NDIR Gas Sensors and Optical Devices
By optimizing the combination of an optical filter and infrared receiving/emitting element with specific materials and layer configurations, the NDIR gas sensor achieves high accuracy and cost-effectiveness with a simplified design.
Patent Information
- Application Number
- JP2023146329
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-09-08
- Publication Date
- 2024-10-01
- Estimated Expiration
- 2039-12-05
AI Technical Summary
The optimal combination of an infrared light source, infrared receiving/emitting element, and optical filter has not been studied for each gas to be detected, particularly with specifications of optical filters not being optimized, leading to inaccuracies in NDIR gas sensors.
The NDIR gas sensor employs an optical filter with a multilayer film having layers with different refractive indexes, using materials like TiO2, ZnS, Si, and Ge, and an infrared receiving/emitting element with a specific active layer of InAs y Sb 1-y, optimized for wavelength ranges to enhance accuracy and simplify the filter design.
This configuration allows for a highly accurate NDIR gas sensor with a simplified optical filter, improving mass productivity, reducing defects, and maintaining gas detection accuracy while lowering costs.
Smart Images

Figure 0007559170000003 
Figure 0007559170000004 
Figure 0007559170000005
Abstract
Description
[Technical field]
[0001] The present invention relates to an NDIR gas sensor, an optical device, and an optical filter for an NDIR gas sensor. [Background technology]
[0002] Conventionally, a non-dispersive infrared (NDIR) gas concentration measuring device is known as a gas concentration measuring device for measuring the concentration of a gas to be measured in the atmosphere. The non-dispersive infrared absorption type gas concentration measuring device measures the gas concentration by detecting the amount of absorption, utilizing the fact that the wavelength of infrared light absorbed by the type of gas differs. As an example of a gas concentration measuring device using this principle, there is a device that combines a filter (transparent member) that transmits infrared light limited to the wavelength that the gas to be measured has absorption characteristics with an infrared receiving element, and measures the concentration of the gas by measuring the amount of infrared light absorbed by the gas to be measured. A carbon dioxide gas concentration measuring device that applies this principle is disclosed in Patent Document 1. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Japanese Patent Application Publication No. 9-33431 Summary of the Invention [Problem to be solved by the invention]
[0004] However, the optimal combination of infrared light source, infrared light receiving / emitting element, and optical filter for each target gas has not been considered yet. In particular, the specifications of the optical filters have not been optimized. An object of the present invention is to provide an NDIR gas sensor, an optical device, and an optical filter for an NDIR gas sensor that are highly accurate even when a simplified optical filter is used. [Means for solving the problem]
[0005] The gist of the present invention is as follows.
[0006] In one embodiment, the NDIR gas sensor of the present invention comprises: an optical filter including a substrate and a multilayer film having a plurality of layers with different refractive indices formed on at least one surface of the substrate; an infrared emitting / receiving element having a first conductive type semiconductor layer, an active layer, and a second conductive type semiconductor layer; Equipped with the multilayer film includes a structure in which a first layer having a refractive index of 1.2 or more and 2.5 or less in a wavelength range of 6 μm to 10 μm and a second layer having a refractive index of 3.2 or more and 4.3 or less in a wavelength range of 6 μm to 10 μm are alternately laminated; The active layer is InAs y Sb 1-y (0.1≦y≦0.2), The optical filter includes a wavelength range of 6 μm to 10 μm in which the average transmittance is 70% or more over a width of 50 nm or more, has a maximum transmittance of 10% or more in the wavelength range of 12.5 μm to 20 μm, and has an average transmittance of 5% or more and 60% or less in the wavelength range of 12.5 μm to 20 μm.
[0007] In another aspect, the NDIR gas sensor of the present invention comprises: an optical filter including a substrate and a multilayer film having a plurality of layers with different refractive indices formed on at least one surface of the substrate; an infrared emitting / receiving element having a first conductive type semiconductor layer, an active layer, and a second conductive type semiconductor layer; Equipped with The multilayer film includes a structure in which a first layer including at least one selected from the group consisting of TiO2 and ZnS and a second layer including at least one selected from the group consisting of Si and Ge are alternately laminated, The active layer is InAs y Sb 1-y (0.1≦y≦0.2), The optical filter includes a wavelength range of 6 μm to 10 μm in which the average transmittance is 70% or more over a width of 50 nm or more, has a maximum transmittance of 10% or more in the wavelength range of 12.5 μm to 20 μm, and has an average transmittance of 5% or more and 60% or less in the wavelength range of 12.5 μm to 20 μm.
[0008] In one embodiment, the optical device of the present invention comprises: an optical filter including a substrate and a multilayer film having a plurality of layers with different refractive indices formed on at least one surface of the substrate; an infrared emitting / receiving element having a first conductive type semiconductor layer, an active layer, and a second conductive type semiconductor layer; Equipped with the multilayer film includes a structure in which a first layer having a refractive index of 1.2 or more and 2.5 or less in a wavelength range of 6 μm to 10 μm and a second layer having a refractive index of 3.2 or more and 4.3 or less in a wavelength range of 6 μm to 10 μm are alternately laminated; The active layer is InAs y Sb 1-y (0.1≦y≦0.2), The optical filter includes a wavelength range of 6 μm to 10 μm in which the average transmittance is 70% or more over a width of 50 nm or more, has a maximum transmittance of 10% or more in the wavelength range of 12.5 μm to 20 μm, and has an average transmittance of 5% or more and 60% or less in the wavelength range of 12.5 μm to 20 μm.
