Punching method
The method forms annular slopes on the surface and back of plate materials to address burrs and chamfer edges, improving hole quality and efficiency in punching processes.
Patent Information
- Application Number
- JP2023081289
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Filing Date
- 2023-05-17
- Publication Date
- 2024-11-28
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
Existing punching methods fail to address burrs and chamfering on the periphery of holes in plate materials, particularly on the non-punched side, which necessitate additional work to remove defects and form smooth edges.
A method involving the formation of a first annular slope on the surface and a second annular slope on the back surface of the plate material before punching, ensuring a tapered fracture surface and chamfered edges by using specific die configurations.
Reduces the occurrence of burrs and facilitates chamfering on the periphery of holes, enhancing production efficiency by eliminating defects and ensuring smooth edges.
Smart Images

Figure 2024165256000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a punching method. [Background technology]
[0002] For example, Patent Document 1 (JP Patent Publication 63-15048) and Patent Document 2 (JP Patent Publication 3413140) disclose a technique for punching a plate-shaped product (plate member) (e.g., a small round plate) having a predetermined shape from a plate-shaped raw material (plate material) by pressing, in which a V-shaped groove (V-groove) is formed in the plate material beforehand, and the inside of the groove is punched in the next step. These techniques are said to reduce the effective punching distance (plate thickness to be punched), and therefore to reduce, for example, the punching load and the proportion of the fracture surface on the end face of the plate member.
[0003] When it is desired to obtain a particularly remarkable effect, a V-groove is provided on the back surface of the plate material in addition to the front surface, and the dimensions of the portion related to the V-groove are specified.
[0004] For example, the invention described in Patent Document 3 (Patent Publication No. 6448482) specifies the length between the deepest parts of the grooves provided on the front and back surfaces of a workpiece (length of fracture surface = plate thickness at the thinnest part of the workpiece where the grooves are formed) and the width outside the deepest parts of the grooves in the workpiece (width of the scrap part, etc.). According to this, it is said that it is possible to minimize the fracture surfaces on the outer peripheral surface (end surface) of the punched member (round plate), which is the desired molded product, and to make the outer peripheral surface smooth.
[0005] In addition, the invention described in Patent Document 4 (JP 2022-143918 A) aims to maximize the shear surface (minimize the fracture surface) on the outer peripheral surface of the punched member (round plate) by specifying the original plate thickness, the plate thickness at the thinnest part, and the groove bottom length of the plate material, thereby smoothing the outer peripheral surface.
[0006] However, all of these are aimed at smoothing the outer surface (end face) of the punched side component (the part that is punched out of the plate material from the groove in the plate material), and no consideration is given to the inner surface of the hole in the non-punched side component (the part that is punched out from the plate material from the groove in the plate material, which remains after the plate material is punched out).
[0007] On the other hand, there are cases where it is necessary to obtain a porous product (such as a punched metal) by drilling one or more holes in a plate material by press processing (punching). In this case, the punched side member and the non-punched side member are reversed from the above-mentioned case. That is, the part remaining after the plate material is punched out, on the outer periphery side of the groove of the plate material, becomes the product, so if there is a defect such as a burr on the periphery of the hole drilled in that part (the back side in the punching process), additional processing is required to, for example, crush or cut away the defect. Therefore, from the viewpoint of increasing the production efficiency of such products, it is preferable to eliminate defects such as burrs on the periphery of the hole drilled in the non-punched side member.
[0008] Furthermore, in addition to removing burrs on the back side during punching, it may be necessary to form chamfers (sloping edges) on the edges of the front and back sides of a hole drilled in a non-punched side component during punching.
[0009] In other words, in this technical field, there is a demand for a technology that can reduce the occurrence and / or remaining of burrs and the like on the periphery on the back side of a hole when drilling a hole in a plate material by punching, and that can form chamfers on the periphery on the front and back sides of the hole. [Prior art documents] [Patent documents]
[0010] [Patent Document 1] Special Publication No. 63-15048 [Patent Document 2] Patent No. 3413140 [Patent Document 3] Patent No. 6448482 [Patent Document 4] JP 2022-143918 A Summary of the Invention [Problem to be solved by the invention]
[0011] As described above, there is a need in the art for a technology that can reduce the occurrence and / or persistence of burrs and the like on the periphery of the back side of a hole when drilling a hole in a plate material by punching, and that can form chamfers on the periphery of the front and back sides of the hole. [Means for solving the problem]
[0012] In view of the above problems, the inventor conducted intensive research and discovered that the above problems can be solved by forming a recess on the front surface of the plate material including a ring-shaped first inclined portion surrounding the area to be drilled and forming a recess on the back surface of the plate material including a ring-shaped second inclined portion larger than the first inclined portion before pressing a predetermined portion of the plate material with a punch to drill a hole, and by pressing the area surrounded by the first inclined portion with a punch.
[0013] Specifically, the punching process according to the present invention (hereinafter, sometimes referred to as the "method of the present invention") is a punching method in which a predetermined portion of a plate material is pressed with a punch to make a hole.
[0014] The method of the present invention comprises the first and second steps listed below. The first step is a step of pressing a first die having a first inclined surface protruding from its tip surface against the surface of the plate material to form a first recess on the surface of the plate material, and pressing a second die having a second inclined surface protruding from its tip surface against the back surface of the plate material to form a second recess on the back surface of the plate material. The first inclined surface is an annular inclined surface that inclines inward from the base end side to the tip side. The first recess is a recess that includes a first inclined portion that is a portion having an annular shape corresponding to the first inclined surface. The second inclined surface is an annular inclined surface that inclines inward from the base end side to the tip side. The second recess is an annular recess that includes a second inclined portion that is a portion having an annular shape corresponding to the second inclined surface. The second step is a step of pressing at least a part of the region surrounded by the first inclined portion on the surface of the plate material with a punch to punch out a part of the plate material.
