APPARATUS, SYSTEM AND METHOD FOR FORMING OPHTHALMIC LENS COMPONENTS USING FUSION CORE AND MOLD - Patent application
The use of soluble cores and molds addresses the challenges of forming complex AIOL components by enabling efficient and defect-free manufacturing of AIOLs with complex geometries, reducing labor intensity and manufacturing time.
Patent Information
- Application Number
- JP2024525516
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2021-12-20
- Filing Date
- 2022-12-16
- Publication Date
- 2024-12-05
AI Technical Summary
Conventional methods for manufacturing ophthalmic lenses, particularly accommodative intraocular lenses (AIOLs), face challenges in forming components with complex cavities or conduits, leading to labor-intensive processes, material seepage, and surface defects like flash lines, which increase manufacturing time and complexity.
The use of soluble cores and molds to form ophthalmic lens components, where a fusible core is placed within a mold, lens material is cured, and then dissolved using a solvent, allowing for the creation of complex geometries without the need for solid inserts and reducing surface defects.
This method enables cost-effective manufacturing of AIOL components with complex shapes and geometries, eliminating labor-intensive steps and surface imperfections, thereby improving production efficiency and quality.
Smart Images

Figure 2024544852000001_ABST
Abstract
Description
[Technical field]
[0001] CROSS-REFERENCE TO RELATED APPLICATIONS This application claims the benefit of U.S. Provisional Patent Application No. 63 / 265,735, filed December 20, 2021, which is incorporated herein by reference.
[0002] The present disclosure relates generally to the field of ophthalmic devices, and more specifically to apparatus, systems, and methods for forming ophthalmic lens components using fusible cores and molds. [Background technology]
[0003] Cataracts are a condition involving the clouding of the normally transparent lens of a patient's eye. Cataracts develop as a result of aging, genetic factors, trauma, inflammation, metabolic disease, or exposure to radiation. Age-related cataracts are the most common type of cataract. In cataract treatment, surgeons remove the lens matrix from the patient's lens capsule and replace it with an intraocular lens (IOL). Traditional IOLs provide one or more selected focal lengths that allow the patient to see in the distance. However, after cataract surgery, patients with traditional IOLs inserted often require glasses or other corrective eyewear to perform certain activities because the eye can no longer accommodate (i.e., change its refractive power) to retain a sharp image of an object or to focus on an object as the distance changes.
[0004] Newer IOLs, such as accommodative IOLs, allow the eye to regain at least some focusing ability. Accommodative IOLs (AIOLs) use the power available in the eye to change some portion of the optical system to refocus the eye to a distant or near target. Examples of AIOLs are discussed in the following U.S. Patent Publications: U.S. Patent Application Publication No. 2018 / 0256315, U.S. Patent Application Publication No. 2018 / 0153682, U.S. Patent Application Publication No. 2017 / 0049561, and the following issued U.S. patents: U.S. Patent No. 10,299,913, U.S. Patent No. 10,195,020, U.S. Patent No. 8,968,396, the contents of which are incorporated herein by reference in their entireties.
[0005] Conventional ophthalmic lenses are often fabricated using molding techniques that rely on a polished mold with a mold cavity formed in the shape of the lens. Common molding techniques include injection molding, liquid silicone rubber injection molding, compression molding, and transfer molding. However, unlike conventional ophthalmic lenses, AIOLs are often made from components that contain cavities or conduits for holding or transporting fluids. In some cases, AIOL components, such as AIOL haptics, are molded using solid inserts that are carefully pulled from the molded haptics after a curing process. Such steps are labor intensive and difficult to adjust. Furthermore, solid inserts often cannot be used for AIOL components with cavities or conduits with complex shapes or geometries. This is especially true for AIOL components with cavities with multiple interconnected compartments or portions.
[0006] In addition, conventional molding techniques often leave small gaps between mold components during the molding process. As a result, material introduced into the mold often seeps or flows through these small gaps, forming visible lines or surface imperfections along the surface of the lens component (often referred to as "flash"). These flash lines and imperfections must then be smoothed or polished away, thereby increasing manufacturing time. Summary of the Invention [Problem to be solved by the invention]
[0007] Therefore, there is a need for a solution that allows for the formation of ophthalmic lens components having cavities or conduits with complex shapes or geometries. Such a solution should not be too complex and should allow the lens components to be manufactured in a cost-effective manner. [Means for solving the problem]
[0008] Disclosed herein are devices, systems, and methods for forming an ophthalmic lens component (e.g., haptic or optic portion) using a fusible core and a mold. In one embodiment, a method for manufacturing a lens component includes providing a first mold component including a first molding surface defined by a first component cavity portion, and providing a second mold component including a second molding surface defined by a second component cavity portion. The method can include placing at least a portion of the fusible core component on either the first molding surface or the second molding surface.
[0009] In some embodiments, placing at least a portion of the soluble core component on either the first or second molding surface can include placing at least one positioning piece of the soluble core on the first or second molding surface. The at least one positioning piece can be at one end of the soluble core component. Another portion or segment of the soluble core component can be positioned above the first or second molding surface without physical contact with the first or second molding surface. In other embodiments, the remaining portion of the soluble core component connected to the positioning piece can be positioned above the first or second molding surface without physical contact with the first or second molding surface.
[0010] The method may also include mating a second mold component with the first mold component to form an assembly mold. The second mold component may include a second molding surface defined by a second component cavity portion. A segment of the fusible core component may be disposed within the component mold cavity formed by the first component cavity portion and the second component cavity portion. Another segment of the fusible core component may be disposed outside the component mold cavity when the second mold component is mated with the first mold component.
[0011] The method may also include introducing a lens component material into the component mold cavity and curing the lens component material in the assembly mold to form a molded lens component. The method may also include separating the first mold component from the second mold component after curing the lens component material to form the molded lens component. The method may further include removing the molded lens component from the first mold component or the second mold component. At least one segment of the fusible core component may be within the molded lens component when the molded lens component is removed from at least one of the first mold component and the second mold component.
[0012] The method may also include immersing the molded lens component in a solvent to dissolve the soluble core component. In some embodiments, the soluble core component may be made in part of polyvinyl alcohol. In these and other embodiments, the solvent may be water. The method may also include heating the solvent and agitating the solvent by sonication to facilitate dissolution of the soluble core component.
[0013] In some embodiments, the first molding surface can be further defined by a first plug cavity portion connected to the first component cavity portion. In these embodiments, the second molding surface can be defined by a second plug cavity portion connected to the second component cavity portion. Furthermore, in these embodiments, the method can include placing a fusible plug in the first plug cavity portion or the second plug cavity portion prior to forming the assembly mold. The fusible plug can occupy a plug receiving space formed by the first plug cavity portion and the second plug cavity portion when the second mold component is mated with the first mold component. The method can further include hardening the lens component material in the assembly mold when the assembly mold also includes a fusible plug.
[0014] The method may also include removing the molded lens component and the soluble plug from the first mold component or the second mold component. The method may further include immersing the molded lens component and the soluble plug in a solvent to dissolve the soluble core component and the soluble plug. The soluble plug may be configured to prevent flashing at the periphery of the molded lens component.
[0015] In some embodiments, the lens component can be a haptic of a lens, and a haptic chamber can be formed in the haptic when the soluble core component dissolves. In other embodiments, the lens component can be an optic portion of a lens, and an optic chamber can be formed in the optic when the soluble core component dissolves. In additional embodiments, the lens component can be a part of the optic portion of a lens (e.g., an anterior lens element or a posterior lens element), and at least a portion of an optic chamber can be formed when the soluble core component dissolves.
[0016] A system for manufacturing a lens component is also disclosed. The system can include a first mold component including a first molding surface defined by a first component cavity portion and a second mold component including a second molding surface defined by a second component cavity portion. The system can also include a fusible core component configured to be placed on the first molding surface or the second molding surface.
[0017] The soluble core component can include at least one positioning piece. The at least one positioning piece can be configured to be placed on either the first molding surface or the second molding surface. The at least one positioning piece can be at one end of the soluble core component. Other portions or segments of the soluble core component can be positioned above the first molding surface or the second molding surface without physical contact with the first molding surface or the second molding surface. In other embodiments, the remaining portion of the soluble core component that is connected to the positioning piece can be positioned above the first molding surface or the second molding surface without physical contact with the first molding surface or the second molding surface.
[0018] The first mold component can be configured to be mated with the second mold component to form an assembly mold, and a segment or portion of the fusible core component can be configured to be disposed within a component mold cavity formed by the first component cavity portion and the second component cavity portion when the first mold component is mated with the second mold component.
[0019] A component mold cavity in the assembly mold can receive a lens component material for hardening into a molded lens component. The lens component material can be hardened into the molded lens component in the assembly mold. When the first mold component is separated from the second mold component after hardening, the molded lens component can be removed from the first mold component or the second mold component. When the molded lens component is removed from at least one of the first mold component and the second mold component, at least one segment of the soluble core component can be in the molded lens component.
[0020] The soluble core component can be configured to dissolve in a solvent when the molded component is immersed in the solvent. In some embodiments, the soluble core component can be made, in part, from polyvinyl alcohol. In these and other embodiments, the solvent can be water.
[0021] In some embodiments, the system can also include a warm water bath configured to heat the solvent when the molded lens component is immersed in the solvent. The system can also include an ultrasonicator configured to agitate the solvent and promote dissolution of the soluble core component.
[0022] The system can further include a fusible plug configured to be placed in a first plug cavity portion defined along the first molding surface or to be placed in a second plug cavity portion defined along the second molding surface prior to forming the assembly mold. The fusible plug can be configured to occupy a plug receiving space formed by the first plug cavity portion and the second plug cavity portion when the second mold component is mated with the first mold component. The assembly mold including the lens component material, the fusible core component, and the fusible plug can be cured together.
[0023] After the curing step, the molded lens component, including the soluble core component and the soluble plug, can be removed from the first mold component or the second mold component for immersion in a solvent.
[0024] The soluble core component and the soluble plug can be configured to dissolve when immersed in a solvent, and the soluble plug can be configured to prevent flashing at the periphery of the molded lens component.
[0025] In some embodiments, the lens component can be a haptic of a lens (e.g., an IOL or AIOL). In these embodiments, the haptic chamber can be formed when the soluble core component is dissolved by a solvent.
[0026] In other embodiments, the lens component can be the optic portion of the lens. In these embodiments, an optic portion chamber can be formed in the optic portion when the soluble core component is dissolved by the solvent. Additionally, the lens component can also be part of the optic portion of the lens. At least a portion of the optic portion chamber can be formed when the soluble core component is dissolved by the solvent.
[0027] Another method of manufacturing a lens component is also disclosed. The method includes providing a first mold component fabricated from a soluble material. The first mold component can include a first molding surface defined by a first component cavity portion. The method can further include providing a second mold component fabricated from a soluble material. The second mold component can include a second molding surface defined by a second component cavity portion.
[0028] The method may also include placing at least a portion of a fusible core component made of a fusible material on the first molding surface or the second molding surface and mating a second mold component with the first mold component to form an assembly mold. A segment of the fusible core component may be disposed within a component mold cavity formed by the first component cavity portion and the second component cavity portion when the first mold component is mated with the second mold component.
[0029] In some embodiments, placing at least a portion of the soluble core component on the first or second molding surface can include placing at least one positioning piece of the soluble core component on the first or second molding surface. The at least one positioning piece can be at one end of the soluble core component. Other portions or segments of the soluble core component can be positioned above the first or second molding surface without physical contact with the first or second molding surface. In other embodiments, the remaining portion of the soluble core component connected to the positioning piece can be positioned above the first or second molding surface without physical contact with the first or second molding surface.
[0030] In some embodiments, the method can include wetting at least one of the first and second molding surfaces with a wetting agent prior to mating the second mold component with the first mold component to prevent flash from occurring at the periphery of the molded lens component at a parting line created by the first and second mold components, hi some embodiments, the wetting agent can be water.
[0031] The method may also include introducing a lens component material into the component mold cavity and curing the lens component material in the assembly mold to form a molded lens component. The method may further include immersing the assembly mold including the molded lens component in a solvent to dissolve the soluble core component, the first mold component, and the second mold component. Additionally, the method may also include heating the solvent and agitating the solvent by sonication to promote dissolution of the soluble core component, the first mold component, and the second mold component.
[0032] In one embodiment, the soluble core component, the first mold component, and the second mold component can all be made, in part, of polyvinyl alcohol. In other embodiments, at least one of the soluble core component, the first mold component, and the second mold component can be made, in part, of a soluble material other than polyvinyl alcohol. In some embodiments, the solvent can be water.
[0033] In some embodiments, the lens component can be a haptic of a lens (e.g., an IOL or AIOL). In these embodiments, a haptic chamber can be formed in the haptic when the soluble core component dissolves in a solvent.
[0034] In other embodiments, the lens component can be the optic portion of the lens. In these embodiments, an optic portion chamber can be formed in the optic portion when the soluble core component dissolves in the solvent. Additionally, the lens component can also be part of the optic portion of the lens. At least a portion of the optic portion chamber can be formed when the soluble core component dissolves in the solvent.
[0035] Another system for manufacturing lens components is also disclosed. The system can include a first mold component fabricated from a soluble material and a second mold component also fabricated from a soluble material. The first mold component can include a first molding surface defined by a first component cavity portion. The second mold component can include a second molding surface defined by a second component cavity portion.
[0036] The system may also include a soluble core component configured to be placed on either the first molding surface or the second molding surface. The soluble core component may include at least one positioning piece. The at least one positioning piece may be configured to be placed on either the first molding surface or the second molding surface. The at least one positioning piece may be at one end of the soluble core component. Other portions or segments of the soluble core component may be positioned above the first molding surface or the second molding surface without physical contact with the first molding surface or the second molding surface. In other embodiments, the remaining portion of the soluble core component coupled to the positioning piece may be positioned above the first molding surface or the second molding surface without physical contact with the first molding surface.
[0037] The first mold component can be configured to mate with the second mold component to form an assembly mold. A segment of the fusible core component can be configured to be disposed within a component mold cavity formed by the first component cavity portion and the second component cavity portion when the first mold component is mated with the second mold component. The component mold cavity can also receive lens component material for curing into a molded lens component.
[0038] The entire assembly mold can be immersed in a solvent after curing. At least one segment of the soluble core component can be within the molded lens component when the assembly mold containing the molded lens component is immersed in the solvent. The soluble core component, the first mold component, and the second mold component can be dissolved by the solvent when immersed in the solvent.
[0039] In some embodiments, the system can also include a warm water bath configured to heat the solvent when the soluble core component, the first mold component, and the second mold component are immersed in the solvent. The system can also include an ultrasonicator configured to agitate the solvent to facilitate dissolution of the soluble core component, the first mold component, and the second mold component.
[0040] In one embodiment, the soluble core component, the first mold component, and the second mold component can all be made, in part, of polyvinyl alcohol. In other embodiments, at least one of the soluble core component, the first mold component, and the second mold component can be made, in part, of a soluble material other than polyvinyl alcohol. In some embodiments, the solvent can be water.
[0041] In some embodiments, the lens component can be a haptic of a lens (e.g., an IOL or AIOL). In these embodiments, a haptic chamber can be formed in the haptic when the soluble core component is dissolved by a solvent.
[0042] In other embodiments, the lens component can be the optic portion of the lens. In these embodiments, an optic portion chamber can be formed in the optic portion when the soluble core component is dissolved by the solvent. Additionally, the lens component can also be part of the optic portion of the lens. At least a portion of the optic portion chamber can be formed when the soluble core component is dissolved by the solvent.
[0043] Other methods of manufacturing lens components are also disclosed. The methods include providing a first mold component made of a soluble material and a second mold component made of an insoluble material, or providing a first mold component made of an insoluble material and a second mold component made of a soluble material. The first mold component can include a first molding surface defined by a first component cavity portion. The second mold component can include a second molding surface defined by a second component cavity portion.
[0044] The method may also include placing at least a portion of a fusible core component made of a fusible material on either the first molding surface or the second molding surface, and mating a second mold component with the first mold component to form an assembly mold. When the first mold component is mated with the second mold component, a segment of the fusible core component may be disposed within a component mold cavity formed by the first component cavity portion and the second component cavity portion.
[0045] In some embodiments, placing at least a portion of the soluble core component on the first or second molding surface can include placing at least one positioning piece of the soluble core component on the first or second molding surface. The at least one positioning piece can be at one end of the soluble component. Another portion or segment of the soluble core component can be positioned above the first or second molding surface without physical contact with the first or second molding surface. In other embodiments, the remaining portion of the soluble core component connected to the positioning piece can be positioned above the first or second molding surface without physical contact with the first or second molding surface.
[0046] The method may also include introducing a lens component material into the component mold cavity and curing the lens component material in the assembly mold to form a molded lens component. The method may further include separating the second mold component from the first mold component after the curing step.
