Magnetic sensor and manufacturing method thereof

The magnetic sensor addresses sensitivity and variation issues by using a magnetic flux collector with precise surface flatness to minimize gaps, enhancing detection consistency and reducing manufacturing costs.

JP7553280B2Active Publication Date: 2024-09-18TDK CORP
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2020135062
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-08-07
Publication Date
2024-09-18
Estimated Expiration
2040-08-07

AI Technical Summary

Technical Problem

Existing magnetic sensors face issues with gaps between the element forming surface of the sensor chip and the magnetic collector, affecting detection sensitivity and variation between products due to low machining accuracy and unclear surface properties.

Method used

The magnetic sensor is designed with a magnetic flux collector having surfaces with an arithmetic mean waviness of 0.1 μm or less, ensuring close contact and reduced gaps, and using selective grinding or polishing to enhance flatness without unnecessary cost increases.

Benefits of technology

This design significantly reduces detection sensitivity variations and maintains high sensitivity by controlling gap size, ensuring consistent performance across products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007553280000008
    Figure 0007553280000008
  • Figure 0007553280000007
    Figure 0007553280000007
  • Figure 0007553280000004
    Figure 0007553280000004
Patent Text Reader

Abstract

To control the size of a gap generated between an element formation surface and a magnetism collecting body based on the surface nature of the magnetism collecting body so that variations between products fall within a certain range.SOLUTION: A magnetic sensor comprises: a sensor chip 20 that is mounted such that an element formation surface 20a becomes perpendicular to a substrate 2; and a magnetism collecting body 30 that is mounted such that a surface 31 is opposite to the substrate 2 and a surface 32 is opposite to the element formation surface 20a. In the magnetism collecting body 30, the arithmetic average waviness Wa of the surface 32 is 0.1 μm or less. In this way, when the surface 32 of the magnetism collecting body 30 opposite to the element formation surface 20a is flattened to have an arithmetic average waviness of 0.1 μm or less, a reduction in detection sensitivity caused by the gap between the element formation surface 20a and the magnetism collecting body 30 can be reduced to a large extent and variations in detection sensitivity between products can be reduced to a large extent.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a magnetic sensor and a manufacturing method thereof, and more particularly to a magnetic sensor including a sensor chip and a magnetic collector mounted on the surface of a substrate, and a manufacturing method thereof. [Background technology]

[0002] Magnetic sensors are widely used in ammeters, magnetic encoders, etc. In some magnetic sensors, a magnetic collector is provided to collect magnetic flux on a sensor chip in order to increase detection sensitivity. For example, Patent Document 1 discloses a magnetic sensor including a sensor chip mounted on a substrate such that an element forming surface is perpendicular to the substrate, and a magnetic collector mounted on the substrate such that an end of the sensor chip faces the element forming surface.

[0003] The magnetic sensor described in Patent Document 1 has the sensor chip mounted on the substrate at an angle of 90 degrees so that the element formation surface is perpendicular to the substrate. This has the advantage that even when a long magnetic collector is used, the magnetic collector can be stably held on the substrate. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2017-090192 A Summary of the Invention [Problem to be solved by the invention]

[0005] However, if the processing precision of the magnetic collector is low, the element formation surface of the sensor chip and the magnetic collector may not be completely in contact with each other, resulting in a small gap between them. This gap has a large effect on the detection sensitivity of the magnetic field, so it is desirable to make it as small as possible, and it is also desirable to control the size of the gap so that the variation between products falls within a certain range.

[0006] Here, in order to make the gap between the element formation surface of the sensor chip and the magnetic collector as small as possible and to control the size of the gap so that the variation between products falls within a certain range, one method is to grind or polish the surface of the magnetic collector to increase the flatness of each surface and make the angle between the two surfaces closer to 90°.

[0007] However, in the past, the relationship between the surface properties of the magnetic collector and the gap that occurs between the element formation surface and the magnetic collector was unclear, making it difficult to suppress variation between products.

