Shrinkable label and method for manufacturing container with shrinkable label

The shrink label design with a flat-supplied cylindrical shape and selective medium layer coverage addresses the need for cost reduction and environmental impact by maintaining operational efficiency.

JP2024162874APending Publication Date: 2024-11-21FUJI SEAL INC
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
JP2023078827
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Filing Date
2023-05-11
Publication Date
2024-11-21

AI Technical Summary

Technical Problem

The rising unit price of materials for shrink labels necessitates reducing manufacturing costs while maintaining the ease of handling and application, and the environmental impact of using less material is desirable.

Method used

A shrink label design that includes a cylindrical shape supplied in a flat state with a main body layer and a transparent medium layer, featuring a first region covered by the medium layer and a second region not covered, allowing for reduced material usage without compromising operational smoothness.

Benefits of technology

The design enables efficient material reduction while ensuring ease of handling and application, contributing to cost-effectiveness and environmental friendliness.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 2024162874000001_ABST
    Figure 2024162874000001_ABST
Patent Text Reader

Abstract

To provide a shrinkable label with which it is possible to reduce the amount of materials used, without impairing the smooth conduct of work.SOLUTION: A shrinkable label 101 is a cylindrical shrinkable label which is supplied in a flat state for covering an object from top to bottom or from bottom to top, and which comprises a body layer 6 and a transparent medium layer 4 which is located inward of the body layer 6. The inside surface of the body layer 6 includes a first region 41 extending in the vertical direction, a second region 42, and a seal region. In the first region 41, the body layer 6 is covered with the medium layer 4, and the medium layer 4 constitutes the innermost layer; in the second region 42, the body layer 6 is not covered with the medium layer 4.SELECTED DRAWING: Figure 11
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for producing a shrink label and a container with a shrink label. [Background technology]

[0002] There is a known technology for packaging an object by covering the object with a cylindrical shrink label. The object is, for example, a container. The container referred to here is, for example, a container for drinks, food, medicine, toiletry products, etc. The container referred to here is, for example, a plastic bottle, a cup, a glass bottle, a metal can, etc.

[0003] Such shrink labels are typically tubular and long, and are supplied in the form of a roll, which is then cut to obtain tubular shrink labels of the desired length.

[0004] Shrink labels are thin and are supplied in a flattened tube, but in order to place them over an object, the opening of the tube must be widened. To make this process easy, the shrink label itself needs to have a certain degree of strength.

[0005] Furthermore, if the inner surface of the shrink label is charged, the inner surfaces will stick to each other and it will become difficult to open the opening of the tube smoothly; therefore, to prevent this from happening, an antistatic layer is provided, as described in Patent No. 5,930,760 (Patent Document 1). [Prior art documents] [Patent documents]

[0006] [Patent Document 1] Patent No. 5930760 Summary of the Invention [Problem to be solved by the invention]

[0007] In recent years, the unit price of the materials that make up shrink labels has risen sharply, so there is a demand to reduce the manufacturing cost of shrink labels. To achieve this, it is possible to reduce the amount of material used to manufacture shrink labels. However, it is necessary to be able to smoothly transport the shrink label, open the opening of the tube, and place it on the target object.

[0008] Therefore, an object of the present invention is to provide a shrink label that can reduce the amount of material used without impairing the smoothness of the process. Furthermore, if the amount of material used can be reduced, it is expected that the shrink label will be more environmentally friendly. [Means for solving the problem]

[0009] In order to achieve the above-mentioned object, a shrink label according to the present invention comprises a tubular shrink label which is supplied in a flat state to be placed over an object from top to bottom or bottom to top, a main body layer, and a transparent medium layer arranged inside the main body layer, the inner surface of the main body layer having a first region extending in the vertical direction, a second region, and a seal region for use in joining, in the first region the main body layer is covered by the medium layer and the medium layer forms the innermost layer, and in the second region the main body layer is not covered by the medium layer. Effect of the Invention

[0010] According to the present invention, the main body layer is covered by the medium layer in the first region and the main body layer is not covered by the medium layer in the second region, so it is possible to provide a shrink label that enables the amount of material used to be reduced without impairing ease of operation. [Brief description of the drawings]

