Electronic Board Stacking
The composite substrate with precise alignment and bonding methods addresses CTE mismatch issues, enhancing mechanical and electrical performance for high-density chip integration, improving yield and reliability in electronic device assembly.
Patent Information
- Application Number
- JP2024513302
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-09-29
- Filing Date
- 2022-09-27
- Publication Date
- 2024-10-04
- Estimated Expiration
- 2042-09-27
AI Technical Summary
Existing electronic device assembly methods face challenges in achieving high-density electrical interconnects, fine-pitch wiring, and coefficient of thermal expansion (CTE) matching for chip-to-chip or chiplet-to-chiplet integration, particularly in applications requiring high bandwidth and multi-chiplet integration, leading to mechanical reliability and assembly yield limitations.
A composite substrate with a CTE between 3 and 12 ppm/°C, featuring high-density board layers with trace and via widths less than 10 micrometers, embedded high-k substrate layers with capacitors, and a method involving metal posts and solder connections for precise alignment and bonding of multiple chips on a single package.
The solution enhances mechanical integrity, thermal management, and electrical connectivity, reducing thermomechanical stresses and improving yield by closely matching CTE values, enabling high-density interconnects and flexible power distribution across diverse chip types.
Smart Images

Figure 2024535997000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates generally to electronic device assembly, and more specifically to mechanically and electrically bonding substrates containing electronic components. [Background technology]
[0002] A conventional method of electronic device assembly involves attaching electronic components such as multiple chips or chiplets to a multi-chip substrate and then assembling one or more substrates to a printed circuit board (PCB). The substrate may be an organic substrate, a thin-film organic layer or molded organic, silicon or glass interposer or combinations thereof, with through silicon vias (TSVs), through glass vias (TGVs) and wiring layers, a ceramic substrate, a combination of the above substrates, or other substrate materials and structures. The printed circuit board may consist of a core layer with pin through holes (PTHs) for vertical connections, one or more wiring layers such as for power delivery and distribution, and additional build-up layers on either side of the core to provide additional high density horizontal wiring layers and vertical via interconnects. The multi-layer ceramic carrier includes vias, contact pads and connecting conductors or strips. Electronic components such as chips may be stacked using TSV or wire bonding, or a substrate may be stacked on another substrate using micro solder interconnects or micro ball grid array solder joints, or solder and copper pillar arrays, or a substrate may be connected to a PCB using larger solder ball grid arrays such as pitches greater than 500 micrometers, or using multi-pin sockets. There is a need for high bandwidth chip-to-chip or chiplet-to-chiplet interconnects, direct stacking of chips and / or substrates with high density electrical interconnects, fine pitch wiring, large packaging, and good matching of coefficient of thermal expansion (CTE). These features can support high reliability in applications such as artificial intelligence, cloud data centers, and other applications. Similarly, there is a need for high bandwidth chip or chiplet integration with multi-chiplet integration in smaller XY size formats, such as for mobile communication applications and other applications. Summary of the Invention
[0003] The composite substrate includes a base substrate having a coefficient of thermal expansion (CTE) between 3 and 12 ppm / °C, a surface area greater than 25 mm x 25 mm, an electrical connection on a bottom surface, an electrical connection on a top surface, and one or more wiring layers electrically connected between the bottom surface and the top surface, and a set of high density substrate layers electrically and mechanically connected to a top surface of the base substrate, each layer of the set of high density substrate layers including wiring and vias connecting the top and bottom of each layer of the set of high density substrate layers, each layer of the set of high density substrate layers supporting wiring with a width of less than 2 micrometers to about 10 micrometers and a spacing between wires of less than 2 micrometers to about 10 micrometers, a pitch connection between the top surface of the base substrate and the bottom surfaces of the set of high density substrate layers supporting a pitch of less than 50 micrometers to about 300 micrometers, and a pitch connection on the top surfaces of the set of high density substrate layers supporting a pitch of less than about 150 micrometers.
[0004] The composite substrate comprises a base substrate having a coefficient of thermal expansion (CTE) between 3 and 12 ppm / °C, a surface area greater than 25 mm x 25 mm, an electrical connection on a bottom surface, an electrical connection on a top surface, and one or more wiring layers electrically connected between the bottom surface and the top surface, a set of high-dielectric constant substrate layers electrically and mechanically connected to the top surface of the base substrate, each layer of the set of high-dielectric constant substrate layers including wiring and vias connecting the top and bottom of each layer of the set of high-dielectric constant substrate layers, and a set of one or more discrete decoupling capacitors embedded within the set of high-dielectric constant substrate layers; a set of connected high density substrate layers, each layer of the set of high density substrate layers including wiring and vias connecting the top and bottom of each layer of the set of high density substrate layers, each layer of the set of high density substrate layers supporting wiring with widths of less than 2 micrometers to about 10 micrometers and spacing between wires of less than 2 micrometers to about 10 micrometers, a pitch connection between a top surface of the high dielectric constant substrate layer and a bottom surface of the set of high density substrate layers supporting a pitch of less than 50 micrometers to about 300 micrometers, and a pitch connection on the top surface of the set of high density substrate layers supporting a pitch of less than about 150 micrometers.
[0005] The method includes attaching a set of metal posts to each contact on a bottom surface of a set of high density substrate layers, attaching the set of high density substrate layers to a handler, attaching an interconnect layer to the base substrate, the interconnect layer including openings aligned with the contacts on a top surface of the base substrate, and attaching the set of high density substrate layers to the base substrate with each metal post aligned with the contacts on the top surface of the base substrate.
