Lipid bilayer substrate and method for producing lipid bilayer substrate

The lipid bilayer membrane substrate with an ionic liquid seal addresses ion leakage issues, enabling accurate ion channel analysis by blocking inorganic ion movement and improving measurement precision.

JP7557157B2Active Publication Date: 2024-09-27NIPPON TELEGRAPH & TELEPHONE CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
JP2023501918
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-02-25
Publication Date
2024-09-27
Estimated Expiration
2041-02-25

AI Technical Summary

Technical Problem

Existing lipid bilayer membrane substrates experience ion leakage due to the movement of inorganic substances like metal and halogen ions, which can introduce noise and affect the accuracy of measurements in ion channel analysis.

Method used

A lipid bilayer membrane substrate is created with a microwell structure sealed by a sealing liquid containing an ionic liquid, which prevents ion leakage by blocking the passage of inorganic ions through the interfacial gap between the substrate and the lipid bilayer.

Benefits of technology

The use of an ionic liquid seal effectively suppresses ion leakage, enhancing the accuracy of ion channel measurements and allowing for precise functional analysis of membrane proteins.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007557157000013
    Figure 0007557157000013
  • Figure 0007557157000018
    Figure 0007557157000018
  • Figure 0007557157000021
    Figure 0007557157000021
Patent Text Reader

Abstract

Provided is a lipid bimolecular membrane substrate 1A having a substrate 12 in which formed are microwells 20 that are open at one surface; a lipid bimolecular membrane 30 disposed on the substrate 12, covering the openings of the microwells 20; and a sealing fluid 22 disposed between the substrate 12 and the lipid bimolecular membrane 30. The sealing fluid 22 contains an ionic liquid.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a lipid bilayer substrate and a method for producing a lipid bilayer substrate. [Background technology]

[0002] In basic molecular biological research, the Human Genome Project, which aimed to decipher the entire base sequence of human DNA, was announced as completed in 2003, and we are now entering the post-genome era in which we investigate the information encoded in the genome.

[0003] In the post-genomic era, the functions of proteins are being actively studied. Among proteins, membrane proteins are responsible for transporting substances necessary for life and transmitting signals, and are deeply involved in physiological functions such as various diseases, drug responses, and immune responses. Therefore, attempts are being made to control the structure of membrane proteins present in cell membranes and to utilize and elucidate their functions.

[0004] A representative method for arranging membrane proteins in vitro is to dissolve lipid molecules in an organic solvent such as n-decane, apply the lipid solution in an aqueous solution to small holes provided on a substrate to form a black film, and then fuse the membrane protein to the black film (see, for example, non-patent document 1).

[0005] In the method of fusing membrane proteins to black membranes, it has been pointed out that residual organic solvents and heterogeneity in the black membrane may affect the physiological activity of membrane proteins. In addition, the stability of the black membrane is low, and the lifespan of the black membrane is only a few hours at most.

[0006] In response to this, the inventors created a lipid bilayer substrate in which the openings of the microwells were covered with lipid membranes by forming microwells on a semiconductor substrate and spreading giant lipid membrane vesicles on an electrolyte solution dropped into the microwells. Furthermore, the inventors succeeded in reconstituting membrane proteins in the lipid bilayer membranes covering the microwells (Non-Patent Document 2).

[0007] The lipid bilayer substrate described above was made using giant lipid vesicles, so the lipid bilayer covering the microwells does not contain organic solvents. In addition, the lifespan of the lipid bilayer is about a few days, which is significantly longer than that of the black membrane described above. In addition, it was confirmed by optical techniques (fluorescence observation) that the membrane protein reconstituted in the lipid bilayer covering the microwells has activity.

[0008] As described above, a substrate on which a lipid bilayer containing a membrane protein is reconstituted is useful as a platform for measuring the function of the membrane protein. [Prior art documents] [Non-patent literature]

[0009] [Non-Patent Document 1] "New Patch Clamp Experimental Techniques" edited by Yasunobu Okada (2001, Yoshioka Shoten) [Non-Patent Document 2] K. Sumitomo et al. Ca2+ ion transport through channels formed by α-hemolysin analyzed using a microwell array on a Si substrate, Biosensors and Bioelectronics, 2012: 31;445-450. Summary of the Invention [Problem to be solved by the invention]

[0010] However, even when no membrane proteins are present on the lipid bilayer membrane, results were observed suggesting that inorganic ions such as metal ions and halogen ions move from the outside of the microwell to the inside of the microwell, or from the inside of the microwell to the outside of the microwell (hereinafter, this may be referred to as ion leakage).

[0011] When analyzing the characteristics of an ion channel using a lipid bilayer membrane that holds a membrane protein such as an ion channel, such ion leakage may become noise and affect the measurement results.

[0012] Therefore, an object of the present invention is to provide a lipid bilayer membrane substrate in which ion leakage is suppressed and a method for producing the lipid bilayer membrane substrate. [Means for solving the problem]

[0013] One aspect of the present invention is a lipid bilayer membrane substrate comprising a substrate having open microwells formed on one side thereof, a lipid bilayer membrane disposed on the substrate to cover the openings of the microwells, and a sealing liquid disposed between the substrate and the lipid bilayer membrane, the sealing liquid containing an ionic liquid.

[0014] Moreover, one aspect of the present invention is a method for producing a lipid bilayer membrane substrate, comprising the steps of: dripping a sealing liquid onto a substrate having open microwells formed on one side thereof, filling the insides of the microwells with the sealing liquid and covering the edges of the microwells with the sealing liquid; adding lipid membrane vesicles to the sealing liquid on the microwells; and spreading the lipid membrane vesicles in the sealing liquid to cover the openings of the microwells with a lipid bilayer membrane, wherein the sealing liquid contains an ionic liquid. Effect of the Invention

[0015] According to the present invention, it is possible to provide a lipid bilayer membrane substrate in which ion leakage is suppressed, and a method for producing a lipid bilayer membrane substrate. [Brief description of the drawings]

[0016] [Figure 1] FIG. 1 is a perspective view of one embodiment of a lipid bilayer substrate according to the present invention. [Diagram 2] FIG. 1 is a cross-sectional view of one embodiment of a lipid bilayer substrate according to the present invention. [Diagram 3] FIG. 1 is a schematic diagram showing ion leakage in a conventional lipid bilayer substrate. [Figure 4] FIG. 1 is a cross-sectional view of one embodiment of a lipid bilayer substrate according to the present invention. [Figure 5A] FIG. 2 is a schematic cross-sectional view of a laminate. [Figure 5B] FIG. 2 is a schematic cross-sectional view of a laminate in which a recess is formed. [Figure 5C] FIG. 2 is a schematic cross-sectional view of a substrate on which microwells are formed. [Figure 5D] FIG. 2 is a schematic cross-sectional view of a substrate onto which a sealing liquid is dropped. [Figure 5E] FIG. 1 is a cross-sectional view showing a schematic view of a lipid membrane vesicle being expanded to cover the opening of a microwell. [Figure 6A] FIG. 4 is a schematic cross-sectional view of a second layer. [Figure 6B] FIG. 4 is a schematic cross-sectional view of a second layer in which electrodes are laminated. [Figure 6C] 3 is a schematic cross-sectional view of a laminate in which a first layer and a resist film are laminated on a second layer. FIG. [Figure 6D] FIG. 4 is a schematic cross-sectional view of the laminate after the resist film has been etched. [Figure 6E] FIG. 2 is a schematic cross-sectional view of a laminate having a through hole formed in a first layer. [Figure 6F] FIG. 2 is a schematic cross-sectional view of the laminate after etching through holes. [Figure 6G] FIG. 4 is a schematic cross-sectional view of the laminate after the resist film has been removed. [Figure 7] This is a photograph taken with a fluorescence microscope showing fluorescent molecules placed inside a microwell and trapped in a lipid bilayer membrane. [Figure 8] This is a photograph taken with a fluorescence microscope showing calcium inflow into the microwells. [Figure 9] 1 is a photograph taken by an electron microscope of a plating layer laminated on an electrode at the bottom of a microwell. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0017] In a conventional method for producing a lipid bilayer substrate, an electrolyte solution containing potassium ions, etc. is first dripped onto a semiconductor substrate on which microwells are formed. Then, giant lipid membrane vesicles are developed on the electrolyte solution dripped onto the microwells, thereby obtaining a lipid bilayer substrate in which the openings of the microwells are covered with lipid bilayer membranes.