[0009] In another aspect, the optical device of the present invention comprises: an optical filter including a substrate and a multilayer film having a plurality of layers with different refractive indices formed on at least one surface of the substrate; an infrared emitting / receiving element having a first conductive type semiconductor layer, an active layer, and a second conductive type semiconductor layer; Equipped with The multilayer film includes a structure in which a first layer including at least one selected from the group consisting of TiO2 and ZnS and a second layer including at least one selected from the group consisting of Si and Ge are alternately laminated, The active layer is InAs y Sb 1-y(0.1≦y≦0.2), The optical filter includes a wavelength range of 6 μm to 10 μm in which the average transmittance is 70% or more over a width of 50 nm or more, has a maximum transmittance of 10% or more in the wavelength range of 12.5 μm to 20 μm, and has an average transmittance of 5% or more and 60% or less in the wavelength range of 12.5 μm to 20 μm.
[0010] In one embodiment, the optical filter for an NDIR gas sensor of the present invention comprises: An optical filter for an NDIR gas sensor, comprising: a substrate; and a multilayer film having a plurality of layers with different refractive indices formed on at least one surface of the substrate, the multilayer film includes a structure in which a first layer having a refractive index of 1.2 or more and 2.5 or less in a wavelength range of 6 μm to 10 μm and a second layer having a refractive index of 3.2 or more and 4.3 or less in a wavelength range of 6 μm to 10 μm are alternately laminated; The optical filter includes a wavelength range of 6 μm to 10 μm in which the average transmittance is 70% or more over a width of 50 nm or more, has a maximum transmittance of 10% or more in the wavelength range of 12.5 μm to 20 μm, and has an average transmittance of 5% or more and 60% or less in the wavelength range of 12.5 μm to 20 μm.
[0011] In another aspect, the optical filter for an NDIR gas sensor of the present invention comprises: An optical filter for an NDIR gas sensor, comprising: a substrate; and a multilayer film having a plurality of layers with different refractive indices formed on at least one surface of the substrate, The multilayer film includes a structure in which a first layer including at least one selected from the group consisting of TiO2 and ZnS and a second layer including at least one selected from the group consisting of Si and Ge are alternately laminated, The optical filter includes a wavelength range of 6 μm to 10 μm in which the average transmittance is 70% or more over a width of 50 nm or more, has a maximum transmittance of 10% or more in the wavelength range of 12.5 μm to 20 μm, and has an average transmittance of 5% or more and 60% or less in the wavelength range of 12.5 μm to 20 μm.
[0012] The above summary of the invention does not list all of the necessary features of the present invention. Also, subcombinations of these features may also be inventions. Effect of the Invention
[0013] According to the present invention, it is possible to provide a highly accurate NDIR gas sensor, an optical device, and an optical filter for an NDIR gas sensor even when a simplified optical filter is used. [Brief description of the drawings]
[0014] [Figure 1] FIG. 2 is a diagram showing an example of a cross section of an optical filter in the present embodiment. [Diagram 2] FIG. 1 is a diagram illustrating an example of an NDIR gas sensor in an embodiment. [Diagram 3] 1A and 1B are diagrams for explaining an optical filter according to the present invention in comparison with an optical filter according to a comparative example; [Figure 4] 1 is a diagram showing the difference between an optical filter according to a comparative example and an optical filter according to the present invention. [Diagram 5] 1 is a diagram showing a laminated structure of each layer of an infrared emitting / receiving element according to Examples 1 to 3. FIG. [Figure 6] FIG. 2 is a diagram showing the optical spectrum of the infrared receiving elements according to Examples 1 to 3. [Figure 7] 1 is a diagram showing the transmission spectrum of the optical filters (simplified filters) according to Examples 1 to 3 in comparison with the transmission spectrum of an optical filter (filter having a conventional configuration) according to a comparative example. [Figure 8] 1 is a diagram showing a laminated structure of a simplified filter according to Examples 1 to 3. FIG. [Figure 9] FIG. 2 is a diagram showing the optical spectrum of an IR sensor for alcohol detection configured by combining an infrared receiving element and an optical filter (simplified filter) in Example 1. [Figure 10] FIG. 11 is a diagram showing the optical spectrum of an IR sensor for alcohol detection configured by combining an infrared receiving element and an optical filter (simplified filter) in Example 2. [Figure 11] FIG. 11 is a diagram showing the optical spectrum of an IR sensor for alcohol detection configured by combining an infrared receiving element and an optical filter (simplified filter) in Example 3. [Figure 12] 1 shows wavelength dispersion data of the refractive index of a dielectric material used in an optical filter. [Figure 13] FIG. 2 is a diagram showing the cutoff wavelength of the light receiving and emitting component. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] Hereinafter, the present invention will be described through embodiments of the present invention (hereinafter, referred to as "present embodiments"); however, the invention according to the claims is not limited to the following embodiments. Furthermore, not all of the combinations of features described in the embodiments are necessarily essential to the solutions of the invention.
[0016] In the following, the present embodiment will be described with reference to the drawings. However, in the drawings described below, the same reference numerals are used to designate corresponding parts, and the description of overlapping parts will be omitted as appropriate. Furthermore, this embodiment is merely an example of a configuration for embodying the technical idea of the present invention, and the material, shape, structure, arrangement, dimensions, etc. of each part are not specified as described below. Moreover, this embodiment includes all combinations of the characteristic configurations described below. The technical idea of the present invention can be modified in various ways within the technical scope defined by the claims.
[0017] [NDIR gas sensor] In one aspect, the NDIR gas sensor according to the present embodiment includes an optical filter having a substrate and a multilayer film having a plurality of layers with different refractive indexes formed on at least one surface of the substrate, and an infrared ray receiving and emitting element having a first conductive type semiconductor layer, an active layer, and a second conductive type semiconductor layer, the multilayer film includes a structure in which a first layer having a refractive index of 1.2 or more and 2.5 or less in a wavelength range of 6 μm to 10 μm and a second layer having a refractive index of 3.2 or more and 4.3 or less in a wavelength range of 6 μm to 10 μm are alternately laminated, and the active layer is InAs y Sb 1-y (0.1≦y≦0.2), and the optical filter includes a wavelength range of 50 nm to 800 nm in which the average transmittance is 70% or more and 95% or less within the wavelength range of 6 μm to 10 μm, and the maximum transmittance in the wavelength range of 12.5 μm to 20 μm is 10% or more.