[0011] [Figure 1] FIG. 2 is a diagram showing a first stage of a method of using the shrink label in accordance with the first embodiment of the present invention. [Diagram 2] FIG. 4 is a diagram showing a second stage of a method of using the shrink label in accordance with the first embodiment of the present invention. [Diagram 3] FIG. 4 is a diagram showing a third stage in a method of using the shrink label in accordance with the first embodiment of the present invention. [Figure 4] FIG. 1 is a conceptual diagram of a roll that serves as a supply source of a shrink label in a first embodiment according to the present invention. [Diagram 5] FIG. 2 is a conceptual diagram of a shrink label in the first embodiment according to the present invention cut from a roll. [Figure 6] FIG. 2 is an explanatory diagram of a state in which the opening portion of the shrink label in the first embodiment according to the present invention is widened. [Figure 7] FIG. 4 is an explanatory diagram of the shrink label in the first embodiment according to the present invention after it has been deformed into a folded state at a second fold-back portion. [Figure 8] FIG. 1 is a perspective view of a shrink label being conveyed in a first embodiment according to the present invention. [Figure 9] FIG. 2 is a perspective view of the shrink label in the first embodiment according to the present invention, in a state where it has been unfolded again to cover an object. [Figure 10] FIG. 1 is a plan view of a shrink label in a first embodiment according to the present invention when unfolded to expose its inner surface. [Figure 11] 1 is a partial cross-sectional view of a shrink label in accordance with a first embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0012] (Embodiment 1) (composition) A shrink label in a first embodiment according to the present invention will be described with reference to Figs. 1 to 11.

[0013] First, a method of using the shrink label 101 in this embodiment will be described. As shown in FIG. 1, the shrink label 101 is in the shape of a rectangular prism. Here, a rectangular prism is used as an example, but a polygonal prism other than a rectangular prism may be used. The shrink label 101 has a seal portion 11 at one side. The shrink label 101 has openings 10 at the upper and lower ends. As shown in FIG. 1, the shrink label 101 is placed on a container 5 as an object from above. The container 5 may be, for example, a plastic bottle. After the shrink label 101 is placed on the container 5, the container 5 becomes as shown in FIG. 2. In this state, the shrink label 101 shrinks by blowing hot air, steam, superheated steam, or the like onto the entire container, and the shrink label 101 becomes as shown in FIG. 3. That is, the shrink label 101 is attached to the outer surface of the container 5.

[0014] A shrink label is originally long and is supplied as a roll 501 as shown in FIG. 4. The term "long" here means that a number of individual shrink labels 101 are connected in the longitudinal direction. A long shrink label in this state may be called a "raw roll." The shrink label is cylindrical even in this long state, but is folded flat. At this point, the label pulled out from the roll 501 has first folded portions 51a and 51b. For ease of explanation, FIG. 4 shows the opening 10 slightly open. In reality, the opening 10 may not be open at all. FIG. 5 shows the state in which the individual shrink labels 101 are cut from the roll 501 shown in FIG. 4.

[0015] As shown in FIG. 5, the shrink label 101 includes first folded portions 51a, 51b and second folded portions 52a, 52b. The first folded portions 51a, 51b are already folded. The second folded portions 52a, 52b are not folded at this point. The second folded portions 52a, 52b are to be folded. For convenience of explanation, the shrink label 101 is shown in an upright state. As shown in FIG. 6, the opening 10 is widened. As shown by the arrow 93, the first folded portions 51a, 51b are brought closer to each other, while the second folded portions 52a, 52b are pulled away from each other, as shown by the arrow 94. For this deformation, a folding position changing tool called a tetra guide may be used. As a result, the shrink label 101 is as shown in FIG. 7. In this state, the shrink label 101 is flattened by being folded at the second folded portions 52a, 52b. The first folded portions 51a and 51b have fold marks, but are not folded, because they were folded just before. The shrink label 101 in this state is transported by the holders 12a and 12b, as shown in FIG. 8. Each of the holders 12a and 12b includes two rod-shaped members. The holder 12a holds the shrink label 101 by pinching it between the two rod-shaped members. The holder 12b holds the shrink label 101 in the same manner. The holders 12a and 12b hold the shrink label 101 at a portion that does not overlap with either the first folded portions 51a and 51b or the second folded portions 52a and 52b. In the example shown in FIG. 8, the holder 12a holds the shrink label 101 at a middle portion between the first folded portions 51a and 51b and the second folded portion 52a, and the holder 12b holds the shrink label 101 at a middle portion between the first folded portions 51a and 51b and the second folded portion 52b. While being transported by the holders 12a and 12b, the vicinity of the second folded portions 52a and 52b is in a free state. That is, the vicinity of the second folded portions 52a and 52b can be displaced to some extent. In the portion sandwiched by the holder 12a, there is a region where the second regions 42 abut against each other. The second regions 42 will be described later. The same is true in the portion sandwiched by the holder 12b.

