Solar cell and barrier structure with optical element used for the solar cell
The integration of a barrier layer and ultrafine optical elements in perovskite solar cells addresses moisture and air infiltration issues, enhancing photoelectric conversion efficiency and reliability by optimizing sunlight flux and reducing resistance.
Patent Information
- Application Number
- JP2023080719
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-16
- Publication Date
- 2024-11-28
AI Technical Summary
Perovskite solar cells face challenges in achieving high photoelectric conversion efficiency due to moisture and air infiltration, especially as the size of the solar cells increases, and there is a lack of studies on optimizing sunlight flux propagation to the light absorption layer based on optical knowledge.
The solar cell design includes a barrier layer to prevent moisture and air ingress, with ultrafine optical elements on the surface to enhance sunlight focusing, and a layered structure with electron and hole transport layers to improve charge propagation, using materials like organic-inorganic perovskite compounds and metal foils for flexibility and durability.
The design significantly enhances photoelectric conversion efficiency by blocking moisture and air while optimizing sunlight flux, reducing electrical resistance, and maintaining reliability even at larger sizes.
Smart Images

Figure 2024164965000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a solar cell, in particular a perovskite solar cell, which has high barrier performance against moisture and gas and has an optical effect by shaping the surface shape of the components that constitute the solar cell, and has high photoelectric conversion efficiency. [Background technology]
[0002] Conventionally, as a solar cell, a laminated body in which an N-type semiconductor layer and a P-type semiconductor layer are arranged between opposing electrodes has been actively developed, and inorganic semiconductors such as silicon are mainly used as the N-type and P-type semiconductors. However, such inorganic solar cells have problems in that they require a vacuum process, making them difficult to enlarge, and they require large-scale equipment and are expensive in terms of materials, so that the range of use is limited. In recent years, therefore, perovskite solar cells have been attracting attention, in which an organic-inorganic perovskite compound having a perovskite structure using lead, tin, or the like as a central metal is used in the photoelectric conversion layer. Perovskite solar cells are expected to have high photoelectric conversion efficiency, and can be manufactured by a printing method, so that the manufacturing cost can be significantly reduced. On the other hand, there is a problem with water resistance, and the development of a corresponding technical means has been urgently required (for example, Patent Document 1).
[0003] As shown in FIG. 1, this perovskite crystal structure is a schematic diagram of a cubic crystal structure in which a metal atom M is located at the body center, an organic molecule R is located at each vertex, and a halogen atom or chalcogen atom X is located at the face center.
[0004] As mentioned above, solar cells using perovskite compounds (hereinafter referred to as "perovskite solar cells") are one of the candidates for low-cost, highly efficient next-generation solar cells, and research and development into them is being conducted around the world.
[0005] The photoelectric conversion layer of the solar cell preferably contains an organic-inorganic perovskite compound represented by the general formula RM-X3 (wherein R is an organic molecule, M is a metal atom, and X is a halogen atom or a chalcogen atom) shown in Figure 1. By using the organic-inorganic perovskite compound in the photoelectric conversion layer, the photoelectric conversion efficiency of the flexible solar cell can be improved.
[0006] In this context, tandem solar cells have been developed to further increase photoelectric conversion efficiency. Tandem (multi-junction) solar cells are made by stacking solar cells with different absorption wavelengths, which makes it possible to efficiently utilize the wavelengths of light, thereby further increasing photoelectric conversion efficiency.
[0007] For example, in the case of a tandem solar cell that uses a perovskite solar cell as the first layer where sunlight enters and a silicon solar cell as the second layer on the substrate side, the band gap of the perovskite solar cell must be optimized, and the V OC It is important to increase the efficiency and reliability of cells (to the same level as silicon-based solar cells) to reduce (open circuit voltage) losses. On the other hand, for silicon-based solar cells, surface shape control and interface control technology are important for forming a uniform film of perovskite material, and much research has been conducted on these topics (e.g., Patent Document 2).
[0008] Meanwhile, in recent years, flexible solar cells using polyimide, polyester-based heat-resistant polymer materials or metal foil as a substrate have been attracting attention. Flexible solar cells have advantages such as being thin and lightweight, making them easy to transport and install, and being impact resistant. For example, they are manufactured by laminating a plurality of layers, such as a photoelectric conversion layer having a function of generating an electric current when irradiated with light, in a thin film form on a flexible substrate. Furthermore, if necessary, the upper and lower surfaces of the flexible solar cell are sealed by laminating a solar cell encapsulant sheet. For example, Patent Document 3 describes a substrate for a semiconductor device including a sheet-like aluminum substrate, and an organic thin-film solar cell including the substrate for a semiconductor device. [Prior art documents] [Patent documents]
[0009] [Patent Document 1] JP 2018-163938 A [Patent Document 2] Patent Publication No. 2022-183700 [Patent Document 3] JP 2013-253317 A [Non-Patent Document 1] Materials presented at the "JST Research Results Optimal Deployment Support Program (A-STEP) (2) ~ Functional Materials ~ New Technology Briefing" held on November 18, 2022) "Ultra-high barrier comparable to glass that can be created by printing" Summary of the Invention [Problem to be solved by the invention]
[0010] In recent years, the characteristics of perovskite solar cells have been significantly improved through advances in their components and element structures, with initial photoelectric conversion efficiencies exceeding 20% and approaching those of single-crystal silicon solar cells. In addition, developments have been made to improve reliability by sufficiently blocking moisture and air by using barrier sheets, etc. However, no study has been done on the specific element configuration or arrangement that transmits the solar flux to the light absorption layer based on optical knowledge in order to improve the photoelectric conversion efficiency.
[0011] An object of the present invention is to provide a highly reliable solar cell that has high photoelectric conversion efficiency in the light absorption layer and blocks the intrusion of moisture and air by providing extremely fine optical elements in a barrier member that constitutes the solar cell. [Means for solving the problem]
[0012] In order to solve the above problems, for example, the configuration described in the claims is adopted. The present application includes a number of means for solving the above problems, but the basic configuration of a solar cell (cell) as one example thereof is a configuration in which transparent electrodes are provided on both sides of a light absorbing layer 102 that absorbs sunlight and generates electricity, as shown in Fig. 3, and a hole transport layer 106 is provided between the photoelectric conversion layer (light absorbing layer) 102 and the transparent electrode that serves as the anode. By providing an electron transport layer 105 on the other side of the photoelectric conversion layer (light absorbing layer) 102, the propagation of holes and electrons to the electrodes can be performed more efficiently.
[0013] A barrier layer 110 is provided on the outer surface of the solar cell having the above-described basic configuration to prevent air and moisture from penetrating into the light absorbing layer, as shown in Fig. 4. It goes without saying that the same effect can be obtained by providing the barrier layer 110 in a solar cell having a configuration in which the above-described hole transport layer and electron transport layer are not provided. Effect of the Invention
[0014] According to the solar cell disclosed in the present invention, the barrier layer covering the outer surface of the basic structure blocks air and moisture, and the photoelectric conversion efficiency can be significantly improved by the action of the extremely fine optical elements provided on the surface of the barrier layer. Problems, configurations and effects other than those described above will become apparent from the following description of the embodiments. In addition, the contents of the description below regarding the materials constituting the solar cell, the thicknesses of the multiple layers having specific functions formed by the materials, and the manufacturing methods that are not directly related to the present application have been excerpted from prior patent applications that were publicly known at the time of writing this application, and have been written in a way that makes the present invention clearer. [Brief description of the drawings]
[0015] [Figure 1] FIG. 1 is a schematic diagram showing an example of a crystal structure of an organic-inorganic perovskite compound. [Diagram 2] FIG. 1 is a cross-sectional view illustrating a schematic diagram of the basic structure of a perovskite solar cell. [Diagram 3]FIG. 1 is a cross-sectional view showing the basic structure of a perovskite solar cell in which lead wiring is provided on a transparent electrode. [Figure 4] 1 is a cross-sectional view showing a schematic diagram of a solar cell in which an end (extraction portion) of an extraction wiring according to an embodiment of the present invention is covered with a barrier layer. [Diagram 5] 1A and 1B are a top view and a cross-sectional view showing a schematic diagram of a solar cell structure in which an end (extraction portion) of an extraction wiring of a solar cell unit according to an embodiment of the present invention is covered with a barrier layer. [Figure 6] 11A and 11B are a top view and a cross-sectional view showing a schematic diagram of a solar cell structure in which the end (extraction portion) of the lead-out wiring of a solar cell unit according to another embodiment of the present invention is covered with a barrier layer. [Figure 7] FIG. 2 is a top view that illustrates a schematic example of an end portion of an extraction wiring (an "end portion connection type") in a solar cell of the present invention. [Figure 8] FIG. 1 is a top view diagrammatically illustrating an example of an end portion ("T-shaped") of an extraction wiring in a solar cell of the present invention. [Figure 9] FIG. 2 is a top view that illustrates an example of an end portion of an extraction wiring in a solar cell of the present invention. [Figure 10] 1A and 1B are cross-sectional views and characteristic diagrams illustrating the shape of a fine optical element provided on the surface of a barrier sheet or barrier layer according to an embodiment of the present invention and the refractive index distribution in the height direction of the element. [Figure 11] 1 is a cross-sectional view of a solar cell substrate and a fine optical element provided on a barrier layer surface according to an embodiment of the present invention. [Figure 12] FIG. 2 is a characteristic diagram showing the distribution of the irradiation energy of VUV light irradiated to form a barrier layer of the present invention and the distribution of the refractive index of the barrier layer in the thickness direction. [Figure 13] FIG. 1 is a characteristic diagram showing the change in the average refractive index and thickness of the barrier layer during irradiation with VUV light to form the barrier layer of the present invention. [Figure 14] FIG. 2 is a characteristic diagram showing the spectral energy distribution of sunlight. [Figure 15] FIG. 4 is a characteristic diagram illustrating a schematic diagram of sensitivity characteristics of a light absorbing layer to sunlight. [Figure 16]1A and 1B are schematic diagrams showing the shape and function of a micro-optical element having a moth-eye structure, which is a first embodiment of the present invention, provided on the surface of a barrier sheet or barrier layer according to an embodiment of the present invention. [Figure 17] 5A to 5C are schematic diagrams showing the shape and function of a micro-optical element having a moth-eye structure, which is a second embodiment of the present invention, provided on the surface of a barrier sheet or barrier layer according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0016] Hereinafter, the embodiments of the present invention will be described in detail with reference to the drawings. Note that the present invention is not limited to the contents of the embodiments described below (hereinafter, also referred to as "the present disclosure"). The present invention also covers the spirit of the invention or the scope of the technical ideas described in the claims, or equivalents thereof. Furthermore, the configurations of the embodiments (examples) described below are merely examples, and various changes and modifications are possible by those skilled in the art within the scope of the technical ideas disclosed in this specification.
