Display device
By forming pixel electrodes and laminated films with a single resist mask and using a metal film to cover stepped surfaces, the manufacturing process is simplified, reducing costs and improving reliability in active matrix display devices.
Patent Information
- Application Number
- JP2024145344
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2005-10-14
- Filing Date
- 2024-08-27
- Publication Date
- 2024-11-19
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Conventional active matrix display devices require multiple resist masks and etching processes for forming laminated wiring, particularly for pixel electrodes, leading to a complex and costly manufacturing process.
The pixel electrode and the film laminated with it are formed using a single resist mask, with a metal film in contact with the pixel electrode to cover stepped portions and prevent disconnection, allowing for a simplified manufacturing process.
This approach reduces the number of manufacturing steps and costs while preventing pixel electrode disconnection and improving the reliability of display devices by using a metal film to cover stepped surfaces.
Smart Images

Figure 2024161594000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a semiconductor device having a pixel electrode, and more particularly to a display device. [Background technology]
[0002] When manufacturing an active matrix display device, thin film transistors ( Forming wiring that connects to the semiconductor film of a TFT (Thin Film Transistor) Then, a conductive film that will become a pixel electrode is formed on the wiring. A resist mask and a resist mask for forming the pixel electrodes were required.
[0003] In another example, a conductive film is formed to connect to the semiconductor film of the TFT, and the conductive film is There are examples where a metal film is formed on a conductive film, with the film also functioning as a pixel electrode (see, for example, Patent Document 2). 1) This differs from the above example in that a transparent conductive film is used as the conductive film, and the transparent conductive film is directly Since transparent conductive films are often made of materials with high resistance, the electrical resistance of the transparent conductive film In order to cover the size of the transparent conductive film, a metal film is formed on the transparent conductive film.
[0004] Patent Document 1, which directly connects a transparent conductive film to a semiconductor film, also etches the transparent conductive film. A resist mask for forming pixel electrodes and a resist mask for etching the metal film are used. A scooter was needed. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] Japanese Patent Application Publication No. 6-230425 Summary of the Invention [Problem to be solved by the invention]
[0006] In conventional active matrix display devices, resist is used to form laminated wiring. A mask was required for each layer. In particular, when forming pixel electrodes, many layers are stacked. At least the resist mask for forming the pixel electrode and the etching of the film laminated with the pixel electrode are provided. A resist mask for the masking was required, and the number of manufacturing steps was large. The manufacturing costs of such semiconductor devices have not decreased.
[0007] Therefore, in the present invention, the pixel electrode and the film laminated with the pixel electrode are formed with one resist mask. The objective of the present invention is to shorten the manufacturing process. [Means for solving the problem]
[0008] One of the features of the present invention is a thin film transistor on a substrate, and a thin film transistor electrically connected to the thin film transistor. The metal film is connected to a pixel electrode and is in contact with the pixel electrode. The metal film covers the step portion of the pixel electrode. The metal film is in contact with the pixel electrode as shown in FIG. The pixel electrodes are formed on a flat surface.
[0009] This configuration can prevent the pixel electrode from being broken at the step portion. Cutting occurs when a film is formed on a surface with a step, causing the film to crack at the step. Or, the film coverage is poor at the step portion, and the film is not formed in parts. .
[0010] One of the features of the present invention is a thin film transistor on a substrate, and a thin film transistor electrically connected to the thin film transistor. The metal film is flatter than the pixel electrode. The area is small, and the side surface of the metal film is disposed along the side surface of the pixel electrode. The second electrode is located inside the side of the pixel electrode.
[0011] This configuration makes it possible to use the metal film as a part of the light-shielding film, and the position of the light-shielding film This can make alignment easier.
[0012] A thin film transistor on a substrate, a pixel electrode electrically connected to the thin film transistor, A metal film contacting a part of the pixel electrode, and a pixel electrode formed on the metal film. a partition wall exposing a part of the pixel electrode; an electroluminescent layer formed in contact with the partition wall and the pixel electrode; and an electrode on the light-emitting layer. At least one side of the metal film is inclined, and the metal film is a partition wall. A display device characterized in that it is covered.
[0013] This configuration prevents short circuits of light-emitting elements in an electroluminescence display device. It is possible to do so.
[0014] Using one resist pattern, the pixel electrode and the metal film that contacts a part of the pixel electrode are The two patterns, the pixel electrode and the metal film, can be formed using a single resist pattern. Since the display device can be formed using the above method, the manufacturing process can be shortened, and a low-cost display device can be realized. It is possible. Effect of the Invention
[0015] According to the present invention, the number of manufacturing steps can be reduced compared to the conventional method, and the manufacturing cost of the semiconductor device can be reduced. In addition, since the metal film is formed on the pixel electrode, the step portion can be prevented from being damaged. This prevents the pixel electrodes from being broken. A display device can be formed. [Brief description of the drawings]
[0016] [Figure 1] 1 is a cross-sectional view showing a manufacturing process of a semiconductor device according to the first embodiment. [Diagram 2] 1 is a cross-sectional view showing a manufacturing process of a semiconductor device according to the first embodiment. [Diagram 3] 1 is a top view of a semiconductor device according to the first embodiment. [Figure 4] 1 is a cross-sectional view showing a manufacturing process of a semiconductor device according to the first embodiment. [Diagram 5] 1 is a cross-sectional view showing a manufacturing process of a semiconductor device according to a second embodiment of the present invention. [Figure 6] 1 is a cross-sectional view showing a manufacturing process of a semiconductor device according to a second embodiment of the present invention. [Figure 7] 1 is a top view of a semiconductor device according to a second embodiment of the present invention; [Figure 8] 1 is a cross-sectional view showing a manufacturing process of a semiconductor device according to a second embodiment of the present invention. [Figure 9] 1 is a cross-sectional view showing a manufacturing process of a semiconductor device according to a second embodiment of the present invention. [Figure 10] 1 is a cross-sectional view of a semiconductor device according to a second embodiment of the present invention. [Figure 11] 13A and 13B are a top view and a diagram showing a light intensity distribution of an exposure mask (Embodiment 3). [Figure 12] 1 is a top view and a cross-sectional view of an EL display device (Embodiment 4). [Figure 13] 1 is a top view and a cross-sectional view of an EL display device (Embodiment 4). [Figure 14] 11A and 11B are a top view and a cross-sectional view of a liquid crystal display device (Embodiment 5). [Figure 15] 11A and 11B are a top view and a cross-sectional view of a liquid crystal display device (Embodiment 5). [Figure 16] 11A and 11B are a top view and a cross-sectional view of a liquid crystal display device (Embodiment 5). [Figure 17] 11A and 11B are a top view and a cross-sectional view of a liquid crystal display device (Embodiment 5). [Figure 18] 11 is a top view of a liquid crystal display device according to the fifth embodiment. [Figure 19] 1 is a cross-sectional view of a semiconductor device according to the first embodiment. [Figure 20]Diagram of an electronic device (Embodiment 6) [Figure 21] Diagram of a mobile phone (Embodiment 6) DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0017] Hereinafter, an embodiment of the present invention will be described. However, the present invention is not limited to the above embodiment. However, the present invention is not limited to the above-mentioned embodiments, and may be embodied in many different forms without departing from the spirit and scope of the present invention. It will be easily understood by those skilled in the art that the form and details of the present invention may be modified in various ways without departing from the spirit and scope of the present invention. Therefore, the present invention should not be construed as being limited to the description of the present embodiment. The embodiments can be combined as appropriate.
[0018] (Embodiment 1) In this embodiment, a method for forming a top-gate type TFT on a substrate 1 will be described with reference to FIG. The substrate 1 is a light-transmitting substrate, such as a quartz substrate, a glass substrate, or a plastic substrate. The substrate 1 may be a light-shielding substrate, such as a semiconductor substrate, an SOI (Silicon Insulator) substrate, or the like. A silicon on insulator (SiC) substrate may also be used.
[0019] An insulating film 2 is formed as a base film on a substrate 1. The insulating film 2 is a silicon oxide film, Silicon nitride film or silicon oxynitride film (SiO x N y ) or other insulating film. A laminate consisting of at least two of these films is used. Next, an island-shaped semiconductor film is formed on the insulating film 2. Form 3.
[0020] The island-like semiconductor film 3 is formed on the insulating film 2 by sputtering, LPCVD, or plasma CVD. After forming a semiconductor film on the entire surface by a method such as photolithography, a mask formed by a method such as photolithography is formed. The island-shaped semiconductor film 3 is formed from a crystalline semiconductor film. When the semiconductor film is to be formed, a method of forming a crystalline semiconductor film directly on the substrate 1 and a method of forming an amorphous semiconductor film on the substrate 1 are available. There is a method in which a semiconductor film is formed on a substrate and then crystallized by heat treatment to form a crystalline semiconductor film. In the method of the present invention, the heat treatment for crystallization is performed by using a heating furnace, laser irradiation, or laser light. Instead, irradiation with light emitted from a lamp (hereinafter referred to as lamp annealing) or This is done by using them in combination.
[0021] In addition, a thermal crystallization method is used in which nickel or the like is added to an amorphous semiconductor film and then the above-mentioned heat treatment is performed. The crystalline semiconductor film may be formed by a thermal crystallization method using nickel. When a crystalline semiconductor film is obtained by crystallization, a gettering process is performed to remove nickel after the crystallization. It is preferable to carry out the treatment.