[0015] Furthermore, the method of the present invention satisfies the first and second requirements listed below. The first requirement is that in the first projection view, the entire first region, which is the region surrounded by the first end, which is the end on the tip side of the first inclined surface in the first step, is included in the second region, which is the region surrounded by the second end, which is the end on the tip side of the second inclined surface. The first projection view is a projection view in the pressing direction, which is the direction in which the plate material is pressed by the punch in the second step. The second requirement is that in the first projection view, the entire punch area, which is at least the area corresponding to the portion of the punch that progresses further in the pressing direction than the surface of the plate material in the second punch step, overlaps with or is included in the first area. Effect of the Invention
[0016] In the method of the present invention, as described above, before pressing a predetermined portion of a plate material with a punch to make a hole, a recess including a first annular inclined portion surrounding the region to be drilled is formed on the front surface of the plate material, and a recess including a second annular inclined portion wider than the first inclined portion is formed on the back surface of the plate material, and the region surrounded by the first inclined portion is pressed by the punch. Since the fracture surface in such a punching process spreads in a tapered shape toward the punching direction, the fracture surface can be continuously formed from the deepest part (corresponding to the first end) of the first recess to the deepest part (corresponding to the second end) of the second recess. As a result, the generation of burrs due to tearing and the like can be reduced. That is, the generation of burrs and the like on the periphery of the back side of the hole can be reduced when a hole is drilled in the plate material by punching. In addition, the first annular inclined portion included in the first recess and the second annular inclined portion included in the second recess can form chamfers on the periphery of the front surface side and the back side side of the hole.
[0017] In other words, according to the method of the present invention, when a hole is drilled in a plate material by punching, the occurrence and / or remaining of burrs and the like on the peripheral edge on the back side of the hole can be reduced, and chamfers can be formed on the peripheral edges on the front and back sides of the hole.
[0018] Other objects, features and attendant advantages of the present invention will become readily apparent from the following description of the embodiments of the present invention which are given with reference to the accompanying drawings. [Brief description of the drawings]
[0019] [Figure 1] 1 is a schematic perspective view showing an example of the configuration of a product made of a plate material having a plurality of holes drilled therein by a punching method. FIG. [Diagram 2] 1 is a flowchart illustrating the flow of each step included in a punching method (first method) according to a first embodiment of the present invention. [Diagram 3] 5A to 5C are schematic cross-sectional views illustrating the shapes and positional relationships of the members when a first step and a second step included in a first method are completed. [Figure 4] 5A to 5C are schematic diagrams showing some examples of shapes in a first projection view of a first region and a second region in a first method. [Diagram 5] 11A to 11C are schematic cross-sectional views illustrating the shape of a protrusion formed in association with the execution of the first step included in a punching method (third method) according to a third embodiment of the present invention, and problems that arise in association with the formation of the protrusion. [Figure 6] FIG. 13 is a schematic diagram showing an example of the configuration of a first die and a second die used in a punching method (fourth method) according to a third embodiment of the present invention. [Figure 7] FIG. 13 is a schematic cross-sectional view (a) showing an example of the configuration of a first die and a second die used in the fourth method, and schematic cross-sectional views (b) and (c) showing how a scrap is punched out in the second step included in the fourth method. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0020] First Embodiment Hereinafter, a method for forming a sidewall portion according to a first embodiment of the present invention (hereinafter, may be referred to as a "first method") will be described.
[0021] <composition> The first method is a punching method in which a predetermined portion of a plate material is pressed with a punch to make holes. FIG. 1 is a schematic perspective view showing an example of the configuration of a product made of a plate material in which a plurality of holes are made by a punching method. The product 200 shown in FIG. 1 includes a top plate portion 210 and a side wall portion (flange portion) 220 standing at a substantially right angle from an end portion of the top plate portion 210, and a plurality of holes 230 are made in the top plate portion 210. However, in a product in which one or more holes are made by the first method, the side wall portion is not an essential component. The material constituting the plate material is not particularly limited as long as it can be made to make holes by pressing with a punch. Specific examples of such materials include metals such as stainless steel, copper, and aluminum, and alloys containing these metals.
[0022] The first method includes the first and second steps listed below. The first method may further include other steps before the first step, after the second step, and / or between the first and second steps, as long as the effect achieved by the first method is not substantially impaired. FIG. 2 is a flow chart illustrating the flow of each step included in the first method. FIG. 3 is a schematic cross-sectional view illustrating the shape and positional relationship of each member at the completion of the first and second steps included in the first method. In FIG. 3(b), only the left side of the axis AX of the punch that presses a predetermined portion of the plate material to make a hole is depicted, but the same is true for the right side of the axis AX.
[0023] The first process executed in step S10 of the flowchart illustrated in FIG. 2 is a process in which a first die D1 having a first inclined surface S1 protruding from a tip surface T1 is pressed against the surface of the sheet material PM to form a first recess C1 in the surface of the sheet material PM, and a second die D2 having a second inclined surface S2 protruding from a tip surface T2 is pressed against the back surface of the sheet material PM to form a second recess C2 in the back surface of the sheet material PM, as illustrated in FIG. 3(a).
[0024] The first inclined surface S1 is an annular inclined surface that inclines inward (i.e., toward the axis AX) from the base end side (i.e., toward the tip surface T1 of the first die D1) toward the tip side. In the example shown in Fig. 3(a), the first inclined surface S1 is linearly inclined at a constant angle over the entire area, but the inclination angle of the first inclined surface S1 does not necessarily have to be constant over the entire area, and the inclination angle may change continuously or discontinuously along the way.