[0018] It is known that a thin interfacial water layer with a thickness of about 1 to 2 nm exists between the substrate and the lipid bilayer (for example, Johnson SJ et al., Structure of an adsorbed dimyristoylphosphatidylcholine bilayer measured with specular reflection of neutrons, Biophys J. 1991; 59: 289-94.).

[0019] Ion diffusion through this interfacial water layer is thought to be the cause of the movement of inorganic ions such as metal ions and halide ions from the outside to the inside of the microwell or from the inside to the outside of the microwell (i.e., ion leakage) (e.g., Forbes et al., Hermetically sealed microwell with a lipid bilayer created using a self-assembled monolayer, Appl. Phys. Express. 2015; 8:117201).

[0020] The inventors have come to the idea that ion leakage through the interfacial water layer can be suppressed by sealing the space between the substrate and the lipid bilayer membrane with an ionic liquid aqueous solution containing an ionic liquid, rather than with an inorganic electrolyte solution such as potassium chloride or sodium chloride.

[0021] [Lipid bilayer membrane substrate] (First embodiment) A lipid bilayer membrane substrate according to one embodiment will be described with reference to the drawings. Fig. 1 is a perspective view of a lipid bilayer membrane substrate 1. FIG. 2 is a cross-sectional view taken along line II-II of the lipid bilayer substrate 1 in FIG.

[0022] 1 and 2, the lipid bilayer substrate 1A includes a substrate 12 and a lipid bilayer membrane 30 disposed on the substrate 12. Microwells 20 are formed in the substrate 12. The lipid bilayer membrane 30 is disposed so as to cover the openings 21b of the microwells 20.

[0023] The substrate 12 has a substrate body 10 having an open recess 13 formed on one surface thereof, and a thin film layer 11 laminated on the substrate body 10 .

[0024] The material of the substrate body 10 is not particularly limited, and examples thereof include silicon, silicon oxide, silicon nitride, quartz, mica, glass, plastic, etc. As the material of the substrate body 10, it is preferable to use a material that the surface of the substrate body 10 is negatively charged in an aqueous solution of pH 3 to 10. The thickness and shape of the substrate body 10 are appropriately adjusted depending on the application.

[0025] As a method for forming the recess 13 on the substrate body 10, a known method can be applied, for example, a method that combines photolithography and dry etching, or a microfabrication technique such as electron beam lithography.

[0026] The thin film layer 11 has an overhanging portion 11a that protrudes in a direction narrowing the opening 21a of the recess 13. The opening 21b of the thin film layer 11 is smaller than the opening 21a of the recess 13.

[0027] The material of the thin film layer 11 is a known material, and may be the same as the material of the substrate body 10, but is preferably different from the material of the substrate body 10. This makes it easier to perform etching when forming the overhang portion 11a.

[0028] When silicon oxide or silicon nitride is used as the material of the thin film layer 11, the thin film layer 11 constituting the surface of the substrate body 10 has a negative surface charge in a neutral solution.

[0029] The method for forming the thin film layer 11 may be, for example, a method for sputtering the material of the thin film layer 11 onto the substrate body 10. Alternatively, when the substrate body 10 is a silicon substrate, the method for forming the thin film layer 11 may be a method for forming the thin film layer 11 of a silicon oxide film on the silicon substrate by a thermal oxidation method.

[0030] The well 20 is a space surrounded by the recess 13, the overhang portion 11a, and the opening 21b of the thin film layer 11.

[0031] The thin film layer 11 may not have the overhang portion 11a. In this case, the opening 21a of the recess 13 is the same size as the opening 21b of the thin film layer 11. In this case, the microwell 20 is a space surrounded by the recess 13 and the opening 21b of the thin film layer 11.

[0032] The substrate 12 may not have the thin film layer 11. In this case, the microwell 20 is a space surrounded by the recess 13 and the opening 21a of the recess 13.

[0033] The number of wells 20 that the substrate 12 has is not particularly limited, and may be one, or two or more, for example, 1 to 10,000.

[0034] The diameter of the opening 21a of the recess 13 and the opening 21b of the microwell 20 is preferably 100 nm or more. This allows the membrane protein 31 with a size of 10 to 20 nm to be disposed on the lipid bilayer membrane 30.

[0035] The diameter of the opening 21a of the recess 13 and the opening 21b of the microwell 20 is preferably 5 μm or less, so that the lipid membrane vesicle 60 can be expanded to cover the opening 21b.

[0036] The depth of the microwells 20 may be appropriately designed depending on the diameter of the openings 21a and 21b, and may be, for example, 0.1 μm or more and 10 μm or less.

[0037] The lipid bilayer 30 may include a ternary system of saturated lipids, unsaturated lipids, and cholesterol. The type of lipid molecule of the lipid bilayer membrane 30 is not particularly limited as long as it can form a lipid bilayer membrane (lipid double membrane), and examples thereof include neutral or anionic lipid molecules such as phosphatidylcholine (PC), phosphatidylethanolamine (PE), phosphatidylserine (PS), phosphatidylinositol (PI), phosphatidylinositol phosphate (PIP), phosphatidic acid (PA), phosphatidylglycerol (PG), and sphingolipids; and cationic lipid molecules such as 1,2-dioleyl-3-trimethylammoniumpropane, trimethylammoniumpropane (TAP), and ethylphosphocholine (EPC). Only one type of these lipid molecules may be used, or two or more types may be used in combination.

[0038] The method for forming the lipid bilayer membrane 30 will be described in detail later, but for example, a method of spreading a lipid membrane vesicle on the substrate 12 can be mentioned. Here, the "lipid membrane vesicle" is formed by a lipid bilayer membrane (lipid double membrane) forming a vesicle (small follicle).

[0039] In this specification, the term "developing a lipid bilayer membrane" means that a lipid membrane vesicle is cleaved to form a lipid bilayer membrane. The lipid bilayer membrane covers the opening 21b of the microwell 20.

[0040] The material of the substrate body 10 or the thin film layer 11 is preferably one that is negatively charged in an aqueous solution of pH 3 to 10. This makes it easy for the lipid bilayer membrane to be attracted to the negatively charged surface of the thin film layer 11 by electrostatic attraction, and for the openings 21b of the microwells 20 to be covered with the lipid bilayer membrane 30.

[0041] A membrane protein 31 is introduced into the lipid bilayer membrane 30 . A method for introducing the membrane protein 31 into the lipid bilayer membrane 30 includes a method in which a proteoliposome into which the target membrane protein 31 has been introduced is prepared in advance by a known method, and the proteoliposome is fused to the lipid bilayer membrane 30. As a result, the target membrane protein 31 is introduced into the lipid bilayer membrane 30.