[0018] In another aspect, the NDIR gas sensor according to the present embodiment includes an optical filter having a substrate and a multilayer film having a plurality of layers with different refractive indexes formed on at least one surface of the substrate, and an infrared ray receiving and emitting element having a first conductive type semiconductor layer, an active layer, and a second conductive type semiconductor layer, the multilayer film having a structure in which a first layer including at least one selected from the group consisting of TiO2 and ZnS and a second layer including at least one selected from the group consisting of Si and Ge are alternately stacked, and the active layer is InAs. y Sb 1-y (0.1≦y≦0.2), and the optical filter includes a wavelength range of 50 nm to 800 nm in which the average transmittance is 70% or more and 95% or less within the wavelength range of 6 μm to 10 μm, and the maximum transmittance in the wavelength range of 12.5 μm to 20 μm is 10% or more.
[0019] FIG. 1 shows an example of a cross section of an optical filter according to this embodiment. As shown in Fig. 1, the optical filter of this example has a multilayer film formed by alternately laminating a layer made of a low refractive index material (L) having a refractive index of 1.2 to 2.5 in the wavelength range of 6 μm to 10 μm and a layer made of a high refractive index material (H) having a refractive index of 3.2 to 4.3 in the wavelength range of 6 μm to 10 μm on both sides of a Si substrate such that the layer directly provided on the Si substrate is the high refractive index material (H). The optical filter of this embodiment is not limited to the configuration of Fig. 1, and the multilayer film may be formed only on one side of the substrate, or on both sides of the substrate. In addition, in the optical filter of this embodiment, the multilayer film is not particularly limited as long as it is formed by alternately laminating a first layer having a refractive index of 1.2 to 2.5 and a second layer having a refractive index of 3.2 to 4.3. However, in order to enhance the effect of the present invention, it is preferable that the high refractive index material (H) is provided directly on the substrate, as in the example shown in FIG. 1.
[0020] In this embodiment, the optical filter is a mid-infrared interference bandpass filter. In general, a mid-infrared interference bandpass filter has a large number of layers, and defects during film formation are likely to increase. In addition, if the optical filter has a large number of layers, it is difficult to miniaturize the NDIR gas sensor. Therefore, it is preferable that the optical filter has a small number of layers. However, simply reducing the number of layers of the optical filter to simplify it may degrade the accuracy of the gas sensor.
[0021] Furthermore, to realize a highly accurate NDIR gas sensor, it is necessary to reduce the influence of infrared absorption by gases other than the target gas.
[0022] The inventors have investigated the optimal combination of infrared emitting / receiving elements and optical filters, and as a result, have realized an NDIR gas sensor whose accuracy does not deteriorate even when a simplified optical filter is used, as described below.
[0023] Here, the simplified optical filter is an optical filter in which the number of laminations of optical thin films required for blocking the sensor-insensitive region is reduced by limiting the blocking function of the sensor-insensitive region. By using a simplified optical filter with a small number of laminations, mass productivity can be improved. Furthermore, by reducing the number of laminations, defects during film formation can be reduced, and as a result, the yield can be improved. Furthermore, by reducing warping caused by multiple laminations, chipping caused by dicing can be suppressed, and mass production stability can be improved. The sensor-insensitive region is determined as follows. Although details will be described later, the cutoff wavelength on the long wavelength side of the infrared emitting / receiving element is determined by the band gap energy Eg (see FIG. 13). The band gap energy Eg can be set in the range of 10 μm to 12.5 μm, for example. In this embodiment, the band gap energy Eg corresponds to 12.5 μm, and the element does not have sensitivity in the wavelength range of, for example, 12.5 μm to 20 μm. Hereinafter, in this embodiment, the sensor-insensitive region is described as being in the wavelength range of 12.5 μm to 20 μm.
[0024] In the NDIR gas sensor according to this embodiment, the active layer of the infrared light emitting / receiving element is InAs. y Sb 1-y (0.1≦y≦0.2), and the wavelength range of the optical filter from 6 μm to 10 μm includes a wavelength range of 50 nm to 800 nm in which the average transmittance is 70% or more and 95% or less, and even if the maximum transmittance in the wavelength band of 12.5 μm to 20 μm is 10% or more, it is possible to use an inexpensive optical filter that can be easily manufactured while maintaining gas detection accuracy.
[0025] An example of the gas to be detected is a gas species such as alcohol that has an absorption characteristic for infrared rays in the wavelength band of 9 μm to 10 μm, but is not limited to this.
[0026] FIG. 2 is a diagram showing an example of an NDIR gas sensor according to the present embodiment. In the NDIR gas sensor according to this embodiment, as shown in FIG. 2, an infrared receiving element is placed in the optical path of the infrared light output from the infrared emitting element, and an optical filter that selectively transmits the absorption wavelength of the gas to be detected is placed in front of the infrared receiving element.