[0022] When producing a crystalline semiconductor film by crystallizing it with laser irradiation, continuous wave (CW) :continuous-wave) type laser beam or pulsed type laser beam ( The laser beam that can be used here is a pulsed laser beam. Gas lasers such as Ar laser, Kr laser, and excimer laser, as well as single crystal YAG and YVO 4. Forsterite (Mg2SiO4), YAlO3, GdVO4, or polycrystalline ( Ceramic) YAG, Y2O3, YVO4, YAlO3, GdVO4 with dopants One or more of Nd, Yb, Cr, Ti, Ho, Er, Tm, and Ta are added. Lasers that use materials that are the medium, glass lasers, ruby lasers, and alexandrite lasers One or more of the following lasers: Ti:sapphire laser, copper vapor laser, or gold vapor laser The fundamental wave of such a laser beam and the By irradiating the laser beam with the second to fourth harmonic of the fundamental wave, large grain crystals can be produced. For example, the second harmonic of a Nd:YVO4 laser (fundamental wave 1064 nm) can be obtained. The laser can be used with a C It can be fired in W or pulsed. When firing in CW, Laser power density is 0.01 to 100MW / cm 2 (preferably 0.1 to 10MW / cm 2 ) is necessary. The scanning speed is set to about 10 to 2000 cm / sec. do.
[0023] In addition, single crystal YAG, YVO4, forsterite (Mg2SiO4), YAlO 3. GdVO4 or polycrystalline (ceramic) YAG, Y2O3, YVO4, YAl O3, GdVO4, dopants Nd, Yb, Cr, Ti, Ho, Er, Tm, T Lasers using one or more of the above-mentioned a as a medium, Ar ion lasers, Alternatively, the Ti:sapphire laser can be operated in continuous oscillation mode and can be Q-switched. By performing mode locking, etc., pulse oscillation can be achieved at an oscillation frequency of 10 MHz or more. It is also possible to oscillate a laser beam at a frequency of 10 MHz or more. Between the time when the film is melted by the laser beam and when it solidifies, the next pulse is irradiated onto the semiconductor film. Therefore, unlike the case of using a pulsed laser with a low oscillation frequency, Since the solid-liquid interface can be moved continuously in the scanning direction, the solid-liquid interface can be moved continuously in the scanning direction. Longer crystal grains can be obtained.
[0024] If ceramic (polycrystalline) is used as the medium, it is possible to form the medium into any shape in a short time and at low cost. When using a single crystal, the diameter is usually several mm and the length is several tens of mm. A cylindrical medium of is used, but when using ceramics, a larger one can be made. It is possible.
[0025] The concentration of dopants such as Nd and Yb in the medium that directly contribute to light emission is high even in single crystals. Since the concentration cannot be changed significantly even in the crystal, increasing the concentration can improve the laser output. However, in the case of ceramics, the size of the medium is larger than that of a single crystal. This allows for a significant increase in output.
[0026] Furthermore, in the case of ceramics, it is easy to form a medium having a parallelepiped or rectangular shape. By using a medium with such a shape, it is possible to make the oscillating light zigzag inside the medium. By propagating the light, the oscillation path can be made longer. This results in greater amplification and higher output. In addition, the laser beam emitted from the medium with such a shape can be The cross-sectional shape of the beam when it is emitted is square, so compared to a round beam, it has a linear beam. The laser beam emitted in this way can be shaped using an optical system. This makes it easy to produce a linear beam with a short side length of 1 mm or less and a long side length of several mm to several meters. In addition, by irradiating the medium with the excitation light uniformly, the linear beam The energy distribution is uniform along the long side.
[0027] By irradiating the semiconductor film with this linear beam, the entire surface of the semiconductor film can be more uniformly annealed. If uniform annealing is required up to both ends of the linear beam, It may be necessary to provide slits on both ends of the beam to block the areas where energy is attenuated.
[0028] The thus obtained linear beam having a uniform intensity is used to anneal the semiconductor film, When an electronic device is manufactured using the semiconductor film, the characteristics of the electronic device are excellent and uniform. .
[0029] Next, if necessary, a small amount of impurity element (boron) is added to control the threshold voltage of the TFT. In this case, the doping of the semiconductor film is performed without mass separation. The method uses ion doping with excitation current.
[0030] The island-shaped semiconductor film 3 is formed to a thickness of 25 to 80 nm (preferably 30 to 70 nm). The material of the semiconductor film is not limited, but is preferably silicon or silicon germanium. It is preferable to form it from a (SiGe) alloy.
[0031] Then, a gate insulating film 4 is formed so as to cover the island-like semiconductor film 3. Examples of the film include a thermal oxide film, a silicon oxide film, a silicon nitride film, and a silicon oxynitride film. The gate insulating film 4 in contact with the island-shaped semiconductor film 3 is an oxidized layer or a laminated structure. A silicon film is preferable because when the gate insulating film 4 is a silicon oxide film, the interface with the island-like semiconductor film This is because the number of trap levels in the gate electrode is reduced. In this case, the gate insulating film in contact with the gate electrode is preferably a silicon nitride film. This is because the silicon film does not oxidize Mo.
[0032] Here, the gate insulating film 4 is a 115 nm thick oxynitride film formed by plasma CVD. A silicon film (composition ratio: Si=32%, O=59%, N=7%, H=2%) is formed.
[0033] Next, a conductive layer is formed on the gate insulating film 4 by a photolithography method or the like. The conductive layer is shaped using the mask to form a gate electrode 5. The elements are Mo, Ti, W, Al, Nd, Cr, and alloys of these elements. The gate electrode 5 may be formed by laminating layers of these elements or alloys of these elements. Next, the island-shaped semiconductor is formed by using the gate electrode 5 or the resist as a mask. The semiconductor film 3 is doped with an impurity element to form a channel forming region 8 and a source region and a drain region. The impurity region 9 is formed as a region.
[0034] Then, a first interlayer insulating film 6 is formed using silicon nitride. The added impurity element is activated and hydrogenated. Note that the first interlayer insulating film 6 is not formed. It's good to come.
[0035] Next, a light-transmitting inorganic material (silicon oxide, silicon nitride, silicon oxynitride, etc.) is ) or low-dielectric-constant organic compound materials (photosensitive or non-photosensitive organic resin materials) are used. The second interlayer insulating film 7 is formed by using a material containing siloxane. Siloxane has a skeleton structure formed by the bond between silicon (Si) and oxygen (O). The material is made of a structure that contains an organic group (e.g., an alkyl group) that contains at least hydrogen as a substituent. A fluoro group may be used as a substituent. As the substituent, an organic group containing at least hydrogen and a fluoro group may be used. The insulating film 7 may have a laminated structure.
[0036] Next, a mask made of resist is formed using a photomask, and Then, the first interlayer insulating film 6, the second interlayer insulating film 7, and the gate insulating film 4 are selectively etched. Then, contact holes are formed, and the resist mask is removed.
[0037] Then, a conductive film is formed on the second interlayer insulating film 7 by a sputtering method or a printing method. The conductive film may be a transparent conductive film or may have reflectivity. In the case of a transparent conductive film, for example, Indium tin oxide (ITO) film, which is a mixture of indium oxide and tin oxide, Indium tin silicon oxide (ITSO) film, which is a mixture of indium tin oxide (ITO) and silicon oxide, Indium zinc oxide (IZO) film, zinc oxide film, or acid IZO is a film of ITO with 2 to 20 wt% zinc oxide. Transparent conductive material formed by sputtering using a target containing (ZnO) It is a fee.
[0038] A transparent conductive film 10 is formed on the second interlayer insulating film 7, and then a metal film 1 is formed on the transparent conductive film 10. The transparent conductive film 10 and the metal film 11 can be formed successively by sputtering. .
[0039] Since transparent conductive films are often made of materials with high resistance, the metal film 11 has a lower resistance than the transparent conductive film. For example, Ti, Mo, Ta, Cr, W, Al, etc. can be used. In addition, there are two-layer structures in which Al is laminated with Ti, Mo, Ta, Cr, or W; Alternatively, a three-layer laminate structure may be formed by sandwiching the above between metals such as Ti, Mo, Ta, Cr, and W. After a resist film is applied to the entire surface of the metal film 11, the resist film is exposed using an exposure mask shown in FIG. Do light.
[0040] When an ITO film is used as the transparent conductive film, a process of heat treating the ITO film to crystallize it is required. In that case, the ITO film is formed by sputtering, and after baking, the metal film 11 is formed. If an ITSO film is used, the crystallization process is unnecessary, so the number of steps can be reduced.
[0041] In FIG. 1A, the exposure mask has light-shielding portions 12a and 12b that block exposure light, The semi-transparent portion 13 is provided with a semi-transparent film 19, and the exposure light is partially transmitted through the semi-transparent portion 13. The light intensity of the light is reduced. The light shielding portions 12a and 12b are formed by laminating a metal film 20 on a semi-permeable film 19. The width of the light-shielding portion 12b is denoted as t1, and the width of the semi-transparent portion 13 is denoted as t2. Although an example in which a semi-transparent film is used for the semi-transparent portion has been shown, the present invention is not limited to this, and the semi-transparent portion may be any other suitable material that can reduce the light intensity of the exposure light. Any material that can reduce the reflection may be used. Also, a diffraction grating pattern may be used in the semi-transparent portion.
