Electronic devices

The package design with a high thermal conductivity heat sink and chamfered edges in the frame and lid addresses bonding reliability issues, enhancing heat dissipation and airtightness by reducing stress concentration in the adhesive layer.

JP7558882B2Active Publication Date: 2024-10-01NGK ELECTRONICS DEVICES INC +1
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2021074861
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-04-27
Publication Date
2024-10-01
Estimated Expiration
2041-04-27

AI Technical Summary

Technical Problem

Existing packages with heat sinks face challenges in ensuring bonding reliability between the frame and lid due to high thermal expansion coefficients, leading to cracks and loss of airtightness, while maintaining high thermal conductivity is also difficult with limited expansion coefficients.

Method used

A package design with a heat sink having a linear expansion coefficient of 9 ppm/°C to 15 ppm/°C, a ceramic frame, and a lid with chamfered edges, where the ratio of distances between specific edges is controlled to reduce stress concentration in the adhesive layer.

Benefits of technology

The design enhances heat dissipation performance and ensures reliable bonding between the frame and lid by minimizing stress concentration in the adhesive layer, preventing cracks and maintaining airtightness under thermal cycles.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007558882000003
    Figure 0007558882000003
  • Figure 0007558882000004
    Figure 0007558882000004
  • Figure 0007558882000005
    Figure 0007558882000005
Patent Text Reader

Abstract

To provide a package that can secure reliability on a joint between a frame body and a lid body, while enhancing heat radiation performance of a heat sink, and an electronic apparatus including the same.SOLUTION: A package 10C has a cavity CV that is sealed with a lid body 80C. The package 10C includes: a heat sink 13 having a linear expansion coefficient of 9 ppm / °C or more and 15 ppm / °C or less at temperatures of 25°C-100°C; and a frame body 14C, provided on the heat sink 13 and made of ceramics, which surrounds the cavity CV in a planar view. In the planar view, an outer edge of the frame body 14C includes a first straight line portion LN1 extending along a first direction, a second straight line portion LN2 extending along a direction orthogonal to the first direction, and a chamfering portion CM1 joining the first straight line portion LN1 to the second straight line portion LN2.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] Books Disclosure The present invention relates to a package and an electronic device, and more particularly to a package having a heat sink and an electronic device including the same. [Background technology]

[0002] Japanese Patent Application Laid-Open No. 2005-150133 (Patent Document 1) discloses a container for housing a semiconductor element. The container for housing a semiconductor element is composed of a base (package) and a lid. The package has a heat sink made of a metal plate, a ceramic frame, and an external connection terminal. A semiconductor element is mounted in a cavity portion formed by the heat sink and the ceramic frame. After the semiconductor element is mounted, the lid is bonded to the ceramic frame using a resin adhesive such as epoxy resin. The lid bonded to the ceramic frame by the resin adhesive covers the upper surface of the cavity portion, thereby airtightly sealing the cavity. The heat sink is made of a composite metal plate of copper (Cu) and another metal. In order to impart high thermal conductivity to the heat sink, the linear expansion coefficient of the heat sink may be set to 8 ppm / °C or more by slightly sacrificing the similarity of the thermal expansion coefficients between the heat sink and the ceramic frame. According to what the above publication claims, even if the heat sink has a high thermal expansion coefficient, the reliability of the bond between the package and the lid can be ensured by making the lid from a resin material.

[0003] Japanese Patent Laid-Open Publication No. 2007-115731 (Patent Document 2) discloses a clad material (composite metal plate) for a heat dissipation substrate (heat sink). The clad material is composed of a total of five or more copper layers and molybdenum layers alternately laminated together. This makes it possible to obtain a high thermal conductivity close to that of pure Cu while suppressing the thermal expansion coefficient to 14 ppm / °C or less. The high thermal conductivity can improve the heat dissipation properties of the heat sink. [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2005-150133 A [Patent Document 2] JP 2007-115731 A Summary of the Invention [Problem to be solved by the invention]