[0027] FIG. 3 is a diagram for explaining a comparison between an optical filter according to the present invention and an optical filter according to a comparative example. In the sensor (infrared receiving element) in the technology of the comparative example in Fig. 3, there is no wavelength selectivity in the spectral sensitivity (sensitivity change due to wavelength). On the other hand, in the present invention, there is wavelength selectivity as shown in Fig. 3. Therefore, in the present invention, there is no need to cut off wavelengths for which there is no sensitivity with an optical filter, and the function required of the optical filter can be simplified. Although not shown in the figure, in the case of an infrared light emitting element having wavelength selectivity in the emission intensity, there is also no need to cut off wavelengths for which no light is emitted with an optical filter, and the function required of the optical filter can be simplified. FIG. 4 is a diagram showing the difference between an optical filter according to a comparative example and an optical filter according to the present invention. As shown in Fig. 4, in the NDIR gas sensor of this embodiment, the thickness of the multilayer laminate called the cut surface, which determines the cut characteristics, can be significantly reduced. For example, when the multilayer film is formed on both sides of the substrate, the ratio of the total thickness of each surface can be included in the range of 0.5 to 2.0. In other words, the thickness of the cut surface, which is usually more than twice that of the bandpass surface, can be reduced to 0.5 to 2.0 times that of the bandpass surface.
[0028] Hereinafter, each component of the NDIR gas sensor according to one embodiment of the present invention will be described.
[0029] -Optical filters- The optical filter includes a substrate and a multilayer film formed on the substrate, the multilayer film having a plurality of layers with different refractive indices. The multilayer film may be formed on only one surface of the substrate, or on both surfaces. The optical filter is disposed at a position within the NDIR gas sensor along the optical path from the infrared emitting element to the infrared receiving element. The optical filter may be integrally formed with the infrared emitting element or may be integrally formed with the infrared receiving element. The optical filter may be disposed at a predetermined position within the optical path. A configuration including a plurality of optical filters may also be used. The optical filter can be produced by forming a first layer and a second layer on a substrate by a vapor deposition method.
[0030] --substrate-- Since the multilayer film is formed on one surface of the substrate, the substrate may be any suitable substrate for forming each layer of the multilayer film, such as, but not limited to, a Si substrate, a Ge substrate, a ZnS substrate, or a sapphire substrate.
[0031] --Multilayer film-- A multilayer film is a film having multiple layers with different refractive indices, and specifically includes a structure in which a first layer having a refractive index of 1.2 or more and 2.5 or less in the wavelength range of 6 μm to 10 μm and a second layer having a refractive index of 3.2 or more and 4.3 or less in the wavelength range of 6 μm to 10 μm are alternately stacked.
[0032] The optical filter in this embodiment includes a wavelength range of 50 nm to 800 nm in which the average transmittance is 70% to 95% within the wavelength range of 6 μm to 10 μm, and has a maximum transmittance of 10% or more within the wavelength range of 12.5 μm to 20 μm. When there are a plurality of wavelength ranges in which the average transmittance is 70% or more and 95% or less, the width of the wavelength range refers to the total width of the wavelength ranges.
[0033] In the optical filter of this embodiment, the average transmittance in the wavelength range of 12.5 μm to 20 μm is preferably 5% to 60%, more preferably 10% to 60%, and even more preferably 30% to 60%. Here, the optical filter has the above-mentioned cut surface and a bandpass surface provided on either side of the Si substrate (see FIG. 1). Alternatively, a multilayer film may be provided on one side of the Si substrate. The upper limit of the average transmittance in the wavelength range of 12.5 μm to 20 μm, 60%, corresponds to the upper limit of the average transmittance in the same wavelength range of the bandpass surface in this embodiment. In general, the transmittance of the bandpass surface is not 100% even in a region with no sensor sensitivity. Therefore, in the optical filter, the average transmittance in the wavelength range of 12.5 μm to 20 μm has an upper limit value smaller than 100%, and the upper limit value is determined by the average transmittance of the bandpass surface. On the other hand, the lower limit of the average transmittance of the optical filter in the wavelength range of 12.5 μm to 20 μm varies depending on the average transmittance of the cut surface. In other words, depending on the lamination state of the cut surface, the lower limit of the average transmittance of the optical filter can be changed to, for example, 30%, 10%, or 5%.
[0034] The reason why there is a suitable value for the average transmittance in the wavelength range of 12.5 μm to 20 μm is as follows. The number of layers of the optical filter tends to depend on the width of the wavelength range to be blocked. In particular, in an NDIR gas sensor, since there is absorption of multiple gases (CO2, H2O, SO2, C3H8, CH2O, NO, etc.) in the range of 12.5 μm to 20 μm, it is necessary to block mid-infrared light in the wavelength range of 12.5 μm to 20 μm in order to detect a specific gas with high accuracy.
[0035] On the other hand, the sensitivity range of the semiconductor light receiving and emitting component affects the density of states and the Boltzmann distribution. FIG. 13 is a diagram showing the cutoff wavelength of the semiconductor light receiving and emitting component. In particular, the rising wavelength of the sensitivity on the long wavelength side depends on the band gap energy Eg. In the present invention, by optimally designing the band gap energy of the light receiving and emitting component, a sensor can be realized that has sensitivity to a specific absorption wavelength range corresponding to the detection target gas, but has no sensitivity to the wavelength range of 12.5 μm to 20 μm. As a result, the blocking of 12.5 μm to 20 μm by the optical filter becomes unimportant, the design of the optical filter is simplified, and cost reduction and improvement of mass productivity can be achieved. At that time, the average transmittance in the wavelength range of 12.5 μm to 20 μm exceeds 5%, and in the range of average transmittance of 5 to 60%, it becomes possible to simplify the optical filter while maintaining the performance as an NDIR gas sensor.
[0036] On the other hand, to realize a highly accurate gas sensor, it is desirable to make the shape of the transmission spectrum with an average transmittance of 70% or more in the wavelength range of 6 μm to 10 μm closer to a rectangle. In order to make the rising and falling shapes of the transmission spectrum sharper and closer to a rectangle, the number of laminated optical filters is increased, and as a result, a certain blocking effect is received even in the wavelength range of 12.5 μm to 20 μm. Therefore, the average transmittance is kept within 60%. In other words, the upper and lower limit values in the wavelength range of 12.5 μm to 20 μm indicate the range in which the optical filter can be simplified while maintaining the performance as an NDIR gas sensor.
