Printing stencil and its manufacturing method

The printing stencil with a hard film and controlled through holes addresses the challenge of thin film thickness and pattern continuity, ensuring uniformity and durability in printed layers.

JP7554035B2Active Publication Date: 2024-09-19TAIYO YUDEN KK
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2018079525
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2018-04-18
Publication Date
2024-09-19
Estimated Expiration
2038-04-18

AI Technical Summary

Technical Problem

Existing printing stencils face challenges in achieving thin film thickness with minimal variations and forming continuous planar patterns due to issues with ink or paste division by opening walls and difficulty in producing uniform metal plates with submicron thickness.

Method used

A printing stencil with a hard film having concave portions or holes that define a printing pattern, featuring through holes with controlled thickness variations and a smaller opening area than the printed pattern, and a base material with fine irregularities to enhance ink transfer.

Benefits of technology

The solution enables the formation of thin printed layers with minimal thickness variations and uniformity, preventing ink separation by mesh intersections and improving durability and handleability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007554035000002
    Figure 0007554035000002
  • Figure 0007554035000003
    Figure 0007554035000003
  • Figure 0007554035000001
    Figure 0007554035000001
Patent Text Reader

Abstract

To provide a printing stencil having little dispersion of a printed film thickness, capable of obtaining a thin print layer.SOLUTION: A printing stencil includes a tabular substrate having a surface on the printed substrate side, and a surface on the squeegee side opposite thereto, a hard film formed on the surface on the printed substrate side of the substrate, and including a concave part or a hole part for defining a printing pattern, and a penetration hole having an opening space smaller than an area of a printing pattern shape part, and penetrating the printing pattern shape part from the concave part or the hole part to the surface on the squeegee side of the substrate, in which the hard film has a thickness of 1 nm-5 μm, and has thickness dispersion of 10% or less.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a printing stencil and a method for manufacturing the same. [Background technology]

[0002] Recently, there has been a high demand for print position accuracy in multilayer electronic components in which internal electrodes are formed by printing. For example, there is now a demand for a control width of several microns for print position accuracy and bleeding of printed matter, which are related to the lamination accuracy of electronic components. Also, for multilayer electronic components with thin-film internal electrodes such as capacitors, the printing film thickness is becoming less than 100 nm. Thus, in the field of thin-film printing, such as printing of internal electrodes for electronic components, there is a steady demand for thinner, more precise printing with less misalignment.

[0003] The emulsion screen plate, which is the most popular printing stencil plate, is manufactured as a screen printing plate having a pattern by using, for example, a metal mesh or a resin mesh such as polyester, which is formed by electroplating or etching, or stainless steel or tungsten, which is previously stretched on a frame, as a support, and applying a flowable photosensitive emulsion to the surface layer of the mesh with a bucket or a coating machine to form a photosensitive film, and then exposing and developing the film by a known photolithography method to form a patterned member for printing.In addition, instead of applying the emulsion, a method is also known in which a photosensitive layer of a photosensitive film, which is a film coated with a photosensitive layer, is attached to the surface layer of the mesh, dried, and then the film is peeled off and exposed and developed in the same manner to form a printing patterning member (direct-indirect method). Emulsion screen printing plates have problems in that the printing pattern itself is composed of a soft emulsion resin, and therefore the printing durability, the resistance to wiping and cleaning, and the resistance to the solvents used for cleaning are insufficient.

[0004] A mesh-integrated metal mask (suspended metal mask) in which a printed pattern is formed from metal foil or plated foil is known as a mask that has improved printing durability, wipe-cleanability, and resistance to solvents used in cleaning compared to emulsion screen plates. This is a mask in which a metal foil on which a printed pattern is formed by mechanical processing such as etching, drilling, or punching, or a method of irradiating a laser beam to make holes, or a plated foil on which a printed pattern is formed by electroforming, is attached to the surface of a metal mesh that is previously stretched on a frame. However, masks other than those using a material that can be bonded to the metal mesh by plating, such as Ni, Ni alloy, or stainless steel, for the metal foil or plated foil on which the printed pattern is formed, have not yet become widespread.

[0005] In the case of the above-mentioned emulsion screen plate, when forming the emulsion layer, it is common to hand-paint liquid emulsion using a bucket onto a screen mesh stretched over a frame, and it has been difficult to suppress variation in the thickness of the emulsion layer, which determines the thickness of the printed material, to the order of several hundred nm. Furthermore, in the above-mentioned emulsion screen plate and mesh-integrated metal mask, an "intersection" where the fiber threads of the mesh fabric overlap is always located at the opening of the wiring pattern. The "intersection" is "bump-shaped" and is thicker toward the printed substrate than the thickness of a single fiber thread that constitutes the mesh, so that the part of the transferred printed wiring pattern that corresponds to the "intersection" is depressed (thinned) in a shape corresponding to the "bump", resulting in the occurrence of so-called "mesh marks". Since the printing film thickness of such mesh marks is thinner than other wiring parts, the cross-sectional area of ​​the printed wiring in the thin part determines the power transmission capacity of the entire wiring, which also causes problems with power transmission loss.

[0006] On the other hand, as a printing stencil not using a mesh, a metal mask is known in which a printing pattern (openings) is formed on a metal plate such as stainless steel by mechanical processing such as etching, drilling, punching, or by irradiating a laser beam to make holes. A method for producing such a metal mask by electroforming is also known. In a method for producing a metal mask by electroforming, for example, a die having a plating resist layer formed on the surface layer of a plate-like member such as a metal such as stainless steel or glass that has been polished smoothly in advance, called a plating mother die, is used, a plating metal layer is formed by depositing plating on the die, and the patterned plating metal layer is peeled off from the die to obtain a metal mask.

[0007] In a printing stencil having openings such as a metal mask, since it is not necessary to form an emulsion layer, there is no variation in the thickness of the printed matter due to the variation in the thickness of the emulsion layer, and since no screen mesh is installed in the openings, the above-mentioned "mesh marks" do not occur. However, the fact that no screen mesh is installed in the openings also means that there is nothing in the printing pattern that reduces the ink permeation volume. In this case, the ink of the volume calculated by multiplying the area of ​​the openings and the thickness of the mask is transferred from the openings during printing, so there is a problem that it is difficult to print thin films with a printing stencil having openings.

