Secondary battery

By incorporating grooves in the negative electrode active material layer to control electrolyte penetration, the secondary battery addresses uneven metal salt distribution, improving Li precipitation resistance and overall performance.

JP2024152469AInactive Publication Date: 2024-10-25TOYOTA BATTERY CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023066693
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-04-14
Publication Date
2024-10-25
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

Existing secondary batteries face a decrease in Li precipitation resistance due to uneven distribution of metal salts in the negative electrode active material layer, leading to high resistance areas and reduced battery performance.

Method used

The secondary battery incorporates grooves in the negative electrode active material layer, extending orthogonally to the electrolyte permeation direction, which slows down solvent penetration, allowing for a dispersed coating formation and reducing Li precipitation resistance.

Benefits of technology

The grooves in the negative electrode active material layer facilitate even distribution of metal salts, preventing high-resistance areas and suppressing Li precipitation, thereby enhancing battery performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024152469000001_ABST
    Figure 2024152469000001_ABST
Patent Text Reader

Abstract

To suppress the decrease in Li precipitation resistance.SOLUTION: A lithium ion secondary battery 10 includes a wound body 30 in which a positive electrode sheet 50, a negative electrode sheet 40 having a negative electrode active material layer 42 containing a metal salt on the surface of a negative electrode current collector 41, and a separator 60 arranged between the positive electrode sheet 50 and the negative electrode sheet 40 are wound together, an electrolyte solution S containing an additive B that reacts with the metal salt, and grooves 45 formed in end regions W2, W4 in the width direction G of the negative electrode active material layer 42 and extending in a perpendicular direction that is approximately perpendicular to the penetration direction of the electrolyte solution S.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a secondary battery. [Background technology]

[0002] It is known that a secondary battery includes a wound body in which a positive electrode sheet, a negative electrode sheet, and a separator are wound in a stacked state (see, for example, Patent Document 1).

[0003] Patent Document 1 discloses a lithium ion secondary battery including a wound electrode body formed by stacking a positive electrode sheet having a positive electrode active material layer on the surface of a long positive electrode collector and a negative electrode sheet having a negative electrode active material layer on the surface of a long negative electrode collector with a long separator sheet interposed therebetween and winding them in the longitudinal direction. In this lithium ion secondary battery, a groove is formed on the surface of the central part in the winding axis direction of the negative electrode active material layer, which groove is continuous in the circumferential direction from the inside to the outside of the wound negative electrode active material layer. As a result, gas generated inside the wound electrode body is discharged to the outside of the wound electrode body through the groove.

[0004] Incidentally, in a secondary battery, it is preferable to suppress a decrease in Li precipitation resistance. [Prior art documents] [Patent documents]

[0005] [Patent Document 1] Patent Publication No. 2022-079876 Summary of the Invention [Problem to be solved by the invention]

[0006] In consideration of the above, an object of the present invention is to suppress the decrease in Li precipitation resistance. [Means for solving the problem]

[0007] A secondary battery according to a first aspect of the present invention comprises a wound body in which a positive electrode sheet, a negative electrode sheet having a negative electrode active material layer containing a metal salt on a surface of a negative electrode current collector, and a separator arranged between the positive electrode sheet and the negative electrode sheet are wound together, an electrolyte solution containing an additive that reacts with the metal salt, and a groove portion formed in an end region in the winding axis direction of the negative electrode active material layer and extending in a perpendicular direction that is approximately perpendicular to the penetration direction of the electrolyte solution.

[0008] In a secondary battery according to a second aspect of the present invention, in the secondary battery according to the first aspect of the present invention, the groove portion extends in the winding direction of the wound body.

[0009] In a secondary battery of a third aspect of the present invention, in the secondary battery of the first or second aspect of the present invention, the grooves are formed intermittently in a direction substantially perpendicular to a direction in which the electrolyte solution permeates.

[0010] In a secondary battery according to a fourth aspect of the present invention, in the secondary battery according to any one of the first to third aspects of the present invention, the groove portion is an uncoated portion of the negative electrode active material layer.