[0008] Therefore, an object of the present invention is to provide a magnetic sensor and a manufacturing method thereof that can control the size of the gap between the element forming surface and the magnetic collector based on the surface properties of the magnetic collector so that variation between products falls within a certain range. [Means for solving the problem]

[0009] The magnetic sensor according to the present invention comprises a substrate, a sensor chip having an element forming surface on which a magnetic sensing element is formed, the sensor chip being mounted on the surface of the substrate so that the element forming surface is perpendicular to the surface of the substrate, and a magnetic collector mounted on the surface of the substrate so that its first surface faces the surface of the substrate and its second surface faces the element forming surface of the sensor chip, and is characterized in that the arithmetic mean waviness Wa of the second surface is 0.1 μm or less.

[0010] According to the present invention, the arithmetic mean waviness Wa of the second surface of the magnetic collector facing the element forming surface is flattened to 0.1 μm or less, thereby making it possible to significantly reduce the decrease in detection sensitivity caused by the gap between the element forming surface and the magnetic collector, and to significantly suppress the variation in detection sensitivity between products.

[0011] In the present invention, the magnetic collector may have a first and second surface with a higher flatness than at least one other surface. In this case, the flatness of the at least one other surface of the magnetic collector is not improved, and therefore unnecessary manufacturing costs for processing the surface are not incurred. This makes it possible to suppress an increase in manufacturing costs.

[0012] In the present invention, the magnetic collector has a third surface, the sensor chip and the magnetic collector are fixed to each other via an adhesive applied to the third surfaces of the sensor chip and the magnetic collector, and the flatness of the first and second surfaces may be higher than that of the third surface. This avoids unnecessary manufacturing costs for processing the third surface. Moreover, since the third surface has low flatness, it is possible to ensure sufficient adhesive strength by the adhesive.

[0013] In the present invention, the magnetic collector further has a fourth surface, the substrate and the magnetic collector are fixed to each other via an adhesive applied to the surface of the substrate and the fourth surface of the magnetic collector, and the flatness of the first and second surfaces may be higher than the flatness of the fourth surface. This avoids unnecessary manufacturing costs for processing the fourth surface. Moreover, since the fourth surface has low flatness, it is possible to ensure sufficient adhesive strength by the adhesive.

[0014] In the present invention, the magnetic collector may be made of a ferrite material. Although the ferrite material has low flatness in the state after cutting, it is possible to selectively increase the flatness of the first and second surfaces by grinding or polishing.

[0015] The method for manufacturing a magnetic sensor according to the present invention is characterized by comprising a first step of cutting out a magnetic collector from a block made of a magnetic material; a second step of grinding or polishing the magnetic collector having first and second surfaces so that the arithmetic mean waviness Wa of the second surface is 0.1 μm or less; a third step of mounting a sensor chip on the surface of a substrate so that the element forming surface on which the magnetic sensing element is formed is perpendicular to the surface of the substrate; and a fourth step of mounting the magnetic collector on the surface of the substrate so that the first surface faces the surface of the substrate and the second surface faces the element forming surface of the sensor chip.

[0016] According to the present invention, the arithmetic mean waviness Wa of the second surface of the magnetic collector facing the element forming surface is flattened to 0.1 μm or less, thereby making it possible to significantly reduce the decrease in detection sensitivity caused by the gap between the element forming surface and the magnetic collector, and to significantly suppress the variation in detection sensitivity between products.

[0017] In the second step, the first and second surfaces of the magnetic collector may be selectively ground or polished to selectively increase the flatness of the first and second surfaces. In this manner, by selectively grinding or polishing the first and second surfaces of the magnetic collector, the flatness of the first and second surfaces is increased, while the increase in manufacturing costs associated with grinding or polishing can be minimized.

[0018] In the present invention, the fourth step may be performed while biasing the magnetic collector so that the second surface of the magnetic collector is pressed against the element formation surface of the sensor chip, thereby making it possible to further reduce the gap between the element formation surface of the sensor chip and the magnetic collector.