[0008] As a means for solving the above-mentioned problems, it has been proposed to make the mask have a dual structure consisting of a pattern portion having a pattern opening corresponding to the printing pattern, and a paste supply portion having a paste supply port for supplying conductive paste to the pattern opening and in contact with the squeegee (Patent Document 1). In addition, as printing stencils of a multilayer (laminate) structure, there have been proposed a printing stencil (Patent Document 2) characterized in that an organic polymer layer having a thickness of 100 nm or more is provided via a coupling agent layer on a substrate made of an inorganic material, an organic material, or an inorganic and organic composite material, and having openings for a printing pattern; a mask for stencil printing having openings for a printing pattern provided on a substrate, the substrate having an aromatic polyimide resin layer and having a diamond-like carbon film on its surface (Patent Document 3); and a mask (Patent Document 4) characterized in that a hard coating is formed on the outer peripheral surface of the mask substrate or at least a portion of the inner wall surface of the through holes formed in the mask substrate. [Prior art documents] [Patent documents]

[0009] [Patent Document 1] JP 2015-229287 A [Patent Document 2] JP 2017-39320 A [Patent Document 3] JP 2005-144973 A [Patent Document 4] Japanese Patent Application Publication No. 11-245371 Summary of the Invention [Problem to be solved by the invention]

[0010] However, even the above-mentioned methods have not yet achieved the formation of a sufficiently thin printed layer. Another method of forming a thin film using a printing stencil having openings is to process the openings into discrete holes and obtain a continuous desired printing pattern by the joining of ink or paste that passes through each of the openings during printing. However, in many cases, the ink or paste is divided by the walls of the openings, making it difficult to form a continuous planar pattern. Another method is to reduce the thickness of the metal plate itself to reduce the amount of ink transferred during printing, but it is difficult to manufacture or obtain a uniform metal plate with a thickness of less than 10 μm, and when it comes to a thickness of submicron, handling is extremely difficult even if it is manufactured by electroforming or other methods.

[0011] SUMMARY OF THE PRESENT EMBODIMENTS An object of the present invention is to provide a printing stencil which solves the above problems and which has a small variation in the printing film thickness and allows a thin printing layer to be obtained. [Means for solving the problem]

[0012] As a result of intensive research into solving the above-mentioned problems, the inventors have found that the above-mentioned problems can be solved by forming a hard film having recesses or holes defining the printing pattern on the surface of the substrate side of the base material forming the printing stencil so as to reduce variation in thickness, and by providing through holes having an opening area smaller than the area of ​​the printing pattern shape portion that penetrates the printing pattern shape portion from within the recesses or holes to the squeegee side surface of the base material.

[0013] That is, in order to solve the above problems, the present invention employs the following means. <1> A printing stencil comprising: a plate-shaped substrate having a surface facing the printed substrate and an opposing surface facing the squeegee; a hard film formed on the surface of the substrate facing the printed substrate and having recesses or holes defining a printing pattern; and through holes penetrating a printing pattern shaped portion from within the recesses or holes to the surface of the substrate facing the squeegee, the opening area of ​​which is smaller than the area of ​​the printing pattern shaped portion, wherein the hard film has a thickness of 1 nm to 5 μm and a variation in thickness is within 10%. <2> A plurality of the through holes are formed in the print pattern shape portion. <1> A printing stencil. <3> The substrate has a surface having minute irregularities. <1> or <2> A printing stencil. <4> The substrate has a corrosion-resistant layer on a surface thereof. <1> ~ <3> Any of the above printing stencils. <5> The substrate is stretched on a plate frame. <1> ~ <4> Any of the above printing stencils. <6> The hard film is one or more films selected from an amorphous carbon film, a metal (including Si) oxide film, a metal (including Si) nitride film, a metal (including Si) carbide film, and a metal (including Si) oxynitride film. <1> ~ <5> Any of the above printing stencils. <7> The amorphous carbon film contains one or more elements selected from N, O, Si, Ti, Al, Zr, B, and As. <6> A printing stencil. <8> The hard film has a Vickers hardness (Hv) of 100 or more. <1> ~ <7> Any of the above printing stencils. <9> The hard film has a Vickers hardness (Hv) of 450 or more. <1> ~ <8> Any of the above printing stencils. <10> A water-repellent layer or a water- and oil-repellent layer is further formed on the print substrate side of the hard film. <1> ~ <9> Any of the above printing stencils. <11> The water-repellent layer or the water- and oil-repellent layer mainly comprises a fluorine-containing coupling agent capable of forming a hydrogen bond and / or an -OM bond (wherein M is any element selected from the group consisting of Si, Ti, Al, and Zr) with the hard film by a condensation reaction. <1> ~ <10> Any of the above printing stencils. <12> A method for manufacturing a printing stencil having a hard film on a surface facing a printed substrate, the method comprising the steps of: preparing a plate-shaped substrate; forming a through hole having an opening area smaller than the area of ​​the printed pattern shape portion in a printed pattern shape portion of the substrate; covering the printed pattern shape portion on the surface of the substrate facing the printed substrate with a masking material; forming a hard film by a dry process on the surface of the substrate facing the printed substrate that is covered with the masking material; and removing the masking material from the substrate on which the hard film has been formed. <13> A method for manufacturing a printing stencil having a hard film on a surface facing a printed substrate, the method comprising: preparing a plate-shaped substrate; forming a hard film on the surface of the substrate facing the printed substrate by a dry process; removing a part or all of the hard film located in a printing pattern shape portion on the surface of the substrate facing the printed substrate; and forming a through hole in the printing pattern shape portion of the substrate, the opening area of ​​which is smaller than the area of ​​the printing pattern shape portion. <14> forming a plurality of the through holes in the print pattern shape portion; <12> or <13> A method for manufacturing printing stencils. <15> The method further includes forming fine irregularities on a surface of the substrate before forming a hard film on the substrate. <12> ~ <14> A method for manufacturing any one of the printing stencils. <16> The method further includes forming a corrosion-resistant layer on a surface of the substrate before forming the hard film on the substrate. <12> ~ <15> A method for manufacturing any one of the printing stencils. <17> The method further includes stretching the substrate on which the hard film is formed on a plate frame. <12> ~ <16> A method for manufacturing any one of the printing stencils. <18> The hard film is one or more films selected from an amorphous carbon film, a metal (including Si) oxide film, a metal (including Si) nitride film, a metal (including Si) carbide film, and a metal (including Si) oxynitride film. <12> ~ <17> A method for manufacturing any one of the printing stencils. <19> The amorphous carbon film contains one or more elements selected from N, O, Si, Ti, Al, Zr, B, and As. <18> A method for manufacturing printing stencils. <20> The hard film has a Vickers hardness (Hv) of 100 or more. <12> ~ <19> A method for manufacturing any one of the printing stencils. <21> The hard film has a Vickers hardness (Hv) of 450 or more. <12> ~ <20> A method for manufacturing any one of the printing stencils. <22> A water-repellent layer or a water- and oil-repellent layer is further formed on the print substrate side of the hard film. <12> ~ <21> A method for manufacturing any one of the printing stencils. <23> The water-repellent layer or the water- and oil-repellent layer mainly comprises a fluorine-containing coupling agent capable of forming a hydrogen bond and / or an -OM bond (wherein M is any element selected from the group consisting of Si, Ti, Al, and Zr) with the hard film by a condensation reaction. <12> ~ <22> A method for manufacturing any one of the printing stencils. Effect of the Invention