[0037] (Method for measuring the average transmittance of optical filters) To confirm that the average transmittance of the optical filter in the wavelength range of 6 μm to 10 μm is 70% or more and 95% or less, for example, a micro FT-IR device (Hyperion 3000 + TENSOR 27 manufactured by Bruker) is used to measure the transmittance in the wavenumber range of 500 cm. -1 From 4200cm -1 , wave number resolution 8cm -1The transmission spectrum is obtained by dividing the numerical integral value of the transmittance in the above wavelength range by the wavelength range (range). The number of measurement points is 200 points per 1000 nm (= 1 point per 5 nm). The average transmittance in the wavelength range of 12.5 μm to 20 μm can also be confirmed in the same way.
[0038] Here, when the first layer is laminated multiple times, the material and film thickness of each first layer may be the same or different. The same applies to the second layer. The multilayer film may further include layers other than the first and second layers. When the first and second layers are laminated alternately, it is also possible to have a laminate structure such as the first layer → the second layer → the third layer → the first layer → the second layer, etc.
[0039] The thickness of the multilayer film is preferably 10 μm to 50 μm, more preferably 10 μm to 40 μm, and even more preferably 10 μm to 20 μm. This provides the effect of shortening the time required for manufacturing the optical filter and improving the yield. The film thickness can be measured by cross-sectional SEM observation.
[0040] The number of times the first layer and the second layer are alternately laminated, in terms of the number of repeating units when one first layer and one second layer are regarded as one repeating unit, is preferably from 10 to 60, and more preferably from 10 to 40. This provides the effect of shortening the time required for manufacturing the optical filter and improving the yield. The number of times the layers are alternately stacked can be measured by cross-sectional SEM observation.
[0041] ---1st layer--- The first layer of the multilayer film of this embodiment has a refractive index of 1.2 or more and 2.5 or less in the wavelength range of 6 μm to 10 μm. Specific materials for the first layer include TiO2, ZnS, etc. The first layer may be made of the above materials.
[0042] ---2nd layer--- The second layer of the multilayer film of this embodiment has a refractive index of 3.2 or more and 4.3 or less in the wavelength range of 6 μm to 10 μm. Specific examples of the material for the second layer include Si, Ge, etc. The second layer may be made of the above-mentioned materials.
[0043] (Method of measuring refractive index of first layer and second layer) In the present embodiment, the refractive index is a value measured by an ellipsometer in accordance with JIS K7142.
[0044] -Infrared receiving / emitting element- The infrared light emitting / receiving element is a first conductive type semiconductor layer, an active layer InAs y Sb 1-y (0.1≦y≦0.2), and a second conductivity type semiconductor layer.
[0045] Here, "receiving and emitting" means having at least one of the functions of receiving and emitting light, and the infrared receiving and emitting element specifically refers to an infrared emitting diode or an infrared photodiode.
[0046] Also, here, y Sb 1-y "(0.1≦y≦0.2)" means that the layer contains In, As, and Sb, but this expression also includes cases where other elements are contained. Specifically, this expression also includes cases where the composition of this layer is slightly changed by adding small amounts of other elements (for example, elements such as As, P, Ga, N, etc., a few percent or less). The same meaning is intended when the wording "contains" is used to describe the composition of other layers.
[0047] (Method of measuring As composition in each layer) The As composition of each layer was determined by secondary ion mass spectrometry (SIMS) as follows. A magnetic SIMS device IMS 7f manufactured by CAMECA was used for the measurements. This method involves irradiating a solid surface with a beam of primary ion species, digging in the depth direction by the sputtering phenomenon, and detecting the secondary ions generated at the same time to perform composition analysis. Note that the As composition here refers to the ratio of the As element to the elements contained in each layer.
[0048] Specifically, the primary ion species was cesium ion (Cs+), the primary ion energy was 2.5 keV, the beam incidence angle was 67.2°, and MCs+ (where M is Al, Ga, In, As, Sb, etc.), which has a small matrix effect, was detected as the secondary ion species.
[0049] In this case, sputtering was performed under the above-mentioned constant conditions, and the composition of the target layer was analyzed by continuing sputtering for a specified time until the target layer depth was reached. The target layer depth can be determined from the thickness of each layer by cross-sectional TEM measurement, which will be described later. The conversion of sputtering time to depth in SIMS analysis was performed by measuring the sputtering depth for a certain period of time under the same conditions as the analysis, for example using a stylus-type step gauge, to determine the sputtering rate, and then using this to convert the sputtering time during sample measurement into depth.
[0050] The As composition was calculated from the signal intensity of MCs+ in each layer. For example, in the case of an InAsSb layer, the As composition was calculated by (signal intensity of AsCs+)÷((signal intensity of AsCs+)+(signal intensity of SbCs+)).
[0051] Even if each layer has a uniform composition in the depth direction, the signal intensity may be distributed in the depth direction due to the influence of sputtering. In this case, the maximum signal intensity is taken as the representative value of the signal intensity of each layer.
[0052] The quantitative value of the Al composition obtained by the analysis may deviate from the true value. In order to correct this deviation from the true value, a separate sample was prepared for which the lattice constant value was obtained by X-ray diffraction (XRD) and used as a standard sample with a known As composition value. SIMS analysis was performed using the measurement conditions for the As composition of each layer to determine the sensitivity coefficient of the Al composition to the signal intensity. The As composition of each layer was determined by multiplying the SIMS signal intensity by the above sensitivity coefficient.