[0016] After this, the shrink label 101 is unfolded again so as to cover the object. The unfolded state is shown in FIG. 9. As shown in FIG. 9, the inner surface of the cylindrical shrink label 101 has a first region 41 and a second region 42. It is preferable that a suction mechanism is provided on the surfaces of the holders 12a and 12b that contact the shrink label 101. In order to unfold the shrink label 101 to the state shown in FIG. 9, it is preferable to use the suction mechanisms of the holders 12a and 12b to pull and unfold the shrink label 101 while sucking its outer surface. In particular, when unfolding the label 101 while sucking its outer surface, it is preferable that in the portion sandwiched by the holders 12a, there is an area where the second regions 42 are in contact with each other, and in the area where the second regions 42 are in contact with each other, the surfaces where the white ink layers are exposed are in contact with each other.

[0017] As shown in FIG. 9, the shrink label is folded back approximately 90 degrees at four points, namely, two first fold portions 51a, 51b and two second fold portions 52a, 52b, to form a rectangular cylindrical shape, and is then placed over an object.

[0018] As already shown in FIG. 9, the shrink label 101 has a first region 41 and a second region 42 on its inner surface. In order to explain this inner surface in more detail, FIG. 10 shows the state in which the shrink label 101 is unfolded in its entirety after the bonding at the seal portion 11 is released. FIG. 10 shows the state of the inner surface as seen from FIG. 9. All of the hatched areas in FIG. 10 are the first region 41. A seal region 45 is provided at the left end in FIG. 10. To clearly show the extent of the seal region 45, the seal region 45 is hatched with dots in FIG. 10. The seal region 45 is an area where a solvent is applied to form the seal portion 11. The right end is overlapped with the seal region 45 at the left end of the shrink label 101. In other words, the right end is overlapped inside the seal region 45. The seal portion 11 is formed by bonding using the seal region 45, and the shrink label 101 is cylindrical in FIG. 9. In the case where the entire sealing area 45 overlaps the outside of the right end portion, when the shrink label 101 is formed into a cylindrical shape, the sealing area 45 is not exposed inside the cylinder, and the inner surface of the cylinder is composed of the first area 41 and the second area 42. The first folded portions 51a, 51b and the second folded portions 52a, 52b each extend in the up-down direction.

[0019] In FIG. 10, all of the regions other than the seal region 45 that are not hatched are the second region 42. In the example shown here, the first region 41 includes an upper end annular portion 411, a lower end annular portion 412, a first connecting portion 415, and a second connecting portion 416. The upper end annular portion 411 is shown in FIG. 10 as a region that extends linearly from side to side with a width W1 at the upper end of the shrink label 101. The lower end annular portion 412 is shown in FIG. 10 as a region that extends linearly from side to side with a width W2 at the lower end of the shrink label 101. The first connecting portion 415 and the second connecting portion 416 each extend in the up-down direction. The second region 42 is divided into several rectangular regions by being separated by the first region 41. A cross-sectional view of one of the multiple divided regions of the second region 42 and some of the first regions 41 in its vicinity is shown in FIG. 11. In FIG. 11, arrow 91 indicates the outside when attached to an object, and arrow 92 indicates the inside when attached to an object.

[0020] The shrink label 101 in this embodiment can be expressed as follows. The shrink label 101 is a tubular shrink label that is supplied in a flat state to be placed on an object from top to bottom or bottom to top, and includes a main body layer 6 and a transparent medium layer 4 disposed inside the main body layer 6. The inner surface of the main body layer 6 has a first region 41, a second region 42, and a seal region 45 for use in bonding. In the first region 41, the main body layer 6 is covered by the medium layer 4, and the medium layer 4 forms the innermost layer. In the second region 42, the main body layer 6 is not covered by the medium layer 4.

[0021] The main body layer 6 includes a base material layer 1, a color ink layer 2, and a white ink layer 3. The base material layer 1 is transparent. The base material layer 1 is formed of resin. The color ink layer 2 is a layer printed on the inner surface of the base material layer 1 to display information about the product. The white ink layer 3 is a layer printed so as to cover the color ink layer 2. The color ink layer 2 does not necessarily exist over the entire area of ​​the main body layer 6. The white ink layer 3 does not necessarily exist over the entire area of ​​the main body layer 6. In the seal area 45, the base material layer 1 exists, but the color ink layer 2 and the white ink layer 3 do not exist.