[0005] As described in the above-mentioned Japanese Patent Application Laid-Open No. 2005-150133, the reliability of the bond between the package and the lid can be easily ensured by making the lid contain a resin material. However, according to the study by the present inventors, this reliability of the bond is difficult to ensure if the thermal expansion coefficient of the heat sink is excessively high. If the lid is made of ceramics rather than resin, the rigidity of the lid increases, making it more difficult to ensure the reliability of the bond. This will be explained below. In the following description of this specification, the coefficient of linear expansion (CTE) at temperature T (°C) is expressed as the length L at a temperature of 25°C (room temperature). 25 and the length at temperature T is L T When {(L T -L 25 ) / (T-25)} / L 25 In this specification, the linear expansion coefficient is sometimes referred to as the linear expansion coefficient between 25°C and T (°C). The linear expansion coefficient of the composite metal plate is calculated based on the length along the in-plane direction. Here, the in-plane direction is the direction perpendicular to the lamination direction (thickness direction) of the composite metal plate.

[0006] According to the inventors' study, when the thermal expansion coefficient of the heat sink is 9 ppm / °C or more, cracks are likely to occur in the resin adhesive layer for bonding the frame and the lid together under heat cycles. The inventors actually observed such cracks as a result of heat cycle tests between -65°C and 150°C. When the cracks extend between the cavity and the outside atmosphere, the airtightness of the cavity is lost.

[0007] On the other hand, as disclosed in the above-mentioned JP 2007-115731 A, the thermal expansion coefficient of a material intended to obtain high thermal conductivity is not necessarily limited to less than 9 ppm / ° C. If the thermal expansion coefficient is restricted to less than 9 ppm / ° C., it may not be possible to ensure the required thermal conductivity, and as a result, the heat dissipation performance of the heat sink may become insufficient.

[0008] Books Disclosure This has been made to solve the above-mentioned problems, and its purpose is to provide a package that can ensure the reliability of the joint between the frame body and the lid body while improving the heat dissipation performance of the heat sink, and an electronic device that includes the package. [Means for solving the problem]

[0009] The package in one embodiment has a cavity to be sealed by a lid. The package includes a heat sink having a linear expansion coefficient of 9 ppm / °C or more and 15 ppm / °C or less between 25°C and 100°C, and a frame provided on the heat sink, made of ceramics, and surrounding the cavity in a plan view. In a plan view, an outer edge of the frame has a first straight portion extending along a first direction and a second straight portion perpendicular to the first direction. Second and a chamfered portion connecting the first straight portion and the second straight portion.

[0010] In a plan view, the shortest distance between a virtual intersection point of the first straight line portion and the second straight line portion and an inner edge of the frame body may be defined as distance a, and the shortest distance between the intersection point and the outer edge of the frame body may be defined as distance b, with the ratio of distance b to distance a being 10% or more and 50% or less. The lid body may be made of ceramics.

[0011] The electronic device in one embodiment includes the package, an electronic component housed in the cavity of the package, and the lid that seals the cavity of the package. In a plan view, an edge of the lid includes a third straight portion extending along the first direction and a fourth straight portion extending along the second direction. In a plan view, The shortest distance between a virtual intersection point of the first straight line portion and the second straight line portion and the outer edge of the frame body is defined as a distance b, and The shortest distance between a virtual intersection point of the third straight portion and the fourth straight portion and the edge of the lid body is defined as distance c, and the ratio of distance c to distance b is not less than 0% and not more than 120%.

[0012] In a plan view, the shortest distance between a virtual intersection point of the first straight line portion and the second straight line portion and an inner edge of the frame body is defined as a distance a, The edge of the lid may include a chamfered portion connecting the third straight portion and the fourth straight portion. A ratio of the distance c to the distance a may be 10% or more and 50% or less. Effect of the Invention

[0013] According to one embodiment, at the outer edge of the frame, the corners connecting the first straight portion and the second straight portion are formed by chamfered portions. This reduces stress concentration on the adhesive layer near the corners due to differences in thermal expansion and contraction. Therefore, even if the linear expansion coefficient of the heat sink is 9 ppm / °C or more due to increased heat dissipation, excessive stress concentration in the adhesive layer can be avoided as long as the linear expansion coefficient is 15 ppm / °C or less. Therefore, it is possible to ensure the reliability of the bond between the frame and the lid while increasing the heat dissipation of the heat sink.

