Semiconductor Wafer

The semiconductor wafer design with a protective film and side tape attachment, along with a low etching rate member, addresses chemical seepage and adhesive residue issues, ensuring efficient and residue-free plating processes.

JP7559954B2Active Publication Date: 2024-10-02DENSO CORP
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2023534762
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2021-07-14
Filing Date
2022-07-07
Publication Date
2024-10-02
Estimated Expiration
2042-07-07

AI Technical Summary

Technical Problem

Existing methods for suppressing chemical seepage during semiconductor wafer plating are inadequate due to surface unevenness, leading to gaps between protective tapes and electrodes, requiring additional processing and adhesion enhancements that cause adhesive residue issues.

Method used

A semiconductor wafer design with a protective film covering the surface electrode and a side protective tape attached outside the electrode area, ensuring tight contact without gaps, and using a low etching rate member to isolate conductor plugs, preventing chemical penetration and adhesive residue.

Benefits of technology

Accurate chemical suppression during plating without additional steps, easy tape peeling, and prevention of residue formation, enhancing manufacturing efficiency and product quality.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007559954000001
    Figure 0007559954000001
  • Figure 0007559954000002
    Figure 0007559954000002
  • Figure 0007559954000003
    Figure 0007559954000003
Patent Text Reader

Abstract

According to the present invention, a protective film (50) is formed so as to cover a part of a surface electrode (40) and to extend beyond the surface electrode toward the outer edge of a semiconductor substrate (10); and the protective film (50) is formed so as to cover an interlayer insulating film (20) and a conductor plug (30) on the outside of the surface electrode. The present invention is also provided with a lateral surface protection tape (70) that is bonded to the outer edge of the protective film at the outer periphery of the semiconductor substrate and the outer edge of the semiconductor substrate. In addition, the region of the protective film, the region being bonded to the lateral surface protection tape, is positioned outside a portion of the protective film, the portion covering the surface electrode.
Need to check novelty before this filing date? Find Prior Art

Description

CROSS-REFERENCE TO RELATED APPLICATIONS

[0001] This application is based on Japanese Patent Application No. 2021-116506 filed on July 14, 2021, the contents of which are incorporated herein by reference. [Technical field]

[0002] The present disclosure relates to semiconductor wafers having semiconductor devices. [Background technology]

[0003] Conventionally, after forming an electrode on the surface side of a semiconductor wafer in which a semiconductor element is fabricated, the surface of the semiconductor wafer is covered with a protective film such as polyimide, and then a plating process is performed to form a metal plating layer on the surface of the electrode. Since the chemical solution may seep into the outer edge of the semiconductor wafer during the plating process, a protective tape is attached to the outer edge of the semiconductor wafer to prevent the chemical solution from seeping in (see Patent Document 1). [Prior art documents] [Patent documents]

[0004] [Patent Document 1] JP 2016-152317 A Summary of the Invention

[0005] However, unevenness on the surface of the semiconductor wafer, such as steps between areas where the electrodes are exposed, areas covered with the protective film, and areas where only the protective film is present, creates gaps between the protective tape and the surface of the semiconductor wafer, making it difficult to adequately prevent the chemicals from seeping in even when the protective tape is applied.

[0006] To address this issue, it is possible to prevent the seepage of chemicals into the protective tape by using a method to improve adhesion by performing a vacuum process after the protective tape is applied, or by using a method to increase the adhesion of the adhesive material of the tape, etc. However, this requires dedicated equipment for the additional process, and there is also the problem that the increased adhesion makes it easier for adhesive to remain when the tape is peeled off.

[0007] The present disclosure aims to provide a semiconductor wafer having a structure that does not require additional processes, is easy to peel off after plating, and can accurately suppress penetration of chemical solutions during plating, and a method for manufacturing a semiconductor device using the same.

[0008] A semiconductor wafer according to one aspect of the present disclosure includes a semiconductor substrate on which a semiconductor element is formed, an interlayer insulating film formed on the semiconductor substrate and having a plurality of contact holes at least a portion of which is connected to a predetermined position of the semiconductor element, a plurality of conductor plugs embedded in the plurality of contact holes, a surface electrode formed inside the outer edge of the semiconductor substrate and connected to at least a portion of the plurality of conductor plugs, a protective film covering a portion of the surface electrode and extending to the outer edge of the semiconductor substrate from the surface electrode to cover the interlayer insulating film and the conductor plugs outside the surface electrode, a side protective tape attached to the outer edge of the protective film at the outer periphery of the semiconductor substrate and the outer edge of the semiconductor substrate, and a plating layer formed on the surface of the portion of the surface electrode exposed from the protective film. The region of the protective film attached to the side protective tape is an outer region of the protective film covering the portion of the surface electrode.