[0042] When the resist film is exposed using the exposure mask shown in FIG. A light region 14a and an exposed region 14b are formed. During exposure, light is blocked by the light-shielding portions 12a and 12b. By passing through the semi-transparent portion 13, the exposed area 14b shown in FIG. 1(A) is formed. It is done.
[0043] Then, when development is performed, the exposed region 14b is removed, and a large The resist pattern 15a has two different thicknesses, and the resist pattern 15b has a substantially uniform thickness. Turns 16a are obtained on the metal film 11. The resist pattern 15a has a thick region and The region having a smaller thickness than the region having a smaller thickness is provided with a smaller exposure energy or The film thickness can be adjusted by adjusting the transmittance of the semipermeable membrane 19. The resist pattern 5a is asymmetric, whereas the resist pattern 16a is symmetric.
[0044] Next, the metal film 11 and the transparent conductive film 10 are etched by dry etching. Dry etching is performed using ECR (Electron Cyclotron Resonanc e) and ICP (Inductive Coupled Plasma) This is done using a dry etching device that uses a laser source.
[0045] In this example, an ICP type etching device is used, but the present invention is not limited to this. For example, parallel plate type etching equipment, magnetron type etching equipment, ECR type etching equipment A lithography apparatus or a helicon type etching apparatus may also be used.
[0046] The metal film 11 and the transparent conductive film 10 may be etched by wet etching. However, dry etching is preferable because it is suitable for fine processing. In addition, since the materials of the metal film 11 and the transparent conductive film 10 are different from those of the second interlayer insulating film 7, Even if dry etching is performed, the second interlayer insulating film 7 is not easily damaged by the metal film 11 and the transparent conductive film 10. In order to further increase the etching selectivity, the second layer is At least the uppermost layer of the inter-insulating film 7 may be made of a silicon nitride film.
[0047] Thus, as shown in FIG. 1C, a transparent conductive film 17a and a gold film are formed on the second interlayer insulating film 7. A pattern formed by laminating a transparent conductive film 18a and a metal film 18b. A pattern consisting of
[0048] Next, the resist patterns 15a and 16a are ashed or etched (FIG. 2( A) This process etches the thin areas of the resist pattern 15a. At the same time, the entire film of the resist patterns 15a and 16a is increased by the thickness of the thin film region. The thickness of the resist pattern 15b is also reduced. Then, resist patterns 15b and 16b are formed. Since the resist patterns 5a and 16a are etched not only in the thickness direction but also in the width direction, The width of the metal films 17b and 18b is smaller than the width of the transparent conductive films 17a and 18a. Therefore, the side surfaces of the resist patterns 15b and 16b are in contact with the underlying metal film and The side surfaces of the resist patterns 15b and 16b are recessed from the side surfaces of the transparent conductive film. In FIG. 2B, the resist pattern 15b is asymmetric. 16b is symmetrical.
[0049] Next, the metal film 18b is etched using the resist pattern 15b, and the metal film 18c is At this time, in order to prevent the transparent conductive film 18a from being unnecessarily etched, Thus, it is preferable that the material of the metal film 18b has a high selectivity with respect to the transparent conductive film 18a. For example, if the material of the transparent conductive film 18a is ITSO, the material of the metal film 18b is Ti. , Mo, Cr, Al, etc. are preferable, and the metal film 18b may have a laminated structure made of these materials. In addition, the pattern is smaller than that of the transparent conductive film 18a, that is, the planar area of the metal film is smaller. On the other hand, the metal film 17b is also etched using the resist pattern 16b. As a result, a metal film 17c having a smaller planar area than the transparent conductive film 17a is formed.
[0050] The etching of the metal films 17b and 18b in FIG. 2(A) and FIG. 2(B) is performed by dry etching. This can be done by either dry etching or wet etching, but in FIG. 2(B) dry etching is used. In the example shown, the metal films 17c and 18c are formed by dry etching. In this case, the side surface of the metal film 18c in the cross section becomes asymmetric. This is because the shape of the metal film 18c is asymmetric and reflects the asymmetric shape. The film 18c has a cross-sectional shape in which one side surface is more inclined than the other side surface. The metal film 7c is formed so that its side faces coincide with the side faces of the resist pattern 16b. c has one side on the extension of one side of the resist pattern 15b, and the other side corresponds to the other side of resist pattern 15b.
[0051] When the metal films 17b and 18b are wet-etched, the etching proceeds isotropically. Therefore, a metal film smaller than the resist patterns 15b and 16b is formed. FIG. 4A shows the state where the metal films 17b and 18b are etched. Then, the metal films 17d and 18d are formed by wet etching. ) is the same as
[0052] The sides of the resist patterns 15b and 16b do not coincide with the sides of the metal films 17d and 18d. Therefore, even if the same resist patterns 15b and 16b are used as a mask, the etching can be performed more efficiently than by dry etching. By using wet etching, smaller metal films 17d and 18d are formed. do.
[0053] FIG. 4B shows a case where the metal film 17d is formed of a three-layer laminate. The metal film 17d has a laminated structure in which an aluminum film 92a is sandwiched between Ti films 91a and 93a. The side surfaces of the metal film 17d and the resist pattern 16b do not coincide with each other. The aluminum film 92b is sandwiched between Ti films 91b and 93b. The side surface of the resist pattern 15b does not coincide with that of the resist pattern 15d.
[0054] In FIGS. 4A and 4B, the transparent conductive films 17a and 18a are formed by dry etching. Therefore, the side surface has an angle θ1 that is nearly perpendicular or close to 90 degrees with respect to the substrate surface. On the other hand, when the metal films 17d and 18d are formed by wet etching, the isotropic etching Due to the shaping, the side surface has an acute angle θ2 with respect to the substrate surface. Comparing the angle θ1 of the side surface of the film with the angle θ2 of the side surface of the metal film, θ1>θ2. The angle θ1 is the inclination angle of the transparent conductive film side surface with respect to the surface of the substrate 1, and the angle θ2 is is the inclination angle of the side surface of the metal film with respect to the surface of the substrate 1, and both θ1 and θ2 are in the range of 0° to 90°. It is within range.
[0055] When the metal film has a layered structure as shown in Figure 4(B), the etching speed differs for each layer. As a result, the angles of the side faces of each layer relative to the substrate surface may differ. Therefore, when the metal film is laminated, the side of the bottom layer of the film relative to the substrate surface is Let the angle be θ2.
[0056] In addition, the side surfaces of the metal films 17d and 18d and the transparent conductive films 17a and 18a In some cases, the surface is not smooth and has bumps. In that case, the angles θ1 and θ2 are For example, roughly draw straight or curved lines on the uneven side surface, and then The angles θ1 and θ2 can be determined using the above formula. Also, based on the uneven side surface, It is possible to take multiple angles θ1 and θ2 and set the average values to angles θ1 and θ2. Yes, you can. Just use the method that makes the most sense.
[0057] From the above, the etching method can be selected from either the dry etching method or the wet etching method. The metal films 17c and 18c or the metal films 17d and 18d are formed by the method. Even if the insulating layer is formed by the etching method, the insulating layer has a side surface recessed from the side surfaces of the transparent conductive films 17a and 18a. The metal film 17c and the metal film 18c or the metal film 17d and the metal film 18d are formed. The metal film 17c or 17d has a smaller planar area than the transparent conductive film 17a, and The metal film 18c or 18d is formed with a smaller planar area than the film 18a. The first is a resist pattern 15a which is a mask for forming the transparent conductive films 17a and 18a. , 16a, and the resist patterns 15b, 16b which are masks for forming a metal film. This is because they are different in size, with resist patterns 15b and 16b being smaller.
[0058] Thereafter, the resist patterns 15b and 16b are removed (FIG. 2(C)). A wiring or electrode made of a conductive film 17a and a metal film 17c, a transparent conductive film 18a and a metal film 18c The transparent conductive film 18a functions as a pixel electrode. When the resist patterns 15b and 16b are removed from (A) and (B), the transparent conductive film 17a and a wiring or electrode made of the metal film 17d, and a wiring made of the transparent conductive film 18a and the metal film 18d. Or an electrode is formed.
[0059] When the metal film 18b is etched using the resist pattern 15b as a mask, Part of the surface of the transparent conductive film 18a is slightly etched. When forming the film 18c, it is difficult to obtain a selectivity with respect to the transparent conductive film below. A part of the surface of the film 18a is easily etched. Therefore, the transparent conductive film 18a in FIG. When comparing the thickness a and thickness b of the metal film 18, the thickness a is smaller than the thickness b. c or the average thickness of the transparent conductive film 18a in the portion not overlapping with the metal film 18d. The thickness b is the thickness of the transparent conductive film 18a at the bottom of the contact hole that reaches the impurity region 9. say.
[0060] A light-emitting device in which a light-emitting element is stacked on the TFT shown in FIG. 2(C) and emits light toward the substrate 1. When the transparent conductive film 18a is formed, the thin film thickness of the transparent conductive film 18a increases the transmittance, thereby providing a bright display. Therefore, it is preferable that the film thickness a is thin. When etching the metal film 18b as a mask, the surface of the transparent conductive film 18a can be etched. This makes it possible to remove dirt from the surface and prevent short circuits in the light-emitting element caused by dirt. Cut.