[0011] In a secondary battery of a fifth aspect of the present invention, in the secondary battery of any one of the first to fourth aspects of the present invention, the groove portion is provided in a range of 1 / 3 of the negative electrode active material layer from an end of the negative electrode active material layer in the winding axis direction.

[0012] In a sixth aspect of the secondary battery of the present invention, in any one of the first to fifth aspects of the secondary battery of the present invention, the grooves are formed in a plurality of areas in an end region in the winding axis direction of the negative electrode active material layer. Effect of the Invention

[0013] In the secondary battery according to the first embodiment of the present invention, the grooves are formed in the end regions in the winding axis direction of the negative electrode active material layer and extend in a direction perpendicular to the direction of permeation of the electrolyte, so that the permeation of the electrolyte solvent is slowed down by the grooves. Therefore, before the electrolyte solvent causes the metal salt to be unevenly distributed in the width direction center of the wound body, the metal salt reacts with the solution containing the additive. As a result, the coating is formed in a dispersed manner on the wound body, and the decrease in Li deposition resistance can be suppressed.

[0014] In the secondary battery according to the second embodiment of the present invention, the grooves extend in the winding direction of the wound body, and thus the penetration rate of the solvent of the electrolyte is slowed down in the grooves. Therefore, before the solvent of the electrolyte causes the metal salt to be unevenly distributed in the width direction center of the wound body, the metal salt reacts with the solution containing the additive. As a result, the coating is formed in a dispersed manner on the wound body, and the decrease in Li deposition resistance can be suppressed.

[0015] In the secondary battery according to the third aspect of the present invention, the grooves are formed intermittently in a direction perpendicular to the direction of permeation of the electrolyte, so that in the permeation direction, the permeation of the electrolyte solvent is slowed down in the portion where the grooves are formed, and is not slowed down in the portion where the grooves are not formed. Therefore, due to the difference in permeation speed, the electrolyte solvent permeates radially from the portion where the grooves are formed. As a result, the coating is formed in a dispersed manner on the wound body, and the decrease in Li deposition resistance can be suppressed.

[0016] In the secondary battery according to the fourth aspect of the present invention, the grooves are uncoated portions of the negative electrode active material layer, so that the penetration rate of the electrolyte solvent is slowed down in the uncoated portions. Therefore, before the electrolyte solvent causes the metal salt to be unevenly distributed in the width direction center of the wound body, the metal salt reacts with the additive-containing solution. As a result, the coating is formed in a dispersed manner on the wound body, and the decrease in Li deposition resistance can be suppressed.

[0017] In the secondary battery of the fifth aspect of the present invention, the groove is provided in the range of 1 / 3 of the negative electrode active material layer from the end of the negative electrode active material layer in the winding axis direction, so that the penetration speed of the electrolyte solvent can be slowed down before the solvent penetrates into the range where a coating tends to be formed if the groove is not provided. Therefore, the metal salt reacts with the solution containing the additive before the electrolyte solvent causes the metal salt to be unevenly distributed in the center of the width direction of the wound body. As a result, the coating is formed in a dispersed manner on the wound body, and the decrease in Li deposition resistance can be suppressed.

[0018] In the secondary battery according to the sixth embodiment of the present invention, a plurality of grooves are formed in the end region in the winding axis direction of the negative electrode active material layer, so that the penetration of the solvent of the electrolyte is further slowed down by the plurality of grooves. Therefore, before the solvent of the electrolyte causes the metal salt to be unevenly distributed in the width direction center of the wound body, the metal salt reacts with the solution containing the additive. As a result, the coating is formed in a dispersed manner on the wound body, and the decrease in Li deposition resistance can be suppressed. [Brief description of the drawings]