[0047] The method may also include immersing the first mold component made of the soluble material and the molded lens component in a solvent or immersing the second mold component made of the soluble material in a solvent to dissolve the soluble core component and the mold component made of the soluble material. Additionally, the method may also include heating the solvent and agitating the solvent by sonication to promote dissolution of the soluble core component and the mold component made of the soluble material.
[0048] In some embodiments, the method can include wetting at least one of the first and second molding surfaces with a wetting agent prior to mating the second mold component with the first mold component to prevent flash at a parting line created by the first and second mold components along the periphery of the molded lens component, hi some embodiments, the wetting agent can be water.
[0049] In one embodiment, the soluble core component and either the first mold component or the second mold component can be made in part of polyvinyl alcohol. In other embodiments, the soluble core component can be made in part of a soluble material other than polyvinyl alcohol. In these and other embodiments, either the first mold component or the second mold component can be made in part of a soluble material other than polyvinyl alcohol. In some embodiments, the solvent can be water.
[0050] In some embodiments, the lens component can be a haptic of a lens (e.g., an IOL or AIOL). In these embodiments, a haptic chamber can be formed in the haptic when the soluble core component is dissolved by a solvent.
[0051] In other embodiments, the lens component can be the optic portion of the lens. In these embodiments, an optic portion chamber can be formed in the optic portion when the soluble core component is dissolved by the solvent. Additionally, the lens component can be part of the optic portion of the lens. At least a portion of the optic portion chamber can be formed when the soluble core component is dissolved by the solvent.
[0052] The method can also include, prior to forming the assembly mold, placing a soluble plug into a plug cavity defined along either the first molding surface or the second molding surface. The soluble plug can be configured to occupy the plug cavity when the second mold component is mated with the first mold component. The assembly mold including the lens component material, the soluble core component, and the soluble plug can be cured together.
[0053] After the curing step, the second mold component can be separated from the first mold component. The molded lens component, the soluble plug, and the mold component made of the soluble material can be immersed in a solvent. The molded lens component, the soluble plug, and the molded lens component made of the soluble material can be dissolved when immersed in the solvent. The soluble plug can be configured to prevent flash along the periphery of the molded lens component.
[0054] Another system for manufacturing lens components is also disclosed. The system may include either a first mold component made of a soluble material and a second mold component made of an insoluble material, or a first mold component made of an insoluble material and a second mold component made of a soluble material. The first mold component may include a first molding surface defined by a first component cavity portion. The second mold component may include a second molding surface defined by a second component cavity portion.
[0055] The system may also include a soluble core component configured to be placed on either the first molding surface or the second molding surface. The soluble core component may include at least one positioning piece. The at least one positioning piece may be configured to be placed on either the first molding surface or the second molding surface. The at least one positioning piece may be at one end of the soluble core component. Another portion or segment of the soluble core component may be positioned above the first molding surface or the second molding surface without physical contact with the first molding surface or the second molding surface. In another embodiment, the soluble core component may include at least one positioning piece at one end of the soluble core component and at a free distal end at an opposite end of the soluble core component. The free distal end of the soluble core component may be configured to be positioned above the first molding surface or the second molding surface without physical contact with the first molding surface or the second molding surface when the at least one positioning piece is positioned on the first molding surface.
[0056] The first mold component can be configured to be mated with the second mold component to form an assembly mold. A segment of the fusible core component can be configured to be disposed within a component mold cavity formed by the first component cavity portion and the second component cavity portion when the first mold component is mated with the second mold component. The component mold cavity can also receive lens component material for curing into a molded lens component.
[0057] The second mold component can be separated from the first mold component and the molded lens component after curing. The molded lens component and the mold component made of the soluble material can be immersed in a solvent after curing. At least one segment of the soluble core component can be within the molded lens component when the molded lens component and the mold component made of the soluble material are immersed in the solvent. The soluble core component and the mold component made of the soluble material can be dissolved by the solvent when immersed in the solvent.
[0058] In some embodiments, the system can also include a warm water bath configured to heat the solvent as the soluble core component and the mold components fabricated from the soluble material are immersed in the solvent. The system can also include an ultrasonicator configured to agitate the solvent to promote dissolution of the soluble core component and the mold components fabricated from the soluble material.
[0059] In one embodiment, the soluble core component and either the first mold component or the second mold component can be made, in part, of polyvinyl alcohol. In other embodiments, the soluble core component can be made, in part, of a soluble material other than polyvinyl alcohol, or either the first mold component or the second mold component can be made, in part, of a soluble material other than polyvinyl alcohol. In some embodiments, the solvent can be water.
[0060] In some embodiments, the lens component can be a haptic of a lens (e.g., an IOL or AIOL). In these embodiments, a haptic chamber can be formed in the haptic when the soluble core component is dissolved by a solvent.
[0061] In other embodiments, the lens component can be the optic portion of the lens. In these embodiments, an optic portion chamber can be formed in the optic portion when the soluble core component is dissolved by the solvent. Additionally, the lens component can also be part of the optic portion of the lens. At least a portion of the optic portion chamber can be formed when the soluble core component is dissolved by the solvent.
[0062] The system can further include a soluble plug configured to be placed in a plug cavity defined along either the first molding surface or the second molding surface prior to forming the assembly mold. The soluble plug can be configured to occupy the plug cavity when the second mold component is mated with the first mold component. The assembly mold including the lens component material, the soluble core component, and the soluble plug can be cured together.
[0063] After the curing step, the second mold component can be separated from the first mold component. The molded lens component, the soluble plug, and the mold component made of the soluble material can be immersed in a solvent. The soluble core component, the soluble plug, and the mold component made of the soluble material can be configured to dissolve when immersed in the solvent. The soluble plug can be configured to prevent flash along the periphery of the molded lens component. [Brief description of the drawings]
[0064] [Figure 1A] 1 shows a top view of an embodiment of an accommodating intraocular lens that includes a soluble core and components that can be fabricated using a mold. [Figure 1B-1C] 1 shows a cross-sectional view of an accommodating intraocular lens. [Figure 1D] 1 shows an exploded view of one embodiment of an accommodating intraocular lens that includes components that can be fabricated using a soluble core and a mold. [Figure 2A]1 illustrates an embodiment of a first mold component including a first molding surface defined by a first component cavity portion. [Figure 2B] 1 illustrates an embodiment of a second mold component including a second molding surface defined by a second component cavity portion. [Figure 2C] 1 illustrates an embodiment of a clamp member for securing a first mold component to a second mold component. [Figure 2D] 1 illustrates an embodiment of a fusible core component disposed on a first molding surface of a first mold component. [Figure 2E] 1 shows an assembly mold including a first mold component mated with a second mold component. [Figure 3A] FIG. 1 illustrates a perspective view of an embodiment of a fusible core component. [Figure 3B] FIG. 13 shows a perspective view of another embodiment of a fusible core component. [Figure 4A-4D] 1 illustrates a cross-sectional view of an embodiment of a fusible core component. [Figure 5A] 4B shows a cross-sectional view of an embodiment of a haptic fabricated using the fusible core component of FIG. 4A. [Figure 5B] 4C shows a cross-sectional view of an embodiment of a haptic fabricated using the fusible core component of FIG. 4B. [Figure 6] 1 illustrates a top view of an embodiment of a haptic that includes an internal cavity pattern fabricated using the fusible core and mold disclosed herein. [Figure 7] 1 illustrates an embodiment of a system for manufacturing a lens component. [Figure 8] 1 illustrates a cross-sectional view of an embodiment of an assembly mold including a fusible plug to prevent flash. [Figure 9A] 1 illustrates an embodiment of the optic portion of an accommodating intraocular lens. [Figure 9B]9B shows an exploded cross-sectional view of an embodiment of a mold component and a fusible core component for fabricating the optical portion of FIG. 9A. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0065] Disclosed herein are devices, systems, and methods for forming components of an IOL or AIOL using a soluble core and a mold. For example, Figures 1A-1D show embodiments of an AIOL that can be fabricated from a lens component (e.g., haptics or optic portion) formed using a soluble core and a mold according to the methods described herein.
[0066] 1A shows a top view of an embodiment of an accommodating intraocular lens (AIOL) 100 including lens components that can be fabricated using a soluble core and a mold. The AIOL 100 can be implanted in a subject to correct defocus aberration, corneal astigmatism, spherical aberration, or a combination thereof. The AIOL 100 can include an optic portion 102 and a peripheral portion 103 including one or more haptics 104, including a first haptic 104A and a second haptic 104B in this embodiment coupled to the optic portion 102 and extending along the periphery. The AIOL 100 is configured to be positioned in a natural lens capsule from which the natural lens has been removed.
[0067] When implanted within the natural lens capsule, the optic portion 102 can be adapted to refract light entering the eye's retina. The peripheral portion 103 (e.g., one or more haptics 104) can be configured to engage the lens capsule and is adapted to deform in response to ciliary muscle movement (e.g., muscle relaxation, muscle contraction, or a combination thereof) in conjunction with deformation of the lens capsule. Engagement of the peripheral portion 103 (e.g., one or more haptics 104) with the lens capsule is described in more detail in the following sections.
[0068] Figures 1B and 1C show cross-sectional views of the AIOL 100 taken along cross-section AA of Figure 1A. As shown in Figures 1B and 1C, the optic portion 102 can include an anterior element 106 and a posterior element 108. A fluid-filled optic portion fluid chamber 110 can be defined between the anterior element 106 and the posterior element 108.
[0069] The anterior element 106 can include a front optical surface 112 and a front inner surface 114 opposite the anterior optical surface 112. The posterior element 108 can include a posterior optical surface 116 and a posterior inner surface 118 opposite the posterior optical surface 116. Either the anterior optical surface 112, the posterior optical surface 116, or a combination thereof can be considered and referred to as an optical outer surface. The anterior inner surface 114 and the posterior inner surface 118 can face the optical portion fluid chamber 110. At least a portion of the anterior inner surface 114 and at least a portion of the posterior inner surface 118 can serve as a chamber wall of the optical portion fluid chamber 110.
[0070] Each of the one or more haptics 104 can include a haptic fluid chamber 120 within the haptic 104. For example, a first haptic 104A can include a first haptic fluid chamber 120A within the first haptic 104A, and a second haptic 104B can include a second haptic fluid chamber 120B within the second haptic 104B. Haptic fluid chamber 120 (e.g., either first haptic fluid chamber 120A, second haptic fluid chamber 120B, or a combination thereof) can be in fluid communication with or fluidly connectable to optical portion fluid chamber 110.
[0071] The optical portion fluid chamber 110 can be in fluid communication with one or more haptic fluid chambers 120 through a fluid channel pair 122 (see FIG. 1A). The fluid channel 122 can be a conduit or passage that fluidly connects the optical portion fluid chamber 110 to the haptic fluid chamber 120. The fluid channel pair 122 can be spaced apart from one another. For example, the fluid channel pair 122 can be spaced apart by about 0.1 mm to about 1.0 mm. In some embodiments, the diameter of each of the fluid channel pairs 122 is about 0.4 mm to about 0.6 mm.
[0072] In some embodiments, the fluid channel pair 122 can be defined and extend through a portion of the optical portion 102. More specifically, the fluid channel pair 122 can be defined and extend through the posterior element 108.
[0073] 1A shows that one or more haptics 104 of the peripheral portion 103 can be coupled to the optic portion 102 at a haptic-optical portion boundary 124. For example, one or more haptics 104 can be coupled to the optic portion at a reinforcement portion 126 (see FIG. 1D ) along the optic portion 102. The reinforcement portion 126 can be part of the haptic-optical portion boundary 124. The fluid channel pair 122 can be defined or formed in a portion of the reinforcement portion 126.
[0074] The optical portion fluid chamber 110 can be in fluid communication with a first haptic fluid chamber 120A through a first fluid channel pair 122A. The optical portion fluid chamber 110 can also be in fluid communication with a second haptic fluid chamber 120B through a second fluid channel pair 122B.
[0075] The two fluid channels of the first fluid channel pair 122A can be spaced apart from each other. The two fluid channels of the first fluid channel pair 122A can be spaced apart from each other by about 0.1 mm to about 1.0 mm. The two fluid channels of the second fluid channel pair 122B can be spaced apart from each other. The two fluid channels of the second fluid channel pair 122B can be spaced apart from each other by about 0.1 mm to about 1.0 mm.
[0076] In some embodiments, the first fluid channel pair 122A and the second fluid channel pair 122B can be positioned substantially opposite one another in the optical portion 102. The first fluid channel pair 122A can be positioned substantially opposite the second fluid channel pair 122B.
[0077] The first fluid channel pair 122A and the second fluid channel pair 122B can be defined or extend through a portion of the optical portion 102. The first fluid channel pair 122A and the second fluid channel pair 122B can be defined or extend through the posterior element 108.
[0078] The design with two fluid channels 122 rather than one channel helps maintain dimensional stability during assembly, which can be important when assembling flexible, thin components. Additionally, through experimentation, it has been observed that the design with two fluid channels 122 provides better optical quality throughout the adjustment range than certain one-channel designs. The two fluid channel design is stiffer, resulting in less deflection due to pressure changes within the fluid channels.
[0079] 1D, the optical portion 102 can include a first reinforcement portion 126A and a second reinforcement portion 126B on substantially opposite sides of the optical portion 102 or substantially diametrically opposed to each other. The first fluid channel pair 122A can be defined or formed in the first reinforcement portion 126A. The second fluid channel pair 122B can be defined or formed in the second reinforcement portion 126B.
[0080] The fluid channel pair 122 (e.g., either the first fluid channel pair 122A or the second fluid channel pair 122B) can have an inner opening pair 128 disposed at one end of the fluid channel 122 and another outer opening pair 130 disposed at the other end of the fluid channel 122. The inner opening pair 128 can be defined or formed in a portion of the rear element 108. As shown in FIGS. 1B-1D , the inner opening 128 can be defined or formed in a portion of a raised inner surface 132 of the rear element 108. In some embodiments, the raised inner surface 132 can be an angled or chamfered surface.
[0081] The outer aperture pair 130 can be defined or formed in a portion of a protruding outer surface 134 of the posterior element 108. The protruding outer surface 134 can be a portion of the reinforcement portion 126. The protruding outer surface 134 can also be a portion of the haptic-optical portion interface 124.
[0082] For example, Figure 1D shows one inner opening pair 128 disposed at one end of the first fluid channel pair 122A and defined along the raised inner surface 132 of the rear element 108. Figure 1D also shows one outer opening pair 130 serving as an end of the second channel pair 122B and defined along the protruding outer surface 134 of the rear element 108. The outer opening pair 130 of the first fluid channel pair 122B and the inner opening pair 128 of the second fluid channel pair 122B are obscured in Figure 1D.
[0083] The two openings of the inner opening pair 128 can be spaced apart from each other by about 0.1 mm to about 1.0 mm. The two openings of the outer opening pair 130 can be spaced apart from each other by about 0.1 mm to about 1.0 mm. The inner opening pair 128 of the first fluid channel pair 122A can be positioned directly opposite or on the opposite side of the rising inner surface 132 from the inner opening pair 128 of the second fluid channel pair 122B.
[0084] FIG. 1D also shows that each of the haptics 104 (e.g., the first haptic 104A or the second haptic 104B) can have an optical portion attachment end 136 and a closed free end 138. A haptic fluid port 140 can be defined at the optical portion attachment end 136 of the haptic 104. The haptic fluid port 140 can serve as a chamber mouth of the haptic fluid chamber 120. When the haptic 104 is coupled to the optical portion 102, the fluid in the haptic fluid chamber 120 can flow out of the haptic fluid chamber 120 through the haptic fluid port 140 and into the optical portion fluid chamber 110 via the fluid channel pair 122. Similarly, the fluid in the optical portion fluid chamber 110 can flow out of the optical portion fluid chamber 110 through the fluid channel pair 122 and into the haptic fluid chamber 120 through the haptic fluid port 140.
[0085] 1A and 1D, haptics 104 can be coupled to optic portion 102 at reinforcement portion 126. For example, a first haptic 104A can be coupled or attached to optic portion 102 at first reinforcement portion 126A, and a second haptic 104B can be coupled or attached to optic portion 102 at second reinforcement portion 126B.
[0086] More specifically, the haptic attachment end 136 can be coupled to a protruding outer surface 134 of the posterior element 108. The protruding outer surface 134 can also be referred to as a "landing" or a "haptic attachment landing." The protruding outer surface 134 can extend radially outward from an outer circumferential surface 142 of the optic portion 102. For example, the protruding outer surface 134 can extend radially outward from an outer circumferential surface 142 of the posterior element 108 of the optic portion 102. The protruding outer surface 134 can extend radially outward from the outer circumferential surface 142 by between about 10 micrometers and 1.0 mm, or between about 10 micrometers and 500 micrometers.
[0087] The haptic attachment ends 136 have a substantially flat surface and can be glued or otherwise coupled to the substantially flat surface of the protruding outer surface 134. When the haptic attachment ends 136 are coupled to the protruding outer surface 134, the haptic fluid ports 140 can surround the outer surface 130 of the fluid channel 122. The haptics 104 can be coupled or bonded to the optical portion 102 by a biocompatible adhesive 148. In some embodiments, the adhesive 148 can be the same adhesive used to couple or bond the anterior element 106 to the posterior element 108. The adhesive 148 is discussed in more detail in the following section.