[0017] In addition, in the drawings for explaining the present invention, the same reference numerals are given to components having the same or similar functions, and different names are used as appropriate, while repeated explanations of functions, etc. may be omitted. In the following description of the embodiments, the term "solar cell" is used to refer to an element that converts sunlight into electricity. Instead of this term, it may be expressed as "perovskite solar cell", "dye-sensitized solar cell", "semiconductor solar cell", etc. The term "solar cell" mainly used in the description of the embodiments is used as a representative example of these terms. In the following description of the solar cell of the present invention, a general structure that is currently being widely researched and developed will be described in the first part, and a highly reliable solar cell that has an extremely fine optical element provided in the barrier member constituting the solar cell of the present invention to increase the photoelectric conversion efficiency in the light absorption layer and block the intrusion of moisture and air will be described in the second part.
[0018] <Basic structure of perovskite solar cells> The basic structure of a perovskite solar cell is, as shown in FIG. 2, provided with at least a photoelectric conversion layer (also written as a light absorbing layer) 102 on a substrate 101 and electrodes 104 and 103 on both sides. The electrode provided on the side where sunlight is incident is made of a highly transparent material to obtain high photoelectric conversion efficiency. Regarding technical means for improving the photoelectric conversion efficiency of solar cells in which the photoelectric conversion layer (light absorbing layer) 102 contains an organic-inorganic perovskite compound, leading manufacturers have been actively studying materials that improve the conductivity and adhesion between materials and layers, but are also studying the enlargement and area of solar cells to improve productivity. However, as the area of solar cells increases, the area of transparent electrodes with high resistance (electrical resistance) and the barrier properties against air and moisture also increase, and a new problem has emerged in which sufficient photoelectric conversion efficiency cannot be obtained.
[0019] In order to reduce the electrical resistance, the solar cell 100 shown in FIG. 3 has a linear (multiple linear), lattice-like, mesh-like, or other lead wiring 107 formed, for example, using silver paste on the transparent electrode 104. As a result, even if the transparent electrode 104 has a large area, the resistance value is small, so that the internal loss of the element is reduced, and as a result, a high photoelectric conversion efficiency is obtained. On the other hand, since organic-inorganic perovskite compounds are very sensitive to moisture, deterioration of the photoelectric conversion layer (light absorption layer) 102 due to the intrusion of moisture from the atmosphere is a problem in solar cells in which the photoelectric conversion layer (light absorption layer) 102 contains an organic-inorganic perovskite compound, compared to other solar cells (for example, CIGS solar cells, which are polycrystalline silicon solar cells). As a countermeasure against this problem, the present invention shown in FIGS. 4 to 6, which will be described later, was developed.
[0020] <Barrier structure> As mentioned above, moisture can easily pass through the lead-out wiring portion. In order to prevent moisture from entering the lead-out wiring portion, for example, as shown in FIG. 4, a barrier layer 110 is provided in a solar cell 200 to cover and seal the lead-out wiring 107 with a shielding material.
[0021] Furthermore, as a solar cell (unit), the lead wire must be exposed at only its end (extraction portion) without being covered by a barrier layer in order to extract current. Therefore, for example, as shown in FIG. 5, only the end (extraction portion) 5' of the lead wire 5 is exposed without being covered by a barrier layer. A top view (FIG. 5(A)) and a cross-sectional view (FIG. 5(B)) are shown for an example of a solar cell according to the present invention. In the solar cell (unit) 20 shown in FIG. 5, a photoelectric conversion layer (light absorbing layer) 3 and a transparent electrode 4 are provided on a substrate 1, a lead wire 5 is provided on the transparent electrode 4, and a first barrier layer 7 is provided to cover and seal the lead wire 5. However, the end (extraction portion) 5' of the lead wire 5 is exposed without being covered by the first barrier layer 7. For this reason, it is preferable to cover the entire solar cell 20 with a second barrier layer 10 to improve the blocking performance against air and moisture. The end of the lead wire 5 means the end of the lead wire that is close to the extraction electrode for extracting current from the lead wire. In FIG. 5, the end 5' of the lead wire 5 also functions as the extraction electrode.
[0022] Furthermore, the lead wire and the current extraction section (extraction electrode) are separated, and a second barrier layer is provided to cover and seal the entire lead wire, thereby separating the terminal section and the solar cell (unit) 20, thereby further improving the blocking performance. That is, for example, as shown in Fig. 6 (Fig. 6(A): top view, Fig. 6(B): cross-sectional view), a second barrier layer 10 is provided to cover and seal the entire lead wire 5, and an extraction electrode 8 is provided separately on the outside of the barrier layer, thereby finding a configuration that suppresses the intrusion of air and moisture in the atmosphere from the lead wire 5, thereby solving the first problem of the present invention. In Fig. 6, the lead wire 5 and the extraction electrode 8 are not directly connected.
[0023] The solar cell of the present invention has at least a photoelectric conversion layer (light absorbing layer) and a transparent electrode on a substrate. In this specification, the term "layer" refers not only to a layer having a clear boundary, but also to a layer having a concentration gradient in which the contained elements change gradually. The elemental analysis of the layer can be performed, for example, by performing FE-TEM / EDS line analysis measurement of the cross section of the solar cell to confirm the elemental distribution of a specific element. In addition, the term "layer" described in this specification refers not only to a flat thin-film layer, but also to a layer that can form a complex and intricate structure together with other layers.
[0024] <Base material> The substrate is not particularly limited, but is preferably a flexible substrate, and examples thereof include substrates having a heat-resistant polymer such as polyimide or polyester, or a metal foil. Among these, substrates having a polyethylene naphthalate film or a metal foil are preferred. In particular, by using the metal foil, costs can be reduced compared to the case of using a heat-resistant polymer, and high-temperature treatment can be performed. That is, even if thermal annealing (heat treatment) is performed at a temperature of 80 (°C) or higher for the purpose of imparting light resistance (resistance to photodegradation) during the formation of a photoelectric conversion layer containing an organic / inorganic perovskite compound, the occurrence of distortion can be minimized, and high photoelectric conversion efficiency can be obtained.
[0025] The above-mentioned metal foil is not particularly limited, and examples thereof include metal foils made of metals such as aluminum, titanium, copper, and gold, and alloys such as stainless steel (SUS). These may be used alone or in combination of two or more. Aluminum foil is a preferred candidate for the above-mentioned substrate. By using the above-mentioned aluminum foil, costs can be reduced compared to the case of using other metal foils, and workability can be improved due to its flexibility.
[0026] The substrate may consist of only the metal foil. In this case, the metal foil may also function as an electrode. The substrate may further include an insulating layer formed on the metal foil. In this case, it is preferable that the solar cell of the present invention further includes an electrode formed on the insulating layer.