[0014] The objects, features, aspects and advantages of the present invention will become more apparent from the following detailed description and the accompanying drawings. [Brief description of the drawings]

[0015] [Figure 1] 1 is a schematic perspective view showing a configuration of an electronic device according to an embodiment, with a portion of the device omitted so that the inside of a cavity can be seen; [Diagram 2] 2 is a schematic cross-sectional view of the electronic device of FIG. 1 taken along line II-II. [Diagram 3] 3 is a schematic cross-sectional view of the electronic device of FIG. 1 taken along line III-III. [Figure 4] 1 is a plan view showing a schematic configuration of a package of an electronic device according to an embodiment of the present invention, with metal terminals not shown; [Diagram 5] 5 is a partial plan view illustrating a schematic configuration of a frame of the package of FIG. 4. [Figure 6] 6 is a partial plan view showing a schematic configuration of a lid to be attached to the frame of FIG. 5. FIG. [Figure 7] 5 is a plan view showing a schematic view of the configuration of a package of a comparative example in the same field of view as FIG. 4, with metal terminals not shown. [Figure 8] 8 is a partial cross-sectional view showing the configuration of an electronic device having the package of FIG. 7, taken from the same perspective as FIG. 3. [Figure 9] FIG. 1 is a graph illustrating the linear expansion coefficient CTEA of a composite metal plate for a heat sink (type A), the linear expansion coefficient CTEB of a composite metal plate for a heat sink (type B), and the linear expansion coefficient CTEC of a ceramic material for a frame. [Figure 10] FIG. 13 is a partial perspective view showing a simulation result of stress distribution in an adhesive layer in an electronic device of a comparative example. [Figure 11] 11 is a partial perspective view illustrating a simulation result of stress distribution in an adhesive layer in an electronic device according to an embodiment; [Figure 12] 13 is a partial perspective view illustrating a simulation result of stress distribution in an adhesive layer in an electronic device according to a modified example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0016] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.

[0017] Fig. 1 is a schematic perspective view showing the configuration of an electronic device 90C in this embodiment, with a portion of the cavity CV omitted so that the inside of the cavity CV can be seen. Fig. 2 and Fig. 3 are schematic cross-sectional views of the electronic device 90C in Fig. 1 taken along lines II-II and III-III, respectively.

[0018] The electronic device 90C includes a package 10C having a cavity CV, an electronic component 8 housed in the cavity CV, a wiring portion 9, a lid 80C, and an adhesive layer 70. The package 10C includes a heat sink 13, a frame 14C, and a metal terminal 15. The electronic component 8 is, for example, a high-frequency power semiconductor element, and in this case, the package 10C is a high-frequency package. The electronic component 8 may be electrically connected to the metal terminal 15 of the package 10C by the wiring portion 9. The lid 80C is joined to the frame 14C by the adhesive layer 70 to seal the cavity CV.

[0019] The cover 80C is made of ceramics, which may contain alumina as a main component, and may be the same as or different from the ceramics of the frame 14C.

[0020] The material of the lid body 80C is not limited to ceramics. For example, the lid body 80C may contain a resin material. The resin material is, for example, a liquid crystal polymer. The resin material may have an inorganic filler dispersed therein, and the inorganic filler is, for example, silica particles. By dispersing the inorganic filler in the resin material, the strength and durability of the lid body 80C can be increased.