[0009] In this way, by making the area of ​​the protective film that is attached to the side protective tape be an area outside the portion of the protective film that covers the surface electrode, the outer edge of the protective film and the side protective tape can be adhered tightly without any gaps.

[0010] Therefore, when plating is performed on the surface of the front electrode, the chemical solution can be appropriately prevented from seeping into the side protective tape, which eliminates the need for an additional process and allows for easy peeling after plating, resulting in a semiconductor wafer having a structure that can appropriately prevent the chemical solution from seeping in during plating.

[0011] The reference symbols in parentheses attached to each component indicate an example of the correspondence between the component and specific components described in the embodiments described below. [Brief description of the drawings]

[0012] [Figure 1] 1 is a cross-sectional view of an outer periphery side of a semiconductor wafer according to a first embodiment. [Diagram 2] 1 is a flowchart showing a manufacturing process of a semiconductor device. [Diagram 3] FIG. 11 is a cross-sectional view of the outer periphery of a semiconductor wafer shown as a comparative example. [Figure 4] 13 is a cross-sectional view showing a structure in which a contact hole in which a conductor plug is to be disposed is stopped by a low etching rate member according to the second embodiment. FIG. [Diagram 5] 13 is a cross-sectional view showing a case where the protective film and the side protective tape are arranged apart from each other. FIG. [Figure 6A] FIG. 11 is an enlarged cross-sectional view of the vicinity of a conductor plug according to a modified example of the second embodiment. [Figure 6B] FIG. 11 is an enlarged cross-sectional view of the vicinity of a conductor plug according to a modified example of the second embodiment. [Figure 6C] FIG. 11 is an enlarged cross-sectional view of the vicinity of a conductor plug according to a modified example of the second embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0013] Hereinafter, embodiments of the present disclosure will be described with reference to the drawings. In the following embodiments, parts that are the same or equivalent to each other will be denoted by the same reference numerals.

[0014] (First embodiment) A first embodiment will be described below, which describes a semiconductor wafer having a structure suitable for suppressing penetration of chemicals during plating processing, and a method for manufacturing a semiconductor device using the semiconductor wafer.

[0015] First, the configuration of a semiconductor wafer 1 according to this embodiment will be described with reference to Fig. 1. The semiconductor wafer 1 shown in Fig. 1 has been subjected to a plating process, and a side protection tape 70, which will be described later, is attached to the outer edge of the wafer. In other words, the semiconductor wafer 1 is shown at an intermediate stage during the manufacturing process of a semiconductor device, which will be described later, and the semiconductor device is manufactured by carrying out the remaining part of the manufacturing process.

[0016] As shown in FIG. 1, the semiconductor wafer 1 includes a semiconductor substrate 10 having a semiconductor element (not shown) fabricated therein, an interlayer insulating film 20 and a conductor plug 30 formed on the semiconductor substrate 10, a surface electrode 40, a protective film 50, a plating layer 60, and a side protective tape 70.

[0017] The semiconductor substrate 10 is in the form of a wafer, and a semiconductor element is formed in advance by carrying out a manufacturing process for the semiconductor element. Although a detailed structure is not shown here, the semiconductor elements are formed in a predetermined layout in an effective region that is extracted as a chip from the semiconductor wafer 1. Any semiconductor element may be formed on the semiconductor substrate 10, and for example, a vertical MOSFET with a trench gate structure is formed. When a vertical MOSFET with a trench gate structure is formed as a semiconductor element, a vertical MOSFET having a trench gate structure in which multiple MOSFETs are arranged in a stripe shape with one direction as the longitudinal direction is formed for each chip arranged in the effective region.

[0018] The interlayer insulating film 20 is formed so as to cover the front surface side of the semiconductor substrate 10 on which the semiconductor elements are formed, and is composed of a silicon oxide film or the like. A plurality of contact holes 21 are formed in the interlayer insulating film 20, at least a part of which exposes a predetermined position of the semiconductor element. For example, when a vertical MOSFET is formed as the semiconductor element, source contact holes connected to the n-type source region and the high concentration p-type contact layer in the base region are formed as the contact holes 21. In addition to the source contact holes, gate contact holes connected to gate liners drawn from the gate electrodes provided in each trench gate structure are also formed as the contact holes 21.