[0019] [Figure 1] FIG. 1 is a perspective view showing a lithium-ion secondary battery according to a first embodiment. [Diagram 2] 2 is an enlarged cross section of the wound body according to the first embodiment, showing the cross section AA of FIG. [Diagram 3] FIG. 2 is a development view that illustrates a schematic view of the negative electrode sheet according to the first embodiment. [Figure 4] FIG. 1 is a front view showing a lithium-ion secondary battery according to a first embodiment. [Diagram 5] 5A and 5B are diagrams illustrating the penetration of an electrolyte solution into a negative electrode sheet according to the first embodiment, in which FIG. 5(A) shows the solvent penetrating into the grooves, and FIG. 5(B) shows the solution penetrating beyond the grooves. [Figure 6] 6A and 6B are graphs showing the resistance distribution of a negative electrode sheet when an electrolyte solution permeates therein, where FIG. 6(A) is a graph showing the case where the electrolyte solution permeates at a fast rate, and FIG. 6(B) is a graph showing the case where the electrolyte solution permeates at a slow rate. [Figure 7]FIG. 6 is a development view that illustrates a schematic view of a negative electrode sheet according to a second embodiment. [Figure 8] FIG. 11 is a development view that illustrates a schematic view of a negative electrode sheet according to a third embodiment. [Figure 9] FIG. 4 is a development view that illustrates a schematic view of a negative electrode sheet according to another embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0020] [First embodiment] Hereinafter, the secondary battery according to the embodiment will be described with reference to the drawings. The secondary battery according to the first embodiment will be described as an example of a lithium ion secondary battery constituting a battery module used as an on-board power source for electric vehicles, hybrid vehicles, etc. In each drawing, an arrow D indicates the longitudinal direction D of the lithium ion secondary battery 10, an arrow E indicates the depth direction E of the lithium ion secondary battery 10, an arrow F indicates the up-down direction F of the lithium ion secondary battery 10, an arrow T indicates the thickness direction T of the wound body 30, and an arrow R indicates the winding direction R of the wound body 30. The longitudinal direction D of the lithium ion secondary battery 10 coincides with the width direction (winding axis direction) G of the wound body 30, and one side of the width direction G of the wound body 30 is a positive electrode, and the other side of the width direction G of the wound body is a negative electrode.

[0021] [Configuration of lithium-ion secondary battery 10] As shown in FIG. 1, the lithium ion secondary battery 10 includes a lid assembly 20, a wound body 30, a battery case 70, and an electrolyte S (see FIG. 4).

[0022] (battery case 70) The battery case 70 is made of, for example, aluminum, and is formed in the shape of a rectangular box that is long in the longitudinal direction D and has an open top.

[0023] (Lid Assembly 20) The lid assembly 20 includes a lid member 21, a negative electrode current collector terminal 22 as a current collector terminal, a positive electrode current collector terminal 23 as a current collector terminal, a negative electrode external terminal 24 as an external terminal, and a positive electrode external terminal 25 as an external terminal.

[0024] <Cover member 21> The lid member 21 is made of, for example, aluminum, and is formed in a rectangular plate shape extending in the longitudinal direction D. The lid member 21 is provided with a safety valve 21A and a cap 26 that closes the injection port 21B.

[0025] The safety valve 21A opens when the internal pressure of the battery case 70 reaches a predetermined pressure, and discharges gas generated inside the battery case 70.

[0026] Inlet 21B is formed as a through hole penetrating in the plate thickness direction of lid member 21. Inlet 21B is used when injecting an electrolyte into battery case 70. Cap 26 is attached to inlet 21B, for example, by laser welding, and is hermetically sealed.

[0027] With the wound body 30, the negative electrode collector terminal 22, and the positive electrode collector terminal 23 housed inside the battery case 70, the lid member 21 is attached, for example, by laser welding, so as to cover the opening of the battery case 70.

[0028] <Negative electrode current collector terminal 22 and negative electrode external terminal 24> The negative electrode current collector terminal 22 and the negative electrode external terminal 24 are made of copper, and are disposed on the other end side in the longitudinal direction D of the battery case 70. The negative electrode current collector terminal 22 is formed in a rectangular plate shape with the plate thickness direction being the depth direction E. The negative electrode current collector terminal 22 is joined to the negative electrode current collector part 32 of the wound body 30 by, for example, ultrasonic welding. The negative electrode external terminal 24 is electrically connected to the negative electrode current collector terminal 22, and is exposed to the outside of the lid member 21.