[0014] According to the present invention, it is possible to provide a printing stencil which has small variations in the printing film thickness and gives a thin printing layer. [Brief description of the drawings]

[0015] [Figure 1] 1A and 1B are schematic diagrams showing the structure of a printing stencil according to one embodiment of the present invention ((a): cross-sectional view, (b): view from the squeegee side). [Diagram 2] Schematic cross-sectional views showing the structure of a recess or hole in a hard film ((a): hole, (b): recess). [Diagram 3] FIG. 2 is a schematic cross-sectional view showing the structure of a printing stencil according to one embodiment of the present invention, on which a water-repellent layer or a water- and oil-repellent layer is formed. [Figure 4] 1A to 1C are schematic diagrams showing a method for manufacturing a printing stencil according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] Hereinafter, the configuration, operation and effect of the present invention will be described together with the technical concept with reference to the drawings.

[0017] [Printing stencil] As shown in Fig. 1, a printing stencil according to one embodiment of the present invention (hereinafter, referred to as "this embodiment") is basically composed of a two-layer (or multi-layer) structure of a plate-shaped substrate 1 having a surface 11 on the printed substrate side and a surface 12 on the squeegee side, and a hard film 3 formed on the surface 11 on the printed substrate side of the substrate 1. The hard film 3 has recesses or holes that define a printing pattern, which will be described later, in a printing pattern shape portion 2 of the substrate 1. The printing pattern shape portion 2 has through holes 13 formed therein for passing ink or paste, which penetrate from the recesses or holes to the surface 12 on the squeegee side of the substrate 1. Details of each part will be described below.

[0018] <Base material> The substrate 1 in the printing stencil according to this embodiment is not particularly limited, and may be any of various metal elements such as Fe, Cu, Ni, Al, and W, various alloys such as stainless steel, chromium-molybdenum steel, Ni-Co, Ni-W, Ni-Cr, aluminum alloys, copper alloys, and iron alloys, various inorganic materials such as amorphous metals, carbon, carbon cloth, glass, glass cloth, and ceramics, and inorganic and organic composite materials such as FRP, CFRP, and various engineering plastics. Also, composite materials in which resins such as PET, PEN, PMMA, OPP, polyimide, polyimide amide, vinyl chloride, and polycarbonate, rubber, and cellulose (wood, paper, etc.) are provided on the substrate surface may be used.

[0019] Since the variation in thickness of the substrate 1 directly leads to the variation in the shape and thickness of the printed pattern, it is preferable to suppress the variation in thickness and surface roughness to a low level. The surface roughness required for the substrate 1 cannot be generalized because it varies depending on the printing object, but as an example, the arithmetic mean surface roughness (Ra) of the portion requiring print transfer thickness accuracy is 0.2 μm or less, preferably 0.1 μm or less. Furthermore, in the case of a stencil for printing on a capacitor, Ra is preferably 0.05 μm or less, more preferably 0.03 μm or less. On the other hand, if the surface roughness of the substrate 1 is too low (if the surface is too smooth), there is a risk that the surface of the printing stencil on the substrate side of the printing stencil is difficult to introduce air into the contact surface when the stencil is released from the surface contact state with the substrate to be printed during printing, which may result in poor stencil release properties. In this case, there is also a risk that the ink or paste moving on the plate surface by the squeegee slips, making it difficult to fill the ink or paste, or that it is difficult to obtain thixotropy due to the rotation of the ink or paste. For this reason, the surface roughness of the entire substrate 1 or a necessary part may be made rough, or slits or uneven structures having a depth exceeding the surface roughness of the substrate may be intentionally formed in any part of the substrate 1. In this specification, the unevenness formed in this way is collectively referred to as "fine unevenness". The preferred height (depth) of the fine irregularities cannot be generalized as it differs depending on the required printing precision and the properties of the ink or paste used, but an example is an arithmetic mean surface roughness (Ra) of about 0.01 μm to 0.1 μm. As a specific position and shape of the fine irregularities, for example, in a printing stencil surface having a rectangular printing substrate surface of 300 mm, a cross-shaped portion of width 50 mm is set in the center where no printing pattern (group) is formed, and only the surface roughness of the portion is roughened, a slit is provided in the portion, or an irregularity is provided in the portion. Other examples include making the surface roughness of only a frame-shaped portion within a distance of 100 mm from each side of the 300 mm rectangular printing substrate surface, or a specific portion where the stencil sheet first begins to separate, or providing a slit or irregularity only in each of the portions.

[0020] The thinner the thickness of the substrate 1, the thinner the printed pattern can be formed by suppressing the amount of ink or paste supplied during printing, but the strength is lower, so durability and handling tend to decrease. Conversely, the thicker the substrate 1, the better the durability and handling, but the amount of ink or paste supplied increases, which may make it difficult to form a thin printed pattern. For this reason, the thickness of the substrate 1 is determined in consideration of the area and thickness of the printed pattern to be formed, and the durability required for the printing stencil. An example of the thickness of the substrate 1 is 10 μm to 100 μm, but is not limited to this thickness. The thickness of the substrate 1 can be changed within one stencil. For example, the thickness of the printing film can be reduced while maintaining the rigidity of the printing stencil by making the portion where the printing pattern is present thinner and the peripheral portion where the printing pattern is not present thicker.