[0027] The insulating layer is not particularly limited, and examples thereof include inorganic insulating layers made of aluminum oxide, silicon oxide, zinc oxide, etc., and organic insulating layers made of epoxy resin, polyimide, etc. Among these, when the metal foil is an aluminum foil, the insulating layer is preferably an aluminum oxide coating. By using the aluminum oxide coating as the insulating layer, it is possible to suppress the deterioration of the photoelectric conversion layer containing the organic-inorganic perovskite compound due to the moisture in the atmosphere penetrating the insulating layer, as compared with the case of an organic insulating layer.
[0028] It is also already known that by using the aluminum oxide coating as the insulating layer, the phenomenon of discoloration and corrosion of the photoelectric conversion layer (light absorption layer) containing an organic-inorganic perovskite compound over time due to contact with the aluminum foil can be suppressed. Note that, in other general solar cells, there have been no reports of the photoelectric conversion layer reacting with aluminum to cause discoloration, and the above-mentioned phenomenon of corrosion occurring is described in a prior-filed publication as a problem specific to perovskite solar cells in which the photoelectric conversion layer contains an organic-inorganic perovskite compound.
[0029] According to the above publication, the thickness of the aluminum oxide coating is not particularly limited, but the preferred lower limit is 0.1 (μm), the preferred upper limit is 20 (μm), and the more preferred lower limit is 0.5 (μm), and the more preferred upper limit is 10 (μm). If the thickness of the aluminum oxide coating is 0.1 (μm) or more, the aluminum oxide coating can sufficiently cover the surface of the aluminum foil, and the insulation between the aluminum foil and the electrode is stable. Furthermore, if the thickness of the aluminum oxide coating is 20 (μm) or less, cracks are unlikely to occur in the aluminum oxide coating even if the substrate is curved. The thickness of the aluminum oxide coating can be measured, for example, by observing the cross section of the substrate with an electron microscope (e.g., S-4800, manufactured by HITACHI, etc.) and analyzing the contrast of the obtained photograph.
[0030] The ratio of the thickness of the aluminum oxide coating to the thickness of the substrate is not particularly limited, but the preferred lower limit of the ratio of the thickness of the aluminum oxide coating to the thickness of the substrate (100%) is 0.1% and the preferred upper limit is 15%. If the ratio is 0.1% or more, the hardness of the aluminum oxide coating increases, and the patterning of the electrode can be performed well while suppressing peeling of the aluminum oxide coating, thereby suppressing the occurrence of insulation failure and conduction failure. If the ratio is 15% or less, when a heat treatment is performed during the formation of a photoelectric conversion layer containing an organic-inorganic perovskite compound, it is possible to suppress the occurrence of cracks in the aluminum oxide coating and / or the electrode formed thereon due to the difference in thermal expansion coefficient with the aluminum foil. This makes it possible to suppress an increase in the resistance value of the solar cell, and to suppress the exposure of the aluminum foil, which causes corrosion of the photoelectric conversion layer containing an organic-inorganic perovskite compound.
[0031] The method for forming the aluminum oxide film is not particularly limited, and examples thereof include a method of anodizing the aluminum foil, a method of applying an aluminum alkoxide or the like to the surface of the aluminum foil, and a method of forming a natural oxide film on the surface of the aluminum foil by heat treatment. Among these, the method of anodizing the aluminum foil is preferred because the entire surface of the aluminum foil can be uniformly oxidized. That is, the aluminum oxide film is preferably an anodized film. When anodizing the aluminum foil, the thickness of the aluminum oxide film can be adjusted by changing the treatment concentration, treatment temperature, current density, treatment time, etc. in the anodization.
[0032] The thickness of the substrate is not particularly limited, but the preferred lower limit is 5 (μm) and the preferred upper limit is 500 (μm). If the thickness of the substrate is 5 (μm) or more, the solar cell can have sufficient mechanical strength and can be made to be easy to handle. Furthermore, by making the thickness of the substrate 500 (μm) or less, a solar cell with excellent flexibility can be realized. The more preferred lower limit of the thickness of the substrate is 10 (μm), and the more preferred upper limit is 100 (μm). The thickness of the substrate means the thickness of the entire substrate including the metal foil and the insulating layer when the substrate has the metal foil and an insulating layer formed on the metal foil.
[0033] As described above, when the substrate has a metal foil and an insulating layer formed on the metal foil, it is preferable that the substrate has an electrode formed on the insulating layer.
[0034] <Electrodes and transparent electrode materials> Either of the electrode and the transparent electrode may be a cathode or an anode. Examples of materials for the electrode and the transparent electrode include metals such as FTO (fluorine-doped tin oxide), sodium, sodium-potassium alloy, lithium, magnesium, aluminum, magnesium-silver mixture, magnesium-indium mixture, aluminum-lithium alloy, Al / Al2O3 mixture, Al / LiF mixture, gold, etc., conductive transparent materials such as CuI, ITO (indium tin oxide), SnO2, AZO (aluminum zinc oxide), IZO (indium zinc oxide), GZO (gallium zinc oxide), conductive transparent polymers, etc. These materials may be used alone or in combination of two or more.
[0035] <Photoelectric conversion layer: organic-inorganic perovskite compound> The photoelectric conversion layer (light absorbing layer) 102 includes an organic-inorganic perovskite compound. By using an organic-inorganic perovskite compound in the photoelectric conversion layer, the photoelectric conversion efficiency of the solar cell can be improved. The organic-inorganic perovskite compound is preferably represented by the general formula RM-X3 (wherein R is an organic molecule, M is a metal atom, and X is a halogen atom or a chalcogen atom).
[0036] R is an organic molecule, C l N m H n (l, m, and n are all positive integers). Specific examples of R include methylamine, ethylamine, propylamine, butylamine, pentylamine, hexylamine, dimethylamine, diethylamine, dipropylamine, dibutylamine, dipentylamine, dihexylamine, trimethylamine, triethylamine, tripropylamine, tributylamine, tripentylamine, trihexylamine, ethylmethylamine, methylpropylamine, butylmethylamine, methylpentylamine, hexylmethylamine, ethylpropylamine, ethylbutylamine, imidazole, azole, pyrrole, aziridine, azirine, azetidine, azeto, imidazoline, carbazole, methylcarboxyamine, ethylcarboxyamine, propylcarboxyamine, butylcarboxyamine, pentylcarboxyamine, hexylcarboxyamine, formamidinium, guanidine, aniline, pyridine, and ions thereof (e.g., methylammonium (CH3NH3), etc.), and phenethylammonium, etc. Among these, methylamine, ethylamine, propylamine, propylcarboxyamine, butylcarboxyamine, pentylcarboxyamine, formamidinium, guanidine, and ions thereof are preferred, and methylamine, ethylamine, pentylcarboxyamine, formamidinium, guanidine, and ions thereof are more preferred. Among these, methylamine, formamidinium, and ions thereof are even more preferred because they provide high photoelectric conversion efficiency.
[0037] The above M is a metal atom, and examples thereof include lead, tin, zinc, titanium, antimony, bismuth, nickel, iron, cobalt, silver, copper, gallium, germanium, magnesium, calcium, indium, aluminum, manganese, chromium, molybdenum, and europium. Among these, lead or tin is preferred from the viewpoint of overlapping of electron orbitals. These metal atoms may be used alone or in combination of two or more.
[0038] The X is a halogen atom or a chalcogen atom, such as chlorine, bromine, iodine, sulfur, and selenium. These halogen atoms or chalcogen atoms may be used alone or in combination of two or more. Among them, halogen atoms are preferred because the organic-inorganic perovskite compound is soluble in an organic solvent by containing halogen in the structure, and can be applied to inexpensive printing methods and the like. Furthermore, iodine is more preferred because the energy band gap of the organic-inorganic perovskite compound is narrowed.
[0039] The organic inorganic perovskite compound preferably has a cubic structure in which a metal atom M is arranged at the body center, an organic molecule R is arranged at each vertex, and a halogen atom or chalcogen atom X is arranged at the face center. FIG. 1 is a schematic diagram showing an example of a crystal structure of a general organic inorganic perovskite compound having a cubic structure in which a metal atom M is arranged at the body center, an organic molecule R is arranged at each vertex, and a halogen atom or chalcogen atom X is arranged at the face center. Although the details are not clear, it is presumed that the above structure allows the orientation of the octahedron in the crystal lattice to be easily changed, thereby increasing the mobility of electrons in the organic inorganic perovskite compound and improving the photoelectric conversion efficiency of the solar cell.
[0040] The organic inorganic perovskite compound is preferably a crystalline semiconductor. A crystalline semiconductor means a semiconductor in which a scattering peak can be detected by measuring an X-ray scattering intensity distribution. If the organic inorganic perovskite compound is a crystalline semiconductor, the mobility of electrons in the organic inorganic perovskite compound is increased, and the photoelectric conversion efficiency of the solar cell is improved. In addition, if the organic inorganic perovskite compound is a crystalline semiconductor, the decrease in photoelectric conversion efficiency (photodegradation) caused by continuous irradiation of light to the solar cell, particularly photodegradation caused by a decrease in short-circuit current, is easily suppressed.