[0019] The conductor plugs 30 are embedded in the contact holes 21 and are electrically connected to the respective parts exposed in the contact holes 21. The conductor plugs 30 are made of a metal conductor, such as W (tungsten), and are formed from the surface of the interlayer insulating film 20 in which the contact holes 21 are formed to the surface of the semiconductor substrate 10. The conductor plugs 30 are surrounded by the interlayer insulating film 20, so that they are isolated from each other.

[0020] The surface electrode 40 is an electrode of various types that is electrically connected to the conductor plug 30 and is electrically connected to a predetermined position of the semiconductor element, and is made of, for example, an Al (aluminum)-based electrode material. For example, when forming a vertical MOSFET as a semiconductor element, a gate pad including a source electrode and a gate wiring layer is formed as the surface electrode 40, and the surface electrode 40 is patterned into a predetermined shape so that these are electrically separated. The surface electrode 40 is formed in an effective area of ​​the semiconductor wafer 1 that is extracted as a chip, and is not formed at least in the vicinity of the outer edge of the semiconductor wafer 1. In other words, the area within a predetermined distance from the outer periphery of the semiconductor wafer 1 is set as an area where the surface electrode 40 is not formed. In the area where the surface electrode 40 is not formed, the interlayer insulating film 20 and the conductor plug 30 are exposed from the surface electrode 40.

[0021] The protective film 50 covers at least a part of the surface electrode 40 and also plays a role in covering and protecting the interlayer insulating film 20 and the conductor plug 30 that are exposed from the surface electrode 40, and is made of, for example, polyimide. The protective film 50 is formed so as to cover the outer edge of each surface electrode 40 formed in the effective region of the semiconductor wafer 1. The protective film 50 is also formed in the ineffective region of the semiconductor wafer 1 that is not extracted as a chip, that is, in the region arranged to surround the periphery of the effective region. In the effective region, the surface is unevenly formed by forming a pattern of the surface electrode 40, etc., so that the protective film 50 formed on the surface is also in a state in which a pattern having an unevenness is formed. However, in the ineffective region, the pattern of the surface electrode 40, etc. is not formed, and the interlayer insulating film 20 and the conductor plug 30 located outside the surface electrode 40 are exposed. For this reason, in the region outside the surface electrode 40, the protective film 50 has a structure in which the interlayer insulating film 20 and the conductor plug 30 are directly covered by the protective film 50, and the surface of the protective film 50 is a flat surface with almost no unevenness.

[0022] Note that the flat surface without irregularities here means that there are no irregularities caused by the thickness of the surface electrode 40, and does not mean that there are no unevenness caused by film thickness variations that occur when forming the protective film 50 or by the surface roughness of the interlayer insulating film 20 and the conductor plug 30. A surface without irregularities caused by the thickness of the surface electrode 40 when only the protective film 50 is formed on the interlayer insulating film 20 and the conductor plug 30 is called a flat surface without irregularities.

[0023] The protective film 50 may be formed up to the outer circumferential edge of the semiconductor wafer 1 , but in this embodiment, the outer circumferential edge of the protective film 50 is located inside the outer circumferential edge of the semiconductor wafer 1 .

[0024] The plating layer 60 is formed on the surface of the portion of the front electrode 40 that is exposed from the protective film 50. The plating layer 60 is formed by plating, for example, a barrier metal material or a material that improves bonding properties. Here, the plating layer 60 is made of Ni (nickel). The plating layer 60 is formed in a state where the side surface of the semiconductor substrate 10 and the outer edge of the protective film 50 are covered by a side surface protective tape 70 or the like.

[0025] The side protection tape 70 is attached to the semiconductor substrate 10 so as to cover the side of the semiconductor substrate 10, that is, a predetermined range of the outer peripheral end and the outer edge, and the entire circumference of the inner peripheral portion is attached to the protective film 50. The side protection tape 70 may be made of any material that is used in semiconductor plating, such as elastomer composition, PP (polypropylene), PET (polyethylene terephthalate), silicone, UV tape, etc. The side protection tape 70 is adhered to the outer peripheral end of the semiconductor substrate 10, the exposed parts at the outer edge of the interlayer insulating film 20 and the conductor plug 30, and a predetermined range of the outer edge located inside from the outer peripheral end of the protective film 50. The inner side of the side protection tape 70 is adhered to the outer edge part of the protective film 50 whose surface is flat, and is adhered only to the area of ​​the protective film 50 where no pattern is formed, and is not adhered to the area where the pattern is formed. In other words, the area of ​​the protective film 50 to which the side protective tape 70 is attached is only an area outside the portion of the protective film 50 that covers the front electrode 40. Therefore, the side protective tape 70 is in close contact with the area of ​​the protective film 50 that does not have any irregularities on its surface, without any gaps.