[0006] The following detailed description, given by way of example and not intended to be limiting, is best understood when read in conjunction with the accompanying drawings. [Brief description of the drawings]
[0007] [Figure 1] FIG. 2 is a top view of electronic components mounted on a substrate, according to one embodiment. [Diagram 2] FIG. 2 is a side view of FIG. 1 taken along section line AA, according to one embodiment. [Diagram 3] FIG. 2 is a top view of a thin film substrate on a substrate according to one embodiment. [Figure 4] FIG. 4 is a side view of FIG. 3 taken along section line AA, according to one embodiment. [Diagram 5] FIG. 2 is a side view of a thin film substrate attached to a handler according to one embodiment. [Figure 6] FIG. 2 is a side view of a substrate and interconnect layers according to one embodiment. [Figure 7] FIG. 2 is a side view of a substrate and interconnect layers according to one embodiment. [Figure 8] FIG. 2 is a side view of a thin film substrate and a substrate according to one embodiment. [Figure 9] FIG. 2 is a side view of a thin film substrate and a substrate according to one embodiment. [Figure 10] FIG. 2 illustrates a top view of a thin film substrate and a high dielectric constant substrate (or integrated decoupling capacitor (or discrete capacitor) and / or inductor layer (or discrete inductor)) attached to a substrate according to one embodiment. [Figure 11] FIG. 11 is a side view of FIG. 10 taken along section line AA, according to one embodiment. [Figure 12] FIG. 2 is a side view of a high dielectric constant substrate mounted on a handler according to one embodiment. [Figure 13] FIG. 2 is a side view of a substrate according to one embodiment. [Figure 14] FIG. 2 is a side view of a substrate and interconnect layers according to one embodiment. [Figure 15] FIG. 2 is a side view of a thin film substrate attached to a substrate according to one embodiment. [Figure 16] FIG. 2 is a side view of a thin film substrate attached to a substrate according to one embodiment. [Figure 17] FIG. 2 is a side view of a high dielectric constant substrate mounted on a handler according to one embodiment. [Figure 18] FIG. 2 is a side view of a substrate according to one embodiment. [Figure 19] FIG. 2 is a side view of a substrate according to one embodiment. [Figure 20] FIG. 2 is a side view of a high dielectric constant substrate attached to a substrate according to one embodiment. [Figure 21] FIG. 2 is a side view of a high dielectric constant substrate attached to a substrate according to one embodiment. [Figure 22] FIG. 2 is a side view of a high dielectric constant substrate attached to a substrate according to one embodiment. [Diagram 23] FIG. 2 is a side view of a high dielectric constant substrate and a thin film substrate attached to the substrate, according to one embodiment. [Figure 24] 1 is a flow chart of a method for stacking substrates, according to one embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0008] It should be understood that for ease of illustration, elements illustrated in the figures have not necessarily been drawn to scale, for example, the dimensions of some of the elements may be exaggerated relative to other elements for clarity, and where considered appropriate, reference numerals may be repeated among the figures to indicate corresponding or analogous features.
[0009] Although detailed embodiments of the claimed structures and methods are disclosed herein, it can be understood that the disclosed embodiments are merely exemplary of the claimed structures and methods, which may be embodied in various forms. However, the present invention may be embodied in many different forms and should not be construed as being limited to the illustrative embodiments set forth herein. The description may omit details of well-known features and techniques so as not to unnecessarily obscure the presented embodiments.
[0010] References herein to "one embodiment," "an embodiment," "exemplary embodiment," and the like indicate that a described embodiment may include a particular feature, structure, or characteristic, but not all embodiments may necessarily include that particular feature, structure, or characteristic. Furthermore, such phrases do not necessarily refer to the same embodiment. Furthermore, when a particular feature, structure, or characteristic is described in connection with one embodiment, it is recognized that it is within the knowledge of others skilled in the art to include such feature, structure, or characteristic in connection with other embodiments, whether or not expressly described.
[0011] In the following description, the terms "top," "bottom," "right," "left," "vertical," "horizontal," "top," "bottom," and derivatives thereof, are intended to relate to the disclosed structures and methods as oriented in the drawings. The terms "overlying," "atop," "on top," "positioned on," or "positioned atop" mean that a first element, such as a first structure, is above a second element, such as a second structure, where there may be an intervening element, such as an interface structure, between the first and second elements. The term "direct contact" means that a first element, such as a first structure, and a second element, such as a second structure, are connected without an intermediate conductive, insulating, or semiconducting layer at the interface between the two elements.
[0012] In the following detailed description, some process steps or operations known in the art may be grouped together for presentation or illustration purposes and may not be described in detail in some cases so as not to obscure the presentation of the embodiments of the present invention. In other cases, some process steps or operations known in the art may not be described at all. It should be understood that the following description instead focuses on distinct features or elements of various embodiments of the present invention.
[0013] The present invention relates generally to semiconductor packaging, and more specifically to the mechanical and electrical bonding of substrates containing electronic components, photonic components and / or chips.
[0014] There is a need to enable direct stacking of electronic components and substrates containing chips and chip stacks on a substrate that supports high density electrical interconnects, fine pitch wiring, large packaging and sufficient matching of coefficient of thermal expansion (CTE) without the need for traditional silicon interposers or packaging implementations with glass, ceramic or hybrids. Currently, the CTE of organic substrates is relatively high at about 18 ppm, and depending on the interconnect pitch of these chips and / or interposers, it may be difficult to mount large chips and / or interposers with fine pitch interconnects on a 400mm substrate due to mechanical reliability and / or assembly yield limitations, especially as the interconnect pitch narrows from 30 micrometers to below 100 micrometers. 2 Approximately 3000mm from 2 This creates large CTE mismatches and therefore thermo-mechanical stresses and strains, especially on the interconnects with the greatest distance from the neutral point.
[0015] For example, silicon components may have a CTE of approximately 3 ppm / °C. Ceramic base substrates may have a CTE ranging between 8-10 ppm / °C, and some as low as 3 ppm / °C. Glass base substrates may have a CTE ranging between 3-12 ppm / °C. As the number of electronic components increases, the surface area of the base substrate may increase and may be 25 mm x 25 mm, 50 mm x 50 mm, 100 mm x 100 mm or more.
[0016] To complement the needs of multi-chip modules, there is an industry shift towards chiplet integration and segmented packaging. Instead of a single electronic component or large system on a chip (system-on-chip (SOI)), there is a shift towards the use of segmented smaller electronic components, chips or chiplets, each with separate blocks of content or functionality optimized for a different function. Different electronic components may come from different foundries and / or different nodes, resulting in the need for hybrid or composite packages with different types of combinations of electronic components such as processors, accelerators, memory, memory chip stacks and other types, each with different power level requirements. There may be different types of interconnects or metal posts on each electronic component, such as different pitches between connections, different numbers of connections, and different bandwidths of some connections required between different electronic component combinations.
[0017] A chip may also be called a chiplet, die, die stack, integrated circuit, electronic component, component, electronic device, semiconductor device, or device, among other names. A chip may be a logic chip, a voltage reference device, a digital signal processor, a microprocessor, a microcontroller, a graphics processor, a memory device, a memory cube, a booting device, a radio frequency device, a high bandwidth memory device, a discrete component, or any other semiconductor device.
[0018] Industry shifts also include an increase in the number of input / output signal lines between components. As the number of connections for input / output increases, the pitch becomes finer, thereby reducing the space between each connected chip being packaged. For example, pitch sizes are getting smaller and smaller, from 100 micrometers to 50 micrometers to 30 micrometers to 10 micrometers or less. As pitch sizes get smaller, tighter specifications drive more stringent flatness and rigidity requirements, increasing the need for both the chip side and the package to remain flat to maintain the integrity of the connection between the chip and the package.
[0019] Additionally, package sizes and form factors are increasing to accommodate more integration on modules in multi-packaged models that can keep energy consumption at low levels, unlike individually packaged chips or components.
[0020] The above factors increase the need to combine multiple chips of different sizes, power requirements, contact spacing, etc. onto a single package. Additionally, there is a need to control thermal properties by minimizing the difference in thermal expansion between the chip and the package, and to manage the power requirements and signals between the chips. As chip requirements change over time, flexibility in packaging allows for better management when combining multiple chips into a single package.