[0021] The adhesive layer 70 has a portion disposed between the frame 14C and the lid 80C, thereby bonding them together. The adhesive layer 70 is made of a thermosetting adhesive in a cured state. This thermosetting adhesive may contain at least one of an epoxy resin, a phenolic resin, and a silicone resin as a main component. In particular, epoxy resin is preferable because it has a good balance of heat resistance, mechanical strength, and chemical resistance. In order for the thermosetting adhesive in a cured state to preferably have the above-mentioned characteristics, the content of the epoxy resin as the main component is preferably 20 to 40 wt% (weight %), and the remainder may be made of a secondary component such as a curing agent. Specifically, the secondary component may be, for example, 1 to 10 wt% of a curing agent, 50 to 70 wt% of an inorganic filler, 0.5 to 2 wt% of a coupling agent, 0.5 to 2 wt% of a catalyst, and 0.1 to 5 wt% of a low-stress agent. A phenoxy resin compound may be used as the curing agent. Silica may be used as the inorganic filler. Organic phosphorus or boron salt may be used as the catalyst. Silicone may be used as the low stress agent. The thickness of the adhesive layer 70 between the lid 80C and the package 10C is, for example, 100 μm or more and 360 μm or less. The adhesive layer 70 may have a bending modulus smaller than that of the lid 80C.

[0022] In the package 10C, the heat sink 13, the frame 14C, and the metal terminals 15 may be bonded to one another using a bonding material (not shown). The bonding material is, for example, silver solder. To enable bonding between ceramic and metal by silver solder, a metal layer made of tungsten, molybdenum, or the like may be provided on the surface of the frame 14C that is bonded to the heat sink 13 and the metal terminals 15. After bonding by the bonding material, the package 10C is typically subjected to a plating process.

[0023] The heat sink 13 is made of metal. The electronic component 8 is mounted on the mounting surface of the heat sink 13 facing the cover body 80C. The heat sink 13 has a linear expansion coefficient of 9 ppm / °C or more and 15 ppm / °C or less between 25°C and 100°C. By allowing the linear expansion coefficient to be 9 ppm / °C or more, it is easy to impart high thermal conductivity to the heat sink 13, and for example, a high thermal conductivity of about 330 (W / m·K) or more and 360 (W / m·K) or less can be imparted. The thermal conductivity value here may be a value at 25°C. On the other hand, by allowing the linear expansion coefficient of the heat sink 13 to be 15 ppm / °C or less, excessive expansion / contraction difference between the heat sink 13 and the frame body 14C is avoided. The heat sink 13 may be a composite metal plate, for example, a composite metal plate (clad material) in which a plurality of Cu plates and a plurality of Mo (molybdenum) plates are alternately laminated. This laminated structure is, for example, a five-layer structure of Cu / Mo / Cu / Mo / Cu.

[0024] Ceramic particles may be dispersed in the metal that constitutes the heat sink 13. The ceramic particles are made of, for example, SiC (silicon carbide) or diamond.

[0025] The frame body 14C is provided on the heat sink 13 and surrounds the cavity CV in a plan view. The frame body 14C is made of ceramics. The ceramics contain, for example, alumina as a main component. The flexural modulus of the frame body 14C is usually greater than the flexural modulus of the adhesive layer 70. The metal terminal 15 is bonded onto the frame body 14C. The metal terminal 15 constitutes an electrical path connecting the inside and outside of the cavity CV sealed by the package 10C and the lid body 80C. Inside the cavity CV, the electronic component 8 is electrically connected to the metal terminal 15 by a wiring portion 9. The wiring portion 9 is, for example, a bonding wire. The adhesive layer 70 is provided on the package 10C so as to surround the cavity. Referring to FIG. 1, the adhesive layer 70 may have a portion on the metal terminal 15 and a portion on the frame body 14C.

[0026] The outer surface (the lower surface in Figs. 1 to 3) of the heat sink 13 of the electronic device 90C is to be attached to a support member (not shown). The support member is, for example, a mounting board or a heat dissipation member. The heat sink 13 may have a through-hole (not shown) through which a fastener (for example, a screw) for attachment to the support member passes.