[0021] A corrosion-resistant layer that prevents corrosion of the substrate 1 may be formed on the surface of the substrate 1. The corrosion-resistant layer is not particularly limited as long as it can prevent corrosion of the substrate 1, and examples thereof include plating.

[0022] <Through holes in the substrate> The substrate 1 of the printing stencil according to this embodiment has through holes 13 for supplying ink or paste to the printing pattern shape portion 2. The through holes 13 partially replace the functions of conventional stencil components, but their structure is significantly different. Conventional printing stencils have a "printing pattern through hole portion" that is approximately the same shape as the actual printing pattern to define the printing pattern, but the through holes 13 in this embodiment have an opening area smaller than the actual printing pattern, and their shape does not need to be similar to the actual printing transfer pattern. In this embodiment, the shape, size, number and position of the through holes 13 are not particularly limited as long as a printing pattern corresponding to the printing pattern shape portion 2 can be formed on the printed substrate (sheet). For example, the cross section or opening shape of the through holes 13 can be set to a circle, ellipse, polygon, star, slit, or indefinite shape. If the cross section or opening shape of the through holes 13 has corners, stress may be concentrated at the corners when tension is applied to the substrate, and the substrate 1 may be damaged from the corners. Therefore, in the case of a shape having corners, it is preferable that the corners have a curved line (R).

[0023] <Hard membrane> In this embodiment, the hard film 3 is a film having a Vickers hardness Hv larger than that of the substrate 1. The hard film 3 is formed on the surface 11 of the substrate 1 facing the substrate to be printed, and has a function of defining a print pattern in the print pattern shape portion 2. Specifically, the hard film 3 is provided with a concave portion or hole portion 31 corresponding to the print pattern shape portion 2, and is configured so that the ink or paste filled in the concave portion or hole portion 31 is transferred to the substrate to be printed. Here, the concave portion or hole portion 31 means a portion (corresponding to a hole portion) where the hard film 3 is not formed on the substrate 1 as shown in FIG. 2(a), or a portion (corresponding to a concave portion) where the hard film 3 is formed thinner than other portions as shown in FIG. 2(b). The thickness of the hard film 3 is 1 nm to 5 μm. If the hard film 3 is too thick, there is a risk that the hard film 3 may peel off due to deformation of the substrate during printing or handling. Furthermore, the variation in thickness is within 10%. By reducing the variation in the thickness of the hard film 3, the variation in the thickness of the obtained print pattern can be reduced. In this embodiment, the hard film 3 only needs to be formed on one side of the substrate 1 (side 11 facing the printed substrate). However, in cases where a thin substrate 1 is used, for example, forming the hard film 3 only on side 11 of the substrate 1 facing the printed substrate would cause the substrate 1 to warp due to residual stress in the hard film 3. In such cases, the hard film 3 can be formed also on the opposite side of the substrate 1 (side 12 facing the squeegee) to eliminate or mitigate the warping.

[0024] As the hard film 3, an amorphous carbon film, a metal (including Si) oxide film, a metal (including Si) nitride film, a metal (including Si) carbide film, and a metal (including Si) oxynitride film can be suitably used. More preferably, the amorphous carbon film contains one or more elements selected from N, O, Si, Ti, Al, Zr, B, and As. Specific examples of suitable hard films include diamond-like carbon (DLC), TiAlN, TiCrN, TiC, TiN, CrC, SiC, SiO X ,ZrO x , c-BN, and the like.

[0025] The amorphous carbon film contains nitrogen (N), oxygen (O) and metal elements such as silicon (Si), titanium (Ti), aluminum (Al) and zirconium (Zr), which allows polar functional groups such as hydroxyl groups to adhere or bond to the surface layer of the film. Therefore, when a water-repellent layer or a water-repellent / oil-repellent layer is formed on a hard film as described below, the film forms chemical bonds such as dehydration condensation reactions or hydrogen bonds with polar functional groups contained in a fluorine-containing silane coupling agent, which is a component of the hard film, to enhance adhesion to the water-repellent layer or the water-repellent / oil-repellent layer. Examples of such DLC films include a film containing titanium (Ti) in addition to carbon (C) and hydrogen (H) (aC:H:Ti film), and a film containing silicon (Si) in addition to carbon (C) and hydrogen (H) (aC:H:Si film). When the DLC film contains Si, the content is, for example, 0.1 to 50 atomic %, preferably 10 to 40 atomic %.

[0026] Furthermore, when oxygen or nitrogen is contained in the amorphous carbon film, the wettability of the amorphous carbon film to water (for example, wettability to water-based ink) can be improved. Therefore, as described above, when a hard film is also formed on the squeegee side surface of the substrate for the purpose of preventing warping of the substrate due to residual stress, by making the hard film an amorphous carbon film containing oxygen or nitrogen, it is possible to promote the wetting and spreading of the ink or paste during squeegeeing, and to suppress the occurrence of voids (air bubbles) in the printed matter due to insufficient wettability, and the occurrence of smearing or pinfall in the printed matter due to the inclusion of voids.

[0027] Furthermore, when the amorphous carbon film contains either Si, Si and oxygen, or Si and nitrogen, it has a high affinity with an adhesive made of a resin material, so that when the substrate 12 is made into a printing stencil, it can be reliably fixed to a frame using an adhesive.

[0028] The hard film 3 as described above is formed by various methods such as a CVD (chemical vapor deposition) method such as a plasma CVD method, a physical vapor deposition (PVD) method such as a plasma sputtering method, ECR plasma, etc. The plasma CVD methods used in this embodiment include a high-voltage DC micro-pulse plasma CVD method, a high-voltage pulse plasma CVD method, a high-frequency plasma CVD method using high-frequency discharge, a direct-current plasma CVD method using direct-current discharge, and a microwave plasma CVD method using microwave discharge. The hard film 3 can also be formed by a wet plating method. Any wet plating method can be selected as appropriate as long as it can form a hard film on the base material with sufficient bonding strength.