[0021] The advantage of combining multiple chips into a single package is the ability to segment different elements of the packaging technology, such as input / output requirements, processing, memory, etc., and then integrate those segments together.
[0022] Packaging is needed to accommodate the increasingly fine pitch interconnects used for high bandwidth signal connections between chips across the package, along with providing differential power delivery or distribution at the correct voltage and current levels as required by each chip or set of chips. Fine pitch interconnects are sometimes referred to as thin film interconnects or fan-out interconnects in wafer level packaging. There is a need for packaging with greater dimensional flexibility to package several components into more complex systems, including heterogeneous components with different pitches, high currents and isolated power domains, while maintaining high reliability, profitability and cost effectiveness.
[0023] Traditionally, power is delivered from the back of the package upwards through the package and distributed to each of the chips or chip stacks. With a combination of different electronic components, each with different voltage and current requirements, power is delivered to each electronic component through both horizontal and vertical connections, thereby increasing the total power consumption. Coarser wires are required for power distribution, and as the package size increases, the power distribution may have to travel longer distances, requiring wider wires for signal integrity over longer distances. For example, signal lines may be 2 microns and are shrinking to 1 micron or less, while power lines may need to be thicker than 2 microns, such as 4 microns. The spacing between signal lines may be 5 microns or less, for example 4 microns. The pitch may shrink from 150 microns to 100 microns, 55 microns, and 50 microns. A pitch connection on the top surface of a set of high density board layers may support a pitch of 100 microns. The pitch connection between the top surface of the base substrate and the bottom surface of its set of dense substrate layers can support a 100 micrometer pitch.
[0024] We propose a composite substrate or module with multiple chips mounted in a single package, including one or more integrated high density substrate layers (HDSLs), secondary or lower density substrate layers (LDSLs), optional additional layers, and optional interconnects.
[0025] HDSL provides high density interconnect with fine pitch routing and power for circuit, power distribution and connection integrity. This composite substrate allows assembly integration that can include on-package test platforms, allowing selective sequencing of die, die stacks, chips, chip stacks, electronic components and chip placement with the desired chip being placed last. This composite structure allows rework for replacement of defective components or integrated structures. The composite structure can support chip or multi-chip thermal cooling mechanisms and provide mechanical support for all components.
[0026] LDSL defines the mechanical and thermal properties of composite boards by supporting low density interconnects, sparse pitch wiring, making it easy to control the XY CTE. LDSL can also provide power delivery, power distribution and power quality and multi-chip integration and provide a test platform. LDSL supports the possibility of adding one or more high density board layers and supports "Quality Assured Boards" with high density and low density board layers. LDSL supports chip, multi-chip thermal cooling integration / mechanical support to enable assembly integration (preferred chip last) and / or rework of chips, chip stacks and components to facilitate fabrication of integrated modules, subsystems or system solutions.
[0027] HDSL and LDSL layers can have mixed pitch and diameter vias, pads and interconnects, such as larger diameters to accommodate higher power delivery for hot spots and higher power chips, and smaller diameters for signal communication at high interconnect density. HDSL and LDSL can have segmented power planes and layers to optimize power delivery or interconnects to high-k capacitive layers or structures, discrete capacitors or integrated voltage regulating dies to support heterogeneous integration of dies, die stacks and components that may be from multiple foundries, using different technology nodes, different power levels, and have different voltage specifications / operating limits.
[0028] HDSL and LDSL may have electrical connections for testing or powering, and these electrical connections may be opened using select wires, or connection disconnection by laser and dielectric sealing, local encapsulation, etc., or by other methods that leave modified structures with select wires or interconnects open for testing, yield, functionality or other application operations of the board or module.
[0029] HDSL and LDSL also have optional structures that support mechanical or thermal cooling enhancements using heat sinks, caps, thermal vias, thermal wires, sealing bands, or other means that benefit the yield, mechanical integrity, thermal cooling of the substrate and integrated die, die stack, components, and thermal cooling structures for cost or product function or product reliability or other benefit to the product application.
[0030] The HDSL and LDSL may also have any structure that provides artificial intelligence (AI) learning for manufacturing yield, assembly yield improvement, or functionality optimization, or a combination thereof, based on AI structure learning and enhancement in manufacturing.
[0031] HDSL and LDSL may also have optional structures supporting on-module optical or electrical links from the top, bottom or edge of the substrate layer, or a combination thereof, to support enhanced off-board or off-module communications with other substrates / modules, memory storage, memory cards, subsystems or systems, etc.
[0032] Fabricated and assembled integrated HDSL with chips, chip stacks and electronic components can be bonded and tested using built-in self-test (BIST) sites as part of the HDSL and using test dies for full or partial assembly and functional testing. The BIST test sites and test dies can later be removed from the handle wafer or panel carrier. Tested integrated HDSL with qualified subassemblies are available.
[0033] Optional additional layers may also include integrated or embedded components to provide high density embedded capacitance, integrated discrete capacitance, efficient power delivery and management, and voltage regulation to one or more heterogeneous dies, die stacks, or other components.
[0034] Any interconnects may include optical link chips and / or waveguides, or chip sets for off-board or off-module, "on-module optical links" to other modules, memory cards, subsystems or systems.
[0035] An embodiment of a composite substrate or module with multiple chips mounted in a single package includes using solder paste to implement the interconnects, using solder studs to implement the interconnects, and stacking layers in sequence using solder paste or solder studs. An embodiment includes using HDSL and LDSL, and verifying mechanical and electrical integrity of the composite substrate prior to chip attachment. An embodiment uses copper-copper (Cu-Cu) bonding, copper pads / studs, or pillar bonding, nickel / gold (Ni / Au) solder, under bump metallurgy (UBM), or other interconnects, injection molded solder (IMS) technology for via and / or bump interconnects, or other electrical and / or thermal interconnects, or encapsulation structures.
[0036] One embodiment uses assembly on or into a stacked electronics board with additional testing such as testing of substrate layers for qualified low and high density layers, testing after assembly and / or rework of low and high density layers to create a qualified stacked electronics board, testing of die, die stacks and / or components for qualified good die (KGD), statistical partial or full testing to support multi-chip integration and / or rework to achieve high board and module yields.
[0037] Hereinafter, embodiments of a composite substrate or a composite module in which multiple chips are mounted in a single package will be described in detail with reference to the accompanying drawings, FIGS. 1 to 24.
[0038] 1 and 2, a package 10 of electronic components mounted on a substrate is shown according to one example embodiment. Figure 1 is a top view of package 10, and Figure 2 is a side view of Figure 1 along section line AA. Package 10 includes a base substrate 12, a high dielectric constant substrate 14, an interconnect layer 16, a thin film substrate 18, an integrated circuit 20, a memory chip 22, a hub controller integrated circuit 24, a long reach input / output integrated circuit 26, and wires 28.