[0088] Each of the haptics 104 can also include a radially outer portion 144 configured to face and contact an inner surface of the capsular bag when the AIOL 100 is implanted in the patient's capsular bag. Each of the haptics 104 can also include a radially inner portion 146 configured to face an outer circumferential surface 142 of the optic portion 102. The engagement of the radially outer portions 144 of the haptics 104 with the capsular bag is discussed in more detail in the following section.
[0089] The optic portion 102 can have a base power or a base spherical power. The base power of the optic portion 102 can be configured to change based on the internal fluid pressure within the fluid-filled optic portion fluid chamber 110. The base power of the optic portion 102 can be configured to increase or decrease as fluid enters or exits the fluid-filled optic portion fluid chamber 110.
[0090] The base power of the optic portion 102 can be configured to increase as fluid enters the fluid-filled optic portion fluid chamber 110 from the haptic fluid chamber 120, as shown in Figure 1B. The base power of the optic portion 102 can be configured to decrease as fluid exits or is withdrawn from the fluid-filled optic portion fluid chamber 110 and into the haptic fluid chamber 120, as shown in Figure 1C.
[0091] It should be noted that while Fig. 1B uses curved dashed arrows to show fluid entering the optical portion fluid chamber 110 from the haptic fluid chamber 120, the fluid enters the optical portion fluid chamber 110 via the fluid channel 122 (including through the inner opening 128 and the outer opening 130) and via the haptic fluid port 140. It should also be noted that while Fig. 1C uses curved dashed arrows to show fluid leaving the optical portion fluid chamber 110 and entering the haptic fluid chamber 120, the fluid exits the optical portion fluid chamber 110 via the fluid channel 122 (including through the inner opening 128 and the outer opening 130) and via the haptic fluid port 140.
[0092] The optic portion 102 can be made, in part, of a deformable or flexible material. In some embodiments, the optic portion 102 can be made, in part, of a deformable or flexible polymer material. For example, the anterior element 106, the posterior element 108, or a combination thereof, can be made, in part, of a deformable or flexible polymer material. One or more haptics 104 (e.g., the first haptic 104A, the second haptic 104B, or a combination thereof) can be made, in part, of the same deformable or flexible material as the optic portion 102. In other embodiments, the one or more haptics 104 can be made, in part, of a different material than the optic portion 102.
[0093] In some embodiments, the optic portion 102 can include or be made in part of a lens body material. The lens body portion can be made in part of a cross-linked copolymer, including a copolymer blend. The copolymer blend can include an alkyl acrylate or methacrylate, a fluoroalkyl (meth)acrylate, and a phenyl-alkyl acrylate. It is contemplated by this disclosure and should be understood by those skilled in the art that these types of acrylic cross-linked copolymers can generally be copolymers of multiple acrylates, methacrylates, or combinations thereof, and the term "acrylate," as used herein, can be understood to mean interchangeable acrylates, methacrylates, or combinations thereof, unless otherwise specified. The cross-linked copolymers used to make the lens body material can include an alkyl acrylate in an amount of about 3% to 20% (wt%), a fluoroalkyl acrylate in an amount of about 10% to 35% (wt%), and a phenyl-alkyl acrylate in an amount of about 50% to 80% (wt%). In some embodiments, the crosslinked copolymer can include or be made, in part, of n-butyl acrylate as the alkyl acrylate, trifluoroethyl methacrylate as the fluoro-alkyl acrylate, and phenylethyl acrylate as the phenyl-alkyl acrylate. More specifically, the crosslinked copolymer used to make the lens body material can include n-butyl acrylate in an amount of about 3%-20% (wt%) (e.g., about 12%-16%), trifluoroethyl methacrylate in an amount of about 10%-35% (wt%) (e.g., about 17%-21%), and phenylethyl acrylate in an amount of about 50%-80% (wt%) (e.g., about 64%-67%).
[0094] The final composition of the crosslinked copolymer used to make the lens body material may also include a crosslinker or crosslinking agent, such as ethylene glycol dimethacrylate (EGDMA). For example, the final composition of the crosslinked copolymer used to make the lens body material may also include a crosslinker or crosslinking agent (e.g., EGDMA) in an amount of about 1.0%. The final composition of the crosslinked copolymer used to make the lens body material may also include an initiator or initiator agent (e.g., Perkadox 16) and a UV absorber.
[0095] Haptics 104 can include or be made, in part, of a haptic material. The haptic material can include or be made, in part, of a cross-linked copolymer, including a copolymer blend. The copolymer blend can include an alkyl acrylate, a fluoroalkyl acrylate, and a phenyl-alkyl acrylate. For example, a cross-linked copolymer used to make the haptic material can include an alkyl acrylate in an amount of about 10%-25% (wt%), a fluoroalkyl acrylate in an amount of about 10%-35% (wt%), and a phenyl-alkyl acrylate in an amount of about 50%-80% (wt%). In some embodiments, the crosslinked copolymer used to make the haptic material can include n-butyl acrylate in an amount of about 10% to 25% (wt%) (e.g., about 19% to 23%), trifluoroethyl methacrylate in an amount of about 10% to 35% (wt%) (e.g., about 14% to 18%), and phenylethyl acrylate in an amount of about 50% to 80% (wt%) (e.g., about 58% to 62%). The final composition of the crosslinked copolymer used to make the haptic material can also include a crosslinker, i.e., a crosslinking agent, such as EGDMA, in an amount of about 1.0%. The final composition of the crosslinked copolymer used to make the haptic material can also include a number of photoinitiators, i.e., photopolymerization initiators, such as camphorquinone, 1-phenyl-1,2-propanedione, and 2-ethylhexyl-4-(dimethylamino)benzo.
[0096] In some embodiments, the refractive index of the lens body material can be from about 1.48 to about 1.53. In certain embodiments, the refractive index of the lens body material can be from about 1.50 to about 1.53 (e.g., about 1.5178).
[0097] The optic portion 102 can be configured to deform, deflect, or otherwise change shape in response to fluid entering or exiting the optic portion fluid chamber 110 (see FIGS. 1B and 1C). The optic portion 102 can be configured to deform, deflect, or otherwise change shape as a result of a material composition (e.g., a polymer composition) of the optic portion 102 described above. The haptics 104 can also be configured to deform, or otherwise change shape in response to interaction or engagement with a patient's lens capsule when the AIOL 100 is implanted within the patient's eye. The haptics 104 can be configured to deform, or otherwise change shape as a result of a material composition of the haptics 104.
[0098] In some embodiments, the anterior element 106 can be configured to deform, deflect, or otherwise change shape in response to fluid entering or exiting the optical portion fluid chamber 110. In other embodiments, the posterior element 108 can be configured to deform, deflect, or otherwise change shape (e.g., change its curvature) in response to fluid entering or exiting the optical portion fluid chamber 110. In another embodiment, both the anterior element 106 and the posterior element 108 can be configured to deform, deflect, or otherwise change their shape in response to fluid entering or exiting the optical portion fluid chamber 110.
[0099] In some embodiments, the fluid in the optical portion fluid chamber 110, the haptic fluid chamber 120, or a combination thereof can be an oil. More specifically, in certain embodiments, the fluid in the optical portion fluid chamber 110, the haptic fluid chamber 120, or a combination thereof can be a silicone oil or fluid. The fluid can flow between the optical portion fluid chamber 110 and the haptic fluid chamber 120 in response to a deformation, deflection, or shape change of the haptics 104, the components of the optical portion 102 (e.g., the anterior element 106, the posterior element 108, or a combination thereof), or a combination thereof.
[0100] The fluid in the optical portion fluid chamber 110, the haptic fluid chamber 120, or a combination thereof can be a silicone oil or fluid that includes or is made, in part, from diphenylsiloxane. In other embodiments, the silicone or fluid can include or be made, in part, from a ratio of two units of dimethylsiloxane to one unit of diphenylsiloxane. More specifically, in some embodiments, the silicone oil or fluid can be diphenyltetramethylcyclotrisiloxane. In additional embodiments, the silicone oil or fluid can include or be made, in part, from a diphenylsiloxane and dimethylsiloxane copolymer.
[0101] The fluid (e.g., silicone oil) can have a refractive index that matches the lens body material used to fabricate the optical portion 102. When the fluid has a refractive index that matches the lens body material, the entire optical portion 102 including the fluid functions as a lens. For example, the fluid can be selected to have a refractive index of about 1.48 to 1.53 (or about 1.50 to 1.53). In some embodiments, the fluid (e.g., silicone oil) can have a polydispersity index of about 1.2 to 1.3. In other embodiments, the fluid (e.g., silicone oil) can have a polydispersity index of about 1.3 to 1.5. In other embodiments, the fluid (e.g., silicone oil) can have a polydispersity index of about 1.1 to 1.2. Other examples of fluids are described in U.S. Patent Application Publication No. 2018 / 0153682, the entire contents of which are incorporated herein by reference.
[0102] The base power of the optic portion 102 can be configured to change in response to a shape-changing component of the optic portion 102 (e.g., the anterior element 106, the posterior element 108, or a combination thereof). The optic portion 102 can be configured to change shape in response to physiological muscle movements (e.g., ciliary muscle movements) that occur in the patient when the AIOL 100 is implanted in the capsular bag of a patient's eye and the AIOL 100 deforms or changes shape in response to deformation of the capsular bag associated with the ciliary muscle.
[0103] The AIOL 100 can be implanted or introduced into a patient's natural lens after removal from the capsule. The patient's capsule is connected to the zonules, which are connected to the patient's ciliary muscles. The capsule is elastic and can be deformed by ciliary muscle movement via the zonules. For example, when the ciliary muscles relax, the zonules stretch. This stretching pulls the capsule generally radially outward with a radially outward force. This tension on the capsule lengthens the capsule and creates space within the capsule. When the patient's natural lens is within the capsule, the natural lens is typically flattened (in the anterior-posterior direction), which reduces the refractive power of the lens and allows distance vision. In this state, the patient's natural lens is said to be in a disaccommodated state or to be disaccommodated.
[0104] However, when the ciliary muscle contracts, as occurs when the eye attempts to focus on a nearby object, the radially inner portion of the muscle moves radially inward and the zonules relax. Relaxation of the zonules causes the elastic lens to contract and exert a radially inward force on the lens within the lens. When the patient's natural lens is within the capsular bag, the natural lens is typically more curved (e.g., the anterior portion of the lens is more curved), which allows the lens to have more refractive power and enables the eye to focus on nearby objects. In this state, the patient's natural lens is said to be in accommodation, or accommodating.
[0105] Therefore, any AIOL implanted within the capsular bag should also have a mechanism that allows the base power of the AIOL to be increased when the ciliary muscle contracts and decreased when the ciliary muscle relaxes.
[0106] In this case, when the AIOL 100 is implanted or otherwise introduced into the patient's natural lens capsule, the radially outer portions 144 of the haptics 104 of the AIOL 100 can directly engage or physically contact the portions of the lens capsule that connect to the ciliary zonules, i.e., the zonules of Zinn. Thus, the radially outer portions 144 of the haptics 104 can be configured to respond to radially applied lens capsule deformation forces as the zonules relax and stretch as a result of ciliary muscle movement.
[0107] When the ciliary muscles contract, the peripheral region of the elastic lens capsule deforms and exerts a radially inward force on the radially outer portion 144 of the haptic 104 (e.g., the elastic lens capsule exerts a radially inward force on the radially outer portion 144 of the first haptic 104A and the radially outer portion 144 of the second haptic 104B). The radially outer portion 144 of the haptic 104 then deforms or otherwise changes shape, and this deformation or change in shape reduces the volume of the haptic fluid chamber 120. The reduction in the volume of the haptic fluid chamber 120 causes the fluid in the haptic fluid chamber 120 to be displaced or forced into the optical portion fluid chamber 110 in the optical portion 102. As previously described, the fluid moves from the haptic fluid chamber 120 to the optical portion fluid chamber 110 through a fluid channel 122 (e.g., a fluid channel pair 122) formed in the optical portion 102.
[0108] The optic portion 102 (either the anterior element 106, the posterior element 108, or a combination thereof) can change shape (increase its curvature) in response to fluid entering the optic portion fluid chamber 110 from the haptic fluid chamber 120. This increases the base power or base spherical power of the AIOL 100, thereby enabling a patient having the AIOL 100 implanted in their eye to focus on nearby objects. The AIOL 100 can also be considered to be in an accommodated state or to have accommodated.
[0109] When the ciliary muscles relax, the peripheral region of the elastic capsule stretches radially outward, lengthening the capsule and creating more space within the capsule. The radially outer portions 144 of the haptics 104 can be configured to respond to this deformation of the capsule by returning to their undeformed or unstressed state. This causes the volume of the haptic fluid chamber 120 to increase or return to its undeformed volume. This increase in the volume of the haptic fluid chamber 120 causes the fluid in the optical portion fluid chamber 110 to be drawn or otherwise discharged from the optical portion fluid chamber 110 and returned to the haptic fluid chamber 120. As previously described, the fluid travels out of the optical portion fluid chamber 110 and into the haptic fluid chamber 120 through the same fluid channels 122 (e.g., fluid channel pairs 122) formed in the optical portion 102.
[0110] As previously mentioned, the optic portion 102 (either the anterior element 106, the posterior element 108, or a combination thereof) can change shape (reduce its curvature or become flatter) in response to fluid exiting the optic portion fluid chamber 110 and entering the haptic fluid chamber 120. This reduces the base power or base spherical power of the AIOL 100, thereby enabling a patient having the AIOL 100 implanted in their eye to focus on distant objects or obtain distance vision. The AIOL 100 can also be considered to be in a disaccommodated state or to be disaccommodated.
[0111] As shown in Figures 1B and 1C, the radially inner portion 146 of the haptic 104 can be designed to be thicker or bulkier (relative to the radially outer portion 144) to provide the haptic 104 with rigidity or resilience in the anterior-posterior direction. In this way, when a capsular force is applied to the haptic 104 in the anterior-posterior direction, less deformation occurs and less fluid movement occurs between the haptic fluid chamber 120 and the optical portion fluid chamber 110 than if the force was applied in the radial direction. Because less fluid movement occurs, a smaller change in the base power of the AIOL 100 occurs when a force is applied to the AIOL 100 in the anterior-posterior direction. Therefore, the design and material properties of the haptic 104 and the optical portion 102 allow the AIOL 100 to maintain high sensitivity to radial forces applied to the haptic 104 by capsular deformation caused by ciliary muscle movement.
[0112] The anterior element 106 may be attached or otherwise adhered to the posterior element 108 by an adhesive 148 or adhesive layer. In addition, the haptics 104 may also be attached to the optic portion 102 by an adhesive 148.
[0113] The adhesive layer can be substantially annular in shape. The adhesive 148 or adhesive layer can be positioned on a peripheral edge 150 (see FIG. 1D ) of the optic portion 102 between the anterior element 106 and the posterior element 108. For example, the adhesive 148 can be positioned on the elevated inner surface 132 of the posterior element 108.
[0114] The adhesive 148 or adhesive layer may include or be made, in part, of a biocompatible adhesive. The adhesive 148 or adhesive layer may include or be made, in part, of a biocompatible polymer adhesive.
[0115] The adhesive 148 or adhesive layer may include or be made, in part, of a cross-linkable polymer precursor formulation that may include or be made, in part, of a copolymer blend, a hydroxyl functional acrylic monomer, and a photoinitiator.
[0116] The copolymer blend can include an alkyl acrylate (e.g., n-butyl acrylate in an amount of about 41% to about 45% (wt%)), a fluoro-alkyl acrylate (e.g., trifluoroethyl methacrylate in an amount of about 20% to about 24% (wt%)), and a phenyl-alkyl acrylate (phenylethyl acrylate in an amount of about 28% to about 32% (wt%)). The hydroxyl functional acrylic monomer can be 2-hydroxyethyl acrylate (HEA). A photoinitiator can be used to facilitate curing of the adhesive. For example, the photoinitiator can be Darocur 4265 (a 50 / 50 blend of diphenyl(2,4,6-trimethylbenzoyl)phosphine oxide and 2-hydroxy 2-methylpropiophenone).
[0117] The first step in the adhesive manufacturing process is the preparation of a hydroxyl-functional polymer precursor by photopolymerizing a crosslinkable polymer precursor formulation to obtain a cured composition. The second step is the chemical conversion of the precursor polymer pendant hydroxyl moieties, or hydroxyl pendant groups, to pendant methacrylate functional groups by reacting with methacrylic anhydride or methacrylic chloride, thereby forming a methacrylate- or methacrylic-functional crosslinkable polymer, including alkyl acrylates or methacrylates (e.g., n-butyl acrylate), fluoro-alkyl (meth)acrylates (e.g., trifluoroethyl methacrylate), phenyl-alkyl acrylates (phenylethyl acrylate), and 2-(2-methyl-acryloyloxy)ethyl acrylate.