[0029] <Positive electrode current collector terminal 23 and positive electrode external terminal 25> The positive electrode current collector terminal 23 is made of aluminum, for example, and is disposed at one end side in the longitudinal direction D of the battery case 70. The positive electrode current collector terminal 23 is formed in a rectangular plate shape with the depth direction E as the plate thickness direction. The positive electrode current collector terminal 23 is joined to the positive electrode current collector part 33 of the wound body 30 by, for example, resistance welding. The positive electrode external terminal 25 is electrically connected to the positive electrode current collector terminal 23 and exposed to the outside of the lid member 21.

[0030] (Wound body 30) 1 and 2, the wound body 30 has a power generating body 31, a negative electrode current collecting part 32, and a positive electrode current collecting part 33. The wound body 30 is formed by winding a negative electrode sheet 40 as an electrode sheet, a positive electrode sheet 50 as an electrode sheet, and two separators 60 in a stacked state, to have a flat cross section.

[0031] The power generation body 31 is formed by stacking a region of the positive electrode sheet 50 coated with a positive electrode active material, a region of the negative electrode sheet 40 coated with a negative electrode active material, and a separator 60. The power generation body 31 has a function of storing electric energy of the lithium ion secondary battery 10.

[0032] The negative electrode current collecting part 32 is not coated with an active material, and is formed by winding a negative electrode sheet 40. The positive electrode current collecting part 33 is not coated with an active material, and is formed by winding a positive electrode sheet 50.

[0033] <Negative electrode sheet 40> As shown in FIG. 2, the negative electrode sheet 40 is formed by coating a negative electrode mixture on both sides of a long strip-shaped negative electrode current collector 41, and forming a negative electrode active material layer .

[0034] The negative electrode active material layer 42 has a negative electrode active material. The negative electrode active material is a material capable of absorbing and releasing lithium, and for example, a powdered carbon material made of graphite or the like can be used. The negative electrode active material layer 42 is produced by kneading the negative electrode active material, a solvent, and a binder, and applying the kneaded negative electrode mixture to the negative electrode current collector 41 and drying it. The binder contains a metal salt. The metal salt can be, for example, a sodium salt.

[0035] The negative electrode active material layer 42 has an outer periphery-side negative electrode active material layer 43 arranged on the outer periphery-side, and an inner periphery-side negative electrode active material layer 44 arranged on the inner periphery-side. Since the outer periphery-side negative electrode active material layer 43 and the inner periphery-side negative electrode active material layer 44 have the same configuration, only the outer periphery-side negative electrode active material layer 43 will be described below.

[0036] <<Outer peripheral side negative electrode active material layer 43>> 2 and 3, the outer peripheral negative electrode active material layer 43 has a groove 45 extending in the winding direction R of the wound body 30. The groove 45 is continuously formed from the inner peripheral side to the outer peripheral side of the outer peripheral negative electrode active material layer 43. The groove 45 is formed extending in a direction perpendicular to the permeation direction of the electrolyte S into the wound body 30. The permeation direction of the electrolyte S into the wound body 30 is the width direction G of the wound body 30.

[0037] As shown in FIG. 3, the entire region W1 in the width direction G of the outer negative electrode active material layer 43 is divided into an end region W2 at the other end, an end region W4 at one end, and a central region W3.

[0038] The end region W2 may be 1 / 3 of the region from the other end of the outer peripheral negative electrode active material layer 43 in the width direction G. The end region W4 may be 1 / 3 of the region from one end of the outer peripheral negative electrode active material layer 43 in the width direction G.

[0039] The grooves 45 are formed in the end regions W2 and W4 in the width direction G. The end regions W2 and W4 can be in the range of 1 / 3 of the outer peripheral negative electrode active material layer 43 from the end of the outer peripheral negative electrode active material layer 43 in the width direction G.

[0040] The grooves 45 are desirably provided within 25 to 33% of the coating width from the end in the width direction G of the outer peripheral negative electrode active material layer 43.

[0041] As shown in Fig. 2, the groove portion 45 is formed in a concave shape with a rectangular cross section. The groove portion 45 is formed as an uncoated portion of the outer peripheral negative electrode active material layer 43. The groove portion 45 may be formed as an uncoated portion during coating, or may be formed by peeling after coating. The groove portion 45 may be a groove having a depth equal to or greater than half the thickness of the outer peripheral negative electrode active material layer 43.