[0019] In the present invention, the magnetic collector has a third surface, and in the second step, the first and second surfaces are ground or polished without grinding or polishing the third surface, and in the fourth step, an adhesive may be applied to the third surfaces of the sensor chip and the magnetic collector. This avoids unnecessary manufacturing costs for processing the third surface. Moreover, since the third surface has low flatness, it is possible to ensure sufficient adhesive strength by the adhesive.

[0020] In the present invention, the magnetic collector further has a fourth surface, and in the second step, the first and second surfaces are ground or polished without grinding or polishing the fourth surface, and in the fourth step, an adhesive may be applied to the surface of the substrate and the fourth surface of the magnetic collector. This avoids unnecessary manufacturing costs for processing the fourth surface. Moreover, since the fourth surface has low flatness, it is possible to ensure sufficient adhesive strength by the adhesive. Effect of the Invention

[0021] Thus, according to the present invention, it is possible to control the size of the gap that occurs between the element formation surface and the magnetic collector based on the surface properties of the magnetic collector so that variation between products falls within a certain range. [Brief description of the drawings]

[0022] [Figure 1] FIG. 1 is a schematic perspective view showing the appearance of a magnetic sensor 10 according to a preferred embodiment of the present invention. [Diagram 2] FIG. 2 is a schematic perspective view for explaining the structure of an element formation surface 20a of the sensor chip 20. As shown in FIG. [Diagram 3] FIG. 3 is a circuit diagram for explaining the connection relationship of the magnetic sensing elements R1 to R4. [Figure 4] FIG. 4 is a schematic perspective view for explaining the structure of the magnetic collector 30. As shown in FIG. [Diagram 5] 5(a) to (c) are schematic diagrams for explaining the application positions of adhesives 71 to 73. FIG. [Figure 6] FIG. 6 is a graph showing the relationship between the arithmetic mean waviness Wa of the surface 32 of the magnetic collector 30 and the gap G occurring between the element forming surface 20a and the magnetic collector 30. As shown in FIG. [Figure 7] FIG. 7 is a graph showing the relationship between the gap G and the sensitivity of the magnetic sensor 10. As shown in FIG. [Figure 8] FIG. 8 is a flowchart illustrating the manufacturing process of the magnetic sensor 10. [Figure 9] FIG. 9 is a schematic diagram for explaining a method for supplying and hardening the adhesive 71 while biasing the magnetic collector 30. As shown in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0023] Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the accompanying drawings.

[0024] FIG. 1 is a schematic perspective view showing the appearance of a magnetic sensor 10 according to a preferred embodiment of the present invention.

[0025] 1, the magnetic sensor 10 according to this embodiment includes a substrate 2 whose surface constitutes an xz plane, and a sensor chip 20 and magnetic collectors 30, 41, 42 mounted on the surface of the substrate 2. The sensor chip 20 has an element forming surface 20a that constitutes an xy plane, and one end of the magnetic collector 30 in the z direction faces the element forming surface 20a. The magnetic collectors 41, 42 are provided on the back side of the sensor chip 20. The magnetic collectors 30, 41, 42 are blocks made of a soft magnetic material with high magnetic permeability, such as ferrite.

[0026] 1, in this embodiment, the sensor chip 20 is mounted so that the element forming surface 20a of the sensor chip 20 is perpendicular to the surface of the substrate 2. That is, the sensor chip 20 is mounted in a state where it is laid down at an angle of 90° with respect to the substrate 2. Therefore, even if the length of the magnetic collector 30 in the z direction is long, the magnetic collector 30 can be stably fixed to the substrate 2.

[0027] FIG. 2 is a schematic perspective view for explaining the structure of an element formation surface 20a of the sensor chip 20. As shown in FIG.