[0118] The methacrylic functional crosslinkable polymer can be blended with a reactive acrylic monomer diluent, such as 1-adamantyl methacrylate (ADMA), and a photoinitiator, such as Darocur 4265. For example, the final composition of the adhesive 148 can include the crosslinkable polymer precursor formulation in an amount of about 50% to about 85% (wt%) (e.g., about 61% to about 65%), the reactive acrylic monomer diluent in an amount of about 10% to about 40% (wt%) (32% to about 36%), and the photoinitiator, such as Darocur 4265, in an amount of about 2% to about 3% (wt%).
[0119] The adhesive 148 or adhesive layer can bond, adhere, or otherwise join the anterior element 106 to the posterior element 108. As discussed in more detail in the following section, the thickness of the adhesive layer can be adjusted after implantation to adjust the base power of the AIOL 100.
[0120] In some embodiments, the same adhesive 148 used to bond the anterior element 106 to the posterior element 108 can also be used to bond or secure the peripheral portion 103 (e.g., one or more haptics 104) to the optical portion 102.
[0121] 2A illustrates one embodiment of a first mold component 200 including a first molding surface 202 defined by a first component cavity portion 204. The first component cavity portion 204 may be a depression or recess defined along the first molding surface 202. The first component cavity portion 204 may be shaped, sized, or otherwise configured to receive a portion of a fusible core component 236 (see FIGS. 2D and 3A-3B). In some embodiments, the first mold component 200 may also be referred to as a wafer mold.
[0122] In some embodiments, the first component cavity portion 204 can be connected to or continuous with the first positioning cavity portion 206. For example, the first component cavity portion 204 can be in fluid communication with the first positioning cavity portion 206. In other embodiments, the first component cavity portion 204 can be positioned proximate to the first positioning cavity portion 206. For example, the first component cavity portion 204 can be proximate to the first positioning cavity portion 206 but not directly connected to the first positioning cavity portion 206.
[0123] The first component cavity portion 204 can be shaped, sized, or otherwise configured to receive at least a portion of the core body 238 (see FIGS. 2D and 3A-3B) of the fusible core component 236. For example, the first component cavity portion 204 can be shaped, sized, or otherwise configured to receive the aft half of the core body 238 of the fusible core component 236.
[0124] The first positioning cavity portion 206 can be shaped, sized, or otherwise configured to receive a positioning piece 240 (see FIGS. 2D and 3A-3B) of the fusible core component 236. For example, the first positioning cavity portion 206 can be shaped, sized, or otherwise configured to receive a front half of the positioning piece 240 of the fusible core component 236.
[0125] Although Figures 2A and 2D show the first mold component 200 including one first positioning cavity 206, it is envisioned in the present disclosure that the first mold component 200 may include multiple first positioning cavity portions 206 for accommodating multiple positioning parts 240.
[0126] In some embodiments, the first component cavity portion 204 can terminate at a first cavity distal end 208. The first cavity distal end 208 can be positioned away from the first positioning cavity portion 206. The first cavity distal end 208 can be positioned closer to the first mold component wall 212 than the first positioning cavity portion 206. In these embodiments, the first cavity distal end 208 does not contact the first mold component wall 212.
[0127] In certain embodiments, the first cavity distal end 208 can be rounded or curved. For example, the first cavity distal end 208 can be substantially in the shape of an oval or a portion of an ellipsoid. The first cavity distal end 208 can be substantially in the shape of a portion of a sphere.
[0128] 2A , in other embodiments contemplated by the present disclosure, the first component cavity portion 204 can be connected to other positioning cavity portions rather than terminating in a closed distal end. In these embodiments, the first component cavity portion 204 can be disposed between two positioning cavity portions.
[0129] 2A, the first mold component 200 can also include a number of leg cavities 210 defined along the first molding surface 202. The leg cavities 210 can be divots or depressions configured to receive legs or other support structures extending from a complementary mold component (e.g., a second mold component 218, see FIG. 2B).
[0130] The leg cavities 210 may surround or be positioned radially outward of the first component cavity portion 204. The leg cavities 210 may be arranged in a particular pattern or positioned in a particular manner such that a complementary mold component (e.g., second mold component 218) may be aligned with the first mold component 200. For example, the leg cavities 210 may be arranged in a particular pattern or aligned in a particular manner such that the first component cavity portion 204 may be matched or otherwise aligned with a second component cavity portion 222 (e.g., see FIG. 2B ) on the second mold component. The first component cavity portion 204 may be properly aligned with the second component cavity portion 222 when the leg or other support structure of the second mold component 218 is inserted or placed into the leg cavity 210 of the first mold component 200.
[0131] 2A, the leg cavities 210 can be arranged in a substantially triangular pattern. Although not shown, in other embodiments contemplated by this disclosure, the leg cavities 210 can be arranged in a circular pattern, a diamond or lozenge pattern, a square pattern, or other polygonal pattern.
[0132] The first molding surface 202 can be recessed or sunken with respect to the first mold component wall 212. The sunken or sunken first molding surface 202 can create a storage space 214 within the first mold component 200. The storage space 214 can receive lens component material when the entire mold is assembled.
[0133] 2A, in one embodiment, the first mold component 200 can be configured as a circular cap or a circular mold section. In this embodiment, the first mold component wall 212 can be substantially in the shape of the side of a cylinder. Additionally, the first molding surface 202 can also be substantially circular.
[0134] In other embodiments, the first mold component 200 can be configured as a rectangular cap or a rectangular mold section. In these embodiments, the first mold component wall 212 can be substantially in the shape of the side of a rectangular solid. Additionally, the first molding surface 202 can also be substantially rectangular.
[0135] In another embodiment, first mold component 200, including first molding surface 202 and first mold component wall 212, can be elliptical or ellipsoidal in shape. In an additional embodiment, first mold component 200, including first molding surface 202 and first mold component wall 212, can be triangular or other type of polygonal in shape.
[0136] The first mold component 200 may also include a number of engagement features 216 extending radially outward from the first mold component wall 212. In some embodiments, the engagement features 216 may be tabs or flaps extending radially outward from the first mold component wall 212. In other embodiments, the engagement features 216 may include threads or thread patterns defined on an outer surface of the first mold component wall 212. The engagement features 216 may allow the first mold component 200 to more easily engage or couple with a clamping member 232 (see, e.g., FIG. 2C ) for securing or holding the assembly mold together.
[0137] 2B illustrates an embodiment of a second mold component 218 that includes a second molding surface 220 defined by a second component cavity portion 222. The second component cavity portion 222 may be a depression or recess defined along the second molding surface 220. The second component cavity portion 222 may be shaped, sized, or otherwise configured to receive a portion of the fusible core component 236. In some embodiments, the second mold component 218 may also be referred to as a wafer mold.
[0138] Second molding surface 220 can be configured or otherwise designed to face first molding surface 202 (see FIG. 2E) when second mold component 218 is mated with first mold component 200 to form assembly mold 250. Second molding surface 220 can be positioned on the underside of second mold component 218 (the underside faces up in FIG. 2B).
[0139] In some embodiments, the second component cavity portion 222 can be connected to or contiguous with the second positioning cavity portion 224. For example, the second component cavity portion 222 can be in fluid communication with the second positioning cavity portion 224. In other embodiments, the second component cavity portion 222 can be positioned proximate to the second positioning cavity portion 224. For example, the second component cavity portion 222 can be proximate to the second positioning cavity portion 224 but not directly connected to the second positioning cavity portion 224.
[0140] The second component cavity portion 222 can be shaped, sized, or otherwise configured to receive at least a portion of the core body 238 of the fusible core component 236. For example, the second component cavity portion 222 can be shaped, sized, or otherwise configured to receive a front half of the core body 238 of the fusible core component 236.
[0141] Additionally, the second positioning cavity portion 224 can be shaped, sized, or otherwise configured to receive at least a portion of the positioning piece 240 of the fusible core component 236. For example, the second positioning cavity portion 224 can be shaped, sized, or otherwise configured to receive the rear half of the positioning piece 240 of the fusible core component 236.
[0142] Although FIG. 2B shows the second mold component 218 including one second positioning cavity portion 224, it is envisioned in the present disclosure that the second mold component 218 may include multiple second positioning cavity portions 224 for accommodating multiple positioning parts 240.
[0143] In some embodiments, the second component cavity portion 222 can terminate at a second cavity distal end 226. The second cavity distal end 226 can be positioned away from the second positioning cavity portion 224. The second cavity distal end 226 can be positioned closer to the edge or periphery of the second molding surface 220 than the second positioning cavity portion 224. In these embodiments, the second cavity distal end 226 does not reach the edge of the second molding surface 220.
[0144] In certain embodiments, the second cavity distal end 226 can be rounded or curved. For example, the second cavity distal end 226 can be shaped substantially as an oval or a portion of an ellipsoid. The second cavity distal end 226 can be shaped substantially as a portion of a sphere.
[0145] 2B, in other embodiments contemplated by the present disclosure, the second component cavity portion 222 can be connected to other positioning cavity portions rather than terminating in a closed distal end. In these embodiments, the second component cavity portion 222 can be disposed between two positioning cavity portions.
[0146] The second mold component 218 can also include a number of legs 228 or support structures that protrude or otherwise extend from the second molding surface 220. In some embodiments, the legs 228 can protrude or extend substantially perpendicularly or perpendicularly from the second molding surface 220. The legs 228 of the second mold component 218 can fit into the leg cavities 210 of the first mold component 200 when the second mold component 218 is mated or otherwise coupled with the first mold component 200.
[0147] 2B, the legs 228 can surround or be positioned radially outward from the second component cavity portion 222. The legs 228 can be arranged in a particular pattern or aligned in a particular manner so that the second mold component 218 is properly aligned with the first mold component 200. For example, the legs 228 can be arranged in a particular pattern or aligned in a particular manner so that the first component cavity portion 204 can match or otherwise align with the second component cavity portion 222. The first component cavity portion 204 can properly align with the second component cavity portion 222 when the legs 228 of the second mold component 218 are inserted or placed into the leg cavities 210 of the first mold component 200.
[0148] 2B, the legs 228 can be arranged in a substantially triangular pattern. Although not shown, in other embodiments contemplated by this disclosure, the legs 228 can be arranged in a circular pattern, a diamond or lozenge pattern, a square pattern, or other polygonal pattern.
[0149] 2B, in one embodiment, the second mold component 218 can be configured as a circular mold section. In this embodiment, the second molding surface 220 can also be substantially circular.
[0150] In other embodiments, the second mold component 218 can be configured as a rectangular mold section. In these embodiments, the second molding surface 220 can also be substantially rectangular.
[0151] In another embodiment, the second mold component 218 including the second molding surface 220 can be oval or elliptical. In an additional embodiment, the second mold component 218 including the second molding surface 220 can be triangular or other type of polygonal.
[0152] In some embodiments, the second mold component 218 can be sized to fit within the storage space 214 of the first mold component 200. At least a portion of the second mold component 218 can fit within the storage space 214 when the first mold component 200 is mated or otherwise coupled with the second mold component 218.
[0153] The first component cavity portion 204 and the second component cavity portion 222 can come together to form a component mold cavity when the first mold component 200 is mated or otherwise coupled with the second mold component 218. For example, the first mold component 200 can come together with the second mold component 218 when the first mold component 200 is fastened to the second mold component 218. Additionally, the first positioning cavity portion 206 and the second positioning cavity portion 224 can come together to form a positioning cavity when the first mold component 200 is mated or otherwise coupled with the second mold component 218.
[0154] The component mold cavity can be in fluid communication with the storage space 214 of the first mold component 200. The lens component material can seep into the component mold cavity from the storage space 214. The low viscosity lens component material can seep into the component mold cavity through the parting line between the first mold component 200 and the second mold component 218. The lens component material can be drawn from the storage space 214 into the component mold cavity when the assembly mold 250 is placed in a vacuum chamber and a vacuum is pulled.
[0155] The second mold component 218 may also include a vent 230 or opening that connects the second positioning cavity portion 224 to an edge or periphery of the second mold component 218. The vent 230 allows air to escape when the component mold cavity is being filled with a low viscosity lens component material.
[0156] In some embodiments, the lens component material can be a haptic material as disclosed in the previous section. For example, the lens component material can include a curable acrylic monomer. The lens component material can be a substantially hydrophobic material.
[0157] 2C illustrates one embodiment of a clamp member 232 for securing the first mold component 200 to the second mold component 218. In the exemplary embodiment illustrated in FIG 2C, the clamp member 232 can be a clamp cap configured to be removably secured to the top of the first mold component 200 when the second mold component 218 is mated with the first mold component 200.
[0158] As mentioned above, the first mold component 200 can include a number of engagement features 216 that extend radially outward from the first mold component wall 212. In some embodiments, the engagement features 216 can be tabs or flaps that extend radially outward from the first mold component wall 212. The clamp member 232 can include a number of grooves 234 or notches for mating with or otherwise receiving the engagement features 216.
[0159] In other embodiments, the engagement feature 216 can include a thread or thread pattern defined on an exterior surface of the first mold component wall 212. In these embodiments, the clamp member 232 can include a complementary thread pattern to allow the clamp member 232 to be threadably coupled to the first mold component 200.
[0160] In another embodiment, the clamping member 232 can be a conventional clamp or vice type device for securely securing the first mold component 200 to the second mold component 218 .
[0161] The clamping members 232 can rigidly secure the first mold component 200 to the second mold component 218 to prevent the various mold parts from shifting or moving relative to one another. The clamping members 232 can rigidly secure the first mold component 200 to the second mold component 218 during the curing step to prevent the lens component material from seeping out of the mold parting line. The clamping members 232 can be coupled to the first mold component 200 to form a closed chamber. Although not shown in FIG. 2C , if the clamping members 232 are implemented as a clamp cap, the clamp cap can have a septum or inlet port defined along a surface (e.g., a top surface) of the clamp cap. An injection nozzle or other delivery device can be inserted through the septum or inlet port to inject or otherwise introduce the curable lens component material into the storage space 214 within the closed chamber.
[0162] In some embodiments, the clamping members 232 can be made, in part, of a polymeric material, a metallic material, or a combination thereof. In another embodiment, the clamping members 232 can be made, in part, of a ceramic material. The clamping members 232 can be disengaged or separated from the first mold component 200 after the curing step. The clamping members 232 can be disengaged or separated from the first mold component 200 prior to separating the first mold component 200 from the second mold component 218.
[0163] 2D illustrates that at least a portion of the soluble core component 236 can be disposed on the first molding surface 202 of the first mold component 200. Although FIG. 2D illustrates the soluble core component 236 disposed on the first molding surface 202, the present disclosure also contemplates that the soluble core component 236 can be initially disposed on the second molding surface 220 of the second mold component 218. In the following sections, any reference to disposing or positioning the soluble core component 236 on the first molding surface 202 of the first mold component 200 can also refer to disposing or positioning the soluble core component 236 on the second molding surface 220 of the second mold component 218. Additionally, while FIGS. 2A, 2B, and 2D illustrate mold components used to form the haptics of an AIOL, the present disclosure contemplates that similar types of mold components can also be used to form the optic portion of a lens.
[0164] If the lens component being formed is a haptic of an AIOL (e.g., any of the haptics 104 shown in FIGS. 1A-1D), the soluble core component 236 can include a core body 238 connected to at least one positioning member 240. In these embodiments, the core body 238 can terminate at a core distal end 242. The soluble core component 236 is discussed in more detail in the following section.
[0165] At least a portion of the positioning piece 240 of the soluble core component 236 can be pressed or inserted into the first positioning cavity portion 206 of the first mold component 200. The positioning piece 240 can be configured to fit securely within the first positioning cavity portion 206 when the positioning piece 240 is pressed or inserted into the first positioning cavity portion 206. The soluble core component 236 can be removably coupled to the first mold component 200 when the positioning piece 240 is pressed or inserted into the first positioning cavity portion 206.
[0166] In some embodiments, the positioning feature 240 of the soluble core component 236 can be the only portion of the soluble core component 236 that physically contacts the first molding surface 202. For example, the positioning feature 240 of the soluble core component 236 can physically contact a sunken or recessed portion of the first molding surface 202 that defines the first positioning cavity portion 206. In these embodiments, the remaining portions of the soluble core component 236 that are coupled to or extend from the positioning feature 240 (e.g., the curved core body 238 and the core distal end 242) do not physically contact the first molding surface 200 above the first molding surface 202 when the soluble core component 236 is removably coupled to the first mold component 200. For example, the core body 238 and the core distal end 242 can be raised or elevated by the positioning member 240 so that no portion of the core body 238 or the core distal end 242 is in physical contact with the first molding surface 202 .
