Nonwoven fabric manufacturing method and nonwoven fabric manufacturing device
The use of a flexible support and engaging pushing member with a heat-fusible web and heated fluid in nonwoven fabric manufacturing addresses limitations in pattern flexibility and damage susceptibility, achieving a thick, permeable fabric with varied patterns.
Patent Information
- Application Number
- JP2020187347
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-11-10
- Publication Date
- 2024-09-26
- Estimated Expiration
- 2040-11-10
AI Technical Summary
Existing nonwoven fabric manufacturing methods face limitations in shaping flexibility, pattern changeability, and susceptibility to damage due to collisions between rigid supports and pushing members, restricting the range of thickness and unevenness that can be achieved.
A method involving a flexible support with an uneven shape and a pushing member that engages with the flexible support, using a heat-fusible web fused with a heated fluid, allowing for high flexibility in pattern changes and reducing damage risks.
The method enables a high degree of freedom in changing uneven patterns while minimizing damage to the support and pushing member, resulting in a nonwoven fabric with increased thickness and improved fluid permeability.
Smart Images

Figure 0007556752000004 
Figure 0007556752000002 
Figure 0007556752000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method and an apparatus for producing a nonwoven fabric. [Background technology]
[0002] Regarding the manufacturing method of nonwoven fabrics for use in absorbent articles, many techniques have been proposed for manufacturing nonwoven fabrics having excellent feel. For example, Patent Document 1 describes a method for producing a nonwoven fabric, in which a fiber web is fixed onto a breathable base having numerous protrusions, and then hot air is blown onto the fiber web on the base to shape the fiber web along the protrusions and fuse the fibers. Patent Document 2 describes a method for producing a nonwoven fabric, which includes a pressing step in which a fiber web is placed on a support having predetermined protrusions, recesses, and apertures, and the fiber web is pressed along the recesses with a pressing member, and then a heat fusion step in which hot air is blown to fuse the fibers in the fiber web to each other. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2012-136791 A [Patent Document 2] JP 2019-112747 A Summary of the Invention [Problem to be solved by the invention]
[0004] The method for producing a nonwoven fabric described in Patent Document 1 does not shape a fiber web by engaging a base with another member, but by pressing the fiber web with hot air pressure. In this shaping process, it is necessary to blow hot air at a high speed. That is, there is a certain restriction on the range of the hot air speed, and there is a limit to the thickness of the unevenness that can be formed. In addition, the nonwoven fabric manufacturing method described in Patent Document 2 specifically uses a drum-shaped support, and the engagement of the drum-shaped support and a pressing member allows the formation of a fibrous web with a convexo-concave shape with greater height differences. On the other hand, the convexo-concave shape is often formed as part of the drum. Therefore, changing the convexo-concave pattern often requires replacing the drum, making it difficult to freely change the pattern. Furthermore, the base and support are hard materials, and thermal expansion or the like can cause the support and the push-in member to misalign and collide with each other, resulting in damage.
[0005] In view of the above, the present invention relates to a method for producing a nonwoven fabric that has a high degree of freedom in changing the pattern of uneven shaping and is less likely to be damaged when a support body and a pushing member collide with each other. The present invention also relates to an apparatus for producing a nonwoven fabric, which can suitably carry out the method for producing a nonwoven fabric. [Means for solving the problem]
[0006] The present invention provides a method for producing a nonwoven fabric, comprising the steps of: clamping and shaping a heat-fusible web between a flexible support having an uneven shape and a pushing member that can engage with the flexible support; and fusing the heat-fusible web on the flexible support with a heated fluid.
[0007] The present invention also provides a nonwoven fabric manufacturing apparatus having a flexible support having an uneven shape, a pushing member that can engage with the flexible support, and a heated fluid spraying mechanism that can perform a fusion process on a heat-sealable web on the flexible support. Effect of the Invention
[0008] According to the method for producing a nonwoven fabric of the present invention, there is a high degree of freedom in changing the pattern of the uneven shaping, and the fabric is less likely to be damaged when the support and the pushing member collide with each other. The nonwoven fabric manufacturing apparatus of the present invention can suitably carry out the nonwoven fabric manufacturing method of the present invention. [Brief description of the drawings]
[0009] [Figure 1] FIG. 1 is a schematic front view showing a preferred embodiment of an apparatus used in a method for producing a nonwoven fabric of the present invention. [Diagram 2] FIG. 2 is a schematic front view showing another preferred embodiment of an apparatus used in the method for producing a nonwoven fabric of the present invention. [Diagram 3] 11 is a partial cross-sectional view showing an example of the positional relationship between a protrusion of a flexible support and a convex portion of a push-in member. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0010] Hereinafter, the method and apparatus for producing a nonwoven fabric according to the present invention will be described with reference to the drawings. In this specification, the conveying direction during the manufacture of the nonwoven fabric is referred to as the MD direction (Machine Direction), the width direction perpendicular to the conveying direction is referred to as the CD direction (Cross Direction), the direction of the surface including the MD direction and the CD direction is referred to as the planar direction, and the normal direction of the tangent to the planar direction is referred to as the thickness direction.
[0011] (Formation process) The method for producing a nonwoven fabric of the present invention includes a step of clamping and shaping a heat-fusible web between a flexible support having an uneven surface and a pressing member that can mesh with the flexible support (hereinafter referred to as the "shaping step"). For example, as shown in FIG. 1, the heat-sealable web 11 can be processed by bending the flexible support 21 into a belt conveyor shape. The flexible support 21 has a plurality of protrusions 24 at a predetermined interval and has an uneven surface. The flexible support 21 and a pushing member 31 arranged to face the flexible support 21 are rotated at the same speed, and the heat-sealable web 11 conveyed from the upstream side is sandwiched between the flexible support 21 and the pushing member 31. In this belt conveyor method, the ring-shaped flexible support 21 is hooked on rolls 22, 22 at both ends, and the flexible support 21 is rotated. The pushing member 31 engages with the uneven shape of the flexible support 21 and sandwiches the heat-sealable web 11 (pushes the heat-sealable web 11 between the protrusions 24, 24 of the flexible support 21). The intermeshing gives the heat-sealable web 11 an uneven shape, while the constituent fibers of the heat-sealable web 11 are oriented in the thickness direction, making it possible to produce a nonwoven fabric 10 with a large thickness.