[0042] In the lipid bilayer membrane substrate 1A, a gap (gap 18) exists between the substrate 12 and the lipid bilayer membrane 30. The width of the gap 18 in the thickness direction is 1 to 2 nm, and the gap 18 is sealed by a sealing liquid 22. The sealing liquid 22 contains an ionic liquid. The ionic liquid contained in the sealing liquid 22 will be described in detail later.

[0043] The inside of the microwell 20 is filled with an internal liquid 22a. The composition of the internal liquid 22a is the same as the composition of the sealing liquid 22, as will be described in detail later.

[0044] The internal liquid 22a contains fluorescent molecules (fluorescent probes) 23. When ions and the like are exchanged between the external liquid 22b covering the lipid bilayer membrane 30 and the internal liquid 22a via the membrane protein 31, the exchange of ions can be observed by observing the fluorescence intensity of the fluorescent molecules 23 with a fluorescence microscope.

[0045] The internal liquid 22a may not contain the fluorescent molecules 23. In this case, as described below, the electrode section 40 and the counter electrode section 41 are connected to a measuring device to measure the current (ion current) passing through the pores of the membrane protein 31 of the lipid bilayer membrane 30, thereby making it possible to perform an electrophysiological functional analysis of the membrane protein 31 introduced into the lipid bilayer membrane 30.

[0046] The fluorescent molecules (fluorescent probes) 23 may be, for example, water-soluble molecules that emit fluorescence when a change occurs in the state inside the microwells 20. By measuring the change in the fluorescence intensity of the fluorescent molecules 23, it is possible to analyze the function of the membrane protein introduced into the lipid bilayer membrane 30.

[0047] Specific examples of the fluorescent molecules 23 include Fluo4, Quin2, etc., whose fluorescence intensity changes with changes in calcium ion concentration inside the microwells 20. When a calcium ion-permeable membrane protein is introduced into the lipid bilayer membrane 30, calcium ions permeate the lipid bilayer membrane 30 via the membrane protein, and when the calcium ion concentration inside the microwells 20 changes, the fluorescence intensity from the fluorescent molecules changes. By detecting this change with a fluorescence microscope or the like, the function of the membrane protein can be analyzed.

[0048] As shown in FIG. 2, the upper part of the lipid bilayer membrane 30 and the periphery of the opening 21b of the microwell 20 are covered with an external liquid 22b.

[0049] The type of solute in the external solution 22b is not particularly limited. Examples of the solute include pH buffers for adjusting the pH of each solution (e.g., HEPES, MOPS, TRIS, phosphates, etc.); salts (e.g., NaCl, KCl, CaCl 2 , MgCl 2 , physiological salts, etc.); sugars (glucose, sucrose, etc.); alcohols (for example, glycerol, xylitol, etc.); glycols (for example, ethylene glycol, propylene glycol, polyethylene glycol, etc.).

[0050] In the lipid bilayer membrane substrate 1A, a gap (gap 18) exists between the substrate 12 and the lipid bilayer membrane 30. The width of the gap 18 in the thickness direction is 1 to 2 nm, and the gap 18 is sealed with a sealing liquid 22. The sealing liquid 22 contains an ionic liquid.

[0051] An ionic liquid is a salt that exists in a liquid state at room temperature. An ionic liquid is a salt that is composed of cations and anions, and the electrostatic interaction between these ions is weak, making it difficult to crystallize. In this specification, room temperature is 10 to 40°C.

[0052] Ionic liquids have a melting point of 100°C or less, and further have the following characteristics 1) to 5). Characteristic 1) Extremely low vapor pressure. Characteristic 2) Non-flammable over a wide temperature range. Characteristic 3) Remains liquid over a wide temperature range. Characteristic 4) Density can be changed significantly. Characteristic 5) Polarity can be controlled.

[0053] 3 shows an example of a conventional lipid bilayer substrate, in which the sealing liquid 22 and the internal liquid 22a contain inorganic ions 22c.

[0054] Here, inorganic ions refer to inorganic cations and inorganic anions.

[0055] Examples of inorganic cations include metal ions, such as lithium ions, sodium ions, magnesium ions, aluminum ions, potassium ions, calcium ions, manganese ions, iron ions, cobalt ions, nickel ions, copper ions, and zinc ions.

[0056] Examples of inorganic anions include halide ions, such as fluoride ions, chloride ions, bromide ions, and iodide ions.

[0057] The width of the gap 18 in the thickness direction is 1 to 2 nm. In contrast, the ionic radius of the inorganic ion is 0.05 to 0.2 nm.

[0058] When the sealing liquid 22 and the internal liquid 22a contain inorganic ions 22c, the inorganic ions 22c can pass through the gap 18. Therefore, the inorganic ions 22c can move between the internal liquid 22a and the external liquid 22b of the well 20.

[0059] On the other hand, in the lipid bilayer substrate 1A according to one embodiment of the present invention, the cations and anions contained in the ionic liquid are large relative to the width in the thickness direction of the gap 18. Therefore, they cannot pass through the gap 18 at all, or cannot pass through it substantially.

[0060] Here, a case will be described in which, in a conventional lipid bilayer substrate as exemplified in FIG. 3, the external liquid 22b contains calcium ions, and the sealing liquid 22 in the gap 18 and the internal liquid 22a contain potassium ions.

[0061] When calcium ions contained in the external liquid 22b pass through the gap 18 and flow into the internal liquid 22a, the internal liquid 22a needs to be electrically neutral. Therefore, potassium ions contained in the internal liquid 22a pass through the gap 18 and flow out into the external liquid 22b.

[0062] In contrast, in a lipid bilayer membrane substrate 1A according to one embodiment of the present invention, as exemplified in FIG. 2, a case will be described in which the external liquid 22b contains calcium ions, and the sealing liquid 22 and the internal liquid 22a contain ionic liquids.

[0063] In this case, the cations of the ionic liquid contained in the internal liquid 22a cannot flow into the external liquid 22b through the gap 18. Therefore, it is presumed that the calcium ions contained in the external liquid 22b cannot flow into the internal liquid 22a through the gap 18.

[0064] In this way, it is presumed that by the sealing liquid 22 and the internal liquid 22a in the gap 18 containing ionic liquid, inorganic cations contained in the external liquid 22b can be prevented from passing through the gap 18 and flowing into the internal liquid 22a.

[0065] Similarly, it is presumed that the sealing liquid 22 and the internal liquid 22a in the gap 18 contain an ionic liquid, which can prevent inorganic anions contained in the external liquid 22b from passing through the gap 18 and flowing into the internal liquid 22a.

[0066] When it is desired to measure the amount of ions passing through the pores of the membrane protein 31 of the lipid bilayer membrane 30, the amount of ions passing through the gap 18 is reflected as noise in the measurement value.

[0067] By containing an ionic liquid in the sealing liquid 22 and the internal liquid 22a in the gap 18, the amount of ions passing through the gap 18 is reduced, and noise is reduced. Therefore, the amount of ions passing through the pores of the membrane protein 31 of the lipid bilayer membrane 30 can be measured more accurately.

[0068] The ionic liquid contained in the sealing liquid 22 and the internal liquid 22a contains one or more types of cations, and the ionic liquid contained in the sealing liquid 22 and the internal liquid 22a contains one or more types of anions.

[0069] Examples of the cations contained in the ionic liquid include the cations represented by the following formulas (ca-1) to (ca-5). In this specification, the mere mention of "cation" does not include the inorganic cations mentioned above.