[0167] In these embodiments, at least a portion of the core body 238 and the core distal end 242 may be positioned within the first component cavity portion 204 when the positioning piece 240 is forced or inserted into the first positioning cavity portion 206, but do not touch any portion of the first molding surface 202 that defines or serves as the walls and bottom of the first component cavity portion 204. In addition, no portion of the core body 238 of the fusible core component 236 extends beyond the contour or boundary of the first component cavity portion 204 when the positioning piece 240 is forced or inserted into the first positioning cavity portion 206. Furthermore, the first cavity distal end 208 may extend beyond or extend beyond the core distal end 242 of the fusible core component 236 when the positioning piece 240 is forced or inserted into the first positioning cavity portion 206. Moreover, the raised first mold component wall 212 can surround the fusible core component 236 when the positioning piece 240 is forced or inserted into the first positioning cavity portion 206 .
[0168] 2D also shows that the core body 238 of the fusible core component 236 can include a radially inner body portion 244 and a radially outer body portion 246. The radially inner body portion 244 can be a surface of the core body 238 that faces or is near the positioning component 240 when the positioning component 240 is pressed or inserted into the first component cavity portion 204 and the core body 238 is partially positioned within the first component cavity portion 204. The radially outer body portion 246 can be a surface of the core body 238 that faces away from the positioning component 240 when the positioning component 240 is pressed or inserted into the first component cavity portion 204 and the core body 238 is partially positioned within the first component cavity portion 204. The radially inner body portion 244 can be separated from an inner edge 248 of the first component cavity portion 204 by a radially inner separation distance. The inner edge 248 of the first component cavity portion 204 may be part of an inner contour or boundary of the first component cavity portion 204. The radially outer body portion 246 may be separated from an outer edge (not shown in FIG. 2D ) of the first component cavity portion 204 by a radially outer separation distance. The outer edge of the first component cavity portion 204 may be part of an outer contour or boundary of the first component cavity portion 204.
[0169] In some embodiments, the radially inner separation distance can be greater than the radially outer separation distance. This difference in separation distance allows a greater amount of lens component material to occupy the space separating the radially inner body portion 244 from the inner edge 248 than the space separating the radially outer body portion 246 from the outer edge of the first component cavity portion 204. This allows a haptic (see, e.g., haptic 104 in FIGS. 1B and 1C ) to be formed having a thicker radially inner portion (see, e.g., radially inner portion 146 in FIGS. 1B and 1C ) relative to the radially outer portion of the haptic (see, e.g., radially outer portion 144 of haptic 104 in FIGS. 1B and 1C ).
[0170] This unique positioning of the soluble core component 236 relative to the mold component allows the lens component material (e.g., haptic material) to enter and fill the space surrounding the soluble core component 236 in the component cavity. The haptic material can then be hardened to form a molded haptic surrounding the soluble core component 236. After the hardening process, the molded haptic, including the soluble core component 236 within the molded haptic, can then be immersed in a solvent to dissolve the soluble component 236. Once the soluble component 236 has dissolved, the space in the molded haptic formerly occupied by the soluble component 236 can act as a haptic fluid chamber (see, e.g., haptic fluid chamber 120 of haptic 104).
[0171] 2E illustrates that an assembly mold 250 can be formed by mating the second mold component 218 with the first mold component 200. The soluble core component 236 can be pressed or otherwise placed in place within the first mold component 200 prior to mating the second mold component 218 with the first mold component 200. The soluble core component 236 can be placed in place within the first mold component 200 by pressing or inserting the positioning piece 240 of the soluble core component 236 into the first positioning cavity portion 206 to position at least a portion of the core body 238 of the soluble core component 236 within the first component cavity portion 204. As previously mentioned, the soluble core component 236 can also be initially pressed or otherwise placed in place within the second mold component 218 prior to mating the two mold components with one another. The fusible core component 236 can be disposed between the first molding surface 202 and the second molding surface 220 when the assembly mold 250 is formed.
[0172] Mating the second mold component 218 with the first mold component 200 can include inserting the legs 228 of the second mold component 218 into the leg cavities 210 of the first mold component 200 and pressing the second mold component 218 against the first mold component 200. As previously described, the legs 228 of the second mold component 218 and the leg cavities 210 of the first mold component 200 can be positioned such that the first component cavity portion 204 of the first mold component 200 fits precisely over the second component cavity portion 222 of the second mold component 218. For example, a contour or boundary of the first component cavity portion 204 can align with a contour or boundary of the second component cavity portion 222 when the second mold component 218 is mated with the first mold component 200. Additionally, the contour or boundary of the first positioning cavity portion 206 may also align with the contour or boundary of the second positioning cavity portion 224 when the second mold component 218 is mated with the first mold component 200 .
[0173] The first component cavity portion 204 and the second component cavity portion 222 can form a component mold cavity when the assembly mold 250 is formed by mating the second mold component 218 with the first mold component 200. The core body 238 of the fusible core component 236 can be located within the component mold cavity when the second mold component 218 is mated with the first mold component 200. The positioning piece 240 of the fusible core component 236 can be located outside of the component mold cavity when the second mold component 218 is mated with the first mold component 200.
[0174] In some embodiments, the method of forming the assembly mold 250 may include the additional step of wetting at least one of the first molding surface 202 and the second molding surface 220 with a wetting agent prior to mating the second mold component 218 with the first mold component 200. Wetting the first molding surface 202, the second molding surface 220, or a combination thereof may include spraying, sponging, swabbing, or otherwise applying the wetting agent to the surface until the wetting agent uniformly coats the surface. In certain embodiments, the wetting agent may be water or deionized water. Wetting the first molding surface 202, the second molding surface 220, or a combination thereof may allow the first mold component 200 to bond more firmly to the second mold component 218 when at least one of the mold components is made of a water-soluble material. Wetting of the first molding surface 202, the second molding surface 220, or a combination thereof can prevent flash from occurring at the parting line created by the first mold component 200 and the second mold component 218 along the periphery of the molded lens component by sealing at least a portion of the interface between the first mold component 200 and the second mold component 218.
[0175] 2E shows that the second mold component 218 can fit within the storage space 214 of the first mold component 200 when the second mold component 218 is mated with the first mold component 200. A curable lens component material (e.g., haptic material or lens body material when the optic portion is formed) can be introduced (e.g., poured, injected, etc.) into the storage space 214 once the assembly mold 250 is formed. In some embodiments, the low viscosity lens component material can seep into the component mold cavity through the parting line between the first mold component 200 and the second mold component 218 when the mold components are mated with one another. In other embodiments, the lens component material can enter the component mold cavity through other openings or conduits defined along the second molding surface 220, the first molding surface 202, or a combination thereof.
[0176] As mentioned above, the clamp member 232 (see, e.g., FIG. 2C or FIG. 7) can be removably coupled to or secured to the first mold component 200 after the first mold component 200 is mated with the second mold component 218. For example, the clamp member 232 can be a clamp cap configured to be removably secured to the top of the first mold component 200 when the second mold component 218 is mated with the first mold component 200. The clamp cap can create a closed chamber and firmly press the second mold component 218 against the first mold component 200.
[0177] The curable lens component material can then be introduced into this closed chamber. For example, the lens component material can be injected or otherwise introduced into the storage space 214 through a septum 710 (see FIG. 7) or other opening defined along the clamping member 232. Once the lens component material has been introduced, the assembly mold 250, including the clamping member 232 coupled to the assembly mold 250, can be placed in a vacuum chamber. After the assembly mold 250 is placed in the vacuum chamber, a vacuum can be pulled to draw the lens component material into the component mold cavities. The low viscosity lens component material can seep into the component mold cavities through the parting line or tiny gap between the first mold component 200 and the second mold component 218. Under vacuum, the lens component material can fill any space in the assembly mold 250 that is not occupied by the soluble core component 236. For example, the lens component material can fill any space in the component mold cavities that is not occupied by the core body 238 of the soluble core component 236.
[0178] Once the lens component material fills the component mold cavities, the assembly mold 250 containing the lens component material may be cured in a curing chamber. In some embodiments, the assembly mold 250 may be cured using light, such as ultraviolet (UV) light or blue light.
[0179] More specifically, in some embodiments, the assembly mold 250 can be cured in a UV light chamber. For example, the assembly mold 250 can be cured using a UV-generating xenon lamp or a xenon mercury lamp. For example, the assembly mold 250 can be cured under UV light for 30 to 60 minutes. In other embodiments, the assembly mold 250 can be cured using blue light, such as light emitted by a high-intensity blue light-emitting diode (LED) light. For example, the assembly mold 250 can be cured under blue light for 10 to 12 hours. In other embodiments, the assembly mold 250 can also be cured using heat or a combination of light and heat.
[0180] A clamping member 232 can clamp the first mold component 200 to the second mold component 218 during the curing procedure. The lens component material can be cured into molded lens components, such as haptics. As discussed in more detail in the following sections, the lens component material can also be cured using other mold components into other molded lens components, such as molded optics.
[0181] In some embodiments, both the first mold component 200 and the second mold component 218 can be made of an insoluble material. An insoluble material can be a material that cannot be dissolved in a solvent (e.g., water) for a reasonable amount of time. For example, the first mold component 200 and the second mold component 218 can be made of an insoluble polymeric material. In some embodiments, the first mold component 200 and the second mold component 218 can be made of a thermoplastic resin, including polyolefins such as medium to high density polyethylene (PE), polypropylene (PE) or copolymers thereof, poly-4-methylpentene, and polystyrene. The first mold component 200 and the second mold component 218 can also be made of various nylons, including polyacetal resins, polyacrylic ethers, polyaryl ether sulfones, nylon 6, nylon 66, and nylon 11. As a more specific example, first mold component 200, second mold component 218, or a combination thereof, can be fabricated in part from a 4-methylpentene-1-based olefin copolymer, such as TPX™ polymethylpentene sold by Mitsui Chemicals, Inc.
[0182] In another embodiment, first mold component 200 and second mold component 218 can be fabricated from a corrosion-resistant metallic material, such as stainless steel.
[0183] In examples where both the first mold component 200 and the second mold component 218 are made of an insoluble material, the method of forming the lens component (e.g., haptics) can include separating the first mold component 200 from the second mold component 218 after the curing step, and removing the molded lens component from either the first mold component 200 or the second mold component 218. At least one segment of the soluble core component 236 can be within or partially surrounded by the molded lens component after the molded lens component is removed from the first mold component 200 or the second mold component 218. For example, the core body 238 of the soluble core component 236 can be within or partially surrounded by the molded lens component when the molded lens component is removed from the first mold component 200 or the second mold component 218. Additionally, the positioning piece 240 of the fusible core component 236 may be connected to the molded lens component, but is not contained or surrounded within the molded lens component.
[0184] The method may further include immersing the molded lens component in a solvent to dissolve the soluble core component 236. The method may also include heating the solvent to about 35° C.-55° C. and agitating the solvent by sonication or stirring to facilitate dissolution of the soluble core component 236. In some embodiments, the soluble core component 236 may dissolve after immersion in the solvent for about 6 hours to about 24 hours. What remains after the soluble core component dissolves is the molded lens component (e.g., the haptic or optic portion having a cavity defined therein).
[0185] As discussed in more detail in the following sections, the soluble component 236 can be made of a soluble material, such as polyvinyl alcohol. In some embodiments, the solvent can be water. The soluble component 236 and soluble materials are discussed in more detail in the following sections.
[0186] In some embodiments, both first mold component 200 and second mold component 218 can be made of a soluble material. In certain embodiments, first mold component 200 and second mold component 218 can be made of the same soluble material as the material used to fabricate soluble core component 236. For example, first mold component 200, second mold component 218, and soluble component 236 can be made of polyvinyl alcohol. Alternatively, one or both of first mold component 200 and second mold component 218 can be made of a different soluble material than the material used to fabricate soluble core component 236.
[0187] In examples where both first mold component 200 and second mold component 218 are made of a soluble material, the method of forming the lens components (e.g., haptics) can include immersing the entire assembly mold 250 in a solvent after the curing step. The entire assembly mold 250 can be immersed in the solvent to dissolve the soluble core component 236, the first mold component 200, and the second mold component 218. The method can also include heating the solvent to about 35° C. to 55° C. and agitating the solvent by sonication or stirring to promote dissolution of the soluble core component 236, the first mold component 200, and the second mold component 218. In some embodiments, the soluble component 236, the first mold component 200, and the second mold component 218 can be dissolved after immersion in the solvent for about 6 hours to about 24 hours. What remains after all of the soluble material has dissolved is a molded lens component (eg, haptics or optic having a cavity defined therein).
[0188] In some embodiments, either the first mold component 200 or the second mold component 218 (but not both) can be made of a soluble material. In these embodiments, the other mold component can be made of an insoluble material. An insoluble material can be a material that cannot be dissolved in a solvent (e.g., water) for a reasonable length of time.
[0189] For example, either first mold component 200 or second mold component 218 can be made of the same soluble material used to fabricate soluble core component 236. More specifically, in some embodiments, first mold component 200 or second mold component 218 and soluble core component 236 can be made of polyvinyl alcohol. Alternatively, either first mold component 200 or second mold component 218 can be made of a soluble material different from the material used to fabricate soluble core component 236. The other mold component in these examples can be made of an insoluble material. In some embodiments, first mold component 200 can be made of polyvinyl alcohol and second mold component 218 can be made of a thermoplastic resin including polyolefins such as medium to high density polyethylene (PE), polypropylene (PE) or copolymers thereof, poly-4-methylpentene, and polystyrene. The insoluble mold components can also be made from various nylons including polyacetal resins, polyacrylates, polyarylethersulfones, nylon 6, nylon 66, and nylon 11. Additionally, the insoluble mold components can also be made from corrosion resistant metallic materials such as stainless steel.
[0190] In an example where either the first mold component 200 or the second mold component 218 is made of a soluble material and the other mold component is made of an insoluble material, the method of forming the lens component (e.g., haptics) can include separating the two mold components after the curing step. After the two mold components are separated, at least one segment of the soluble core component 236 can be in or partially surrounded by the molded lens component. For example, the core body 238 of the soluble core component 236 can be in or partially surrounded by the molded lens component after the molded lens component is removed from the first mold component 200 or the second mold component 218. Additionally, the positioning piece 240 of the soluble core component 236 can be connected to the molded lens component but is not included in or surrounded by the molded lens component.
[0191] The method may further include immersing the soluble mold component (either first mold component 200 or second mold component 218) along with the molded lens component in a solvent to dissolve the soluble core component 236 and the soluble mold component (either first mold component 200 or second mold component 218). The method may also include heating the solvent to about 35° C. to 55° C. and agitating the solvent by sonication or stirring to facilitate dissolution of the soluble core component 236 and the soluble mold component. In some embodiments, the soluble core component 236 and the soluble mold component may dissolve after immersion in the solvent for about 6 hours to about 24 hours. What remains after all of the soluble material has dissolved is the molded lens component (e.g., the haptic or optic portion with a cavity defined therein).
[0192] 3A and 3B show perspective views of an embodiment of a fusible core component 236. The fusible core component 236 can include a curved or arcuate core body 238 connected to a positioning piece 240. In other embodiments not shown, the core body 238 can be substantially straight, wavy, or zigzag shaped.
[0193] As described above, the positioning member 240 allows the core body 238 to be elevated or raised so that when the positioning member 240 is placed on a flat surface, no portion of the core body 238 is in direct contact with the flat surface.
[0194] 3A and 3B, the fusible core component 236 can have a core distal end 242 that is free and not attached to the positioning member 240. In certain embodiments, the core distal end 242 can be rounded or curved. In other embodiments, the core distal end 242 can be flat, tapered, or pinched. As discussed in more detail in the following sections, in some embodiments: The soluble core component 236 can include two or more positioning pieces 240, and one or more core bodies 238 can extend between such positioning pieces 240 (see, for example, FIG. 9B). In some embodiments, the soluble core component 236 does not include a free core distal end 242.
[0195] As previously described, the core body 238 of the soluble core component 236 can be disposed within the component mold cavity formed by the first component cavity portion 204 and the second component cavity portion 222 when the first mold component 200 is mated with the second mold component 218 to form the assembly mold 250 (see, e.g., FIGS. 2A, 2B, and 2D). In this manner, a molded lens component (e.g., haptics) can be formed around the core body 238 of the soluble core component 236.
[0196] The positioning component 240 can be positioned within the positioning cavity formed by the first positioning cavity portion 206 and the second positioning cavity portion 224 when the first mold component 200 is mated with the second mold component 218 to form the assembly mold 250 (see, for example, Figures 2A, 2B, and 2D).
[0197] 3A and 3B, the positioning component 240 can include a first support wall 300, a second support wall 302, and a bridge component 304 connecting the first support wall 300 to the second support wall 302. The unique shape and design of the positioning component 240 allows a manufacturer to more easily remove the fusible core component 236 from the mold component using tweezers or other small plucking or gripping tools. The unique shape and design of the positioning component 240 also ensures that the positioning component 240 does not deform or distort during the injection molding process.
[0198] The core body 238 can be connected to an outer surface of the first support wall 300. The outer surface of the first support wall 300 can be substantially flat to form a substantially flat optic mounting end (see, e.g., optic mounting end 136 in FIG. 1D ) to allow the optic mounting end to more easily connect with a substantially flat protruding outer surface of the lens optic (see, e.g., protruding outer surface 134 in FIG. 1D ).