[0061] In the present embodiment, the metal film 18c has one side inclined. When used in a display device, rubbing is performed from the inclined side surface of the metal film 18c. Then, rubbing can be smoothly performed on the side surface of the metal film 18c. When rubbing is performed from the direction in which the side of c is vertical, the vertical side part is strained against the rubbing cloth. Rubbing may be incomplete due to the influence of laser beams, resulting in incomplete alignment. Therefore, it is preferable to perform rubbing from the side where the side surface of the metal film 18c is inclined.
[0062] In addition, as shown in Figure 4, the metal with inclined sides was removed by wet etching. When forming the films 17d and 18d, rubbing can be performed smoothly from either direction. It is more effective.
[0063] FIG. 3 shows a top view of FIG. 2(C). FIG. 2(C) is a cross-sectional view taken along line AA' in FIG. 3. As can be seen from FIG. 3, the wiring or the like is made of a laminate of a transparent conductive film 17a and a metal film 17c. The electrodes function as the source and drain electrodes of the TFTs, and also as source wiring. The wiring or electrodes made of the transparent conductive film 18a and the metal film 18c function as a TFT. The pixel electrode also functions as a source electrode or a drain electrode of the pixel electrode. In the second embodiment, the portion of the transparent conductive film 18a that does not overlap with the metal film 18c functions as a pixel electrode and transmits light. The capacitance wiring 21 is formed from the same layer as the gate electrode 5. The wiring 21 overlaps with the transparent conductive film 18a to form a capacitance. The side surface of the metal film 17c may be formed of a layer different from that of the transparent conductive film 17a. The side of the metal film 18c does not coincide with the transparent conductive film 17a, but is located inside the side of the transparent conductive film 17a. The side of the transparent conductive film 18a is not aligned with the side of the transparent conductive film 18a, but is located inside the side of the transparent conductive film 18a. The same applies to the relationship between the metal film 17d and the transparent conductive film 17a, and the relationship between the metal film 18d and the transparent conductive film 18a. It is.
[0064] In this embodiment, a transparent conductive film that functions as a pixel electrode is formed on a flat surface. This is extremely beneficial in terms of preventing the transparent conductive film from being broken. When the metal film 18c is formed, the surface of the underlying transparent conductive film 18a exposed from the metal film 18c is also slightly etched. Therefore, the transparent conductive film 18a is formed on a surface having a step. If the thickness of the conductive film is not uniform, the etching for forming the metal film 18c may result in the thin conductive film being etched away. The transparent conductive film may be etched, causing the transparent conductive film to break. This can cause light leakage at the broken parts, or the area of the pixel electrode can become smaller, resulting in a lower aperture ratio. Therefore, the part of the transparent conductive film 18a exposed from the metal film 18c is not flat. For this purpose, it is preferable to form the second interlayer insulating film 7 with an organic material and to form the second interlayer insulating film 7 with a flat surface. It is preferable to form the second interlayer insulating film having the following structure.
[0065] When a metal film and a conductive film are laminated according to the present invention, the conductive film is positioned below and in contact with the metal film. However, in areas with large steps, the conductive film does not necessarily contact the bottom of the metal film. This is because there is a possibility that the conductive film may be broken due to the step. Therefore, in the portion of the contact hole that reaches the impurity region 9 in FIG. It is good to place the membrane.
[0066] FIG. 19 shows a state in which the conductive film is broken at the contact hole. Contact hole Due to the inclination of the side surface, the conductive films 94 and 95 are partially cut. If metal films 96 and 97 are formed on the conductive films 94 and 95 in the contact hole portions, the transparent Even if the conductive film is cut, the cut conductive film can be electrically connected via the metal film. In this case, the metal films 96 and 97 are in contact with the second interlayer insulating film 7 on the side of the contact hole. In addition, the conductive film in the contact hole does not function as a pixel electrode. Therefore, there is no problem even if the metal film is left on the upper portion. Even if the transparent conductive film is broken at the contact hole, the transparent conductive film can be maintained by the metal film formed on top. This can compensate for the electrical connection of the conductive film and prevent display defects.
[0067] In addition, even in the portion where the conductive film has a step due to the capacitance wiring 21 in FIG. 3, a metal is formed on the conductive film. Even if the conductive film is cut due to a step, the conductive film will remain in the same state through the metal film. Since the two elements can be electrically connected, it is possible to reliably form a capacitance.
[0068] The shape of the transparent conductive film 18a in FIG. 3 is an example, and other shapes may be used. For example, by giving it a comb-like edge, it is possible to use the IPS (In-Plane-Switching) method. The pixel electrodes are used in the FFS (Fringe Field Switching) method. By inserting slits, MVA (Multi-domain Vertical Alignment) can be achieved. Alignment) method, PVA (Patterned Vertical Alignment) method The pixel electrodes can be used in a photoelectron stimulating (PES) system.
[0069] From the above, the transparent conductive film and the metal film can be formed using a single resist pattern. The number of manufacturing steps can be reduced. In addition, the transparent conductive film can be used as wiring or electrodes. However, by laminating a metal film, the resistance can be reduced and the conductivity can be increased.
[0070] During the etching of the transparent conductive film 10 and the metal film 11 from the state shown in FIG. Naturally, the resist patterns 15a and 16a are also etched, and the resist patterns 15b and 16 If the result is b, remove the resist pattern by ashing or etching. The process of forming 15b and 16b may be omitted.
[0071] In this embodiment, a top-gate TFT having an island-shaped semiconductor film made of a crystalline semiconductor film is used. Although the embodiment has been described using a bottom-gate TFT, this embodiment can also be applied to a bottom-gate TFT made of a crystalline semiconductor film. In this embodiment, the island-shaped semiconductor film serves as a source region and a drain region. It has an impurity region 9 and a channel forming region 8, but also has a low concentration impurity region, an offset It may have a to region, etc.
[0072] (Embodiment 2) This embodiment will be described with reference to FIG. The types, methods of forming each layer, and materials thereof can be referred to in the first embodiment.
[0073] An insulating film 402 is formed as a base film on a substrate 401. Note that the base film is not necessary. Next, a conductive layer is formed over the insulating film 402 by a photolithography method or the like. The conductive layer is processed using the mask to form a gate electrode 403 .
[0074] A gate insulating film 404 is formed so as to cover the gate electrode 403. The material of the amorphous semiconductor film is not limited, but it is preferably silicon. It is recommended to form the amorphous silicon layer using silicon germanium (SiGe) alloy. A conductive layer is formed on the amorphous semiconductor film. For example, an amorphous silicon film containing phosphorus is used for the conductive layer. Then, a mask formed by photolithography or the like is used to The shape of the amorphous semiconductor film and the conductive layer is processed to form an island-shaped semiconductor film 405 and a conductive layer 406. do.
[0075] A transparent conductive film 407 and a metal film 408 are laminated on the conductive layer 406. A conductive layer having reflectivity may be used instead of the transparent conductive film. The transparent conductive film material shown in is usable. Next, a resist is applied to the entire surface of the metal film 408. After the film is applied, exposure is performed using the exposure mask shown in FIG. 5(A).
[0076] In FIG. 5A, the exposure mask has light-shielding portions 409a and 409b and a semi-transparent portion 410. The semi-permeable portion 410 may be a diffraction pattern or a semi-permeable membrane. When the resist film is exposed using the exposure mask shown in FIG. A light region 412 is formed. Then, development is performed, and as shown in FIG. 5(B), a resist pattern is formed. The resist pattern 414a is exposed at the light-shielding portion 409b. The exposed and developed area 422 (the left side of the dashed line in the resist pattern 414a) and the semi-transparent area 423 are The area 423 exposed and developed in the transparent portion 410 (the area to the right of the dashed line in the resist pattern 414a) side part).
[0077] Next, the metal film 408 and the transparent conductive film 407 are etched by dry etching. As shown in FIG. 5C, the transparent conductive film 415 and the metal film 416 are laminated. A pattern formed by laminating a transparent conductive film 419 and a metal film 420 is formed. This etching may be performed by wet etching. Dry etching is preferable because dry etching is suitable for the metal film 40. 8 and the transparent conductive film 407, and the gate insulating film 404 are made of different materials. A large etching selectivity can be obtained even when the etching is performed with the etchant. Therefore, at least the uppermost layer of the gate insulating film 404 may be formed of a silicon nitride film.
[0078] Next, as shown in FIG. 6(A), the resist patterns 413a and 414a are removed by ashing or This process removes the region 423 of the resist pattern 414a. The thickness of the region 422 of the resist pattern 414a is d2. The resist pattern 413a also becomes thinner, forming a resist pattern 414b. The resist pattern 413b is formed by ashing only d2. Therefore, the width of the resist patterns 413b and 414b is The width of the resist pattern 413 is smaller than the width of the transparent conductive films 415 and 419. b, the side of 414b does not match the side of the underlying metal film and transparent conductive film, The side surfaces of the resist patterns 413b and 414b are recessed. The angles that the two side surfaces make with respect to the substrate surface are different from each other. The angles that the side surfaces make with respect to the substrate surface are approximately the same.
