Process for refining pyrolysis oil

JP2024540134AInactive Publication Date: 2024-10-31BASF SE

Patent Information

Application Number
JP2024525492
Authority / Receiving Office
JP · JP
Patent Type
Applications
Current Assignee / Owner
Priority Date
2021-10-27
Filing Date
2022-10-26
Publication Date
2024-10-31
Estimated Expiration
Not applicable · inactive patent

Smart Images

  • Figure 2024540134000012
    Figure 2024540134000012
  • Figure 2024540134000013
    Figure 2024540134000013
  • Figure 2024540134000014
    Figure 2024540134000014
Patent Text Reader

Abstract

The invention relates to a method for purifying a pyrolysis oil comprising the steps of providing a stream S0 comprising a pyrolysis oil, the pyrolysis oil comprising one or more halogenated organic compounds and one or more organic compounds comprising conjugated double bonds, subjecting stream S0 to hydrogenation in at least one reaction zone Z1 containing a heterogeneous hydrogenation catalyst to obtain a stream S1 which is depleted in said one or more organic compounds comprising conjugated double bonds compared to S0, and subjecting stream S1 to dehalogenation in at least one dehalogenation zone Z2 downstream of Z1 to obtain a stream S2 which is depleted in one or more halogenated organic compounds compared to S1.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for refining a pyrolysis oil comprising a hydrogenation step prior to a dehalogenation step, a production unit for carrying out said method, and a refined pyrolysis oil obtained or obtainable by said method. [Background technology]

[0002] Currently, the majority of plastic waste is still landfilled or incinerated to generate heat. Chemical recycling is an attractive method to convert waste plastic materials into useful chemicals. An important technology for chemically recycling plastic waste is pyrolysis. Pyrolysis is the thermal degradation of plastic waste in an inert atmosphere, producing value-added products such as pyrolysis gas, liquid pyrolysis oil and char (residue), with pyrolysis oil being the main product. Pyrolysis gas and char can be used as fuel to generate heat, e.g. for reactor heating purposes. Pyrolysis oil can be used as a feedstock for synthesis gas production and / or processed, e.g. in (steam) crackers, into chemical feedstocks, e.g. ethylene, propylene, C4 cuts, etc.

[0003] Typically, plastic waste is mixed plastic waste composed of various types of polymers. The polymers are often composed of carbon and hydrogen in combination with other elements, such as chlorine, bromine, fluorine, sulfur, oxygen and nitrogen, which often complicate recycling efforts. Elements other than carbon and hydrogen can be harmful during further processing of the crude pyrolysis oil, as they can deactivate or impair the operation of catalysts used in the further processing of the pyrolysis oil. During (steam) cracking, halogen-containing compounds can damage the cracker by corrosion, in that they release hydrogen halides. Sulfur-containing compounds can deactivate or impair the operation of catalysts used in the cracker, or can contaminate the cracker products. Nitrogen-containing impurities can also impair the operation of downstream catalysts. Furthermore, they can cause safety hazards by forming explosive NOx when heated. Thermal degradation of mixed plastics containing polyvinyl chloride (PVC) leads to the formation of compounds with carbon double bonds and hydrogen chloride. Hydrogen chloride liberated from PVC attacks compounds with carbon-carbon double bonds, resulting in the formation of chlorinated organic compounds. Plastic waste typically contains heteroatom-containing additives, such as stabilizers and plasticizers, incorporated to improve the performance of the polymer. Such additives often also contain nitrogen-, halogen- and sulfur-containing compounds as well as heavy metals. For example, waste engine oil, transformer oil, hydraulic oil and machine oil may contain heavy metal wear products. Heavy metals are often toxic, and the presence of heavy metal impurities reduces the quality of pyrolysis oil. In addition, plastic waste may often be unwashed plastics with residues that may also contain other carbon and hydrogen elements. Therefore, reduction of the nitrogen, sulfur, halogen content as well as heavy metal content in pyrolysis oil is essential for any profit-generating processing of pyrolysis oil. In particular, high-quality pyrolysis oil, rich in carbon and hydrogen and low in elements other than carbon and hydrogen, is desirable as a feedstock to prevent catalyst deactivation and corrosion problems in downstream refining processes.

[0004] WO 2017 / 083018 A1 discloses a process for reducing the chloride content of a hydrocarbon feed stream. Furthermore, FR 3 103 822 discloses a process for treating pyrolysis oil for subsequent steam cracking, said process including a hydrogenation step before the hydrotreating step. However, there is still a need to provide an improved process for purifying pyrolysis oil obtained from plastic waste.

[0005] There is therefore a need to provide a method for purifying pyrolysis oil, preferably obtained from plastic waste, in particular by reducing the diene content as well as the chlorine, nitrogen and sulfur content. Indeed, there is a need to provide a high-value refined pyrolysis oil using an economical method.

[0006] Surprisingly, it has been found that the process of the present invention allows for a reduction in diene content as well as chlorine, nitrogen and sulfur content, which reduction is particularly suitable for subsequent steam cracking. Furthermore, it has been surprisingly found that the process of the present invention is an economical way of providing high-value refined pyrolysis oil.

[0007] Moreover, it has been found that dehalogenation of pyrolysis oil is an essential step to maintain stable reactor downstream operation. The reason for the instability is believed to be the formation of ammonium halides, e.g., ammonium chloride, which may desalt when the temperature of the effluent of the hydrotreating step is reduced. Since nitrogen is typically present in the pyrolysis oil feed in greater amounts than halogens, e.g., chlorine, and can only be removed by hydrotreating, then present as ammonia, it is believed to be essential to reduce the halogen content upstream of the hydrotreating step, thereby avoiding the desalting of ammonium halides and reducing their absolute content.

[0008] Furthermore, it is believed that for example HCl may reduce corrosive attack of technical equipment as it is produced from organic chlorides under hydroprocessing conditions. Ammonium chloride itself may also cause corrosion.

[0009] Furthermore, in operation as dechlorination and / or hydrotreating, it has been found that the performance of the catalyst and / or sorbent suffers from an increase in the content of dienes and / or conjugated aromatic olefins, the respective oligomerization polymerization of which is believed to be caused by an increase in temperature and / or radical-forming compounds, such as peroxides or other impurities, such as acting acids or metal salts, such as Lewis acids. It has been found that such oligomerization or polymerization can coke the catalyst and / or sorbent or block their pore system, reducing the accessibility of reactants to the catalyst and / or sorbent. [Prior art documents] [Patent documents]

[0010] [Patent Document 1] International Publication No. 2017 / 083018 A1 Brochure [Patent Document 2] French Patent Specification No. 3 103 822 Summary of the Invention [Means for solving the problem]

[0011] The present invention therefore provides a method for purifying pyrolysis oil, comprising the steps of: (i) providing a pyrolysis oil-containing stream S0, the pyrolysis oil comprising one or more halogenated organic compounds and one or more organic compounds comprising conjugated double bonds; (ii) subjecting the stream S0 provided in (i) to hydrogenation in at least one reaction zone Z1 containing a heterogeneous hydrogenation catalyst to obtain a stream S1 depleted in one or more organic compounds containing conjugated double bonds compared to S0; (iii) subjecting the stream S1 obtained from (ii) to a dehalogenation in at least one dehalogenation zone Z2 downstream of Z1 to obtain a stream S2 depleted in one or more halogenated organic compounds compared to S1; The present invention relates to a method comprising the steps of:

[0012] The term "dehalogenation" as used in the context of the present invention generally includes "dechlorination", "debromination" and "defluorination". According to the present invention, the term "dehalogenation" preferably includes "dechlorination". For example, when the pyrolysis oil subjected to the method according to the present invention does not contain brominated organic compounds and fluorinated organic compounds, but contains only chlorinated compounds as halogenated organic compounds, the term "dehalogenation" covers "dechlorination", and the method of the present invention is a method for purifying pyrolysis oil, and the method includes: (i) providing a pyrolysis oil-containing stream S0, the pyrolysis oil comprising one or more chlorinated organic compounds and one or more organic compounds containing conjugated double bonds; (ii) subjecting the stream S0 provided in (i) to hydrogenation in at least one reaction zone Z1 containing a heterogeneous hydrogenation catalyst to obtain a stream S1 depleted in one or more organic compounds containing conjugated double bonds compared to S0; (iii) subjecting the stream S1 obtained from (ii) to dechlorination in at least one dechlorination zone Z2 downstream of Z1 to obtain a stream S2 depleted in one or more chlorinated organic compounds compared to S1, A preferred step (iii) is (iii.1) introducing a gas stream G1 into a preferably adsorption zone Z2, more preferably the gas stream comprises one or more of hydrogen and nitrogen, more preferably hydrogen; (iii.2) (ii) introducing the stream S1 obtained into Z2; (iii.3) contacting S1 with a heterogeneous adsorbent material suitable for adsorbing chlorides present in at least one of the one or more chlorinated organic compounds present in G1 and Z2 to obtain a stream S2 depleted in the one or more chlorinated organic compounds compared to S1; (iii.4) removing S2 from Z2; Includes.

[0013] In general, the pyrolysis oil contained in S0 can be untreated crude pyrolysis oil. Furthermore, the pyrolysis oil contained in S0 can be a crude pyrolysis oil that has been appropriately pretreated. Such suitable pretreatment procedures are non-hydrogenation methods, including, but not limited to, distillation, dilution, precipitation, filtration, and extraction. The crude pyrolysis oil can be subjected to one suitable pretreatment procedure, or two or more suitable pretreatment procedures.

[0014] If the pretreatment is, for example, distillation, it is possible to enrich the pyrolysis oil with at least one of one or more organic compounds containing conjugated double bonds, or at least one of one or more halogenated organic compounds, or at least one of one or more organic compounds containing conjugated double bonds and at least one of one or more halogenated organic compounds. If the pretreatment agent is, for example, a diluent, it is possible to add one or more alkanes. By doing so, it may be possible to precipitate one or more asphaltenes from the mixture obtained from the dilution, which can then be removed by filtration. If the pretreatment is, for example, extraction, it is possible to use an aqueous extraction medium, for example an acidic aqueous extraction medium or a basic extraction medium.

[0015] Generally, 1 to 100% by weight, or 5 to 100% by weight, or 10 to 100% by weight, or 20 to 100% by weight, or 30 to 100% by weight, or 40 to 100% by weight, or 50 to 100% by weight, or 60 to 100% by weight, or 70 to 100% by weight, or 80 to 100% by weight, or 90 to 100% by weight of the S0 may consist of pyrolysis oil.

[0016] Preferably, 95 to 100% by weight of S0 consists of pyrolysis oil, more preferably 98 to 100% by weight, more preferably 99 to 100% by weight.

[0017] 99.5 to 100% by weight, or 99.8 to 100% by weight, or 99.9% by weight of S0 may consist of pyrolysis oil.

[0018] Preferably, the pyrolysis oil according to (i) comprises one or more organic compounds containing conjugated double bonds in a total amount ranging from 0.1 to 75 g(I2) / 100 g, more preferably from 0.4 to 60 g(I2) / 100 g, more preferably from 1 to 30 g(I2) / 100 g of the pyrolysis oil, determined as described in Reference Example 1.

[0019] Preferably, the one or more organic compounds containing conjugated double bonds have the formula (I) R 1 R 2 C 1 =C 2 R 3 -C 3 R 4 =X (I) (wherein =X is =O, =S, =NR 5 , or =C 4 R 6 R 7 and preferably =C 4 R 6 R 7 is) The compound includes one or more organic compounds according to the present invention.

[0020] Preferably, R 1 , R 2、 R 3、 R 4、 R 5 are each independently H, alkyl having 1 to 6 carbon atoms, alkenyl having 1 to 6 carbon atoms, or aryl having 5 to 10 carbon atoms, more preferably H.

[0021] Preferably, R 6 and R 7are each independently H, alkyl having 1 to 6 carbon atoms, alkenyl having 1 to 6 carbon atoms, or aryl having 5 to 10 carbon atoms, more preferably H.

[0022] Alternatively, preferably, R 4 and R 6 or R 4 and R 7 are concatenated together, so C 3 =C 4 together form an aromatic ring having more preferably 5 or 6 members.

[0023] Preferably, the one or more organic compounds according to formula (I) include one or more of butadiene, isoprene, dienes having 5 or 6 carbon atoms, styrene, methylstyrene, indene, substituted styrenes, substituted indenes, and 3-methyl-2-butenal, more preferably one or more of butadiene, isoprene, dienes having 5 or 6 carbon atoms, styrene, methylstyrene, indene, and 3-methyl-2-butenal.

[0024] With regard to the one or more organic compounds according to formula (I), it is preferred that they comprise styrene.

[0025] Preferably, the pyrolysis oil according to (i) has a styrene content, determined as described in Example 8, in the range of 0.2 to 30 area %, more preferably in the range of 1 to 20 area %.

[0026] Any halogenated organic compound may be included in the pyrolysis oil included in S0 provided in (i). Preferably, the one or more halogenated organic compounds include one or more of mono-, oligo-, or polyhalogenated aromatic compounds, alkyl halides, and alkenyl halides.

[0027] In the context of the present invention, the pyrolysis oil to be refined can have any chlorine content, however, it is preferred that the pyrolysis oil has a total chlorine content, determined as described in Example 2.1, ranging from 30 to 3,000 wppm (ppm by weight), more preferably from 30 to 500 wppm, more preferably from 30 to 200 wppm.

[0028] In the context of the present invention, the pyrolysis oil to be refined can have any chloride content, however, it is preferred that the pyrolysis oil has a chloride content of up to 100 wppm, more preferably in the range of 0 to 30 wppm, determined as described in Example 2.2.