[0199] The first support wall 300 of the positioning component 240 can also function as a barrier to separate the component mold cavity from the positioning cavity in the assembly mold 250. The first support wall 300 can prevent the lens component material in the component mold cavity from contacting the lens component material in the positioning cavity. In this manner, the first support wall 300 can act as a temporary boundary for the open end of the molded haptic.
[0200] The second support wall 302 of the positioning component 240 may include one or more deformable or crushable protrusions 306 extending laterally from an outer surface of the second support wall 302. The protrusions 306 may create gaps between the outer surface of the second support wall 302 and the mold component wall, which define the positioning cavities. These gaps may ensure that the second support wall 302 (and thus the positioning component 240) does not get stuck or jammed in the positioning cavities. The gaps created by the protrusions 306 may allow a user to more easily remove the positioning component 240 from the first positioning cavity portion 206 or the second positioning cavity portion 224 when the first mold component 200 is separated from the second mold component 218.
[0201] 3A and 3B also show a bridge component 304 that can connect the first support wall 300 to the second support wall 302. The bridge component 304 can connect an inner surface of the first support wall 300 to an inner surface of the second support wall 302. The bridge component 304 can be raised or elevated such that a passageway 308 or clearance is formed above or below the bridge component 304. In some embodiments, the passageway 308 allows a low viscosity lens component material to be injected or otherwise admitted into the interior of the assembly mold 250 through the passageway 308.
[0202] One technical problem faced by the applicant is how to use a fusible core with a mold component to form a lens component with complex internal shapes and geometric features. One technical solution that the applicant has arrived at is the fusible core component disclosed herein, which has a unique shape for positioning the fusible core component on the surface of the mold component. The positioning part is also designed to have structural features that complement the mold component and can provide a passageway for the curable lens material to enter the component mold cavity.
[0203] Yet another technical problem faced by the applicant is how to prevent deformation of the first support wall 300 and the second support wall 302 of the positioning part 240 during the injection molding process. One technical solution arrived at by the applicant is that rather than designing the positioning part 240 as a solid hexahedron or rectangular parallelepiped shaped structure, the applicant designed the positioning part 240 with two support walls connected by a bridge component as shown and described herein. The two support walls can include a rigid or non-deformable portion and a crushable or deformable component extending from the support walls.
[0204] The soluble core component 236 can be made of a soluble or dissolvable material. As previously mentioned, the first mold component 200 and / or the second mold component 218 can also be made of the same soluble or dissolvable material.
[0205] In some embodiments, the soluble core component 236, the first mold component 200, the second mold component 218, or a combination thereof can be made entirely or in part from a soluble vinyl alcohol or other polymer. For example, the soluble core component 236, the first mold component 200, the second mold component 218, or a combination thereof can be made entirely or in part from a soluble polyvinyl alcohol (PVOH). In some embodiments, the soluble core component 236, the first mold component 200, the second mold component 218, or a combination thereof can be made entirely or in part from a soluble polyvinyl alcohol that includes a plasticizer. In certain embodiments, the soluble polyvinyl alcohol can include glycerol and other additives. More specifically, the fusible core component 236, the first mold component 200, the second mold component 218, or a combination thereof, may be made in whole or in part from Mowiflex™ C-30 or Mowiflex™ C-600 sold by Kuraray Europe.
[0206] In other embodiments, the soluble core component 236, the first mold component 200, the second mold component 218, or a combination thereof can be made in whole or in part from a butenediol vinyl alcohol (BVOH) copolymer. The soluble core component 236, the first mold component 200, the second mold component 218, or a combination thereof can be made in whole or in part from a soluble biocompatible material.
[0207] The soluble core component 236 can be completely dissolved when immersed in a solvent, such as water, for about 6 to 24 hours. The solvent can be heated to about 35° C. to about 55° C. In other embodiments, the soluble core component 236 can be dissolved in a solvent held at room temperature. The solvent can also be agitated by sonication to facilitate dissolution of the soluble core component 236. In other embodiments, the solvent can be agitated by stirring the solvent. For example, the soluble core component 236 can be immersed in a heated ultrasonic water bath to dissolve the soluble core component 236. In these and other embodiments, the first mold component 200, the second mold component 218, or a combination thereof can also be dissolved under similar conditions if these mold components are made of a soluble material.
[0208] In some embodiments, the entire soluble core component 236, including the positioning piece 240 and the core body 238, can be made of the same soluble material. In other embodiments, the positioning piece 240 or a portion of the positioning piece 240 can be made of a different soluble material than the core body 238.
[0209] Although the soluble core component 236 is made of a soluble material, the soluble core component 236 can harden into a substantially hard or rigid component when used in a molding process. Additionally, if the first mold component 200, the second mold component 218, or a combination thereof is made of a soluble material, the mold components can harden into a substantially hard or rigid component when used in a molding process.
[0210] 3B illustrates that the fusible core component 236 can include a second core feature 310 that protrudes or extends outwardly from the core body 238. As shown in FIG. 3B, the second core feature 310 can be a fin-shaped feature that protrudes from the radially inner body portion 244 of the core body 238.
[0211] Second core features 310 can enable the lens designer to create additional cavities or passageways in the molded lens component. For example, the fin-shaped feature shown in Figure 3B can be used to create a channel 500 (see, e.g., channel 500 in Figure 5B) that extends into the radially inner portion of the haptic.
[0212] Figure 3B also shows that the core body 238 of the fusible core component 236 can include a core opening 312. The core opening 312 can be a hole or opening along the core body 238 that extends into at least a portion of the core body 238. As shown in Figure 3B, the core opening 312 can be located on the second core feature 310.
[0213] The core opening 312 may include a stabilizing member, such as a stabilizing pin 708 (see, e.g., FIG. 7), to hold the core body 238 in place during the molding process. For example, the stabilizing pin 708 may be inserted into the core opening 312 to prevent the core body 238 from shifting or moving during the molding process (e.g., when the lens component material is injected under vacuum into the assembly mold 250).
[0214] Figure 4A shows a cross-sectional view of the core body 238 of the fusible core component shown in Figure 3A taken along transverse line AA. As shown in Figure 4A, the core body 238 can have curved or rounded sides and sloping upper and lower surfaces. In another embodiment, either the upper or lower surface can be substantially straight or horizontal.
[0215] Figure 4B shows a cross-sectional view of the core body 238 of the fusible core component 236 shown in Figure 3B taken along transverse line BB. The core body 238 can have a second core feature 310 protruding or extending from the core body 238. As shown in Figure 3B, the second core feature 310 can be a fin-shaped feature. Although Figure 4B shows the second core feature 310 protruding from a longitudinally central region of the core body 238, it is contemplated in accordance with the present disclosure that the second core feature 310 can also protrude from upper or lower regions of the core body 238.
[0216] 4C illustrates a cross-sectional view of a core body 238 of another embodiment of a fusible core component 236. In this embodiment, the core body 238 can have a substantially D-shaped (or inverted D-shaped) cross-sectional shape.
[0217] 4D illustrates a cross-sectional view of the core body 238 of yet another embodiment of the fusible core component 236. In this embodiment, the core body 238 can have a substantially elliptical or oval cross-sectional shape.
[0218] FIG 5A shows a cross-sectional view of one embodiment of a haptic 104 fabricated using the soluble core component 236 shown in FIG 3A and 4A. Additionally, FIG 5B shows a cross-sectional view of another embodiment of a haptic 104 fabricated using the soluble core component 236 shown in FIG 3B and 4B. As shown in FIG 5A and 5B, when a molded lens component is immersed in a solvent and the soluble core component 236 dissolves in the solvent, a hollow haptic chamber 120 can be formed. The haptic chamber 120 can assume the shape of the core body 238 of the soluble core component 236.
[0219] FIG. 5B also shows that when the soluble core component 236 includes a second core feature 310 (e.g., a fin-shaped feature) protruding from the core body 238, an additional channel 500 can be formed extending into the radially inner portion 146 of the haptic 104.
[0220] 5A and 5B also illustrate that positioning of the core body 238 within the component mold cavity can also affect the interior or cross-sectional shape or design of the haptic 104. For example, the core body 238 can be positioned closer to an outer edge or boundary of either the first molding surface 202 used to define the first component cavity portion 204 or the second molding surface 220 used to define the second component cavity portion 222 than to an inner edge or boundary of such surface. By doing so, the haptic 104 can be formed having a radially inner portion 146 that is thicker than the radially outer portion 144.
[0221] 6 shows a top view of an embodiment of a haptic 104 that includes an internal cavity pattern fabricated using one or more soluble core components 236. For example, the haptic 104 can be formed to include a curved haptic chamber 120 and comb-shaped cavities 502 positioned along the radially inner portion 146 of the haptic 104. These cavities can be fabricated using multiple soluble core components 236 or a single soluble core component 236 that includes comb-shaped protrusions or surface features.
[0222] 7 shows an exploded view of an embodiment of a system 700 for manufacturing a lens component (e.g., an AIOL haptic) that includes portions made of different curable materials. The system 100 can include a first mold component 200, a soluble core component 236, a second mold component 218, a third mold component 704, a stabilizing pin 708, a fourth mold component 712, and a clamp member 232. The first mold component 200 can be similar to the first mold component 200 described above and shown in FIGS. 2A, 2D, and 2E. The soluble core component 236 can be similar to the soluble core component 236 described above and shown in FIG. 3B.
[0223] 7 can have an elongated opening 702 defined along the second molding surface 220. The elongated opening 702 can be positioned along at least a portion of the second component cavity portion 222. A portion of the second component cavity portion 222 can be absent from the second mold component 218 due to the presence of the elongated opening 702. The elongated opening 702 can be aligned with a mold feature defined along the third mold component 704.
[0224] The second mold component 218 may also have a recessed portion 706 defined along a top surface of the second mold component 218. The third mold component 704 may be installed or otherwise positioned within the recessed portion 706. In some embodiments, an initial step of forming an assembly mold using components of the system 700 may include installing or purchasing the third mold component 704 within the recessed portion 706 of the second mold component 218. Once the third mold component 704 is installed within the recessed portion 706, the third mold component 704 may be removably coupled to the second mold component 218 by an interference fit.
[0225] The soluble core component 236 can then be placed or pressed against the underside of the second mold component 218, which includes the second molding surface 220. For example, the positioning piece 240 of the soluble core component 236 can be pressed into the second positioning cavity portion 224 (not shown in FIG. 7 ) defined along the second molding surface 220, and the core body 238 of the soluble core component 236 can be positioned partially within the second component cavity portion 224, but not in physical contact with the second molding surface 220. The soluble core component 236 can be removably coupled to the second mold component 218 by an interference fit when the positioning piece 240 is pressed or otherwise inserted into the second positioning cavity portion 224.
[0226] With the fusible core component 236 removably coupled to the second mold component 218, the stabilizing pin 708 can be inserted through a core opening 312 defined along the core body 238 or the second core feature 310 extending or protruding from the core body 238. The stabilizing pin 708 can be inserted through the core opening 312 to prevent the core body 238 from shifting or moving during the molding process. For example, the stabilizing pin 708 can be made, in part, of a metallic material. The diameter of the stabilizing pin 708 can be from about 0.5 mm to about 2.0 mm. The stabilizing pin 708 can be inserted into a receiving conduit or space defined along the bottom surface of the third mold component 704.
[0227] The third mold component 704 can include a third molding surface (not shown in FIG. 7) along which surface features, cavities, or combinations thereof are defined. For example, the third mold component 704 can be used to introduce negative space into a part of the molded lens component.
[0228] Thereafter, the second mold component 218 including the third mold component 704 and the soluble core component 236 can be mated with the first mold component 200 to form a first assembly mold. The clamp member 232 can then be removably secured to the first mold component 200 to form a closed chamber. As shown in FIG. 7 , the clamp member 232 (e.g., a clamp cap) can have a septum 710 or opening defined along a top of the clamp member 232 such that an injector nozzle can enter the septum 710 or opening to deliver a first curable material, such as the lens component material (e.g., haptic material) described above, into the closed chamber. For example, the first curable material can be injected or introduced into the storage space 214 of the first mold component 200.
[0229] The closed chamber including the clamping member 232 coupled to the first assembly mold can be cured to form the preformed lens component. The clamping member 232 and the third mold component 704 can then be separated from the first mold component 200 and the second mold component 218. At this point, a fourth mold component 712 including a fourth molding surface can be placed or otherwise positioned in the recessed portion 706 of the second mold component 218. The fourth mold surface can include surface features and cavities that can be used to define the shape or positioning of the additional portion of the molded lens component. The additional portion of the molded lens component can be fabricated with a second curable material. The second curable material can be different from the first curable material (or lens component material) used to fabricate the preformed lens component. In some embodiments, the second curable material can include a composite polymeric material including an energy absorbing component and an expandable component. For example, the second curable material can include expandable thermoplastic microspheres. As a more specific example, the second curable material can be a composite material as described in U.S. Patent Application No. 62 / 911,039, filed October 4, 2019, the contents of which are incorporated herein by reference. Once cured, portions of the molded lens component made of the second curable material can expand in response to external energy directed at such portions.
[0230] In some embodiments, the fourth mold component 712 can include an opening or port defined along a surface of the fourth mold component 712, allowing an injector nozzle or fluid delivery device to deliver a second hardenable material into the cavity created by the fourth molding surface and into the negative space defined along the preformed lens. The same or other clamping members 232 can then be removably coupled to the first mold component 200 to form a second assembly mold. The second assembly mold can then be cured to form a molded lens component. This molded lens component including the soluble core component 236, or a combination of the soluble core component 236 and any or all of the first mold component 200, second mold component 218, and fourth mold component 712 (depending on whether any of the mold components are made of a soluble material), can be immersed in a solvent to dissolve the soluble core component 236 or one or more of the mold components.
[0231] While the system 700 shown in FIG. 7 includes four mold components (e.g., first mold component 200, second mold component 218, third mold component 704, and fourth mold component 712), it is contemplated in accordance with the present disclosure that the system 700 can include more mold components, including five mold components, six mold components, seven mold components, eight mold components, or nine or more mold components. These additional mold components can be used to form even more complex or sophisticated molded lens components that include different portions made of different curable materials, multiple internal chambers, or combinations thereof. For example, a variation of the system 700 shown in FIG. 7 can be used to form the haptics 104 shown in FIG. 6.
[0232] One technical problem faced by the applicant is how to form a haptic that includes a complex internal shape and geometry, such as a uniquely shaped internal chamber surrounded by chamber walls of different thicknesses. One technical solution arrived at by the applicant is to form a haptic using the soluble core and mold disclosed herein. Furthermore, the haptic formed using the soluble core and mold disclosed herein can be coupled to an optical portion that includes an optical portion fluid chamber to form an AIOL optimized for placement in a subject's lens capsule. The haptic formed using the soluble core and mold disclosed herein can be made to deform in a specific manner due to the uniquely shaped chamber walls in response to ciliary muscle movement that is involved in the deformation of the lens capsule. The deformation of the haptic allows the fluid in the haptic fluid chamber to enter the optical portion fluid chamber and change the refractive power of the AIOL. The haptic formed using the soluble core and mold disclosed herein is suitable for such deformation.
[0233] 8 shows a cross-sectional view of an embodiment of an assembly mold 250 including one or more fusible plugs 800 to prevent flash along one or more parting lines 802 between the mold components. For example, the fusible plugs 800 can be inserted or otherwise positioned between the first mold component 200 and the second mold component 218 prior to mating the two mold components together.
[0234] One or more fusible plugs 800 can be located within a first plug cavity portion defined along the first molding surface 202. The first plug cavity portion can be disposed or positioned along a parting line 802 between the mold components (e.g., the parting line 802 between the first mold component 200 and the second mold component 218). The first plug cavity portion can be disposed or positioned within an interface area between the parting line 802 and a boundary or beginning of the first component cavity portion 204. The first plug cavity portion can be connected to the first component cavity portion 204.
[0235] In some embodiments, one or more fusible plugs 800 can be located within a second plug cavity portion defined along the second molding surface 220. The second plug cavity portion can also be disposed or positioned along a parting line 802 between the mold components (e.g., the parting line 802 between the first mold component 200 and the second mold component 218). The second plug cavity portion can be disposed or positioned within an interface area between the parting line 802 and a boundary or beginning of the first component cavity portion 204. The second plug cavity portion can be connected to the second component cavity portion 222.
[0236] The soluble plug 800 can be made of a soluble material configured to dissolve when immersed in a solvent. In some embodiments, the soluble plug 800 can be made of the same soluble material as the soluble core component 236. In other embodiments, the soluble plug 800 can be made of a different soluble material than the soluble material used to make the soluble core component 236.
[0237] The first plug cavity portion and the second plug cavity portion can form a plug-receiving space when the first mold component 200 is mated with the second mold component 218 to form the assembly mold 250. A fusible plug can be configured to occupy the plug-receiving space.
[0238] The assembly mold 250 containing the soluble core component 236, the soluble plugs 800, and the lens component material can be cured together. After the curing step, the molded lens component containing the soluble core component 236 and the soluble plugs 800 can be removed from the first mold component 200 or the second mold component 218 and immersed in a solvent (e.g., water).