[0025] The first recess C1 is formed on the surface of the sheet material PM by pressing the first inclined surface S1 protruding from the tip surface T1 of the first die D1 against the surface of the sheet material PM as described above. Therefore, the first recess C1 is a recess including a first inclined portion that is a portion having an annular shape corresponding to the first inclined surface S1. The first recess C1 illustrated in FIG. 1 is a recess including the first inclined portion that is a portion having an annular shape corresponding to the first inclined surface S1 and having an annular shape as a whole. However, as will be described later in the description of other embodiments, the first recess C1 does not necessarily have to have an annular shape as a whole as long as it includes the first inclined portion that is a portion having an annular shape corresponding to the first inclined surface S1.
[0026] The second inclined surface S2 is an annular inclined surface that inclines inward (i.e., toward the axis AX) from the base end side (i.e., toward the tip surface T2 of the second die D2) toward the tip side. In the example shown in Fig. 3(a), the second inclined surface S2 is linearly inclined at a constant angle over the entire area, but the inclination angle of the second inclined surface S2 does not necessarily have to be constant over the entire area, and the inclination angle may change continuously or discontinuously along the way.
[0027] The second recess C2 is formed on the back surface of the sheet material PM by pressing the second inclined surface S2 protruding from the tip surface T2 of the second die D2 against the back surface of the sheet material PM as described above. Therefore, the second recess C2 is an annular recess including a second inclined portion that is a portion having an annular shape corresponding to the second inclined surface S2.
[0028] The second step is a step of pressing at least a part of the region surrounded by the annular first inclined portion included in the first recess C1 on the surface of the plate material PM with a punch P1 to punch out a part of the plate material PM. In the example shown in FIG. 3(b), a part of the plate material PM adjacent to the outside of the region to be perforated is clamped between a first holding member H1 (e.g., a pad) arranged on the surface side of the plate material PM and a second holding member H2 (e.g., a die) arranged on the back side of the plate material PM. Then, at least a part of the region surrounded by the annular first inclined portion included in the first recess C1 on the surface of the plate material PM is pressed from the surface side to the back side of the plate material PM with the punch P1 (see the black arrow shown in the figure) to punch out a part of the plate material PM as scrap SC.
[0029] The drive mechanism for pressing the first die D1 against the surface of the plate material PM in the first step and punching out a part of the plate material PM with the punch P1 in the second step can be appropriately selected from various drive mechanisms well known in the art depending on, for example, the properties (e.g., mechanical strength and hardness) of the material constituting the plate material PM, the thickness of the plate material PM, and the shape and size of the hole to be drilled in the plate material PM. Typically, a press machine such as a hydraulic press machine is used as the drive mechanism.
[0030] Furthermore, the first method satisfies the first and second requirements listed below.
[0031] The first requirement is that the area surrounded by the annular second inclined portion included in the annular second recess C2 on the back surface of the plate material PM is larger than the area surrounded by the annular first inclined portion included in the first recess C1 on the front surface of the plate material PM. More specifically, the first requirement is that in the first projection view, the entire first area, which is the area surrounded by the first end E1 (shown by a hollow circle in FIG. 3(a)) which is the end on the tip side of the first inclined surface S1 in the first step, is included in the second area, which is the area surrounded by the second end E2 (shown by a filled circle in FIG. 3(a)) which is the end on the tip side of the second inclined surface S2. The first projection view is a projection view in the pressing direction, which is the direction in which the plate material is pressed by the punch in the second step. For example, the first projection view is a vertical projection view onto a plane perpendicular to the axis AX shown in FIG. 3.
[0032] Fig. 4 is a schematic diagram showing some examples of shapes of the first and second regions in the first projection in the first method. In Fig. 4, the dashed line represents the position of the first end E1 in the first projection, and the solid line represents the position of the second end E2 in the first projection. That is, the figure surrounded by the dashed line E1 represents the shape of the first region in the first projection, and the figure surrounded by the solid line E2 represents the shape of the second region in the first projection.
[0033] (a), (b), (c), (d), (e) and (f) in Fig. 4 respectively show examples in which the shapes of the first region and the second region in the first projection are a circle, an ellipse, a square, a rectangle, a regular hexagon and a U-shape. The shapes of the first region and the second region in the first projection are not limited to these examples as long as the entire first region is included in the second region. Note that in Fig. 4, the difference in size between the first region and the second region is emphasized in order to clearly show the shapes of the first region and the second region in the first projection, and does not accurately show the actual shapes of the first region and the second region in the first projection.
[0034] The second requirement is that the part of the punch P1 that penetrates deeper than the surface of the plate material PM in the process of pressing the punch P1 to punch out a part of the plate material PM in the second step can pass through the hole drilled in the plate material PM. More specifically, the second requirement is that in the first projection view, the entire punch region, which is at least the region corresponding to the part of the punch that advances further in the pressing direction than the surface of the plate material in the second step, overlaps with or is included in the first region. In other words, the second requirement is that the shape in the first projection view of the entire part of the punch P1 that penetrates deeper than the surface of the plate material PM in the process of pressing the punch P1 to punch out a part of the plate material PM in the second step overlaps with or is included in the first region, which is the region surrounded by the dashed line E1 in FIG. 4.