[0041] <Indicators of crystallization> Generally, the degree of crystallization is evaluated as an index of crystallization. The degree of crystallization can be obtained by separating the scattering peak derived from the crystalline material and the halo derived from the amorphous part detected by X-ray scattering intensity distribution measurement by fitting, obtaining the respective intensity integrals, and calculating the ratio of the crystalline part to the whole. The preferable lower limit of the degree of crystallization of the organic-inorganic perovskite compound is 30(%), and if the degree of crystallization is 30(%) or more, the mobility of electrons in the organic-inorganic perovskite compound is improved, and the photoelectric conversion efficiency of the solar cell is increased. In addition, if the above-mentioned degree of crystallization is 30(%) or more, the decrease in the photoelectric conversion efficiency (photodegradation) caused by continued irradiation of light to the solar cell, particularly photodegradation caused by a decrease in short-circuit current, is easily suppressed. The more preferable lower limit of the above-mentioned degree of crystallization is 50(%), and the even more preferable lower limit is 70(%). In addition, examples of methods for increasing the degree of crystallization of the above-mentioned organic-inorganic perovskite compound include thermal annealing (heat treatment), irradiation with strong light such as a laser, and plasma irradiation.
[0042] In addition, the crystallite size can be evaluated as another index of crystallization. The crystallite size can be calculated by the Halder-Wagner method from the half-width of the scattering peak derived from the crystalline substance detected by X-ray scattering intensity distribution measurement. If the crystallite size of the organic-inorganic perovskite compound is 5 (nm) or more, the decrease in photoelectric conversion efficiency (photodegradation) caused by continuous irradiation of light to the solar cell, particularly photodegradation caused by a decrease in short-circuit current, is suppressed. In addition, the mobility of electrons in the organic-inorganic perovskite compound is increased, and the photoelectric conversion efficiency of the solar cell is improved. A more preferable lower limit of the crystallite size is 10 (nm), and a further more preferable lower limit is 20 (nm).
[0043] <Photoelectric conversion layer (light absorption layer)> The photoelectric conversion layer (light absorbing layer) may further contain an organic semiconductor or an inorganic semiconductor in addition to the organic-inorganic perovskite compound, as long as the effect of the present invention is not impaired. Examples of organic semiconductors include compounds having a thiophene skeleton, such as polythiophene (3-alkylthiophene). Examples of conductive polymers having a polyparaphenylenevinylene skeleton, a polyvinylcarbazole skeleton, a polyaniline skeleton, a polyacetylene skeleton, and the like. Examples of compounds having a porphyrin skeleton, such as a phthalocyanine skeleton, a naphthalocyanine skeleton, a pentacene skeleton, a benzoporphyrin skeleton, and the like, a spirobifluorene skeleton, and carbon-containing materials such as carbon nanotubes, graphene, and fullerene, which may be surface-modified, are also included.
[0044] Examples of inorganic semiconductors include titanium oxide, zinc oxide, indium oxide, tin oxide, gallium oxide, tin sulfide, indium sulfide, zinc sulfide, CuSCN, Cu2O, CuI, MoO3, V2O5, WO3, MoS2, MoSe2, and Cu2S.
[0045] When the photoelectric conversion layer (light absorbing layer) contains an organic / inorganic perovskite compound and an organic semiconductor or an inorganic semiconductor, it may be a laminate in which a thin-film organic semiconductor or inorganic semiconductor portion is laminated with a thin-film organic / inorganic perovskite compound portion, or it may be a composite film in which an organic semiconductor or inorganic semiconductor portion is composited with an organic / inorganic perovskite compound portion. A laminate that is easy to manufacture in mass production is preferred, while a composite film is preferred in terms of being able to improve the charge separation efficiency in the organic semiconductor or inorganic semiconductor.
[0046] The thickness of the portion formed of the organic-inorganic perovskite compound has a preferred lower limit of 5 nm and a preferred upper limit of 1000 nm. If the thickness is 5 nm or more, light can be absorbed sufficiently, and the photoelectric conversion efficiency is high. However, as the thickness increases, the resistance value also increases, and the loss during extraction of electrons and holes also increases, resulting in a decrease in efficiency.
[0047] Therefore, in the present invention, as will be described in detail later, sunlight is concentrated by the lens action of the optical element formed on the barrier layer surface. As a result, sunlight passes obliquely through the photoelectric conversion layer, thereby obtaining a photoelectric conversion efficiency equivalent to that of a thick photoelectric conversion layer, and a first effect unique to the present invention can be obtained, which is that high photoelectric conversion efficiency and low loss can be achieved at the same time.
[0048] When the light absorption layer (photoelectric conversion layer) is a composite film formed by providing multiple layers of organic-inorganic perovskite compound moieties as shown in Figures 4, 16 and 17, the preferred lower limit of the thickness of the composite film is 30 nm, and the preferred upper limit is 2000 (nm). Furthermore, if the thickness is 30 (nm) or more, sufficient light can be absorbed, and the photoelectric conversion efficiency is high.
[0049] At this time, by providing a shaped optical element on the surface of the barrier layer, sunlight is concentrated by the lens action of this optical element. As a result, the sunlight passes through the photoelectric conversion layer at an angle, and the photoelectric conversion efficiency equivalent to that of a thick photoelectric conversion layer can be obtained, and the first effect unique to the present invention can be obtained, which is that high photoelectric conversion efficiency and low loss can be simultaneously achieved. With this configuration, even if the thickness is 1500 (nm) or less, sunlight passes through the photoelectric conversion part at an angle, making it easier for charges to reach the electrode, and the photoelectric conversion efficiency is increased.
[0050] It is preferable that the photoelectric conversion layer is subjected to thermal annealing (heat treatment) after the formation of the photoelectric conversion layer. By performing thermal annealing (heat treatment), the crystallinity of the organic-inorganic perovskite compound in the photoelectric conversion layer can be increased, and the decrease in photoelectric conversion efficiency (photodegradation) caused by continued irradiation with light can be further suppressed. When such thermal annealing (heat treatment) is performed on a solar cell using a substrate made of a conventional heat-resistant polymer, distortion occurs during annealing due to the difference in thermal expansion coefficient between the substrate and the photoelectric conversion layer, etc., and as a result, it becomes difficult to achieve high photoelectric conversion efficiency. When the above-mentioned metal foil is used, it is preferable because it is possible to minimize the occurrence of distortion and obtain high photoelectric conversion efficiency even when thermal annealing (heat treatment) is performed.
[0051] When the thermal annealing (heat treatment) is performed, the temperature at which the photoelectric conversion layer is heated is not particularly limited, but is preferably 100 (°C) or higher and lower than 250 (°C). If the heating temperature is 100 (°C) or higher, the crystallinity of the organic-inorganic perovskite compound can be sufficiently increased. If the heating temperature is lower than 250 (°C), the heat treatment can be performed without thermally deteriorating the organic-inorganic perovskite compound. More preferably, the heating temperature is 120 (°C) or higher and 200 (°C) or lower. In addition, the heating time is not particularly limited, but is preferably 3 minutes or more and 2 hours or less. If the heating time is 3 minutes or more, the crystallinity of the organic-inorganic perovskite compound can be sufficiently increased. If the heating time is 2 hours or less, the heat treatment can be performed without thermally deteriorating the organic-inorganic perovskite compound. These heating operations are preferably performed in a vacuum or in an inert gas, and the dew point temperature is preferably 10 (°C) or lower, more preferably 7.5 (°C) or lower, and even more preferably 5 (°C) or lower.
[0052] The solar cell of the present invention may have an electron transport layer between the cathode side of the substrate and the transparent electrode and the photoelectric conversion layer. The material of the electron transport layer is not particularly limited, and examples thereof include N-type conductive polymers, N-type low molecular weight organic semiconductors, N-type metal oxides, N-type metal sulfides, alkali metal halides, alkali metals, surfactants, etc., and specific examples thereof include cyano group-containing polyphenylene vinylene, boron-containing polymers, bathocuproin, bathophenanthrene, hydroxyquinolinatoaluminum, oxadiazole compounds, benzimidazole compounds, naphthalene tetracarboxylic acid compounds, perylene derivatives, phosphine oxide compounds, phosphine sulfide compounds, fluoro group-containing phthalocyanines, titanium oxide, zinc oxide, indium oxide, tin oxide, gallium oxide, tin sulfide, indium sulfide, zinc sulfide, etc.
[0053] The electron transport layer may be composed of only a thin-film electron transport layer (buffer layer), but preferably includes a porous electron transport layer. In particular, when the photoelectric conversion layer is a composite film obtained by combining an organic semiconductor or an inorganic semiconductor portion with an organic-inorganic perovskite compound, a more complex composite film (a more complex and intricate structure) is obtained, and the photoelectric conversion efficiency is increased, so that the composite film is preferably formed on the porous electron transport layer.