[0039] The base substrate 12 may be a multi-layer ceramic substrate, silicon wafer, glass wafer or panel or other substrate having a top surface and an array of electrical contact pads patterned on the top surface. Each of the layers of the multi-layer substrate may have an array of electrical vias and wires for circuitry for connection to other layers of the base substrate 12 and to the electrical contact pads on the top surface of the base substrate 12. The base substrate 12 may be square or rectangular, between 10-600 square millimeters or more, and may be between 1-10 millimeters or more thick. There may be 20-30 or more layers in the base substrate 12. Each of the layers may be ceramic with metallization for vias, wiring, and contact pads. The input / output pitch of the base substrate 12 may be between 150-200 micrometers on the top surface and between 750-1000 micrometers on the bottom surface, although the input / output pitch may be larger or smaller on the top and bottom surfaces, respectively. The material of the base substrate 12 can be a combination of mixed / low CTE and high dielectric constant materials or embedded components.
[0040] The high-k substrate 14 can be conformally formed on the base substrate 12 and covers the top surface of the base substrate 12. The high-k substrate 14 can be deposited using common deposition techniques, such as atomic layer deposition (ALD), molecular layer deposition (MLD), chemical vapor deposition (CVD), physical vapor deposition (PVD), high density plasma (HDP) deposition, and spin-on techniques, followed by an anisotropic vertical etching process, such as reactive ion etching (RIE), or any suitable etching process. In one embodiment, the high-k substrate 14 can include one or more layers. The high-k substrate 14 can include materials such as HfO2, ZrO2, Al2O3, La2O3, TiO2, SrTiO3, LaAlO3, Y2O3, HfOxNy, silicates thereof, and alloys thereof. The high-k substrate 14 can be 2 nm thick. The high dielectric constant substrate 14 has openings corresponding to contact pads on the top surface of the base substrate 12 that support vertical interconnects, such as for low loss signal integrity electrical link communication through a low dielectric constant dielectric. The high dielectric constant substrate 14 supports decoupling capacitance, such as for voltage regulation.
[0041] The interconnect layer 16 can be conformally formed on the base substrate 12 and covers the top surface of the high dielectric constant substrate 14. The interconnect layer 16 can include a dielectric adhesive material or sheet. Examples of materials used for the interconnect layer 16 include HD3007 from HD MicroSystems™ (HD MicroSystems™ is a trademark of HD MicroSystems, LLC), Su-8 photoresist, PSPI, NCF, B-stage adhesive layer, or other materials. In one embodiment, the interconnect layer 16 can be between 1 and 120 micrometers thick. The interconnect layer 16 can provide electrical connections such as metal vias, vias with pads, vias with jogs, which can be copper (Cu), solder, and other conductive materials. The metal vias and jogs can be a single layer or multiple layers with vias formed by lithography, etching, laser, copper (Cu) plating, solder plating, IMS, or other means. The jogs can be overlapping contacts on the lower layer of the interconnect layer that allow for dimensional changes during thermal cycling. For example, the contacts on the substrate, which may be a ceramic substrate, may move in the xy dimensions. The jogs may be short electrical redistribution contacts that take into account ceramic shrinkage and distortion tolerances due to processing to allow for one or more design points of electrical connection adjustments, such as machining, sintering or other thermal / processing changes that affect size and feature location accuracy in the X, Y and Z dimensions of the substrate. Each of the contacts on the substrate may be characterized for movement after thermal cycling, and a corresponding jog may be formed for each corresponding contact on the bottom of the interconnect layer.
[0042] The interconnect layer 16 can be an LDSL as described above. The interconnect layer 16 can include several layers of first thin films with wiring. In one embodiment, each layer of the first thin films can include a polyimide-based dielectric between 5-8 micrometers and a copper thickness for a 20 micrometer line width and spacing, 150 micrometer bump pitch, and there can be 8 to 10 or more first thin film layers in the build-up layer 16. The interconnect layer 16 can provide circuitry to connect the chips on the package 10. The interconnect layer 16 can provide wiring, vias, and circuitry on each of the first thin film layers. The interconnect layer 16 can have contact pads on its top surface that electrically and mechanically connect to the inputs and outputs of the chips mounted on the package 10, including the hub controller integrated circuit 24, the long reach input / output integrated circuit 26, wires 28, and any other electronic components on the package 10. In one embodiment, the interconnect layer 16 can provide circuitry for the global input / output of the package 10. The bottom surface of the interconnect layer 16 may have contact pads that align with the contact pads on the top surface of the base substrate 12 to electrically and mechanically connect to one another. The interconnect layer 16 may have openings that correspond to the openings in the high dielectric constant substrate 14 and the contact pads on the top surface of the base substrate 12.
[0043] The thin film substrate 18 can be HDSL as described above. The thin film substrate 18 can cover a portion of the top surface of the interconnect layer 16. The thin film substrate 18 can include several layers of second thin films with wiring. In one embodiment, each layer of the second thin films can include a polyimide-based dielectric between 5-8 micrometers, a copper thickness for line width and spacing between 2-3 micrometers, and a bump pitch of 55 micrometers on the top surface and 150 micrometers on the bottom surface. There may be four or more second thin film layers in the thin film substrate 18. The thin film substrate 18 can provide circuitry connecting the chips on the thin film substrate 18 to the package 10. The thin film substrate 18 can have contact pads on the top surface that electrically and mechanically connect to inputs and outputs of chips mounted on the thin film substrate 18, including memory chips 22, hub controller integrated circuits 24, and any other electronic components on the thin film substrate 18. In one embodiment, the thin film substrate 18 can provide circuitry for local input / output of the package 10. The bottom surface of thin film substrate 18 may have contact pads that align with the contact pads on the top surface of interconnect layer 16 such that they are electrically and mechanically connected to one another.
[0044] As shown in Figures 1 and 2, package 10 has two thin film substrates 18. There may be any number of thin film substrates 18 in package 10. As shown in Figures 1 and 2, each of thin film substrates 18 has four chips mounted thereto, however there may be any number of chips mounted thereto.
[0045] 3 and 4, a thin-film-substrate-on-substrate package 30 is shown according to one example embodiment. Figure 3 is a top view of the package 30, and Figure 4 is a side view of Figure 3 taken along section line AA. The package 30 includes a base substrate 32, an interconnect layer 34, a thin-film substrate 36, metal posts 38, and solder 40.
[0046] The base substrate 32 may be as described above with respect to the base substrate 12. An interconnect layer 34 may be attached to an upper surface of the substrate 32.