[0079] Next, the metal film 416 is etched using the resist pattern 414b to form the metal film 4 21 is formed. In addition, the metal film 420 is etched using the resist pattern 413b. Then, the metal film 424 is formed (FIG. 6(B)). At this time, the transparent conductive film 415 is unnecessarily etched. The metal films 424 and 421 are thicker than the transparent conductive films 419 and 415. The transparent conductive films 415 and 419 are used as masks to form a conductive layer. The semiconductor film 406 is etched to form conductive layers 417 and 418. One end of the transparent conductive film 419 and one end of the conductive layer 417 are also slightly etched. One end of the transparent conductive film 415 and one end of the conductive layer 418 are aligned with each other. The metal films 421 and 424 are formed in the same process.
[0080] At the same time as etching to form the metal films 421 and 424, the conductive layer 406 is Etching may also be performed.
[0081] Then, the resist patterns 413b and 414b are removed, and the transparent conductive film 419 and the metal The wiring or electrode is made of the film 424, the metal film 421 and the transparent conductive film 415. The transparent conductive film 415 functions as a pixel electrode (FIG. 6(C)).
[0082] The conductive layers 417 and 418 can be formed simultaneously with the etching shown in FIG. 5(C). However, as shown in FIG. 6, it is preferable to perform this during or after the formation of the metal films 424 and 421. This is because if the island-shaped semiconductor film is exposed at the stage of FIG. When forming 21, the island-shaped semiconductor film may be further etched. It is.
[0083] The etching in FIG. 6(B) may be dry etching or wet etching. When dry etching is used, the cross-sectional shape of the metal film 421 is as shown in FIG. 6(B) and (C). The shape of the metal film 42 is asymmetrical, reflecting the shape of the resist pattern 414b. 1 has a cross-sectional shape in which one side is more inclined than the other side, and one side is The other side of the resist pattern 414b is an extension of the resist pattern 414b. The metal film 424 has a side surface that matches the other side surface of the resist pattern 413b. It is formed to match the sides.
[0084] The case where the metal films 421 and 424 are formed by wet etching will be described with reference to FIG. Instead of the metal films 421 and 424 formed by dry etching, If formed, they are called metal films 425 and 426 .
[0085] In the case of wet etching, resist patterns 413b and 414 are formed as shown in FIG. Metal films 425 and 426 smaller than b are formed, and resist patterns 413b and 414 are formed. The side of the metal film 425, 426 does not coincide with the side of the resist pattern 4b. Even if 13b and 414b are used as a mask, wet etching is used rather than dry etching. In addition, as in Figure 4, the wet method produces a metal film with a smaller planar area. When a metal film is formed by etching, the angle θ1 on the side surface of the transparent conductive film 415, 419 When comparing the angle θ1 at the side surface of the metal films 425 and 426 with the angle θ2, θ1>θ2 is satisfied. The angle θ1 is the inclination angle of the transparent conductive film side surface with respect to the surface of the substrate 401. The angle θ2 is the inclination angle of the side of the metal film with respect to the surface of the substrate 401. The angle is within the range of 0° to 90°. Also, the metal films 425 and 426 have a laminated structure as shown in FIG. In the case of this structure, the angle that the side of the bottom layer of the film makes with the substrate surface is defined as θ2.
[0086] In the case of wet etching, the conductive layer 406 is etched in the same manner as in FIG. This may be done simultaneously with etching or after forming the metal films 425 and 426 in FIG. 6(B). good.
[0087] Regardless of the etching method used to form the metal film, the side surface of the metal film is larger than the side surface of the transparent conductive film 419. The metal film 425 or the metal film 424 is recessed from the side of the transparent conductive film 415. In other words, the metal film 421 or the metal film 426 is formed. The metal film 424 or 425 has a smaller planar area than the transparent conductive film 415. 21 or 426 are formed.
[0088] Then, the resist patterns 413b and 414b are removed, and the transparent conductive film 419 and the metal The wiring or electrode is made of the film 424, the metal film 421 and the transparent conductive film 415. (FIG. 6(C)) The resist patterns 413b and 414b are removed from FIG. For example, a wiring or electrode made of a transparent conductive film 419 and a metal film 425, a transparent conductive film 415 and a metal A wiring or electrode is formed from the metal film 426 .
[0089] The resist pattern 414a having regions of different thicknesses according to the present invention is used to form a metal film 42 When the metal film 421 is formed, the transparent conductive film 415 is laminated. Part of the surface of 415 is slightly etched. In particular, the metal film 42 is slightly etched by dry etching. When forming the transparent conductive film 1, it is difficult to obtain a selectivity with the transparent conductive film 415 below. A part of the surface of the film 415 is easily etched. Therefore, the transparent conductive film 415 in FIG. The thickness a (thickness of the transparent conductive film 415 exposed from the metal film 421) and the thickness c (gate insulating film When comparing the thickness of the transparent conductive film in contact with the metal film 421 and the film thickness a, it is found that the thickness a is smaller than the thickness c. Note that film thickness a and film thickness c refer to average film thicknesses.
[0090] When a light-emitting device is formed by stacking a light-emitting element on the TFT of FIG. 6(C), the thickness a<thickness c In the case of a light emitting device that emits light in the direction of the substrate 401, the thickness The thinness of a allows for bright display. In addition, the surface of the transparent conductive film 415 can be etched. Therefore, dust on the surface can be removed and short-circuiting of the light emitting element can be prevented.
[0091] In this embodiment, the metal film 421 has one side inclined. When used in a display device, rubbing is performed from the inclined side of the metal film 421. Then, rubbing can be smoothly performed on the side surface of the metal film 421. If rubbing is performed from a direction in which the side of 1 is vertical, the vertical side part will be strained against the rubbing cloth. Rubbing may be incomplete due to the influence of laser beams, resulting in incomplete alignment. Therefore, rubbing is preferably performed from the side of the metal film 421 where the side surface is inclined.
[0092] In addition, as shown in Figure 8, the metal with inclined sides was removed by wet etching. When forming the films 425 and 426, rubbing can be performed smoothly from either direction. It is more effective.
[0093] FIG. 7 shows a top view of FIG. 6(C). FIG. 6(C) is a cross-sectional view taken along line AA' in FIG. As shown in FIG. 7, the wiring or electrode formed by laminating the transparent conductive film 419 and the metal film 424 is It functions as a source electrode or a drain electrode, and also as a source wiring. The wiring or electrode made of the transparent conductive film 415 and the metal film 421 is a source electrode or a drain electrode of the TFT. Strictly speaking, the metal film 421 and the pixel electrode The portion of the transparent conductive film 415 that does not overlap functions as a pixel electrode. The capacitance wiring 430 formed from the same layer as the transparent conductive film 415 overlaps with the transparent conductive film 415 to form a capacitance. The capacitance wiring 430 may be formed from a layer different from that of the gate electrode. The side of the film 424 does not match the side of the transparent conductive film 419, but is on the inside of the side of the transparent conductive film 419. The side of the metal film 421 does not match the side of the transparent conductive film 415. The relationship between the metal film 425 and the transparent conductive film 419 described in FIG. The relationship between the film 426 and the transparent conductive film 415 is similar.
[0094] In addition, the step caused by the capacitance wiring 430, the gate electrode 403, or the island-like semiconductor film 405 The transparent conductive film 415 formed on the substrate is covered with a metal film 421, which functions as a pixel electrode. This is beneficial in preventing the transparent conductive film from being cut off. When the transparent conductive film 415 is formed, the transparent conductive film 415 is also etched to some extent, so that the thickness of the transparent conductive film is uniform. Otherwise, the transparent conductive film will be broken during the etching process. It is preferable to use a transparent conductive film portion on a flat surface, where the film thickness is easily formed uniformly, as the electrode. For this purpose, the metal film 415 is formed so as to cover the transparent conductive film 415 located on the surface having the step. Then, the transparent conductive film 415 on the stepped surface is etched. It will not break or be cut off.
[0095] In addition, in order to cover the transparent conductive film 415 on the step surface with the metal film 421, The thickness of the region 423 of the resist pattern 414a is d2, and the thinnest film of the region 422 is d3. When the thickness is d1, it must be at least d1>d2. This is the same as the thickness in Figure 6(A). During ashing of the resist, the thickness d2 is ashed away, and the total thickness of the resist is d2. However, even if the thickness is reduced by d2 due to this ashing, the thickness of the film in the region 422 is This is because the resist must remain. In the section 414a, the thickness d1 of the thinnest part of the region 422 is It is preferable that the thickness is thicker than the thickness d2.
[0096] By the above steps, a bottom-gate type TF having an island-shaped semiconductor film made of an amorphous semiconductor film is obtained. It is possible to form a T by laminating a metal film while using a transparent conductive film as wiring or an electrode. By doing so, it is possible to make the resistance low and the conductivity high. Since there is no need to provide a special resist pattern for this purpose, the number of steps can be reduced.
[0097] As another TFT configuration of this embodiment, a TFT configuration having a channel protection film is This is shown in FIG. 9(A). In the TFT in FIG. 9(A), the same elements as those in FIG. 5 to FIG. 8 are denoted by the same reference numerals. Detailed description will be omitted.