[0239] In embodiments in which either the first mold component 200 or the second mold component 218 is made of a soluble material, the mold component made of the soluble material (the first mold component 200 or the second mold component 218) can also be immersed in a solvent and dissolved.
[0240] Although the fusible plug 800 is depicted as a block or nodule in the cross-sectional view of FIG. 8, it is contemplated and would be understood by one of ordinary skill in the art that the present disclosure contemplates that the fusible plug 800 may be implemented as a long cord or strand that extends along the periphery of the first component cavity portion 204, the second component cavity portion 222, or a combination thereof.
[0241] The soluble plug 800 can act as a barrier or gasket to prevent lens component material from seeping or leaking into any gaps created between the mold components along the parting line 802. The soluble plug 800 can be configured to prevent flash or surface defects along the periphery of the molded lens component.
[0242] One technical problem faced by applicants is how to prevent flash from forming at the periphery of a molded lens component that is made using separable mold components. One technical solution derived by applicants is to place one or more soluble plugs along the periphery of the mold cavity. The soluble plugs can be made of the same soluble material as the soluble core component.
[0243] 9A illustrates one embodiment of an optic portion 102 of a fluid-filled AIOL. The optic portion 102 can include an anterior element 106, a posterior element 108, and an optic fluid chamber 110 defined therebetween.
[0244] The systems and methods disclosed herein can also be used to mold such an optical portion 102. For example, the optical portion fluid chamber 110 and a plurality of fluid channels (not shown in FIG. 9A, see FIG. 1A, fluid channel 122) can be formed when a soluble core component 900 (see FIG. 9B) is dissolved in a solvent. In additional embodiments, the systems and methods disclosed herein can form a portion of the optical portion 102, such as the anterior element 106 or the posterior element 108. In these embodiments, at least a portion of the optical portion fluid chamber 110 can be formed when the soluble core component 900 is dissolved.
[0245] In some embodiments, the haptics 104 formed with the fusible core and mold disclosed herein can be adhered or otherwise connected to the optical portion 102 formed with the fusible core and mold disclosed herein using the adhesives disclosed in the previous section.
[0246] 9B shows an exploded cross-sectional view of a system 900 including an alternative embodiment of a soluble core component 902, a first mold component 904, and a second mold component 906. The system 900 can be used to form the optic portion 102 shown in FIG. 9A, including the optic portion fluid chamber 110. In other embodiments, modifications of the soluble core component 902, the first mold component 904, and the second mold component 906 can be used to form at least a portion of the optic portion 102, such as the anterior element 106 or the posterior element 108.
[0247] The fusible core component 902 may include a core body 908, a plurality of positioning parts including a first positioning part 910 and a second positioning part 912, a first connecting shaft set 914 connecting the first positioning part 910 to the core body 908, and a second connecting shaft set 916 connecting the second positioning part 912 to the core body 908.
[0248] The core body 908 can be shaped and sized to define the shape and size of the optical fluid chamber 110 (see FIG. 9A). The first connecting shaft set 914 can include multiple connecting shafts connecting the core body 908 to the first positioning component 910. The first connecting shaft set 914 can be sized and shaped to define the size and shape of the first fluid channel set 122A (see, e.g., FIG. 1A) connecting the haptic fluid chamber 120 to the optical portion fluid chamber 110. In some embodiments, the first connecting shaft set 914 can include two connecting shafts 914 connecting the core body 908 to the first positioning component 910.
[0249] The second connecting shaft set 916 can include multiple connecting shafts connecting the core body 908 to the second positioning component 912. The second connecting shaft set 916 can be sized and shaped to define the size and shape of the second fluid channel set 122B (see, for example, FIG. 1A ) connecting the optical portion fluid chamber 110 to the other haptic fluid chamber 120. In some embodiments, the second connecting shaft set 916 can include two connecting shafts 916 connecting the core body 908 to the second positioning component 912. The optical portion fluid chamber 110 and the fluid channels 122 can be formed when the soluble core component 902 dissolves in a solvent.
[0250] 9B, the first mold component 904 can include a first component cavity portion 918 defined along a first molding surface 920. Additionally, the second mold component 906 can include a second component cavity portion 922 defined along a second molding surface 924. The first component cavity portion 918 and the second component cavity portion 922 can form a component mold cavity when the first mold component 904 is mated or otherwise coupled with the second mold component 906. The component mold cavity can be filled with a curable lens component material, such as the lens body material disclosed in the previous section. The lens component material can be introduced into the component mold cavity through a conduit, gate, or port defined along the mold components.
[0251] The first mold component 904 can also have a plurality of first positioning cavity portions 926 defined along the first mold surface 920. The first positioning cavity portions 926 can be configured to accommodate or receive a plurality of positioning pieces of the fusible core component 902, including the first positioning piece 910 and the second positioning piece 912.
[0252] The second mold component 906 can also have a plurality of second positioning cavity portions 928 defined along the second mold surface 924. The second positioning cavity portions 928 can be configured to accommodate or receive a plurality of positioning pieces of the fusible core component 902, including the first positioning piece 910 and the second positioning piece 912.
[0253] In some embodiments, the first mold component 904, the second mold component 906, or a combination thereof, can be made, in part, of a soluble material. In these and other embodiments, the first mold component 904, the second mold component 906, or a combination thereof, can be made, in part, of the same soluble material as the soluble core component 908. In other embodiments, the first mold component 904, the second mold component 906, or a combination thereof, can be made, in part, of a soluble material that is different from the soluble material used to make the soluble core component 908.
[0254] A molded lens component (e.g., a molded optic) including a soluble core component 908 can be immersed in a solvent (e.g., water) to dissolve the soluble core component 908. In some embodiments, the entire assembly mold can be immersed in the solvent, or one of the mold components can be immersed in the solvent along with the molded lens component.
[0255] Although not shown, in another embodiment contemplated by this disclosure, fusible plugs 800 can also be placed at the periphery of the mold cavity to prevent flash from forming along the periphery of the molded lens component.
[0256] In certain embodiments, the optic portion 102 formed using the system 900 can be a one-piece optic portion 102 that includes the anterior element 106 connected to the posterior element 108 without the use of adhesives. In other embodiments, portions of the system 900 or modifications of the first mold component 904, the second mold component 906, and the fusible core component 908 can be used to form a portion of the optic portion 102 that includes the anterior element 106 or the posterior element 108. In these embodiments, the molded anterior element 106 and the molded posterior element 108 can then be bonded or otherwise coupled together using adhesives as discussed in the previous section.
[0257] One technical problem faced by the applicant is how to form an optical portion of an AIOL that includes a uniquely shaped fluid channel that extends through a portion of the optical portion. One technical solution that the applicant has arrived at is to form the optical portion using the soluble core and mold disclosed herein. Furthermore, the optical portion formed using the soluble core and mold disclosed herein can be coupled to a haptic (also formed using the soluble core and mold disclosed herein) that includes a haptic fluid chamber. The optical portion formed using the soluble core and mold disclosed herein can be made to change shape (thereby changing the optical power of the AIOL) in response to fluid entering the optical portion fluid chamber from the haptic fluid chamber through the fluid channel and exiting the optical portion fluid chamber back to the haptic fluid chamber through the same fluid channel.
[0258] The present disclosure also covers the following sections:
[0259] Item 1: A method of manufacturing a lens component, comprising: providing a first mold component including a first molding surface defined by a first component cavity portion; providing a second mold component including a second molding surface defined by a second component cavity portion; placing at least a portion of a soluble core component on either the first molding surface or the second molding surface; mating the second mold component with the first mold component to form an assembly mold, wherein a segment of the soluble core component is disposed in the mold cavity formed by the first component cavity portion and the second component cavity portion; introducing a lens component material into the mold cavity; curing the lens component material in the assembly mold to form a molded lens component; and immersing the molded lens component in a solvent to dissolve the soluble core component.
[0260] Item 2: The method of item 1, wherein the soluble component is made, in part, of polyvinyl alcohol.
[0261] Item 3: The method of item 1, wherein the solvent is water.
[0262] Item 4: The method of item 1, further comprising the steps of heating the solvent and agitating the solvent to promote dissolution of the soluble core component.
[0263] Item 5: The method of item 1, further comprising the steps of separating the first mold component from the second mold component after the lens component material is hardened to form a molded component, and removing the molded lens component from the first mold component or the second mold component, wherein at least one segment of the soluble core component is within the molded lens component when the molded lens component is removed.
[0264] Item 6: The method of item 1, wherein the step of placing at least a portion of the soluble core component on the first molding surface or the second molding surface includes placing at least a portion of a positioning piece of the soluble core component on the first molding surface or the second molding surface, wherein the at least one positioning piece is at one end of the soluble core component, and wherein the portion of the soluble core component coupled to the at least one positioning piece does not contact the first molding surface or the second molding surface.
[0265] Item 7: The method of item 1, wherein the step of placing the soluble core component on the first molding surface or the second molding surface includes placing at least one positioning piece of the soluble core component on the first molding surface or the second molding surface, wherein the at least one positioning piece is at one end of the soluble core component and a remaining portion of the soluble core component coupled to the at least one positioning piece does not contact the first molding surface or the second molding surface.
[0266] Item 8: the first molding surface is further defined by a first plug cavity portion connected to the first component cavity portion and the second molding surface is further defined by a second plug cavity portion connected to the second component cavity portion, the method further including the steps of placing a fusible plug in the first plug cavity portion or the second plug cavity portion prior to forming the assembly mold, wherein the fusible plug occupies a plug receiving space formed by the first plug cavity portion and the second plug cavity portion when the second mold component is mated with the first mold component, and hardening the lens component material in the assembly mold, wherein the assembly mold includes the fusible plug.
[0267] Item 9: The method of item 1, wherein the lens component is a haptic of the lens and a haptic chamber is formed in the haptic upon dissolution of the soluble core component.
[0268] Item 10: The method of item 1, wherein the lens component is an optic portion of a lens, and when the soluble core component dissolves, an optic portion chamber is formed within the optic portion.
[0269] Item 11: The method of item 1, wherein the lens component is part of an optical portion of the lens, and when the soluble core component dissolves, at least a portion of the optical chamber is formed.
[0270] Item 12: The method of item 1, further comprising the step of securing the first mold component to the second mold component using a clamping member after mating the second mold component with the first mold component.
[0271] Item 13: The method of item 12, wherein the clamping member is a clamping cap configured to be removably secured to an upper portion of the first mold component when the second mold component is mated with the first mold component.
[0272] Item 14: The method of item 1, wherein the second mold component includes a vent configured to allow air to exit while the lens component material is being introduced into the mold cavity.
[0273] Item 15: The method of item 1, wherein the lens component material is made, in part, from a curable acrylic monomer.
[0274] Item 16: A system for manufacturing a lens component, comprising: a first mold component including a first molding surface defined by a first component cavity portion; a second mold component including a second molding surface defined by a second component cavity portion; and a soluble core component configured to be placed on the first molding surface or the second molding surface, the first mold component configured to be mated with the second mold component to form an assembly mold, a segment of the soluble core component configured to be disposed in a mold cavity formed by the first component cavity portion and the second component cavity portion when the first mold component is mated with the second mold component, the mold cavity in the assembly mold configured to receive lens component material for hardening into a molded lens component, and the soluble core component configured to dissolve in a solvent when the molded lens component is immersed in the solvent.
[0275] Item 17: The system of item 16, wherein the soluble core component is fabricated, in part, from polyvinyl alcohol.
[0276] Item 18: The system of item 16, wherein the solvent is water.
[0277] Item 19: The system of item 16, further comprising a warm water bath configured to heat the solvent when the molded lens component is immersed in the solvent, and an ultrasonic processor configured to agitate the solvent to promote dissolution of the soluble core component.
[0278] Item 20: The system of item 16, wherein the lens component material is configured to be cured into a molded lens component in the assembly mold, and the molded lens component is configured to be removed from either the first mold component or the second mold component after curing when the first mold component is separated from the second mold component, and at least one segment of the soluble component is within the molded lens component when the molded lens component is removed from either the first mold component or the second mold component.
[0279] Item 21: The system of item 16, wherein the soluble core component includes at least one positioning piece at one end of the soluble core component, the at least one positioning piece configured to be placed on the first molding surface or the second molding surface, and no portion of the soluble core component contacts the first molding surface or the second molding surface when the at least one positioning piece is placed on the first molding surface or the second molding surface.
[0280] Item 22: The system of item 16, wherein the soluble core component includes at least one positioning part at one end of the soluble core component and a free distal end at an opposite end of the soluble core component, the at least one positioning part configured to be placed on the first molding surface or the second molding surface, and the free distal end of the soluble core component does not contact the first molding surface or the second molding surface when the at least one positioning part is placed on the first molding surface or the second molding surface.
[0281] Item 23: The system of item 16, further including a fusible plug configured to be placed in the first plug cavity portion defined along the first molding surface or in the second plug cavity portion defined along the second molding surface prior to forming the assembly mold, the fusible plug configured to occupy a plug receiving space formed by the first plug cavity portion and the second plug cavity portion when the second mold component is mated with the first mold component, and the assembly mold including the lens component material, the fusible core component, and the fusible plug is configured to be cured.
[0282] Item 24: The system of item 16, wherein the lens component is a haptic of the lens and the haptic chamber is formed in the haptic when the soluble core component melts.
[0283] Item 25: The system of item 16, wherein the lens component is an optic portion of the lens and an optic portion chamber is formed within the optic portion when the soluble core component dissolves.
[0284] Item 26: The system of item 16, wherein the lens component is part of the optical portion of the lens and at least a portion of the optical chamber is formed when the soluble core component melts.
[0285] Item 27: A method of manufacturing a lens component, comprising the steps of: providing a first mold component including a first molding surface defined by a first component cavity portion, the first mold component being made of a soluble material; providing a second mold component including a second molding surface defined by a second component cavity portion, the second mold component being made of a soluble material; placing at least a portion of a soluble core component on the first molding surface or the second molding surface, the soluble core component being made of a soluble material; and disposing the second mold component on the first molding surface or the second molding surface. the first mold component to form an assembly mold, where one segment of the soluble core component is disposed within the mold cavity formed by the first component cavity portion and the second component cavity portion; introducing a lens component material into the mold cavity; hardening the lens component material in the assembly mold to form a molded lens component; and immersing the assembly mold including the molded lens component in a solvent to dissolve the soluble core component, the first mold component, and the second mold component.
[0286] Item 28: The method of item 27, further comprising wetting at least one of the first molding surface and the second molding surface prior to mating the second mold component with the first mold component to prevent flash from being generated along the periphery of the molded lens component at a parting line created by the first and second mold components.
[0287] Item 29: The method of item 27, wherein the soluble core component, the first mold component, and the second mold component are fabricated, in part, from polyvinyl alcohol.
[0288] Item 30: The method of item 27, wherein the solvent is water.
[0289] Item 31: The method of item 27, further comprising the steps of heating the solvent and agitating the solvent to promote dissolution of the soluble core component, the first mold component, and the second mold component.
[0290] Item 32: The method of item 27, wherein the step of placing at least a portion of the soluble core component on the first molding surface or the second molding surface includes placing at least one positioning piece of the soluble core component on the first molding surface or the second molding surface, wherein the at least one positioning piece is at one end of the soluble core component, and wherein a portion of the soluble core component coupled to the at least one positioning piece does not contact the first molding surface or the second molding surface.
[0291] Item 33: The method of item 27, wherein the step of placing the soluble core component on the first molding surface or the second molding surface includes placing at least one positioning piece of the soluble core component on the first molding surface or the second molding surface, wherein the at least one positioning piece is at one end of the soluble core component and a remaining portion of the soluble core component coupled to the at least one positioning piece does not contact the first molding surface or the second molding surface.
[0292] Item 34: The method of item 27, wherein the lens component is a haptic of the lens and a haptic chamber is formed in the haptic upon dissolution of the soluble core component.
[0293] Item 35: The method of item 27, wherein the lens component is an optic portion of a lens and an optic portion chamber is formed within the optic portion upon dissolution of the soluble core component.
[0294] Item 36: The method of item 27, wherein the lens component is part of the optic portion of the lens, and wherein dissolving the soluble core component forms at least a portion of the optic portion chamber.
[0295] Item 37: A system for manufacturing a lens component, comprising: a first mold component including a first molding surface defined by a first component cavity portion, the first mold component made of a soluble material; a second mold component including a second molding surface defined by a second component cavity portion, the second mold component made of a soluble material; and a soluble core component configured to be placed on either the first molding surface or the second molding surface, wherein the first mold component is configured to be mated with the second mold component to form an assembly mold, a segment of the soluble core component is configured to be disposed within a mold cavity formed by the first component cavity portion and the second component cavity portion when the first mold component is mated with the second mold component, the mold cavity in the assembly mold is configured to receive lens component material to be cured into a molded lens component, and the soluble core component, the first mold component, and the second mold component are configured to dissolve in a solvent when the assembly mold is immersed in the solvent.
