the focal position of the electron beam 15 to shift downward from the printing surface 32a, i.e., an underfocused state.
[0060] Furthermore, the polarization amplifier control circuit 101 and the PC 104 control the beam irradiation device 2 to scan the electron beam 15 over a wider area than the opening 30a of the mask cover 30. As a result, the electron beam 15 is irradiated onto the entire surface 32a to be molded that is exposed to the opening 30a. The surface 32a to be molded is heated to a temperature at which the powder material 32 is provisionally sintered. When the surface 32a to be molded is heated to a predetermined temperature, the beam irradiation device 2 stops irradiating the electron beam 15.
[0061] Next, the shaping plate 22 is lowered by a predetermined amount (ΔZ). The plate moving device 26 lowers the inner base 24 by ΔZ so that the shaping surface 32a is slightly lower than the upper surface of the powder material 32 spread on the shaping table 18.
[0062] Thereafter, the above-mentioned steps are repeated until the modeling is completed up to the final layer, i.e., until the modeling of the model 38 is completed. The modeling of the model 38 is completed at the stage where the powder material 32 has been melted and solidified for the number of layers required to form the model 38. In this way, the desired model 38 is obtained.
[0063] In this way, the PC 104 selects the calculation formula for acquiring the BSE image according to the modeling process. This allows the judgment to be made using appropriate information when performing judgment using the BSE image. As a result, the judgment can be easily performed and the judgment accuracy can be improved. Furthermore, by preparing multiple calculation formulas in advance, multiple types of images can be acquired from the reflected electron signal, so that the reflected electron signal can be used for multiple types of judgment processing, expanding the applications of the reflected electron signal.
[0064] The calculation formula is not limited to the above example. For example, the BSE image used when determining the degree of spreading of the powder material 32 may be calculated by the calculation formula A+B+C+D using the first reflected electron signal A, the second reflected electron signal B, the third reflected electron signal C, and the fourth reflected electron signal D. This makes it possible to obtain a reflected electron image in which the contour of the model 38 is more emphasized. As a result, it becomes easier to check whether the powder material 32 has been properly spread, and the PC 104 can more accurately perform the process of determining the degree of spreading of the powder material 32.
[0065] Furthermore, the BSE image used when determining the melting degree of the powder material 32 may be calculated using an arithmetic formula that combines (AB) / (A+B) and (CD) / (C+D). A backscattered electron image in which the unevenness of the molding surface 32a of the molded object 38 is more emphasized can be acquired. As a result, it becomes easier to check whether the powder material 32 has been properly melted, and the PC 104 can accurately perform the process of determining the melting degree of the powder material 32.
[0066] Furthermore, as an arithmetic formula for acquiring a BSE image used when determining the melting degree of the powder material 32, for example, the following arithmetic formula may be used. First, a BSE image is acquired using the arithmetic formula (AB) / (A+B) or (CD) / (C+D). Then, a BSE image is acquired using the arithmetic formula A+B or C+D. Then, two BSE images acquired using the two arithmetic formulas are simultaneously displayed on the display screen 106. This allows not only the melting degree of the molded object 38 but also the shape and dimensions of the molded object 38 to be confirmed simultaneously. In other words, the arithmetic formula selected by the PC 104 is not limited to one, and depending on the contents of the molding process, one or more arithmetic formulas may be selected from a plurality of arithmetic formulas, and a plurality of calculation signals may be acquired using each arithmetic formula.
[0067] 1-3. Example of powder material spreading condition evaluation Next, an example of determining the degree of spreading of the powder material 32 will be described with reference to FIGS. Fig. 5 is a backscattered electron image acquired after powder heating, showing an example in which the powder material 32 was not properly spread. Note that the backscattered electron image shown in Fig. 5 is an image acquired by the calculation formula A+B.
[0068] If the powder material is properly laid, the reflected electron image will be a nearly entirely black image (see Figure 4). If no powder material is laid at all, the entire melted area in the previous layer will be white, and the other areas will be black, as shown in Figure 5. If only a portion of the powder material is laid, a part of the melted area in the previous layer (the area where the powder material was laid) will be black, the remaining melted area (the area where the powder material 32 was not laid) will be white, and the remaining powder material 32 will be all black.
[0069] Here, consider the three-dimensional coordinate system of xyz. Then, the data of the post-melt BSE image of the previous layer and the pre-melt BSE image of the current layer are digitized in the form of (x,y,z) for all pixel counts to create three-dimensional data of xyz. In other words, the position of the BSE image as the x coordinate, the position of the BSE image as the Y coordinate, and the brightness values of the BSE image corresponding to the X and Y coordinates are set. At this time, the whiter the image, the higher the brightness value, and the darker the image, the lower the value.