[0012] (flexible support) "Flexibility" in the case of a flexible support refers to the property of not breaking or cracking even when a linear or planar object is bent 180° with a curvature radius of 100 mm and then stretched back into a linear or planar shape 100 times. By repeating this bending and stretching operation 100 times, it is possible to determine whether or not the object has flexibility. In this specification, the property of breaking or cracking is referred to as "inflexibility." In the case of a flexible support, the base material portion between the protrusions has flexibility. In such a flexible support, the protrusions firmly hold the heat-sealable web, while the base material of the flexible support flexibly receives the pressing of the heat-sealable web by the pressing member, so that it is possible to form a shape with a larger three-dimensional thickness and a deeper bottom.
[0013] Since the flexible support 21 has flexibility, it can be made to conform to various shapes, such as flat surfaces and curved surfaces. That is, various types of processing lines can be constructed to accommodate the production of nonwoven fabrics with various patterns. For example, it may be a belt conveyor type as shown in FIG. 1, or may be fixed to the peripheral surface of a drum 23 as shown in FIG. 2. In the case of the drum type shown in FIG. 2, even if the drum 23 does not have flexibility, the flexible support 21 has flexibility, so that the flexible support 21 can be replaced without replacing the drum 23. This makes it easy to change the shape and size of the protrusions 24 on the surface of the flexible support 21, making it easy to change the pattern of uneven shaping. However, from the viewpoint of preventing the heat-sealable web 11 from lifting off the flexible support 21 due to the centrifugal force caused by the rotation of the drum 23, and from the viewpoint of lengthening the section of the nonwoven fabric fusion processing step described below, the belt conveyor type (the configuration shown in FIG. 2) is preferable to the drum type (the configuration shown in FIG. 2). In addition, in terms of the point where the heat-fusible web 11 is sandwiched between the pushing member 31 and the flexible support 21, it is preferable to have a backup roll (not shown) such as a guide roll or a drum on the back side (opposite the surface that comes into contact with the heat-fusible web 11) of the flexible support 21. The presence of the backup roll makes it difficult for the flexible support 21 to be displaced in the thickness direction, and stabilizes the meshing amount D described below.
[0014] The flexibility of the flexible support 21 used in the present invention allows for greater freedom in changing or fine-tuning the pattern of the production line for the nonwoven fabric 10. For example, if the flexible support 21 is in the form of a belt conveyor as shown in FIG. 1, the section of the nonwoven fabric fusion treatment process described below can be lengthened, and the fusion treatment time can be extended to match the production line. In this way, the fusion treatment can be performed slowly over time at a low wind speed, and the thickness of the fiber layer of the nonwoven fabric 10 produced increases. That is, it becomes easier to produce the desired nonwoven fabric 10. In addition, the separation of fibers due to hot air is suppressed, and the inter-fiber distance of the obtained nonwoven fabric 10 is maintained high, resulting in a good texture and increased permeability to fluids such as liquids and air. In addition, even if the projections 24 are misaligned when the flexible support 21 and the pushing member 31 engage with each other, the flexible support 21 deforms, thereby reducing the force caused by the collision between the projections 24 and the pushing member 31. As a result, damage to the flexible support 21 and the pushing member 31 can be prevented. At the same time, the heat-sealable web 11 can be prevented from being cut at the collision portion. When the pushing member 31 engages with the flexible support 21, if the tip of the pushing member 31 comes into contact with the protrusion 24, a force is applied that causes the protrusion 24 to fall in a planar direction. If the protrusion is fixed to a non-flexible support as in the past, the protrusion may bend or break. Or the pushing member may bend or break. On the other hand, if the protrusion 24 is fixed to the flexible support 21 as in the present invention, the flexible support 21 deforms, thereby preventing the protrusion 24 from bending or breaking. When the flexible support 21 and the pushing member 31 are released from the engagement and the flexible support 21 is no longer in contact with the pushing member 31, no force is applied to the protrusion 24, and the position of the protrusion 24 returns to its original position due to the elastic force of the flexible support 21. In addition to the flexible support 21 being flexible, it is preferable that the protrusion 24 is also flexible, it is more preferable that the joint between the protrusion 24 and the flexible support 21 is also flexible, and it is even more preferable that the pushing member 31 is also flexible. From the viewpoint of preventing bending or breakage of the protrusions 24, the deformation amount of the protrusions 24 is preferably 0.8 mm or more, and more preferably 1 mm or more. Moreover, from the viewpoint of having appropriate rigidity for deforming the heat-fusible web 11, the deformation amount of the protrusions 24 is preferably 10 mm or less, and more preferably 8 mm or less. Furthermore, when the deformation amount of the protrusions 24 is within the above range, when the manufactured nonwoven fabric 10 is peeled off from the flexible support 21, the protrusions 24 on the surface of the flexible support 21 are tilted, for example, so that the flexible support 21 deforms in the direction in which the nonwoven fabric 10 is peeled off, making it easier to peel off the nonwoven fabric 10.