[0054] The thickness of the electron transport layer is preferably 1 nm at the lower limit and 2000 nm at the upper limit. If the thickness is 1 nm or more, holes can be blocked sufficiently. If the thickness is 2000 nm or less, resistance during electron transport is unlikely to occur, and photoelectric conversion efficiency is high. The thickness of the electron transport layer is more preferably 3 nm at the lower limit and 1000 nm at the upper limit, and even more preferably 5 nm at the lower limit and 500 nm at the upper limit.
[0055] The solar cell of the present invention may have a hole transport layer between the photoelectric conversion layer and the anode side of the substrate and the transparent electrode. The material of the hole transport layer is not particularly limited, and examples thereof include P-type conductive polymers, P-type low molecular weight organic semiconductors, P-type metal oxides, P-type metal sulfides, surfactants, etc., and specifically, examples thereof include compounds having a thiophene skeleton such as poly(3-alkylthiophene). Examples of the conductive polymers include those having a triphenylamine skeleton, a polyparaphenylenevinylene skeleton, a polyvinylcarbazole skeleton, a polyaniline skeleton, a polyacetylene skeleton, etc. Further examples include compounds having a porphyrin skeleton such as a phthalocyanine skeleton, a naphthalocyanine skeleton, a pentacene skeleton, a benzoporphyrin skeleton, or the like, a spirobifluorene skeleton, or the like; molybdenum oxide, vanadium oxide, tungsten oxide, nickel oxide, copper oxide, tin oxide, molybdenum sulfide, tungsten sulfide, copper sulfide, tin sulfide, or the like; fluoro group-containing phosphonic acid, carbonyl group-containing phosphonic acid, copper compounds such as CuSCN and CuI; and carbon-containing materials such as carbon nanotubes and graphene.
[0056] The hole transport layer may be partially immersed in the photoelectric conversion layer, or may be disposed in the form of a thin film on the photoelectric conversion layer. When the hole transport layer is in the form of a thin film, the preferred lower limit of the thickness is 1 (nm), and the preferred upper limit is 2000 (nm). If the thickness is 1 (nm) or more, electrons can be blocked sufficiently. If the thickness is 2000 (nm) or less, the layer is unlikely to become a resistance during hole transport, and the photoelectric conversion efficiency is high. The more preferred lower limit of the thickness is 3 (nm), and the more preferred upper limit is 1000 (nm), and the even more preferred lower limit is 5 (nm), and the even more preferred upper limit is 500 (nm).
[0057] The solar cell of the present invention further includes an extraction wiring disposed on the transparent electrode. By providing the extraction wiring, high photoelectric conversion efficiency can be obtained even if the area of the transparent electrode is large.
[0058] The lead wiring is not particularly limited as long as it is made of a conductive material, and examples thereof include wiring made of metals such as copper, aluminum, silver, gold, platinum, etc., or alloys thereof, and wiring made of carbon. These may be used alone or in combination of two or more. When the lead wiring is made of silver, it is formed on the transparent electrode using, for example, silver paste.
[0059] The shape of the lead wire is not particularly limited, and examples thereof include a line shape (multiple lines), a lattice shape, a mesh shape, etc. These shapes may be used alone, or two or more kinds may be used in combination.
[0060] The width of the lead wiring is not particularly limited, but a preferable lower limit is 5 (μm), and a preferable upper limit is 500 (μm). If the width of the lead wiring is 5 (μm) or more, the resistance of the lead wiring can be reduced. If the width of the lead wiring exceeds 500 (μm), the area where the incident light is blocked increases, and the photoelectric conversion efficiency of the solar cell may decrease. A more preferable lower limit of the width of the lead wiring is 10 (μm), and a more preferable upper limit is 200 (μm). The width of the lead wiring can be measured, for example, by an optical microscope with a length measurement function, a line width measurement device, or the like.
[0061] <Barrier layer> The solar cell 20 of the present invention further includes a second barrier layer 10 that entirely covers and seals the lead wire 5, and an extraction electrode 8 disposed on the transparent electrode 4 outside the barrier layer 10 (see FIG. 6). By providing the second barrier layer 10 that entirely covers and seals the lead wire 5 and separately providing the extraction electrode 8 outside the second barrier layer 10, it is possible to suppress the intrusion of moisture in the atmosphere from the lead wire 5. This makes it possible to suppress deterioration of the photoelectric conversion layer due to the intrusion of moisture in the atmosphere. On the other hand, the lead wire 5 and the extraction electrode 8 are not connected and are separated, but a current flows from the end of the lead wire 5 through the transparent electrode 4 and then to the extraction electrode 8, so that current can be extracted without any problem.
[0062] The materials of the first barrier layer 7 and the second barrier layer 10 shown in Fig. 5 and Fig. 6 will be described below. The material of the first barrier layer 7 is not particularly limited as long as it has water vapor barrier properties, but inorganic materials are preferable. Examples of the inorganic materials include oxides, nitrides, and oxynitrides of Si, Al, Zn, Sn, In, Ti, Mg, Zr, Ni, Ta, W, Cu, or alloys containing two or more of these. Among them, oxides, nitrides, and oxynitrides of metal elements containing both metal elements Zn and Sn are preferable in order to impart water vapor barrier properties and flexibility to the barrier layer.
[0063] When the material of the first barrier layer 7 is an inorganic material, the thickness of the first barrier layer 7 (inorganic layer) is preferably 30 nm in lower limit and 2500 nm in upper limit. If the thickness is 30 nm or more, the inorganic layer can have sufficient water vapor barrier properties, and the durability of the solar cell is improved. If the thickness is 2500 nm or less, even if the thickness of the inorganic layer increases, the generated stress is small, so that peeling between the inorganic layer and other layers can be suppressed. The more preferable lower limit of the thickness is 50 nm, the more preferable upper limit is 1500 nm, the even more preferable lower limit is 100 nm, and the even more preferable upper limit is 1200 nm. The thickness of the inorganic layer can be measured using an optical interference type film thickness measuring device (for example, FE-3000 manufactured by Otsuka Electronics Co., Ltd.).
[0064] Of the materials for the first barrier layer 7, preferred methods for covering and sealing the entire lead wiring 5 with the inorganic material include vacuum deposition, sputtering, chemical vapor deposition (CVD), and ion plating. Of these, sputtering is preferred for forming a dense layer, and among sputtering methods, DC magnetron sputtering is more preferred. In the sputtering method, a metal target and oxygen gas or nitrogen gas are used as raw materials, and the raw materials are deposited on the lead wiring to form a film, thereby forming an inorganic layer made of an inorganic material.
[0065] The first barrier layer 7 is not necessarily required to be formed, but it is preferable to form the first barrier layer 7 from the viewpoint of further improving the water vapor barrier property.
[0066] Next, the material of the second barrier layer 10 will be described. The second barrier layer 10 formed on the outer periphery of the above-mentioned solar cell is formed by applying a precursor, PHPS (Perhydro-polysilazane), by the method shown in "An Ultra-High Barrier Like Glass that Can be Created by Printing" shown in Non-Patent Document 1, and irradiating VUV (Vacuum Ultra Violet) light for a specific time in an inert gas atmosphere such as nitrogen to form a thin film containing silicon nitride that has high transparency against ultraviolet rays and near-infrared rays and has a blocking property like glass. This second barrier layer 10 can be formed by a wet process by making the film thickness of the precursor uniform with a spin coater or roll-roll, and has a great advantage in that a manufacturing process with reduced investment can be realized compared to a dry film formation process.
[0067] Although PHPS (perhydropolysilazane) is exemplified as a precursor material used for forming the second barrier layer 10, the precursor can be any compound having a silazane skeleton, i.e., a polysilazane compound, without any particular limitation. Polysilazane is a polymer having a silicon-nitrogen bond, and is a ceramic precursor inorganic polymer. Examples of polysilazane compounds include perhydropolysilazane and organopolysilazane in which a part of the hydrogen atom portion bonded to Si is substituted with an alkyl group or the like. Examples of the alkyl group include linear, branched, or cyclic alkyl groups having 1 to 8 carbon atoms. Among these, perhydropolysilazane is particularly preferable from the viewpoint of the denseness of the resulting water vapor barrier layer.
[0068] The solvent for preparing the coating solution containing the polysilazane compound is not particularly limited as long as it can dissolve polysilazane, and examples thereof include pentane, hexane, cyclohexane, toluene, xylene, Solvesso, Turbine, methylene chloride, trichloroethane, ethyl acetate, butyl acetate, acetone, methyl ethyl ketone, dibutyl ether, dioxane, tetrahydrofuran, dibutyl ether, mono- and polyalkylene glycol dialkyl ethers (diglymes), and the like.
[0069] The coating solution containing the polysilazane compound is coated and dried, and then irradiated with vacuum ultraviolet light (VUV) in an inert gas atmosphere such as nitrogen or argon, or in a vacuum atmosphere, to be modified into a dense barrier layer containing silicon nitride (second barrier layer 10). The second barrier layer 10 may contain silicon oxynitride within a range that does not impair the performance as a water vapor barrier layer.