[0029] In the context of the present invention, the pyrolysis oil to be refined can have any nitrogen content, however, it is preferred that the pyrolysis oil has a nitrogen content, determined as described in Example 3, in the range of 50 to 20,000 wppm (ppm by weight), more preferably 50 to 5,000 wppm, more preferably 100 to 4,000 wppm.

[0030] In the context of the present invention, the pyrolysis oil to be refined can have any sulfur content, however, it is preferred that the pyrolysis oil has a sulfur content in the range of 50 to 30,000 weight ppm (wppm), preferably 50 to 5,000 wppm, more preferably 100 to 3,000 wppm, determined as described in Example 4.

[0031] In the context of the present invention, the pyrolysis oil is preferably obtained from plastic waste.

[0032] In the context of the present invention, the "plastic waste" to be pyrolyzed is typically mixed or pre-sorted plastic waste. However, it is also possible to use plastic waste from tires, plastic waste that is pure polymeric plastic waste, or film waste that contains dirt, adhesive materials, fillers, residues, etc. The pyrolysis oil to be refined can typically contain a solid phase and a liquid phase, the liquid phase including an organic phase and an aqueous phase. For example, the weight ratio between the aqueous phase and the organic phase in the liquid phase of the pyrolysis oil can be in the range of 0.01:1 to 3.2:1, preferably in the range of 0.05:1 to 3:1.

[0033] In the context of the present invention, stream S0 is preferably a liquid stream. It is considered that the pyrolysis oil is at least partially in the form of a wax that is suitably liquefied before being subjected to the process of the present invention.

[0034] Before hydrogenation With regard to (ii), the stream SO subjected to hydrogenation in (ii) preferably has a temperature in the range of from 60 to 250°C, more preferably from 80 to 220°C, more preferably from 100 to 200°C.

[0035] In the context of the present invention, any heterogeneous hydrogenation catalyst can be used as long as it allows the hydrogenation (pre-hydrogenation) according to (ii), the stream S0 comprising the pyrolysis oil to be refined before the dehalogenation according to (iii). Preferably, the heterogeneous hydrogenation catalyst according to (ii) comprises an element from groups 8 to 12, more preferably from groups 8 to 10, more preferably from groups 9 and 10 of the Periodic Table of the Elements, more preferably an element selected from the group consisting of Ni, Pd and Co, more preferably an element selected from the group consisting of Ni and Pd.

[0036] Preferably, the heterogeneous hydrogenation catalyst according to (ii) further comprises a support material for said elements of groups 8 to 12 of the periodic table of the elements, the support material being preferably selected from the group consisting of oxide materials and carbon, the oxide material being more preferably one or more of alumina, silica, magnesia, zirconia, titania, zeolitic materials, silica-alumina phosphate (SAPO) materials, zinc oxide, sodium oxide, mixed silica-alumina, zeolites and calcium oxide, more preferably alumina.

[0037] With regard to the heterogeneous hydrogenation catalyst according to (ii), it is more preferred that said catalyst comprises an amount of Ni in the range of from 0.5 to 70 wt.-%, more preferably from 0.75 to 45 wt.-%, more preferably from 1 to 20 wt.-%, calculated as NiO, based on the total weight of the hydrogenation catalyst.

[0038] Preferably, the heterogeneous hydrogenation catalyst according to (ii) further comprises an element from group 6 of the periodic table of the elements, more preferably the element from group 6 is one or more of Mo and W, more preferably Mo.

[0039] Preferably, the heterogeneous hydrogenation catalyst according to (ii) comprises from 1 to 40 wt.-%, more preferably from 2 to 35 wt.-%, more preferably from 3 to 30 wt.-% of an oxide of said element of group 6, more preferably Mo oxide or W oxide, based on the total weight of the hydrogenation catalyst.

[0040] Preferably, the heterogeneous hydrogenation catalyst according to (ii) comprises Ni and Mo supported on a support material, more preferably on a support material as defined above. More preferably, the hydrogenation catalyst comprises Ni and Mo supported on alumina.

[0041] Alternatively, with regard to the heterogeneous hydrogenation catalyst according to (ii), said catalyst more preferably comprises an amount of Pd in ​​the range of from 0.01 to 5 wt.-%, more preferably from 0.1 to 1 wt.-%, more preferably from 0.15 to 0.8 wt.-%, calculated as elemental Pd, based on the total weight of the catalyst.

[0042] Preferably, the heterogeneous hydrogenation catalyst according to (ii) further comprises a promoter, more preferably one or more of elements from groups 10 and 11 of the periodic table of the elements, preferably one or more of Cu, Au, Ag and Pt, more preferably one or more of Ag and Pt, more preferably Ag.

[0043] Preferably, the atomic ratio of the promoter to an element from Groups 8 to 12 of the Periodic Table, more preferably Pd, is in the range of 0.1:1 to 10:1, more preferably 2:1 to 7:1, more preferably 2.5:1 to 6:1.

[0044] Preferably, the heterogeneous hydrogenation catalyst according to (ii) comprises Pd supported on a support material, preferably a support material as defined above, the support material being more preferably alumina or carbon, more preferably alumina.

[0045] In the context of the present invention, the heterogeneous hydrogenation catalyst according to (ii) is preferably in the form of extrudates, pellets, rings, spherical particles or spheres, more preferably spherical particles or extrudates.

[0046] Preferably, (ii) is (ii.1) introducing a gas flow G0 into Z1, the gas flow comprising H2; (ii.2) introducing a flow S0 into Z1; (ii.3) contacting S0 with G0 and a heterogeneous hydrogenation catalyst contained in Z1 to obtain a stream S1 depleted in one or more organic compounds containing conjugated double bonds compared to S0; (ii.4) removing S1 from Z1; Includes.

[0047] Preferably, the gas stream G0 has a temperature in the range of from 100 to 250°C, more preferably from 120 to 220°C, more preferably from 140 to 200°C.

[0048] Preferably, the gas stream G0 is introduced at a pressure in the range of from 10 to 100 bar (abs), more preferably in the range of from 15 to 90 bar (abs), more preferably in the range of from 20 to 80 bar (abs), more preferably in the range of from 20 to 55 bar (abs).

[0049] Preferably, 70 to 100 wt. % of the gas stream G0 consists of H2, more preferably 80 to 100 wt. %, more preferably 90 to 100 wt. %. Further possible ranges are 92 to 100 wt. % or 94 to 100 wt. % or 96 to 100 wt. % or 98 to 100 wt. %.

[0050] According to (ii.1), G0 is preferably introduced into Z1 continuously or semi-continuously, more preferably continuously.

[0051] According to (ii.2), S0 is preferably introduced into Z1 semi-continuously or continuously, more preferably continuously.

[0052] Preferably, G0 is introduced into Z1 according to (ii.1) for a period of time Δt before introducing S0 into Z1 according to (ii.2).

[0053] In particular, when the hydrogenation catalyst comprises Ni, it may be preferred to sulfide the catalyst, preferably after drying, before it is used as a hydrogenation catalyst. Drying may be achieved by subjecting the catalyst to a gas atmosphere, preferably containing nitrogen, e.g., technical grade nitrogen, preferably having a temperature in the range of 150 to 250° C., e.g., 170 to 230° C. or 190 to 210° C. When drying is carried out semi-continuously or continuously, the gas space velocity may be from 1,000 to 3,000 h -1 , for example, 1,500 to 2,500 h -1 or 1,800 to 2,200 hours -1 After drying, H2S is charged, preferably at a temperature in the range of 300 to 400°C, for example 325 to 375°C, preferably until saturation with sulfur is achieved.

[0054] Alternatively, Ni-containing hydrogenation catalysts can be presulfided according to the following (or similar) method: The catalyst is dried at atmospheric pressure under nitrogen flow (GHSV=2000 / h) at 200 °C (heating rate 1 K / min) for at least 2 hours until water is no longer condensed downstream. The catalyst is then cooled to 135 °C, hydrogen is fed to the reactor at GHSV=2000 / h and the reactor is pressurized (1 bar / min). After 1 hour, hexadecane with 2 wt.% dimethyl disulfide is dosed at LHSV=2 / h for 1 hour. The temperature is then increased to 350 °C at 0.25 K / min and held for 2 hours. The introduction of the hexadecane solution is then stopped and the temperature and pressure are adjusted before the introduction of the feed.

[0055] If the hydrogenation catalyst comprises Pd, it may be preferred to activate it under hydrogen flow (GHSV=1000 / h) at 50 to 130° C. (1 K / min), e.g. for 6 to 24 h, e.g. for 12 h, preferably under atmospheric conditions. If the catalyst is reduced in a larger reactor, the hydrogen can be diluted with nitrogen to avoid excessive temperatures.

[0056] During Δt, G0 is contacted with a heterogeneous hydrogenation catalyst, preferably contained in Z1, G0 having a temperature in the range of from 50 to 250° C., more preferably from 120 to 220° C., more preferably from 140 to 200° C.

[0057] At Z1, the liquid hourly space velocity (LHSV) is preferably 0.2 to 10 m 3 / (m 3 h), more preferably in the range of 0.3 to 5 m 3 / (m 3 h), more preferably in the range of 0.5 to 2 m 3 / (m 3 h), and the LHSV is Z1(m 3 S0 to Z1 (m2) per volume of heterogeneous hydrogenation catalyst 3 / h) is defined as the volumetric flow rate.

[0058] In general, according to the invention, it is possible to recycle part of S1, S1' obtained from (ii) and removed from Z1 back into Z1 as part of the starting material subjected to hydrogenation. In this case, not only is stream S0 hydrogenated, but also an additional stream S1'. As far as S1' is concerned, its LHSV in Z1 relative to the LHSV of S0, LHSV(S1'):LHSV(S0), which corresponds to the recycle ratio, is preferably in the range of 1:1 to 20:1, for example 1:1 to 5:1, or 5:1 to 10:1, or 10:1 to 15:1, or 15:1 to 20:1.

[0059] In general, S1' can be mixed with S0 at any suitable position in the process, preferably upstream of Z1. If part of S1 is recycled, the remaining part of S1 is referred to herein as stream S1 subjected to dehalogenation according to (iii).

[0060] In general, the process comprises: (ii.5) removing a gas flow G0′ from Z1, the gas flow G0′ comprising H2; Further includes:

[0061] In general, according to the invention, it is possible to recycle part of G0', G0" obtained from (ii) and removed from Z1 back into Z1 as part of the starting material. In this case, not only is stream G0' introduced into Z1, but also an additional stream G0" is introduced. As far as G0" is concerned, its hourly space velocity GHSV in Z1 relative to the GHSV of G0, which corresponds to the recycle ratio, LHSV(G0"):LHSV(G0), is preferably in the range of 1:1 to 20:1, for example 1:1 to 5:1, or 5:1 to 10:1, or 10:1 to 15:1, or 15:1 to 20:1.

[0062] Preferably, reaction zone Z1 is comprised in a continuous stirred tank reactor (CSTR) or a fixed bed reactor, more preferably a fixed bed reactor, which is more preferably a trickle bed reactor.

[0063] According to (ii), preferably two or more reaction zones Z1 arranged in series and / or in parallel are used, more preferably one single reaction zone Z1 is used according to (ii).

[0064] Preferably, the stream S1 obtained from (ii) and subjected to dehalogenation in (iii) comprises a reduced amount of one or more organic compounds containing conjugated double bonds of 50 to 100%, more preferably 70 to 100%, more preferably 75 to 100% compared to S0. The total amount of one or more organic compounds containing conjugated double bonds is determined as described in Reference Example 1.

[0065] Preferably, the stream S1 obtained from (ii) and dehalogenated in (iii) comprises one or more organic compounds containing conjugated double bonds in a total amount ranging from 0 to 3 g (I2) / 100 g, preferably from 0 to 2 g (I2) / 100 g, more preferably from 0 to 1 g (I2) / 100 g, more preferably from 0 to 0.25 g (I2) / 100 g, more preferably from 0 to 0.1 g (I2) / 100 g of stream S1, determined as described in Reference Example 1.

[0066] Preferably, the stream S1 obtained from (ii) and dehalogenated in (iii) contains a reduced amount of styrene of from 50 to 100%, more preferably from 70 to 100%, more preferably from 75 to 100%, compared to S0. The amount of styrene is determined as described in Example 8.

[0067] Preferably, the stream S1 obtained from (ii) and dehalogenated in (iii) has a styrene content, determined as described in Example 8, in the range of from 0 to 1.5 area %, more preferably in the range of from 0 to 0.1 area %.

[0068] Dehalogenation Preferably, the stream S1 subjected to dehalogenation in (iii) has a temperature in the range of from 150 to 450°C, more preferably from 200 to 400°C, more preferably from 250 to 350°C.

[0069] Adsorption Zone Z2 Preferably, the dehalogenation zone Z2 according to (iii) comprises, more preferably consists of, an adsorption zone, more preferably comprising a heterogeneous adsorption material suitable for adsorbing the halides contained in at least one of the one or more halogenated organic compounds, preferably contained in all of the one or more halogenated organic compounds.

[0070] In the context of the present invention, any heterogeneous adsorbent material can be used according to (iii) as long as it is capable of adsorbing the halides contained in at least one of the one or more halogenated organic compounds. Preferably, the heterogeneous adsorbent material according to (iii) comprises one or more of a carbon-containing adsorbent material and an aluminum-containing adsorbent material, more preferably an aluminum-containing adsorbent material.