[0035] <effect> In the first method, as described above, before pressing a predetermined portion of the plate material PM with the punch P1 to punch a hole, a first annular recess C1 surrounding the region to be punched is formed on the surface of the plate material PM, and a second annular recess C2 wider than the first recess C1 is formed on the back surface of the plate material PM. Then, the region surrounded by the first annular inclined portion included in the first recess C1 is pressed by the punch P1. The fracture surface in such a punching process spreads in a tapered shape toward the punching direction (downward in the direction of the axis AX), as illustrated by the arrow drawn by a dashed line from the first end E1 (white circle) to the second end E2 (black circle) in (a) of FIG. 3. Therefore, the fracture surface can be continuously formed from the deepest part of the first recess C1 (corresponding to the first end E1) to the deepest part of the second recess C2 (corresponding to the second end E2). As a result, the generation of burrs due to tearing or the like can be reduced. That is, when a hole is drilled in the plate material PM by punching, the occurrence of burrs and the like on the periphery on the back side of the hole can be reduced. Also, the annular first inclined portion included in the first recess C1 and the annular second inclined portion included in the second recess C2 can form a chamfer on the periphery on the front side of the hole.
[0036] In other words, according to the first method, when a hole is drilled in a plate material by punching, the occurrence and / or remaining of burrs and the like on the periphery on the back side of the hole can be reduced, and a chamfer can be formed on the periphery on the front side of the hole.
[0037] Second Embodiment Hereinafter, a method for forming a sidewall portion according to a second embodiment of the present invention (hereinafter, may be referred to as a "second method") will be described.
[0038] As described above, in the first method, before pressing a predetermined portion of the plate material PM with the punch P1 to perforate the plate material PM, a first annular recess C1 surrounding the region to be perforated is formed on the surface of the plate material PM, and a second annular recess C2 wider than the first recess C1 is formed on the back surface of the plate material PM. This allows a fracture surface to be continuously formed from the deepest part of the first recess C1 (corresponding to the first end E1) to the deepest part of the second recess C2 (corresponding to the second end E2) in a punching process in which the punch P1 presses the region surrounded by the annular first inclined portion included in the first recess C1 (see the arrow drawn by the dashed line in (a) of FIG. 3). As a result, it is possible to reduce the occurrence of burrs due to tearing or the like.
[0039] In the punching process as described above, the angle of the fracture surface tapering toward the punching direction (downward in the direction of the axis AX in the example shown in Figure 3) with respect to the punching direction varies depending on, for example, the properties (e.g., mechanical strength and hardness) of the material constituting the plate material PM, the thickness of the plate material PM, the shape and size of the hole to be drilled in the plate material PM, and the punch speed in the punching process.
[0040] However, the inventor has discovered that in the punching method of the present invention (method of the present invention), when the angle between the first axis and a straight line passing through the first end and the second end and the first axis in a cross section taken along a plane including the first axis, which is a common axis of the first region and the second region, is within a predetermined range, a fracture surface connecting the deepest part of the first recess C1 (corresponding to the first end E1) to the deepest part of the second recess C2 (corresponding to the second end E2) can be more reliably formed.
[0041] <composition> Therefore, the second method is the above-mentioned first method, and further satisfies the third and fourth requirements listed below.
[0042] The third requirement is that in a first cross section, which is a cross section taken along a plane including the first axis, which is the common central axis of the first region and the second region, the angle between the first line, which is a line passing through the first end portion and the second end portion, and the first axis is greater than or equal to 7 degrees and less than or equal to 12 degrees.
[0043] For example, in the example shown in FIG. 3 referred to in the description of the first method, the first straight line, which is a straight line passing through the first end E1 and the second end E2, is drawn by a dashed line. In addition, the first axis, which is a common axis of the first region and the second region, coincides with the axis AX of the punch, which is drawn by a dashed line. In the example shown in FIG. 3, the angle θ between the first straight line (dashed line) and the first axis (dashed line) is drawn large in order to clearly illustrate the shape and positional relationship of each member at the time of completing the first step and the second step included in the first method. However, by setting this angle θ to be 7 degrees or more and 12 degrees or less, in the second step of punching out the region surrounded by the annular first inclined portion included in the first recess C1 on the surface of the plate material PM with the punch P1, a fracture surface connecting the deepest part of the first recess C1 (corresponding to the first end E1) to the deepest part of the second recess C2 (corresponding to the second end E2) can be more reliably formed.
[0044] Incidentally, for example, from the viewpoint of reducing deformation and / or distortion at the periphery of the hole punched in the second step, it is preferable that the shape of the first region corresponding to the shape of the scrap SC punched by the punch P1 is rotationally symmetric about the central axis (first axis). Therefore, it is preferable that the shape of the second region is also rotationally symmetric about the central axis (first axis). In other words, it is preferable that the shapes of the first region and the second region are coaxially rotationally symmetric.
[0045] Furthermore, in order for the angle θ between the above-mentioned first straight line (dashed line) and the first axis (dotted line) to be within the above-mentioned specified range throughout the entire circumference of the first region and the second region, it is preferable that the shape of the first region and the shape of the second region are similar to each other.
[0046] Therefore, the fourth requirement is that, in the first projection view, the first region and the second region are rotationally symmetric about the first axis and have shapes similar to each other.
[0047] For example, in the example shown in FIG. 4 referred to in the explanation of the first method, the first region (surrounded by dashed line E1) and the second region (surrounded by solid line E2) illustrated in (a) to (e) are rotationally symmetric about the first axis (see X in the figure), which is a common axis, and have shapes similar to each other. That is, these first and second regions satisfy the fourth requirement. On the other hand, the first and second regions illustrated in (f) of FIG. 4 are not rotationally symmetric and do not have shapes similar to each other. That is, the first and second regions illustrated in (f) do not satisfy the fourth requirement.