[0070] [ka] [In the formula, R c1 ~R c6 R is each independently an alkyl group having 1 to 12 carbon atoms. c7 ~R c9 R is an aryl group which may have a substituent. c10 ~R c13 are each independently a linear alkyl group having 1 to 20 carbon atoms.]

[0071] The ionic radius of the cations contained in the ionic liquid is preferably larger than the gap 18 between the lipid bilayer membrane 30 and the substrate 12. More specifically, the ionic radius of the cations contained in the ionic liquid is preferably 1 nm or more, more preferably 1.5 nm or more, and even more preferably 2 nm or more.

[0072] Examples of the anion contained in the ionic liquid include anions represented by the following formulas (an-1) to (an-3). In this specification, the mere mention of "anion" does not include the inorganic anions mentioned above.

[0073] [ka] [In formula (an-1), R a1 represents an aromatic hydrocarbon group which may have a substituent, an aliphatic cyclic group which may have a substituent, or a chain hydrocarbon group which may have a substituent. a2 represents an alkyl group having 1 to 5 carbon atoms which may be substituted with a fluorine atom, k is an integer of 1 to 4, l is an integer of 0 to 3, and k+l=4. a3 represents an alkyl group having 1 to 5 carbon atoms which may be substituted with a fluorine atom, m is an integer of 1 to 6, n is an integer of 0 to 5, and m+n=6.

[0074] The ionic radius of the anion contained in the ionic liquid is preferably larger than the gap 18 between the lipid bilayer membrane 30 and the substrate 12. More specifically, the ionic radius of the anion contained in the ionic liquid is preferably 1 nm or more, more preferably 1.5 nm or more, and even more preferably 2 nm or more.

[0075] As the ionic liquid, it is preferable to use a hydrophilic ionic liquid. In this specification, "hydrophilic" means that it can be dissolved or completely dispersed in an aqueous solvent.

[0076] Examples of the cation of the hydrophilic ionic liquid include a quaternary ammonium cation, a phosphonium cation, a pyridinium cation, and a piperidinium cation.

[0077] Examples of anions of hydrophilic ionic liquids include phosphate ions, acetate ions, citrate ions, tetrafluoroborate ions, and hexafluorophosphate ions.

[0078] More specifically, examples of hydrophilic ionic liquids include choline dihydrogen phosphate, choline dihydrogen citrate, 1-ethylpyridinium tetrafluoroborate, 1-butylpyridinium bromide, 1-butyl-4-methylpyridinium tetrafluoroborate, 1-(3-cyanopropyl)pyridinium chloride, 1-butyl-1-methylpiperidinium hexafluorophosphate, and choline acetate.

[0079] The ionic liquid contained in the sealing liquid 22 and the internal liquid 22a may contain one or more types of cations and one or more types of anions.

[0080] When the ionic liquid contained in the sealing liquid 22 and the internal liquid 22a contains the above-mentioned cations, the sealing liquid 22 and the internal liquid 22a may contain anions other than the above-mentioned anions.

[0081] Examples of other anions include the above-mentioned inorganic anions and polyatomic anions.

[0082] When the ionic liquid contains the above-mentioned cations, it is preferable that the sealing liquid 22 and the internal liquid 22a do not contain the above-mentioned inorganic cations, which makes it possible to prevent the inorganic cations contained in the internal liquid 22a from passing through the gap 18 and flowing out into the external liquid 22b.

[0083] As a result, it is possible to suppress inorganic cations contained in the external liquid 22b from passing through the gap 18 and flowing into the internal liquid 22a. This makes it possible to more accurately measure the amount of inorganic cations that pass through the pores of the membrane protein 31 of the lipid bilayer 30 from the external liquid 22b and flow into the internal liquid 22a.

[0084] In addition, when the ionic liquid contained in the sealing liquid 22 and the internal liquid 22a contains the above-mentioned anions, the sealing liquid 22 and the internal liquid 22a may contain cations other than the above-mentioned cations.

[0085] Other cations include the above-mentioned inorganic cations and polyatomic cations.

[0086] When the ionic liquid contained in the sealing liquid 22 and the internal liquid 22a contains the above-mentioned anions, it is preferable that the sealing liquid 22 and the internal liquid 22a do not contain the above-mentioned inorganic anions, which makes it possible to prevent the inorganic anions contained in the internal liquid 22a from passing through the gap 18 and flowing out into the external liquid 22b.

[0087] As a result, it is possible to suppress inorganic anions contained in the external liquid 22b from passing through the gap 18 and flowing into the internal liquid 22a. This makes it possible to more accurately measure the amount of inorganic anions flowing from the external liquid 22b through the pores of the membrane protein 31 of the lipid bilayer 30 and into the internal liquid 22a.

[0088] 2, the lipid bilayer membrane substrate 1A has an electrode section 40 and a counter electrode section 41. The electrode section 40 has an electrode 40a in contact with the internal liquid 22a filling the inside of the microwell 20, and a conducting wire 40b connected to the electrode 40a. The electrode 40a is disposed on the inner circumferential surface of the microwell 20.

[0089] The counter electrode portion 41 of the lipid bilayer membrane substrate 1A has a counter electrode 41a in contact with the external liquid 22b that covers the outside of the microwells 20, and a conducting wire 41b connected to the counter electrode 41a.

[0090] Examples of materials for the electrode 40a and the counter electrode 41a include silver / silver chloride, gold, and platinum.

[0091] By connecting the electrode unit 40 and the electrode unit 41 to a measuring instrument and measuring the current (ion flow) passing through the pores of the membrane protein 31 in the lipid bilayer membrane 30, an electrochemical functional analysis can be performed on the membrane protein 31 introduced into the lipid bilayer membrane 30.

[0092] The lipid bilayer membrane substrate 1A may not have the electrode portion 40. In this case, the amount of ions passing through the pores of the membrane protein 31 can be measured using the fluorescent molecules 23 contained in the internal liquid 22a of the microwells 20.

[0093] The lipid bilayer membrane substrate 1A may not have the electrode portion 41. In this case, a separately prepared electrode is brought into contact with the external liquid 22b of the microwell 20, and this electrode and the electrode portion 40 are connected to a measuring device to measure the potential difference or current.

[0094] By using a sealing liquid 22 containing an ionic liquid, it is possible to more accurately measure the amount of ions passing through the pores of the membrane protein 31 of the lipid bilayer membrane 30, for example, using the electrode unit 40 and the counter electrode unit 41.

[0095] Second embodiment FIG. 4 illustrates a cross-sectional view of a lipid bilayer substrate 1B according to one embodiment. 4, the lipid bilayer substrate 1B has a substrate 100 having a first layer 51 and a second layer 52. The substrate 100 has an electrode 43 sandwiched between the first layer 51 and the second layer 52.

[0096] In the lipid bilayer membrane substrate 1B, the same parts as those in the lipid bilayer membrane substrate 1A of the first embodiment are denoted by the same reference numerals and the description thereof will be omitted.

[0097] The first layer 51 of the lipid bilayer substrate 1B has a substrate body 10a in which a through-hole 13a is formed penetrating in the thickness direction. The first layer 51 does not necessarily have to have a thin film layer 11.

[0098] The second layer 52 has a second layer substrate body 52a and an insulating layer 52b laminated on the second layer 52 substrate body 52a.

[0099] The material of the insulating layer 52b is not particularly limited, and examples thereof include silicon, silicon oxide, silicon nitride, quartz, mica, glass, plastic, etc. When the substrate body 52a is insulating, examples of the material of the substrate body 52a include the insulating materials described above.