[0015] (Method of measuring deformation of protrusion) The deformation amount of the protrusion 24 can be measured as follows. A metal block with a tip angle of 90 degrees is fixed to the load cell of a tensile tester (product name: Autograph AG-1kNIS, manufactured by Shimadzu Corporation) so that the inclined surface of the tip is at an angle of 45 degrees with respect to the thickness direction. At this time, the metal block is fixed to the load cell so that the tip of the metal block is positioned on the central axis of the load cell. The load cell is fixed to the movable frame of the tensile tester. The inclined surface of the metal block is made smooth. A flexible support 21 is set under the tensile tester, and the flexible support 21 is placed over it so that the protrusion 24, which is intended for a 150 mm square flat plate (thickness: 10 mm) with a 50 mm square window frame, is at the center of the window frame, and weights are placed around the window frame so that the flexible support 21 does not float. The load from the weight is about 0.05 kg / cm 2 At this time, the flexible support 21 is set so that the thickness direction of the flexible support 21 coincides with the compression direction of the load cell. The flexible support 21 is set so that the protrusion 24 is located at a position shifted about 1 mm from the central axis of the load cell, and a metal block having an inclination angle of 45 degrees is displaced in the compression direction at a speed of 10 mm / min, and the tip of the metal block is brought into contact with the protrusion 24. The displacement point where the load is 0.1 N is set as the zero point, and the displacement amount (mm) in the compression direction when the compression load becomes 1 N is measured. The flexible support 21 is reset so that the planar direction of the flexible support 21 is random with respect to the direction in which the protrusions 24 fall, and measurements are similarly taken for different protrusions 24. The average of the five displacement measurement results is taken as the deformation amount of the protrusions 24. For reference, a load cell with a rated capacity of approximately 100 N is used.
[0016] (Heat-sealable web) The heat-fusible web 11 to be processed is an aggregate of heat-fusible fibers before the fibers are bonded to each other. In other words, it is a material before being made into a nonwoven fabric. By using such a web, the fibers can be easily moved during the manufacturing process of the nonwoven fabric 10, and it is easy to manufacture a nonwoven fabric 10 with a deep three-dimensional pattern and a large thickness. In a heat-sealable web, there is no heat fusion or entanglement between the fibers to maintain the integrity of the nonwoven fabric as a sheet, and the freedom of fiber movement is ensured. This is a so-called unfused state. As long as the integrity of the heat-sealable web as a sheet is not maintained and the freedom of fiber movement is high, there may be pressure bonding or slight fusion between the fibers. Note that those that have been mechanically entangled or hydroentangled are not included in the heat-sealable web.
[0017] The heat-sealable web 11 in the present invention may be a single-layer web consisting of only one layer, or may be a laminated web in which two or more layers are laminated in the thickness direction. In the shaping step, it is preferable to open holes in the heat-fusible web 11. By opening holes before nonwoven fabric formation and accumulating the separated fibers around the holes, the thickness of the nonwoven fabric 10 around the holes can be increased, resulting in a nonwoven fabric 10 that is less likely to allow excreted liquid to return even if it is crushed. From the viewpoint of increasing the permeability of excretory liquid, the holes opened in the heat-sealable web 11 are preferably circular with a diameter of 0.5 mm or more, more preferably circular with a diameter of 1.0 mm or more, and even more preferably circular with a diameter of 2.0 mm or more. Furthermore, from the viewpoint of preventing contact between the skin and a sheet (such as a sublayer or absorbent core wrap) on the non-skin side of the nonwoven fabric 10 when the nonwoven fabric 10 is incorporated and used as a top sheet in an absorbent article, the holes opened in the heat-sealable web 11 are preferably circular with a diameter of 10 mm or less, and more preferably circular with a diameter of 8 mm or less. When the shape of the holes is not circular, it is preferable that the holes are within the range of the upper and lower limits of the area of the circles. The holes to be made in the heat-sealable web 11 may or may not penetrate the web in the thickness direction. That is, one surface of the heat-sealable web 11 may be recessed in the thickness direction, and the other surface may be sealed. The method of making holes in the heat-sealable web 11 will be described later.
[0018] (Nonwoven fabric fusion processing process) The method for producing a nonwoven fabric of the present invention includes a step of subjecting a heat-fusible web to a fusion treatment on a flexible support with a heated fluid (hereinafter referred to as a "nonwoven fabric fusion treatment step"). Heat fusion means that the heat-fusible web 11 melts, and the constituent fibers of the heat-fusible web 11 no longer have the fiber form before the fusion treatment. For example, at least a part of the outer peripheral surface of the constituent fibers of the heat-fusible web 11 melts, and the boundary with the outer peripheral surface of the other fibers becomes indistinguishable, and the fiber form before the fusion treatment is no longer retained. When the constituent fibers of the heat-fusible web 11, such as composite fibers, are made of two or more resins, even if a specific resin does not melt and maintains its fiber form, the other resins melt, and the boundary between the outer peripheral surfaces of the constituent fibers of the heat-fusible web 11 becomes indistinguishable, and the fiber form before the fusion treatment is no longer retained. These can be observed by observing the cross section of the fused fiber part with a scanning electron microscope (SEM, product name: JCM-600, manufactured by JEOL Ltd.). In the nonwoven fabric fusion treatment step, a heated fluid 41 is sprayed onto the heat-fusible web 11 on the flexible support 21, and heat treatment is performed. Specifically, as shown in Figures 1 and 2, while the heat-fusible web 11 is transported on the flexible support 21, the heated fluid 41 heated to a predetermined temperature is sprayed onto the heat-fusible web 11 in the thickness direction by an air-through method. In this manner, the intersections between the constituent fibers of the heat-fusible web 11 are bonded by heat fusion to form a nonwoven fabric, and the nonwoven fabric 10 can be manufactured.