[0048] <effect> In the second method, as described above, the angle between the first line, which is a line passing through the first end and the second end in the first cross section, and the first axis, which is a common axis of the first region and the second region, is 7 degrees or more and 12 degrees or less (satisfying the third requirement). This makes it possible to more reliably form a fracture surface that connects the deepest part of the first recess to the deepest part of the second recess in the second step of punching out the region surrounded by the first inclined portion included in the first recess on the surface of the plate material with a punch.
[0049] Furthermore, in the first projection view, the first and second regions are rotationally symmetric about the first axis and have similar shapes (satisfying the fourth requirement). This reduces deformation and / or distortion at the periphery of the hole drilled in the second step, and allows the angle between the first straight line (dashed line) and the first axis (dotted line) to fall within the above-mentioned predetermined range over the entire circumference of the first and second regions.
[0050] Third Embodiment Hereinafter, a method for forming a sidewall portion according to a third embodiment of the present invention (hereinafter, may be referred to as a "third method") will be described.
[0051] The first step included in the side wall forming method (first method) according to the first embodiment of the present invention, as explained with reference to (a) of Figure 3, is a step of pressing a first die D1 having a first inclined surface S1 protruding from a tip surface T1 against a surface of the plate material PM to form a first recess C1 in the surface of the plate material PM, and pressing a second die D2 having a second inclined surface S2 protruding from a tip surface T2 against the back surface of the plate material PM to form a second recess C2 in the back surface of the plate material PM.
[0052] The configuration of the first inclined surface S1 on the front end surface T1 of the first die D1 and the inner side (center side) of the second inclined surface S2 on the front end surface T2 of the second die D2 is not particularly limited as long as the first recess C1 and the second recess C2 can be formed on the front and back surfaces of the sheet material PM by performing the above-mentioned first step. However, from the viewpoint of reliably forming the first recess C1 and the second recess C2 on the front and back surfaces of the sheet material PM, it is preferable that a protrusion like an annular mountain having an annular ridgeline formed by the first end E1, which is the end on the front end side of the first inclined surface S1, and the second end E2, which is the end on the front end side of the second inclined surface S2, is formed on the front end surface T1 of the first die D1 and the front end surface T2 of the second die D2, respectively.
[0053] <composition> Therefore, the third method is the above-mentioned first or second method, which further satisfies the fifth and sixth requirements listed below.
[0054] The fifth requirement is that, on the tip surface T1 of the first die D1, an annular inclined surface is formed adjacent to the inside (center side) of the annular first inclined surface S1, and inclined outward (i.e., the opposite side to the axis AX) from the base end side (i.e., the tip surface T1 side of the first die D1) to the first end E1, which is the end on the tip side. In other words, the fifth requirement is that, as illustrated in (a) of Fig. 3, in the first die D1, a third inclined surface S3, which is an annular inclined surface that inclins outward from the base end side to the tip side and is adjacent to the first inclined surface S1 at the first end E1, is protruded from the tip surface T1.
[0055] On the other hand, the sixth requirement is, like the fifth requirement, that the tip surface T2 of the second die D2 has an annular inclined surface that is adjacent to the inside (center side) of the annular second inclined surface S2 and inclined outward (i.e., the opposite side to the axis AX) from the base end side (i.e., the tip surface T2 side of the second die D2) to the second end E2, which is the end on the tip side. In other words, the sixth requirement is that, as illustrated in (a) of Fig. 3, the second die D2 has a fourth inclined surface S4, which is an annular inclined surface that inclins outward from the base end side to the tip side and is adjacent to the second inclined surface S2 at the second end E2, protruding from the tip surface T2.
[0056] With the above-mentioned configuration, a ring-shaped mountain-like protrusion having a ring-shaped ridgeline formed by the first end E1, which is the end on the tip side of the first inclined surface S1, and the second end E2, which is the end on the tip side of the second inclined surface S2, is formed on the tip surface of the first die and the tip surface of the second die, respectively. However, in the protrusion having such a ring-shaped mountain-like shape, the ring-shaped ridgeline formed by the first end E1 and the second end E2 does not necessarily have to be a sharp ridgeline. In other words, as long as it is possible to form the first recess C1 and the second recess C2 on the front and back surfaces of the plate material PM, respectively, these ridgelines may be gentle ridgelines having a certain width, for example, as illustrated in FIG. 5(a) which will be referred to in the description of the method for forming a sidewall portion according to the fourth embodiment of the present invention described later.
[0057] 3(a), the inclination angles of the third slant surface S3 and the fourth slant surface S4 both change discontinuously along the way. However, the inclination angles of the third slant surface S3 and / or the fourth slant surface S4 may change continuously along the way, or the inclination angles of the third slant surface S3 and / or the fourth slant surface S4 may be constant over the entire range.
[0058] <effect> In the third method, as described above, a third inclined surface which is an annular inclined surface inclined outward from the base end side to the tip end side and adjacent to the first inclined surface at a first end, and a fourth inclined surface which is an annular inclined surface inclined outward from the base end side to the tip end side and adjacent to the second inclined surface at a second end are provided on the tip end surfaces of the first die and the second die, respectively. That is, a protrusion like an annular mountain having an annular ridgeline formed by the first end which is the tip end of the first inclined surface and the second end which is the tip end of the second inclined surface is formed on the tip end surface of the first die and the tip end surface of the second die, respectively.
[0059] In the first step included in the third method, since the tip surface of the first die and the tip surface of the second die have such a configuration, the first recess and the second recess can be reliably formed on the front and back surfaces of the plate material. As a result, according to the third method, when a hole is drilled in the plate material by punching, the generation and / or remaining of burrs and the like on the periphery on the back surface side of the hole can be more reliably reduced, and chamfers can be more reliably formed on the periphery on the front and back surfaces of the hole.