[0027] 2, the cover 80C has an inner surface 81i facing the cavity and an outer surface 81o opposite thereto. Typically, a frame portion 81p, which is a protrusion having a frame shape roughly corresponding to the frame shape of the frame 14C, is provided on the inner surface 81i. In this case, the adhesive layer 70 contacts the frame portion 81p.

[0028] Fig. 4 is a plan view that diagrammatically illustrates the configuration of package 10C while omitting illustration of metal terminals 15 (Figs. 1 and 2). Fig. 5 is a partial plan view that diagrammatically illustrates the configuration of frame body 14C of package 10C (Fig. 4).

[0029] In a plan view, the outer edge of frame body 14C includes a straight line portion LN1 (first straight line portion) extending along the horizontal direction (first direction) of FIG. 5, a straight line portion LN2 (second straight line portion) extending along the vertical direction (direction perpendicular to the first direction) of FIG. 5, and a chamfered portion CM1 connecting straight line portion LN1 and straight line portion LN2.

[0030] In a plan view, the shortest distance between a virtual intersection point PT1 (FIG. 5) between the straight line portions LN1 and LN2 and the inner edge of the frame body 14C is defined as distance a, and the shortest distance between the intersection point PT1 and the outer edge of the frame body 14C is defined as distance b. The ratio of distance b to distance a is preferably 10% or more and 50% or less.

[0031] In addition, Fig. to 5 In the embodiment, the chamfered portion CM1 forms the same angle (45 degrees) with respect to each of the straight portion LN1 and the straight portion LN2 in a plan view. However, the angle of the chamfered portion CM1 is not limited to 45 degrees. to 5In this embodiment, a chamfered portion CM1 that is linear in plan view is shown (see also FIG. 11), but a chamfered portion that is curved (typically arc-shaped) in plan view may be used instead (see also FIG. 12).

[0032] Fig. 6 is a partial plan view showing a schematic configuration of a lid body 80C to be attached to a frame body 14C (Fig. 5) using an adhesive layer 70 (Figs. 1 to 3). The horizontal direction in Fig. 6 corresponds to the horizontal direction in Fig. 5, and the vertical direction in Fig. 6 corresponds to the vertical direction in Fig. 5.

[0033] In plan view, the edge of the lid body 80C includes a straight line portion LN3 (third straight line portion) extending along the horizontal direction (first direction) of FIG. 6 and a straight line portion LN4 (fourth straight line portion) extending along the vertical direction (second direction) of FIG. 6. In plan view, the shortest distance between a virtual intersection point PT2 of the straight line portion LN3 and the straight line portion LN4 and the edge of the lid body 80C is defined as a distance c. The ratio of the distance c (FIG. 6) to the distance b (FIG. 5) is 0% or more and 120% or less. When the ratio is 0%, the intersection point PT2 is the apex of the edge of the lid body 80C. In plan view, the straight line portion LN1 (FIG. 5) and the straight line portion LN3 (FIG. 6) may be substantially on a common straight line. In plan view, the straight line portion LN2 (FIG. 5) and the straight line portion LN4 (FIG. 6) may be substantially on a common straight line. Furthermore, in plan view, the intersection point PT1 (FIG. 5) and the intersection point PT2 (FIG. 6) may substantially overlap each other.

[0034] The edge of the cover 80C may include a chamfered portion CM2 connecting the straight portion LN3 and the straight portion LN4. The ratio of the distance c to the distance a (FIG. 5) may be 10% or more and 50% or less. In a plan view, the chamfered portion CM2 (FIG. 6) may substantially overlap the chamfered portion CM1 (FIG. 5), in which case the chamfered portion CM2 and the chamfered portion CM1 have a common shape.

[0035] Next, a method for manufacturing the electronic device 90C will be described below.

[0036] A package 10C is prepared. An electronic component 8 is mounted on a heat sink 13 of the package 10C. For example, the electronic component 8 is soldered onto the heat sink 13. Next, the electronic component 8 is electrically connected to a metal terminal 15 by a wiring portion 9.