[0071] The carbon-containing adsorbent material is preferably a carbon-containing molecular sieve, more preferably activated carbon. The aluminum-containing adsorbent material is preferably alumina, an aluminum-containing molecular sieve, a silicoaluminophosphate, a silica-alumina hydrate or a hydrotalcite. The aluminum-containing molecular sieve is preferably an aluminosilicate, more preferably having a molar ratio of Si:Al calculated as SiO2:Al2O3 ranging from 2:1 to 10:1, more preferably from 2:1 to 4:1. The silica-alumina hydrate preferably has a weight ratio of Al2O3:SiO2 ranging from 1:1 to 10:1, more preferably from 1:1 to 2:1. The hydrotalcite is preferably an aluminum and magnesium containing hydrotalcite, more preferably an aluminum-magnesium hydroxycarbonate, preferably having a weight ratio of MgO:Al2O3 ranging from 63:37 to 70:30.

[0072] Preferably, the heterogeneous adsorptive material comprises hydrotalcite as defined above.

[0073] Heterogeneous adsorbent materials according to (iii) may also contain elements of groups 1, 2, 11 and 12.

[0074] Preferably, the aluminosilicate contains one or more of potassium oxide, sodium oxide, magnesium oxide and calcium oxide.

[0075] Preferably, according to the invention, from 0 to 0.001% by weight, preferably from 0 to 0.0001% by weight, more preferably from 0 to 0.00001% by weight, of the heterogeneous adsorptive material according to (iii) consists of Ni.

[0076] Preferably, the heterogeneous adsorptive material according to (iii) comprises particles characterized by a particle size distribution having a D50 value in the range of 1 to 6,500 micrometers, more preferably 2 to 2,000 micrometers, more preferably 8 to 500 micrometers, more preferably 10 to 50 micrometers or 3 to 9 micrometers, the D50 particle size being determined as described in Reference Example 5.

[0077] More preferably, the heterogeneous adsorptive material, being a hydrotalcite as defined above, comprises particles characterized by a particle size distribution having a D50 value in the range of 3 to 9 micrometers, the D50 particle size being determined as described in Reference Example 5.

[0078] In the context of the present invention, the heterogeneous adsorbent material according to (iii) preferably has an average pore volume in the range of 0.1 to 5 ml / g, more preferably in the range of 0.15 to 2 ml / g, the average pore volume being determined as described in Reference Example 6.

[0079] Preferably, the heterogeneous adsorbent material according to (iii) has a thickness of 50 to 1,000 m 2 / g, more preferably in the range of 100 to 900 m 2 / g, more preferably in the range of 150 to 600 m 2 / g, the BET specific surface area being determined as described in Reference Example 7.

[0080] According to the present invention, the adsorbent material can be suitably regenerated, if desired.

[0081] Preferably, (iii) is (iii.1) introducing a gas stream G1 into a preferably adsorption zone Z2, more preferably the gas stream comprises one or more of hydrogen and nitrogen, more preferably hydrogen; (iii. 2) introducing the stream S1 obtained from (ii) into Z2; (iii. 3) contacting S1 with a heterogeneous adsorbent material suitable for adsorbing the halides present in at least one of the one or more halogenated organic compounds present in G1 and Z2 to obtain a stream S2 depleted in the one or more halogenated organic compounds compared to S1; (iii. 4) removing S2 from Z2; Includes.

[0082] Preferably, the gas stream G1 has a temperature in the range of 250 to 500°C, more preferably in the range of 300 to 400°C.

[0083] Preferably, the gas stream G1 is introduced at a pressure in the range of 1 to 100 bar (abs), more preferably in the range of 5 to 80 bar (abs), more preferably in the range of 10 to 50 bar (abs).

[0084] Preferably, in Z2, the liquid hourly space velocity (LHSV) is 0.2 to 10 m 3 / (m 3 h), more preferably in the range of 0.3 to 5 m 3 / (m 3 h), more preferably in the range of 0.5 to 2 m 3 / (m 3 h), and the LHSV is in the range of Z2(m 3S1 to Z2 per volume of adsorbent material contained in (m 3 / h) is defined as the volumetric flow rate.

[0085] Preferably, 90 to 100% by weight of gas stream G1 consists of H2, more preferably 95 to 100% by weight, more preferably 98 to 100% by weight. Alternatively, preferably, 90 to 100% by weight of gas stream G1 consists of nitrogen, more preferably 95 to 100% by weight, more preferably 98 to 100% by weight.

[0086] According to (iii.1), G1 is preferably introduced continuously or semi-continuously, more preferably continuously, into Z2, and according to (iii.2), S1 is introduced continuously or semi-continuously, more preferably continuously, into Z2.

[0087] Preferably, the adsorption zone Z2 is comprised in a continuous stirred tank reactor (CSTR) or a fixed bed reactor, more preferably a fixed bed reactor, more preferably a trickle bed reactor, the reactor preferably comprising an adsorption bed comprising a heterogeneous adsorption material.

[0088] According to (iii), preferably two or more reaction zones Z2 arranged in series and / or in parallel are used, or one single reaction zone Z2 is preferably used according to (iii), more preferably one single reaction zone Z2 is used according to (iii).

[0089] Preferably, the stream S2 obtained from (iii) has a reduced total chlorine content of from 50 to 100%, preferably from 60 to 100%, more preferably from 75 to 100%, compared to S0 and S1.

[0090] Preferably, the stream S2 obtained from (iii) has a total chlorine content, determined as described in Example 2.1, in the range of from 0 to 200 wppm (ppm by weight), more preferably from 0 to 160 wppm, more preferably from 0 to 130 wppm.

[0091] Preferably, the stream S2 obtained from (iii) has a chloride content, determined as described in Example 2.2, of at most 40 wppm (ppm by weight), more preferably from 0 to 30 wppm, more preferably from 0 to 20 wppm, more preferably from 0 to 1 wppm.

[0092] Preferably, the stream S2 obtained from (iii) comprises one or more organic compounds containing conjugated double bonds in a total amount in the range of from 0 to 3 g (I2) / 100 g, more preferably from 0 to 2 g (I2) / 100 g, more preferably from 0 to 1 g (I2) / 100 g, more preferably from 0 to 0.25 g (I2) / 100 g, more preferably from 0 to 0.1 g (I2) / 100 g of stream S2, determined as described in Reference Example 1.

[0093] Preferably, the stream S2 obtained from (iii) has a nitrogen content, determined as described in Example 3, in the range of from 50 to 20,000 wppm, more preferably from 50 to 5,000 wppm, more preferably from 100 to 4,000 wppm.

[0094] Preferably, the stream S2 obtained from (iii) has a sulfur content, determined as described in Example 4, in the range of from 50 to 30,000 ppm by weight (wppm), more preferably from 50 to 5,000 wppm, more preferably from 100 to 3,000 wppm.

[0095] Preferably, stream S2 has a chlorine content, a nitrogen content, a sulphur content and a total amount of one or more organic compounds containing conjugated double bonds as defined above.

[0096] Catalyst Zone Z2 Alternatively, the dehalogenation zone Z2 according to (iii) comprises a catalytic zone, more preferably is a catalytic zone, which more preferably comprises a heterogeneous dehalogenation catalyst, said catalyst preferably comprising one or more catalytically active elements of groups 8 to 12 of the Periodic System of the Elements.

[0097] In this case, (iii) is preferably (iii.1') introducing a gas stream G1 into a catalytic zone Z2, preferably comprising hydrogen and nitrogen, more preferably hydrogen; (iii.2') (ii) introducing the flow S1 obtained in step (ii) into Z2; (iii.3') contacting S1 with a heterogeneous dehalogenation catalyst, contained in G1 and Z2, to obtain a stream S2 depleted in one or more halogenated organic compounds compared to S1; (iii.4') removing S2 from Z2; (iii.5') more preferably, cooling the S2 removed according to (iii.4'); Includes.

[0098] Preferably, the stream S2 obtained from (iii), before being subjected to hydrotreatment according to (iv) as defined below, is subjected to an extraction, more preferably an extraction using an aqueous extraction medium, to obtain a stream S2 depleted of one or more dissolved halides contained in S2 obtained from the dehalogenation zone Z2, said halides more preferably comprising one or more halides of N-containing organic compounds.

[0099] Hydrotreating The process of the present invention preferably further comprises, after (iii), (iv) subjecting the stream S2 obtained from (iii) to hydrotreating in at least one reaction zone Z3 downstream of Z2, Z3 comprising a heterogeneous hydrotreating catalyst, to obtain a stream S3. Further comprising: Stream S2 subjected to (iv) has a temperature in the range of from 150 to 400°C, more preferably in the range of from 200 to 375°C, more preferably in the range of from 250 to 350°C.

[0100] Concerning the heterogeneous hydrotreating catalyst according to (iv), any heterogeneous hydrotreating catalyst can be used, provided that it allows obtaining stream S3. Preferably, the heterogeneous hydrotreating catalyst according to (iv) comprises an element selected from the group consisting of elements of groups 8 to 10, more preferably groups 9 and 10, of the periodic table of the elements, more preferably Ni and Co, and more preferably the hydrotreating catalyst comprises Ni.

[0101] Preferably, the heterogeneous hydrotreating catalyst according to (iv) comprises an amount of Ni in the range of 0.5 to 10 wt.-%, more preferably in the range of 1 to 6 wt.-%, calculated as NiO, based on the weight of the hydrotreating catalyst.

[0102] Preferably, the heterogeneous hydrotreating catalyst according to (iv) further comprises a support for an element of groups 8 to 10 of the periodic table of the elements, the support being preferably an oxide material. Preferably, the oxide material is one or more of alumina, silica, magnesia, zirconia, zinc oxide, calcium oxide, mixed silica-alumina, zeolites, Mo-doped alumina and titania, more preferably alumina, zeolites and silica-alumina, more preferably alumina.

[0103] Preferably, the heterogeneous hydrotreating catalyst according to (iv) further comprises an element of group 6 of the periodic table of the elements, more preferably the element of group 6 is one or more of Mo and W. Preferably, the hydrotreating catalyst comprises an oxide of said element of group 6, more preferably Mo oxide or W oxide, in the range of from 1 to 40 wt.%, more preferably from 3 to 30 wt.%, based on the weight of the hydrotreating catalyst.

[0104] Preferably, the heterogeneous hydrotreating catalyst according to (iv) comprises Ni and Mo on a support, more preferably on a support as defined above, and the hydrotreating catalyst more preferably comprises Ni and Mo on alumina.

[0105] According to the present invention, the hydrotreating catalyst, in particular the Ni-containing hydrotreating catalyst, may contain from 0.1 to 5 wt. %, preferably from 0.1 to 4 wt. %, more preferably from 0.1 to 3 wt. % phosphorus, calculated as P2O5, based on the total weight of the catalyst.

[0106] Ni-containing hydrotreating catalysts can be presulfided before use according to the following (or similar) method: The catalyst is dried at atmospheric pressure under nitrogen flow (GHSV=2000 / h) at 200°C (heating rate 1 K / min) for at least 2 hours until water is no longer condensed downstream. The catalyst is then cooled to 135°C, hydrogen is fed to the reactor at GHSV=2000 / h and the reactor is pressurized (1 bar / min). After 1 hour, hexadecane with 2 wt.% dimethyl disulfide is dosed at LHSV=,2 / h for 1 hour. The temperature is then increased to 350°C at 0.25 K / min and held for 2 hours. The dose of hexadecane solution is then stopped and the temperature and pressure are adjusted before the feed is dosed.

[0107] Preferably, (iv) is (iv.1) introducing a gas stream G2 into Z3, G2 comprising H2; (iv. 2) introducing the stream S2 obtained from (iii) into Z3; (iv. 3) contacting S2 with G2 and a heterogeneous hydrotreating catalyst contained in Z3 to obtain stream S3; (iv. 4) removing S3 obtained in (iv. 3) from Z3; Includes.

[0108] Preferably, gas stream G2 has a temperature in the range of from 250 to 550°C, more preferably in the range of from 300 to 450°C, more preferably in the range of from 325 to 400°C.

[0109] Preferably, gas stream G2 is introduced at a pressure in the range of from 20 to 150 bar (abs), more preferably in the range of from 30 to 90 bar (abs), more preferably in the range of from 40 to 80 bar (abs), more preferably in the range of from 45 to 60 bar (abs).

[0110] Preferably, in Z3, the liquid hourly space velocity (LHSV) is from 0.1 to 10 m 3 / (m 3 h), more preferably in the range of 0.15 to 5 m 3 / (m 3 h), more preferably in the range of 0.2 to 2 m 3 / (m 3 h), and the LHSV is in the range of Z3(m 3 S2 to Z3 (m2) per volume of heterogeneous hydrotreating catalyst 3 / h) is defined as the volumetric flow rate.

[0111] According to the invention, G2 can preferably be recycled from the stream obtained from the hydroprocessing.

[0112] Preferably, 50 to 100 wt.% of the gas stream G2 consists of H2, more preferably 70 to 100 wt.%, more preferably 90 to 100 wt.%. Further contemplated ranges are 92 to 100 wt.% or 94 to 100 wt.% or 96 to 100 wt.% or 98 to 100 wt.%.

[0113] According to (iv.1), G2 is preferably introduced into Z3 continuously or semi-continuously, more preferably continuously.

[0114] According to (iv.2), S2 is preferably introduced into Z3 continuously or semi-continuously, more preferably continuously.

[0115] Preferably, reaction zone Z3 is contained in a reactor and more preferably comprises n series-connected catalyst beds B(i), i=1...,n, n>2, where catalyst bed B(i) comprises a heterogeneous hydrotreating catalyst, more preferably 2<n<10, more preferably 2<n<5, and B(1) is the most upstream catalyst bed and B(n) is the most downstream catalyst bed.