[0028] As shown in FIG. 2, the sensor chip 20 has a substantially rectangular parallelepiped shape, and four magnetic sensing elements R1 to R4 are formed on the element forming surface 20a that constitutes the xy plane. The magnetic sensing elements R1 to R4 are not particularly limited as long as they are elements whose characteristics change depending on the direction or strength of a magnetic field, and for example, magnetoresistance elements can be used. In the following description, an example will be described in which the magnetic sensing elements R1 to R4 are magnetic resistance elements and have the same magnetization fixed direction. Here, the positions of the magnetic sensing elements R1 and R3 in the x direction are the same, and the positions of the magnetic sensing elements R2 and R4 in the x direction are the same. In addition, the positions of the magnetic sensing elements R1 and R4 in the y direction are the same, and the positions of the magnetic sensing elements R2 and R3 in the y direction are the same.

[0029] The magnetic layers 21 to 23 are formed on the element forming surface 20a of the sensor chip 20. The magnetic layer 21 is located at the approximate center of the element forming surface 20a in a plan view, and the magnetic layers 22 and 23 are arranged on both sides of the magnetic layer 21 in the x direction. Although not particularly limited, the magnetic layers 21 to 23 may be a film made of a composite magnetic material in which a magnetic filler is dispersed in a resin material, a thin film or foil made of a soft magnetic material such as nickel or permalloy, or a thin film or bulk sheet made of ferrite or the like. The magnetic sensing elements R1 and R3 are arranged in the gap formed by the magnetic layer 21 and the magnetic layer 22, and the magnetic sensing elements R2 and R4 are arranged in the gap formed by the magnetic layer 21 and the magnetic layer 23.

[0030] The magnetic collector 30 is disposed between the magnetic sensing elements R1, R3 and the magnetic sensing elements R2, R4 in a plan view, i.e., when viewed from the z direction, and has a rectangular parallelepiped shape with the z direction as the longitudinal direction. The magnetic collector 30 collects magnetic flux in the z direction and splits it to both sides in the x direction on the element forming surface 20a. The height of the magnetic collector 30 in the z direction is not particularly limited, but by increasing the height in the z direction, the selectivity of the magnetic flux in the z direction can be improved. In this embodiment, the width of the magnetic collector 30 in the y direction is approximately the same as the width of the sensor chip 20 in the y direction, but the present invention is not limited thereto.

[0031] One side surface and half of the back surface of the sensor chip 20 are covered by a magnetic collector 41. Similarly, the other side surface and the remaining half of the back surface of the sensor chip 20 are covered by a magnetic collector 42. Although the provision of the magnetic collectors 41 and 42 is not essential in the present invention, providing the magnetic collectors 41 and 42 makes it possible to further improve selectivity for magnetic flux in the z direction. The magnetic collectors 41 and 42 are extended in the z direction so that their positions in the z direction exceed the element forming surface 20a, and further have overhanging portions OH1 and OH2 bent from this extended portion toward the element forming surface 20a.

[0032] With this configuration, when viewed from the z direction, the magnetic sensing elements R1, R3 are located between the magnetic collector 30 and the overhanging portion OH1 of the magnetic collector 41, and the magnetic sensing elements R2, R4 are located between the magnetic collector 30 and the overhanging portion OH2 of the magnetic collector 42. Therefore, the magnetic flux collected by the magnetic collector 30 is distributed almost evenly to both sides in the x direction, and then is absorbed into the magnetic collectors 41, 42 via the overhanging portions OH1, OH2. At this time, a part of the magnetic flux passes through the magnetic sensing elements R1 to R4, so that the magnetic sensing elements R1, R3 and the magnetic sensing elements R2, R4 are provided with magnetic flux in the opposite directions to each other.

[0033] FIG. 3 is a circuit diagram for explaining the connection relationship of the magnetic sensing elements R1 to R4.

[0034] As shown in Fig. 3, the magnetic sensing element R1 is connected between the terminal electrodes 53 and 56, the magnetic sensing element R2 is connected between the terminal electrodes 54 and 55, the magnetic sensing element R3 is connected between the terminal electrodes 53 and 54, and the magnetic sensing element R4 is connected between the terminal electrodes 55 and 56. Here, the terminal electrode 56 is given a power supply potential Vcc, and the terminal electrode 54 is given a ground potential GND. The magnetic sensing elements R1 to R4 all have the same magnetization fixed direction, and there is a difference between the resistance change amount of the magnetic sensing elements R1 and R3 located on one side as viewed from the magnetic collector 30 and the resistance change amount of the magnetic sensing elements R2 and R4 located on the other side as viewed from the magnetic collector 30. As a result, the magnetic sensing elements R1 to R4 form a differential bridge circuit, and the change in the electrical resistance of the magnetic sensing elements R1 to R4 according to the magnetic flux density appears on the terminal electrodes 53 and 55.