[0042] However, if the groove width J of the groove portion 45 is wide, the area of ​​the negative electrode current collector 41 covered with the outer circumferential negative electrode active material layer 43 decreases, and the Li deposition resistance deteriorates. From this viewpoint, the groove width J of the groove portion 45 is preferably set to 0.2 mm or less.

[0043] <Positive electrode sheet 50> The positive electrode sheet 50 is formed by coating a positive electrode mixture on both sides of a long strip-shaped positive electrode current collector 51 to form a positive electrode active material layer 52 .

[0044] The positive electrode active material layer 52 has a positive electrode active material. The positive electrode active material is a material capable of absorbing and releasing lithium, and examples of the material that can be used include lithium cobalt oxide (LiCoO2), lithium manganese oxide (LiMn2O4), and lithium nickel oxide (LiNiO2).

[0045] The positive electrode active material layer 52 has an outer periphery side positive electrode active material layer 53 arranged on the outer periphery side, and an inner periphery side positive electrode active material layer 54 arranged on the inner periphery side.

[0046] <Separator 60> The separator 60 is formed of an insulating material such as polypropylene, polyethylene, etc. The separator 60 is disposed between the positive electrode sheet 50 and the negative electrode sheet 40, and insulates the positive electrode sheet 50 from the negative electrode sheet 40.

[0047] (electrolyte) As shown in FIG. 4, the battery case 70 contains an electrolyte solution S together with the wound body 30. The electrolyte solution S is a composition in which a supporting salt is contained in a solvent. An additive that reacts with the metal salt contained in the negative electrode active material layer 42 is added to the electrolyte solution S. The additive may be, for example, a lithium salt. The lithium salt may be, for example, lithium bis(oxalato)borate (LiBOB).

[0048] [Operation of lithium-ion secondary battery 10] In the lithium ion secondary battery 10 configured as described above, the output of the wound body 30 is taken from the negative electrode external terminal 24 and the positive electrode external terminal 25, and is used as a power source for electric vehicles, hybrid vehicles, and the like.

[0049] [Causes of decrease in Li precipitation resistance] In the lithium-ion secondary battery 10, an overvoltage occurs due to a reaction between an excessive current and lithium at a location of high film resistance in the negative electrode sheet 40, causing Li metal to precipitate. The Li metal becomes inactive due to a reaction with the electrolyte S, which causes a decrease in battery capacity. For this reason, in a device using the lithium-ion secondary battery 10, current control is performed so that Li metal does not precipitate, and poor resistance to Li precipitation is one of the causes of performance degradation.

[0050] The coating is formed by a decomposition reaction of the electrolyte S. The coating affects the life characteristics, input / output characteristics, and Li precipitation resistance of the lithium ion secondary battery 10, so various additives are added to the electrolyte S to improve the battery performance. When the electrolyte S is injected into the lithium ion secondary battery 10, it permeates the wound body 30, but the solution containing the electrolyte additive permeates slower than the solvent. Therefore, the components in the negative electrode mixture that are easily dissolved in the solvent are unevenly distributed near the center of the width direction G of the wound body 30. If there is a substance that reacts with the electrolyte additive among the components unevenly distributed in the center, a coating with high resistance is formed near the center of the width direction G of the wound body 30. The local high resistance portion is a factor that reduces the Li precipitation resistance of the battery. In the first embodiment, a groove portion 45 is provided in the negative electrode active material layer 42 in order to suppress such a decrease in Li precipitation resistance.

[0051] [Penetration of electrolyte S] As shown in FIG. 4, the electrolyte S permeates from the end portions in the width direction G of the wound body 30 toward the center portion in the width direction G.

[0052] When the electrolyte solution S permeates from the end of the wound body 30 in the width direction G, the electrolyte solution S permeates into the negative electrode active material layer 42. As shown in FIG. 5(A), when the electrolyte solution S permeates into the negative electrode active material layer 42, the solvent S1 not containing additive B, which has a faster permeation speed than the solution S2 containing additive B, reaches the groove portion 45 first. Then, the solvent S1 is stored in the groove portion 45. That is, the permeation of the solvent S1 into the negative electrode active material layer 42 is slowed down by the groove portion 45.