[0047] Openings in the interconnect layer 34 may have metal posts 38 and solder 40 that electrically and mechanically connect the contacts and vias on the top surface of the substrate 32 to the bottom surface of the thin film substrate 36. As shown in Figures 3 and 4, there are 36 metal posts 38 in the interconnect layer 34, but there may be any number of metal posts 38 in the interconnect layer 34. The dielectric material may be polyimide (PI) or may be photosensitive polyimide (PSPI) or other dielectric materials. Non-conductive films (NCF), adhesive layers, molding compounds or capillary underfill (CUF) materials may be used for integration. The interconnect layer 34 may be planarized, for example, using chemical mechanical polishing (CMP) techniques, milling, grinding, lasers or other means to achieve fine pitch interconnects between the substrate 32 and the interconnect layer 34, and between the interconnect layer 34 and the thin film substrate 36.
[0048] The openings can have a diameter between 50-100 micrometers, a height between 1-120 micrometers, and a pitch between openings of 150-250 micrometers, and are filled with metal posts 38 and solder 40, respectively. The metal posts can be from 1 micrometer to 75 micrometers.
[0049] The vias in the interconnect layer 34 can be formed with a wider shape than the contacts on the top surface of the substrate 32 to allow for the different CTE and possible shrinkage of the substrate 32, yet still allow electrical connection between the vias in the interconnect layer 34 and the substrate 32.
[0050] Thin film substrate 36 may be as described above with respect to thin film substrate 18 .
[0051] 5, a side view of a first structure 100 is shown according to one example embodiment. The first structure 100 includes a metal post 102, a thin film substrate 104, and a handler 106.
[0052] The thin film substrate 104 can be as described above with respect to thin film substrate 18. The metal posts 102 can be connected to the underside of the thin film substrate. Each of the metal posts 102 can be connected to a via or contact pad on the underside of the thin film substrate 104. There can be any number of metal posts 102 in the handler, for example 144 posts on a 100 mm square thin film substrate 104.
[0053] The top surface of the thin film substrate 104 can then be attached to the handler 106. The handler 106 can provide a stable surface for the thin film substrate 104. The handler 106 can be glass, silicon or other materials. The thin film substrate 104 can be attached to the handler 106 by transfer and adhesion from a handle wafer or panel using a mechanical or laser release layer and adhesive before or after bonding.
[0054] 6, a side view of a substrate and interconnect layer second structure 110 is shown according to one example embodiment. The second structure 110 includes a base substrate 112 having an interconnect layer 114 and an outer pad 118.
[0055] The interconnect layer 114 may be as described above for the interconnect layer 16. The interconnect layer 114 may include a cavity 116.
[0056] The interconnect layer 114 may be attached to the top surface of the base substrate 112. Each of the cavities 116 in the interconnect layer 114 is alignable with an outer pad 118 on the top surface of the base substrate 112. The base substrate 112 may be as described above with respect to the base substrate 12. The outer pads 118 may each provide a contact for the circuitry in the base substrate 112. The interconnect layer 114 may be attached by using heat for solder reflow for electrical connection, and by using a dielectric adhesive and heat and pressure for dielectric bonding.
[0057] 7, a side view of the second structure 110 is shown, according to one example embodiment. Solder paste 120 can be applied into each of the cavities 116 of the interconnect layer 114 of the second structure 110.
[0058] 8, a side view of a resulting composite structure 126 is shown, in which a first structure 100 is mounted onto a second structure 110, in accordance with one illustrative embodiment.
[0059] The metal posts 102 of the first structure 100 are alignable with the solder paste 120 filled cavities 116 of the interconnect layer 114. There may be as many metal posts 102 as there are solder paste 120 filled cavities 116. The first structure 100 and the second structure 110 can be heated to a temperature above the solder melting point of the solder paste 120 and pressed together. The amount of solder paste 120 and the volume of the metal posts 102 in each of the cavities 116 should fill each cavity 116 without metal overflow and should provide electrical and mechanical connection between each outer pad 118 of the base substrate 112 and each corresponding contact or via on the underside of the thin film substrate 104.
[0060] 9, a side view of a composite structure 126 is shown in accordance with one illustrative embodiment.
[0061] 8, after the first structure 100 is mounted on the second structure 110, the composite structure 126 needs to be held in place during a cooling phase until the adhesive resin used for the connection cures or reaches high viscosity and the solder or solder paste 120 forms the electrical connections and pads and solidifies. The adhesive resin can be a polyimide-based adhesive or other dielectric material.
[0062] The handler 106 can then be removed. The composite structure 126 has a thin film substrate 104 with a layer of vias and wiring mounted on an interconnect layer 114 with a layer of vias and wiring. There is a resulting aligned connection between the underside of the thin film substrate 104 and the outer pads 118 on the top side of the base substrate 112 with each metal post 102 embedded in reflowed solder paste 120.
[0063] 10 and 11, a package 150 is shown in accordance with an example embodiment. Figure 10 is a top view of package 150, and Figure 11 is a side view of Figure 10 along section line AA. Package 150 includes a base substrate 152, an interconnect layer 154, a high dielectric constant substrate 160, an interconnect layer 162, and a thin film substrate 168.
[0064] Base substrate 152 may be as described above with respect to base substrate 12. Interconnect layer 154 may be attached to an upper surface of base substrate 152 and may be as described above with respect to interconnect layer 16.
[0065] The openings in the interconnect layer 154 may have metal posts 156 and solder paste 158 that electrically and mechanically connect the contacts and vias on the top surface of the base substrate 152 to the bottom surface of the high dielectric constant substrate 160. The metal posts 156 and solder paste 158 may be formed as described above with respect to the metal posts 102 and solder paste 120 above.
[0066] The high dielectric constant substrate 160 may be as described above with respect to the high dielectric constant substrate 14. The high dielectric constant substrate 160 may be attached to the interconnect layer 154 by dielectric adhesive bonding and electrical pad solder bonding. The high dielectric constant substrate 160 may have metal contacts that electrically and mechanically connect the contacts and vias on the top surface of the interconnect layer 154 to the contacts and vias on the bottom surface of the interconnect layer 162.
[0067] The interconnect layer 162 may be formed as described above with respect to the interconnect layer 16 above. The openings in the interconnect layer 162 may have metal posts 164 and solder paste 166 that electrically and mechanically connect the contacts and vias on the top surface of the high dielectric constant substrate 160 to the bottom surface of the thin film substrate 168. The metal posts 164 and solder paste 166 may be formed as described above with respect to the metal posts 102 and solder paste 120 above.
[0068] The thin-film substrate 168 may be formed as described above with respect to the thin-film substrate 18. The thin-film substrate 168 may be on top of the interconnect layer 162.
[0069] As shown in FIG. 11, the interconnect layer 154 has six metal posts 156, however, the interconnect layer 154 may have any number of metal posts 156.
[0070] 12, a side view of a third structure 200 is shown, according to one example embodiment. The third structure 200 includes a metal post 202, a thin film substrate 204, and a handler 206.