[0035] The differential signal output from the terminal electrodes 53, 55 is input to a differential amplifier 61 provided on the substrate 2 or outside thereof. The output signal of the differential amplifier 61 is fed back to the terminal electrode 52. As shown in FIG. 3, a compensation coil C is connected between the terminal electrodes 51 and 52, and the compensation coil C generates a magnetic field according to the output signal of the differential amplifier 61. The compensation coil C can be integrated into the sensor chip 20. With this configuration, when the change in the electrical resistance of the magnetic sensing elements R1 to R4 according to the magnetic flux density appears in the terminal electrodes 53, 55, a current according to the magnetic flux density flows in the compensation coil C, generating a magnetic flux in the opposite direction. This cancels out the external magnetic flux. Then, if the current output from the differential amplifier 61 is converted into a current-voltage by the detection circuit 62, it becomes possible to detect the strength of the external magnetic flux.

[0036] FIG. 4 is a schematic perspective view for explaining the structure of the magnetic collector 30. As shown in FIG.

[0037] As shown in Fig. 4, the magnetic collector 30 is a substantially rectangular parallelepiped having six surfaces 31 to 36. Of these, surface 31 is a surface that constitutes an xz plane, and faces the surface of the substrate 2 when mounted. Surface 32 is a surface that constitutes an xy plane, and faces the element formation surface 20a of the sensor chip 20 when mounted. Surface 33 is an xz plane located opposite surface 31. Surface 34 is an xy plane located opposite surface 32. Surfaces 35 and 36 are yz planes located opposite each other.

[0038] In this embodiment, the flatness of the surfaces 31 and 32 of the magnetic collector 30 is higher than that of the other surfaces 33 to 36. This is the result of selectively grinding or polishing the surfaces 31 and 32 of the magnetic collector 30, as described later. By grinding or polishing the surfaces 31 and 32 of the magnetic collector 30, not only is the flatness of the surfaces 31 and 32 increased, but the angle between the surfaces 31 and 32 is made closer to 90°. As a result, when the magnetic collector 30 is mounted on the substrate 2, the surface 31 adheres to the surface of the substrate 2 with almost no gap, and the surface 32 adheres to the element forming surface 20a of the sensor chip 20 with almost no gap. This makes it possible to suppress a decrease in detection sensitivity caused by a gap between the element forming surface 20a and the magnetic collector 30, and to reduce the variation in detection sensitivity between products.

[0039] In particular, the surface 32 facing the element forming surface 20a is flattened so that the arithmetic mean waviness Wa (defined in JIS B 0601:2013) is 0.1 μm or less. If the arithmetic mean waviness Wa of the surface 32 is 0.1 μm or less, it is possible to significantly reduce the decrease in detection sensitivity caused by the gap between the element forming surface 20a and the magnetic collector 30, and to significantly suppress the variation in detection sensitivity between products. Furthermore, if the surface 31 of the magnetic collector 30 is flattened, the friction between the surface 31 of the magnetic collector 30 and the substrate 2 is reduced, making it easier to slide the magnetic collector 30 on the substrate 2 and bring it into contact with the sensor chip 20 during assembly. The arithmetic mean waviness Wa of the surface 31 may be the same as that of the surface 32, or may be larger than that of the surface 32.