[0053] Next, as shown in FIG. 5(B), the solution S2 that arrives at the grooves 45 later and the solvent S1 that has been decelerated in the grooves 45 permeate toward the center of the negative electrode active material layer 42 in the width direction G.

[0054] [Resistance distribution due to differences in permeation speed] An experiment was carried out to confirm the resistance distribution due to differences in the permeation speed of the electrolyte S into the negative electrode active material layer.

[0055] In the experiment, the resistance distribution when the permeation rate of the electrolyte S into the negative electrode active material layer was increased, and the resistance distribution when the permeation rate of the electrolyte S into the negative electrode active material layer was decreased, were confirmed.

[0056] As shown in Fig. 6(A), when the permeation rate of the electrolyte solution S into the negative electrode active material layer was increased, a local high resistance portion was formed in the central region W3. As shown in Fig. 6(B), when the permeation rate of the electrolyte solution S into the negative electrode active material layer was decreased, no local high resistance portion was formed in the end regions W2, W4 and the central region W3.

[0057] [Effect] Incidentally, the electrolyte S generally permeates from both ends of the width direction G of the wound body 30 toward the center in the width direction. Here, the solvent S1 of the electrolyte S has a faster permeation speed than the solution S2 containing the additive B. Therefore, the metal salt dispersed and arranged in the negative electrode active material layer 42 dissolves in the solvent S1 and becomes unevenly distributed in the width direction center of the wound body 30. Then, the metal salt unevenly distributed in the width direction center of the wound body 30 and the solution S2 containing the additive B that permeates later join together, and a coating is formed in the width direction center of the wound body 30 by a chemical reaction. As a result, the coating resistance becomes high in the width direction center of the wound body 30, and an overvoltage occurs due to a reaction between the excess current and lithium, which may reduce the Li deposition resistance.

[0058] The lithium ion secondary battery 10 of the first embodiment includes a wound body 30 in which a positive electrode sheet 50, a negative electrode sheet 40 having a negative electrode active material layer 42 containing a metal salt on the surface of a negative electrode current collector 41, and a separator 60 arranged between the positive electrode sheet 50 and the negative electrode sheet 40 are wound together, an electrolyte solution S containing an additive B that reacts with the metal salt, and groove portions 45 formed in end regions W2, W4 in the width direction G of the negative electrode active material layer 42 and extending in a perpendicular direction that is approximately perpendicular to the penetration direction of the electrolyte solution S (see FIG. 2).

[0059] The grooves 45 are formed in the end regions W2 and W4 in the width direction G of the negative electrode active material layer 42 and extend in a direction perpendicular to the direction of permeation of the electrolyte S, and thus the permeation of the solvent S1 of the electrolyte S is slowed down by the grooves 45. Therefore, before the metal salt is unevenly distributed in the width direction center of the wound body 30 by the solvent S1 of the electrolyte S, the metal salt reacts with the solution S2 containing the additive B. As a result, a coating is formed in a dispersed manner on the wound body 30, and a decrease in Li precipitation resistance can be suppressed.

[0060] In the lithium ion secondary battery 10 of the first embodiment, the groove portion 45 extends in the winding direction R of the wound body 30 (see FIG. 3).

[0061] Groove 45 extends in the winding direction R of wound body 30, and thus the penetration of solvent S1 of electrolytic solution S is slowed down by groove 45. Therefore, before the metal salt is unevenly distributed in the width direction center of wound body 30 by solvent S1 of electrolytic solution S, the metal salt reacts with solution S2 containing additive B. As a result, a coating is formed in a dispersed manner in wound body 30, and a decrease in Li deposition resistance can be suppressed.

[0062] In the lithium ion secondary battery 10 of the first embodiment, the groove portion 45 is an uncoated portion of the negative electrode active material layer 42 (see FIG. 3).