[0071] The third structure 200 may be as described above with respect to the first structure 100, the metal posts 102, the thin film substrate 104 and the handler 106.
[0072] 13, a side view of a fourth structure 210 is shown according to one example embodiment. The fourth structure 210 includes a base substrate 212 with an outer pad 218.
[0073] The fourth structure 210 may be similar to that described above with respect to the second structure 110, including a base substrate 212 as described with respect to the base substrate 12, and an outer pad 218 as described with respect to the outer pad 118.
[0074] 13, solder studs 220 may be formed on the outer pads 218. The solder studs 220 may be an alternative to the solder paste 120 used above. The solder studs 220 may retain their shape during subsequent manufacturing steps.
[0075] 14, a side view of a fourth structure 210 is shown, according to one example embodiment. An interconnect layer 214 may be formed on a base substrate 212.
[0076] The interconnect layer 214 may be formed as described above for the interconnect layer 114. The interconnect layer 214 may include cavities 216. Each of the cavities 216 may be aligned with a solder stud 220 and an outer pad 218.
[0077] In this embodiment, the solder studs 220 may be formed on the outer pads 218 and then on the interconnect layer 214, as opposed to the embodiment of Figures 5-9, where the interconnect layer 114 is attached to the base substrate 112 and then the solder paste 120 is formed in the cavities 116 of the interconnect layer 114. As shown in Figure 14, there are six solder studs 220, although any number of solder studs 220 may be present.
[0078] 15, a side view of a third structure 200 mounted on a fourth structure 210 resulting in a composite structure 226 is shown according to one illustrative embodiment.
[0079] The metal posts 202 of the third structure 200 can be aligned with the solder studs 220 and cavities 216 of the interconnect layer 214. There can be as many metal posts 202 as there are solder studs 220 and cavities 216. The third structure 200 and the fourth structure 210 can be heated to a temperature above the solder melting point of the solder studs 220 and pressed together. The amount of solder in each of the solder studs 202 and the volume of the metal posts 202 in each of the cavities 216 must fill each cavity 216 without metal overflow and must provide electrical and mechanical connection between each outer pad 218 of the base substrate 212 and each corresponding contact or via on the underside of the thin film substrate 204.
[0080] 16, a side view of a composite substrate 226 is shown, according to one example embodiment.
[0081] As described with respect to FIG. 15, after the third structure 200 is mounted onto the fourth structure 210, the composite substrate 226 needs to be held in place during a cooling phase until both the resin and the solder of the solder studs 220 have set.
[0082] The handler 206 can then be removed. The composite substrate 226 has a thin film substrate 204 with a layer of vias and traces mounted on an interconnect layer 214 with a layer of vias and traces. There is a resulting aligned connection between the underside of the thin film substrate 204 and the outer pads 218 on the top side of the base substrate 212 by way of each of the metal posts 202 embedded within a reflow solder stud 220.
[0083] 17, a side view of a fifth structure 300 of a thin film substrate attached to a handler is shown according to one example embodiment. The fifth structure 300 includes a metal post 302, a high dielectric constant substrate 304, and a handler 306.
[0084] The fifth structure 300 may be as described above with respect to the first structure 100, the metal posts 102 and the handler 106.
[0085] In this embodiment, a high dielectric constant substrate 304 is used instead of the thin film substrate 104 in the first embodiment of FIGS. 5 to 9 or the thin film substrate 204 in the second embodiment of FIGS.
[0086] The high dielectric constant substrate 304 may be as described above with respect to the high dielectric constant substrate of FIGS.
[0087] 18, a side view of a sixth structure 310 is shown according to one example embodiment. The sixth structure 310 includes a base substrate 312 with an outer pad 318.
[0088] The sixth structure 310 may be similar to that described above with respect to the second structure 110, including a base substrate 312 as described with respect to the base substrate 12, and an outer pad 318 as described with respect to the outer pad 118.
[0089] 18, solder studs 320 may be formed on outer pads 318. Solder studs 320 may be as described above with respect to solder studs 220.
[0090] 19, a side view of a sixth structure 310 is shown in accordance with one illustrative embodiment. An interconnect layer 314 may be formed on a base substrate 312.
[0091] The interconnect layer 314 may be formed as described above for the interconnect layer 114. The interconnect layer 314 may have cavities 316. Each of the cavities 316 may be aligned with a solder stud 320 and an outer pad 318.
[0092] In this embodiment, solder studs 320 may be formed on outer pads 318 and then interconnect layer 314 may be formed, whereas in the embodiment of Figures 5-9, interconnect layer 114 may be attached to base substrate 112 and then solder paste 120 may be formed within cavities 116 of interconnect layer 114.
[0093] As shown in FIG. 19, there are six solder studs 320 , although there may be any number of solder studs 320 , each corresponding to an outer pad 318 of the base substrate 312 .
[0094] 20, a side view of a fifth structure 300 mounted on a sixth structure 310 resulting in a composite structure 326 is shown according to one illustrative embodiment.
[0095] The metal posts 302 of the fifth structure 300 can be aligned with the solder studs 320 and cavities 316 of the interconnect layer 314. There can be as many metal posts 302 as there are solder studs 320 and cavities 316. The fifth structure 300 and the sixth structure 310 can be heated to a temperature above the solder melting point of the solder studs 320 and pressed together. The amount of solder in each of the solder studs 302 and the volume of the metal posts 302 in each of the cavities 316 must fill each cavity 316 without metal overflow and must provide electrical and mechanical connection between each outer pad 318 of the base substrate 312 and a respective corresponding contact or via on the underside of the high dielectric constant substrate 304.
[0096] 21, a side view of a composite substrate 326 is shown, according to one example embodiment.
[0097] As described with respect to FIG. 20, after the fifth structure 300 is mounted onto the sixth structure 310, the composite substrate 326 needs to be held in place during a cooling phase until both the resin and the solder of the solder studs 320 have set.
[0098] The handler 306 can then be removed. The composite substrate 326 has a high dielectric constant substrate 304 with a layer of vias and traces mounted on an interconnect layer 314 with a layer of vias and traces. There is a resulting aligned connection between the underside of the high dielectric substrate 304 and the outer pads 318 on the top side of the base substrate 312 by each of the metal posts 302 embedded in a reflow solder stud 320.
[0099] Composite structure 326 may be formed using solder paste rather than solder studs 320 and solder studs 330 in one embodiment.
[0100] Composite structure 326 is similar to composite structure 226, but may use a high dielectric constant substrate 304 rather than thin film substrate 204. High dielectric constant substrate 304 may be used when additional layers of substrate may be added to the structure, as described below in the discussion of Figures 22 and 23.