[0098] The process is the same as that shown in FIG. 5(A) until an island-shaped semiconductor film 405 is formed on a substrate 401. An insulating film such as a silicon nitride film is formed on the insulating film, and the insulating film is shaped by etching to form island-shaped semiconductor layers. A channel protection film 601 is formed near the center on the conductive film 405. Then, A conductive layer 406, a transparent conductive film 407, and a metal film 408 are formed in this order to cover the substrate 601. Then, a resist film is applied to the entire surface of the metal film 408. Then, an exposure mask having a semi-transparent portion is used. After the resist film is exposed using the ion beam, it is developed to form resist patterns 413a and 414a. do.
[0099] Next, the resist patterns 413a and 414a are used for dry etching. The conductive layer 417, the conductive layer 418, the transparent conductive film 415, the transparent conductive film 419, and the metal film 416, and a metal film 420 is formed. The transparent conductive film 415 functions as a pixel electrode (FIG. 9( B) The channel protection film 601 is formed by forming the island-shaped semiconductor This serves as a protective film to prevent the film 405 from being etched.
[0100] Next, the resist patterns 413a and 414a are ashed to form a resist pattern 4 13b and 414b are formed (FIG. 9(C)). Then, the metal films 420 and 416 are etched to form metal films 424 and 421 (FIG. 9( FIG. 9(D) shows a case where metal films 424 and 421 are formed by dry etching. The metal films 425 and 426 shown in FIG. 8 are formed by wet etching. In this case, the shape of the ends of the metal film and the transparent conductive film is the same as that described in FIG. .
[0101] The TFT having the channel protection film 601 has the following effects. In the etching process of the transparent conductive film 407 and the metal film 408 shown in FIG. Therefore, there is no risk of the island-shaped semiconductor film being etched when the transparent conductive film and the metal This increases the degree of freedom in the film etching process, allowing etching to be performed under optimal conditions. Furthermore, the island-shaped semiconductor film 405 can be thinned. This allows the driver TFT to have improved characteristics. It is ideal for active matrix organic light emitting diodes, which require a TFT to pass current.
[0102] Another TFT structure is shown in Figure 10. This structure is a boron formed of a crystalline semiconductor film. The TFT is a Tom gate type TFT. The process is the same as A). Then, a crystalline semiconductor film is formed on the gate insulating film. A crystalline semiconductor film may be formed on the gate insulating film, or an amorphous semiconductor film may be formed on the gate insulating film as in the first embodiment. After the formation, the semiconductor film may be crystallized to form a crystalline semiconductor film. The semiconductor film 405 is selectively doped with impurities. The island-shaped semiconductor film 405 is doped with a pair of impurity regions 602 and a channel forming region 6 After forming an interlayer insulating film 604 on the island-shaped semiconductor film 405, an interlayer insulating film 603 is formed. A contact hole reaching the impurity region 602 is formed in the transparent conductive film 604. A metal film is laminated on top of the photoresist. The photoresist is exposed with the photomask shown in FIG. 5(A) and developed. The transparent conductive film 419 and the metal film 424 are etched using a resist pattern. and an electrode or wiring made of the metal film 421 and the transparent conductive film 415 is formed. In the configuration of FIG. 10, when the interlayer insulating film 604 is made of an organic resin material, the interlayer insulating film 6 04 has a flat surface. In other words, the transparent conductive film 415 can be formed on a flat surface. It is possible to prevent the transparent conductive film 415 from being cut during etching to form the metal film 421. can.
[0103] The TFT shown in FIG. 10 has impurity regions other than the pair of impurity regions 602. That's fine.
[0104] 9 and 10, etching for forming metal films 421 and 424 is performed. The shape characteristics of the metal film due to the method are the same as those described above. Instead, wet etching is used to form metal films 425 and 426 in the shape shown in FIG. Alternatively, a metal film having a laminated structure may be used. Although a transparent conductive film is used as the conductive film, a reflective conductive film may also be used. As the material, the materials shown in the first embodiment can be used.
[0105] This embodiment can be freely combined with embodiment 1 to the extent possible. .
[0106] (Embodiment 3) In this embodiment, the exposure mask used in the first and second embodiments will be described with reference to FIG. 11(A) to 11(C) show the light-shielding portion 12b and the semi-transparent portion of the exposure mask shown in FIG. 1 or FIG. The width of the light-shielding portion 12b of the exposure mask is indicated as t1, and the width of the semi-transparent portion 13 is indicated as It is shown as t2.
[0107] The semi-transparent portion 13 can be provided with a diffraction grating pattern. A diffraction grating pattern having a slit portion consisting of a plurality of slits below the resolution limit of the optical device is shown. A diffraction grating pattern is a pattern that has at least one slit, dot, or other pattern. When multiple slits, dots, etc. are arranged, The fine patterns may be arranged periodically or non-periodically. By using the turn, it is possible to modulate the actual exposure amount, and the exposed It is possible to adjust the film thickness after the resist is developed.
[0108] The direction in which the slits of the slit portion extend is the same as that of the light shielding portion 303, as in the slit portion 301. It may be parallel to one side, or may be perpendicular to one side of the light shielding portion 303 like the slit portion 302. Alternatively, the slit may extend in a direction oblique to one side of the light shielding portion 303. The resist used in the photolithography process is preferably a positive resist.
[0109] As another example of the semi-transparent portion, a semi-transparent portion having a function of reducing the light intensity of the exposure light is shown in FIG. In this example, a semipermeable membrane 304 is provided. In addition to MoSiN, MoSi, M SiO, MoSiON, CrSi, etc. can be used. The exposure method using a mask is also called a halftone exposure method.
[0110] When the exposure masks shown in FIGS. 11(A) to 11(C) are irradiated with exposure light, the light-shielding portion 30 The light intensity of the light transmitting portion 305 is 100%. 301, 302, or a semi-permeable membrane 304. The light intensity can be adjusted within the range of 10 to 70%. FIG. 11(D) shows that when the semi-transparent portion has a diffraction grating pattern, the light intensity passing through the semi-transparent portion is The adjustment of the degree is realized by adjusting the pitch and width of the slits 301 and 302. do.
[0111] This embodiment can be freely combined with the first and second embodiments.
[0112] (Embodiment 4) In this embodiment, an EL (Electro Luminescence) display device is shown in FIG. 2 and 13. The method of forming the substrate and each layer constituting the TFT, the materials, etc. Refer to the first and second embodiments. The TFTs in FIGS. 12 and 13 are top-gate TFTs according to the first embodiment. Although the description will be given using a FT structure, a bottom-gate TFT structure may also be used. 2 are given the same reference numerals and detailed description will be omitted. The pixel configuration is not limited to that shown in FIGS. 12 and 13, and other pixel configurations may be used.
[0113] FIG. 12(A) shows a top view of a pixel portion of an EL display device. Two TFTs are installed: TFT140, which is a driving TFT that controls the current flowing through the EL element, and TFT141, which is a driving TFT. The transparent conductive film that serves as the source electrode or drain electrode of the switching TFT 140 is The gate electrode 5b of the driving TFT 141 is electrically connected to the film 123 and the metal film 124. Fig. 12(B) is a cross-sectional view taken along lines AA' and BB' in Fig. 12(A).
[0114] A TFT is formed on a substrate 1 by the method of embodiment 1. An insulating film 2 is formed on the substrate 1. The island-shaped semiconductor films 3a and 3b are formed on the surface of the amorphous semiconductor film. Next, the gate insulating film 4 and the gate electrodes 5a and 5b are formed. The gate electrode 5a extends from the gate wiring, and the gate electrode 5b extends from the gate wiring ( The gate electrodes 5a and 5b are used as masks to form island-shaped semiconductor layers. The conductive films 3a and 3b are doped with impurity elements to form a pair of impurity regions and a channel forming region. Next, a first layer is formed on each of the island-shaped semiconductor films 3a and 3b. An interlayer insulating film 6 and a second interlayer insulating film 7 are formed.
[0115] Next, the gate insulating film 4, the first interlayer insulating film 6 and the second interlayer insulating film 7 are etched to form an island. Contact holes are formed to reach a pair of impurity regions of the semiconductor film. The first interlayer insulating film 6 and the second interlayer insulating film 7 are etched to form a contact that reaches the gate electrode 5b. A transparent conductive film is formed on the second interlayer insulating film 7, and a metal film is formed on the transparent conductive film. The transparent conductive film and the metal film are then etched in the same manner as in the first embodiment. A wiring or electrode made of a metal film 122 and a transparent conductive film 121, a metal film 124 and a transparent conductive film A wiring or electrode made of 123, a metal film 126 and a transparent conductive film 125. The transparent conductive film 127 is then used to form a wiring or an electrode. The reference numeral 7 functions as a pixel electrode.
[0116] The metal films 122, 124, and 126 are transparent conductive films 121, 123, and 126 located below. 5, and the pattern is one size smaller than each transparent conductive film. In order to form the metal films 122, 124, and 126, the resist pattern shown in FIG. A resist pattern that has been exposed and developed using an exposure mask having a light-shielding portion, such as pattern 16a, On the other hand, the transparent conductive film 127 is partially etched to function as a pixel electrode. Therefore, the metal film 128 does not necessarily have a similar relationship to the transparent conductive film 127. Therefore, the transparent conductive film 127 and the metal film 12 To form the resist pattern 8, a semi-transparent portion and a light-shielding portion are formed as in the resist pattern 15a shown in FIG. The resist pattern is exposed and developed using an exposure mask having a resist pattern.