[0070] Then, 3D data is derived by taking the difference between the z coordinate values (brightness values of the BSE image corresponding to the X and Y coordinates) that correspond to the same x and y coordinates of the two 3D data. If no powder material is laid, the 3D data obtained by taking the difference between the post-melt BSE image of the previous layer and the pre-melt BSE image of the current layer will have z coordinate values (brightness values) that are nearly the same for all x and y coordinates. Therefore, it is expected that the z coordinate value will be close to 0 for all x and y coordinates.
[0071] On the other hand, if the powder material 32 is properly spread, the part of the model that was white in the previous layer will become black, so that the z-coordinate value in the xy coordinate indicating the position of the model in the three-dimensional data from which the difference is taken will be a brightness value indicating the difference between white and black (it will definitely be a value greater than 0). Therefore, two values are noted. The first value is the z-coordinate of the three-dimensional data from which the difference data is taken (the difference between the brightness and darkness of the two BSE images). A threshold value is then set for this value. The second value is the total number of pixels that exceed the threshold value of the z-coordinate of the three-dimensional data from which the difference data is taken (the difference between the brightness and darkness of the two BSE images), divided by the total number of pixels in the part where the BSE image has become white due to the presence of the model in the previous layer (hereinafter referred to as the powder spreading ratio). A threshold value can also be set for this powder spreading ratio, and if the value of the powder spreading ratio is smaller than this threshold, it is determined that the powder has not been spread properly. This makes it easy to determine the degree of spreading of the powder material 32.
[0072] 1-4. Example of determining the degree of melting of powder materials Next, an example of determining the degree of melting of the powder material 32 will be described with reference to FIG. Figure 6 shows a backscattered electron image acquired after the main melting. Figure 6 shows an example including both a portion (i) where the powder material was relatively properly melted and portions (j) to (q) where the powder material was not properly melted. The backscattered electron image shown in Figure 7 is an image acquired using the formula (AB) / (A+B).
[0073] When the powder material 32 is properly melted, the top surface of the surface 32a to be molded becomes flat as shown in part (i) of FIG. 6. When the powder material 32 is not properly melted, the top surface of the surface 32a to be molded becomes very uneven as shown in parts (j) to (q) of FIG. 6. Here, the unevenness of the top surface can be regarded as a three-dimensional wave. Then, the maximum amplitude and maximum period of this three-dimensional wave are obtained. In addition, the unevenness of the top surface can be quantified in the form of three-dimensional coordinates (x, y, z) of xyz with all the number of pixels, and can be made into three-dimensional data of xyz. That is, the brightness value of the BSE image corresponding to the position as the X coordinate of the BSE image and the position X coordinate and Y coordinate of the BSE image are set.
[0074] Then, the maximum amplitude and maximum period are obtained from the three-dimensional data. Threshold values are set for the amplitude and period, and when either or both of the threshold values are exceeded, it is determined that the powder material 32 is not properly melted. This makes it possible to determine the degree of melting of the powder material 32.
[0075] 2. Second embodiment Next, a three-dimensional additive manufacturing apparatus according to a second embodiment will be described with reference to FIG. FIG. 7 is a plan view showing the position of a detection unit in a three-dimensional additive manufacturing apparatus according to the second embodiment.
[0076] The difference between the 3D additive manufacturing device according to the second embodiment and the 3D additive manufacturing device according to the first embodiment is the number of detection units. Therefore, here, the parts common to the 3D additive manufacturing device according to the first embodiment are given the same reference numerals and redundant explanations are omitted.
[0077] 7, the device has eight detection units 46a, 46b, 46c, 46d, 46e, 46f, 46g, and 46h. The eight detection units 46a, 46b, 46c, 46d, 46e, 46f, 46g, and 46h are arranged at equal angular intervals so as to surround the periphery of the model 38. In other words, the three-dimensional additive manufacturing device according to the second embodiment has an electrode divided into eight parts.
[0078] The image processing unit acquires a BSE image using reflected electron signals A, B, C, D, E, F, G, and H from the eight detection units 46a, 46b, 46c, 46d, 46e, 46f, 46g, and 46h. As an arithmetic expression for acquiring a BSE image, for example, A+B+C+D+E+F+G+H or various other arithmetic expressions can be used.
[0079] Furthermore, by configuring the detection units 46a, 46b, 46c, 46d, 46e, 46f, 46g, and 46h as eight-division electrodes, it is possible to obtain inclination information of the printing surface 32a from directions of every 45° from AE to DH. Therefore, it is possible to analyze the surface shape of the printing surface 32a in more detail, and obtain highly accurate unevenness information.