[0029] The Vickers hardness Hv of the hard film 3 is preferably 100 or more, and more preferably 450 or more. By providing a hard film 3 with a high Hv, it is possible to form a print pattern opening that is resistant to wear or abrasion. By making the Vickers hardness Hv 100 or more, the film has a hardness that exceeds that of stainless steel (Hv=100-200), which is a general-purpose base material. In addition, the ceramic coatings such as the above-mentioned DLC, TiAlN, TiCrN, and TiN can achieve an Hv of 450 or more, and those with high hardness can achieve an Hv of nearly 4000.

[0030] In the printing stencil according to this embodiment, the opening area of ​​the through hole 13 for supplying the ink or paste is configured to be smaller than the area of ​​the print pattern shape portion 2, so that the amount of ink or paste supplied to the recessed portion or hole portion 31 defining the print pattern formed in the print pattern shape portion 2 can be reduced. The recessed portion or hole portion 31 defining the print pattern is formed of a hard film having a very thin and uniform thickness, so that the small amount of ink or paste supplied from the through hole 13 can be formed into a print pattern having a very thin and uniform thickness. When a plurality of through holes are opened in one recessed portion or hole portion, the ink or paste supplied to each through hole merges in the recessed portion or hole portion to form one print pattern. In addition, in the printing stencil according to this embodiment, the through holes 13 and the base material 1 in which they are formed do not come into direct contact with the substrate to be printed during printing. Therefore, unlike a conventional screen stencil with a mesh, mesh marks are not formed in the printing pattern due to the intersections of the mesh, and the printing pattern is not divided by the walls of the openings, as in a stencil stencil in which the openings through which the ink or paste passes are processed and formed as discrete holes.

[0031] The printing stencil according to this embodiment may be accompanied by a support frame (stencil frame) made of cast iron, aluminum alloy, wood, or any other material. The stencil frame is not limited to a frame-shaped one, and may be, for example, a cylindrical one such as a rotary printing plate. Furthermore, it may be a flat plate without a frame, and may be chucked to a printing machine or stencil frame during printing.

[0032] <Water-repellent layer / Water- and oil-repellent layer> The printing stencil according to this embodiment may have a water-repellent layer or a water-repellent / oil-repellent layer 4 formed on the substrate 1 or the hard film 3. FIG. 3 shows a schematic cross-sectional view of a printing stencil having a water-repellent layer or a water-repellent / oil-repellent layer 4 formed on the hard film 3. The formation of the water-repellent layer or the water-repellent / oil-repellent layer 4 provides the following: UV scattering prevention effect of the hard film 3; gas barrier effect for preventing contact of the hard film 3 with atmospheric gas; anticorrosion effect of the hard film 3; improvement of the abrasion resistance and sliding properties of the hard film 3; prevention of adhesion of soft metal, which is a component of the ink or paste used during printing, to the hard film; and prevention of bleeding of the ink or paste and its wraparound around the substrate 1 during printing.

[0033] The water-repellent layer or the water- and oil-repellent layer 4 is preferably a thin film made of a fluorine-containing coupling agent, although the composition is not particularly limited. Furthermore, if the fluorine-containing coupling agent is any one of a silane coupling agent, a titanate coupling agent, a zirconate coupling agent, and an aluminate coupling agent, it is more preferable because it is possible to impart a stable water- and oil-repellent surface to the openings of the printing stencil. The fluorine-containing coupling agent can be formed into a thin film of about 10 to 20 nm, and is also preferable in that deterioration of the shape precision of the opening pattern of the stencil can be suppressed.

[0034] The water-repellent layer or the water- and oil-repellent layer 4 can be appropriately formed on the required parts according to the printing application, such as the surface of the printing stencil facing the substrate to be printed, the wall surface of the printing pattern shape portion 2, the surface facing the squeegee, etc. The printing stencil according to this embodiment is often used in such a way that it is placed in contact with the substrate to be printed without offset (without leaving a gap), and then the ink or paste supplied to the surface on the squeegee side is slid by the squeegee to pass through the through holes 13. In this printing method, the ink or paste tends to spread more easily than in normal screen printing, and the releasability (release of the stencil) from the printing substrate tends to be poor. In addition, some inks used in thin-film printing have low viscosity and high fluidity like water, and it may be difficult to print according to the printing pattern shape of the stencil. For this reason, in the printing stencil according to this embodiment, it may be extremely effective to perform water-repellent treatment or water-repellent and oil-repellent treatment on the necessary parts where the ink is likely to spread, and conversely, not to perform it on the unnecessary parts that will hinder the filling of the ink. Specifically, when the printing stencil according to this embodiment is used for thin-film printing, it is preferable to form the water-repellent layer or water- and oil-repellent layer 4 only on the "surface facing (contacting) the substrate to be printed" of the hard film 3 having the "surface facing (contacting) the substrate to be printed" and the "inner wall of the recessed portion or hole that defines the printing pattern". Since the viscosity of the ink or paste used in thin-film printing is low, if the water-repellent treatment or water- and oil-repellent treatment is performed on the "inner wall of the recessed portion or hole that defines the printing pattern", there is a risk that the filling of the ink or paste into the recessed portion or hole 31 that defines the printing pattern may be hindered. In addition, when the water-repellent layer or water- and oil-repellent layer 4 is formed on the surface on the squeegee side, the wetting spread and the uniformity of the thickness may be hindered when the ink or paste is precoated on the surface on the squeegee side with a scraper or the like. On the other hand, applying a water-repellent or water- and oil-repellent treatment to the "surface facing (contacting) the printed substrate" is extremely effective in preventing the highly fluid, low-viscosity ink or paste from seeping out of the printing pattern openings or from wrapping around the screen to the printed substrate side.In addition, when the viscosity of the ink or paste is relatively high, it is possible to perform a water-repellent treatment or a water- and oil-repellent treatment on both the "surface facing (in contact with) the printed substrate" and the "inner walls of the recesses or holes defining the printing pattern". In addition, it is also possible to perform a water-repellent treatment or a water- and oil-repellent treatment on the bottom surfaces of the recesses or holes defining the printing pattern (which may also be the surface of the stencil substrate), and it is also possible to perform a water-repellent treatment or a water- and oil-repellent treatment on the inner walls of the through holes 13 opened in the substrate 1.