[0060] Fourth Embodiment Hereinafter, a method for forming a sidewall portion according to a fourth embodiment of the present invention (hereinafter, may be referred to as a "fourth method") will be described.
[0061] As described above, in the method for forming a sidewall portion according to the third embodiment of the present invention (third method), annular mountain-like protrusions having an annular ridgeline formed by the first end, which is the end on the tip side of the first inclined surface, and the second end, which is the end on the tip side of the second inclined surface, are formed on the tip surface of the first die and the tip surface of the second die, respectively. As a result, according to the third method, when a hole is drilled in a plate material by punching, it is possible to more reliably reduce the occurrence and / or remaining of burrs on the periphery on the back side of the hole and to more reliably form chamfers on the periphery on the front side and back side of the hole.
[0062] As illustrated by the portion hatched with fine diagonal lines in FIG. 3(a), when the annular protrusions formed on the tip surfaces of the first die and the second die are pressed against the sheet material in the first step to form the first and second recesses on the front and back surfaces of the sheet material, the material of the sheet material that was present in the portions that will become the first and second recesses moves to the inside of the annular protrusions due to plastic flow, forming raised portions (hereinafter, these may be simply referred to as "raised portions").
[0063] 5 is a schematic cross-sectional view illustrating the shape of the raised portion formed by performing the first step included in the third method and the problems that occur with the formation of the raised portion. In FIG. 5(a), the parts of the plate material other than the raised portion are omitted in order to easily illustrate the shape of the raised portion. As illustrated in FIG. 5, the top surfaces of the raised portions BP1 and BP2 may be convex curved surfaces depending on, for example, the properties (e.g., ease of plastic flow, etc.) of the material constituting the plate material PM, the thickness of the plate material PM, the shape and size of the holes to be drilled in the plate material PM, the height of the annular protrusions formed on the front end surface T1 of the first die D1 and the front end surface T2 of the second die D2, and the amount of the annular protrusions pressed into the plate material PM.
[0064] For example, when the punching load by the punch P1 in the second step is large due to the properties of the material constituting the plate material PM (e.g., mechanical strength, hardness, ease of plastic flow, etc.) and the shape and size of the hole to be punched in the plate material PM, it is necessary to make the depth of the first recess and the second recess larger. In such a case, the top surfaces of the protrusions BP1 and BP2 are particularly likely to be convexly curved, as described above.
[0065] On the other hand, as described above, in the second step, at least a part of the region surrounded by the annular first inclined portion included in the first recess on the surface of the sheet material PM is pressed by the punch P1, and a part of the sheet material PM is punched out as scrap SC. At this time, if the top surface of the raised portion BP1 formed on the surface of the sheet material PM is a convex curved surface as described above, the contact between the top surface (tip surface) of the punch P1 and the top surface of the raised portion BP1 becomes point contact rather than surface contact, as illustrated in (b) of FIG. 5. As a result, so-called "sagging" occurs at the peripheral portion of the hole punched in the sheet material PM when the scrap SC is punched out, and as indicated by the hollow arrow, the chamfer that should remain on the peripheral portion on the back side of the hole may be crushed due to the second inclined portion formed by the second inclined surface S2 of the second die D2.
[0066] <composition>
[0067] Therefore, the fourth method is the above-mentioned first or second method, which further satisfies the seventh and eighth requirements listed below.
[0068] The seventh requirement is that the first die has a frustum-shaped convex portion protruding from its tip surface, the frustum-shaped convex portion having the first inclined surface as its side surface and a plane perpendicular to the pressing direction defined by the first end portion as its upper base. As described above, the shapes of the first and second regions in the first projection view are not particularly limited as long as the entire first region is included in the second region. Therefore, the shapes and sizes of the upper and lower bases of the frustum-shaped convex portion protruding from the tip surface of the first die are also not particularly limited as long as they satisfy the requirements of the first or second method.
[0069] The eighth requirement is that the second die has a third recess, which is a recess that opens on the tip surface, provided inside the second end. The shape and size of the third recess are not particularly limited as long as it can accommodate the sheet material that undergoes plastic flow when the frustum-shaped convex portion formed on the tip surface of the first die and the annular protrusion formed on the tip surface of the second die are pressed against the sheet material in the first step to form the first recess and the second recess on the front and back surfaces of the sheet material. From the viewpoint of smoothly accommodating the sheet material that undergoes plastic flow as described above, it is preferable that the volume of the third recess is equal to or larger than the volume of the material, and that the opening of the third recess covers as wide an area as possible inside the annular protrusion formed on the tip surface of the second die.
[0070] FIG. 6 is a schematic diagram showing an example of the configuration of the first die and the second die used in the fourth method. FIG. 6(a) is a schematic side view illustrating the arrangement of the first die D1 and the second die D2 in the first step, FIG. 6(b) is a schematic perspective view illustrating the configuration of the first protrusion PP1 formed on the tip surface T1 of the first die D1, and FIG. 6(c) is a schematic perspective view illustrating the configuration of the second inclined surface S2 and the third recess C3 formed on the tip surface T2 of the second die D2. FIG. 7 is a schematic cross-sectional view (a) showing an example of the configuration of the first die and the second die used in the fourth method, and schematic cross-sectional views (b) and (c) showing how the scrap is punched in the second step included in the fourth method.
[0071] In the first die D1 illustrated in Fig. 6(b), a first convex portion PP1 having a frustum shape with the first inclined surface S1 as a side surface and a plane perpendicular to the pressing direction defined by the first end E1 as an upper base UB is protruded from the tip surface T1. That is, the first die D1 illustrated in Fig. 6(b) satisfies the above-mentioned seventh requirement. Note that the first convex portion PP1 illustrated in Fig. 6(b) has a truncated cone shape with circular upper base UB and lower base, but the shape and size of the upper base UB and lower base of the truncated cone-shaped first convex portion PP1 are not particularly limited as long as they satisfy the requirements of the first method or the second method as described above.