[0116] More preferably, (iv) is (iv.1') introducing a gas flow G2 into Z3, G2 comprising H2; (iv.2') introducing the stream S2 obtained from (iii) into Z3; (iv.3') n successive process steps P(i), i = 1...n, In P(1), - introducing the gas stream G2 into the catalyst bed B(1) and contacting it with the stream S2 obtained from (iii) and the heterogeneous hydrotreating catalyst in B(1) to form the stream S P A step of obtaining (1); For each P(i), for i=2...n-1, A gas stream F(i-1) containing H2 is introduced into the catalyst bed B(i) and S P (i-1) and the heterogeneous hydrotreating catalyst in B(i) to form a stream S P obtaining (i); -B(i) to S P removing (i); In P(n), - gas stream F(n-1) is introduced into catalyst bed B(n) and S P with a heterogeneous hydrotreating catalyst in B(n-1) and B(n) to obtain a gas stream S3; (iv.4') removing S3 obtained in (iv.3') from Z3; Includes.

[0117] Preferably, gas stream G2 has a temperature in the range of from 250 to 550°C, more preferably in the range of from 300 to 450°C, more preferably in the range of from 325 to 400°C.

[0118] Preferably, gas stream G2 is introduced at a pressure in the range of from 20 to 150 bar (abs), more preferably in the range of from 30 to 90 bar (abs), more preferably in the range of from 40 to 80 bar (abs), more preferably in the range of from 45 to 60 bar (abs).

[0119] Preferably, 50 to 100 wt.% of the gas stream G2 consists of H2, more preferably 70 to 100 wt.%, more preferably 90 to 100 wt.%. Further contemplated ranges are 92 to 100 wt.% or 94 to 100 wt.% or 96 to 100 wt.% or 98 to 100 wt.%.

[0120] Preferably, in Z3, the liquid hourly space velocity (LHSV) is 0.1 to 10 h -1 in the range of 0.1 to 5 h -1 More preferably, in the range of 0.2 to 2 h -1 and the LHSV is in the range of Z3(m 3 S2 or S per volume of heterogeneous hydrotreating catalyst contained in P (i) to Z3(m 3 / h) is defined as the volumetric flow rate.

[0121] According to (iv.1'), G2 is preferably introduced continuously or semi-continuously, more preferably continuously, into Z3.

[0122] According to (iv.2'), S2 is preferably introduced into Z3 continuously or semi-continuously, more preferably continuously.

[0123] Preferably, 50 to 100 wt.% of the gas stream F(i) consists of H2, more preferably 70 to 100 wt.%, more preferably 90 to 100 wt.%. Further contemplated ranges are 92 to 100 wt.% or 94 to 100 wt.% or 96 to 100 wt.% or 98 to 100 wt.%.

[0124] Preferably, the gas stream F(i) is introduced at a pressure in the range of from 20 to 150 bar (abs), more preferably in the range of from 30 to 90 bar (abs), more preferably in the range of from 40 to 80 bar (abs), more preferably in the range of from 45 to 60 bar (abs).

[0125] Preferably, the n serially connected catalyst beds B(i) are fixed catalyst beds.

[0126] Alternatively, reaction zone Z3 is contained in a reactor with one catalyst bed, the catalyst bed comprising a heterogeneous hydrotreating catalyst.

[0127] In the context of the present invention, reaction zone Z3 is preferably comprised in a continuous stirred tank reactor (CSTR) or a fixed bed reactor, more preferably a fixed bed reactor, more preferably a trickle bed reactor.

[0128] Preferably, the stream S3 obtained from (iii) has a reduced total chlorine content compared to SO and S1 of from 90 to 100%, more preferably from 95 to 100%, more preferably from 99 to 100%, more preferably from 99.5 to 100%.

[0129] Preferably, the stream S3 obtained from (iv) has a total chlorine content, determined as described in Example 2.1, in the range of from 0 to 50 wppm (ppm by weight), more preferably from 0 to 30 wppm, more preferably from 0 to 20 wppm, more preferably from 0 to 10 wppm, more preferably from 0 to 5 wppm, more preferably from 0 to 2 wppm.

[0130] Preferably, stream S3 obtained from (iv) has a chloride content, determined as described in Example 2.2, of at most 40 wppm (ppm by weight), preferably in the range of from 0 to 30 wppm, more preferably from 0 to 20 wppm, more preferably from 0 to 1 wppm.

[0131] Preferably, stream S3 obtained from (iii) has a reduced nitrogen content of from 80 to 100%, more preferably from 85 to 100%, more preferably from 90 to 100% compared to S0, S1 and S2.

[0132] Preferably, the stream S3 obtained from (iv), more preferably after removal of dissolved NH3, has a nitrogen content, determined as described in Example 3, in the range of 0 to 200 weight ppm (wppm), more preferably in the range of 0 to 100 wppm, more preferably in the range of 0 to 50 wppm, more preferably in the range of 0 to 10 wppm.

[0133] Preferably, the stream S3 obtained from (iii) has a reduced sulfur content of from 80 to 100%, more preferably from 85 to 100%, more preferably from 90 to 100%, compared to S0, S1 and S2.

[0134] Preferably, the stream S3 obtained from (iv), more preferably after removal of dissolved H2S, has a sulfur content, determined as described in Example 4, in the range of from 0 to 200 weight ppm (wppm), more preferably from 0 to 100 wppm, more preferably from 0 to 50 wppm.

[0135] Preferably, the stream S3 obtained from (iii) comprises one or more organic compounds containing conjugated double bonds in a total amount ranging from 0 to 3 g (I2) / 100 g, more preferably from 0 to 2 g (I2) / 100 g, more preferably from 0 to 1 g (I2) / 100 g, more preferably from 0 to 0.25 g (I2) / 100 g, more preferably from 0 to 0.1 g (I2) / 100 g of the stream S3 obtained from (iv), determined as described in Reference Example 1.

[0136] Preferably, stream S3 has a chlorine content, a nitrogen content, a sulfur content, and a total amount of one or more organic compounds containing conjugated double bonds as defined above.

[0137] Preferably, stream S3 obtained from (iv) is depleted in one or more nitrogen-containing and sulfur-containing compounds compared to S2, preferably before being subjected to (v) as defined below.

[0138] As mentioned in the introduction to the present invention, the polymers contained in the plastic waste may contain oxygen, which is preferably removed in the hydrotreatment step mentioned above.

[0139] (iv) Downstream steps The method of the present invention preferably comprises, after (iii) or (iv) as defined above, (v) one or more of a steam cracking step, a hydrocracking step, distillation, stripping, and aqueous extraction. Further includes:

[0140] Preferably, the process of the present invention is a continuous or semi-continuous process, more preferably a continuous process.

[0141] Preferably, the method of the present invention comprises (i), (ii), (iii), more preferably (i), (ii), (iii) and (iv), more preferably (i), (ii), (iii), (iv) and (v).

[0142] The present invention further relates to a production unit for carrying out the method for refining pyrolysis oil according to the invention, comprising: at least one reaction zone Z1, Z1 comprising a heterogeneous hydrogenation catalyst; - an inlet means for introducing S0 into Z1; - an outlet means for removing S1 from Z1; at least one dehalogenation zone Z2, preferably comprising a heterogeneous adsorbent material or a heterogeneous dehalogenation catalyst; - an inlet means for introducing S1 into Z2; - an outlet means for removing S2 from Z2; wherein Z1 is located upstream of Z2.

[0143] Preferably, the production unit further comprises an extraction zone for removing halides, more preferably comprising one or more halides of N-containing organic compounds, said extraction zone being more preferably located downstream of Z2.

[0144] Preferably, the production unit comprises: at least one reaction zone Z3, Z3 comprising a heterogeneous hydrotreating catalyst; - an entry means for introducing the S2 into the Z3; - an exit means for removing S3 from Z3; and Z2 is located upstream of Z3.

[0145] The present invention further relates to a refined pyrolysis oil obtainable or obtained by a process according to the invention comprising (i), (ii) and (iii) or (i), (ii), (iii) and (iv).

[0146] When the process according to the invention comprises (i), (ii) and (iii), the refined pyrolysis oil preferably has a chlorine content and a total amount of one or more organic compounds containing conjugated double bonds as defined above for stream S2, more preferably a chlorine content, a nitrogen content, a sulphur content and a total amount of one or more organic compounds containing conjugated double bonds as defined above for stream S2.

[0147] When the process according to the invention comprises (i), (ii), (iii) and (iv), the refined pyrolysis oil preferably has a chlorine content, a nitrogen content, a sulfur content and a total amount of one or more organic compounds containing conjugated double bonds as defined above for stream S3.

[0148] Preferably, the refined pyrolysis oil has a total chlorine content, determined as described in Example 2.1, in the range of from 0 to 50 wppm (ppm by weight), more preferably from 0 to 30 wppm, more preferably from 0 to 20 wppm, more preferably from 0 to 10 wppm, more preferably from 0 to 5 wppm, more preferably from 0 to 2 wppm.

[0149] Preferably, the refined pyrolysis oil has a chloride content, determined as described in Example 2.2, of up to 40 wppm (ppm by weight), preferably in the range of 0 to 30 wppm, more preferably 0 to 20 wppm, more preferably 0 to 1 wppm.

[0150] Preferably, the refined pyrolysis oil has a nitrogen content, determined as described in Example 3, in the range of 0 to 200 weight ppm (wppm), more preferably 0 to 100 wppm, more preferably 0 to 50 wppm, more preferably 0 to 10 wppm.

[0151] Preferably, the refined pyrolysis oil has a sulfur content, determined as described in Example 4, in the range of 0 to 200 weight ppm (wppm), more preferably 0 to 100 wppm, more preferably 0 to 50 wppm.

[0152] Preferably, the refined pyrolysis oil contains one or more organic compounds containing conjugated double bonds in a total amount ranging from 0 to 3 g(I2) / 100 g, more preferably from 0 to 2 g(I2) / 100 g, determined as described in Reference Example 1.

[0153] The present invention is further described by the following set of embodiments and combinations of embodiments resulting from dependencies and back references as indicated. In particular, in each instance where a range of embodiments is mentioned, for example, in the context of the term, for example "any one method of embodiment 1 to 4", it is meant that all embodiments within this range are expressly disclosed to those skilled in the art, that is, the wording of this term should be understood by those skilled in the art as being synonymous with "any one method of embodiment 1, 2, 3, and 4". Furthermore, it is expressly noted that the following set of embodiments represents a properly structured part of the general description directed to the preferred aspects of the present invention, and thus properly supports, but does not represent the scope of the claims of the present invention.

[0154] 1. A method for refining pyrolysis oil, comprising: (i) providing a pyrolysis oil-containing stream S0, the pyrolysis oil comprising one or more halogenated organic compounds and one or more organic compounds comprising conjugated double bonds; (ii) subjecting the stream S0 provided in (i) to hydrogenation in at least one reaction zone Z1 containing a heterogeneous hydrogenation catalyst to obtain a stream S1 depleted in one or more organic compounds containing conjugated double bonds compared to S0; (iii) subjecting the stream S1 obtained from (ii) to a dehalogenation in at least one dehalogenation zone Z2 downstream of Z1 to obtain a stream S2 depleted in one or more halogenated organic compounds compared to S1; A method comprising:

[0155] 2. The method of embodiment 1, wherein 95 to 100% by weight, preferably 98 to 100% by weight, more preferably 99 to 100% by weight of S0 consists of pyrolysis oil.

[0156] 3. The method according to embodiment 1 or 2, wherein the pyrolysis oil according to (i) comprises one or more organic compounds containing conjugated double bonds in a total amount ranging from 0.1 to 75 g(I2) / 100 g, preferably from 0.4 to 60 g(I2) / 100 g, more preferably from 1 to 30 g(I2) / 100 g of the pyrolysis oil, determined as described in Reference Example 1.

[0157] 4. One or more organic compounds containing conjugated double bonds are represented by the formula (I) R 1 R 2 C 1 =C 2 R 3 -C 3 R 4 =X(I) (wherein =X is =O, =S, =NR 5 , or =C 4 R 6 R 7 and preferably =C 4 R 6 R 7 is) 4. The method of any one of the preceding claims, comprising one or more organic compounds according to

[0158] 5.R 1 , R 2 , R 3 , R 4 , R 5 are each independently H, an alkyl having 1 to 6 carbon atoms, an alkenyl having 1 to 6 carbon atoms, or an aryl having 5 to 10 carbon atoms, more preferably H; R 6 and R 7 are, independently of each other, H, alkyl having 1 to 6 carbon atoms, alkenyl having 1 to 6 carbon atoms, or aryl having 5 to 10 carbon atoms, more preferably H; or R 4 and R 6 Or R 4 and R 7 are concatenated together, so C 3 =C 45. The method of embodiment 4, wherein together with

[0159] 6. The method of embodiment 5, wherein the one or more organic compounds according to formula (I) include one or more of butadiene, isoprene, dienes having 5 or 6 carbon atoms, styrene, methylstyrene, indene, substituted styrene, substituted indene, and 3-methyl-2-butenal, more preferably one or more of butadiene, isoprene, dienes having 5 or 6 carbon atoms, styrene, methylstyrene, indene, and 3-methyl-2-butenal.

[0160] 7. The method of embodiment 6, wherein the one or more organic compounds according to formula (I) comprises styrene.

[0161] 8. The method of any one of the preceding claims, wherein the one or more halogenated organic compounds comprise one or more of mono-, oligo-, or poly-halogenated aromatic compounds, alkyl halides, and alkenyl halides.