[0053] Here, another sample is an InAs substrate with a thickness of 800 nm stacked on a GaAs substrate. y Sb 1-y The lattice constant of this sample was determined by X-ray diffraction (XRD: X-ray Diffaction) using an X-ray diffractometer X'Pert MPD manufactured by Spectris Inc. as follows, and the As composition y of the standard sample was determined.
[0054] By performing a 2θ-ω scan using X-ray diffraction, the InAs y Sb 1-y The lattice constant of the layer containing InAs in the normal direction to the substrate surface was obtained, and the As composition x was determined from the lattice constant in the normal direction using Vegard's law. y Sb 1-y It is assumed that there is no anisotropic distortion of the layers. Specifically, Vegard's law is expressed by the following equation (1).
[0055]
number
[0056] where a InAs is the lattice constant of InAs, aInSb is the lattice constant of InSb, and a InAsSb is the InAs determined by the above X-ray diffraction y Sb 1-y is the lattice constant. InAs 6.0585Å, a InSbUse 6.4794 Å for this. As the standard sample for SIMS measurement, those with 0.1 < y < 0.15 were used.
[0057] The first conductivity type and the second conductivity type may each be any of n-type (including n-type impurities), i-type (not containing impurities), and p-type (including p-type impurities). The first conductivity type semiconductor layer, the active layer, and the second conductivity type semiconductor layer may be formed on a semiconductor substrate such as a GaAs substrate or a Si substrate. In this embodiment, each layer may be provided in the order of the first conductivity type semiconductor layer, the active layer, and the second conductivity type semiconductor layer from the substrate, or each layer may be provided in the order of the second conductivity type semiconductor layer, the active layer, and the first conductivity type semiconductor layer from the substrate. And in this embodiment, preferably, the first conductivity type is n-type and the second conductivity type is p-type.
[0058] Also, in this embodiment, one or a plurality of barrier layers may be provided between the first conductivity type semiconductor layer and the active layer and / or between the active layer and the second conductivity type semiconductor layer. In this embodiment, preferably, an n-type barrier layer is provided between the first conductivity type semiconductor layer and the active layer, and a p-type barrier layer is provided between the active layer and the second conductivity type semiconductor layer. As the n-type barrier layer, n-type Al x In 1-x Sb (0.15 ≤ x ≤ 0.35) is preferable for enhancing the effects of the present invention. As the p-type barrier layer, p-type Al x In 1-x Sb (0.15 ≤ x ≤ 0.35) is preferable for enhancing the effects of the present invention.
[0059] [Relationship between the composition of the active layer and the characteristics of the optical filter] Regarding each gas to be detected, the preferable composition of the active layer and the characteristics of the optical filter are as follows. When the gas to be detected contains alcohol, the active layer is InAs y Sb 1-y(0.1≦y≦0.2), and the optical filter preferably includes a wavelength range of 50 nm to 800 nm in which the average transmittance is 70% or more and 95% or less within the wavelength range of 6 μm to 10 μm, and has a maximum transmittance of 10% or more in the wavelength range of 12.5 μm to 20 μm.
[0060] [Optical devices] The optical device according to the present embodiment has the same characteristics as the NDIR gas sensor according to the present embodiment described above. The optical device is not limited to the NDIR gas sensor, and may be an infrared radiation thermometer, an infrared spectroscopic imaging sensor, or a human body detection sensor having similar characteristics. According to the optical device of this embodiment, even when a simplified optical filter is used, it is possible to obtain the effect of being able to selectively receive / emit only infrared light in a desired wavelength band.
[0061] In one aspect, the optical device according to this embodiment includes an optical filter having a substrate and a multilayer film having a plurality of layers with different refractive indexes formed on at least one surface of the substrate, and an infrared ray receiving and emitting element having a first conductive type semiconductor layer, an active layer, and a second conductive type semiconductor layer, the multilayer film having a structure in which a first layer having a refractive index of 1.2 or more and 2.5 or less in the wavelength range of 6 μm to 10 μm and a second layer having a refractive index of 3.2 or more and 4.3 or less in the wavelength range of 6 μm to 10 μm are alternately stacked, and the active layer is InAs y Sb 1-y (0.1≦y≦0.2), and the optical filter includes a wavelength range of 50 nm to 800 nm in which the average transmittance is 70% or more and 95% or less within the wavelength range of 6 μm to 10 μm, and the maximum transmittance in the wavelength range of 12.5 μm to 20 μm is 10% or more.
[0062] In another aspect, the optical device according to the present embodiment includes an optical filter having a substrate and a multilayer film having a plurality of layers with different refractive indexes formed on at least one surface of the substrate, and an infrared ray receiving and emitting element having a first conductive type semiconductor layer, an active layer, and a second conductive type semiconductor layer, the multilayer film having a structure in which a first layer including at least one selected from the group consisting of TiO2 and ZnS and a second layer including at least one selected from the group consisting of Si and Ge are alternately stacked, and the active layer is InAs. y Sb 1-y (0.1≦y≦0.2), and the optical filter includes a wavelength range of 50 nm to 800 nm in which the average transmittance is 70% or more and 95% or less within the wavelength range of 6 μm to 10 μm, and the maximum transmittance in the wavelength range of 12.5 μm to 20 μm is 10% or more. EXAMPLES
[0063] The present invention will be described in detail below based on examples. However, the present invention is not limited to the following examples, and it goes without saying that various modifications can be made without departing from the spirit of the invention.
[0064] [Example 1] The IR sensor of the first embodiment, which combines a simplified filter and an infrared receiving element, will be described. The IR sensor constitutes a part of an optical device such as an alcohol sensor. First, the PIN diode structure was created by the MBE method. The active layer is InAs. 0.14 Sb 0.86 The n-type semiconductor layer contains 1.0×10 Sn. 19 atoms / cm 3 By doping, the energy band is degenerated, making it transparent to infrared light with wavelengths longer than 2 μm. In addition, n-type Al 0.22 In 0.78 Sb and p-type Al 0.22 In 0.78 A barrier layer was formed of Sb. The laminated structure of each layer of the infrared emitting / receiving element according to Examples 1 to 3 is shown in FIG.