[0019] (heated fluid) The heated fluid 41 is not particularly limited as long as it can convert the heat-fusible web 11 into a nonwoven fabric. For example, hot air and steam can be used. However, hot air is preferred from the viewpoint of making the fiber oil on the surface of the heat-fusible web 11 less likely to flow. As described in Patent Document 1, it has been common in the past to set the hot air speed to 20 m / sec or more and 100 m / sec or less. On the other hand, in the present invention, by using the flexible support 21, it is possible to extend the fusion treatment time (lengthen the heat treatment section) as described above. Therefore, after the heat-fusible web 11 is pressed in the thickness direction in the shaping step, it is also possible to perform heat fusion between the fibers directly on the flexible support 21 in the nonwoven fabric fusion treatment step at a wind speed slower than in the past. In addition, a bulky nonwoven fabric 10 can be obtained without the heat-fusible web 11 being compacted by the heating fluid 41. From the viewpoint of increasing the thickness of the produced nonwoven fabric 10, the wind speed of the heated fluid 41 is preferably 10 m / sec or less, more preferably 5 m / sec or less, and even more preferably 2 m / sec or less. Moreover, from the viewpoint of sufficiently forming the heat-fusible web 11 into a nonwoven fabric, the wind speed of the heated fluid 41 is preferably 0.1 m / sec or more, more preferably 0.2 m / sec or more, and even more preferably 0.3 m / sec or more.
[0020] The temperature of the heating fluid 41 is preferably equal to or higher than the lowest melting point of the resin of the constituent fibers of the heat-fusible web 11, and the temperature difference from the melting point is preferably 60° C. or less. This makes it possible to stabilize the shaped shape formed by the formation of the fused fiber parts, and also allows the web to be easily peeled off from the flexible support 21. From the viewpoint of forming a good fiber fusion portion, the length of the heat treatment section is preferably 1 m or more, and more preferably 3 m or more. Also, from the viewpoint of reducing the weight of the flexible support 21, the length of the heat treatment section is preferably 30 m or less, and more preferably 20 m or less. From the viewpoint of forming a good fiber fusion portion, the spraying time of the heated fluid 41 is preferably 0.2 seconds or more, and more preferably 0.5 seconds or more. From the viewpoint of reducing the weight of the flexible support 21, the spraying time of the heated fluid 41 is preferably 20 seconds or less, and more preferably 12 seconds or less.
[0021] The method for producing the nonwoven fabric of the present invention may include other steps in addition to the shaping step and the fusion treatment step to form a nonwoven fabric.
[0022] (Web release process) The method for producing a nonwoven fabric of the present invention preferably includes a step of spraying a fluid 42 from the pushing member 31 side toward the heat-fusible web 11 to release the heat-fusible web 11 after the shaping step and before the nonwoven fabric fusion treatment step (hereinafter referred to as a "web releasing step"). More specifically, at the exit of the meshing between the flexible support 21 and the pushing member 31, the fluid 42 is sprayed to release the heat-fusible web 11 from the pushing member 31. The inclusion of the web releasing step allows for a smooth transition from the shaping step to the nonwoven fabric fusion treatment step. In particular, it is preferable that the heat-fusible web 11 released from the pushing member 31 is held by the flexible support 21. The fibers of the heat-fusible web 11 are fused together in the nonwoven fabric fusion process, but the fibers of the heat-fusible web 11 may be pre-fused together in the web release process. If the pre-fusion is performed by blowing the fluid 42 from the pushing member 31 side so as to pass between the convex parts 32 of the pushing member 31, the fusion process and the peeling process can be performed more satisfactorily without destroying the shape of the shaped heat-fusible web 11. The temperature of the fluid 42 during the pre-fusion is preferably equal to or higher than the lowest melting point of the resin of the constituent fibers of the heat-fusible web 11, and the temperature difference from the melting point is preferably 30° C. or less. In addition, the wind speed of the fluid 42 is preferably 0.5 m / s or more and 3 m / s or less, and the treatment time with the fluid 42 is preferably 0.01 seconds or more and 0.1 seconds or less. By satisfying these numerical ranges, the constituent fibers of the heat-fusible web 11 are less likely to stick to the pushing member 31, and the uneven shape in the meshed state can be maintained.
[0023] (Lamination process) The method for producing the nonwoven fabric of the present invention may include a step of laminating another heat-fusible web or nonwoven fabric on the nonwoven fabric 10 after the fusion treatment step to form a nonwoven fabric. For example, the fusion-treated nonwoven fabric 10 may be laminated in the thickness direction as a raw material nonwoven fabric with another nonwoven fabric to produce a laminated nonwoven fabric consisting of two or more layers.
[0024] (Embossing and fusing process) The method for producing a nonwoven fabric of the present invention may include a step of carrying out a fusion treatment by embossing after the heat-fusible web 11 is released from the pressing member 31 (hereinafter referred to as an "embossing and bonding step"). The embossing and bonding step may be carried out before or after the nonwoven fabric-forming fusion treatment step described above, or may be carried out both before and after. In the embossing and bonding step, the fibers are fused together by heating and clamping. In the nonwoven fabric fusion process, the fibers are heat-fused at their intersections, so two fibers are often heat-fused per fiber fusion section, whereas in the embossing process, several to several tens of fibers are heat-fused per fiber fusion section. The heating method in the embossing and fusion treatment step can be a method using a heating element or a heating medium, or a method using an ultrasonic method. From the viewpoint of suppressing fuzz and improving the liquid absorption performance, the method for producing the nonwoven fabric of the present invention preferably includes an embossing and fusion treatment step after the nonwoven fabric-forming and fusion treatment step.
[0025] (Additional fusion process) In addition to the nonwoven fabric-forming fusion treatment step carried out on the flexible support 21, the nonwoven fabric manufacturing method of the present invention preferably includes a step of performing an additional fusion treatment after peeling the heat-fusible web 11 from the flexible support 21 (hereinafter referred to as the "additional fusion treatment step"). The additional fusion treatment in the additional fusion treatment step can use a heating fluid (not shown) similar to the heating fluid 41 in the nonwoven fabric-forming fusion treatment step. A flat net (conveyor) or the like can be used as the support. This makes it possible to more suitably manufacture a nonwoven fabric 10 that is prevented from fuzzing, has improved strength, and has an appropriate compression hardness. The temperature of the heated fluid in the additional fusion treatment step is preferably equal to or higher than the lowest melting point of the resin of the constituent fibers of the heat-fusible web 11, and the temperature difference from the melting point is preferably 50° C. or less. The wind speed of the heated fluid in the additional fusion treatment step is preferably 5 m / sec or less, more preferably 3 m / sec or less, and even more preferably 1 m / sec or less. From the viewpoint of sufficiently forming the heat-fusible web 11 into a nonwoven fabric, the wind speed of the heated fluid in the additional fusion treatment step is preferably 0.1 m / sec or more, more preferably 0.2 m / sec or more, and even more preferably 0.3 m / sec or more.