[0162] 9. The pyrolysis oil according to (i) has a total chlorine content, determined as described in Reference Example 2.1, in the range of 30 to 3,000 wppm (ppm by weight), preferably 30 to 500 wppm, more preferably 30 to 200 wppm; The method according to any one of the preceding claims, wherein the pyrolysis oil according to (i) has a chloride content, determined as described in Reference Example 2.2, of at most 40 wppm, more preferably in the range of 0 to 30 wppm.

[0163] 10. The method according to any one of the preceding embodiments, wherein the pyrolysis oil according to (i) has a nitrogen content, determined as described in Example 3, ranging from 50 to 20,000 wppm (ppm by weight), preferably from 50 to 5,000 wppm, more preferably from 100 to 4,000 wppm.

[0164] 11. The method according to any one of the preceding embodiments, wherein the pyrolysis oil from (i) has a sulfur content, determined as described in Example 4, ranging from 50 to 30,000 ppm by weight (wppm), preferably from 50 to 5,000 wppm, more preferably from 100 to 3,000 wppm.

[0165] 12. The method of any one of the preceding embodiments, wherein the pyrolysis oil is obtained from plastic waste.

[0166] 13. The method of any one of the preceding claims, wherein the flow S0 is a liquid flow.

[0167] 14. The process according to any one of the preceding embodiments, wherein the stream S0 subjected to hydrogenation in (ii) has a temperature in the range of from 60 to 250°C, preferably from 80 to 220°C, more preferably from 100 to 200°C.

[0168] 15. The method according to any one of the preceding embodiments, wherein the heterogeneous hydrogenation catalyst according to (ii) comprises an element from groups 8 to 12, preferably from groups 8 to 10, more preferably from groups 9 and 10 of the Periodic Table of the Elements, preferably an element selected from the group consisting of Ni, Pd and Co, more preferably an element selected from the group consisting of Ni and Pd.

[0169] 16. The process according to embodiment 15, wherein the heterogeneous hydrogenation catalyst according to (ii) further comprises a support material for said elements of groups 8 to 12 of the periodic table of the elements, the support material being preferably selected from the group consisting of oxide materials and carbon, the oxide material being preferably one or more of alumina, silica, magnesia, zirconia, titania, zeolitic materials, silica-alumina phosphate (SAPO) materials, zinc oxide, sodium oxide, mixed silica-alumina, zeolites and calcium oxide, more preferably alumina.

[0170] 17. The method according to embodiment 15 or 16, wherein the heterogeneous hydrogenation catalyst according to (ii) preferably contains Ni in an amount ranging from 0.5 to 70 wt.-%, more preferably from 0.75 to 45 wt.-%, more preferably from 1 to 20 wt.-%, calculated as NiO, based on the total weight of the hydrogenation catalyst.

[0171] 18. The heterogeneous hydrogenation catalyst used in (ii) further comprises an element of group 6 of the periodic table of the elements, the element of group 6 being preferably one or more of Mo and W, more preferably Mo; 18. The method according to any one of embodiments 15 to 17, wherein the hydrogenation catalyst preferably comprises from 1 to 40 wt.%, more preferably from 2 to 35 wt.%, more preferably from 3 to 30 wt.%, of said elements of group 6, based on the total weight of the hydrogenation catalyst.

[0172] 19. The method according to embodiment 17 or 18, wherein the heterogeneous hydrogenation catalyst according to (ii) comprises Ni and Mo supported on a support material, preferably a support material as defined in embodiment 16, and the hydrogenation catalyst comprises Ni and Mo, preferably supported on alumina.

[0173] 20. The method according to embodiment 15 or 16, wherein the heterogeneous hydrogenation catalyst according to (ii) preferably contains Pd in ​​an amount ranging from 0.01 to 5 wt.-%, 0.1 to 1 wt.-%, more preferably 0.15 to 0.8 wt.-%, calculated as elemental Pd, based on the total weight of the catalyst.

[0174] 21. The method according to embodiment 20, wherein the heterogeneous hydrogenation catalyst according to (ii) further comprises a promoter, the promoter being preferably one or more of elements from groups 10 and 11 of the periodic table of the elements, preferably one or more of Cu, Au, Ag and Pt, more preferably one or more of Ag and Pt, more preferably Ag.

[0175] 22. The method of embodiment 21, wherein the atomic ratio of the element from groups 8 to 12 of the periodic table, preferably Pd, to the promoter is in the range of 0.1:1 to 10:1, preferably 2:1 to 7:1, more preferably 2.5:1 to 6:1.

[0176] 23. The process according to any one of embodiments 20 to 22, wherein the heterogeneous hydrogenation catalyst according to (ii) comprises Pd supported on a support material, preferably a support material as defined in embodiment 16, the support material being preferably alumina or carbon, more preferably alumina.

[0177] 24. The method according to any one of the preceding embodiments, wherein the heterogeneous hydrogenation catalyst according to (ii) is in the form of extrudates, pellets, rings, spherical particles or spheres, preferably spherical particles or extrudates.

[0178] 25.(ii) is (ii.1) introducing a gas flow G0 into Z1, the gas flow comprising H2; (ii.2) introducing a flow S0 into Z1; (ii.3) contacting S0 with G0 and a heterogeneous hydrogenation catalyst contained in Z1 to obtain a stream S1 depleted in one or more organic compounds containing conjugated double bonds compared to S0; (ii.4) removing S1 from Z1; (ii.5) optionally removing a gas flow G1 from Z1, G1 comprising H2; 25. The method of any one of the preceding claims, comprising:

[0179] 26. The method of embodiment 25, wherein the gas stream G0 has a temperature in the range of 100 to 250°C, preferably 120 to 220°C, more preferably 140 to 200°C.

[0180] 27. The method according to embodiment 25 or 26, wherein the gas stream G0 is introduced at a pressure in the range of from 10 to 100 bar (abs), preferably from 15 to 90 bar (abs), more preferably from 20 to 80 bar (abs), more preferably from 20 to 55 bar (abs).

[0181] 28. The method according to any one of embodiments 25 to 27, wherein 70 to 100% by weight, preferably 80 to 100% by weight, more preferably 90 to 100% by weight of the gas stream G0 consists of H2.

[0182] 29. The method according to any one of embodiments 25 to 28, wherein according to (ii.1), G0 is introduced into Z1 continuously or semi-continuously, preferably continuously, and according to (ii.2), S0 is introduced into Z1 semi-continuously or continuously, preferably continuously.

[0183] 30. The method of embodiment 29, wherein prior to introducing S0 into Z1 according to (ii.2), G0 is introduced into Z1 according to (ii.1) for a period of time Δt.

[0184] 31. The method according to embodiment 30, wherein G0 is contacted with the heterogeneous hydrogenation catalyst contained in Z1 for a period of Δt, and G0 has a temperature in the range of from 50 to 250° C., preferably from 120 to 220° C., more preferably from 140 to 200° C.

[0185] 32. At Z1, the liquid hourly space velocity (LHSV) is between 0.2 and 10 m 3 / (m 3 h), preferably in the range of 0.3 to 5 m 3 / (m 3 h), more preferably in the range of 0.5 to 2 m 3 / (m 3 h), and the LHSV is in the range of Z1(m 3 S0 to Z1 (m2) per volume of heterogeneous hydrogenation catalyst 3 The method according to any one of embodiments 25 to 31, wherein the volumetric flow rate is defined as the volumetric flow rate in s / h.

[0186] 33. The method of any one of the preceding embodiments, wherein reaction zone Z1 is comprised in a continuous stirred tank reactor (CSTR) or a fixed bed reactor, preferably a fixed bed reactor, and the fixed bed reactor is preferably a trickle bed reactor.

[0187] 34. The method according to any one of the preceding claims, wherein two or more reaction zones Z1 arranged in series and / or parallel are used according to (ii), or one single reaction zone Z1 is used according to (ii), preferably one single reaction zone Z1 is used according to (ii).

[0188] 35. The method according to any one of the preceding embodiments, preferably any embodiment as long as it depends on embodiment 3, wherein the stream S1 obtained from (ii) and subjected to dehalogenation in (iii) comprises one or more organic compounds containing conjugated double bonds in a total amount ranging from 0 to 3 g (I2) / 100 g, preferably from 0 to 2 g (I2) / 100 g, more preferably from 0 to 1 g (I2) / 100 g, more preferably from 0 to 0.25 g (I2) / 100 g, more preferably from 0 to 0.1 g (I2) / 100 g of stream S1, determined as described in Reference Example 1.

[0189] 36. The process according to any one of the preceding embodiments, wherein the stream S1 dehalogenated in (iii) has a temperature in the range of from 150 to 450°C, preferably from 200 to 400°C, more preferably from 250 to 350°C.

[0190] 37. The method according to any one of the preceding embodiments, wherein the dehalogenation zone Z2 according to (iii) comprises an adsorption zone, preferably an adsorption zone, preferably comprising a heterogeneous adsorption material suitable for adsorbing the halides contained in at least one of the one or more halogenated organic compounds, preferably all of the one or more halogenated organic compounds.

[0191] 38. The heterogeneous adsorbent material according to (iii) comprises one or more of a carbon-containing adsorbent material and an aluminium-containing adsorbent material, preferably an aluminium-containing adsorbent material; The carbon-containing adsorbent material is preferably a carbon-containing molecular sieve, more preferably activated carbon; The aluminum-containing adsorbent material is preferably alumina, an aluminum-containing molecular sieve, a silicoaluminophosphate, a silica-alumina hydrate or a hydrotalcite; the aluminum-containing molecular sieve is preferably an alumina, an aluminosilicate, preferably having a molar ratio of Si:Al, calculated as SiO2:Al2O3, in the range of from 2:1 to 10:1, more preferably from 2:1 to 4:1; the silica-alumina hydrate preferably has a weight ratio of Al2O3:SiO2 ranging from 1:1 to 10:1, more preferably from 1:1 to 2:1; the hydrotalcite is preferably an aluminium and magnesium containing hydrotalcite, more preferably an aluminium-magnesium hydroxycarbonate, preferably having a MgO:Al2O3 weight ratio in the range of 63:37 to 70:30; The heterogeneous adsorbent material more preferably comprises hydrotalcite; 38. The method of embodiment 37, wherein the heterogeneous adsorbent material according to (iii) preferably comprises elements of groups 1, 2, 11 and 12.

[0192] 39. The method according to any one of the preceding embodiments, wherein the heterogeneous adsorbent material according to (iii) comprises particles characterized by a particle size distribution having a D50 value in the range of 1 to 6,500 micrometers, preferably 2 to 2,000 micrometers, more preferably 8 to 500 micrometers, more preferably 10 to 50 micrometers or 3 to 9 micrometers, the D50 particle size being determined as described in Reference Example 5.

[0193] 40. The method according to any one of the preceding embodiments, wherein the heterogeneous adsorbent material according to (iii) has an average pore volume in the range of 0.1 to 5 ml / g, preferably in the range of 0.15 to 2 ml / g, the average pore volume being determined as described in Reference Example 6.

[0194] 41.The heterogeneous adsorbent material according to (iii) is applied to a substrate of 50 to 1,000 m 2 / g, preferably in the range of 100 to 900 m 2 / g, more preferably in the range of 150 to 600 m 2 The method of any one of the preceding claims, wherein the BET specific surface area is in the range of 0.1 to 1.0 μm / g, and the BET specific surface area is determined as described in Reference Example 7.

[0195] 42.(iii) is (iii.1) introducing a gas stream G1 into a preferably adsorption zone Z2, preferably the gas stream comprising one or more of hydrogen and nitrogen, more preferably hydrogen; (iii.2) (ii) introducing the flow S1 obtained in (ii) into Z2; (iii.3) contacting S1 with a heterogeneous adsorbent material contained in G1 and Z2 to obtain a stream S2 depleted in one or more halogenated organic compounds compared to S1; (iii.4) removing S2 from Z2; 42. The method of any one of the preceding embodiments, comprising:

[0196] 43. The method of embodiment 42, wherein the gas stream G1 has a temperature in the range of 250 to 500°C, preferably in the range of 300 to 400°C.

[0197] 44. The method according to embodiment 42 or 43, wherein the gas stream G1 is introduced at a pressure in the range of 1 to 100 bar (abs), preferably in the range of 5 to 80 bar (abs), more preferably in the range of 10 to 50 bar (abs).

[0198] 45. At Z2, the liquid hourly space velocity (LHSV) is between 0.2 and 10 h -1 in the range of 0.3 to 5 h -1 in the range of 0.5 to 2 h -1 45. The method of any one of embodiments 42 to 44, wherein the range is

[0199] 46. ​​90 to 100% by weight, preferably 95 to 100% by weight, more preferably 98 to 100% by weight, of the gas stream G1 consists of H2, or 46. ​​The method according to any one of embodiments 42 to 45, wherein 90 to 100% by weight, preferably 95 to 100% by weight, more preferably 98 to 100% by weight of the gas stream G1 consists of nitrogen.

[0200] 47. According to (iii.1), G1 is introduced continuously or semi-continuously, preferably continuously, into Z2, and according to (iii.2), S1 is introduced continuously or semi-continuously, preferably continuously, into Z2, The method according to any one of embodiments 42 to 46, wherein the adsorption zone Z2 is preferably comprised in a continuous stirred tank reactor (CSTR) or a fixed bed reactor, preferably a fixed bed reactor, more preferably a trickle bed reactor, the reactor preferably comprising an adsorption bed comprising a heterogeneous adsorption material.

[0201] 48. The method according to any one of the preceding embodiments, wherein two or more reaction zones Z2 arranged in series and / or in parallel are used according to (iii), preferably one single reaction zone Z2 is used according to (iii).