[0072] On the other hand, in the second die D2 illustrated in Fig. 6(c), the third recess C3, which is a recess that opens to the tip end surface T2, is provided inside the second end E2. That is, the second die D2 illustrated in Fig. 6(c) satisfies the above-mentioned eighth requirement. Note that the third recess C3 illustrated in Fig. 6(c) has a cylindrical internal space with a circular cross section, but the shape and size of the third recess are not particularly limited as long as they can accommodate the material of the sheet material PM that undergoes plastic flow as the first recess C1 and the second recess C2 are formed on the front and back surfaces of the sheet material PM in the first step as described above.
[0073] FIG. 7(a) is an enlarged cross-sectional view of the part surrounded by the thick dashed line in FIG. 6(a) along the axis AX. As is clear from FIG. 7(a), the first die D1 and the second die D2 used in the fourth method satisfy the above-mentioned seventh and eighth requirements, respectively. As a result, as illustrated in FIG. 7(b), a first recess C1 is formed on the surface of the sheet material PM against which the first die D1 is pressed in the first step, which is a frustum-shaped recess having a bottom surface perpendicular to the pressing direction in correspondence with the shape of the first protrusion PP1 formed on the tip end face T1 of the first die D1. On the other hand, a second recess C2 is formed on the back surface of the sheet material PM against which the second die D2 is pressed in the first step, which is an annular recess corresponding to the second inclined surface S2 formed on the tip end face T2 of the second die D2. In addition, a second protrusion PP2 is formed on the back surface of the sheet material PM by the material of the sheet material PM that plastically flows into the third recess C3 of the second die D2 as a result of the formation of the first recess C1 and the second recess C2 on the front and back surfaces of the sheet material PM in the first step.
[0074] As described above, the first recess C1 formed in the first step included in the fourth method has a bottom surface perpendicular to the pressing direction, so that in the second step, the top surface (tip surface) of the punch P1 and the bottom surface of the first recess C1 can be in surface contact rather than point contact, as shown by the thick solid line in Fig. 7(b). Therefore, as illustrated in Fig. 5(b), when the scrap SC is punched in the second step, the risk of sagging occurring at the periphery of the hole drilled in the plate material PM and the chamfer that should remain at the periphery on the back side of the hole being crushed due to the second inclined portion formed by the second inclined surface S2 of the second die D2 can be reduced. As a result, as illustrated in Fig. 7(c), it is possible to drill a hole having a desired shape in the plate material PM with reduced generation and / or remaining burrs at the periphery on the back side of the plate material PM and with chamfers formed at the periphery on the front side and back side.
[0075] <effect> In the fourth method, as described above, a frustum-shaped convex portion having the first inclined surface as a side surface and a plane perpendicular to the pressing direction defined by the first end portion is protruded from the tip surface of the first die, and a third recess portion, which is a recess portion opening on the tip surface, is provided inside the second end portion of the tip surface of the second die. Therefore, a frustum-shaped recess having a bottom surface perpendicular to the pressing direction can be formed on the surface of the sheet material as the first recess portion while the material constituting the sheet material that plastically flows with the formation of the first recess portion and the second recess portion in the first step is accommodated in the third recess portion. As a result, according to the fourth method, it is possible to reduce the risk that the peripheral portion of the hole drilled in the sheet material when the scrap is punched out in the second step will sag and the chamfer that should remain on the peripheral portion of the back side of the hole will be crushed. In other words, according to the fourth method, the generation and / or remaining of burrs and the like on the peripheral portion of the back side of the sheet material is reduced, and a hole having a desired shape with chamfers formed on the peripheral portions of the front side and back side can be reliably drilled in the sheet material.
[0076] Fifth Embodiment Hereinafter, a method for forming a sidewall portion according to a fifth embodiment of the present invention (hereinafter, may be referred to as a "fifth method") will be described.
[0077] As already mentioned in the explanation of the method for forming a side wall portion according to the third embodiment of the present invention (third method), from the viewpoint of reliably forming the first recess and the second recess on the front and back surfaces of the plate material, it is preferable that a protrusion like an annular mountain having a ring-shaped ridge formed by a first end which is the end on the tip side of the first inclined surface and a second end which is the end on the tip side of the second inclined surface is formed on the tip surface of the first die and the tip surface of the second die, respectively.
[0078] However, in the above-mentioned fourth method, a frustum-shaped convex portion having the first inclined surface as a side surface and a plane perpendicular to the pressing direction defined by the first end as an upper base is provided on the tip surface of the first die. Therefore, in the above-mentioned fourth method, it is not possible to form a protrusion like an annular mountain having an annular ridgeline as described above on the tip surface of the first die.
[0079] On the other hand, a third recess, which is a recess that opens on the tip surface, is provided on the tip surface of the second die, inside the second end. As described above, this third recess is provided for the purpose of accommodating the material of the sheet material that undergoes plastic flow as the frustum-shaped convex portion formed on the tip surface of the first die and the annular protrusion formed on the tip surface of the second die are pressed against the sheet material in the first step to form the first recess and the second recess on the front and back surfaces of the sheet material. Therefore, the shape and size of the third recess are not particularly limited as long as the purpose can be achieved.
[0080] <composition> Therefore, the fifth method is the above-mentioned fourth method, which further satisfies the ninth requirement described below.
[0081] The ninth requirement is that in the second die, a fourth inclined surface, which is an annular inclined surface that inclines outward from the base end side toward the tip end side and is adjacent to the second inclined surface at the second end, is protruded between the second end and the third recess on the tip surface.