[0100] The method for forming the insulating layer 52b may be, for example, a method for sputtering the material of the insulating layer 52b onto the second layer of the substrate body 52a.

[0101] When the insulating layer 52b is made of silicon oxide, the insulating layer 52b may be formed on the substrate body 52a of the second layer 52 by using a thermal oxidation method using a substrate body 52a made of silicon.

[0102] The first layer 51 has a through hole 13a penetrating in the thickness direction. An electrode 43 is exposed at the lower end of the through hole 13a. The space surrounded by the through-hole 13 a , the overhang portion 11 a , the opening 21 b of the thin film layer 11 , and the electrode 43 constitutes a microwell 20 .

[0103] The electrode 43 is plated with a plating layer 42. A part of the plating layer 42 extends over the lower end 13b of the through hole 13a. The electrode 43 does not necessarily have to have the plating layer 42.

[0104] The metal element contained in the plating layer 42 is not particularly limited as long as it has high electrical conductivity and can be used to prepare a plating solution, and examples of the metal element include silver / silver chloride, gold, and platinum.

[0105] The electrode 43 having the plating layer 42 on its surface is preferably a non-polarized electrode. An example of a non-polarized electrode is a chlorinated silver electrode.

[0106] The plating layer 42 has a larger surface area and a larger surface roughness than the surface of the unplated electrode 43. Therefore, the electrode 43 on which the plating layer 42 is formed has a higher measurement sensitivity than the unplated electrode 43.

[0107] The above-mentioned lipid bilayer membrane substrates 1A and 1B make it possible to suppress ion leakage through the thin interfacial water layer existing between the substrate 12 and the lipid bilayer membrane 30.

[0108] The ion current passing through the channel of the membrane protein 31 is weak, so with the conventional technology it was difficult to distinguish whether the response obtained was due to a channel signal derived from the membrane protein or due to ion leakage.

[0109] In contrast, according to the present invention, ion leakage is suppressed, making it possible to measure the function of the membrane protein 31 at the molecular level. Furthermore, the analysis method using the lipid bilayer substrates 1A and 1B is simpler than the patch clamp method, and therefore makes it possible to specifically measure the function of the target protein.

[0110] Furthermore, by forming an array of microwells 20 using semiconductor technology, it is expected that the array will be applicable to high-throughput screening in the field of drug discovery.

[0111] [Manufacturing method] (First embodiment) 5A to 5E are process drawings showing a method for producing the lipid bilayer membrane substrate 1A illustrated in Fig. 2. The method for producing the lipid bilayer membrane substrate 1A includes the following steps (a) to (f).

[0112] Step (a): A step of forming a thin film layer 11 on a substrate body 10 to obtain a laminate 14

[0113] Step (b): A step of etching the laminate 14 to form a recess 13 in the substrate body 10.

[0114] Step (c): Etching the substrate body 10 at the recess 13

[0115] Step (d): A step of dropping a sealing liquid 22 onto the substrate 12 to fill the inside of the microwells 20 with the sealing liquid 22 and cover the periphery of the microwells 20 with the sealing liquid 22.

[0116] Step (e): Adding lipid membrane vesicles 60 to the sealing liquid 22 on the microwells 20

[0117] Step (f): A step of spreading the lipid membrane vesicle 60 in the sealing liquid 22 and covering the opening of the microwell 20 with the lipid bilayer membrane 30.

[0118] Each step will be described in detail below.

[0119] <Process (a)> As illustrated in FIG. 5A, in step (a), a thin film layer 11 is formed on a substrate body 10 to obtain a laminate 14.

[0120] Materials for the substrate body 10 and the thin film layer 11 include those mentioned above. The method for forming the thin film layer 11 may be, for example, a method for sputtering the material of the thin film layer 11 onto the substrate body 10. Alternatively, when the substrate body 10 is a silicon substrate, the thin film layer 11 may be formed of a silicon oxide film on the silicon substrate by a thermal oxidation method.

[0121] <Process (b)> As illustrated in FIG. 5B, in step (b), the laminate 14 is etched to form a recess 13 in the substrate body 10. The method for etching the laminate 14 is not particularly limited, but may be, for example, a combination of electron beam lithography, photolithography and dry etching.

[0122] <Process (c)> 5C, in step (c), the substrate body 10 is etched in the recess 13. As a method for etching the substrate body 10, a wet etching method can be mentioned.

[0123] Examples of solutions used in the wet etching method include alkaline solutions such as sodium hydroxide and potassium hydroxide solutions.

[0124] The etching rate of the substrate body 10 is higher than that of the thin film layer 11. Therefore, an overhanging portion 11a is formed that extends in a direction narrowing the opening 21a of the recess 13. In this manner, a microwell 20, which is a space surrounded by the recess 13, the thin film layer 11, and the opening 21b of the thin film layer 11, is obtained.

[0125] <Process (d)> As illustrated in FIG. 5D, in step (d), a sealing liquid 22 is dropped onto the substrate 12 to fill the inside of the wells 20 with the sealing liquid 22 and to cover the periphery of the wells 20 with the sealing liquid 22.

[0126] The sealing liquid 22 contains an ionic liquid. Examples of the ionic liquid include those mentioned above.

[0127] <Process (e)> As illustrated in FIG. 5E, in step (e), the above-mentioned lipid membrane vesicle 60 is added to the external solution 22b above the microwells 20.

[0128] Representative techniques for forming lipid membrane vesicles 60 include the static hydration method (e.g., Akashi K et al., Preparation of giant liposomes in physiological conditions and their characterization under an optical microscope, Biophys J. 1996; 71: 3242-3250.) and the electric field formation method (e.g., Dimitrov DS and Angelova MI, Lipid swelling and liposome formation mediated by electric fields, 1998; 19: 323-336.).

[0129] It is preferable to adopt an electric field formation method as a method for forming the lipid membrane vesicle 60. The electric field formation method is easy to prepare the lipid membrane vesicle 60, and the reaction time and reaction process are simple. The electric field formation method is a technique in which a phospholipid is made into a thin film on an electrode such as indium tin oxide (ITO), and then an alternating electric field is applied to form a giant lipid membrane vesicle in an aqueous solution.

[0130] The lipid membrane vesicle 60 is large enough that, when it is spread onto the microwell 20 of the substrate 12 to become a planar lipid bilayer membrane 30, it can sufficiently cover the opening 21b of one or more microwells 20 pre-arranged on the substrate.

[0131] The diameter (major axis) of the lipid membrane vesicle 60 is preferably 1 μm or more, more preferably 3 μm or more, further preferably 5 μm or more, and particularly preferably 10 μm or more, so that the lipid bilayer membrane 30 formed by spreading can reliably cover the opening 21b of the microwell 20.

[0132] The diameter of the lipid membrane vesicle 60 is preferably 100 μm or less, more preferably 50 μm or less, and even more preferably 30 μm or less, so that the structure of the lipid membrane vesicle 60 can be maintained. The diameter of the lipid membrane vesicle is measured by a common optical observation method.

[0133] In order to obtain lipid membrane vesicles of uniform size, it is preferable to form a uniform membrane of phospholipid molecules with a thickness of several tens of nm to several μm on an ITO substrate, and it is preferable to apply an AC electric field of about several hundred mV to 2 V.

[0134] <Process (f)> As illustrated in FIG. 5E, in step (f), the lipid membrane vesicle 60 is developed in the sealing liquid 22 to cover the opening 21b of the microwell 20 with the lipid bilayer membrane 30.