[0037] Next, the lid body 80C is placed on the package 10C. Specifically, the lid body 80C is attached to the frame body 14C of the package 10C via the adhesive layer 70 in a semi-cured state. Next, the lid body 80C is pressed against the package 10C with a predetermined load. An appropriate load depends on the dimensional design of the package 10C, but is, for example, about 500 g or more and 1 kg or less. While being pressed with the load, the adhesive layer 70 is heated. The heated adhesive layer 70 first changes to a softened state. This reduces the viscosity of the adhesive layer 70. As a result, the adhesive layer 70 wets and spreads. At this time, due to the chamfered portion CM1 (FIG. 1), the adhesive layer 70 becomes easy to flow so as to cover the side surface of the frame body 14C, as shown by the arrow FL (FIG. 3). Then, as the curing reaction due to heating progresses, the adhesive layer 70 changes to a cured state. As a result, the lid body 80C is bonded to the package 10C. This seals the cavity CV.

[0038] Through the above steps, the electronic device 90C is obtained.

[0039] Fig. 7 is a plan view showing the structure of a package 10S of a comparative example in a view similar to that of Fig. 4, with metal terminals omitted. Fig. 8 is a partial cross-sectional view showing the structure of an electronic device 90S having the package 10S (Fig. 7) in a view similar to that of Fig. 3. The package 10S includes a frame body 14S that does not have a chamfered portion CM1 (Fig. 5). Under a heat cycle, as shown in Fig. 8, the heat sink 13 undergoes expansion / contraction EX1, the frame body 14S undergoes expansion / contraction EX2, and the lid body 80S undergoes expansion / contraction EX3.

[0040] Figure 9 shows the linear expansion coefficient (CTE) of the composite metal plate (type A) for the heat sink. A and the coefficient of linear expansion (CTE) of the composite metal plate (type B) for the heat sinkB and the coefficient of linear expansion (CTE) of typical ceramic materials for the frame C The linear expansion coefficient of the metal material was measured in accordance with JIS Z 2285, and the linear expansion coefficient of the ceramic material was measured in accordance with JIS R 1618. The material design of the composite metal plate differs between types A and B. When a high thermal conductivity of 330 (W / m K) or more and 360 (W / m K) or less is intended, the linear expansion coefficient of the composite metal plate varies depending on the material design. A and the coefficient of linear expansion (CTE) B However, even if such adjustment is made, the linear expansion coefficient of the composite metal plate is still greater than the linear expansion coefficient (CTE) of a typical ceramic material for the frame in the temperature range of the heat cycle (-65°C to +150°C in a typical test). C Much larger than.

[0041] Due to the difference in the linear expansion coefficients, as shown in Fig. 8, the expansion / contraction EX1 is much larger than the expansion / contraction EX2. Furthermore, when the cover body 80S is made of ceramic, the expansion / contraction EX1 is larger than the expansion / contraction EX3. Due to these differences in expansion / contraction, stress is applied to the electronic device 90S. The stress tends to concentrate near the corner CN (Fig. 7) of the frame body 14S in a plan view, and as a result, cracks CR (Fig. 8) are likely to occur in the adhesive layer 70.

[0042] Also, unlike the frame body 14C (FIG. 3), the frame body 14S does not have a chamfered portion CM1 (FIG. 5). Therefore, the frame body 14S extends further outward (to the right in FIG. 8) as shown in FIG. 8. As a result, the adhesive layer 70 is likely to have an end ED on the upper surface of the frame body 14S (the surface facing the lid body 80S). The above-mentioned stress is particularly likely to concentrate near the end ED, which may cause cracks CR.

[0043] In contrast, according to the present embodiment, the chamfered portion CM1 (FIG. 1) is provided, so that the adhesive layer 70 is more likely to flow out so as to cover the side surface of the frame body 14C as described above (see arrow FL in FIG. 3). This makes it difficult to form a structure like the end ED (FIG. 8: comparative example). This makes it possible to suppress the occurrence of cracks CR (FIG. 8) starting from the end ED.