[0101] In some applications, one or more high dielectric constant layers or substrates may be used with discrete decoupling capacitors integrated or embedded in or on the one or more high dielectric constant layers or substrates. The discrete decoupling capacitors may be used to support power delivery and voltage regulation to support increased chip performance. The high dielectric constant substrate 304 may be added to support chip functionality with or without the need for additional high density wiring layers used for low loss, high bandwidth interconnect wiring layers 204, 104 between chips or chiplets.
[0102] 22, a side view of a composite structure 326 is shown in accordance with one illustrative embodiment.
[0103] Solder studs 330 may be formed on the top surface of high dielectric constant substrate 304. Solder studs 330 may be formed at the locations of contacts and vias on the top surface of high dielectric constant substrate 304. Solder studs 320 may be as described above with respect to solder studs 220.
[0104] 23, a side view of a composite structure 326 is shown in accordance with one illustrative embodiment.
[0105] A thin film substrate 334 may be formed on a handler (not shown). The thin film substrate 334 may be formed as described for the thin film substrate 18 above. Metal posts 332, formed as described for the metal posts 156 above, may be attached to the underside of the thin film substrate 334. Each of the metal posts 332 may be attached to the underside of the thin film substrate 334 at a via or contact location.
[0106] A thin film substrate 334 with metal posts 332 on a handler (not shown) can be mounted onto the composite structure 326. The composite structure 326 needs to be held in place during a cooling phase until both the resin and the solder of the solder studs 330 have set. The handler (not shown) can then be removed.
[0107] The composite structure 326 has a high dielectric constant substrate 304 with a layer of vias and traces mounted on an interconnect layer 314 with a layer of vias and traces. Each of the metal posts 302 embedded in a reflow solder stud 320 results in an aligned connection between the bottom surface of the high dielectric constant substrate 304 and an outer pad 318 on the top surface of the base substrate 312. The composite structure 326 has a thin film substrate 334 with a layer of vias and traces mounted on an interconnect layer 336 with a layer of vias and traces. Each of the metal posts 332 embedded in a reflow solder stud 330 results in an aligned connection between the bottom surface of the thin film substrate 334 and an outer pad 318 on the top surface of the high dielectric constant substrate 304.
[0108] The composite structure has additional layers of wiring that may be required for larger scale bonding of the substrates as the number of electrical components mounted on the base substrate 312 increases.
[0109] Referring now to FIG. 24, an operational flow chart illustrating a method 400 of stacking substrates is shown, according to one example embodiment.
[0110] A high density substrate layer (HDSL) is formed (block 402). The HDSL may be as described above with respect to thin film substrate 18. Metal posts may be attached to the underside of the HDSL as described with respect to metal posts 102 above. The metal posts may be metal pads or pillars of copper (Cu), nickel (Ni), gold (Au) or other conductive metal or metal composition. The HDSL is testable.
[0111] The top surface of the HDSL is attached to a handler, such as handler 106 described above, using alignment marks on the handler (block 404).
[0112] An interconnect layer, such as interconnect layer 16, is attached to a top surface of a substrate, such as base substrate 12 (block 406). The interconnect layer may have through holes and optional jogs or spacings that align with the contacts and vias on the top surface of the substrate. Solder paste or solder studs may be placed in the through holes or openings of the interconnect layer with RDL alignment wires or pads adjacent to the ceramic vias with a dielectric layer or a planarizing ceramic surface layer or a planarizing thin-film interconnect adhesive layer or combinations thereof. The interconnect layer may include a redistribution layer (RDL) with jogs to support electrical connections between the layer and corresponding power or signal routing pads. The ceramic vias are electrical conductors, such as copper, molybdenum or tungsten or other metals, that penetrate a ceramic dielectric layer, such as glass, ceramic, cordierite, alumina or other dielectric. The ceramic material may be planarized, such as by grinding, polishing or other methods. A planarized thin film layer can be a single damascene or dual damascene thin film layer, or the "flat" surface of a thin film that is used to fabricate a structure and then removed from a handle wafer or panel, flipped over, detached and / or bonded to a ceramic or other substrate surface by electrical interconnects such as dielectric adhesives and solders.
[0113] The amount of solder in each of the openings is adjustable to accommodate different heights of outer pads or vias on the top surface of the substrate or the bottom surface of the HDSL, or alignment jogs or pads on the interconnect layer.
[0114] The HDSL may be aligned and attached to the substrate using alignment marks or metal posts on the HDSL and alignment marks or solder studs on the substrate (block 408).
[0115] The HDSL, interconnect layers, and substrate can be thermally bonded and compressed at a temperature above the solder melting point (block 410). The total volume of the solder studs and metal posts must be less than or equal to the respective volumes of the openings in the interconnect layers. The combined handler, HDSL, interconnect layers, and substrate must be held in place until the solder solidifies.
[0116] After the solder has solidified, the handler can be removed (block 412). Electronic components can be mounted on the HDSL and electrically and mechanically connected. Each electronic component can be tested prior to mounting. Additional testing can be done at each step of the process to verify the wiring and contacts of each component. Testing can include statistical partial or full testing to support multi-chip integration and rework to achieve high board and module yields.
[0117] Benefits include improved CTE matching, flatness and rigidity compared to high density organic substrate options. The CTE values of thin film substrates, interconnect layers, high dielectric constant substrates and substrates match more closely to the chip due to their inherent material properties, resulting in less warpage during assembly / integration, less damage to the final structure during power cycling and thermal cycling for soldering, and improved reliability during product use.
[0118] Improved flatness due to reduced CTE mismatch during low temperature bonding processes of each thin film substrate as they are assembled / attached to the layers of the substrate, such as by lower temperature solders and dielectric adhesives. Improved stiffness due to stiffness of the ceramic substrate and / or closer matching of CTE between layers of the substrate stack, resulting in less bending or warping than higher CTE organic substrates.
[0119] The structure and method can be used for denser bump pitches, e.g., as large as 200 micrometer pitch, and for interconnects with pitches from less than 10 micrometers to 40 micrometers, and for fine pitch lines and spaces from 20 micrometers to less than 2 micrometers, on large-scale substrates. Benefits include one-pass lamination or integration / assembly with qualified hardware resulting in a higher yield process. One-pass lamination refers to bonding the layers of thin-film substrates before attachment to the substrate. Qualified hardware is used by testing the thin-film substrates before attachment to the handler, if necessary to improve yield.
[0120] Further advantages include the organic substrate option and improved mechanical integrity compared to the sealed bond interface. There is improved mechanical integrity due to the use of coplanar chip-to-substrate layers and coplanar substrate-to-substrate layers. An optional solder seal band around the perimeter of the package seals the structure by baking moisture out of the structure and can provide improved reliability by providing a moisture-to-metal barrier to minimize moisture entrapment.
[0121] Optionally, there may be integrated high density discrete capacitors or high dielectric constant component layers in the thin film substrate. Depending on the decoupling capacitance requirements and component specifications, either multiple discrete components or high dielectric constant layers may be used.