[0065] A positive photoresist for i-line was applied to the surface of the semiconductor wafer thus prepared, and exposure was performed using i-line with a reduced projection exposure machine. Next, development was performed, and multiple resist patterns were regularly formed on the surface of the semiconductor laminate. Next, multiple mesas were formed by dry etching. After forming a SiO2 film as a hard mask on the element having a mesa shape, the element was separated by dry etching, and then a SiN film was formed as a protective film, and contact holes were formed by photolithography and dry etching. Then, multiple mesas were connected in series by photolithography and sputtering. Then, a polyimide resin was formed as a protective film to cover the surface of the element.
[0066] The wafer produced by the above-mentioned pre-processing was diced into individual pieces, Au wires were bonded to the lead frame, and the pieces were sealed with epoxy-based molding resin so that the light receiving surface was exposed. The spectral sensitivity spectrum of the infrared receiving element produced in this way was measured, and the results shown in FIG. 6 were obtained. FIG. 6 shows the spectral spectrum of the infrared receiving element according to Examples 1 to 3. This sensor is sensitive to infrared rays around 9.5 μm, which is the absorption band of alcohol, but has almost no sensitivity to infrared rays on the longer wavelength side than 12.5 μm.
[0067] The optical filter was designed by simulation. A known calculation method using Fresnel coefficients was used for the simulation. Ge and ZnS were assumed to be the materials for the optical thin film, and literature values were used for the wavelength dispersion data of their complex refractive indexes. As shown in Figure 12, the refractive index of Ge in the range of 6 μm to 10 μm is approximately 4, and the refractive index of ZnS is approximately 2.2. The simplified filter design calculated by optical simulation is described below.
[0068] FIG. 7 shows the transmission spectrum of the optical filters (simplified filters) according to Examples 1 to 3 in comparison with the transmission spectrum of the optical filter (filter of conventional configuration) according to the comparative example. FIG. 8 shows the laminated structure of the simplified filters according to Examples 1 to 3. As shown in FIG. 7, the simplified filters have a transmission range from 12.5 μm onwards. By eliminating the need for a blocking function in this range, the thickness of the optical thin film can be reduced to 37.249 μm compared to 60 μm for the conventional filter. The simplified filter shown in FIG. 7 has an average transmittance of 72% in the wavelength range of 9.3 μm to 9.7 μm. In addition, the maximum transmittance in the wavelength range of 12.5 μm to 20 μm is 57%, and the average transmittance in this wavelength range is 28%.
[0069] Next, Fig. 9 shows the spectrum of an IR sensor for alcohol detection configured by combining an infrared receiving element and an optical filter (simplified filter) in Example 1. As shown in this result, the output is equivalent when combined with an infrared receiving element regardless of which optical filter is used. In other words, it was shown that the design of the optical filter can be greatly simplified without any deterioration in performance as a sensor component for an NDIR gas sensor.
[0070] [Example 2] In the second embodiment, the active layer is InAs 0.1 Sb 0.90 The other is the same as in Example 1. FIG. 10 shows the spectrum of an IR-sensor for alcohol detection configured by combining an infrared receiving element and an optical filter (simplified filter) in Example 2. As this result shows, whichever optical filter is used, the output when combined with an infrared receiving element is equivalent. In other words, it has been shown that the design of the optical filter can be greatly simplified without any deterioration in performance as a sensor component for an NDIR gas sensor.
[0071] [Example 3] In the third embodiment, the active layer is InAs 0.19 Sb 0.81The other is the same as in Example 1. FIG. 11 shows the spectrum of an IR-sensor for alcohol detection configured by combining an infrared receiving element and an optical filter (simplified filter) in Example 3. As this result shows, whichever optical filter is used, the output when combined with an infrared receiving element is equivalent. In other words, it has been shown that the design of the optical filter can be greatly simplified without any deterioration in performance as a sensor component for an NDIR gas sensor.
[0072] FIG. 12 shows wavelength dispersion data of the refractive index of the dielectric materials used in the optical simulations of Examples 1 to 3.
[0073] Detailed conditions and results of the Examples and Comparative Examples are shown in Table 1. Here, the wavelength-transmittance curves of Examples 1 to 3 and the Comparative Example are shown in FIG.
[0074] [Table 1]
[0075] In Examples 1 to 3 in Table 1, the film thickness of the optical filter is 63% or less compared to the Comparative Example, but when combined with an infrared light receiving / emitting element, the same performance can be realized. Here, the Comparative Example differs from Examples 1 to 3 in that the maximum transmittance in the wavelength range of 12.5 μm to 20 μm is 3% or less, which is less than 10%. Also, the Comparative Example differs from Examples 1 to 3 in that the average transmittance in the wavelength range is 0.3%, which is less than 5%.
[0076] According to the present invention, it is possible to provide a highly accurate NDIR gas sensor, an optical device, and an optical filter for an NDIR gas sensor even when a simplified optical filter is used. An optical device may be configured by combining the infrared light emitting element of Example 2, the infrared light receiving element of any one of Examples 1 to 3, and a simplified filter.