[0117] After the metal films 122, 124, 126, and 128 are formed, the exposed portions of the metal film 128 are The surface of the transparent conductive film 127 is polished to remove the residue of the metal film on the transparent conductive film. The polishing is done by CMP (Chemical-Mechanical Polishing). This polishing can be performed by a polishing method or the like. Since the electroluminescent layer is a very thin film, the residue of the metal film prevents the electroluminescent layer from being uniformly formed. This prevents the transparent conductive film 127 and the conductive layer 131 on the electroluminescent layer from shorting out. It is very effective.
[0118] Thereafter, an insulating film 129 (also called a partition wall) is formed on the TFT. 29 is formed so as to expose the portion of the transparent conductive film 127 that functions as a pixel electrode. In addition, the insulating film 129 is formed so as to cover the metal film 128. This is because the metal film 128 is an insulating film. If the insulating film 129 is exposed, it may cause a short circuit in the EL element. 9, the thickness of the film is continuously decreased near the exposed transparent conductive film 127, and the film has a curved surface. This is because the electroluminescent layer formed in the upper portion is not cut off by the step of the insulating film 129. The insulating film 129 has a curved surface so that the metal film 12 However, there was a concern that the end of the insulating film 129 may be easily exposed. The metal film 128 has an inclined end as described in the first and second embodiments. Since the insulating film 129 is not easily exposed due to the angle θ2, the EL display device is not Always preferred.
[0119] When the metal film 128 is formed by dry etching, the resist pattern formed on the upper part The shape of the turn is reflected, and when viewed in the cross-sectional view of FIG. 12(B), the direction closer to the curved surface of the insulating film 129 is The end of the metal film 128 is inclined more than the other end. When viewed from the outside, the two sides of the metal film 128 that are farther from the edge of the transparent conductive film 127 are The inclination is larger than that of the other two sides. On the other hand, the metal film 128 is formed by wet etching. In this case, the angle θ2 at the end of the transparent conductive film 127 is set to an angle more acute than the angle θ1 at the end of the metal film 12 Therefore, in either formation method, the gold layer close to the curved surface of the insulating film 129 is The end of the metal film 128 is formed with an inclination or angle θ2, so that the end of the metal film 128 is exposed from the insulating film 129. The shape becomes difficult to mold.
[0120] Next, the electroluminescent layer 13 is formed so as to contact the transparent conductive film 127 exposed from the insulating film 129. 0 is formed, and then the conductive layer 131 is formed. In the above structure, the TFTs that drive the light-emitting elements If the TFT is an N-channel type TFT, the transparent conductive film 127 corresponds to a cathode and the conductive layer 131 corresponds to an anode. When a transparent conductive film is used for the conductive layer 131, the display device emits light both upward and downward. do.
[0121] FIG. 13 shows an EL display device having a different structure from that shown in FIG. 12. FIG. 13(B) is a top view of the pixel portion of the device, and FIG. 13(B) is a cross-sectional view taken along lines A-A' and B-B' in FIG. 13(A). The figure is shown.
[0122] FIG. 13B shows the structure of the island-shaped semiconductor film after the second interlayer insulating film 7 is formed and then etched. The process is the same as that shown in FIG. 12(B) until the contact holes reaching the pair of impurity regions are formed. A switching TFT 1101 and a driving TFT 1102 are formed. Then, a conductive layer Then, etching is performed to form wiring or electrodes 1103a to 1103d.
[0123] A third interlayer insulating film 1104 is formed on the wiring or electrodes 1103a to 1103d. It is preferable that the insulating film 1104 is made of an organic resin film. This is because a transparent conductive film that functions as a pixel electrode can be formed on a flat surface. It is.
[0124] The third interlayer insulating film 1104 is etched to form a contact that reaches the wiring or electrode 1103d. A transparent conductive film and a metal film are laminated on the third interlayer insulating film 1104, The transparent conductive film 1105 and the metal film 1106 are formed by etching. The metal film 1106 is an exposure pattern having a semi-transparent portion, like the resist pattern 15a shown in FIG. The transparent conductive film 1 is etched using a resist pattern that has been exposed and developed using a mask. The element 105 functions as a pixel electrode.
[0125] A contact hole formed in the second interlayer insulating film 7 and a contact hole formed in the third interlayer insulating film 1104 The contact holes are preferably formed so as to overlap each other. By bending the contact hole, the aperture ratio can be increased. This will cause problems with the transparent conductive film 1105 being broken, but The problem of disconnection is solved by leaving the metal film 1106 on the transparent conductive film 1105 in the can be done.
[0126] After the metal film 1106 is formed, the insulating film 129 and the electroluminescent layer 124 are formed in the same manner as in FIG. 12(B). 130, a conductive layer 131 is formed.
[0127] In this embodiment, the conductive film used as the pixel electrode is described as a transparent conductive film. The transparent conductive film may be made of the material shown in the first embodiment. In addition, this embodiment can be freely combined with the first to third embodiments within the scope of feasibility. can.
[0128] (Embodiment 5) In this embodiment, an example in which the present invention is applied to a liquid crystal display device will be described.
[0129] First, a method for manufacturing a liquid crystal display panel will be described with reference to FIG. A bottom gate type TFT is formed on a substrate 401 in the same manner as in FIG. 6(C) of 2. The structure is not limited to the TFT shown in FIG. 6C of the second embodiment, and TFTs of various structures may be used. can be done.
[0130] After forming the TFT by the method of the third embodiment, the metal films 424 and 421 and the transparent conductive film 419 are An alignment film 801 is formed so as to cover the liquid crystal display 415. Then, a color filter 802 and a light-shielding film 807, a substrate 805 on which a counter electrode 803 and an alignment film 804 are formed is prepared. The light-shielding film 807 overlaps the TFT. The color filter 802 is disposed so as to form a transparent conductive film 415 which functions as a pixel electrode. After that, when liquid crystal 806 is injected, a display device having a display function is formed. The display device is completed. Although not shown, the substrates 401 and 805 have polarizing electrodes on the opposite side to the liquid crystal 806. The above steps complete the liquid crystal display panel. Instead, a reflective conductive film can be used.
[0131] Next, in the present embodiment, in the liquid crystal display device, the arrangement of the metal film formed on the transparent conductive film is FIG. 14B is an example of a top view of a liquid crystal display device, and FIG. 14B. An island-shaped semiconductor film 4 is formed on a gate wiring 403. The gate wiring portion overlapping the island-shaped semiconductor film 405 becomes the gate electrode. 403 is a gate wiring and a gate electrode. A laminated film of a metal film 424 serving as a source wiring and a transparent conductive film 419 is electrically connected via a layer 417. 4, and a metal film 421 that becomes a drain wiring and a transparent conductive film 415 are connected to the drain wiring via a conductive layer 418. The laminated film is electrically connected to the transparent conductive film 415. The capacitance wiring 808 may be formed in the same layer as the gate wiring 403, or may be formed in a separate layer. The light-shielding film 807 is indicated by a dashed line. The light-shielding film 807 is formed of a layer of the source wiring, Although it overlaps with the drain wiring and the TFT, the transparent conductive film 415 is a portion that functions as a pixel electrode. do not overlap.
[0132] The metal film 421 on the transparent conductive film 415 is formed along the edge of the transparent conductive film 415. In detail, the side surface of the metal film 421 is formed along the side surface of the transparent conductive film 415. However, the side of the metal film 421 does not coincide with the side of the transparent conductive film 415. In this way, the metal film 421 is formed along the edge of the transparent conductive film 415. By doing so, the positioning accuracy of the light shielding film 807 for shielding the spaces between the pixel electrodes can be relaxed. This is because even if the position of the light-shielding film 807 is slightly misaligned, the metal film 421 continues to function as a light-shielding film. Therefore, the positional deviation of the light-shielding film 807 is permitted within the range where the metal film 421 exists. In particular, when a light-shielding film is provided on the opposing substrate as shown in FIG. 14, high alignment accuracy is required. Therefore, to ensure light shielding between pixels, a transparent conductor is provided along the edge of the pixel electrode. It is advantageous to form a metal film 421 on the conductive film.
[0133] Another liquid crystal display device configuration will be described with reference to FIG. 15. In FIG. 15, an interlayer insulating layer is added to the configuration of FIG. FIG. 15(A) is a top view of the liquid crystal display device shown in FIG. A cross-sectional view of the gate wiring 403. The island-shaped semiconductor film 405 overlaps the gate wiring 403. The gate wiring portion overlapping the conductive film 405 becomes the gate electrode. The source wiring 501 is electrically connected through the conductive layer 417, and the drain wiring 502 is electrically connected through the conductive layer 418. The wiring 502 is electrically connected. The capacitance wiring 808 is connected to the transparent conductive film 504 at the portion where it overlaps. The capacitor wiring 808 may be formed from the same layer as the gate wiring 403, or may be formed from a separate layer. It may be formed in layers.