[0035] [Manufacturing method for printing stencils] The printing stencil according to this embodiment is preferably manufactured by a method including the steps of preparing a plate-shaped substrate 1, forming through holes 13 having an opening area smaller than the area of ​​the printing pattern in a printing pattern shape portion 2 of the substrate 1, covering the printing pattern shape portion 2 on a surface 11 of the substrate 1 facing a substrate to be printed with a masking material 5, forming a hard film 3 by a dry process on the surface 11 of the substrate 1 facing a substrate to be printed that is covered with the masking material 5, and removing the masking material 5 from the substrate 1 on which the hard film 3 has been formed. Details of each operation are described below.

[0036] <Preparation of the substrate> The substrate 1 used may be a commonly available plate material as it is, or may be formed by electroforming. When forming the substrate by electroforming, the substrate may be a flat plate without through holes, or a flat plate with through holes formed in advance.

[0037] In order to adjust the surface condition of the substrate 1, when forming the substrate by electroforming, the type and amount of additives such as a leveling agent in the electroforming bath may be adjusted to give a mirror finish or a matte finish, or after forming the substrate, a mirror finish may be performed by electrolytic polishing or the like, or various processes such as blasting, honing, matte finish, hairline processing, laser processing, scribing, drilling, pressing, and etching may be performed, or a corrosion-resistant layer may be formed by a wet or dry plating film. When the above-mentioned "fine irregularities" are formed on the squeegee-side surface of the substrate, these surface condition adjustment methods can form one or more grooves, openings, other irregularities, and wavy structures in any part in an arrangement perpendicular to or obliquely intersecting the moving direction of the squeegee during printing.

[0038] When forming a portion of the substrate 1 that is thinner than other portions, the relevant portion is partially etched (half-etched), or a protrusion called a COB mask is formed by welding or the like in other portions to increase the thickness.

[0039] <Forming through holes in substrate> The through holes 13 can be formed in the substrate 1 by various methods, including, but not limited to, mechanical processing such as drilling, punching, pressing, etc., irradiation with high-energy ions or electron beams such as laser light or focused ion beams, irradiation with high-pressure liquid (water), etching, or a combination of the above methods.

[0040] In the embodiment of the present invention, when through holes 13 are formed in a substrate 1 that is an aggregate of fine fibers such as carbon fiber cloth or glass cloth, there is a risk that the fibers may escape from the vicinity of the opening or the inner wall of the through holes 13. In order to prevent this, it may be effective to perform a surface treatment on the surface layer of the cloth by a known wet plating method or formation of a dry thin film to fix the fibers before performing the hole drilling process, or to drill holes in the cloth and then perform a surface treatment by a known wet plating method or formation of a dry thin film to fix the fibers. Among fiber aggregates, carbon fiber cloth is suitable for use as the substrate 1 because it is robust, highly corrosion-resistant, and conductive, making it easy to perform wet plating, and also easy to drill holes in by laser processing.

[0041] The through holes 13 may be formed at any appropriate time during the process of producing a stencil. For example, the through holes 13 may be formed in advance in the print pattern shape portion 2 of the substrate 1, the through holes 13 may be formed after the hard film 3 is formed on the surface layer of the substrate 1, or the through holes 13 may be formed after the water-repellent layer or the water-repellent / oil-repellent layer 4 is further formed on the surface layer of the hard film 3. When the through holes 13 are formed by laser light after the water-repellent layer or the water-repellent / oil-repellent layer 4 is formed, it is also possible to destroy the hard film 3 and the water-repellent layer or the water-repellent / oil-repellent layer 4 formed in advance in the laser irradiated portion.

[0042] <Masking> Masking of the substrate 1 is performed by disposing a masking material 5 on the substrate 1 in the shape of the print pattern shape portion 2 prior to the formation of the hard film 3. The type of masking material 5 is not particularly limited, and may be an ink, a film, or a three-dimensional object as long as it can prevent the hard film 3 from being formed at the location where the masking material is disposed when the hard film 3 is formed. When forming a fine masking portion on the substrate 1 with good positional accuracy, a resist liquid or resist film used in known photolithography is suitable. When masking the substrate 1 with a resist liquid or resist film, the resist liquid or resist film is applied or disposed on the entire surface of the substrate 1 to be the surface 11 on the printed substrate side, and then the resist liquid or resist film is irradiated (scanned) with a light beam capable of altering the resist, such as a laser beam, in accordance with the position and shape of the print pattern shape portion 2, and exposed by a "direct imaging method" (direct imaging method) in which only the resist located in the print pattern shape portion 2 is exposed to light, and then development is performed. Of course, it is also possible to arrange another patterned exposure mask on the resist formed on the base material 1 and modify the necessary portions (exposed portions) of the resist, and the method is not particularly limited.

[0043] <Formation of hard film> The method for forming the hard film 3 on the surface of the substrate 1 is not limited as long as it can provide a hard film having a desired thickness and surface roughness, but a dry process is preferable, and a vacuum plasma process is more preferable, in that it can form a thin film with a small variation in thickness. A specific method will be described below using an example in which an amorphous carbon film is formed as the hard film 3.

[0044] When forming an amorphous carbon film by plasma CVD, a hydrocarbon gas such as methane, acetylene, benzene, etc. is used as a reactant gas as a raw material. The conditions during film formation, such as the substrate temperature, gas concentration, pressure, and time, are appropriately set by a known method according to the composition and film thickness of the amorphous carbon film (aC:H film) to be formed.

[0045] In this case, when forming an amorphous carbon film (aC:H:Si film) containing silicon (Si) in addition to carbon (C) and hydrogen (H), for example, tetramethylsilane, methylsilane, dimethylsilane, trimethylsilane, dimethoxydimethylsilane, tetramethylcyclotetrasiloxane, or the like is used as a raw material reactive gas.

[0046] In this case, when forming an amorphous carbon film (aC:H:Ti film) containing titanium (Ti) in addition to carbon (C) and hydrogen (H), the aforementioned plasma CVD method uses, as a raw reactive gas, a mixture of a gas containing Ti, such as titanium chloride (TiCl4), titanium iodide (TiI4), titanium isopropoxide (Ti(OC3H7)4), etc., and a hydrocarbon gas, such as acetylene, ethylene, or methane.