[0135] After a certain period of time has elapsed after step (e), the lipid membrane vesicle 60 is cleaved in the sealing liquid 22 to become a lipid bilayer membrane.

[0136] When the material of the thin film layer 11 is silicon oxide, silicon nitride, or the like, and the sealing liquid 22 is a neutral solution, the thin film layer 11 has a negative surface charge. The lipid bilayer membrane formed by cleavage is attracted to the surface of the thin film layer 11 by electrostatic attraction, and the opening 21 b of the microwell 20 is covered with the lipid bilayer membrane 30 .

[0137] In step (f), the gap 18 between the substrate 12 and the lipid bilayer membrane 30 is sealed with the sealing liquid 22 .

[0138] The certain period of time is not particularly limited, but is preferably, for example, 30 seconds to 10 minutes. This allows the openings 21b of the microwells 20 to be covered with the lipid bilayer membrane 30 reliably.

[0139] When the opening 21b of the microwell 20 is covered with the lipid bilayer membrane 30, the lipid bilayer membrane 30 covering the microwell 20 is covered with the sealing liquid 22. The composition of the internal liquid 22a inside the microwell 20 is the same as that of the sealing liquid 22.

[0140] The sealing liquid 22 covering the openings 21b of the microwells 20 may be removed, and a solution other than the sealing liquid 22 may be dropped onto the substrate 12 to cover the microwells 20 with the external liquid 22b. The types of the external liquid 22b include those mentioned above.

[0141] Second embodiment 6A to 6G are process diagrams showing a method for producing the lipid bilayer membrane substrate 1B illustrated in Fig. 4. The method for producing the lipid bilayer membrane substrate 1B includes the following steps (i) to (x) prior to the above-mentioned steps (d) to (f).

[0142] Step (i): A step of laminating an insulating layer 52b on a substrate body 52a to obtain a second layer 52.

[0143] Step (ii): A step of laminating an electrode 43 on the second layer 52

[0144] Step (iii): A step of forming the substrate body 10 on the electrode 43.

[0145] Step (iv): A step of stacking the thin film layer 11 on the substrate body 10 to form a first layer 51 having the substrate body 10 and the thin film layer 11 on the electrode 43.

[0146] Step (v): forming a resist film 55 on the thin film layer 11

[0147] Step (vi): A step of etching the resist film 55 to form a resist pattern.

[0148] Step (vii): forming through holes 13a in the first layer 51

[0149] Step (viii): A step of etching the substrate body 10 to form a microwell 20 surrounded by the through-hole 13a, the overhang portion 11a, the opening 21a of the through-hole 13a, and the electrode 43 exposed within the through-hole 13a.

[0150] Step (ix): Removing the resist film 55

[0151] Step (x): A step of forming a plating layer 42 on the surface of the electrode 43, which is the bottom surface of the microwell 20.

[0152] Each step will be described in detail below.

[0153] <Process (i)> As illustrated in FIG. 6A, in step (i), an insulating layer 52b is laminated on a substrate body 52a to obtain a second layer 52.

[0154] Examples of the material of the substrate body 50 include the same as the material of the substrate body 10 described above. Examples of the material of the insulating layer 52b include the same as the material of the thin film layer 11. Examples of the method of forming the insulating layer 52b include the same as the method of forming the thin film layer 11.

[0155] <Process (ii)> As illustrated in FIG. 6B, in step (ii), an electrode 43 is laminated on the second layer 52.

[0156] Examples of materials for the electrodes 43 include gold, platinum, silver, and copper. The electrode 43 may be formed by sputtering or by plating the surface of the second layer 52 with a metal material.

[0157] <Step (iii)> As illustrated in FIG. 6C, in step (iii), the substrate body 10 is laminated on the electrode 43. The above-mentioned materials can be used as the material of the substrate body 10. Methods for forming the substrate body 10 on the electrode 43 include, for example, a sputtering method, a plasma method, and the like.

[0158] <Process (iv)> As illustrated in FIG. 6C, in step (iv), the thin film layer 11 is laminated on the substrate body 10 to form a first layer 51 having the substrate body 10 and the thin film layer 11 on the electrode 43. The materials for the thin film layer 11 include those mentioned above. The methods for forming the thin film layer 11 include those mentioned above.

[0159] <Process (v)> As illustrated in FIG. 6C, in step (v), a resist film 55 is formed on the thin film layer 11. Materials known to those skilled in the art can be used as the material of the resist film 55. The method for forming the resist film 55 may be a method known to those skilled in the art.

[0160] <Process (vi)> 6D, in step (vi), a resist pattern is formed by etching the resist film 55. The etching method may be photolithography or electron beam lithography.

[0161] <Process (vii)> As illustrated in FIG. 6E, in step (vii), through holes 13a are formed by dry etching or electron beam lithography in the first layer 51 having the resist film 55 on which the resist pattern is formed.

[0162] <Process (viii)> As illustrated in FIG. 6F, in step (viii), a microwell 20 surrounded by through-hole 13a, overhang portion 11a, opening 21a of through-hole 13a, and electrode 43 exposed within through-hole 13a is formed by wet etching.

[0163] The etching rate of the substrate body 10a is higher than the etching rate of the thin film layer 11. Therefore, an overhanging portion 11a is formed that protrudes in a direction narrowing the opening 21a of the through hole 13a.

[0164] <Process (ix)> 6G, in step (ix), the resist film 55 is removed. As a method for removing the resist film 55, a method known to those skilled in the art can be used.

[0165] <Process (x)> In the step (x), a plating layer 42 is formed on the surface of the electrode 43 in the through hole 13a.

[0166] The above-mentioned materials can be used as the plating layer 42. The plating layer 42 can be formed by electroplating.

[0167] Specifically, in the electroplating method, a plating solution is first dropped onto the microwells 20. As the plating solution, an electrolyte solution known to those skilled in the art may be used.

[0168] Next, a current is passed through the plating metal while it is immersed in the plating solution, and the plating metal is deposited on the surface of the electrode 43. Examples of the plating metal include copper, silver, gold, platinum, etc.

[0169] When silver is used as the plating metal, the silver plating may be chlorinated after the silver plating, so that the electrode 43 in the through hole 13a can be made into a non-polarized electrode. EXAMPLES

[0170] The present invention will be described below with reference to examples, but the present invention is not limited to the following examples. In this specification, the unit "M" means "mol / L".

[0171] [Experimental Example 1] (Preparation of lipid bilayer substrate) Using an ionic liquid as a sealing liquid, lipid membrane vesicles were developed on a substrate having microwells, and a lipid bilayer substrate was obtained in which the openings of the microwells were covered with a lipid bilayer membrane.

[0172] <Substrate> A silicon substrate was used as the substrate body, and then a silicon oxide film layer having a thickness of 120 nm was formed as a thin film layer on the upper surface of the silicon substrate by thermal oxidation.

[0173] Next, recesses having circular openings (diameters of 2 μm and 4 μm) were formed by photolithography and dry etching.

[0174] Next, the substrate body under the thin film layer was selectively etched using an aqueous potassium hydroxide solution (10% by mass) to form an overhanging portion of the thin film layer, thereby obtaining a substrate having microwells.

[0175] <Preparation of giant lipid membrane vesicles> First, a solution was prepared using diphytanylphosphatidylcholine (DPhPC) (80 mol %), which is neutrally charged at about pH 7, cholesterol (20 mol %), and chloroform.

[0176] Rhodamine-dipalmitoylphosphatidylethanolamine (Rhod-DOPE) was added to the obtained solution in an amount of 0.05 mol % relative to the total amount of lipids contained in the solution (100 mol %) to prepare a mixed lipid solution.