[0296] Item 38: The system of item 37, wherein the soluble core component, the first mold component, and the second mold component are fabricated, in part, from polyvinyl alcohol.
[0297] Item 39: The system of Item 37, wherein the solvent is water.
[0298] Item 40: The system of item 37, further including a warm water bath configured to heat the solvent when the assembly mold including the molded lens component is immersed in the solvent, and an ultrasonic processor configured to agitate the solvent to promote dissolution of the soluble core component, the first mold component, and the second mold component.
[0299] Item 41 : The system of item 37, wherein the lens component material is configured to be cured in the assembly mold to form a molded lens component, and at least one segment of the soluble core component is in the mold lens component when the assembly mold containing the molded lens component is immersed in a solvent.
[0300] Item 42: The system of item 37, wherein the soluble core component includes at least one positioning piece at one end of the soluble core component, the at least one positioning piece configured to be placed on the first molding surface or the second molding surface, and no portion of the soluble core component contacts the first molding surface or the second molding surface when the at least one positioning piece is placed on the first molding surface or the second molding surface.
[0301] Item 43: The system of item 37, wherein the soluble core component includes at least one positioning part at one end of the soluble core component and a free distal end at an opposite end of the soluble core component, the at least one positioning part being configured to be placed on the first molding surface or the second molding surface, and the free distal end of the soluble core component does not contact the first molding surface or the second molding surface when the at least one positioning part is placed on the first molding surface or the second molding surface.
[0302] Item 44: The system of item 37, wherein the lens component is a lens haptic and a haptic chamber is formed in the haptic upon dissolution of the soluble core component.
[0303] Item 45: The system of item 37, wherein the lens component is an optic portion of the lens and an optic chamber is formed within the optic portion upon dissolution of the soluble core component.
[0304] Item 46: The system of item 37, wherein the lens component is part of an optic portion of the lens and wherein at least a portion of the optic chamber is formed upon dissolution of the soluble core component.
[0305] Item 47: A method of manufacturing a lens component, comprising: providing a first mold component including a first molding surface defined by a first component cavity portion, the first mold component being made of a soluble material; providing a second mold component including a second molding surface defined by a second component cavity portion; placing at least a portion of a soluble core component on the first molding surface or the second molding surface, the soluble core component being made of a soluble material; mating the second mold component with the first mold component to form an assembly mold, a segment of the soluble core component being disposed in a mold cavity formed by the first component cavity portion and the second component cavity portion; introducing a lens component material into the mold cavity; curing the lens component material in the assembly mold to form a molded lens component; and immersing the first mold component and the molded lens component in a solvent to dissolve the first mold component and the soluble core component.
[0306] Item 48: The method of item 47, further comprising wetting at least one of the first molding surface and the second molding surface prior to mating the second mold component with the first mold component to prevent flash from being generated at a parting line created by the first and second mold components along the periphery of the molded lens component.
[0307] Item 49: The method of item 47, wherein the soluble core component and the first mold component are fabricated, in part, from polyvinyl alcohol.
[0308] Item 50: The method of item 47, wherein the solvent is water.
[0309] Item 51: The method of item 47, further comprising the steps of heating the solvent and agitating the solvent to promote dissolution of the soluble core component and the first mold component.
[0310] Item 52: The method of item 47, wherein the step of placing at least a portion of the soluble core component on the first molding surface or the second molding surface includes placing at least one positioning piece of the soluble core component on the first molding surface or the second molding surface, the at least one positioning piece being at one end of the soluble core component, and a portion of the soluble core component coupled to the at least one positioning piece does not contact the first molding surface or the second molding surface.
[0311] Item 53: The method of item 47, wherein the step of placing at least a portion of the soluble component on the first molding surface or the second molding surface includes placing at least one positioning piece of the soluble core component on the first molding surface or the second molding surface, wherein the at least one positioning piece is at one end of the soluble core component and a remaining portion of the soluble core component that is coupled to the at least one positioning piece does not contact the first molding surface or the second molding surface.
[0312] Item 54: The method of Item 47, wherein the second molding surface is further defined by a plug cavity, the method further including the steps of placing a soluble plug in the plug cavity prior to forming an assembly mold, the soluble plug occupying the plug cavity when the second mold component is mated with the first mold component, and hardening the lens component material in the assembly mold, the assembly mold including the soluble plug.
[0313] Item 55: The method of item 47, wherein the lens component is a haptic of the lens and a haptic chamber is formed in the haptic upon dissolution of the soluble core component.
[0314] Item 56: The method of item 47, wherein the lens component is an optic portion of a lens and an optic portion chamber is formed within the optic portion upon dissolution of the soluble core component.
[0315] Item 57: The method of item 47, wherein the lens component is an optic portion of a lens, and wherein dissolving the soluble core component forms at least a portion of an optic portion chamber.
[0316] Item 58: A system for manufacturing a lens component, comprising: a first mold component including a first molding surface defined by a first component cavity portion, the first mold component made of a soluble material; a second mold component including a second molding surface defined by a second component cavity portion; and a soluble core component configured to be placed on the first molding surface or the second molding surface, the first mold component configured to be mated with the second mold component to form an assembly mold, a segment of the soluble core component configured to be disposed within a mold cavity formed by the first component cavity portion and the second component cavity portion when the first mold component is mated with the second mold component, the mold cavity in the assembly mold configured to receive lens component material for hardening into a molded lens component, and the soluble core component and first mold component configured to dissolve when the first mold component and the molded lens component are immersed in a solvent.
[0317] Item 59: The system of item 58, wherein the soluble core component and the first mold component are fabricated, in part, from polyvinyl alcohol.
[0318] Item 60: The system of Item 58, wherein the solvent is water.
[0319] Item 61: The system of item 58, further including a warm water bath configured to heat the solvent as the first mold component and the molded lens component are immersed in the solvent, and an ultrasonic processor configured to agitate the solvent to promote dissolution of the soluble core component and the first mold component.
[0320] Item 62: The system of item 58, wherein the lens component material is configured to be cured into a molded lens component material in the assembly mold, the second mold component is configured to be separated from the molded lens component and the first mold component after curing, and at least one segment of the soluble core component is within the molded lens component when the first mold component and the molded lens component are immersed in a solvent.
[0321] Item 63: The system of item 58, wherein the soluble core component includes at least one positioning piece at one end of the soluble core component, the at least one positioning piece configured to be placed on the first molding surface or the second molding surface, and a portion of the soluble core component configured not to be in physical contact with the first molding surface or the second molding surface when the at least one positioning piece is placed on the first molding surface or the second molding surface.
[0322] Item 64: The system of item 58, wherein the soluble core component includes at least one positioning part at one end of the soluble core component and a free distal end at an opposite end of the soluble core component, the at least one positioning part configured to be placed on the first molding surface or the second molding surface, and the free distal end of the soluble core component configured not to be in physical contact with the first molding surface or the second molding surface when the at least one positioning part is placed on the first molding surface or the second molding surface.
[0323] Item 65: The system of Item 58, further including a soluble plug configured to be placed in a plug cavity defined along the second molding surface prior to the step of forming an assembly mold, the soluble plug configured to occupy the plug cavity when the second mold component is mated with the first mold component, and the assembly mold including the lens component material, the soluble core component, and the soluble plug is configured to be cured.
[0324] Item 66: The system of item 58, wherein the lens component is a haptic of the lens and a haptic chamber is formed in the haptic when the soluble core component melts.
[0325] Item 67: The system of item 58, wherein the lens component is an optic portion of the lens and an optic portion chamber is formed within the optic portion upon dissolution of the soluble core component.
[0326] Item 68: The system of item 58, wherein the lens component is part of the optic portion of the lens, and wherein at least a portion of the optic portion chamber is formed when the soluble core component dissolves.
[0327] A number of embodiments have been described. Nevertheless, those skilled in the art will appreciate that various changes and modifications may be made to the present disclosure without departing from the spirit and scope of the embodiments. The elements of the systems, devices, apparatuses, and methods shown with any embodiment are illustrative for a particular embodiment and may be used in combination or otherwise with other embodiments within the present disclosure. For example, the steps of any method depicted in the figures or described in this disclosure do not require the particular order or sequential order shown or described to achieve the desired results. In addition, other step operations may be provided or steps or operations may be eliminated or omitted from the described method or process to achieve the desired results. Furthermore, any components or parts of any apparatus or system described in the figures or depicted in this disclosure may be removed, eliminated, or omitted to achieve the desired results. In addition, certain components or parts of the systems, devices, or apparatuses shown or described herein have been omitted for brevity and clarity.
[0328] Accordingly, other embodiments are within the scope of the following claims, and the specification and / or drawings may be regarded in an illustrative sense, rather than a restrictive sense.
[0329] Each individual variation or embodiment described and illustrated herein has distinct components and features that may be readily separated from or combined with the features of any of the other variations or embodiments. Modifications may be made to a particular situation, material, composition of matter, process, process acts or steps, to adapt to the objective, spirit or scope of the present invention.
[0330] Furthermore, when a range of values is provided, every intervening value between the upper and lower limits of that range, and any other stated or intervening value within that stated range, is encompassed within the invention. Optional features of the described invention variations may be set forth and claimed independently or in combination with any one or more of the features described herein.
[0331] All pre-existing subject matter referred to herein (e.g., publications, patents, patent applications, and hardware) is incorporated herein by reference in its entirety, except to the extent that such subject matter may conflict with the subject matter of the present invention, in which case the subject matter present herein shall take precedence. The referenced items are provided solely for their disclosure prior to the filing date of this application. Nothing herein should be construed as an admission that the present invention is not entitled to antedate such material by virtue of prior invention.
[0332] Reference to a singular item includes the possibility that there are plural of the same items. More specifically, as used in this specification and the appended claims, the singular forms "a," "an," "said," and "the" include plural references unless the context clearly dictates otherwise. It is further noted that the claims may be drafted to exclude optional elements. As such, this statement is intended to serve as a predicate against the use of exclusive terminology such as "solely," "only," and the like or the use of a "negative" limitation in connection with the recitation of claim elements. Unless otherwise defined, all technical and scientific terms used herein have the same meaning as commonly understood by one of ordinary skill in the art to which this invention belongs.
Claims
1. 1. A method for manufacturing a lens component, comprising the steps of: providing a first mold component including a first molding surface defined by a first component cavity portion; providing a second mold component including a second molding surface defined by a second component cavity portion; placing at least a portion of a soluble core component on either the first molding surface or the second molding surface; mating a second mold component with the first mold component to form an assembly mold, a segment of the fusible core component being disposed within a mold cavity defined by the first component cavity portion and the second component cavity portion; introducing a lens component material into the mold cavity; curing the lens component material in the assembly mold to form a molded lens component; immersing the molded lens component in a solvent to dissolve the soluble core component; The method includes:
2. The method of claim 1 , wherein the soluble core component is made, in part, of polyvinyl alcohol.
3. The method of claim 1 , wherein the solvent is water.
4. The method of claim 1 further comprising the steps of heating the solvent and agitating the solvent to facilitate the dissolution of the soluble core component.
5. separating the first mold component from the second mold component after curing the lens component material to form the molded lens component; removing the molded lens component from the first mold component or the second mold component, wherein at least one segment of the fusible core component is in the molded lens component when the molded lens component is removed; The method of claim 1 further comprising:
6. 2. The method of claim 1, wherein placing at least a portion of the soluble core component on the first molding surface or the second molding surface comprises placing at least one positioning piece of the soluble core component on the first molding surface or the second molding surface, the at least one positioning piece being at one end of the soluble core component, and a portion of the soluble core component coupled to the at least one positioning piece does not contact the first molding surface or the second molding surface.
7. 2. The method of claim 1, wherein the step of placing the soluble core component on the first molding surface or the second molding surface comprises placing at least one positioning piece of the soluble core component on the first molding surface or the second molding surface, the at least one positioning piece being at one end of the soluble core component, and a remaining portion of the soluble core component coupled to the at least one positioning piece does not contact the first molding surface or the second molding surface.
8. the first molding surface is further defined by a first plug cavity portion connected to the first component cavity portion, and the second molding surface is defined by a second plug cavity portion connected to the second component cavity portion; prior to forming the assembly mold, placing a fusible plug in the first plug cavity portion or the second plug cavity portion, the fusible plug occupying a plug receiving space defined by the first plug cavity portion and the second plug cavity portion when the second mold component is mated with the first mold component; curing the lens component material in the assembly mold, the assembly mold containing the fusible plug; The method of claim 1 further comprising:
9. The method of claim 1 , wherein the lens component is a lens haptic, and a haptic chamber is formed in the haptic when the soluble core component dissolves.
10. The method of claim 1 , wherein the lens component is an optic portion of a lens, and an optic portion chamber is formed within the optic portion when the soluble core component melts.
11. The method of claim 1 , wherein the lens component is part of an optic portion of a lens, and when the soluble core component melts, at least a portion of an optic portion chamber is formed.
12. The method of claim 1 , further comprising the step of securing the first mold component to the second mold component with a clamp member after mating the second mold component with the first mold component.
13. 13. The method of claim 12, wherein the clamp member is a clamp cap configured to be removably secured to an upper portion of the first mold component when the second mold component is mated with the first mold component.
14. The method of claim 1 , wherein the second mold component includes a vent configured to allow air to escape while the lens component material is being introduced into the mold cavity.
15. The method of claim 1 , wherein the lens component material is made, in part, from a curable acrylic monomer.
16. 1. A system for manufacturing a lens component, comprising: a first mold component including a first molding surface defined by a first component cavity portion; a second mold component including a second molding surface defined by a second component cavity portion; a fusible core component configured to be placed on either the first molding surface or the second molding surface; Including, the first mold component is configured to mate with the second mold component to form an assembly mold; a segment of the fusible core component configured to be disposed within a mold cavity formed by the first component cavity portion and the second component cavity portion when the first mold component is mated with the second mold component; The system, wherein the mold cavity in the assembly mold is configured to receive lens component material for hardening into a molded lens component, and the soluble core component is configured to dissolve in a solvent when the molded lens component is immersed in the solvent.
17. 1. A method for manufacturing a lens component, comprising the steps of: providing a first mold component including a first molding surface defined by a first component cavity portion, said first mold component being fabricated from a fusible material; providing a second mold component including a second molding surface defined by a second component cavity portion, said second mold component being fabricated from said fusible material; placing at least a portion of a soluble core component on the first molding surface or the second molding surface, the soluble core component being made of the soluble material; mating the second mold component with the first mold component to form an assembly mold, a segment of the fusible core component being disposed within a mold cavity formed by the first component cavity portion and the second component cavity portion; introducing a lens component material into the mold cavity; curing the lens component material in the assembly mold to form a molded lens component; immersing the assembly mold containing the molded lens component in a solvent to dissolve the soluble core component, the first mold component, and the second mold component; The method includes:
18. 1. A system for manufacturing a lens component, comprising: a first mold component including a first molding surface defined by a first component cavity portion, the first mold component being fabricated from a fusible material; a second mold component including a second molding surface defined by a second component cavity portion, the second mold component being fabricated from the fusible material; a fusible core component configured to be placed on either of the first molding surface and the second molding surface; Including, the first mold component is configured to mate with the second mold component to form an assembly mold; a segment of the fusible core component is disposed within a mold cavity formed by the first component cavity portion and the second component cavity portion when the first mold component is mated with the second mold component; the mold cavity in the assembly mold is configured to receive a lens component material for curing into a molded lens component; The system, wherein the soluble core component, the first mold component, and the second mold component are configured to dissolve in a solvent when the assembly mold is immersed in the solvent.
19. 1. A method for manufacturing a lens component, comprising the steps of: providing a first mold component including a first molding surface defined by a first component cavity portion, said first mold component being fabricated from a fusible material; providing a second mold component including a second molding surface defined by a second component cavity portion; placing at least a portion of a soluble core component on the first molding surface or the second molding surface, the soluble core component being made of the soluble material; mating a second mold component with the first mold component to form an assembly mold, a segment of the fusible core component being disposed within a mold cavity formed by the first component cavity portion and the second component cavity portion; introducing a lens component material into the mold cavity; curing the lens component material in the assembly mold to form a molded lens component; immersing the first mold component and the molded lens component in a melt to dissolve the first mold component and the soluble core component; The method includes:
20. 1. A system for manufacturing a lens component, comprising: a first mold component including a first molding surface defined by a first component cavity portion, the first mold component being fabricated from a fusible material; a second mold component including a second molding surface defined by a second component cavity portion; a soluble core component configured to be placed on the first molding surface or the second molding surface; Including, the first mold component is configured to mate with the second mold component to form an assembly mold; a segment of the soluble component is configured to be disposed within a mold cavity formed by the first component cavity portion and the second component cavity portion when the first mold component is mated with the second mold component; the mold cavity in the assembly mold is configured to receive a lens component material for curing into a molded lens component; The method, wherein the soluble core component and the first mold component are configured to dissolve in a solvent when the first mold component and the molded lens component material are immersed in the solvent.