[0026] Next, a method for manufacturing a semiconductor device, including a manufacturing process for the semiconductor wafer 1 configured as above, will be described with reference to the flowchart shown in FIG.

[0027] First, a surface element structure forming process is performed as step S100 in FIG. 2. That is, a manufacturing process for forming a semiconductor element on a wafer-shaped semiconductor substrate 10 is performed, and various processes are performed on the surface side of the semiconductor substrate 10. If an n-channel vertical MOSFET is to be formed as a semiconductor element, a process for forming each part for constituting a vertical MOSFET is performed. That is, various processes such as forming an n-type drift layer, forming a p-type base region, forming an n-type source region and a high-concentration p-type contact layer, forming a gate trench, forming a gate insulating film, and forming a gate electrode are performed on the n-type semiconductor substrate 10. As a result, a semiconductor element is formed on the semiconductor substrate 10. Furthermore, a process for forming an interlayer insulating film 20 and a conductor plug 30, a process for forming a surface electrode 40, and even a process for forming a protective film 50 are performed.

[0028] Next, in step S105, a surface protective tape attachment step (not shown) is performed. That is, a surface protective tape is attached so as to cover the entire surface side of the semiconductor wafer 1. Then, in step S110, a backside grinding step is performed to grind the backside of the semiconductor wafer 1 by a predetermined thickness, thereby thinning the semiconductor wafer 1. After the grinding step of the backside of the semiconductor wafer 1 is completed, in step S115, a backside etching step of the semiconductor wafer 1 is performed to flatten the backside of the semiconductor wafer 1 and remove damage.

[0029] Thereafter, in step S120, a surface protection tape peeling process is performed to peel off the surface protection tape from the surface of the semiconductor wafer 1. In addition, in step S125, the sample is placed in a sputtering device or the like to perform a back electrode formation process of forming an electrode on the back surface of the semiconductor wafer 1. If a vertical MOSFET is formed as the semiconductor element, this back electrode will be the drain electrode.

[0030] Next, a back surface protective tape attachment step (not shown) is performed as step S130. That is, the back surface protective tape is attached to the back surface of the semiconductor wafer 1. Furthermore, a side surface protective tape attachment step is performed as step S135, whereby the side surface protective tape 70 is attached so as to cover the side surface of the semiconductor wafer 1, that is, the outer peripheral edge and the outer edge portion of the protective film 50. At this time, the protective film 50 and the side surface protective tape 70 are in close contact with each other without any gaps.

[0031] Then, in step S140, a front surface plating process is performed with the side and rear surfaces of the semiconductor wafer 1 covered with the side protective tape 70 and rear protective tape. For example, a plating layer 60 of a Ni layer is formed on the surface of the portion of the front surface electrode 40 that is exposed from the protective film 50. The state in which the plating layer 60 is formed in this manner is shown in FIG.

[0032] At this time, the sample is immersed in the chemical solution during the surface plating process, but since the protective film 50 and the side protective tape 70 are in close contact with each other without any gaps, it is possible to appropriately prevent the chemical solution from seeping into the inside of the side protective tape 70. This prevention of the seepage of the chemical solution is achieved simply by making the outer edge of the protective film 50 into a structure without unevenness or pattern formation. Therefore, no additional processing is required, unlike the method of improving adhesion by performing a vacuum drawing process after the attachment of the side protective tape 70. In addition, unlike the method of increasing the adhesion of the adhesive material of the tape, it is possible to prevent the adhesive from remaining when peeling off after the plating process, and peeling can be easily performed.

[0033] Thereafter, in steps S145 and S150, a step of peeling off the side protective tape 70 and a step of peeling off the back protective tape are performed in this order. In step S155, a step of attaching the back protective tape is performed again to attach a dicing tape to the back surface of the semiconductor wafer 1.