[0070] The thickness of the second barrier layer 10 has a preferred lower limit of 100 (nm) and a preferred upper limit of 500 (nm). If the thickness is 100 (nm) or more, the barrier layer can have sufficient water vapor barrier properties, and the durability of the solar cell is improved. If the thickness is 500 (nm) or less, even if the thickness of the barrier layer increases, the generated stress is small, so that peeling between the barrier layer and other layers and the generation of cracks in the barrier layer can be suppressed. A more preferred lower limit of the thickness is 150 (nm), and a more preferred upper limit is 350 (nm).
[0071] Furthermore, in the present invention, as described above, the second barrier layer 10 obtained by film formation through a wet process by coating is formed on the surface of the precursor by using a roll or stamper having a very fine moth-eye master pattern formed on its surface to impart specific optical properties to the surface of the precursor, and then the surface of the second barrier layer 10 is irradiated with VUV light to impart new optical properties to the surface of the second barrier layer 10, thereby adding new value in the form of reduced reflection loss of sunlight in addition to the moisture and air blocking effect, as will be described in detail later.
[0072] <Extraction electrode> The extraction electrode is not particularly limited as long as it is an electrode made of a conductive material, and examples thereof include an electrode made of the same material as the extraction wiring. The extraction electrode may be disposed on the transparent electrode outside the barrier layer, and is preferably disposed linearly along at least one of the four sides of the solar cell. Furthermore, it is more preferable that the extraction electrode is disposed linearly so as to be perpendicular to the extraction wiring that is disposed linearly (multiple linearly). This allows for better current extraction.
[0073] FIG. 5 is a top view (FIG. 5(A)) and a cross-sectional view (FIG. 5(B)) that typically show an example of a solar cell of the present invention. In FIG. 5, a photoelectric conversion layer (light absorbing layer) 3 and a transparent electrode 4 are provided on a substrate 1, lead wires 5 are provided in a linear shape (multiple lines) on the transparent electrode 4, and a first barrier layer 7 that covers and seals the lead wires 5 is provided. Here, the lead wires 5 are entirely covered and sealed by the first barrier layer 7, and no exposed portion is not covered by the first barrier layer 7. Furthermore, by providing a second barrier layer 10 that covers the entire outer extension portion of the solar cell unit 20, the barrier properties can be further improved.
[0074] In another embodiment of the present invention shown in Figure 6 (Figure 6(A): top view, Figure 6(B): cross-sectional view), an extraction electrode 8 is provided linearly on the outside of the first barrier layer 7 on the transparent electrode 4. In this opening, the extraction wiring 5 and the extraction electrode 8 are not directly connected but are separated, but the current flows from the end of the extraction wiring 5 through the transparent electrode 4 and then to the extraction electrode 8. For this reason, current can be extracted without any problems. Note that, although an outer frame 2 and a planarization layer 6 made of an insulating layer are also provided in Figure 4 as described below, the solar cell of the present invention does not necessarily have to have these.
[0075] As described above, in one embodiment of the solar cell of the present invention, the lead wire 5 and the extraction electrode 8 are not connected but are separated, but the current flows from the end of the lead wire 5 through the transparent electrode 4 and then to the extraction electrode 8, so that the current can be extracted without any problem. From the viewpoint of reducing resistance, the width of the end of the lead wire 5 is preferably equal to or greater than the width of the other part of the lead wire 5, and more preferably equal to or greater than twice the width of the other part. The end of the lead wire means the end of the lead wire that is closer to the extraction electrode, and the other part of the lead wire means the part other than the end of the lead wire.
[0076] 7 and 8 are top views showing an example of the end of the lead wiring in the solar cell of the present invention. In FIG. 7 and FIG. 8, the lead wiring 5 is provided in a line shape (multiple lines), and the shape of the end of the lead wiring 5 can be said to be "end connection type" and "T-shaped", respectively. As shown in the "end connection type" in FIG. 7, the lead wiring 5 may have wiring that is perpendicular to the multiple lead wirings 5 or has a similar wiring so that the multiple lead wirings 5 are connected to each other at their ends. In FIG. 7 and FIG. 8, the width of the end of the lead wiring 5 is made larger than the width of the other part. As a result, the resistance can be reduced and a higher photoelectric conversion efficiency can be obtained.
[0077] In addition, the distance (creepage distance) from the end of the lead wiring to the end of the barrier layer is preferably long from the viewpoint of water vapor barrier properties, and is preferably short from the viewpoint of reducing resistance. The shorter the distance from the end of the lead wiring to the end of the barrier layer, the shorter the distance from the end of the lead wiring to the extraction electrode, so that the distance through which the current passes through the transparent electrode is shortened, and as a result, the resistance can be reduced. As a method for achieving both water vapor barrier properties and reduced resistance, for example, a method of providing additional wiring that is separated into multiple sections between the end of the lead wiring and the end of the barrier layer can be mentioned. This increases the effective creepage distance, thereby improving the water vapor barrier properties. On the other hand, the distance through which the current passes through the transparent electrode is shortened, so that the resistance can be reduced. A plurality of the above-mentioned wirings may be provided to achieve further low resistance.
[0078] 9A and 9B are top views (FIGS. 9A and 9B) showing schematic diagrams of an example of an end of an extraction wiring 5 in a solar cell of the present invention. As shown in FIG. 9B, the solar cell of the present invention may have an additional wiring 9 that separates the solar cell into multiple sections between the end of the extraction wiring 5 and the end of the first barrier layer 7. In this case, it goes without saying that a second barrier layer 10 is provided on the outermost periphery of the solar cell 20.
[0079] If necessary, the solar cell of the present invention may further have an outer frame 2 made of an insulating layer that is arranged under the transparent electrode 4 so as to surround the side surfaces of the photoelectric conversion layer (light absorbing layer) 3. By arranging the outer frame made of the insulating layer around the photoelectric conversion layer, it is possible to suppress the intrusion of moisture from the end of the photoelectric conversion layer, thereby improving the reliability of the solar cell.
[0080] Insulating layer The material of the outer frame 2 made of the insulating layer is not particularly limited as long as it has water vapor barrier properties, and may be an inorganic insulating material or an organic insulating material. Examples of inorganic insulating materials include inorganic oxides such as SiO2, Al2O3, and ZrO, glass, and grates. Organic insulating materials preferably have sufficiently good heat resistance, and examples of such organic insulating materials include thermosetting polyimide.
[0081] <Planarization film> The solar cell of the present invention may further include a planarization layer 6 disposed between the transparent electrode 4 and the barrier layer 7, as necessary. The material of the planarization layer 6 is not particularly limited as long as it has water vapor barrier properties, and examples of the material include thermosetting resins and thermoplastic resins. Examples of the thermosetting resins and thermoplastic resins include epoxy resins, acrylic resins, silicone resins, phenolic resins, melamine resins, urea resins, butyl rubber, polyesters, polyurethanes, polyethylene, polypropylene, polyvinyl chloride, polystyrene, polyvinyl alcohol, polyvinyl acetate, ABS resins, polybutadiene, polyamides, polycarbonates, polyimides, and polyisobutylene.
[0082] The planarization layer described above may be a barrier layer obtained by applying PHPS (Perhydro-polysilazane) as a precursor between the two layers and irradiating VUV (Vacuum Ultra Violet) light for a specific period of time in an inert gas atmosphere such as nitrogen, and using this barrier layer as an adhesive layer (planarization layer). The planarization layer obtained in this case has high transparency and is made of inorganic materials (SiN X ), a planarization layer with high resistance to heat and ultraviolet rays can be realized. When a barrier layer containing silicon nitride using the above-mentioned PHPS as a precursor is applied as a barrier layer formed on the outer periphery of a solar cell, it is preferable to use a silicone resin (polydimethylsiloxane) as the planarization layer 6, which also functions as an impact buffer layer.
[0083] When the material forming the planarization layer 6 is a thermosetting resin or a thermoplastic resin, the method of covering and sealing the entire lead-out wiring is not particularly limited, and examples thereof include a method of sealing the entire lead-out wiring using a sheet-shaped planarization layer material, a method of applying a solution in which the planarization layer material is dissolved in an organic solvent to the entire lead-out wiring, a method of applying a liquid monomer that will become the planarization layer to the entire lead-out wiring and then crosslinking or polymerizing the liquid monomer with heat or UV, etc., and a method of applying heat to the planarization layer material to melt it and then cooling it.
[0084] The solar cell of the present invention may further be covered with, for example, a resin film, a resin film covered with the above-mentioned single or multiple barrier layers, or other materials, etc. This makes it possible to sufficiently block water vapor even if there is a pinhole in the barrier layer, and further improves the durability of the solar cell.