[0044] This effect achieved by providing the chamfered portion CM1 on the frame 14C does not depend on the material of the lid, and this effect is achieved even when the lid contains a resin material.

[0045] According to this embodiment, the corner connecting the linear portion LN1 and the linear portion LN2 at the outer edge of the frame body 14C (FIG. 5) is formed by a chamfered portion CM1. As a result, the range DC (FIG. 4) where the difference in thermal expansion and contraction occurs, which causes stress concentration at the corner portion CN (see FIGS. 1 and 3), is smaller than the range DS (FIG. 7) in the comparative example. As a result, the stress concentration applied to the adhesive layer 70 near the corner portion CN due to the difference in thermal expansion and contraction is reduced. Therefore, even if the linear expansion coefficient of the heat sink 13 is 9 ppm / °C or more due to the improvement of the heat dissipation, if the linear expansion coefficient is 15 ppm / °C or less, excessive stress concentration in the adhesive layer 70 can be avoided. Therefore, the bonding reliability between the frame body 14C and the lid body 80C, specifically, the bonding reliability of the adhesive layer 70 can be ensured while improving the heat dissipation of the heat sink 13.

[0046] 4 and 7, when the package configuration has point symmetry with respect to the center position CT in plan view, the stress is concentrated at the corner CN, regardless of the material of the lid. Therefore, the above effect of providing the chamfered portion CM1 on the frame 14C occurs even when the lid contains a resin material.

[0047] Figure 5 and Figure 6Referring to FIG. 8, when the ratio of distance c to distance b is 0% or more and 120% or less, it is easy to prevent the adhesive layer 70 from having an end ED (FIG. 8) on the upper surface of the frame 14C at the corner CN. This makes it possible to prevent stress concentration at the end ED of the adhesive layer 70. Therefore, it is possible to more reliably ensure the bonding reliability of the adhesive layer 70 under heat cycles.

[0048] The edge of the lid body 80C may include a chamfered portion CM2 (FIG. 6). This allows the edge of the corner of the lid body 80C to be roughly aligned with the outer edge of the frame body 14C having the chamfered portion CM1 (FIG. 5) in a plan view. This makes it easier to appropriately position the adhesive layer 70 between the frame body 14C and the lid body 80C at the corner CN (FIG. 1).

[0049] 5, the following table shows the results of examining the relationship between the loss rate (%), which is the ratio of distance b to distance a, the occurrence of cracks in adhesive layer 70, and the strength of frame 14C.

[0050] [Table 1]

[0051] In the above table, in the row of "Crack", "A" indicates that there is a low concern about cracking of the adhesive layer 70, "C" indicates that there is a high concern, and "B" indicates that there is an intermediate concern. In order to reduce the concern about cracking of the adhesive layer 70, the defect rate is preferably 10% or more, and more preferably 20% or more.

[0052] In addition, in the row of "frame strength", "A" indicates that there is little concern about the strength of the frame body 14C, "C" indicates that the concern is high, and "B" indicates that the concern is somewhere in between. In order to reduce concerns about the strength of the frame body 14C, the defect rate is preferably 50% or less, and 40% or less. under It is more preferable that the frame 14C has a strength of 100%.

[0053] 10 to 12 are partial perspective views illustrating simulation results of stress distribution in the adhesive layer 70 in an electronic device 90S of a comparative example (see FIGS. 7 and 8), an electronic device 90C corresponding to the embodiment (see FIGS. 1 to 6), and an electronic device 90R of a modified example. The electronic device 90R of the modified example has a frame 14R and a cover 80R, each of which is chamfered in an arc shape. In each of these perspective views, shading is applied to make it easy to distinguish between the members and to see the shapes of each member, and further, shading according to the stress is superimposed on the adhesive layer 70. This superimposition is made darker (blacker) as the stress increases, and lighter (whiter) as the stress decreases.