[0034] Thereafter, a dicing process is performed in step S160 to divide the semiconductor wafer 1 into chip units, and then a back surface protective tape peeling process is performed in step S165 to peel each chip from the back surface protective tape to form individual chips. In this manner, chipped semiconductor devices can be manufactured.

[0035] As described above, in this embodiment, the outer edge of the protective film 50 formed on the surface of the semiconductor wafer 1, to which the side protection tape 70 is attached, is a flat surface on which no pattern is formed. Therefore, the outer edge of the protective film 50 and the side protection tape 70 can be closely attached to each other without any gaps.

[0036] More specifically, in the past, the semiconductor wafer 1 had a structure in which the surface electrode 40 and the protective film 50 were formed up to the outer edge of the semiconductor wafer 1 on the interlayer insulating film 20 and the conductor plug 30 formed on the semiconductor substrate 10, as shown in Fig. 3. Therefore, even when the side protective tape 70 is attached to the protective film 50, the surface of the protective film 50 has an uneven state, so that a gap is generated between the side protective tape 70 and the protective film 50, and the chemical solution during plating is allowed to seep in. Note that, in Fig. 3, the surface electrode 40 is shown to be formed on one side with the same thickness, but in reality, it is patterned and has an uneven state corresponding to the thickness.

[0037] In contrast, in the semiconductor wafer 1 of this embodiment, the side surface protective tape 70 is attached to the protective film 50, which has a smooth surface, so that the outer edge of the protective film 50 and the side surface protective tape 70 can be tightly attached without any gaps.

[0038] Therefore, when plating is performed on the surface of the front electrode 40, it is possible to appropriately prevent the chemical solution from seeping into the inside of the side protective tape 70. As described above, no additional process is required, and it is possible to prevent glue from remaining when peeling off after plating. Therefore, it is possible to obtain a semiconductor wafer 1 having a structure that does not require an additional process, is easy to peel off after plating, and can appropriately prevent the chemical solution from seeping in during plating. By manufacturing a semiconductor device using such a semiconductor wafer 1, it is possible to prevent problems caused by the seeping of the chemical solution during plating, such as the occurrence of residual chemical solution.

[0039] Second embodiment The second embodiment will be described. The second embodiment is different from the first embodiment in that it suppresses defects in the inner region of the semiconductor wafer 1, and is otherwise similar to the first embodiment, so only the differences from the first embodiment will be described.

[0040] In the first embodiment, it is intended to suppress the penetration of the chemical solution during plating in the outer edge portion of the semiconductor wafer 1. In addition, in the present embodiment, defects during plating are suppressed in the region inside the outer edge portion of the semiconductor wafer 1, specifically, inside the region where the side protection tape 70 is attached.

[0041] In the inner region of the semiconductor wafer 1, it is preferable to reduce the number of parts formed on the scribe lines as much as possible so that dicing can be easily performed and residues generated during dicing can be prevented from adhering to the final product and causing defects. For this reason, it is preferable to prevent the formation of the front surface electrodes 40 or to eliminate the protective film 50 on the scribe lines. In this case, the interlayer insulating film 20 and the conductor plugs 30 will be exposed to chemicals on the scribe lines during plating.

[0042] In this way, when the conductor plug 30 is exposed to a chemical solution, plating may adhere to the exposed portion of the conductor plug 30, which may cause residues in later processes. Plating is difficult to adhere to the surface of the conductor plug 30, but when plating adheres, it is easy to peel off due to low adhesion, and it is easy to become residues in later processes. Although it is attempted to avoid forming the conductor plug 30 on the scribe line as much as possible, when the alignment mark cannot be formed inside the chip, there are cases where an alignment mark using the material of the conductor plug 30 must be formed on the scribe line. In such a case, the alignment mark formed by the exposed conductor plug 30 on the scribe line is conductive with the semiconductor substrate 10 during plating. It was found that this causes plating to adhere to the exposed surface of the conductor plug 30.

[0043] Therefore, in this embodiment, as shown in FIG. 4, the exposed conductor plug 30 and the semiconductor substrate 10 are spaced apart, and the conductor plug 30 does not contact the semiconductor substrate 10. That is, the conductor plug 30 is separated from the semiconductor substrate 10 and is in an electrically floating state. Specifically, a low etching rate member 22 is provided at the position where the conductor plug 30 is to be formed, which reduces the etching rate when the contact hole 21 is formed in the interlayer insulating film 20 compared to the case where only the interlayer insulating film 20 is formed. In this way, the contact hole 21 can be prevented from reaching the semiconductor substrate 10, and the low etching rate member 22 is disposed between the conductor plug 30 and the semiconductor substrate 10. That is, the alignment mark 41 made of the material of the surface electrode 40 and the conductor plug 30 with the exposed surface are not electrically connected through the semiconductor substrate 10. Therefore, the adhesion of plating to the surface of the exposed conductor plug 30 is suppressed. Therefore, the generation of residue can be suppressed, and it is possible to suppress the residue from adhering to the final product and causing defects.