[0022] (Action and effect) In this embodiment, the second region 42 exists on the inner surface of the main layer 6, i.e., there is a region where the main layer 6 is not covered by the medium layer 4, so that the amount of material used for the medium layer 4 can be reduced. In other words, the amount of material used can be reduced. The first region 41 also exists on the inner surface of the main layer 6, and in the first region 41, the main layer 6 is covered by the medium layer 4, so that the shrink label 101 can have a certain strength. By providing the shrink label 101 with a certain strength in this way, the operations of opening the opening of the tube and covering the object can be performed smoothly.

[0023] As described above, in this embodiment, a shrink label can be provided that can reduce the amount of material used without impairing the smoothness of the operation.

[0024] In this embodiment, the shrink label 101 has been described as being for covering an object from top to bottom, but this is not limited thereto. For example, the shrink label may be for covering an object from bottom to top. Or, it may be for covering from another direction.

[0025] As shown in this embodiment, the shrink label 101 has two first folded portions 51a, 51b that are already folded when the shrink label 101 is supplied in a flat state, and an even number of second folded portions 52a, 52b that are arranged parallel to the two first folded portions 51a, 51b while dividing the area between the two first folded portions 51a, 51b, and are not folded when the shrink label 101 is supplied in a flat state, but become folds when the shrink label 101 is placed over the object. The region 41 preferably includes an upper end annular portion 411 and a lower end annular portion 412 that are annular by extending laterally at the upper end and the lower end of the shrink label 101, a first connecting portion 415 arranged in a strip shape along the two first folded portions 51a, 51b so as to connect the upper end annular portion 411 and the lower end annular portion 412, and a second connecting portion 416 arranged in a strip shape along the even number of second folded portions 52a, 52b so as to connect the upper end annular portion 411 and the lower end annular portion 412. By adopting such a configuration, it is possible to efficiently reduce the amount of material used for the medium layer 4 while ensuring the overall strength. The first connecting portion 415 and the second connecting portion 416 act like pillars for the tubular shrink label 101, ensuring the self-supporting property of the shrink label 101 and increasing the compressive strength. It is preferable that the area sandwiched between the two first folded portions 51a, 51b be divided equally by an even number of second folded portions.

[0026] It is preferable that the first connecting portion 415 has a width of 1 mm or more and 15 mm or less on each side across the first folded portion, and the second connecting portion 416 has a width of 1 mm or more and 15 mm or less on each side across the second folded portion. That is, it is preferable that C1 is 1 mm or more and 15 mm or less, and C2 is also 1 mm or more and 15 mm or less. By adopting this configuration, it is possible to ensure sufficient strength while reducing the amount of material used for the medium layer 4.

[0027] It is preferable that width W1 of upper end annular portion 411 is 5 mm or more. By adopting this configuration, it becomes easier to attach shrink label 101 to an object, and it is possible to prevent folding near the upper end when attaching it to the object, and to prevent wrinkles during shrinking.

[0028] It is preferable that width W2 of bottom end annular portion 412 is 20 mm or more. By adopting this configuration, it becomes easier to attach shrink label 101 to an object, and it is possible to prevent folding near the bottom end when attaching it to an object, and to prevent wrinkles during shrinking.

[0029] The thickness of the base material layer 1 is preferably 30 μm or less. When the base material layer 1 is this thin, the overall strength of the shrink label 101 in particular is likely to be insufficient, so by adopting the configuration shown in this embodiment, the strength can be ensured and the effects can be enjoyed to a greater extent. The base material layer 1 is a member capable of supporting the colored ink layer 2 and the white ink layer 3. The base material layer 1 is formed of a material that has heat shrinkability. When the base material layer 1 is immersed in hot water at 90° C. for 10 seconds, the heat shrinkage rate of the base material layer 1 in the main shrinkage direction is, for example, 30% or more, and preferably 50% or more.

[0030] The resin contained in the base layer 1 may be, for example, a thermoplastic resin. The base layer 1 may be, for example, a shrink film. The resin contained in the base layer 1 may be, for example, a polyolefin resin. Examples of the polyolefin resin include polyethylene and polypropylene. Examples of the polyester resin include polyethylene terephthalate and polylactic acid. Examples of the resin contained in the base layer 1 may be polystyrene resins such as styrene-butadiene copolymers. Examples of the resin contained in the base layer 1 may be polyamide resins and polyvinyl chloride resins. The base layer 1 may be, for example, a single layer including one or more of the above-mentioned resins, or may be a multiple layer in which multiple such single layers are laminated.