[0026] Next, the materials and devices used in the method for producing the nonwoven fabric of the present invention will be described in detail.
[0027] (Material of flexible support) From the viewpoint of imparting flexibility to the flexible support 21, the flexible support 21 is preferably made of a resin or a metal, or both. Furthermore, by using these materials, the flexible support 21 can be prevented from being deformed by heat even when the heated fluid 41 is sprayed on it in the nonwoven fabric fusion processing step. The resin constituting the flexible support 21 is preferably a resin having a melting point higher than the temperature of the heating fluid 41 or a cross-linked curable resin. Specifically, examples of thermoplastic resins include polyamide, polyester (polyethylene terephthalate (PET), etc.), polyethylene (PE), polyphenylene sulfide, and polypropylene, while examples of curable resins include vinyl chloride, silicone resin, fluorine-based resin, and synthetic rubber. Other examples include carbon materials. By using a resin as the material for the flexible support 21, the flexible support 21 can be made lighter. Furthermore, even if a resin with lower durability than metal is used, the present invention allows the flexible support 21 to be easily replaced with a new one. Various known metals can be used as the metal constituting the flexible support 21. By using a metal as the material for the flexible support 21, the flexible support 21 becomes highly durable.
[0028] (Opening of flexible support) The flexible support 21 may or may not have openings. When the flexible support 21 does not have openings, it is preferable to perform the fusion treatment by spraying a heated fluid 41 onto the heat-fusible web 11 sandwiched between the flexible support 21 and a net or the like (not shown) arranged opposite the flexible support 21 in the nonwoven fabric fusion treatment step. In this way, the fusion treatment can be performed without destroying the shape of the shaped heat-fusible web 11. However, from the viewpoint of passing the heated fluid 41 through in the nonwoven fabric fusion treatment step, it is preferable that the flexible support 21 has openings. The degree of openings in the flexible support 21 can be determined by the ratio of the area of the openings to the surface of the flexible support 21 (hereinafter referred to as the "opening ratio"). From the viewpoint of increasing the permeability of the heated fluid 41, the opening ratio of the flexible support 21 is preferably 30% or more, more preferably 40% or more, and even more preferably 50% or more. Furthermore, from the viewpoint of maintaining the strength of the flexible support 21, the opening ratio of the flexible support 21 is preferably 90% or less, more preferably 80% or less, and even more preferably 70% or less.
[0029] (Form of flexible support) Examples of the form of the flexible support 21 having such an opening ratio include a net, a chain, and an opening punching. By adopting any of these forms, it is possible to easily fix the shape of the heat-fusible web 11 on the flexible support 21 and at the same time to easily allow the heating fluid 41 to penetrate. From the viewpoint of increasing the opening ratio, the form of the flexible support 21 is preferably a net. From the viewpoint of increasing the strength of the flexible support 21, the form of the flexible support 21 is preferably an opening punching.
[0030] (Uneven shape of the flexible support surface) By providing the protrusions 24 intermittently on the surface of the flexible support 21, an uneven shape can be formed. Various methods can be used to form the protrusions 24. For example, the protrusions 24 can be formed on the surface of the flexible support 21 by integral resin molding, casting, grinding, etc. In the case of these methods, the protrusions 24 become integrated with the flexible support 21. Furthermore, the protrusions 24 may be attached to the flat surface of the flexible support 21 by means of screws, nuts, rivets, spot welding, adhesives, glue guns, etc. Specific examples of the protrusions 24 to be attached include metal pointed bolts, resin pointed bolts, metal rivets, resin rivets, etc. Alternatively, the protrusions 24 may be formed on the surface of the flexible support 21 using a 3D printer or the like.
[0031] (Push-in member) The pushing member 31 can mesh with the flexible support 21. That is, when the pushing member 31 is disposed so as to face the flexible support 21, the projections 24 can enter the recesses and holes present on the surface of the pushing member 31. Since the pushing member 31 can mesh with the flexible support 21, the heat-fusible web 11 can be sufficiently pushed in the thickness direction in the shaping step, and excessive pushing by the heated fluid 41 can be prevented in the nonwoven fabric fusion processing step. It is preferable that the pushing member 31 pushes in the thickness direction up to the position of the base material of the flexible support 21. In this way, the side of the heat-fusible web 11 that contacts the flexible support 21 becomes dense, and fuzzing on the surface of the manufactured nonwoven fabric 10 can be suppressed. Furthermore, in the nonwoven fabric fusion treatment step, the heat-fusible web 11 is also pushed toward the flexible support 21, further suppressing fuzzing.
[0032] (Shape of the push-in member) Examples of the form of the pushing member 31 that can mesh with the flexible support 21 include a ring roll, a concave-convex roll, a net, a belt, a chain, a leaf spring (elastic plate-like body), and a movable load plate. In Figs. 1 and 2, the pushing member 31 is in the form of a ring roll. Among them, a concave-convex roll is preferred from the viewpoints of making it possible to form the heat-fusible web 11 into a discontinuous concave-convex shape in the MD direction and facilitating adjustment of the degree of meshing with the flexible support 21. Examples of a method for forming a concave-convex shape on the surface of the concave-convex roll include a method of intermittently providing convex portions 32, similar to a method of intermittently providing protrusions 24 on the flexible support 21.
[0033] (Material of the pushing member) The pushing member 31 is preferably made of resin or metal, or both. Specific examples of the resin and metal constituting the pushing member 31 are the same as those given for the flexible support 21.