[0047] When forming an amorphous carbon film by plasma CVD, in order to include oxygen (O) in the film, a method of introducing oxygen together with the main raw material gas during film formation can be adopted. The oxygen content in the obtained hard film is determined by adjusting the flow rate ratio of oxygen to the total flow rate of the main raw material gas and oxygen. The flow rate ratio is, for example, 0.01 to 12%, preferably 0.5 to 10%. As another means for including oxygen (O) in the amorphous carbon film, a method of irradiating a previously formed film with oxygen plasma may be adopted.

[0048] The amorphous carbon film can also contain nitrogen (N). In this case, a method of irradiating the formed amorphous carbon film with nitrogen plasma can be used.

[0049] When oxygen (O) or nitrogen (N) is introduced into an amorphous carbon film by plasma irradiation, after an amorphous carbon film is formed in an amorphous carbon film forming apparatus, plasma irradiation can be performed in the same apparatus without breaking the vacuum, and the formation of the amorphous carbon film and the introduction of oxygen (O) or nitrogen (N) into the film can be performed continuously.

[0050] The amorphous carbon film can also be formed by a physical vapor deposition method (PVD method). In this case, the substrate 1 is placed in a film forming apparatus, the inside of the apparatus is made into a vacuum atmosphere, and then a sputtering gas (e.g., an inert gas such as argon gas) is introduced at a predetermined pressure and flow rate to sputter a carbon target, thereby forming an amorphous carbon film on the substrate 1. In this case, an Si target or a Ti target is sputtered simultaneously with the carbon target, thereby forming an amorphous carbon film containing Si and / or Ti. In addition, by mixing a hydrocarbon gas such as acetylene, oxygen (O), nitrogen (N) or a mixture of these gases with the gas used to sputter a Si target or Ti target, an amorphous carbon film containing silicon, titanium, carbon and hydrogen, oxygen or nitrogen can be formed by a reactive sputtering method.

[0051] After forming a hard film 3 on the surface of the substrate 1 as described above, the masking material 5 is removed to obtain a printing stencil according to this embodiment, in which a hard film 3 having recesses or holes 31 defining the printing pattern is formed in the printing pattern forming portion 2 of the surface 11 of the substrate 1 facing the printed substrate.

[0052] When manufacturing the printing stencil according to this embodiment, the entire surface of the substrate 1 is covered with a hard film 3, and then part or all of the hard film 3 is removed by irradiation with laser light or an ion beam, etc., to form recesses or holes 31 that define the printing pattern. In particular, according to the method of forming the recesses 31 that define the printing pattern by removing only a portion of the hard film 3, the substrate 1 is covered with the hard film except for the through holes 13, so that a material with low chemical durability such as corrosion resistance can be used for the substrate. Therefore, it is possible to use, as the substrate 1, a material that has good mechanical properties such as strength but is poor in chemical durability and therefore could not be used for a printing stencil. For example, medium carbon steel for mechanical structures (S45C) (Young's modulus 205GPa, shear modulus 82GPa, yield strength 727MPa, tensile strength 828MPa, elongation 22%), high tensile steel (HT80) (Young's modulus 203GPa, shear modulus 73GPa, yield strength 834MPa, tensile strength 865MPa, elongation 26%), chromium molybdenum steel (SCM440) (yield strength 833MPa, tensile strength 980MPa, elongation 12%), nickel chromium molybdenum steel (SNCM439) (yield strength 1471MPa, tensile strength 1765MPa, elongation 8%), precipitation hardening stainless steel (SUS631) (Young's modulus 204GPa, yield strength 1029MPa, tensile strength 1225MPa, elongation 4%), martensitic stainless steel (SUS410) (Young's modulus 200GPa, yield strength 345MPa, tensile strength 540MPa, elongation 25%) , Hastelloy (registered trademark) X (Young's modulus 197 GPa, shear modulus 75 GPa, yield strength 384 MPa, tensile strength 775 MPa, elongation 43%), hot die tool steel (SKD6), spring steel (SUP7), 9% Ni steel for low-temperature pressure vessels (SL9N590), maraging steel (350 grade), Monel metal, nichrome (GNC108), titanium 6Al-4V alloy (60 types), and titanium 5-2.5 alloy, etc., are highly likely to be usable as the substrate 1, in consideration of the mechanical properties of stainless steel (SUS304) (Young's modulus 197 GPa, shear modulus 74 GPa, yield strength 205 MPa, tensile strength 520 MPa, elongation 40%) and nickel (99.99Ni) (Young's modulus 204 GPa, shear modulus 81 GPa, yield strength 58 MPa, tensile strength 335 MPa, elongation 28%), which are widely used as substrates for printing stencils.

[0053] <Formation of water-repellent layer / water- and oil-repellent layer> When the above-mentioned water-repellent layer or water- and oil-repellent layer 4 is formed on the substrate 1 or hard film 3, the method of formation is not particularly limited and can be appropriately selected. For example, a liquid starting material (coupling agent liquid) may be applied to the portion where the water-repellent layer or water- and oil-repellent layer 4 is to be formed by penetrating a nonwoven fabric or the like, by hand coating, brush coating, squeegee coating, roller coating, or the like, or by spraying with a spray or the like. Also, a screen may be dipped in the coupling agent liquid, or it may be coated with a bar coater or spin coater, or it may be applied by screen printing. Furthermore, it may be formed by a resistance heating method or other known vacuum process. Examples of the vacuum process include plasmatizing a raw material gas containing at least fluorine, such as CF4 or C6F6, in a vacuum or at atmospheric pressure (atmospheric pressure plasma) to give fluorine to the substrate 1 or hard film 3, or forming a layer containing fluorine on the substrate 1 or hard film 3. EXAMPLES