[0202] 49. The stream S2 obtained from (iii) has a total chlorine content, determined as described in Example 2.1, in the range of from 0 to 200 wppm (ppm by weight), preferably from 0 to 160 wppm, more preferably from 0 to 130 wppm, more preferably from 0 to 120 wppm; The stream S2 obtained from (iii) has a chloride content, determined as described in Example 2.2, of at most 40 wppm (ppm by weight), preferably between 0 and 30 wppm, more preferably between 0 and 20 wppm, more preferably between 0 and 1 wppm, The method according to any one of the preceding embodiments.

[0203] 50. The method according to any one of embodiments 1 to 49, preferably embodiment 3, insofar as it depends on any one of embodiments 1 to 49, preferably embodiment 3, wherein the stream S2 obtained from (iii) comprises one or more organic compounds comprising conjugated double bonds in a total amount ranging from 0 to 3 g (I2) / 100 g, preferably from 0 to 2 g (I2) / 100 g, more preferably from 0 to 1 g (I2) / 100 g, more preferably from 0 to 0.25 g (I2) / 100 g, more preferably from 0 to 0.1 g (I2) / 100 g of stream S2, determined as described in Reference Example 1.

[0204] 51. The stream S2 obtained from (iii) has a nitrogen content, determined as described in Example 3, in the range of 50 to 20,000 ppm by weight, preferably 50 to 5,000 ppm by weight, more preferably 100 to 4,000 ppm by weight; The method of any one of the preceding embodiments, wherein the stream S2 obtained from (iii) has a sulfur content, determined as described in Example 4, in the range of 50 to 30,000 ppm by weight (wppm), preferably 50 to 5,000 wppm, more preferably 100 to 3,000 wppm.

[0205] 52. The method according to any one of the preceding embodiments, wherein the dehalogenation zone Z2 according to (iii) comprises a catalytic zone, preferably a catalytic zone, preferably comprising a heterogeneous dehalogenation catalyst, said catalyst comprising one or more catalytically active elements from groups 8 to 12 of the periodic system of the elements.

[0206] 53. The process according to any one of the preceding embodiments, in which the stream S2 obtained from (iii), before being subjected to hydrotreatment according to (iv) as defined in embodiment 54, is subjected to extraction, preferably using an aqueous extraction medium, to obtain a stream S2 depleted of one or more dissolved halides contained in S2 obtained from the dehalogenation zone Z2, said halides preferably comprising one or more halides of N-containing organic compounds.

[0207] 54. (iv) (iii) subjecting the stream S2 obtained from (iii) to hydrotreating in at least one reaction zone Z3 downstream of Z2, Z3 comprising a heterogeneous hydrotreating catalyst, to obtain a stream S3. Further comprising: the stream S2 subjected to (iv) has a temperature in the range of from 150 to 400° C., preferably in the range of from 200 to 375° C., more preferably in the range of from 250 to 350° C., The method according to any one of embodiments 1 to 53.

[0208] 55. The heterogeneous hydrotreating catalyst used in (iv) comprises an element selected from the group consisting of elements of groups 8 to 10, preferably groups 9 and 10, of the Periodic Table of the Elements, preferably Ni and Co, the hydrotreating catalyst more preferably comprising Ni; The heterogeneous hydrotreating catalyst according to (iv) more preferably comprises an amount of Ni in the range of 0.5 to 10 wt.-%, more preferably in the range of 1 to 6 wt.-%, calculated as NiO, based on the weight of the hydrotreating catalyst; The method of embodiment 54.

[0209] 56. The heterogeneous hydrotreating catalyst according to (iv) further comprises a support for an element of groups 8 to 10 of the periodic table of the elements, the support being preferably an oxide material; The oxide material is preferably one or more of alumina, silica, magnesia, zirconia, zinc oxide, calcium oxide, mixed silica-alumina, zeolite, Mo-doped alumina and titania, more preferably alumina, zeolite and silica-alumina, more preferably alumina; The method of embodiment 55.

[0210] 57. The heterogeneous hydrotreating catalyst according to (iv) further comprises an element of group 6 of the periodic table of the elements, the element of group 6 being preferably one or more of Mo and W; The hydrotreating catalyst preferably comprises from 1 to 40% by weight, more preferably from 3 to 30% by weight, of an oxide of said element of group 6, preferably Mo oxide or W oxide, based on the weight of said hydrotreating catalyst; The method of embodiment 55 or 56.

[0211] 58. The method of embodiment 57, wherein the heterogeneous hydrotreating catalyst according to (iv) comprises Ni and Mo on a support, preferably a support as defined in embodiment 53, and the hydrotreating catalyst preferably comprises Ni and Mo on alumina.

[0212] 59.(iv) (iv.1) introducing a gas stream G2 into Z3, G2 comprising H2; (iv. 2) (iii) introducing the stream S2 into Z3; (iv. 3) contacting S2 with G2 and a heterogeneous hydrotreating catalyst contained in Z3 to obtain stream S3; (iv. 4) removing S3 obtained in (iv. 3) from Z3; 59. The method of any one of embodiments 53 to 58, comprising:

[0213] 60. The method of embodiment 59, wherein gas stream G2 has a temperature in the range of 250 to 550°C, preferably in the range of 300 to 450°C, more preferably in the range of 325 to 400°C.

[0214] 61. The method according to embodiment 59 or 60, wherein the gas stream G2 is introduced at a pressure in the range of 20 to 150 bar (abs), preferably in the range of 30 to 90 bar (abs), more preferably in the range of 40 to 80 bar (abs), more preferably in the range of 45 to 60 bar (abs).

[0215] 62. At Z3, the liquid hourly space velocity (LHSV) is between 0.1 and 10 h -1 in the range of 0.1 to 5 h -1 More preferably, in the range of 0.2 to 2 h -1 62. The method of any one of embodiments 59 to 61, in the range of

[0216] 63. The method according to any one of embodiments 59 to 62, wherein 50 to 100% by weight, preferably 70 to 100% by weight, more preferably 90 to 100% by weight, of the gas stream G2 consists of H2.

[0217] 64. The method according to any one of embodiments 59 to 63, wherein G2 is introduced into Z3 continuously or semi-continuously, preferably continuously, according to (iv.1).

[0218] 65. The method according to any one of embodiments 59 to 64, wherein S2 is introduced into Z3 continuously or semi-continuously, preferably continuously, according to (iv.2).

[0219] 66. The method of any one of the preceding embodiments, wherein reaction zone Z3 is preferably comprised in a reactor comprising n continuously connected catalyst beds B(i), i=1..., n, n>2, wherein catalyst beds B(i) comprise heterogeneous hydrotreating catalysts, preferably 2<n<10, more preferably 2<n<5, and wherein B(1) is the most upstream catalyst bed and B(n) is the most downstream catalyst bed.

[0220] 67.(iv) (iv.1') introducing a gas flow G2 into Z3, G2 comprising H2; (iv.2') (iii) introducing the flow S2 into Z3; (iv.3') n successive process steps P(i), i = 1...n, In P(1), - introducing the gas stream G2 into the catalyst bed B(1) and contacting it with the heterogeneous hydrotreating catalyst of the stream S2 obtained from (iii) and B(1) to form the stream S P A step of obtaining (1); For each P(i), for i=2...n-1, A gas stream F(i-1) containing H2 is introduced into the catalyst bed B(i) and S P (i-1) and the heterogeneous hydrotreating catalyst in B(i) to form a stream S P obtaining (i); -B(i) to S P removing (i); In P(n), - gas stream F(n-1) is introduced into catalyst bed B(n) and S P with a heterogeneous hydrotreating catalyst in B(n-1) and B(n) to obtain a gas stream S3; (iv.4') removing S3 obtained in (iv.3') from Z3; 67. The method of embodiment 66, comprising:

[0221] 68. The method of embodiment 67, wherein the gas stream G2 has a temperature in the range of 250 to 550°C, preferably in the range of 300 to 450°C, more preferably in the range of 325 to 400°C.

[0222] 69. The method according to embodiment 67 or 68, wherein the gas stream G2 is introduced at a pressure in the range of 20 to 150 bar (abs), preferably in the range of 30 to 90 bar (abs), more preferably in the range of 40 to 80 bar (abs), more preferably in the range of 45 to 60 bar (abs).

[0223] 70. The method according to any one of embodiments 67 to 69, wherein 50 to 100% by weight, preferably 70 to 100% by weight, more preferably 90 to 100% by weight, of the gas stream G2 consists of H2.

[0224] 71. At Z3, the liquid hourly space velocity (LHSV) is between 0.1 and 10 h -1 in the range of 0.1 to 5 h -1 More preferably, in the range of 0.2 to 2 h -1 The method of any one of embodiments 67 to 70, wherein the range is

[0225] 72. The method according to any one of embodiments 67 to 71, wherein G2 is introduced into Z3 continuously or semi-continuously, preferably continuously, according to (iv. 1').

[0226] 73. The method according to any one of embodiments 67 to 72, wherein S2 is introduced into Z3 continuously or semi-continuously, preferably continuously, according to (iv. 2').

[0227] 74. The method according to any one of embodiments 67 to 73, wherein 50 to 100% by weight, preferably 70 to 100% by weight, more preferably 90 to 100% by weight, of the gas stream F(i) consists of H2.

[0228] 75. The method according to embodiment 74, wherein the gas stream F(i) is introduced at a pressure in the range of 20 to 150 bar (abs), preferably in the range of 30 to 90 bar (abs), more preferably in the range of 40 to 80 bar (abs), more preferably in the range of 45 to 60 bar (abs).

[0229] 76. The method of any one of embodiments 67 to 75, wherein the n series-coupled catalyst beds B(i) are fixed catalyst beds.

[0230] 77. The method of any one of the preceding embodiments, wherein reaction zone Z3 is comprised in a continuous stirred tank reactor (CSTR) or a fixed bed reactor, preferably a fixed bed reactor, more preferably a trickle bed reactor.

[0231] 78. The stream S3 obtained from (iv) has a total chlorine content, determined as described in Example 2.1, in the range of from 0 to 50 wppm (ppm by weight), preferably from 0 to 30 wppm, more preferably from 0 to 20 wppm, more preferably from 0 to 10 wppm, more preferably from 0 to 5 wppm, more preferably from 0 to 2 wppm; the stream S3 obtained from (iv) has a chloride content, determined as described in Example 2.2, of at most 40 wppm (ppm by weight), preferably in the range of from 0 to 30 wppm, more preferably from 0 to 20 wppm, more preferably from 0 to 1 wppm, The method according to any one of embodiments 53 to 77.

[0232] 79. The method of any one of embodiments 53 to 78, wherein the stream S3 obtained from (iv) has a nitrogen content, preferably after removal of dissolved NH3, determined as described in Reference Example 3, in the range of 0 to 200 ppm by weight (wppm), preferably in the range of 0 to 100 wppm, more preferably in the range of 0 to 50 wppm, more preferably in the range of 0 to 10 wppm.

[0233] 80. The method of any one of embodiments 53 to 79, wherein the stream S3 obtained from (iv) has a sulfur content, preferably after removal of dissolved H2S, determined as described in Example 4, in the range of 0 to 200 ppm by weight (wppm), preferably 0 to 100 wppm, more preferably 0 to 50 wppm.

[0234] 81. The method according to any one of embodiments 1 to 80, preferably any embodiment as long as it depends on embodiment 3, wherein the stream S3 obtained from (iii) comprises one or more organic compounds comprising conjugated double bonds in a total amount ranging from 0 to 3 g (I2) / 100 g, preferably from 0 to 2 g (I2) / 100 g, more preferably from 0 to 1 g (I2) / 100 g, more preferably from 0 to 0.25 g (I2) / 100 g, more preferably from 0 to 0.1 g (I2) / 100 g of the stream S3 obtained from (iv), determined as described in Reference Example 1.

[0235] 82. After (iii) or (iv) as defined in any one of embodiments 53 to 81, (v) one or more of a steam cracking step, a hydrocracking step, distillation, stripping, and aqueous extraction. 82. The method of any one of the preceding embodiments, further comprising:

[0236] 83. The method according to any one of the preceding embodiments, which is a continuous or semi-continuous process, preferably a continuous process.

[0237] 84. The method according to any one of the preceding embodiments, comprising (i), (ii), (iii), preferably (i), (ii), (iii) and (iv), more preferably (i), (ii), (iii), (iv) and (v).

[0238] 85. A production unit for carrying out the method for refining pyrolysis oil according to any one of embodiments 1 to 84, comprising: at least one reaction zone Z1, Z1 comprising a heterogeneous hydrogenation catalyst; - an inlet means for introducing S0 into Z1; - an outlet means for removing S1 from Z1; at least one dehalogenation zone Z2, preferably comprising a heterogeneous adsorbent material or a heterogeneous dehalogenation catalyst; - an inlet means for introducing S1 into Z2; - an outlet means for removing S2 from Z2; wherein Z1 is located upstream of Z2; an extraction zone for removing halides, preferably comprising one or more halides of N-containing organic compounds, preferably located downstream of Z2; The manufacturing unit further comprises:

[0239] 86. at least one reaction zone Z3, Z3 comprising a heterogeneous hydrotreating catalyst; - an entry means for introducing the S2 into the Z3; - an exit means for removing S3 from Z3; 86. The manufacturing unit of embodiment 85, further comprising:

[0240] 87. A refined pyrolysis oil, obtainable or obtained by the method according to any one of embodiments 1 to 53 or the method according to any one of embodiments 54 to 81. [Brief description of the drawings]

[0241] [Figure 1] FIG. 1 is an XRD analysis of the solid obtained in Comparative Example 1 contained in a tube. Crystalline NH4Cl reflections are marked with an asterisk. [Figure 2a] 1 is a photograph of the corundum in the preheat zone of Comparative Example 2 (black powder). [Figure 2b] FIG. 1 is a photograph of the corundum in the preheat zone of Example 1 (lighter powder than a). DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0242] Working Example Reference Example 1 Measurement of the total amount of one or more organic compounds containing conjugated double bonds The diene content is determined by UOP326-17. In this procedure, the diene is reacted with maleic anhydride (MA) and the consumption of MA is determined (by titration of the remaining MA). It can be expressed as g(I2) / 100 g(sample) or g(MA) / 100 g(sample). The units are interconverted by multiplying the MA value (MAV) by the factor 2.59 to obtain a value expressed in g(I2) / 100 g(sample) corresponding to the molar weight of I2 and MA. Thus, 1% by weight of styrene or 0.52% by weight of butadiene corresponds to 0.94 g(MA) / 100 g or 2.43 g(I2) / 100 g.