[0034] (Continuous and intermittent contact) The heat-sealable web 11 may be in continuous or intermittent contact with the flexible support 21 and the pushing member 31. Whether the type of contact corresponds to continuous or intermittent contact can be determined as follows using the distance in the thickness direction from the top of the protrusion 24 of the flexible support 21 to the top of the convex portion 32 of the pushing member 31 when they are engaged (meshing amount D) even when the heat-sealable web 11 is not sandwiched between the flexible support 21 and the pushing member 31 (see FIG. 3).
[0035] The "continuous contact" on the pushing member 31 side means a state in which the tops of the convex portions 32 of the pushing member 31 are continuously engaged in one direction from the tops of the projections 24 toward the flexible support 21 by more than half of the meshing amount D in the thickness direction, and can be determined by whether or not this state is present. When the flexible support 21 and the pushing member 31 clamp the heat-sealable web 11 in this state, the heat-sealable web 11 and the pushing member 31 are in continuous contact with each other. For example, when a ring roll is used as the pushing member 31, the heat-sealable web 11 is in continuous contact with the pushing member 31 in the MD direction. As for the portions other than the convex portions 32 of the pushing member 31, there is a space between the convex portions 32, 32 of the pushing member 31, so that the heat-sealable web 11 may or may not be in contact with the pushing member 31. The "intermittent contact" on the pushing member 31 side means a state in which the protrusions 32 of the pushing member 31 bite into the thickness direction by more than half the meshing amount D, but are interrupted in one direction (a state in which there is a portion where the degree of the pushing member 31 bites into is less than half the meshing amount D), and it can be determined whether or not this state exists. When the flexible support 21 and the pushing member 31 clamp the heat-sealable web 11 in such a state, the heat-sealable web 11 and the pushing member 31 come into intermittent contact. For example, when a gear roll having convex portions continuous in the CD direction is used as the pushing member 31, the tops of the convex portions 32 of the pushing member 31 are interrupted in the MD direction, and the degree of bite into the space between the convex portions 32, 32 is less than half the meshing amount D, so that the heat-sealable web 11 comes into intermittent contact with the pushing member 31 in the MD direction. In addition, when a ring roll is used as the pushing member 31, the heat-sealable web 11 comes into continuous contact with the pushing member 31 in the MD direction and intermittently in the CD direction (see FIG. 3). This is preferable in that damage is reduced when the pushing member 31 shifts from the set position in the CD direction and comes into contact with the protrusions 24 of the flexible support 21. In addition, when a ring roll with a gear-shaped tip is used as the pushing member 31, the heat-sealable web 11 comes into intermittent contact with the pushing member 31 in both the MD direction and the CD direction. This is preferable in that the heat-sealable web 11 is easily held on the flexible support 21 side when the heat-sealable web 11 is released from the pushing member 31 after shaping, and the shaped state is maintained. The portions of the pushing member 31 other than the protrusions 32 are the same as in the case of continuous contact. In the present invention, it is preferable that the heat-fusible web 11 be in continuous contact with the pushing member 31 in either the MD or CD direction, and be in intermittent contact with the other direction.
[0036] The "continuous contact" on the flexible support 21 side means a state in which the tops of the projections 24 of the flexible support 21 are continuously engaged in one direction from the tops of the convex parts 32 toward the pushing member 31 by more than half of the meshing amount D in the thickness direction, and can be determined by whether or not this state is present. When the flexible support 21 and the pushing member 31 clamp the heat-sealable web 11 in this state, the heat-sealable web 11 and the flexible support 21 are in continuous contact with each other. For example, when a flexible support 21 having projections 24 arranged in the MD direction is used, the heat-sealable web 11 is in continuous contact with the flexible support 21 in the MD direction. As for the parts of the flexible support 21 other than the projections 24, there are cases in which the heat-sealable web 11 does not contact the flexible support 21 and cases in which the heat-sealable web 11 contacts the flexible support 21 due to the presence of spaces between the projections 24, 24 of the flexible support 21. The "intermittent contact" on the flexible support 21 side means a state in which the portion where the protrusions 24 of the flexible support 21 bite into the thickness direction by more than half the meshing amount D is interrupted in one direction (a state in which the degree to which the pushing member 31 bites into the flexible support 21 is less than half the meshing amount D), and it can be determined whether or not this state exists. When the flexible support 21 and the pushing member 31 clamp the heat-sealable web 11 in this state, the heat-sealable web 11 and the flexible support 21 come into intermittent contact. For example, when a flexible support 21 having protrusions 24 arranged in a lattice pattern is used, the heat-sealable web 11 comes into intermittent contact with the flexible support 21 in both the MD and CD directions (see FIG. 3). The portions other than the tops of the protrusions 24 of the flexible support 21 are in the same state as in the case of continuous contact. In the present invention, it is preferable that the heat-sealable web 11 be in intermittent contact with the flexible support 21 in both the MD and CD directions.
[0037] By appropriately setting the amount of meshing D according to the shape and size of the protrusions 24, holes can be opened in the heat-sealable web 11 in the shaping step. For example, in the case where the protrusions 24 are conical as shown in Figures 1 and 2, if the diameter of the bottom surface of the protrusions 24 is 2 mm, holes can be opened in the heat-sealable web 11 by setting the amount of meshing D to 2 mm or more. In the case where the protrusions 24 are cylindrical as shown in Figure 3, if the diameter of the top of the protrusions 24 is 1.6 mm, holes can be opened in the heat-sealable web 11 by setting the amount of meshing D to 3 mm or more, and if the diameter of the top of the protrusions 24 is 2 mm, the amount of meshing D to 5 mm or more.