[0040] As shown in FIG. 5, adhesives 71 to 73 can be used to fix the magnetic collector 30. In the example shown in FIG. 5(a), the adhesive 71 is applied over the surface 33 of the magnetic collector 30 and the upper surface (xz surface) 20b of the sensor chip 20, thereby fixing the relative positional relationship between the sensor chip 20 and the magnetic collector 30. The surface 33 of the magnetic collector 30 is preferably rougher than the surfaces 31 and 32. This can increase the adhesive strength of the adhesive 71 compared to a case in which the surface 33 of the magnetic collector 30 has the same flatness as the surfaces 31 and 32. In addition, if the adhesive 71 seeps into the gap between the surface 32 of the magnetic collector 30 and the element forming surface 20a, the gap between them may widen. However, in this embodiment, the flatness of the surface 32 of the magnetic collector 30 is increased, so that the adhesive 71 is unlikely to seep in due to surface tension.

[0041] 5(b), an adhesive 72 is applied over the surface 34 of the magnetic collector 30 and the surface of the substrate 2, thereby fixing the relative positional relationship between the substrate 2 and the magnetic collector 30. The surface 34 of the magnetic collector 30 is preferably rougher than the surfaces 31 and 32. This makes it possible to increase the adhesive strength of the adhesive 72 compared to a case in which the surface 34 of the magnetic collector 30 has the same flatness as the surfaces 31 and 32.

[0042] 5(c), an adhesive 73 is applied over the surfaces 35, 36 of the magnetic collector 30 and the surface of the substrate 2, thereby fixing the relative positional relationship between the substrate 2 and the magnetic collector 30. The surfaces 35, 36 of the magnetic collector 30 are preferably rougher than the surfaces 31, 32. This makes it possible to increase the adhesive strength of the adhesive 73 compared to a case in which the surfaces 35, 36 of the magnetic collector 30 have the same flatness as the surfaces 31, 32.

[0043] However, in the present invention, it is not essential to use all of the adhesives 71 to 73, and some of the adhesives, for example, the adhesive 73, may be omitted.

[0044] FIG. 6 is a graph showing the relationship between the arithmetic mean waviness Wa of the surface 32 of the magnetic collector 30 and the gap G occurring between the element forming surface 20a and the magnetic collector 30. As shown in FIG.

[0045] As shown in Fig. 6, in a plurality of samples in which the arithmetic mean waviness Wa of the surface 32 is 0.5 µm, the measured value of the gap G varies widely between about 20 µm and about 100 µm. The value and the variation of the gap G decrease as the arithmetic mean waviness Wa of the surface 32 decreases, and in a plurality of samples in which Wa is 0.3 µm, the measured value of the gap G is about 10 µm to about 40 µm (variation about 30 µm), in a plurality of samples in which Wa is 0.2 µm, the measured value of the gap G is about 0 µm to about 30 µm (variation about 30 µm), and in a plurality of samples in which Wa is 0.1 µm, the measured value of the gap G is about 0 µm to about 10 µm (variation about 10 µm). In this way, if Wa is 0.1 µm, not only is the absolute value of the gap G reduced, but the variation of the gap G can be significantly suppressed. The smaller the arithmetic mean waviness Wa of the surface 32, the better the characteristics are. However, although it depends on the material properties and polishing method of the magnetic collector 30, it is practically difficult to reduce the arithmetic mean waviness Wa to less than 0.01 μm. Considering this point, a realistic value of Wa is 0.01 μm or more and 0.1 μm or less, and preferably 0.03 μm or more and 0.05 μm or less.

[0046] FIG. 7 is a graph showing the relationship between the gap G and the sensitivity of the magnetic sensor 10. As shown in FIG.

[0047] 7, although the sensitivity of the magnetic sensor 10 is not uniquely determined by the gap G, it is clearly evident that the sensitivity increases as the gap G becomes narrower. In other words, the smaller the arithmetic mean waviness Wa of the surface 32, the higher the sensitivity of the magnetic sensor 10. Furthermore, by flattening the surface 32 so that the arithmetic mean waviness Wa is 0.1 μm or less, it is possible to obtain high sensitivity and significantly suppress the variation in sensitivity.

[0048] Next, a method for manufacturing the magnetic sensor 10 according to the present embodiment will be described.

[0049] FIG. 8 is a flowchart illustrating the manufacturing process of the magnetic sensor 10 according to the present embodiment.