[0080] Other configurations are the same as those of the 3D additive manufacturing apparatus 1 according to the first embodiment, and therefore description thereof will be omitted. The 3D additive manufacturing apparatus according to the second embodiment can also obtain the same effects as those of the 3D additive manufacturing apparatus according to the first embodiment described above.
[0081] 3. Third embodiment Next, a three-dimensional additive manufacturing apparatus according to a third embodiment will be described with reference to FIG. FIG. 8 is a plan view showing the position of a detection unit in a three-dimensional additive manufacturing apparatus according to a third embodiment.
[0082] The difference between the 3D additive manufacturing device according to the third embodiment and the 3D additive manufacturing device according to the first embodiment is the number of detection units. Therefore, here, the parts common to the 3D additive manufacturing device according to the first embodiment are given the same reference numerals and redundant explanations are omitted.
[0083] 8, the three-dimensional additive manufacturing device according to the third embodiment has twelve detection units 46a, 46b, 46c, 46d, 46e, 46f, 46g, 46h, 46i, 46j, 46k, and 46l. The twelve detection units 46a, 46b, 46c, 46d, 46e, 46f, 46g, 46h, 46i, 46j, 46k, and 46l are arranged at equal angular intervals so as to surround the periphery of the model 38. That is, the three-dimensional additive manufacturing device according to the third embodiment has an electrode divided into twelve parts.
[0084] For the printing surface 32a in which the emission direction of reflected electrons is three-fold symmetric (hexagonal crystal, etc.) or four-fold symmetric (cubic crystal, etc.) due to the influence of crystal orientation, etc., a BSE image is obtained using electrode signals in the three-fold symmetric direction (A+E+I, B+F+J, C+G+K, D+H+L) in the reflected electron detection after melting. Also, a BSE image is obtained using electrode signals in the four-fold symmetric direction (A+D+G+J, B+E+H+K, C+F+I+L). Then, by comparing the BSE image consisting of the electrode signals in the three-fold symmetric direction with the BSE image consisting of the electrode signals in the four-fold symmetric direction, crystal orientation information of the printing surface 32a can be obtained.
[0085] Other configurations are the same as those of the three-dimensional additive manufacturing apparatus 1 according to the first embodiment, and therefore description thereof will be omitted. The three-dimensional additive manufacturing apparatus according to the third embodiment can also obtain the same effects as those of the three-dimensional additive manufacturing apparatus according to the first embodiment described above.
[0086] In the three-dimensional additive manufacturing apparatus according to the second embodiment and the three-dimensional additive manufacturing apparatus according to the third embodiment, the shaping plate 22 is formed in a circular shape, but this is not limited thereto, and the shaping plate 22 may be formed in a rectangular shape as in the first embodiment. Also, for the circular shaping plate 22 shown in the three-dimensional additive manufacturing apparatus according to the second embodiment and the three-dimensional additive manufacturing apparatus according to the third embodiment, four detectors 46 may be provided and arranged on both sides in the X direction and the Y direction as in the first embodiment.
[0087] The present invention is not limited to the embodiment described above and shown in the drawings, and various modifications can be made without departing from the spirit of the invention described in the claims.
[0088] In the above-described embodiment, the image processing unit calculates the reflected electron signals, and then visualizes the respective calculation signals. However, the present invention is not limited to this. For example, a calculation formula corresponding to a process may be selected from a plurality of calculation formulas, and the calculation signal may be derived by performing a calculation using the reflected electron signals. Then, without imaging the calculation signal, it may be possible to determine whether the powder material has been properly laid or whether the powder material has been properly melted based on the information of the calculation signal.
[0089] Furthermore, the arithmetic formula is not limited to the above example, and for example, various other arithmetic formulas may be applied. A discrete Fourier transform is performed on the acquired reflected electron signals to decompose them into a plurality of wave number signals. Then, a BSE image may be generated from the decomposed wave number signals according to the modeling process.
[0090] The detection unit may also be one in which a plurality of detection surfaces are arranged in a two-dimensional array. In the case of such a detection unit, the detection surface is divided into predetermined regions. Then, the backscattered electron signals detected by the plurality of detection surfaces arranged in each region may be averaged for each region. In this way, various other configurations can be applied to the configuration of the detection unit.
[0091] For example, in the above-mentioned embodiment, an example was described in which metal powder such as titanium, aluminum, iron, etc. was used as the powder material, but the present invention is not limited thereto, and resin, etc., may be used as the powder material. Also, an example was described in which an electron gun that irradiates an electron beam was used as a heating mechanism for preheating or melting the powder material, but the present invention is not limited thereto. For example, a laser irradiation unit that irradiates a laser may be used as the heating mechanism.