[0054] In the electronic device 90S (FIG. 10) of the comparative example, a portion corresponding to the end portion ED (see FIG. 8) is generated, and a significant stress concentration SS (FIG. 10) is observed directly above the portion. The stress concentration SC in the electronic device 90C (FIG. 11) corresponding to the embodiment is widely distributed in a line in the horizontal direction in the figure, and is milder than the stress concentration SS (FIG. 10). The stress concentration SR in the electronic device 90R (FIG. 12) of the modified example is also widely distributed in a line in the horizontal direction in the figure, and is milder than the stress concentration SS (FIG. 10). If the stress value of the stress concentration SS (FIG. 10) is defined as 100%, the stress value of the stress concentration SC (FIG. 11) is 68.7%, and the stress value of the stress concentration SR (FIG. 12) is 68.1%.

[0055] The conditions for the above simulation are shown below. The linear expansion coefficients in Table 2 below are those between 25°C and 100°C. The lid and frame in Table 2 are both made of ceramics whose main component is alumina, but their sub-components are slightly different. The heat sink in Table 2 is made of metal only.

[0056] [Table 2] [Explanation of symbols]

[0057] 8: Electronic components 10C:Package 13: Heat sink 14C: Frame 70: Adhesive layer 80C: Lid body 90C:Electronic equipment CM1: Chamfered part CM2: Chamfered part CV: Cavity

Claims

1. A package having a cavity, the package comprising: A heat sink having a linear expansion coefficient of 9 ppm / °C or more and 15 ppm / °C or less between 25°C and 100°C; a frame provided on the heat sink, made of ceramics, and surrounding the cavity in a plan view; Equipped with In a plan view, an outer edge of the frame body includes a first straight line portion extending along a first direction, a second straight line portion extending along a second direction perpendicular to the first direction, and a chamfered portion connecting the first straight line portion and the second straight line portion, an electronic component housed within the cavity of the package; a lid for sealing the cavity of the package; an adhesive layer that bonds the lid to the frame of the package; Further equipped with The adhesive layer is made of a thermosetting adhesive material and has a portion covering a side surface of the frame at the chamfered portion of the outer edge of the frame, and is spaced from the heat sink.

2. 2. The electronic device of claim 1, In a plan view, the shortest distance between a virtual intersection point between the first straight line portion and the second straight line portion and an inner edge of the frame body is defined as a distance a, and the shortest distance between the intersection point and the outer edge of the frame body is defined as a distance b, An electronic device, wherein a ratio of distance b to distance a is 10% or more and 50% or less.

3. 3. An electronic device according to claim 1, The electronic device, wherein the lid is made of ceramics.

4. 4. An electronic device according to claim 1, In a plan view, an edge of the cover includes a third linear portion extending along the first direction and a fourth linear portion extending along the second direction, In a plan view, the shortest distance between a virtual intersection point between the first straight line portion and the second straight line portion and the outer edge of the frame body is defined as a distance b, and the shortest distance between a virtual intersection point between the third straight line portion and the fourth straight line portion and the edge of the lid body is defined as a distance c, An electronic device, wherein a ratio of distance c to distance b is equal to or greater than 0% and equal to or less than 120%.

5. 5. The electronic device of claim 4, the edge of the cover includes a chamfered portion connecting the third straight portion and the fourth straight portion.

6. 6. The electronic device of claim 5, In a plan view, the shortest distance between a virtual intersection point of the first straight line portion and the second straight line portion and an inner edge of the frame body is defined as a distance a, An electronic device, wherein a ratio of distance c to distance a is 10% or more and 50% or less.

Citation Information

Patent Citations

  • Container for housing semiconductor element

    JP2005150133A

  • Manufacturing method and forming method of cladding material and radiation substrate using the same

    JP2007115731A

  • Solid-state imaging device

    JP2009016649A

  • Package for housing electronic component

    JP2010219441A

  • Package for housing semiconductor element, and semiconductor device

    WO2013161660A1