[0134] An interlayer insulating film 503 is formed on the source wiring 501 and the drain wiring 502. A contact hole reaching the drain wiring 502 is formed in the interlayer insulating film 503. The insulating film 503 is an organic resin film or an inorganic insulating film. 504 and a metal film 505 are formed. If the interlayer insulating film 503 is an organic resin film, the gate Since the step caused by the electrode 403 and the island-like semiconductor film 405 is reduced, the electrode functions as a pixel electrode. The transparent conductive film 504 can be formed on a flat surface. Therefore, the image can be displayed more widely than in the configuration shown in FIG. The element electrodes can be removed, and the aperture ratio can be improved.
[0135] The transparent conductive film 504 and the metal film 505 are formed in the same manner as the resist pattern 16a shown in FIG. Then, the resist pattern is exposed and developed using an exposure mask having a light-shielding portion, and then etched. The connection between the transparent conductive film 504 and the drain wiring 502 has a large step. Since there is a risk of the conductive film 504 being cut off, the metal film 505 is left on the transparent conductive film 504. It's best to do so.
[0136] In the top view of FIG. 15(B), similarly to FIG. 14(B), the metal film 505 is a transparent conductive film 50. It is formed to fit the edge of 4 and can also function as part of the light-shielding film. .
[0137] The transparent conductive film material shown in the first embodiment can be used for the transparent conductive film 504 .
[0138] In addition, in order to align the liquid crystal in multiple directions, a metal film is formed on the transparent conductive film. An example of using the pixel circuit is shown in FIG. 16(A) and FIG. 16(B) is a top view of the pixel portion. 1 is a cross-sectional view of the liquid crystal layer taken along line AA' of FIG. The transparent conductive film 1002 functions as a light-transmitting layer, and the metal film 1003 is formed on the transparent conductive film 1002. 1004 is a counter substrate, 1005 is a counter electrode, 1006 is a liquid crystal, and 1007 is an alignment film. A plurality of metal films 1003 are disposed on one transparent conductive film 1002. The cross-sectional shape of 03 is triangular, and the slope of the triangle allows the liquid crystal within one pixel to be aligned in two directions. Each metal film is formed on the transparent conductive film 1002 in a ridge-like shape. This configuration is called MVA (Multi-domain Vertical Alignment) This is called the ent type, and it can obtain a large viewing angle characteristic. The cross section of the metal film 1003 is triangular, but may be trapezoidal. The liquid crystal within the element can be oriented in two directions.
[0139] Another example of the arrangement of metal films in the MVA method is shown in Figure 17. Figure 17(A) shows 17B is a cross-sectional view of the liquid crystal layer and its vicinity taken along line AA' in FIG. 17A. Each pixel is made up of a TFT 1201, a transparent conductive film 1202 that functions as a pixel electrode, and The metal film 1203 is formed on the substrate 1204. The substrate 1204 is an opposing substrate, and the substrate 1205 is a The counter electrode, 1206 is a liquid crystal, and 1207 is an alignment film. It is made up of protrusions, each of which has a vertex and is shaped like a pyramid. Therefore, the liquid crystal within one pixel is oriented in four directions, equal to the number of slopes of the protrusions. The shape of the protrusions may be a triangular pyramid or other shape other than a square pyramid, in which case the liquid crystal is oriented in three directions. Therefore, the configuration of FIG. 17 can obtain a larger viewing angle characteristic than that of FIG.
[0140] The example described in this embodiment is a PVA (Patterned Vertical Al It is used as a substitute for slits to give a specific alignment to liquid crystals in the liquid crystal alignment method. By replacing the slits in the PVA method, the transparent conductive film that becomes the pixel electrode This can reduce the number of steps for forming slits.
[0141] Another example of metal film arrangement is shown in Figure 18. A transparent conductive film 1502 which functions as a conductive film is electrically connected to the transparent conductive film 1502. A metal film 1501 is laminated on the metal film 1501. The metal film 1501 has a comb-tooth shape.
[0142] As described above, by devising the arrangement of the metal film on the transparent conductive film, it was possible to ensure light blocking. This improves the viewing angle characteristics. In addition, a special mask is required to form the metal film. Since there is no need to create a new one, the number of steps in the creation can be reduced.
[0143] Although the TFTs shown in FIGS. 13 to 18 have a bottom gate structure, This is just an example, and other TFT configurations can be used. The present invention can be freely combined with any of the first to fourth embodiments to the extent possible.
[0144] (Embodiment 6) The semiconductor device of the present invention can be used in a video camera, a digital camera, a goggle-type display, etc. Head-mounted displays, navigation systems, audio playback devices (car audio) audio components, notebook personal computers, game devices, mobile information Information terminals (mobile computers, mobile phones, portable game consoles, e-books, etc.), recording media An image reproducing device equipped with a Digital Versatile Disc (D (Devices equipped with a display that can play back recording media such as DVDs and VDs and display the images) Specific examples of these semiconductor devices are shown in FIGS.
[0145] FIG. 20A shows a digital camera, which includes a main body 2101, a display unit 2102, an imaging unit, and an operation unit. The operation key 2104, the shutter 2106, etc. are included. The present invention provides a low-cost, reliable, and low-defective display. This makes it possible to create a highly reliable digital camera.
[0146] FIG. 20B shows a notebook personal computer, which includes a main body 2201 and a housing 220 2, display unit 2203, keyboard 2204, external connection port 2205, pointing This invention makes it possible to produce inexpensive, reliable notebooks with few display defects. It is possible to realize a personal computer.
[0147] FIG. 20C shows a portable image reproducing device equipped with a recording medium (specifically, a DVD reproducing device). ) a main body 2401, a housing 2402, a display unit A 2403, a display unit B 2404, a recording medium The device includes a DVD reader 2405, operation keys 2406, and a speaker 2407. The display unit A 2403 mainly displays image information, and the display unit B 2404 mainly displays text information. In addition, image playback devices equipped with recording media also include home game consoles. The invention makes it possible to realize an image reproducing device that is inexpensive, has few display defects, and is highly reliable. Cut.
[0148] FIG. 20D shows a display device, which includes a housing 1901, a support 1902, a display unit 19 1903, a speaker 1904, a video input terminal 1905, etc. The display portion 1903 and The display device is manufactured by using the same in a liquid crystal display device, a light emitting device, and a driving circuit. Specifically, all information such as for computers, television reception, and advertising displays is included. The present invention provides a display device that is inexpensive, has few display defects, and is highly reliable. It is possible to realize a display device, particularly a large display device having a large screen of 22 inches to 50 inches. can.
[0149] The mobile phone 900 shown in FIG. 05, etc., a main body (A) 901, a display panel (A) 908, a display panel (B) 909, a main body (B) 902 equipped with a speaker 906, etc., can be opened and closed with a hinge 910. The display panel (A) 908 and the display panel (B) 909 are connected to a circuit board 9 907 are housed in the housing 903 of the main body (B) 902. The pixel portion of the display panel (B) 909 is visible through an opening formed in the housing 903. will be placed in.
[0150] The display panel (A) 908 and the display panel (B) 909 are For example, the display panel (A) 90 can be set to a desired number of pixels. 8 as a main screen and a display panel (B) 909 as a sub-screen.
[0151] The present invention makes it possible to realize a portable information terminal that is inexpensive, has few display defects, and is highly reliable. This can be done.
[0152] The mobile phone according to this embodiment can be transformed into various forms depending on its functions and uses. For example, an imaging element can be incorporated in the hinge 910 to make it into a mobile phone with a camera. In addition, the operation switches 904, the display panel (A) 908, and the display panel (B) 90 Even if the above-mentioned functions and effects are achieved in a configuration in which the above-mentioned components are housed in a single housing, The same effect can be obtained even if the configuration of this embodiment is applied to an information display terminal equipped with a plurality of display units. can be obtained.
[0153] As described above, the configuration or manufacturing method of any one of the first to eighth embodiments can be applied to the display unit or By using the above as the display panel of FIG. 21, various electronic devices can be completed. [Industrial Applicability]
[0154] In the present invention, a conductive film that functions as a pixel electrode and a metal film laminated thereon are integrated into one matrix. When the conductive film is broken due to a step, the metal The metal film can connect the disconnected conductive films. It is possible to manufacture inexpensive semiconductor devices with little damage, and to realize highly reliable semiconductor devices. can. [Explanation of symbols]
[0155] 1 Board 2. Insulating film 3. Island-shaped semiconductor film 4 Gate insulating film 5. Gate electrode 6 First interlayer insulating film 7 Second interlayer insulating film 8. Channel formation region 9 Impurity region 10 Transparent conductive film 11 Metal Film 12a Light shielding part 12b Light shielding part 13 Semi-transparent part 14a Non-exposed area 14b Exposure area 19 Semi-permeable membrane 20 Metal Film 15a Resist pattern 16a Resist pattern 17a Transparent conductive film 17b Metal film 18a Transparent conductive film 18b Metal film 16b Resist pattern 15b Resist pattern 17c metal film 18c metal membrane 21 Capacitance wiring
Claims
[Claim 1] A transistor; an organic resin film provided above the transistor; a transparent conductive film provided above the organic resin film and electrically connected to the transistor; a metal film provided above the transparent conductive film; the transparent conductive film has a region in contact with the metal film, The side surface of the transparent conductive film is inclined with respect to the substrate, A display device, wherein the side surface of the metal film is inclined with respect to the substrate.
Citation Information
Patent Citations
Wiring board for display device and its manufacturing method
JP2004004680A
Liquid crystal display device and its production
JP1994230425A