[0031] The substrate layer 1 is preferably formed of a polyester-based resin, a polystyrene-based resin, or a combination of these resins. The combination here includes a laminate of a polyester-based resin layer and a polystyrene-based resin layer. The substrate layer 1 is more preferably formed of a polyethylene terephthalate-based resin, a styrene-butadiene copolymer, or a combination of these resins. The polyethylene terephthalate-based resin here includes modified polyethylene terephthalate.

[0032] It is particularly preferable that the base layer 1 contains a polyethylene terephthalate resin. The thickness of base layer 1 is preferably, for example, 10 μm or more and 50 μm or less, and particularly preferably 10 μm or more and 30 μm or less.

[0033] As shown in this embodiment, the main body layer 6 includes a transparent base material layer 1 made of resin, and a white ink layer 3 disposed so as to cover at least a part of the base material layer 1 on the inner side of the base material layer 1, and it is preferable that the white ink layer 3 is exposed in the second region 42. By adopting this configuration, it is possible to prevent the white ink layer 3 from showing through to the back side in regions where it should not show through, and a good label can be realized.

[0034] More practically, the main layer 6 includes the color ink layer 2 disposed so as to cover at least a portion of the base layer 1 on the inner side of the base layer 1, and the white ink layer 3 is disposed so as to cover at least a portion of the color ink layer 2 on the inner side of the color ink layer 2. By employing this configuration, the necessary information is expressed by the color ink layer 2 and displayed toward the outside, while the white ink layer 3 prevents the information from showing through to the back side in areas where it should not.

[0035] In this embodiment, the substrate layer 1, which is a part of the main body layer 6, has been described as being transparent, but this is merely an example. The substrate layer 1 may be opaque. When the substrate layer 1 is opaque, the color-developing ink layer 2 is disposed on the outer surface of the substrate layer 1. In this case, the white ink layer 3 may be disposed between the color-developing ink layer 2 and the substrate layer 1, and the white ink layer 3 may not be disposed. Alternatively, in a configuration in which the substrate layer 1 is opaque and the color-developing ink layer 2 is disposed on the outer surface of the substrate layer 1, the white ink layer 3 may be disposed on the inner surface of the substrate layer 1.

[0036] In the present embodiment, the white ink layer 3 is described as being exposed in the second region 42, but this is merely an example.

[0037] As shown in this embodiment, the object is preferably a plastic bottle. By adopting this configuration, the plastic bottle can be stably packaged with high efficiency.

[0038] In the above embodiment, an example was given in which the target object was a plastic bottle, but the target object may be something other than a plastic bottle.

[0039] In the above embodiment, an example was shown in which the shrink label 101 was in the shape of a quadrangular prism, but the shrink label may also be in the shape of a hexagonal prism, octagonal prism, etc. In the above embodiment, an example was shown in which the number of second fold-back portions was two, but the number of second fold-back portions may be an even number of four or more.

[0040] From the viewpoint of suitability for attaching the label to an object, it is preferable that the coefficient of friction of the second region 42 is greater than that of the first region 41. The coefficient of friction referred to here is the static coefficient of friction. The coefficient of friction referred to here is measured in a dry state without dripping water, by overlapping similar regions of the inner surface of the shrink label so that they are in contact with each other, in accordance with JIS K 7125. The coefficient of friction of the first region 41 is preferably 0.1 or more and 0.7 or less. The coefficient of friction of the second region 42 is preferably 0.2 or more and less than 1.0. The area ratio of the first region 41 to the second region 42 is preferably 20 / 80 or more and 90 / 10 or less. In particular, it is preferably 20 / 80 or more and 60 / 40 or more.

[0041] (Manufacturing method) A method for manufacturing a shrink-labeled container in this embodiment will be described. The method for manufacturing a shrink-labeled container in this embodiment includes a step of preparing the above-mentioned shrink label. In this manufacturing method, the shrink label has two first folds that are already folded when the shrink label is supplied in a flat state, and an even number of second folds that are arranged parallel to the two first folds while dividing the area between the two first folds, and are not folded when the shrink label is supplied in a flat state but become folds when the shrink label is placed on the object. This manufacturing method includes a step of deforming the shrink label so that the folded state at the two first folds is eliminated and the shrink label is folded at two of the even number of second folds.

[0042] By adopting this manufacturing method, containers with shrink labels can be easily obtained.

[0043] The above-described embodiments disclosed herein are illustrative and not restrictive in all respects. The scope of the present invention is defined by the claims, and includes all modifications within the meaning and scope of the claims.