[0077] Here, the optical filter having a band with a width of 50 nm or more and an average transmittance of 70% or more in the wavelength range of 9 μm to 10 μm is a sub-combination of the above embodiment and is included in the present invention. In this case, the multilayer film includes a structure in which a first layer having a refractive index of 1.2 to 2.5 in the wavelength range of 9 μm to 10 μm and a second layer having a refractive index of 3.2 to 4.3 in the wavelength range of 9 μm to 10 μm are alternately stacked. In addition, the optical filter having a band with a width of 50 nm or more and an average transmittance of 70% or more in the wavelength range of 7 μm to 11 μm is also included in the present invention. In this case, the multilayer film includes a structure in which a first layer having a refractive index of 1.2 to 2.5 in the wavelength range of 7 μm to 11 μm and a second layer having a refractive index of 3.2 to 4.3 in the wavelength range of 7 μm to 11 μm are alternately stacked.
Claims
1. an optical filter including a substrate and a multilayer film having a plurality of layers with different refractive indices formed on at least one surface of the substrate; an infrared emitting / receiving element having a first conductive type semiconductor layer, an active layer, and a second conductive type semiconductor layer; Equipped with the multilayer film includes a structure in which a first layer having a refractive index of 1.2 or more and 2.5 or less in a wavelength range of 6 μm to 10 μm and a second layer having a refractive index of 3.2 or more and 4.3 or less in a wavelength range of 6 μm to 10 μm are alternately laminated; the active layer comprises InAs y Sb 1-y (0.1≦y≦0.2); The optical filter includes a wavelength range of 6 μm to 10 μm in which the average transmittance is 70% or more over a width of 50 nm or more, and has a maximum transmittance of 10% or more in a wavelength range of 12.5 μm to 20 μm; The infrared emitting / receiving element is an NDIR gas sensor that has no sensitivity in the wavelength range of 12.5 μm to 20 μm.
2. The optical filter includes a wavelength range of 50 nm to 800 nm in which the average transmittance is 70% or more and 95% or less in the wavelength range of 9 μm to 10 μm, and the maximum transmittance in the wavelength range of 12.5 μm to 20 μm is 10% or more.
2. The NDIR gas sensor of claim 1.
3. 3. The NDIR gas sensor according to claim 2, wherein the gas to be detected is alcohol.
4. 4. The NDIR gas sensor according to claim 1, wherein the multilayer film has a thickness of 10 μm or more and 50 μm or less.
5. 5. The NDIR gas sensor according to claim 1, wherein the number of times the first layers and the second layers are alternately stacked in the multilayer film is 10 to 60.
6. The first layer is TiO 2 6. The NDIR gas sensor of claim 1 , comprising at least one selected from the group consisting of: ZnS.
7. The NDIR gas sensor according to claim 1 , wherein the second layer includes at least one selected from the group consisting of Si and Ge.
8. The NDIR gas sensor according to claim 1 , wherein the infrared light emitting / receiving element is an infrared LED and / or an infrared photodiode.
9. 9. The NDIR gas sensor according to claim 1, wherein the infrared light emitting and receiving elements are an infrared LED and an infrared photodiode.
10. 10. The NDIR gas sensor of claim 1, wherein the multilayer film is formed on both sides of the substrate.
11. an optical filter including a substrate and a multilayer film having a plurality of layers with different refractive indices formed on at least one surface of the substrate; an infrared emitting / receiving element having a first conductive type semiconductor layer, an active layer, and a second conductive type semiconductor layer; Equipped with The multilayer film is made of TiO 2 ZnS and a second layer including at least one selected from the group consisting of Si and Ge, the active layer comprises InAs y Sb 1-y (0.1≦y≦0.2); The optical filter includes a wavelength range of 6 μm to 10 μm in which the average transmittance is 70% or more over a width of 50 nm or more, and has a maximum transmittance of 10% or more in a wavelength range of 12.5 μm to 20 μm; The infrared emitting / receiving element is an NDIR gas sensor that has no sensitivity in the wavelength range of 12.5 μm to 20 μm.
12. an optical filter including a substrate and a multilayer film having a plurality of layers with different refractive indices formed on at least one surface of the substrate; an infrared emitting / receiving element having a first conductive type semiconductor layer, an active layer, and a second conductive type semiconductor layer; Equipped with the multilayer film includes a structure in which a first layer having a refractive index of 1.2 or more and 2.5 or less in a wavelength range of 6 μm to 10 μm and a second layer having a refractive index of 3.2 or more and 4.3 or less in a wavelength range of 6 μm to 10 μm are alternately laminated; the active layer comprises InAs y Sb 1-y (0.1≦y≦0.2); The optical filter includes a wavelength range of 6 μm to 10 μm in which the average transmittance is 70% or more over a width of 50 nm or more, and has a maximum transmittance of 10% or more in a wavelength range of 12.5 μm to 20 μm; The infrared ray receiving and emitting element is an optical device that has no sensitivity in the wavelength range of 12.5 μm to 20 μm.
13. an optical filter including a substrate and a multilayer film having a plurality of layers with different refractive indices formed on at least one surface of the substrate; an infrared emitting / receiving element having a first conductive type semiconductor layer, an active layer, and a second conductive type semiconductor layer; Equipped with The multilayer film is made of TiO 2 ZnS and a second layer including at least one selected from the group consisting of Si and Ge, the active layer comprises InAs y Sb 1-y (0.1≦y≦0.2); The optical filter includes a wavelength range of 6 μm to 10 μm in which the average transmittance is 70% or more over a width of 50 nm or more, and has a maximum transmittance of 10% or more in a wavelength range of 12.5 μm to 20 μm; The infrared ray receiving and emitting element is an optical device that has no sensitivity in the wavelength range of 12.5 μm to 20 μm.
Citation Information
Patent Citations
Infrared optical fiber for detecting sulfur hexafluoride gas and preparation method thereof
CN106125183A
Multilayered film interference filter for gas analyzer
JP1985225803A
Detector for carbon dioxide and detection thereof
JP1997033431A
Gas sensor
JP2017020901A
Infrared-receiving device
JP2017143237A