[0122] The description of various embodiments of the present invention has been presented for illustrative purposes, but is not intended to be exhaustive or limited to the disclosed embodiments. Many modifications and variations will be apparent to those skilled in the art without departing from the spirit and scope of the present invention. The terms used in this specification are selected to best explain the principles of the embodiments, practical applications, or technical improvements to the technology found in the market, or to enable those skilled in the art to understand the embodiments disclosed herein.
Claims
1. a base substrate having a coefficient of thermal expansion (CTE) of 3-12 ppm / °C, a surface area of greater than 25 mm x 25 mm, an electrical connection on a bottom surface, an electrical connection on a top surface, and one or more wiring layers electrically connected between the bottom surface and the top surface; a set of high density substrate layers electrically and mechanically connected to a top surface of the base substrate, each layer of the set of high density substrate layers including traces and vias connecting top and bottom of each layer of the set of high density substrate layers, each layer of the set of high density substrate layers supporting traces with widths of less than 2 micrometers to about 10 micrometers and wire-to-wire spacings of less than 2 micrometers to about 10 micrometers, a pitch connection between the top surface of the base substrate and a bottom surface of the set of high density substrate layers supporting a pitch of less than 50 micrometers to about 300 micrometers, and the pitch connection on the top surface of the set of high density substrate layers supporting a pitch of less than about 150 micrometers; A composite substrate comprising:
2. the base substrate includes a plurality of ceramic layers; The composite substrate of claim 1 , wherein the base substrate includes power lines to the set of high density substrate layers.
3. the base substrate comprises one or more glass layers and one or more organic dielectric layers; The composite substrate of claim 1 , wherein the base substrate includes power lines available to the set of high density substrate layers.
4. 2. The composite substrate of claim 1, further comprising an interconnect layer between the set of dense substrate layers and the base substrate, the interconnect layer providing electrical connection between each upper contact on the top surface of the composite substrate and each lower contact on the bottom surface of the set of dense substrate layers.
5. The composite substrate of claim 1 further comprising one or more layers with embedded discrete components within the set of high density substrate layers.
6. The composite substrate of claim 1 further comprising one or more layers of the set of high density substrate layers including trace and via power lines.
7. 10. The composite substrate of claim 1, further comprising the set of high density substrate layers including test contacts and structures.
8. The composite substrate of claim 1 , wherein each layer of the set of high density substrate layers includes wiring in more than one dimension and vias in more than one dimension.
9. a base substrate having a coefficient of thermal expansion (CTE) of 3-12 ppm / °C, a surface area of greater than 25 mm x 25 mm, an electrical connection on a bottom surface, an electrical connection on a top surface, and one or more wiring layers electrically connected between the bottom surface and the top surface; a set of high dielectric constant substrate layers electrically and mechanically connected to a top surface of the base substrate, each layer of the set of high dielectric constant substrate layers including wiring and vias connecting each layer of the set of high dielectric constant substrate layers from above to below, and a set of one or more discrete decoupling capacitors embedded within the set of high dielectric constant substrate layers; a set of high density substrate layers electrically and mechanically connected to top surfaces of the set of high dielectric constant substrate layers, each layer of the set of high density substrate layers including traces and vias connecting the top and bottom of each layer of the set of high density substrate layers, each layer of the set of high density substrate layers supporting traces with widths of less than 2 micrometers to about 10 micrometers and wire-to-wire spacings of less than 2 micrometers to about 10 micrometers, a pitch connection between the top surfaces of the set of high dielectric constant substrate layers and the bottom surfaces of the set of high density substrate layers supporting a pitch of less than 50 micrometers to about 300 micrometers, and the pitch connection on the top surfaces of the set of high density substrate layers supporting a pitch of less than about 150 micrometers; A composite substrate comprising:
10. the base substrate includes a plurality of ceramic layers; The composite substrate of claim 9 , wherein the base substrate includes power lines to the set of high density substrate layers.
11. the base substrate comprises one or more glass layers and one or more organic dielectric layers; 10. The composite substrate of claim 9, wherein the base substrate includes power lines available to the set of high density substrate layers.
12. 10. The composite substrate of claim 9, further comprising an interconnect layer between the set of dense substrate layers and the base substrate, the interconnect layer providing electrical connection between each upper contact on the top surface of the composite substrate and each lower contact on the bottom surface of the set of dense substrate layers.
13. 10. The composite substrate of claim 9, further comprising one or more layers with embedded discrete components within the set of high density substrate layers.
14. 10. The composite substrate of claim 9, wherein one or more layers of the set of high density substrate layers include power lines of wiring and vias, the set of high density substrate layers includes test contacts and structures, and each layer of the set of high density substrate layers further includes wiring in more than one dimension and vias in more than one dimension.
15. attaching a pair of metal posts to each contact on the bottom surface of a pair of high density substrate layers; Attaching the set of high density substrate layers to a handler; attaching an interconnect layer to the base substrate, the interconnect layer including openings aligned with the contacts on the top surface of the base substrate; attaching the set of high density substrate layers to the base substrate with each metal post aligned with a contact on the top surface of the base substrate; A method comprising:
16. 16. The method of claim 15, wherein the base substrate comprises a coefficient of thermal expansion (CTE) of 3-12 ppm / °C, a surface area greater than 25 mm x 25 mm, an electrical connection on a bottom surface, an electrical connection on a top surface, and one or more wiring layers electrically connected between the bottom surface and the top surface.
17. 16. The method of claim 15, wherein a set of high density substrate layers are electrically and mechanically connected to a top surface of the base substrate, each layer of the set of high density substrate layers including traces and vias connecting the top and bottom of each layer of the set of high density substrate layers, each layer of the set of high density substrate layers supporting traces with widths from less than 2 micrometers to about 10 micrometers and spacings between wires from less than 2 micrometers to about 10 micrometers, a pitch connection between the top surface of the base substrate and a bottom surface of the set of high density substrate layers supporting a pitch of less than 50 micrometers to about 300 micrometers, and the pitch connection of the top surface of the set of high density substrate layers supporting a pitch of less than about 150 micrometers.
18. 20. The method of claim 17, further comprising applying a solder interconnect to each of the interconnect layer openings on the contacts on the top surface of the base substrate.
19. 20. The method of claim 18, further comprising melting the solder interconnects and applying heat and pressure to mechanically and electrically join the set of dense substrate layers to the base substrate.
20. The method of claim 17 , further comprising removing the handler from the bonded set of dense substrate layers and the base substrate.
Citation Information
Patent Citations
Polyimide multilayer wiring board and manufacture thereof
JP1992312998A
Semiconductor package circuit board and semiconductor package using the same
JP2016076697A
Integrated circuits and packaging substrates with cavities, and attachment methods including insertion of protruding contact pads into cavities
US20050136634A1