[0044] Such a low etching rate member 22 can be made of, for example, polysilicon or SiN (silicon nitride film). The low etching rate member 22 can be manufactured by any method, and for example, after forming a part of the interlayer insulating film 20, only the low etching rate member 22 is formed and a process of patterning it can be applied. Furthermore, the low etching rate member 22 can be formed by sharing the process with a process for forming another part used in forming a semiconductor element. For example, in the case of forming a vertical MOSFET as a semiconductor element, after a gate insulating film is formed on the surface of the semiconductor substrate 10, the low etching rate member 22 is formed from the polysilicon when a gate electrode made of polysilicon is formed thereon. If the interlayer insulating film 20 is formed thereafter, the manufacturing process of the low etching rate member 22 can be shared with another process used in forming a semiconductor element, and the manufacturing process can be simplified by suppressing an increase in the manufacturing process.

[0045] In the first embodiment, only the protective film 50 is formed on the interlayer insulating film 20 and the conductive plug 30, and the protective film 50 is arranged up to the outer edge of the semiconductor wafer 1 so that the side protective tape 70 is attached to the surface of the protective film 50. As described above, this is to allow the side protective tape 70 to be attached to the smooth surface of the protective film 50 without any gaps, but it is also possible to have a structure in which the protective film 50 is not provided up to the outer edge of the semiconductor wafer 1 as shown in FIG. 5. In this way, the side protective tape 70 can be attached to the interlayer insulating film 20 and the conductive plug 30 with few irregularities, so that the side protective tape 70 can be attached without any gaps. However, in this case, the conductive plug 30 is exposed between the protective film 50 and the side protective tape 70, so that the plating layer 60 may adhere during the plating process and cause residues to be generated. Therefore, for the outer edge of the semiconductor wafer 1, it is preferable to arrange the protective film 50 up to the outer edge of the semiconductor wafer 1 so that the side protective tape 70 is attached to the surface of the protective film 50 as in the first embodiment.

[0046] In addition, as a technique for suppressing the adhesion of plating to the surface of the conductor plug 30, there are a technique for covering the surface of the conductor plug 30 with a material that causes highly adhesive plating growth, and a technique for covering with a material that does not cause plating growth. However, covering with a material that causes plating growth causes problems such as chipping and shortening of blade life in the dicing process in which the chip is divided into small pieces in a later process, as the covering material and the grown plating become a load on the dicing blade. In addition, covering with a material that does not cause plating growth requires the formation of an additional film, which causes a problem of increased costs. For this reason, it is useful to have a structure in which the conductor plug 30 does not come into contact with the semiconductor substrate 10 by using the low etching rate member 22, as in this embodiment.

[0047] (Modification of the second embodiment) In the above-described second embodiment, an example has been shown in which the low etching rate member 22 is formed on the surface of the semiconductor substrate 10 via an insulating film such as a part of the interlayer insulating film 20 or a gate insulating film, but other structures are also possible.

[0048] For example, when a vertical MOSFET with a trench gate structure is formed as a semiconductor element, the low etching rate member 22 can be formed using a trench gate structure similar to that of the vertical MOSFET. Specifically, as shown in FIG. 6A, a trench 11 is formed from the surface of the semiconductor substrate 10 at a position where a conductor plug 30 is to be formed. Then, the low etching rate member 22 made of a polysilicon layer with a structure similar to that of a gate electrode is provided in the trench 11. In this way, the low etching rate member 22 can be formed with a structure similar to that of the trench gate structure. Even in this way, the manufacturing process of the low etching rate member 22 can be shared with another process used in forming the semiconductor element, and an increase in the manufacturing process can be suppressed to simplify the manufacturing process.