[0082] The fourth inclined surface is already depicted in Fig. 6(c) and Fig. 7(a) referred to in the description of the third method. That is, the second die D2 illustrated in Fig. 6 and Fig. 7 is also the second die used in the fifth method that satisfies the ninth requirement. Specifically, as illustrated in Fig. 6(c) and Fig. 7(a), the fourth inclined surface S4 is an annular inclined surface that inclines outward (i.e., toward the opposite side to the axis AX) from the base end side toward the tip end side and is adjacent to the second inclined surface S2 at the second end E2, and is provided between the second end E2 and the third recess C3 on the tip end surface T2.
[0083] That is, in the second die D2, a protrusion like a ring-shaped mountain having a ring-shaped ridge formed by the second end E2, which is the end on the tip side of the second inclined surface S2, is formed on the tip surface T2, so that the second recess C2 can be reliably formed on the back surface of the plate material PM.
[0084] <effect> In the fifth method, as described above, a frustum-shaped convex portion having a first inclined surface as its side surface and a plane perpendicular to the pressing direction defined by the first end portion as its upper base is protruded from the tip surface of the first die, similar to the first die used in the fourth method, and a fourth inclined surface which is an annular inclined surface that slopes outward as it moves from the base end side to the tip side and is adjacent to the second inclined surface at the second end portion is protruded between the second end portion and the third recess on the tip surface of the second die, similar to the second die used in the third method.
[0085] Therefore, according to the fifth method, like the fourth method described above, the risk of sagging occurring on the peripheral edge of the hole drilled in the plate material when the scrap is punched out in the second step, which would result in crushing of the chamfer that should remain on the peripheral edge on the back side of the hole, is reduced, and a second recess can be reliably formed on the back side of the plate material, like the third method described above.
[0086] For the purpose of explaining the present invention, several embodiments having specific configurations have been described with reference to the attached drawings. However, the scope of the present invention should not be construed as being limited to these exemplary embodiments, and it goes without saying that appropriate modifications can be made within the scope of the claims and the matters described in the specification. [Explanation of symbols]
[0087] PM…Plate material C1…First recess C2: Second recess BP1,BP2…Protuberance PP2: Second protrusion D1…First die T1…Tip surface S1: First slope E1...first end S3: Third slope PP1: First protrusion UB…upper bottom D2: Second die T2…Tip surface S2…Second slope E2…Second end C3…3rd recess S4: Fourth slope P1…Punch AX…Axis H1…1st holding material H2…Second holding material SC…Scrap
Claims
1. A punching method for punching a predetermined portion of a plate material by pressing the plate material with a punch, a first step of pressing a first die, the tip surface of which is provided with a first inclined surface that is an annular inclined surface that inclines inward as it moves from the base end side to the tip side, against a surface of the plate material to form a first recess, the recess including a first inclined portion that is a portion having an annular shape corresponding to the first inclined surface, on the surface of the plate material, and pressing a second die, the tip surface of which is provided with a second inclined surface that is an annular inclined surface that inclines inward as it moves from the base end side to the tip side, against a rear surface of the plate material to form a second recess, the annular recess including a second inclined portion that is a portion having an annular shape corresponding to the second inclined surface, on the rear surface of the plate material; a second step of pressing at least a part of a region surrounded by the first inclined portion included in the first recess on the front surface of the plate material with the punch to punch out a part of the plate material; Including, In the second step, the plate material is pressed by the punch in a pressing direction, which is a first projection view, In the first step, a first region, which is a region surrounded by a first end portion, which is an end portion on the tip side of the first inclined surface, is entirely included in a second region, which is a region surrounded by a second end portion, which is an end portion on the tip side of the second inclined surface; At least in the second step of the punch, the entire punch region, which is a region corresponding to a portion of the plate material that advances in the pressing direction further than the surface of the plate material, overlaps with the first region or is included in the first region. Punching method.
2. The punching method according to claim 1, In a first cross section, which is a cross section taken along a plane including a first axis that is a common central axis of the first region and the second region, an angle between a first line that is a line passing through the first end portion and the second end portion and the first axis is equal to or greater than 7 degrees and equal to or less than 12 degrees; In the first projection view, the first region and the second region are rotationally symmetric about the first axis and have similar shapes. Punching method.
3. The punching method according to claim 1 or 2, In the first die, a third inclined surface is provided on the tip surface, the third inclined surface being an annular inclined surface that is inclined outwardly from the base end side toward the tip end side and adjacent to the first inclined surface at the first end portion, In the second die, a fourth inclined surface is provided on the tip surface, the fourth inclined surface being an annular inclined surface that is inclined outwardly from the base end side toward the tip side and adjacent to the second inclined surface at the second end portion. Punching method.
4. The punching method according to claim 1 or 2, In the first die, a frustum-shaped convex portion is provided on the tip surface, the convex portion having the first inclined surface as a side surface and a plane perpendicular to the pressing direction defined by the first end portion as an upper base, In the second die, a third recess which is a recess that opens to the tip surface is provided on the inner side of the second end portion. Punching method.
5. The punching method according to claim 4, In the second die, a fourth inclined surface is inclined outwardly from the base end side to the tip end side and is an annular inclined surface adjacent to the second inclined surface at the second end portion, and is provided between the second end portion and the third recessed portion on the tip surface. Punching method.
Citation Information
Patent Citations
Absorption refrigerator
JP1988015048A
Manufacture of semiconductor luminous element
JP1989048482A
Manufacturing method of punched article
JP2022143918A
Overtaking processing method by press machine
JP3413140B2