[0063] Since the grooves 45 are uncoated portions of the negative electrode active material layer 42, the penetration of the solvent S1 of the electrolyte S is slowed down in the uncoated portions. Therefore, before the solvent S1 of the electrolyte S causes the metal salt to be unevenly distributed in the width direction center of the wound body 30, the metal salt reacts with the solution S2 containing the additive B. As a result, a coating is formed in a dispersed manner in the wound body 30, and a decrease in Li deposition resistance can be suppressed.

[0064] Incidentally, if the groove portion 45 is not provided, a coating is formed in the central region W3 of the negative electrode active material layer 42. Therefore, as shown in Fig. 6(A), in the central region W3 of the negative electrode active material layer 42, the coating resistance becomes high, and an overvoltage occurs due to a reaction between the excess current and lithium, which may result in a decrease in Li deposition resistance.

[0065] In the lithium ion secondary battery 10 of the first embodiment, the grooves 45 are provided in the width direction G over a range of ⅓ of the negative electrode active material layer 42 from the end of the negative electrode active material layer 42 in the width direction G (see FIG. 3).

[0066] The grooves 45 are provided in the range of 1 / 3 of the negative electrode active material layer 42 from the end of the negative electrode active material layer 42 in the width direction G, and this allows the permeation speed of the solvent S1 of the electrolytic solution S to be slowed down before the solvent S1 permeates into the range where a coating tends to be formed if the grooves 45 are not provided. Therefore, before the metal salt is unevenly distributed in the center of the width direction of the wound body 30 by the solvent S1 of the electrolytic solution S, the metal salt reacts with the solution S2 containing the additive B. As a result, the coating is formed in a dispersed manner in the wound body 30, and the decrease in Li precipitation resistance can be suppressed.

[0067] Second Embodiment The lithium ion secondary battery of the second embodiment differs from the lithium ion secondary battery of the first embodiment in that the configuration of the groove is different. Note that the same or equivalent parts as those described in the first embodiment will be described using the same terms or symbols. In addition, since the outer periphery side negative electrode active material layer 43 and the inner periphery side negative electrode active material layer 44 have the same configuration, the outer periphery side negative electrode active material layer 43 will be described below.

[0068] 7, the grooves 145 are formed discontinuously from the inner periphery side to the outer periphery side of the outer negative electrode active material layer 43. The length L1 of the grooves 145 in the winding direction R is preferably longer than the length L2 between the grooves 145.

[0069] [Effect] In the lithium ion secondary battery 10 of the second embodiment, the grooves 145 are formed intermittently in the winding direction R (see FIG. 7).

[0070] As a result, in the permeation direction, the permeation of the solvent S1 of the electrolyte S is slowed down in the portion where the groove portion 145 is formed, and the permeation of the solvent S1 of the electrolyte S is not slowed down in the portion where the groove portion 145 is not formed. Therefore, due to this difference in permeation speed, the solvent S1 of the electrolyte S permeates radially from the portion where the groove portion 145 is formed. As a result, the coating is formed in a dispersed manner on the wound body 30, and the decrease in Li deposition resistance can be suppressed.

[0071] Other configurations and functions and effects are substantially the same as those of the first embodiment, and therefore description thereof will be omitted.

[0072] Third Embodiment The lithium ion secondary battery of the third embodiment differs from the lithium ion secondary battery of the first embodiment in that the configuration of the groove is different. Note that the same or equivalent parts as those described in the first embodiment will be described using the same terms or symbols.

[0073] As shown in FIG. 8, a plurality of grooves 45 (two in the third embodiment) are formed in each of the end regions W2 and W4 in the width direction G of the negative electrode active material layer .

[0074] [Effect] In the lithium ion secondary battery 10 of the third embodiment, a plurality of grooves 45 are formed in end regions W2, W4 in the width direction G of the negative electrode active material layer 42 (see FIG. 8).

[0075] This causes the penetration of the solvent S1 of the electrolytic solution S to be slowed down by the multiple grooves 45. Therefore, before the solvent S1 of the electrolytic solution S causes the metal salt to be unevenly distributed in the width direction center of the wound body 30, the metal salt reacts with the solution S2 containing the additive B. As a result, a coating is formed in a dispersed manner on the wound body 30, and a decrease in Li deposition resistance can be suppressed.