[0177] Next, the ITO substrate (SiO 2 200 μL of the mixed chloroform solution was uniformly applied onto a substrate (size: 40×40 mm) on which an ITO thin film had been formed.

[0178] This substrate was dried under reduced pressure at room temperature for 2 hours to completely remove the chloroform solvent, forming a uniform lipid molecular thin film on the ITO substrate. A 1 mm thick silicone rubber with an outer dimension of 30 × 30 mm and a 20 × 20 mm window was placed on top of the substrate, and 500 μL of 200 mM sucrose solution was dropped into the window.

[0179] Furthermore, an ITO substrate was placed on top of it while being careful not to trap air bubbles, and the solution in the silicone rubber window was sandwiched between the ITO substrates. Next, a clip electrode was attached to the ITO substrate, and an AC electric field was applied in a thermostatic chamber to obtain a sucrose dispersion of lipid membrane vesicles by the electric field formation method.

[0180] <Deployment of lipid membrane vesicles onto substrates> On the substrate having the microwells, 100 μL of an ionic liquid aqueous solution (a mixed solution of 160 mM glucose, 20 μM calcein, 1 mM EDTA, and 20 mM choline dihydrogen phosphate) was dropped as a sealing liquid.

[0181] A sucrose dispersion of lipid membrane vesicles was dropped onto the substrate and left to stand for 5 minutes to spread the lipid membrane vesicles on the substrate, covering the openings of the microwells of the substrate with a lipid bilayer membrane, thereby sealing the gap between the substrate and the lipid bilayer membrane with a sealing liquid.

[0182] At this time, the inner liquid of the microwell was filled with the sealing liquid, and the microwell and the lipid bilayer membrane were covered with the sealing liquid (external liquid).

[0183] Next, the sealing solution was removed from the external solution covering the top of the microwells, and the external solution in the wells was replaced with a 200 mM glucose solution. The results are shown in Figure 7.

[0184] Figure 7 is a photograph of calcein fluorescence taken by a fluorescence microscope. In Figure 7, 30 indicates a lipid bilayer membrane spread on a substrate, 20a indicates a microwell in which calcein fluorescence was observed, and 20b indicates a microwell in which calcein fluorescence was not observed. In Figure 7, 11 indicates a thin film layer, and 30 indicates a lipid bilayer membrane spread on the thin film layer.

[0185] 20a shows that the opening of the well is covered with a lipid bilayer, so that calcein is trapped inside the well, and 20b shows that the opening of the well is not covered with a lipid bilayer, so that calcein is not trapped inside the well.

[0186] [Experimental Example 2] (Suppression of ion leakage by ionic liquid) Two types of lipid bilayer substrates were prepared in the same manner as in Experimental Example 1, except that an inorganic ion aqueous solution (a mixed solution of 200 mM glucose, 20 μM fluo-4, 1 mM EDTA, and 20 mM potassium chloride) or an ionic liquid aqueous solution (a mixed solution of 160 mM glucose, 20 μM fluo-4, 1 mM EDTA, and 20 mM choline dihydrogen phosphate) was used as the sealing liquid. Here, fluo-4 is a calcium fluorescent probe.

[0187] Next, a calcium chloride solution was dropped into the external solution covering the microwells of each lipid bilayer substrate. By observing the fluorescence of fluo-4 in the microwells, the flow of calcium ions contained in the external solution through the gaps and into the internal solution was monitored in the two types of lipid bilayer substrates obtained.

[0188] Here, the inventors speculate as follows. It is known that an interfacial water layer with a thickness of 1 to 2 nm is formed between the lipid bilayer and the substrate (hereinafter, simply referred to as the "gap"). The ionic radius of potassium ions is approximately 0.15 nm, and it is believed that potassium ions can easily pass through the gap.

[0189] The chemical structure of choline dihydrogen phosphate is shown below. The cation and anion of choline dihydrogen phosphate are bulky compared to inorganic ions. It is believed that the choline ion, which is a cation, has difficulty passing through gaps.

[0190] [ka]

[0191] In order for calcium ions contained in the external liquid of the microwell to pass through the gap and flow into the internal liquid of the microwell, it is necessary for cations contained in the internal liquid of the microwell to pass through the gap and flow out from the internal liquid of the microwell to the external liquid, so that the internal and external liquids of the microwell must maintain electrical neutrality.

[0192] When a potassium chloride solution is used as the sealing liquid, potassium ions can easily pass through the gap and move from the liquid inside the well to the liquid outside the well, and therefore calcium ions contained in the liquid outside the well can pass through the gap and flow into the liquid inside the well.

[0193] On the other hand, when a choline dihydrogen phosphate aqueous solution is used as the sealing liquid, choline has difficulty passing through the gap and is difficult to move from the internal liquid of the microwell to the external liquid, so that calcium ions contained in the external liquid of the microwell are prevented from passing through the gap and flowing into the internal liquid of the microwell.

[0194] FIG. 8 shows the results of measuring the time course of the fluorescence intensity of fluo-4 inside the microwells. In Fig. 8, (a) shows the results when an inorganic ion aqueous solution was used as the sealing liquid, and (b) shows the results when an ionic liquid aqueous solution was used as the sealing liquid. In Fig. 8, t indicates the time elapsed after the calcium chloride aqueous solution was dropped, and the arrow indicates the microwell covered with the lipid bilayer membrane.

[0195] Immediately after the addition of the calcium chloride solution (t = 0), almost no change in fluorescence intensity was observed in any of the lipid bilayer substrates. In other words, it was confirmed that no calcium flowed from the external solution to the internal solution of the microwell immediately after the calcium chloride solution was added to the external solution of the microwell.

[0196] In the lipid bilayer substrate using an aqueous inorganic ion solution as the sealing liquid, fluo-4 fluorescence was observed in the microwells covered with the lipid bilayer in about 8 minutes.

[0197] These results indicate that in the lipid bilayer substrate using an aqueous inorganic ion solution as the sealing liquid, calcium ions contained in the external liquid covering the lipid bilayer passed between the lipid bilayer and the substrate and flowed into the inside of the microwell.

[0198] In contrast, in the case of the lipid bilayer substrate using an ionic liquid aqueous solution as the sealing liquid, no significant change in fluorescence intensity was observed even after 30 minutes or more.

[0199] These results indicate that in lipid bilayer substrates using an ionic liquid aqueous solution as a sealing liquid, calcium ions contained in the external liquid covering the lipid bilayer do not pass between the lipid bilayer membrane and the substrate and flow into the inside of the microwells, or else flow into the inside of the wells is significantly suppressed.

[0200] In other words, it was revealed that the movement of ions through the gap between the lipid bilayer membrane and the substrate was reduced by sealing the gap between the lipid bilayer membrane and the substrate with a sealing liquid containing an ionic liquid.

[0201] It has become clear that the lipid bilayer membrane substrate of the present invention, which uses a sealing liquid containing an ionic liquid, is suitable for introducing a membrane protein into a lipid bilayer membrane substrate, reducing noise in the measured current and potential, and measuring the function of the membrane protein with high sensitivity.

[0202] [Experimental Example 3] (Production of lipid bilayer substrate with electrodes) First, a silicon wafer was used as the substrate body for the second layer, and the second layer was obtained by covering it with a thermal oxide film (the second insulating layer) having a thickness of 120 nm by thermal oxidation.

[0203] A 60 nm thick gold layer was then deposited on the second layer and patterned by photolithography to form an electrode approximately 60 nm thick.