[0050] First, the magnetic collector 30 is cut out from a block made of a magnetic material such as ferrite (step S11), and then the surfaces 31, 32 of the magnetic collector 30 are ground or polished to improve the flatness of the surfaces 31, 32 (step S12). Immediately after the magnetic collector 30 is cut out, the flatness of each of the surfaces 31 to 36 is low, and the angle between the two surfaces is also low in accuracy. However, if the surfaces 31, 32 of the magnetic collector 30 are ground or polished, the flatness of the surfaces 31, 32 is improved, and the angle between the surfaces 31 and 32 approaches 90°. The other surfaces 33 to 36 are not ground or polished, which prevents an unnecessary increase in manufacturing costs. However, grinding or polishing may be performed on some of the surfaces 33 to 36.

[0051] Meanwhile, in parallel with the processing of the magnetic collector 30, the sensor chip 20 is mounted so that the element forming surface 20a is perpendicular to the substrate 2 (step S21). Thereafter, the processed magnetic collector 30 is mounted on the surface of the substrate 2 (step S22). The magnetic collector 30 is mounted so that the surface 31 faces the surface of the substrate 2 and the surface 32 faces the element forming surface 20a of the sensor chip 20. As described above, the surfaces 31 and 32 of the magnetic collector 30 are highly flat, and the angle between the surfaces 31 and 32 is as close to 90° as possible, so that the surface 32 of the magnetic collector 30 can be closely attached to the element forming surface 20a of the sensor chip 20 with almost no gap.

[0052] Next, the magnetic collector 30 is fixed by supplying and curing adhesives 71 to 73 (step S23). At this time, it is preferable to supply and cure the adhesive while biasing the magnetic collector 30 so that the front surface 32 of the magnetic collector 30 is properly pressed against the element formation surface 20a of the sensor chip 20 and fixed. For example, as shown in FIG. 9, it is preferable to supply the adhesive 71 from the dispenser 70 after placing the magnetic collector 30 on the substrate 2 while biasing the magnetic collector 30 from the front surface 34 side in the -z direction by a biasing jig 81. At this time, it is preferable to support the back side of the sensor chip 20 by a fixing jig 82 so that the sensor chip 20 does not move in the -z direction or fall over. If such jigs 81, 82 are used to supply and harden the adhesive 71, the surface 32 of the magnetic collector 30 is kept properly pressed against the element forming surface 20a of the sensor chip 20, and the adhesive 71 can be prevented from seeping between the surface 32 of the magnetic collector 30 and the element forming surface 20a of the sensor chip 20. If the surface 31 of the magnetic collector 30 is also flattened, friction between the magnetic collector 30 and the substrate 2 is reduced, making it easier to slide the magnetic collector 30 on the substrate 2 and bring it into contact with the sensor chip 20.

[0053] The adhesives 72 and 73 can be supplied and hardened in the same manner, and can be hardened while the jigs 81 and 82 are used to fix the adhesives 72 and 73 in place.

[0054] As described above, in the magnetic sensor 10 according to this embodiment, the flatness of the surfaces 31, 32 of the magnetic collector 30 is selectively enhanced, so that the surface 32 of the magnetic collector 30 can be closely attached to the element forming surface 20a of the sensor chip 20 with almost no gap. Moreover, seepage of the adhesive 71 between the surface 32 of the magnetic collector 30 and the element forming surface 20a of the sensor chip 20 is also unlikely to occur. Furthermore, since grinding or polishing is not performed on at least a part of the other surfaces 33 to 36, the adhesive strength of the adhesives 71 to 73 can be sufficiently ensured.