[0076] Other configurations and functions and effects are substantially the same as those of the first embodiment, and therefore description thereof will be omitted.

[0077] The lithium ion secondary battery of the present invention has been described above based on the first to third embodiments. However, the specific configuration is not limited to these embodiments, and design changes and the like are permitted as long as they do not deviate from the gist of the invention according to each claim of the claims.

[0078] In the first to third embodiments, the grooves 245 are provided to extend in a direction perpendicular to the permeation direction of the electrolytic solution S. However, the grooves 245 may be provided to extend in a direction perpendicular to the permeation direction of the electrolytic solution S. For example, as shown in FIG. 9, the grooves 245 may be provided to meander with respect to the winding direction R of the wound body 30.

[0079] In the first to third embodiments, an example has been shown in which the grooves are provided in the negative electrode active material layer 42 on both sides of the negative electrode current collector 41. However, the grooves may be provided in the negative electrode active material layer 42 on one side of the negative electrode current collector 41. Furthermore, the position of the groove provided on one side of the negative electrode current collector 41 and the position of the groove provided on the other side of the negative electrode current collector 41 may be shifted in the width direction G.

[0080] In the first to third embodiments, the grooves are formed as uncoated portions of the negative electrode active material layer 42. However, the grooves may be formed as grooves having a depth equal to or greater than half the thickness of the outer peripheral negative electrode active material layer. Alternatively, the grooves may be formed such that either one of the end region W2 and the end region W4 is formed as an uncoated portion, and the other is formed as a groove having a depth equal to or greater than half the thickness of the outer peripheral negative electrode active material layer.

[0081] In the first to third embodiments, the grooves are formed in the end region W2 and the end region W4. However, the grooves may be formed in either the end region W2 or the end region W4.

[0082] In the first to third embodiments, the grooves are formed from the inner periphery to the outer periphery of the negative electrode active material layer 42. However, the grooves may be formed wider or deeper on the outer periphery than on the inner periphery. This makes it possible to deal with the outer periphery of the negative electrode active material layer having poor resistance to Li deposition.

[0083] In the first to third embodiments, the battery is a lithium ion secondary battery, but the battery is not limited to this, and the present invention can be applied to a secondary battery having a wound body having a negative electrode sheet with a negative electrode active material layer containing a metal salt, and an electrolyte solution containing an additive that reacts with the metal salt. [Explanation of symbols]

[0084] 10 Lithium-ion secondary battery (example of battery) 50 Positive electrode sheet 30 Wound body 40 Negative electrode sheet 41 Negative electrode current collector 42 Negative electrode active material layer 45 Groove B. Additives R Winding direction S Electrolyte W2,W4 End area

Claims

1. a wound body in which a positive electrode sheet, a negative electrode sheet having a negative electrode active material layer containing a metal salt on the surface of a negative electrode current collector, and a separator disposed between the positive electrode sheet and the negative electrode sheet are wound; an electrolyte solution containing an additive that reacts with the metal salt; a groove portion formed in an end region in the winding axis direction of the negative electrode active material layer and extending in a direction perpendicular to a permeation direction of the electrolyte; A secondary battery comprising:

2. The groove portion extends in a winding direction of the winding body. The secondary battery according to claim 1 .

3. The grooves are formed intermittently in a direction perpendicular to the direction in which the electrolyte permeates. The secondary battery according to claim 1 .

4. The groove portion is an uncoated portion of the negative electrode active material layer. The secondary battery according to claim 1 .

5. The groove portion is provided in a range of 1 / 3 of the negative electrode active material layer from an end portion in the winding axis direction of the negative electrode active material layer. The secondary battery according to claim 1 .

6. The groove portion is formed in a plurality of regions in an end portion of the negative electrode active material layer in the winding axis direction. The secondary battery according to claim 1 .

Citation Information

Patent Citations

  • Non-aqueous electrolyte secondary battery and method for manufacturing non-aqueous electrolyte rechargeable battery

    JP2022079876A