[0243] Reference Example 2.1 Measurement of total chlorine content (wppm) The samples are filtered through a 0.45 μm syringe filter before analysis. The chlorine content is determined by combustion of each sample at 1050° C. The resulting combustion gases, i.e. hydrogen chloride, are led to a cell where the coulometric titration is performed.

[0244] Reference Example 2.2 Measurement of chloride content (wppm) The samples are filtered through a 0.45 μm syringe filter before analysis. The chloride content is determined by ion chromatography. Equipment: Ion Chromatograph 850 Professional (Metrohm) (precolumn: Metrosep A Supp4 / 5S-Guard and analytical column: Metrosep A Supp 5 250 / 4; flow rate: 0.7 mL / min; column temperature: 30 °C; detector temperature: 40 °C; injection volume: 25 μL; suppressor MSM HC rotor A). As eluents: 3.2 mmol / L Na2CO3; 1.0 mmol / L NaHCO3 and as inhibitor regenerant: 50 mmol / L sulfuric acid were used.

[0245] Sample preparation: 0.2 g to 0.4 g of sample was weighed and dissolved in 10 mL of toluene. For analyte extraction, 10 mL of deionized water was added. After centrifugation, the aqueous phase was extracted and analyzed. Recovery was confirmed by adding 20 μg / L chloride standard solution (corresponding to the limit of 1 mg / kg chloride in the sample) to samples with concentrations below the method limit.

[0246] Reference Example 3 Measurement of N content (wppm) Nitrogen content is determined by combustion of each sample at 1000°C. NO contained in the resulting combustion gases reacts with ozone to form NO2*. Relaxation of excited nitrogen species is detected by a chemiluminescence detector according to ASTM D4629(N). The calibration range is 0.5 wppm to 50 wppm. Higher concentration samples are diluted with xylene to the calibration range.

[0247] Reference Example 4 Measurement of S content (wppm) The sulfur content is determined by combustion of each sample at 1000°C.

[0248] The sulfur dioxide contained in the resulting combustion gases is excited by UV (ultraviolet) light. The light emitted during relaxation is detected by a UV fluorescence detector according to ASTM D5453(S). The calibration range is 0.5 wppm to 50 wppm. Higher concentration samples are diluted with xylene to the calibration range.

[0249] Reference example 5 Particle size (D50) The D50 particle size was determined by optical methods or by air sieve, for example by different instruments, namely a Cilas Granulometer 1064 supplied by Quantachrome, a Malvern Mastersizer or a Luftstrahlsieb (air sieve) supplied by Alpine.

[0250] Reference Example 6 Determination of average pore volume Pore ​​volumes can be derived from BET measurements (for micro- and mesopores) or alternatively Hg porosimetry (for macropores). The Determination of Pore Volume and Area Distributions in Porous Substances. I. Computations from Nitrogen Isotherms JACS 1951 (73) 373-380 EP Barret, LG Joyner, PP Halenda.

[0251] Reference Example 7 Determination of BET specific surface area The BET surface area of ​​the adsorbent material is measured using instruments supplied by Quantachrome (Nova series) or Micromeritics (Gemini series). The method involves low temperature adsorption of nitrogen in the BET region of the adsorption isotherm.

[0252] Reference Example 8 Determination of styrene content GC method using a non-polar 100% dimethylpolysiloxane phase column and FID detector. Final column and inlet temperatures were 330°C and 320°C, respectively. The integrated area signal of styrene is the ratio of all integrated peaks multiplied by 100% to give the area %. Area % correlates closely to weight %.

[0253] Reference Example 9 Determination of Total Acid Number (TAN) Total acid number was determined by titration with KOH according to ASTM D3242.

[0254] Example 10 Reactor charge and test setup All reaction steps of the examples were carried out in a reactor with an internal diameter of 10 mm and operated in trickle bed mode (downward flow). The reactor (80 cm long) is loaded from the bottom with corundum (WSK F46; commercially available corundum) so that the bottom 25 cm is filled with inert corundum (cooling zone). On top of this, a catalyst or adsorbent bed of 30 cm length is placed from 25 to 55 cm, in this zone the reaction temperature is maintained. In the case of shaped catalysts as P-doped NiMo catalyst and E-157 SDU catalyst, the voids of the catalyst bed are also filled with corundum (WSK F46; commercially available corundum). On top of the catalyst, respectively, an adsorbent bed corundum (WSK F46; commercially available corundum) is filled from 55 to 80 cm. In this corundum zone the feed is preheated to the reaction temperature, while in the lower corundum filled zone the product stream is cooled from the reactor temperature to the microheating temperature. EXAMPLES

[0255] Example 1: Method for refining pyrolysis oil according to the present invention A feed stream S0 containing a pyrolysis oil having an MAV of 9.01 g(I2) / 100 g, a styrene content of 6.1 area % determined by GC, a total chlorine content of 560 wppm, a chloride content of 1 wppm, a nitrogen content of about 3260 wppm, a sulfur content of about 2630 wppm, a total acid number (TAN) of 3.69 mg (KOH / g(feed)) and a density of 0.8653 g / ml was subjected to hydrogenation at a temperature of 50 bar and 195°C in a reactor containing an activated Pd catalyst (Catalyst E-157 SDU 1 / 8": 0.7 wt% Pd on 1 / 8" alumina beads commercially available from BASF) with H2. The Pd catalyst was activated in hydrogen flow at ambient pressure with GHSV = 1000 / h while heating to 195°C with a gradient of 0.5 K / min. The hydrogenation was continued for 12 h at 195°C. After 1 h, the GHSV was reduced to 500 / h, the pressure was increased to 50 bar within 1 h, and after a 2 h hold, the addition of S0 was started at LHSV = 1 / h. The resulting feed stream S1 had a MAV reduction of about 80% to 1.75 g(I2) / 100 g, a styrene content reduction to 1.1 area % (>80% conversion), and the N and S contents were unchanged compared to S0. Also, the chlorine content was essentially unchanged (see Table 1).

[0256] [Table 1]

[0257] Stream S1 was then subjected to dechlorination in a reactor containing Cl sorbent (hydrotalcite: aluminum-magnesium hydroxycarbonate powder with a weight ratio of MgO:Al2O3 of 70:30) at 350 °C and 50 bar pressure in the presence of H2. Before use, the sorbent was pressed, then crushed and sieved to an average particle size of 500-1000 micrometers. It was further calcined at 450 °C for 5 h in air and equilibrated overnight in ambient air. Before placing S1 in the reactor, the obtained Cl sorbent was dried at 100 °C and 200 °C in nitrogen at ambient pressure with a gas hourly space velocity (GHSV) = 2000 / h for 1 h each, with a temperature increase of 1 K / min. At 200 °C, the gas was switched from N2 to H2 and the pressure was increased to 50 bar within 1 h. After pressure was reached, the GHSV was reduced to 475 / h and the reactor was heated at 1 K / min to 350°C. Once 350°C was reached, S1 was introduced into the reactor at a liquid hourly space velocity (LHSV) = 0.95 / h. The resulting product stream was analyzed as shown in Table 2.1 and showed a reduction in the total chlorine content (approximately 90% reduction at the start of operation).

[0258] [Table 2]

[0259] Intermediate products (S2) within the course of the reaction were combined to form feed S2.

[0260] Stream S2 was further washed with an equal volume of water and analyzed (see Table 2.2). The N, S content was unchanged compared to S1.

[0261] [Table 3]

[0262] Further, the (washed) stream S2 was subjected to hydrotreatment in a reactor containing an activated P-doped NiMo catalyst supported on alumina (4.75 wt.% NiO, 19.57 wt.% MoO3, 2.89 wt.% P2O5 and 72.79% of the support Al2O3 respectively; prepared according to US Pat. No. 4,409,131) in the presence of 50 bar H2 at temperatures ranging from 350 to 395 °C. The P-doped NiMo catalyst was activated by drying by heating at 1 K / min with N2 at ambient pressure and GHSV=2000 / h and left at 200 °C for 2 h. After that, the temperature was reduced to 135 °C and the atmosphere was switched to H2 for catalyst activation. After 1 h, the pressure was increased to 50 bar within 1 h. After another 1 h, the injection of the sulfide feed was started at LHSV=2 / h and the GHSV was adjusted to 1000 / h. The sulfide feed consisted of a hydrocarbon fluid (a commercial mixture with a boiling range of 176-209 °C, e.g. Varsol™ 60) with the addition of 2 wt.% DMDS (dimethyl disulfide). After 2 h, the temperature was further increased to 350 °C at 0.25 K / min. The temperature was then kept constant for 1 h, the LHSV was reduced to 1 / h and the GHSV was reduced to 500 / h, after which the addition of S2 was started in the reactor at LHSV=1 / h.

[0263] After 73 hours TOS, the temperature was increased to 395°C and the system was operated for an additional 49 hours without showing any increase in pressure drop compared to Comparative Example 1 at longer operating times at both temperatures. The LHSV and GHSV were then reduced by 50% for an additional day before the pressure was increased to 110 bar. The LHSV reduction and pressure increase further increased the N and S conversion.

[0264] The resulting feed stream S3 had an average total chlorine content of less than 2 wppm, a chloride content of less than 1 wppm (see Table 2.3), and also had significantly reduced N and S contents, from 3264 wppm to about 31 wppm for N and from 2630 wppm to about 47 wppm for S (see Table 3).

[0265] [Table 4]

[0266] [Table 5]

[0267] Comparative Example 1: Process for refining pyrolysis oil not according to the invention (representative of French patent No. 3 107 530) Feed stream S0 containing pyrolysis oil similar to that of Example 1 was subjected to hydrogenation at a temperature of 50 bar and 195° C. in a reactor containing an activated Pd catalyst (Catalyst E-157 SDU 1 / 8″:0.7 wt.% Pd on 1 / 8″ alumina beads, commercially available from BASF) with H2. The Pd catalyst was activated in hydrogen flow at ambient pressure with GHSV=1000 / h while heating to 195° C. with a gradient of 0.5 K / min. After 12 h at 195° C., the GHSV was reduced to 500 / h and the pressure was increased to 50 bar within 1 h and held for 2 h before the addition of S0 was started with LHSV=1 / h. The resulting feed stream S1 had a MAV reduced by about 80% to 1.75 g(I2) / 100 g, a styrene content reduced to 1.1 area % (>80% conversion), and N and S contents unchanged compared to S0, i.e., N content was about 3260 wppm and S content was about 2630 wppm. The chlorine and chloride contents are shown in Table 4.

[0268] [Table 6]

[0269] Furthermore, stream S1 was directly subjected to hydrotreating in the presence of H2 at 50 bar and temperatures ranging from 350 to 395 °C in a reactor containing an activated P-doped NiMo catalyst supported on alumina (4.75 wt.% NiO, 19.57 wt.% MoO3, 2.89 wt.% P2O5 and 72.79% of the support Al2O3, respectively; the catalyst was prepared according to the process described in US Pat. No. 4,409,131). Catalyst activation was performed as in Example 1. The temperature in the reactor was kept constant after 1 h of catalyst activation, and the LHSV was reduced to 0.95 / h and the GHSV to 475 / h before starting the addition of S1 in the reactor with LHSV = 1 / h.

[0270] After 48 h TOS, the reactor temperature was increased to 395°C, but after about 70 h TOS, the pressure drop in the reactor system increased by more than 10 bar, so the feed injection was stopped and the reactor was cooled. The first intermediate pressure drop increase was observed between 55 and 60 h TOS.

[0271] To demonstrate that such a pressure rise was due to clogging of the downstream tube, the tube was replaced as described below. Indeed, to allow access to the downstream section, the system was depressurized and purged with nitrogen. A thin tube 1 m long with an internal diameter of 1.5 mm and heated to 40 ° C (as the downstream section below complete) was located after the transfer line from the reactor (180 ° C, internal diameter 4 mm) and before the gas-liquid separator. This tube was replaced. This change of tube allowed to substantially reduce the pressure drop across the reactor system, so that it was no longer noticeable.

[0272] Additionally, 5 mg of the solid was removed from the tube. XRD detected NH4Cl as the predominant crystalline phase in the solid, as seen in Figure 1.

[0273] After this tube replacement, the reactor was restarted with sulfide feed and hydrogen and heated to 350 °C at 1 K / min. At this temperature, the original feed was re-introduced to allow for another 15 h of hydrotreating operation, after which an increase in pressure drop was again observed, so feed injection was stopped after about 100 h of TOS. Despite intermediate system clogging, the catalyst still revealed relatively good performance after restart with >90% N conversion (see Table 5). For the combined product streams, a total chlorine content of <2 wppm and a chloride content of <1 wppm were determined, suggesting that the converted Cl was not present in the liquid product stream in dissolved form and in significant amounts, or as particulate matter that was filtered out during sample preparation for Cl analysis.