[0055] Although a preferred embodiment of the present invention has been described above, the present invention is not limited to the above embodiment, and various modifications are possible without departing from the spirit of the present invention, and it goes without saying that these modifications are also included within the scope of the present invention. [Explanation of symbols]

[0056] 2. Board 10 Magnetic Sensor 20 Sensor chip 20a Element formation surface 20b Top surface of sensor chip 21~23 Magnetic layer 30,41,42 Magnetic collector 31~36 Surface of magnetic collector 51~56 Terminal electrode 61 Differential Amplifier 62 Detection circuit 70 Dispenser 71~73 Adhesive 81 Pressing tool 82 Fixture C Compensation coil OH1,OH2 overhanging part R1~R4 Magnetic sensing element

Claims

1. A substrate; a sensor chip having an element forming surface on which a magnetic sensing element is formed, the element forming surface being mounted on the surface of the substrate such that the element forming surface is perpendicular to the surface of the substrate; a magnetic collector mounted on the surface of the substrate such that a first surface faces the surface of the substrate and a second surface faces the element formation surface of the sensor chip; the magnetic collector has a third surface opposite the first surface; the sensor chip and the magnetic collector are fixed to each other via an adhesive applied to the third surfaces of the sensor chip and the magnetic collector, the flatness of the second surface is greater than the flatness of the first surface; the first surface has a flatness greater than the flatness of the third surface; A magnetic sensor comprising: said second surface having an arithmetic mean waviness Wa of 0.1 μm or less.

2. the magnetic collector further has a fourth surface opposite the second surface; the substrate and the magnetic collector are fixed to each other via an adhesive applied to the first surface of the substrate and the fourth surface of the magnetic collector; 2. The magnetic sensor according to claim 1, wherein the first and second surfaces have a flatness greater than a flatness of the fourth surface.

3. The magnetic collector further has fifth and sixth surfaces that are perpendicular to the first to fourth surfaces and opposite each other, the substrate and the magnetic collector are fixed to each other via an adhesive applied to the surface of the substrate and the fifth and sixth surfaces of the magnetic collector; 3. The magnetic sensor according to claim 2, wherein the first and second surfaces have a flatness higher than that of the fifth and sixth surfaces.

4. 4. The magnetic sensor according to claim 1, wherein the magnetic collector is made of a ferrite material.

5. A first step of cutting out a magnetic collector from a block of a magnetic material; a second step of grinding or polishing the first and second surfaces of the magnetic collector, the magnetic collector having a first and second surface and a third surface located opposite the first surface, without grinding or polishing the third surface, to make the flatness of the second surface higher than that of the first surface, make the flatness of the first surface higher than that of the third surface, and make the arithmetic mean waviness Wa of the second surface 0.1 μm or less; a third step of mounting the sensor chip on the surface of the substrate such that an element forming surface on which the magnetic sensing element is formed is perpendicular to the surface of the substrate; a fourth step of mounting the magnetic collector on the surface of the substrate so that the first surface faces the surface of the substrate and the second surface faces the element forming surface of the sensor chip, and applying an adhesive to the sensor chip and the third surfaces of the magnetic collector.

6. 6. The method for manufacturing a magnetic sensor according to claim 5, wherein the fourth step is performed while biasing the magnetic collector so that the second surface of the magnetic collector is pressed against the element formation surface of the sensor chip.

7. the magnetic collector further has a fourth surface opposite the second surface; In the second step, the first and second surfaces are ground or polished without grinding or polishing the fourth surface; 6. The method for manufacturing a magnetic sensor according to claim 5, wherein in the fourth step, an adhesive is applied to the surface of the substrate and the fourth surface of the magnetic collector.

8. The magnetic collector further has fifth and sixth surfaces that are perpendicular to the first to fourth surfaces and opposite each other, In the second step, the first and second surfaces are ground or polished without grinding or polishing the fifth and sixth surfaces; 8. The method for manufacturing a magnetic sensor according to claim 7, wherein in the fourth step, an adhesive is applied to the surface of the substrate and the fifth and sixth surfaces of the magnetic collector.

Citation Information

Patent Citations

  • Magnetic sensor for japanese pinball game pachinko machine

    JP1993212152A

  • Manufacturing method of magnet array for magnetic sensor and manufacturing method of magnetic sensor

    JP2012247219A

  • Magnetic sensor

    JP2017090192A

  • Magnetic sensor

    JP2018194393A

  • Magnetic sensor

    JP2019219182A