[0085] <Ultrafine optical elements provided in barrier layer> The ultrafine optical elements provided on at least the surface of the solar light incident side of the barrier layer 110 of the solar cell element shown in FIG. 4 and the second barrier layer 10 of the solar cell shown in FIG. 5 and FIG. 6 will be described in detail below. The above-mentioned organic / inorganic perovskite solar cell can be formed by dividing the material into multiple layers of a desired thickness and forming a film in a coating process, which not only reduces material costs but also allows for inexpensive production by roll-to-roll. On the other hand, a specific technology for realizing the moisture shielding problem of this solar cell is a method disclosed in "Ultra-high barrier like glass that can be created by printing" published in Non-Patent Document 1, in which a precursor PHPS is applied and VUV (Vacuum Ultra Violet) light is irradiated for a specific time in an inert gas atmosphere such as nitrogen to form a thin film that is highly transparent to visible light and near-infrared light and has the same shielding properties and hardness as glass.
[0086] As described above, this barrier film can be formed by a wet process by uniformly thickening the precursor film using roll-to-roll techniques. The master shapes of the ultrafine structured first optical element and the finely shaped second optical element are provided on the surface of the roll, and the shape of the roll surface is transferred to the precursor surface, followed by irradiating it with VUV light to impart the desired shape to the surfaces of the barrier layer 110 and the second barrier layer 10.
[0087] By providing a moth-eye shape as an ultrafine shape to at least the sunlight incident surface of the barrier layer, it is possible to significantly reduce the reflection loss of sunlight to the solar cell element 200 and solar cell 20 of the present invention shown in Figures 4 to 6. As is widely known, the reflection loss reduction effect of this moth-eye shape has little dependence on the sunlight incidence angle and also has the same dependence on the wavelength.
[0088] Due to changes in the position of the sun, the angle of incidence of light on the solar cell and the wavelength components of the emitted light change, so even if a general anti-reflection film is formed on the surface of a solar cell element or solar cell, the angle dependency and wavelength dependency of the reflectance cannot be eliminated. Therefore, by providing ultra-fine optical elements with a moth-eye shape with a pitch P0 of 100 to 200 nm formed on the surface of the barrier layer, a solar cell element and solar cell with an anti-reflection effect that is almost completely independent of the incidence angle and wavelength, which is different from the general anti-reflection film described above, can be realized, and the photoelectric conversion efficiency of the entire system can be increased by reducing reflection loss.
[0089] Moth-eye shaped ultrafine optical elements 110A shown in Fig. 10 and Fig. 11 (schematic cross-sectional views of the barrier layer) are provided on the sunlight incident side of the barrier layer 110 of the solar cell element 200 shown in Fig. 4 and the second barrier layer 10 provided on the outermost periphery of the solar cell 20 shown in Fig. 5 and 6. For convenience, the moth-eye shape of the ultrafine optical elements 110A shown in Fig. 11 is omitted. As shown in Fig. 10, this cross-sectional shape can minimize reflection loss by changing the average value of the refractive index n of the substrate and the refractive index (1.0) of air linearly (linear function) with respect to the height h of the moth-eye structure. In the moth-eye structure of the present invention, the tip portion T0 of the protrusion is elliptical in shape as shown in FIG. 10. This shape is preferably an elliptical shape with a minor axis length of 1 / 5 to 1 / 10 of the pitch P0 of the protrusions. As described above, by making the tip portion of the protrusion elliptical, releasability from the mold can be ensured. In addition, by making the connecting portion between the protrusions flat and forming a concave surface on the sunlight incidence side, both the processing accuracy of the mold and the releasability of the molded product from the mold can be improved at the same time. As a result, the ultrafine optical elements 110A provided on the surface of the barrier layer 110 and the second barrier layer 10 can have good shape accuracy.
[0090] The precursor PHPS was applied to the substrate by the method disclosed in "Ultra-high barrier like glass that can be created by printing" published in Non-Patent Document 1, and the irradiation intensity was 20 (mW / cm) in an inert gas atmosphere such as nitrogen. 2 ) and irradiated with VUV light of wavelength 172 (nm). Figure 12 is a characteristic diagram showing the results of measuring the refractive index distribution of the barrier film formed in the thickness direction when the irradiation time is used as a parameter. The bar graph shown on the far left shows the result of measuring the refractive index of PHPS, the precursor of the barrier layer, for light of 850 (nm) (n = 1.54), and the state of a coating thickness of 357 (nm) and irradiation time of 0 (min). On the other hand, the rightmost bar graph shows the thickness of the barrier film formed with VUV light irradiation time of 60 (min) with a thickness of 281 (nm), and the refractive index is 68 (nm) for the part with a refractive index of 1.76, 92 (nm) for the part with a refractive index of 1.65, and 117 (nm) for the part with a refractive index of 1.56, which shows that the refractive index of the part close to the irradiation light source is high, and the refractive index of the part farther away approaches that of the precursor. Furthermore, a SiO2 film with a thickness of 3 to 4 (nm) is formed on the outermost surface layer, and this film thickness does not change depending on the irradiation time of VUV light.
[0091] As described above, FIG. 12 shows the VUV light irradiation intensity of 20 (mW / cm 2This is a characteristic diagram showing the results of measuring the refractive index distribution of the barrier film formed in the thickness direction when the irradiation time was changed to 5, 10, 20, and 60 minutes with the temperature kept constant. Since a thin SiO2 film was formed on the surface layer regardless of the irradiation time, it is possible that residual components in the atmosphere were formed on the surface layer, but as a result, high transmittance was achieved from the visible light region to the near-infrared light region.
[0092] When optimizing the shape of the moth-eye protrusions, which are ultra-fine optical shapes, on the surface of the barrier layer (film) formed by the above-mentioned method, it is necessary to optimally design them taking into account the refractive index change described above.
[0093] Figure 13 is a characteristic diagram summarizing the relationship between the average refractive index and the thickness of the barrier film (layer) formed using the above-mentioned VUV light irradiation time as a parameter. The thickness decreases in inverse proportion to the VUV light irradiation time, while the refractive index increases inversely. The slope of this trend differs between within 1 minute, 1 to 5 minutes, 5 to 10 minutes, and 10 minutes or more, with the largest change in the first minute. From this result, it was estimated that the largest density change occurs in the first minute.
[0094] The spectral energy distribution of sunlight, which is an energy source for power generation, is shown in FIG. 14. Although there is an absorption characteristic at a specific wavelength due to the absorption of components contained in the Earth's atmosphere, the energy peak is in the visible light region of 450 (nm) to 700 (nm), and it is known that strong energy exists in the near infrared region (B) and far infrared region (C) in addition to the visible light region (A) including the ultraviolet region. Therefore, in the solar cell element and solar cell of the present invention, taking into consideration the spectral energy distribution of sunlight, for example, as shown in FIG. 4 and FIG. 16, a plurality of light absorbing layers (first light absorbing layer 102A, second light absorbing layer 102B, and third light absorbing layer 102C in FIG. 4, and first light absorbing layer 202, second light absorbing layer 203, and third light absorbing layer 204 in FIG. 16) are provided, and the light absorbing member having the highest photoelectric conversion efficiency is contained in each layer (top layer, middle layer, and bottom layer) for each wavelength shown in the characteristic diagram that shows the sensitivity characteristic of the light absorbing layer to the spectral energy characteristic of sunlight shown in FIG. 15. As a result, photoelectric conversion can be performed with high efficiency by the light absorption layer (light conversion layer) provided in a divided form in a plurality of layers.
[0095] <Micro-optical elements provided on the barrier layer> FIG. 16 is a schematic diagram for explaining a micro-optical element 200 (convex surface (positive refractive power) in the sunlight incidence direction in FIG. 16) having a fine light-collecting effect on the surface of the barrier layer of the present invention and its effect. The pitch of this convex surface is preferably about 10 to 300 (μm), but since it needs to be optimized based on the positional relationship between the focal position obtained by this lens effect and the light conversion layer (light absorption layer), which will be described in detail later, it may be up to about 1500 (μm). It is even better if a moth-eye shape, which is an ultra-fine optical element with an ultra-fine pitch of 100 to 200 (nm), is provided on the surface of this micro-optical element 200, and this effect reduces the reflection of sunlight on the incident surface.
[0096] The incident sunlight is focused from a parallel light beam to different focal points according to the wavelength of the light by the action of the micro-optical element having a light-focusing effect. In a general optical element having a positive refractive power, the focal length is shorter as the wavelength of the light is shorter. For example, the focal point of the light beam in the visible light region shown in the (A) region of FIG. 14 is the shortest and is focused at the focal point P1 in the first light absorbing layer 202 in FIG. 16. Similarly, the focal point of the light beam in the near infrared region shown in the (B) region of FIG. 14 is the next shortest and is focused at the focal point P2 in the second light absorbing layer 203 in FIG. 16. Furthermore, the focal point of the light beam in the far infrared region shown in the (C) region of FIG. 14 becomes the focal point P3 in the third light absorbing layer 204, which is the farthest in FIG. 16, and the light beam incident as parallel light is (1) focused toward multiple focal points at different distances from the incident surface according to the wavelength, and (2) the sunlight beam is converted into an oblique light beam by the action of the optical element.