[0274] [Table 7]

[0275] [Table 8]

[0276] The pressure drop through the reactor is determined externally at 100 mln(N2) / min at ambient outlet pressure. The values ​​obtained are shown in Table 6.

[0277] Compared to the method of the present invention, the aforementioned process (representative of French Patent No. 3 107 530), which does not include a dechlorination step between the hydrogenation and hydrotreating steps, shows a high pressure drop increase rate during the course of the reaction, which does not allow a stable operation unless water is injected downstream, which causes serious corrosion problems. In addition, an increase in the pressure drop of the reactor after the reaction (210 mbar vs. 71 mbar according to the method of the present invention; see Table 6) was also observed. Thus, the method of the present invention shows a great improvement compared to this known process, taking into account a more stable operation with regard to increasing the pressure drop and therefore increasing the TOS, making it possible to obtain an improved oil production in terms of stability and duration.

[0278] Comparative Example 2: Method for refining pyrolysis oil according to the present invention In contrast to Example 1, the process started with the dechlorination step. Feed stream S0 containing pyrolysis oil similar to that of Example 1 was subjected to dechlorination in a reactor containing Cl sorbent (hydrotalcite: aluminum-magnesium hydroxycarbonate powder with a weight ratio of MgO:Al2O3 of 70:30) at 350 °C and 50 bar pressure in the presence of H2. Before use, the sorbent was pressed, then crushed and sieved to an average particle size of 500-1000 micrometers. Furthermore, it was calcined at 450 °C in air for 5 h and equilibrated overnight in ambient air. Before entering S0 into the reactor, the obtained Cl sorbent was dried at 100 °C and 200 °C in nitrogen at ambient pressure with a gas hourly space velocity (GHSV) = 2000 / h for 1 h each, with a temperature increase of 1 K / min. At 200 °C, the gas was switched from N2 to H2 and the pressure was increased to 50 bar within 1 h. After pressure was reached, the GHSV was reduced to 475 / h and the reactor was heated at 1 K / min to 350 °C. Once 350 °C was reached, S0 was introduced into the reactor at a liquid hourly space velocity (LHSV) = 0.95 / h.

[0279] After 165 h TOS, the pressure drop in the reactor system increased to more than 10 bar, so the feed injection had to be stopped and the reactor was cooled, purged with toluene and dried with nitrogen. The reactor pressure drop was determined externally at 100 mln(N2) / min at ambient outlet pressure, resulting in 1102 mbar, while the reactor pressure drop before the test was determined at 37 mbar. The chlorine and chloride content in the resulting stream S2 is shown in Table 7.

[0280] [Table 9]

[0281] [Table 10]

[0282] After the reaction, the reactor charge was removed. Different parts of the reactor charge were separated into inert corundum material and adsorbent above (preheat zone) and below (cooling zone) the adsorbent zone. A color gradient was observed over the length, especially in the preheat zone. Therefore, the samples were homogenized before analysis.

[0283] The samples were heated in air up to 700° C. and the resulting mass loss was recorded by thermogravimetric analysis combined with differential scanning calorimetry (Netzsch device STA 449 F3 Jupiter). For all samples obtained from Comparative Example 2, the exothermic mass loss increased, indicating an increase in coke formation. The relative increase in coke formation with respect to Example 1 is most pronounced in the preheating zone, where the mass loss increases by almost 100%.

[0284] In Figures 2a and 2b the coloration of the corundum from the preheat zone can be compared, showing the darker color of dechlorination only (Comparative Example 2-2a). After heating in air, the sample was decolorized to white, similar to the fresh state.

[0285] [Table 11]

[0286] Since both dechlorination experiments of Example 1 and Comparative Example 2 were operated for the same period, conditions and with the same adsorbent and inert corundum and showed significant differences in the subsequent reactor pressure drop and mass loss during heating of the preheat zone material in air, it can be derived that the accumulation of coke in the dechlorination step is accelerated if the feed is not prehydrogenated.

[0287] Therefore, based on this example, it has been demonstrated that a hydrogenation step is mandatory before the dechlorination step. Indeed, starting with the dechlorination directly leads to a very fast increase in pressure loss due to coking, which is unacceptable for the operation of an industrial plant. In addition, the dechlorination efficiency (see Tables 2.1 and 7) increases if the feed is pre-hydrogenated before the dechlorination.

Claims

1. 1. A method for refining pyrolysis oil, comprising: (i) providing a stream SO comprising a pyrolysis oil, said pyrolysis oil comprising one or more halogenated organic compounds and one or more organic compounds comprising conjugated double bonds; (ii) subjecting said stream S0 provided in (i) to hydrogenation in at least one reaction zone Z1 containing a heterogeneous hydrogenation catalyst to obtain a stream S1 depleted in said one or more organic compounds containing conjugated double bonds compared to S0; (iii) subjecting said stream S1 obtained from (ii) to a dehalogenation in at least one dehalogenation zone Z2 downstream of Z1 to obtain a stream S2 depleted in said one or more halogenated organic compounds compared to S1; A method comprising:

2. 2. The method according to claim 1, wherein the pyrolysis oil according to (i) comprises one or more organic compounds containing said conjugated double bonds in a total amount ranging from 0.1 to 75 g (I2) / 100 g, preferably from 0.4 to 60 g (I2) / 100 g, more preferably from 1 to 30 g (I2) / 100 g of the pyrolysis oil.

3. The one or more organic compounds containing conjugated double bonds are represented by the formula (I) R 1 R 2 C 1 =C 2 R 3 -C 3 R 4 =X (I) (wherein =X is =O, =S, =NR 5 , or = C 4 R 6 R 7 , preferably = C 4 R 6 R 7 and Preferably R 1 , R 2 , R 3 , R 4 , R 5 are each independently H, an alkyl having 1 to 6 carbon atoms, an alkenyl having 1 to 6 carbon atoms, or an aryl having 5 to 10 carbon atoms, more preferably H; Preferably R 6 and R 7 are each independently H, alkyl having 1 to 6 carbon atoms, alkenyl having 1 to 6 carbon atoms, or aryl having 5 to 10 carbon atoms, more preferably H; or preferably R 4 and R 6 Or R 4 and R 7 are linked together to form C 3 = C 4 together with the aryl group, preferably forming an aromatic ring having 5 or 6 members. and one or more organic compounds according to The one or more organic compounds containing conjugated double bonds according to formula (I) more preferably comprise one or more of butadiene, isoprene, dienes having 5 or 6 carbon atoms, styrene, methylstyrene, indene, substituted styrenes, substituted indenes, and 3-methyl-2-butenal, more preferably one or more of butadiene, isoprene, dienes having 5 or 6 carbon atoms, styrene, methylstyrene, indene, and 3-methyl-2-butenal; More preferably, the one or more organic compounds comprising conjugated double bonds according to formula (I) comprise styrene.

4. said heterogeneous hydrogenation catalyst according to (ii) comprises an element from groups 8 to 12, preferably from groups 8 to 10, more preferably from groups 9 and 10 of the Periodic Table of the Elements, preferably an element selected from the group consisting of Ni, Pd and Co, more preferably an element selected from the group consisting of Ni and Pd, 4. The process according to any one of claims 1 to 3, wherein the heterogeneous hydrogenation catalyst according to (ii) further comprises a support material, preferably for said elements of groups 8 to 12 of the periodic table of the elements, said support material being more preferably selected from the group consisting of oxidic materials and carbon, said oxidic material being more preferably one or more of alumina, silica, magnesia, zirconia, titania, zeolitic materials, silica-alumina phosphate (SAPO) materials, zinc oxide, sodium oxide, mixed silica-alumina, zeolites and calcium oxide, more preferably alumina.

5. (ii) (ii.1) introducing a gas flow G0 into Z1, said gas flow being H 2 and (ii.2) introducing said flow S0 into Z1; (ii.3) contacting S0 with G0 and said heterogeneous hydrogenation catalyst contained in Z1 to obtain a stream S1 depleted in said one or more organic compounds containing conjugated double bonds compared to S0; (ii.4) removing S1 from Z1; Including, 5. The method according to any one of claims 1 to 4, wherein the gas stream G0 is introduced at a pressure preferably in the range of from 10 to 100 bar (abs), more preferably in the range of from 15 to 90 bar (abs), more preferably in the range of from 20 to 80 bar (abs), more preferably in the range of from 20 to 55 bar (abs).

6. 6. The method according to claim 5, wherein the gas stream G0 has a temperature in the range of from 100 to 250°C, preferably from 120 to 220°C, more preferably from 140 to 200°C.

7. 7. The process according to any one of claims 1 to 6, wherein the stream S1 obtained from (ii) and subjected to dehalogenation in (iii) comprises one or more organic compounds containing conjugated double bonds in a total amount ranging from 0 to 3 g (I2) / 100 g, preferably from 0 to 2 g (I2) / 100 g, more preferably from 0 to 1 g (I2) / 100 g, preferably from 0 to 0.25 g (I2) / 100 g, more preferably from 0 to 0.1 g (I2) / 100 g of stream S1.

8. 8. The process according to any one of the preceding claims, wherein the stream S1 subjected to dehalogenation in (iii) has a temperature in the range of from 150 to 450°C, preferably from 200 to 400°C, more preferably from 250 to 350°C.

9. (iii) (iii.1) introducing a gas stream G1 into a preferably adsorption zone Z2, preferably the gas stream comprising one or more of hydrogen and nitrogen, more preferably hydrogen; (iii.2) introducing the stream S1 obtained from (ii) into Z2; (iii.3) contacting S1 with a heterogeneous adsorbent material suitable for adsorbing the halides contained in at least one of G1 and said one or more halogenated organic compounds contained in Z2 to obtain a stream S2 depleted in said one or more halogenated organic compounds compared to S1; (iii.4) removing S2 from Z2; 9. The method of any one of claims 1 to 8, comprising:

10. said gas flow G1 having a temperature in the range of 250 to 500° C., preferably in the range of 300 to 400° C.; 10. The method according to claim 9, wherein the gas stream G1 is introduced at a pressure preferably in the range of 1 to 100 bar (abs), more preferably in the range of 5 to 80 bar (abs), more preferably in the range of 10 to 50 bar (abs).

11. 9. The process according to any one of claims 1 to 8, wherein the dehalogenation zone Z2 according to (iii) comprises a catalytic zone, preferably a catalytic zone, preferably comprising a heterogeneous dehalogenation catalyst, said catalyst comprising one or more catalytically active elements from groups 8 to 12 of the Periodic System of the Elements.

12. 12. The process according to any one of the preceding claims, wherein the stream S2 obtained from (iii) has a total chlorine content in the range of from 0 to 200 wppm (ppm by weight), preferably from 0 to 160 wppm, more preferably from 0 to 130 wppm.

13. (iv) subjecting said stream S2 obtained from (iii) to hydrotreating in at least one reaction zone Z3 downstream of Z2, Z3 comprising a heterogeneous hydrotreating catalyst, to obtain a stream S3. Further comprising: said stream S2 subjected to (iv) has a temperature in the range of from 150 to 400° C., preferably in the range of from 200 to 375° C., more preferably in the range of from 250 to 350° C., The heterogeneous hydrotreating catalyst used in (iv) preferably comprises an element selected from the group consisting of elements from groups 8 to 10, preferably groups 9 and 10, of the Periodic Table of the Elements, more preferably Ni and Co, and the heterogeneous hydrogenation catalyst more preferably comprises Ni; 13. The process according to any one of the preceding claims, wherein the heterogeneous hydrotreating catalyst according to (iv) more preferably comprises an amount of Ni in the range of 0.5 to 10 wt.-%, more preferably in the range of 1 to 6 wt.-%, calculated as NiO, based on the weight of the heterogeneous hydrotreating catalyst.

14. (iv) (iv.1) introducing a gas flow G2 into Z3, wherein G2 is H 2 and (iv.2) (iii) introducing the stream S2 into Z3; (iv.3) contacting S2 with G2 and a heterogeneous hydrotreating catalyst contained in Z3 to obtain stream S3; (iv.4) removing S3 obtained in (iv.3) from Z3; 14. The method of claim 13, comprising:

15. 15. The process according to any one of claims 1 to 14, which is a continuous or semi-continuous process, preferably a continuous process.

16. A production unit for carrying out the method for refining pyrolysis oil according to any one of claims 1 to 15, at least one reaction zone Z1, Z1 comprising a heterogeneous hydrogenation catalyst; - an inlet means for introducing S0 into Z1; - exit means for removing S1 from Z1; at least one dehalogenation zone Z2, preferably comprising a heterogeneous adsorbent material or a heterogeneous dehalogenation catalyst; - an inlet means for introducing S1 into Z2; - an exit means for removing S2 from Z2; Equipped with Z1 is located upstream of Z2, Preferably, an extraction zone for removing halides, preferably comprising one or more halides of N-containing organic compounds, preferably located downstream of Z2; Further equipped with The manufacturing unit preferably comprises: at least one reaction zone Z3, Z3 comprising a heterogeneous hydrotreating catalyst; - an entry means for introducing S2 into Z3; - an exit means for removing S3 from Z3; Further equipped with The Z2 is a manufacturing unit located upstream of the Z3.

17. 16. Refined pyrolysis oil obtainable or obtained by a method according to any one of claims 1 to 12 and 15 or any one of claims 13 to 15.

Citation Information

Patent Citations

  • PROCESS FOR TREATMENT OF PLASTICS PYROLYSIS OILS FOR THEIR VALORIZATION IN A STEAM CRACKER UNIT

    FR3103822A1

  • A catalytic process for reducing chloride content of a hydrocarbon feed stream

    WO2017083018A1

Cited By

  • Hydrotreated oil and method for producing same

    WO2026160302A1