[0038] (Alignment) Since the flexible support 21 has flexibility, it may expand in the MD direction or shrink in the CD direction due to long-term use in the production of the nonwoven fabric 10. As a result, the planar position of the convex portion 32 of the pushing member 31 may no longer be optimal for meshing with the protrusion 24. From the viewpoint of controlling such misalignment and maintaining appropriate meshing, it is preferable to align the flexible support 21 with the pushing member 31 in the planar direction in the shaping step. The alignment may be performed by aligning the flexible support 21 in the planar direction, by aligning the push-in member 31 in the planar direction, or by combining these methods. The alignment in the planar direction may be performed by using an adjustment mechanism in the MD direction for the flexible support 21 and the push-in member 31, or by using an adjustment mechanism in the CD direction for both of them, or by performing both of them. Since the flexible support 21 is flexible and tends to expand in the MD direction and contract in the CD direction, misalignment is likely to occur at the meshing points. Therefore, it is preferable to align the flexible support 21 and the push-in member 31 in the planar direction by providing an adjustment mechanism at least for the flexible support 21.
[0039] As an example of the planar positioning of the flexible support 21, the flexible support 21 is fixed to a drum, a chain, a timing belt, or the like, and the position of the protrusion 24 is detected using an image, a laser, or the like, and then the position of the pushing member 31 is adjusted in the planar direction so that the protrusion 24 meshes with the convex portion 32. The fixing positions of the flexible support 21 and the drum, the chain, the timing belt, or the like may be on both sides of the flexible support 21 (both ends in the CD direction of the flexible support 21) or in multiple rows in the MD direction. The planar positioning of the flexible support 21 may be performed manually or by using an adjustment mechanism. Examples of the adjustment mechanism in the MD direction include a gear meshing drive and a mechanism for adjusting the tension in the MD direction. Examples of the adjustment mechanism in the CD direction include a mechanism for adjusting the CD position of the side fixing portion of the flexible support 21 and a mechanism for adjusting thermal expansion due to axial heating of the flexible support 21. Furthermore, a method of providing a regulating guide groove (or rail) in a CD direction meandering correction device or a guide roll may also be used. The positioning of the push-in member 31 in the planar direction may be performed manually or by using an adjustment mechanism. An example of an adjustment mechanism in the MD direction is a gear meshing drive. An example of an adjustment mechanism in the CD direction is an adjustment mechanism for thermal expansion of the push-in member 31 due to axial heating, or a spline that moves in the CD direction. Among them, from the viewpoint of reducing the force caused by the collision between the protrusion 24 and the push-in member 31 and preventing damage to the flexible support 21 and the push-in member 31, it is preferable to use a spline that moves in the CD direction as the adjustment mechanism for the push-in member 31. It is also preferable to provide an adjustment mechanism in both the flexible support 21 and the push-in member 31, and in that case, it is more preferable to provide an adjustment mechanism in the CD direction in both. However, from the viewpoint of automating the alignment, it is preferable to perform the alignment by feeding back the detection result of the position of the protrusion 24 to the adjustment mechanism.
[0040] (Nonwoven fabric manufacturing equipment) The method for producing a nonwoven fabric of the present invention can be realized, for example, by a nonwoven fabric production apparatus as shown in Figures 1 and 2. Specifically, the method can be realized by a nonwoven fabric production apparatus having a flexible support 21 having an uneven shape, a pushing member 31 capable of engaging with the flexible support 21, and a heated fluid spraying mechanism capable of performing a fusion process of a heat-fusible web 11 on the flexible support 21. As the heated fluid spraying mechanism, a commonly used mechanism such as an air-through machine can be used.
[0041] (Applications of nonwoven fabric) As described above, the method for producing a nonwoven fabric of the present invention can produce a thick nonwoven fabric. By increasing the thickness of the nonwoven fabric, the distance between fibers increases, making it difficult for excreted liquid to remain on the surface of the nonwoven fabric. Furthermore, by producing a nonwoven fabric with holes, excreted liquid is less likely to return even if the nonwoven fabric is crushed. Therefore, the nonwoven fabric produced by the present invention is preferably used in absorbent articles, such as diapers for adults and children, sanitary napkins, incontinence pads, panty liners, absorbent pads, and the like. EXAMPLES
[0042] The present invention will be described in more detail below with reference to examples, but the present invention is not limited to these examples.
[0043] Example 1 The upper layer (weight 15g / m 2 ) and the lower layer (weight 15g / m 2 The upper layer was made of thermoplastic composite short fibers with a core-sheath (polyethylene terephthalate (PET) (core): polyethylene (PE) (sheath) = 5:5 (mass ratio)) concentric type with a fineness of 1.1 dtex, fiber length of 44 mm, and coated with a hydrophilic oil agent. The lower layer was made of thermoplastic composite short fibers similar to the constituent fibers of the upper layer, except that the fineness was 3.3 dtex. The above heat-sealable web was shaped by meshing with a flexible support having a polyester plain weave mesh with a line pitch of 1.7 mm and a line diameter of 0.5 mm, in which a plurality of M2 bolts with a height of 9 mm were fixed by nuts as protrusions, and a ring roll with a plurality of rings arranged in the CD direction as a pressing member. The M2 bolts on the flexible support were arranged in a plurality of positions with a lattice interval of 5.1 mm in the MD and CD directions. When meshing and shaping, the upper web was brought into contact with the flexible support and the lower web was brought into contact with the ring roll, respectively, and the meshing amount (pressing depth) was set to 6 mm, and the ring roll was pressed with the M2 bolts to penetrate the heat-sealable web, forming an uneven shape on the heat-sealable web. After the above-mentioned shaping process, as a nonwoven fabric fusion processing process, hot air at a temperature of 136°C was blown onto the lower web side of the flexible support 21 at a wind speed of 1.5 m / sec for a blowing time of 1 second to fuse the intersections between the constituent fibers of the heat-sealable web. After the heat-sealable web was peeled off from the flexible support, as an additional fusion treatment step to prevent fuzzing, hot air at a temperature of 136°C was blown onto the lower web side of the heat-sealable web on a flat conveyor net at a wind speed of 0.5 m / sec for a blowing time of 6 seconds to produce the nonwoven fabric of Example 1. In the nonwoven fabric of Example 1, holes penetrating in the thickness direction were formed. During the shaping process, the thermal expansion of the flexible support by the hot air caused a misalignment between the support and the ring roll in the CD direction, but no damage to the M2 bolts or cuts in the heat-sealable web due to friction between the flexible support and the ring roll were observed.