[0092] Although the example in which the PC 104 is applied as the control unit has been described, the present invention is not limited to this. As the control unit, a control unit having various kinds of calculation functions, such as an electron beam control unit that controls the beam irradiation device 2, can be applied.
[0093] In the above-described embodiment, the detection unit 46 is disposed inside the radiation shield cover 28, but the present invention is not limited to this. The detection unit 46 may be disposed outside the radiation shield cover 28.
[0094] In addition, the above-mentioned components, functions, processing units, etc. may be realized in part or in whole in hardware, for example, by designing an integrated circuit. In addition, the above-mentioned components, functions, etc. may be realized in software by a processor interpreting and executing a program that realizes each function. Information such as the program, table, file, etc. that realizes each function can be stored in a recording device such as a memory, a hard disk, or an SSD (Solid State Drive), or in a recording medium such as an IC card, an SD card, or a DVD.
[0095] In this specification, the words "parallel" and "orthogonal" are used, but these do not mean only "parallel" and "orthogonal" in the strict sense, but may also mean a "substantially parallel" or "substantially orthogonal" state that includes "parallel" and "orthogonal" and is within a range in which the respective functions can be exerted. [Explanation of symbols]
[0096] 1...3D additive manufacturing device, 2...beam irradiation device, 3...vacuum chamber, 15...electron beam, 16...powder supply device, 16a...hopper, 16b...powder dropper, 16c...squeegee, 16d...blade, 18...modeling table, 20...modeling box, 21...collection box, 22...modeling plate, 24...inner base, 26...plate moving device, 32...powder material, 32a...modeling surface, 38...modeled object, 42...camera, 44...shutter, 46...detection unit, 101...polarization amplifier control circuit, 102...digital conversion circuit (ADC), 103...preamplifier (Pre-AMP) 104...personal computer (PC, control unit), 105...display unit, 106...display screen
Claims
1. A molding plate, a powder supplying device for supplying a powder material to the build plate to form a powder layer; a beam irradiation device that irradiates the powder layer with an electron beam; a plurality of detection units for detecting reflected electrons generated when the powder material is irradiated with the electron beam; a control unit that acquires a plurality of reflected electron signals detected by the plurality of detection units, performs arithmetic processing on the plurality of reflected electron signals, and calculates an arithmetic signal; The control unit has a plurality of calculation expressions, The control unit selects a predetermined arithmetic expression from a plurality of arithmetic expressions in accordance with a modeling process, and performs arithmetic processing on the plurality of reflected electron signals using the selected arithmetic expression to calculate an arithmetic signal. 3D additive manufacturing device.
2. The control unit judges the degree of spreading of the powder material based on a calculation signal obtained by adding up the plurality of reflected electron signals. The three-dimensional additive manufacturing apparatus according to claim 1 .
3. The control unit determines the degree of melting of the powder material based on a calculation signal obtained by subtracting a plurality of reflected electron signals. The three-dimensional additive manufacturing apparatus according to claim 1 .
4. The control unit, when determining the degree of melting of the powder material, performs the determination based on a calculation signal obtained by dividing a subtraction signal obtained by subtracting a plurality of reflected electron signals by an addition signal obtained by adding the plurality of reflected electron signals. The three-dimensional additive manufacturing apparatus according to claim 3 .
5. Selecting one or more arithmetic expressions from the plurality of arithmetic expressions according to the modeling process, and calculating a plurality of arithmetic signals using each of the arithmetic expressions The three-dimensional additive manufacturing apparatus according to claim 1 .
6. The plurality of detectors are arranged to surround the periphery of the modeling plate. The three-dimensional additive manufacturing apparatus according to claim 1 .
7. A control method for a three-dimensional additive manufacturing device including a modeling plate, a powder supplying device that supplies a powder material to the modeling plate to form a powder layer, a beam irradiation device that irradiates the powder layer with an electron beam, a plurality of detection units that detect reflected electrons generated when the powder material is irradiated with the electron beam, and a control unit that acquires a plurality of reflected electron signals detected by the plurality of detection units, performs arithmetic processing on the plurality of reflected electron signals, and calculates an arithmetic signal, The control unit selects a predetermined arithmetic expression from a plurality of arithmetic expressions in accordance with a modeling process, and performs arithmetic processing on the plurality of reflected electron signals using the selected arithmetic expression to calculate an arithmetic signal. A method for controlling a three-dimensional additive manufacturing device.
Citation Information
Patent Citations
Additive manufacturing device with real-time in-situ detection function
CN113092508A
Detection device for reflection electron or the like in electron beam device
JP1988168951A
Three-dimensional lamination molding device and three-dimensional lamination molding method
JP2021041568A
Three-dimensional lamination molding method and three-dimensional lamination molding device
JP2021042410A