[0054] A SUS304 stainless steel plate with a rectangular shape of 400 mm on each side and a thickness of 30 μm was prepared, and in the central area of ​​50 mm×50 mm of the SUS plate, rectangles with a width of 150 μm and a length of 400 μm, which correspond to the printing pattern of the internal electrode of one capacitor, were virtually arranged at intervals of 100 μm. Next, holes of φ20 μm were formed at equal intervals of 30 μm inside the virtually arranged rectangles by a known YAG laser beam to form a mesh shape. After that, the SUS plate was immersed in an etching solution mainly composed of hydrofluoric acid to remove dross, and then a known electrolytic polishing method was used to remove smut, and a plate with a surface smoothed to about Ra0.03 μm was prepared. Next, a known photoresist film (Hitachi Chemical RY series RY3325, thickness 25 μm) with a thickness of 25 μm was applied to the entire 50 mm square printing pattern area in the central part of one side of the SUS plate (the side that faces the printed substrate in the printing stencil), and a pattern was directly drawn using a UV laser light direct imaging device (Dainippon Screen LI9500 (Mercurex)) so that the photoresist film remained in the virtually positioned rectangular area. Next, the SUS plate masked with a photoresist film was placed in a vacuum chamber of a high-voltage DC micro-pulse plasma CVD apparatus, and the vacuum chamber was heated to 1×10 -3 The vacuum chamber was evacuated to 1 Pa. Then, argon gas at a pressure of 1 Pa was introduced into the vacuum chamber at a flow rate of 30 SCCM, and the substrate surface was plasma cleaned for 10 minutes by applying a voltage of -3 kVp. After argon gas was exhausted from the vacuum chamber, trimethylsilane gas at a pressure of 1 Pa was introduced into the vacuum chamber at a flow rate of 30 SCCM, and a voltage of -5 kVp was applied to form a 300 nm thick Si-containing amorphous carbon film (hard film) on the surface of the SUS plate masked with the photoresist film (the surface that becomes the surface of the printing stencil on the substrate side), and then the vacuum was broken to remove the SUS substrate, and the photoresist film (pattern portion) was developed and removed by a known method. The obtained SUS plate was stretched in a casting frame measuring 650 mm in length and 550 mm in width by a known method and made into a printing stencil.

[0055] The obtained printing stencil had a rectangular printing pattern area of ​​150 μm wide and 400 μm long, in which holes of φ20 μm were formed in a mesh pattern on the surface of the printed substrate side of a rectangular SUS plate of 400 mm × 400 mm, surrounded by a 300 nm thick Si-containing amorphous carbon film. The rectangular printing pattern area was recessed by 300 nm (corresponding to the film thickness of the Si-containing amorphous carbon film) from the surface on which the Si-containing amorphous carbon film was formed, as viewed from the printed substrate side. In other words, the SUS plate located at the printing pattern area has a space of 300 nm between the printed substrate and the Si-containing amorphous carbon film when the Si-containing amorphous carbon film is brought into contact with the printed substrate.

[0056] Next, the thickness and the variation of the Si-containing amorphous carbon film (hard film) formed on the substrate were confirmed. The printing stencil was disassembled, and test pieces measuring approximately 5 mm x 5 mm were cut out from a total of five locations, including the four corners and the center of the printing pattern area. The cross sections were observed under an electron microscope to measure and compare the film thickness of the Si-containing amorphous carbon film in each test piece. As a result, it was confirmed that the difference in film thickness between the thickest and thinnest of the five test pieces was within 10% (within a range of 30 nm). It is difficult to achieve such a narrow film thickness variation industrially with good reproducibility by manually applying the emulsion resin liquid while contacting a bucket on a screen mesh, and the effectiveness of the present invention was confirmed. [Industrial Applicability]

[0057] According to the printing stencil of the present invention, a thin film printing pattern can be formed with high accuracy, and therefore the printing stencil of the present invention can be suitably used for stencils, offset printing plates, and the like. [Explanation of symbols]

[0058] 1 Base material 11 Printed substrate side 12 Squeegee side surface 13 Through hole 2 Printing pattern shape part 3 Hard membrane 31 Concave or hole 4. Water-repellent layer or water- and oil-repellent layer 5 Masking material

Claims

1. a plate-shaped substrate having a single layer and a surface facing a substrate to be printed and a surface facing a squeegee; a hard film formed on the surface of the base material facing the printed substrate and having a concave portion or a hole portion that defines the printing pattern in the printing pattern shape portion; a plurality of through holes penetrating the printing pattern shape portion from within the recessed portion or hole portion to the squeegee side surface of the base material, the opening area of ​​which is smaller than the area of ​​the printing pattern defined by the recessed portion or hole portion of the printing pattern shape portion; Equipped with The hard film has a thickness of 300 nm to 5 μm, and the thickness variation is within 10%.

2. 2. The printing stencil according to claim 1, wherein the substrate has a surface having minute projections and recesses.

3. 3. The printing stencil according to claim 1, wherein the substrate has a surface provided with a corrosion-resistant layer.

4. 4. The printing stencil according to claim 1, wherein the substrate is stretched over a frame.

5. The printing stencil according to any one of claims 1 to 4, wherein the hard film is one or more films selected from an amorphous carbon film, a metal (including Si) oxide film, a metal (including Si) nitride film, a metal (including Si) carbide film, and a metal (including Si) oxynitride film.

6. 6. The printing stencil according to claim 5, wherein said amorphous carbon film contains one or more elements selected from the group consisting of N, O, Si, Ti, Al, Zr, B and As.

7. 7. The printing stencil according to claim 1, wherein the hard film has a Vickers hardness (Hv) of 100 or more.

8. 8. The printing stencil according to claim 1, wherein the hard film has a Vickers hardness (Hv) of 450 or more.

9. 9. The printing stencil according to claim 1, further comprising a water-repellent layer and / or a water- and oil-repellent layer formed on the printing substrate side of said hard film.

10. 10. The printing stencil according to claim 9, wherein the water-repellent layer or the water- and oil-repellent layer is mainly composed of a fluorine-containing coupling agent capable of forming a hydrogen bond and / or an -O-M bond (wherein M is any element selected from the group consisting of Si, Ti, Al, and Zr) with the hard film by a condensation reaction.

Citation Information

Patent Citations

  • Metal mask for printing

    JP2002192850A

  • Perforated printing mask

    JP2005144973A

  • Multilayer structure metal mask, and method for manufacturing the same

    JP2015030162A

  • Screen printing plate

    JP2015229287A

  • Stencil for printing provided with organic polymer layer and method for producing the same

    JP2017039320A