[0044] (Appendix 1) A cylindrical shrink label that is supplied in a flat state to be placed on an object from top to bottom or bottom to top, A main body layer; a transparent medium layer disposed on the inner side of the main body layer, a shrink label, wherein an inner surface of the main body layer has a first region, a second region, and a seal region extending in the vertical direction, wherein in the first region, the main body layer is covered with the medium layer and the medium layer forms the innermost layer, and wherein in the second region, the main body layer is not covered with the medium layer.

[0045] (Appendix 2) two first folded portions that are already folded when the shrink label is supplied in a flat state; an even number of second fold portions that are arranged parallel to the two first fold portions while dividing the area between the two first fold portions, and that are not folded when the shrink label is supplied in a flat state but become folds when the shrink label is placed over the object, The first region is an upper end annular portion and a lower end annular portion each extending laterally at an upper end and a lower end of the shrink label, respectively, to form an annular shape; a first connecting portion arranged in a band shape along the two first folded portions so as to connect the upper end annular portion and the lower end annular portion; and a second connecting portion arranged in a band shape along the even number of second folded portions so as to connect the upper end annular portion and the lower end annular portion.

[0046] (Appendix 3) The main body layer is A transparent base layer made of resin; a white ink layer disposed on the inner side of the base layer so as to cover at least a portion of the base layer, 3. The shrink label according to claim 1, wherein the white ink layer is exposed in the second region.

[0047] (Appendix 4) A method for producing a shrink-labeled container, comprising the steps of: preparing a shrink label according to any one of claims 1 to 3; the shrink label has two first folds which are already folded when the shrink label is supplied in a flat state, and an even number of second folds which are arranged parallel to the two first folds while dividing the area between the two first folds, are not folded when the shrink label is supplied in a flat state, but become folds when the shrink label is placed over the object, The manufacturing method includes: A method for manufacturing a shrink-labeled container, comprising a step of deforming the shrink label so that the folded state at the two first fold portions is eliminated and the shrink label is folded over at two of the even number of second fold portions. [Explanation of symbols]

[0048] 1 base layer, 2 colored ink layer, 3 white ink layer, 4 medium layer, 5 container, 6 main body layer, 10 opening, 11 sealing portion, 12a, 12b holder, 41 first region, 42 second region, 45 sealing region, 51a, 51b first folded portion, 52a, 52b second folded portion, 91, 92, 93, 94 arrows, 101 shrink label, 411 upper end annular portion, 412 lower end annular portion, 415 first connecting portion, 416 second connecting portion, 501 roll.

Claims

1. A cylindrical shrink label that is supplied in a flat state to be placed on an object from top to bottom or bottom to top, A main body layer; a transparent medium layer disposed on the inner side of the main body layer, a first region extending in a vertical direction; a second region; and a seal region for use in joining; wherein in the first region, the main body layer is covered with the medium layer and the medium layer forms the innermost layer; and in the second region, the main body layer is not covered with the medium layer.

2. two first folded portions that are already folded when the shrink label is supplied in a flat state; an even number of second fold portions which are arranged parallel to the two first fold portions while dividing the area between the two first fold portions, which are not folded when the shrink label is supplied in a flat state but which become folds when the shrink label is placed over the object, The first region is an upper end annular portion and a lower end annular portion each extending laterally at an upper end and a lower end of the shrink label, respectively, to form an annular shape; a first connecting portion arranged in a band shape along the two first folded portions so as to connect the upper end annular portion and the lower end annular portion; 2. The shrink label according to claim 1, further comprising a second connecting portion arranged in a band shape along the even number of second folded portions so as to connect the upper end annular portion and the lower end annular portion.

3. The main body layer is A transparent base layer made of resin; a white ink layer disposed on the inner side of the base layer so as to cover at least a portion of the base layer, 3. The shrink label according to claim 1, wherein the white ink layer is exposed in the second region.

4. A method for producing a shrink-labeled container, comprising the step of preparing the shrink label according to claim 1 or 2, the shrink label has two first folds which are already folded when the shrink label is supplied in a flat state, and an even number of second folds which are arranged parallel to the two first folds while dividing an area between the two first folds, are not folded when the shrink label is supplied in a flat state, but become folds when the shrink label is placed over the object, The manufacturing method includes: A method for manufacturing a shrink-labeled container, comprising a step of deforming the shrink label so that the folded state at the two first fold portions is eliminated and the shrink label is folded over at two of the even number of second fold portions.

Citation Information