[0044] Example 2 The nonwoven fabric of Example 2 was produced in the same manner as in Example 1, except that the height of the M2 bolt was set to 6 mm, and only the upper layer was subjected to the shaping process, and then the lower layer was laminated and subjected to the nonwoven fabric fusion treatment process. In the nonwoven fabric of Example 2, holes were formed in the upper layer that were recessed in the thickness direction and blocked by the lower layer. During the shaping process, no damage to the M2 bolts or breakage of the heat-sealable web due to friction between the flexible support and the ring roll was observed.
[0045] Example 3 The nonwoven fabric of Example 3 was produced in the same manner as in Example 1, except that the M2 bolts were clamped between the gaps in the polyester plain weave mesh instead of being fastened with nuts. In the nonwoven fabric of Example 3, holes were formed penetrating through the thickness direction. During the shaping process, no damage to the M2 bolts or breakage of the heat-sealable web due to friction between the flexible support and the ring roll was observed.
[0046] Example 4 Except for using M1.6 bolts with a height of 15 mm instead of the M2 bolts, the nonwoven fabric of Example 4 was produced in the same manner as in Example 3. In the nonwoven fabric of Example 4, holes were formed penetrating through in the thickness direction. During the shaping process, no damage to the M1.6 bolts or breakage of the heat-sealable web due to friction between the flexible support and the ring roll was observed.
[0047] Example 5 Except for using a stainless steel plain weave mesh instead of the polyester plain weave mesh, the nonwoven fabric of Example 5 was produced in the same manner as in Example 4. In the nonwoven fabric of Example 5, holes were formed penetrating through the thickness direction. During the shaping process, no damage to the M1.6 bolts or breakage of the heat-sealable web due to friction between the flexible support and the ring roll was observed.
[0048] Comparative Example 1 A nonwoven fabric of Comparative Example 1 was produced in the same manner as in Example 1, except that an aluminum alloy with 2 mm square columns with a height of 8 mm integrally molded as protrusions was used as a non-flexible support instead of a flexible support. In the nonwoven fabric of Comparative Example 1, both the upper and lower layers had depressions in the thickness direction, resulting in a nonwoven fabric with recesses formed therein. During the shaping process, the thermal expansion of the non-flexible support by the hot air caused a misalignment between the support and the ring roll in the CD direction, and damage to the 2 mm square pillars and breakage of the heat-sealable web were observed due to friction between the non-flexible support and the ring roll.
[0049] (Measurement of deformation of protrusion) For the supports used in Examples 1 to 5 and Comparative Example 1, the deformation amounts of the protrusions were measured according to the method described above. The results are shown in Table 1.
[0050] [Table 1]
[0051] As shown in Table 1, in Examples 1 to 5 in which a flexible support was used, the amount of deformation of the protrusions was large and the protrusions were less likely to be damaged, compared to Comparative Example 1 in which a non-flexible support was used. Furthermore, among Examples 1 to 5, there was a tendency that the greater the height of the projection, the greater the amount of deformation of the projection, and the more unlikely the projection was to be damaged. Furthermore, in Examples 3 to 5, in which the protrusions were clamped between the gaps in the mesh, the protrusions had a higher degree of freedom of movement, so the protrusions were more likely to deform and were less likely to break than in Examples 1 and 2, in which the protrusions were fixed with nuts. In addition, in Examples 4 and 5, the deformation of the protrusions was greater in Example 4, which used a polyester mesh, than in Example 5, which used a metal mesh, and the use of a material with low rigidity for the flexible support tended to make the protrusions even less susceptible to damage.
[0052] 10. Nonwoven Fabrics 11 Heat-sealable web 21 Flexible support 22 rolls 23 Drums 24 protrusions 31 Push-in member 32 Convex 41 Heating fluid 42 Fluid D Engagement amount
Claims
1. A step of sandwiching and shaping a heat-fusible web between a flexible support having an uneven shape and a pushing member capable of engaging with the flexible support; and fusing the heat-sealable web on the flexible support with a heated fluid, A method for producing a nonwoven fabric, wherein the flexible support has protrusions intermittently formed on a surface thereof, and the pushing member has recesses or holes on its surface into which the protrusions can enter.
2. The method for producing a nonwoven fabric according to claim 1, wherein the flexible support is made of a resin or a metal, or both, and is a net or an apertured punched sheet.
3. The method for producing a nonwoven fabric according to claim 1 or 2, wherein the pushing member is made of resin or metal, or both, and is a concave-convex roll, a net, a belt, a leaf spring, or a plate.
4. The method for producing a nonwoven fabric according to any one of claims 1 to 3, further comprising the step of forming holes in the heat-sealable web.
5. The method for producing a nonwoven fabric according to any one of claims 1 to 4, wherein the heated fluid has a wind speed of 10 m / sec or less.
6. The method for producing a nonwoven fabric according to any one of claims 1 to 5, wherein the flexible support and the pushing member are aligned in a planar direction.
7. An apparatus for producing a nonwoven fabric, comprising: a flexible support having an uneven surface; a pushing member capable of engaging with said flexible support; and a heated fluid spraying mechanism capable of performing a fusion process on a heat-fusible web on said flexible support.
Citation Information
Patent Citations
Absorbent article
JP2009153556A
Nonwoven fabric and absorbent article including the same
JP2012136791A
Method of manufacturing nonwoven fabric
JP2019112747A
Absorbent article
JP2019208712A
Method and apparatus for incrementally stretching a web
WO2008112517A1