[0204] This electrode is connected to a sufficiently large pad (300 μm square) and can be connected to an electrophysiological measurement device such as a patch clamp measurement device by normal wire bonding.

[0205] A silicon nitride film was deposited on the electrode to a thickness of 1 μm by plasma CVD to form the first layer of the substrate body. Then, a silicon oxide film (first layer of thin film) was deposited to a thickness of 200 nm by sputtering on the first layer of the substrate body to obtain a substrate having the first and second layers.

[0206] Next, a resist film was laminated on the first layer, and then a resist pattern was formed by photolithography. Next, through holes were formed in the first layer by dry etching, and the surfaces of the electrodes were exposed.

[0207] Next, an overhang was formed in the first thin film layer by wet etching, taking advantage of the selectivity between the first substrate body and the first thin film layer.The resist film was then removed by washing.

[0208] As a result, a substrate was obtained in which a microwell was formed, the microwell being surrounded by the through-hole of the first layer and the electrode exposed within the through-hole.

[0209] A lipid bilayer membrane substrate was obtained by spreading lipid membrane vesicles on the obtained substrate using a sealing liquid containing an ionic liquid, thereby covering the openings of the microwells with a lipid bilayer membrane.

[0210] It is possible to introduce a membrane protein into the lipid bilayer membrane covering the microwells of the obtained lipid bilayer membrane substrate by the vesicle fusion method, etc. In addition, by providing a counter electrode on this lipid bilayer membrane substrate and measuring the current flowing between the electrode and the counter electrode when a voltage is applied between them, it is possible to detect the ionic current mediated by the membrane protein.

[0211] [Experimental Example 4] (Production of lipid bilayer substrate equipped with electrodes having a plating layer) Using the substrate having electrodes obtained in Experimental Example 3, plating was applied to the electrodes to produce a substrate having non-polarized electrodes.

[0212] On the substrate having the electrodes obtained in Experimental Example 3, 200 μL of a silver plating solution (PreciousFab Ag4710, Tanaka Kikinzoku) was dropped.

[0213] A silver wire connected to a manual prober was placed in the plating solution, and the electrode was connected to the manual prober. A constant current (0.1-0.5 nA) was applied between the silver wire and the electrode for 1 minute to plate the surface of the electrode with silver. The electrode was then immersed in a chlorine-based bleaching solution for 2 minutes to chlorinate the silver surface, resulting in a silver / silver chloride electrode. The results are shown in Figure 9.

[0214] Figure 9 is a photograph of the bottom of the microwell taken with an electron microscope. It was clear that a silver / silver chloride electrode was formed on the bottom of the microwell. It was also clear that the silver / silver chloride surface has an uneven surface, increasing the surface area, making it a more suitable shape for electrophysiological measurements.

[0215] A lipid bilayer membrane substrate was produced on this substrate having a non-polarized electrode in the same manner as in Experimental Example 1, using a sealing liquid containing an ionic liquid.

[0216] The obtained lipid bilayer substrate can be used to introduce membrane proteins into the lipid bilayer covering the microwells by the vesicle fusion method, etc. In addition, by providing a counter electrode on this lipid bilayer substrate and measuring the current flowing between the non-polarized electrode and the counter electrode when a voltage is applied between them, the ionic current mediated by the membrane protein can be detected with high sensitivity. [Industrial Applicability]

[0217] The present invention provides a lipid bilayer membrane substrate with suppressed ion leakage and a method for producing the lipid bilayer membrane substrate. The lipid bilayer membrane substrate is suitably used for functional analysis of membrane proteins. [Explanation of symbols]

[0218] 1A, 1B... lipid bilayer substrate, 10, 10a... substrate body, 11... thin film layer, 11a... overhanging portion, 12... substrate, 13... recessed portion, 13a... through hole, 13b... end portion, 14... laminated body, 18... gap, 20... microwell, 21a, 21b... opening portion, 22... sealing liquid, 22a... inner liquid, 22b... outer liquid, 23... fluorescent material Photomolecule, 30... lipid bilayer membrane, 31... membrane protein, 40... electrode section, 40a... electrode, 40b... conducting wire, 41... counter electrode section, 41a... counter electrode, 41b... conducting wire, 43... electrode layer, 51... first layer, 52... second layer, 52a... substrate body, 52b... insulating layer, 55... resist film, 60... lipid membrane vesicle, 100... substrate

Claims

1. A substrate having an open microwell formed on one surface thereof; a lipid bilayer membrane disposed on the substrate and covering the opening of the microwell; a sealing liquid disposed between the substrate and the lipid bilayer membrane; The sealing liquid contains an ionic liquid, the cation of the ionic liquid is at least one selected from a quaternary ammonium cation, a phosphonium cation, a pyridinium cation, and a piperidinium cation; the anion of the ionic liquid is at least one selected from the group consisting of a phosphate ion, an acetate ion, a citrate ion, a tetrafluoroborate ion, and a hexafluorophosphate ion; The lipid bilayer substrate, wherein the phosphonium cation is a cation represented by the following general formula (ca-5): 【Chemistry 1】 [In the formula, R c10 to R c13 each independently represent a linear alkyl group having 1 to 20 carbon atoms.]

2. The lipid bilayer membrane substrate according to claim 1 , wherein an electrode is provided on the inner peripheral surface of the microwell.

3. The lipid bilayer substrate according to claim 2 , wherein the electrode has a plating layer on a surface thereof.

4. the substrate has a first layer, a second layer, and the electrode sandwiched between the first layer and the second layer; The first layer has a through hole penetrating in a thickness direction, The electrode is exposed at a lower end of the through hole, The lipid bilayer membrane substrate according to any one of claims 2 to 3, wherein a space surrounded by said through-hole and said electrode constitutes said microwell.

5. The lipid bilayer substrate according to claim 4 , wherein the second layer comprises an insulating layer.

6. a step of dropping a sealing liquid onto a substrate having an open microwell formed on one surface thereof, filling the inside of the microwell with the sealing liquid, and covering the periphery of the microwell with the sealing liquid; adding lipid membrane vesicles to the sealing liquid on the microwells; and spreading the lipid membrane vesicle in the sealing liquid to cover the opening of the microwell with a lipid bilayer membrane; The sealing liquid contains an ionic liquid, the cation of the ionic liquid is at least one selected from a quaternary ammonium cation, a phosphonium cation, a pyridinium cation, and a piperidinium cation; the anion of the ionic liquid is at least one selected from the group consisting of a phosphate ion, an acetate ion, a citrate ion, a tetrafluoroborate ion, and a hexafluorophosphate ion; The method for producing a lipid bilayer substrate, wherein the phosphonium cation is a cation represented by the following general formula (ca-5): 【Chemistry 2】 [In the formula, R c10 to R c13 each independently represent a linear alkyl group having 1 to 20 carbon atoms.]

7. Prior to the step of covering with the sealing liquid, The method further includes a step of forming the microwells in a substrate body having a first layer, an electrode, and a second layer stacked thereon to obtain the substrate, The method for producing a lipid bilayer substrate according to claim 6, wherein in the step of obtaining the substrate, a through-hole is formed in the first layer, and the microwell is formed so as to be surrounded by the through-hole and the electrode exposed within the through-hole.

Citation Information

Patent Citations

  • Method of controlling biomolecule mobility and electrophoresis tank

    JP2017037029A

  • Lipid bilayer membrane substrate

    JP2017038539A

  • Lipid bimolecular membrane substrate

    JP2019037213A

  • Biological molecule movement control method and device

    JP2019105484A