[0097] For this reason, photoelectric conversion layers (light absorbing layers) 202, 203, and 204 containing components with the highest photoelectric conversion efficiency according to wavelength are placed at each focal position, realizing the highest photoelectric conversion efficiency as a whole system. Furthermore, since sunlight crosses each photoelectric conversion layer (light absorbing layer) at an angle, the effective optical path length is extended and the amount of photoelectric conversion increases. On the other hand, to achieve the same amount of photoelectric conversion, the layer thickness can be made thinner, which reduces the electrical resistance and increases the amount of power that can be extracted from the solar cell. Furthermore, since the sunlight is concentrated, a large amount of light energy is incident on the photoelectric conversion layer (light absorbing layer) in a narrowed state, and it has been found that a photoelectric conversion efficiency several times to several tens of times higher than that of the incident normal sunlight flux (parallel light flux) can be realized.
[0098] Furthermore, because the light density of the photoelectric conversion layer (light absorption layer) is divided into "dense areas" and "sparse areas" on the same plane, a gradient in conversion efficiency and temperature occurs on the same plane. This causes a time lag in heat conduction and a difference in the propagation of light in some areas, which resulted in a significant improvement in the photoelectric conversion efficiency itself.
[0099] As shown in Fig. 17, sunlight (shown by dashed lines) incident on the above-mentioned fine-shaped optical element 200, passing through the photoelectric conversion layers (light absorbing layers) 202, 203, 204, the electron transport layer 105 (not shown), the hole transport layer 106 (not shown), and the two electrodes 103, 104 (not shown), and reflected by the reflective surface 205 (the reflective surface 205 is not shown in Fig. 4) provided on the surface of the substrate 101, is totally reflected inside the incident surface of the fine-shaped optical element, and is directed again toward the photoelectric conversion layer (light absorbing layer), so that it cannot escape from the solar cell element, and the photoelectric conversion efficiency can be further improved. The shape of the fine optical element is more preferably an elliptical incident surface shape, so that even if the light (light flux) incident on the solar cell is incident from a slightly oblique direction due to the movement of the sun during the day, it is focused on the focal point without being affected by aberration, and the radius of curvature of the part away from the optical axis is relatively large to reduce astigmatism.
[0100] Although the above description has focused on the solar cell element and solar cell of the present invention, it goes without saying that a solar cell unit can be made by arranging multiple solar cells in parallel and attaching the whole to a flexible sheet. By providing a barrier layer with the above-mentioned barrier properties on the surface, it is possible to obtain a surface hardness comparable to that of glass, so no special consideration is required for installation, and since the barrier layer is thin, it can be installed on a curved surface or in a folded state, which greatly improves the degree of freedom of installation compared to conventional silicon solar cells arranged on a glass substrate.
[0101] The solar cell of the present invention can be manufactured by a method in which the film (layer) formation process is a printing process (Roll to Roll).The configuration and manufacturing process are not particularly limited, and may include, for example, a manufacturing method including a process of arranging an electron transport layer on a substrate, a process of arranging a photoelectric conversion layer (light absorbing layer) on the electron transport layer, a process of arranging a hole transport layer on the photoelectric conversion layer (light absorbing layer), a process of arranging a transparent electrode on the hole transport layer, a process of providing an extraction wiring on the transparent electrode, a process of providing a barrier layer that covers and seals the entire extraction wiring, and a process of providing the extraction electrode on the outside of the barrier layer on the transparent electrode. [Industrial Applicability]
[0102] According to the present invention, a barrier layer having transmittance and hardness equivalent to glass is provided on the outer periphery of an extraction wiring on a transparent electrode, and the barrier layer is highly reliable in suppressing the intrusion of moisture from the atmosphere through the extraction wiring. By providing ultrafine optical elements and fine optical elements on the surface of the barrier layer, a solar cell having high photoelectric conversion efficiency can be provided. [Explanation of symbols]
[0103] M…Metal atom R…organic molecule X: halogen atom or chalcogen atom 1...Base material 2…Outer frame made of insulating layer 3...Photoelectric conversion layer 4…Transparent electrode 5…Exit wiring 5'...End (extraction part) 6...Planarization layer 7...(First) Barrier layer (film) 8…Extraction electrode 9…More wiring 10...(Second) Barrier layer (film) L: Distance from the edge of the lead wire to the edge of the barrier layer 20...Solar cell (unit) 100...Solar cell element 200...Solar cell element 101...Base material 102...Light absorbing layer 102A...first light absorbing layer (photoelectric conversion layer) 102B: Second light absorbing layer (photoelectric conversion layer) 102C...Third light absorbing layer (photoelectric conversion layer) 103...first electrode 104...Second electrode 105...electron transport layer 106...Hole transport layer 107...Exit wiring 110A…Ultra-fine optical elements 110...Barrier layer (film) 200...Micro-optical elements 201...(second) barrier layer (film) 202...First light absorbing layer (photoelectric conversion layer) 203...Second light absorbing layer (photoelectric conversion layer) 204...Third light absorbing layer (photoelectric conversion layer)
Claims
1. A solar cell having at least a photoelectric conversion layer (light absorbing layer) and a transparent electrode on a substrate, the photoelectric conversion layer contains an organic-inorganic perovskite compound, The solar cell further comprises an inorganic barrier layer that entirely covers and seals the transparent electrode, and a micro-optical element having a moth-eye structure on at least the sunlight-incident surface of the inorganic barrier layer on the transparent electrode.
2. A lead wire is provided on the transparent electrode, 2. The solar cell according to claim 1, further comprising: an inorganic barrier layer that entirely covers and seals the lead-out wiring; and an extraction electrode that is disposed on the transparent electrode outside the inorganic barrier layer.
3. 2. The solar cell according to claim 1, further comprising an outer frame made of an insulating layer disposed on top of said transparent electrode so as to surround a side surface of said photoelectric conversion layer and below said transparent electrode.
4. 4. The solar cell according to claim 1, further comprising a planarizing layer disposed between the transparent electrode and the inorganic barrier layer.
5. The organic-inorganic perovskite compound has the general formula R-M-X 3 4. The solar cell according to claim 1, wherein R is an organic molecule, M is a metal atom, and X is a halogen atom or a chalcogen atom.
6. A solar cell having at least a photoelectric conversion layer (light absorbing layer) and a transparent electrode on a substrate, the photoelectric conversion layer contains an organic-inorganic perovskite compound, The photoelectric conversion layer further includes an inorganic barrier layer that covers and seals the entire transparent electrode, and a micro-optical element having a moth-eye structure on a sunlight incident surface of the barrier layer on the transparent electrode, A solar cell characterized by its ability to concentrate sunlight.
7. The photoelectric conversion layer (light absorption layer) has a first photoelectric conversion layer in a portion where light in the visible light region of sunlight is collected, the first photoelectric conversion layer having a plurality of layers, The solar cell according to claim 6, further comprising a second photoelectric conversion layer in a portion where light in the near-infrared region is collected, and further comprising an organic-inorganic perovskite compound having a component with the highest photoelectric conversion efficiency for each wavelength.
8. A substrate is provided with at least a photoelectric conversion layer (light absorbing layer) and a transparent electrode. The photoelectric conversion layer includes an organic-inorganic perovskite compound, and the inorganic barrier layer or film is used as a barrier layer of the solar cell, An inorganic barrier layer or film, comprising fine optical elements having a moth-eye structure on at least a sunlight incident surface of the barrier layer.
9. 9. The inorganic barrier layer or film according to claim 8, wherein the inorganic barrier layer or film contains silicon nitride.
10. 10. The method for forming an inorganic barrier layer or an inorganic barrier film according to claim 8, wherein the inorganic barrier layer or the inorganic barrier film is formed by a process of applying polysilazane as a precursor onto a substrate and curing the polysilazane by irradiating it with vacuum ultraviolet light.
11. The inorganic barrier layer or inorganic barrier film is formed by applying a precursor to a substrate in a roll-to-roll manner, 10. The method for forming an inorganic barrier layer or an inorganic barrier film according to claim 8 or 9, characterized in that the inorganic barrier layer or the inorganic barrier film is formed by a process of forming a shape of fine optical elements on a roll surface on the surface of the polysilazane, and curing the polysilazane by irradiating it with vacuum ultraviolet light having a wavelength of 200 nm or less.
Citation Information
Patent Citations
Substrate for semiconductor device, semiconductor device, dimming-type lighting device, self light-emitting display device, solar cell and reflective liquid crystal display device
JP2013253317A
Solar cell
JP2018163938A
Solar cell, multi-junction solar cell, and manufacturing method of solar cell
JP2022183700A