[0049] 6B, a structure can also be adopted in which a trench 11 is formed at the position where the conductor plug 30 is to be formed at the same time as the trench gate structure, but no polysilicon layer is formed in the trench 11. In other words, the trench 11 is filled with a part of the gate insulating film or the interlayer insulating film 20, so that the thickness of the insulating film at the position where the conductor plug 30 is to be formed is substantially thicker than the part other than the trench 11. In this way, the aspect ratio of the conductor plug 30 until it reaches the semiconductor substrate 10, that is, the ratio of depth to width, can be increased, and the conductor plug 30 can be prevented from contacting the semiconductor substrate 10, and the same effect as in the second embodiment can be obtained.

[0050] 6C, the width dimension of the contact hole 21 is narrowed to increase the aspect ratio, that is, to make the conductor plug 30 formed in the scribe line smaller in width than the conductor plug 30 formed in the chip. In this way, when the contact hole 21 is formed in the interlayer insulating film 20, the contact hole 21 formed in the scribe line is shallower in depth than the contact hole 21 formed in the chip due to the microloading phenomenon. Therefore, when the conductor plug 30 is formed, the conductor plug 30 formed in the scribe line can be prevented from contacting the semiconductor substrate 10, and the same effect as the second embodiment can be obtained.

[0051] (Other embodiments) Although the present disclosure has been described based on the above-described embodiment, it is not limited to the embodiment, and includes various modifications and modifications within the equivalent range. In addition, various combinations and forms, and other combinations and forms including only one element, more than one element, or less than one element, are also within the scope and concept of the present disclosure.

[0052] For example, in each of the above embodiments, a vertical MOSFET is given as an example of a semiconductor element, but the present invention is not limited thereto, and other semiconductor elements may be used, or horizontal semiconductor elements may be used instead of vertical semiconductor elements. When a vertical IGBT having a trench gate structure is formed as a semiconductor element, the effect of being able to form the structures shown in Figures 4, 6A, and 6B by sharing the process when forming the trench gate structure is obtained.

[0053] In the above second embodiment, the region on the scribe line has been described as an example of an exposed region in which the interlayer insulating film 20 and the conductor plug 30 are exposed from the protective film 50. However, when an exposed region exists other than the region on the scribe line, it is preferable to prevent the conductor plug 30 from contacting the semiconductor substrate 10 in the exposed region as well, as in the structure shown in the second embodiment and its modified example.

[0054] In the first embodiment, the method for manufacturing the semiconductor device has been described based on the flowchart shown in Fig. 2, but it is not necessary to perform all of the processes shown therein. For example, if the back surface of the semiconductor substrate 10 is not ground, the back surface grinding process and the back surface etching process may be omitted.

Claims

1. A semiconductor wafer, A semiconductor substrate (10) on which a semiconductor element is formed; an interlayer insulating film (20) formed on the semiconductor substrate and having a plurality of contact holes (21) at least a portion of which is connected to a predetermined position of the semiconductor element; A plurality of conductor plugs (30) embedded in the plurality of contact holes; a surface electrode (40) formed inside an outer edge portion of the semiconductor substrate and connected to at least some of the conductive plugs; a protective film (50) that covers a portion of the surface electrode and is formed to an outer edge side of the semiconductor substrate beyond the surface electrode, thereby covering the interlayer insulating film and the conductor plug outside the surface electrode; a side protection tape (70) attached to the outer periphery of the protective film at the outer peripheral end of the semiconductor substrate and the outer edge of the semiconductor substrate; a plating layer (60) formed on a surface of a portion of the surface electrode that is exposed from the protective film; A semiconductor wafer, wherein the region of the protective film attached to the side surface protective tape is an area outside a portion of the protective film covering the front surface electrode.

2. an exposed region in which the interlayer insulating film and the conductor plug are exposed from the protective film is provided in a region inside the region to which the side protective tape is attached; 2. The semiconductor wafer of claim 1, wherein in said exposed region, said conductive plug is spaced from said semiconductor substrate.

3. 3. The semiconductor wafer according to claim 2, wherein a low etching rate member (22) having an etching rate lower than that of the interlayer insulating film when the contact hole is formed is disposed between the conductor plug and the semiconductor substrate.

4. the semiconductor element is a vertical MOSFET or a vertical IGBT having a trench gate structure, 4. The semiconductor wafer according to claim 3, wherein the low etching rate member is made of polysilicon, which is a material of a gate electrode constituting the trench gate structure.

5. A trench is formed in the semiconductor substrate, The semiconductor wafer of claim 4 , wherein the low etch rate member is disposed within the trench.

6. 3. The semiconductor wafer of claim 2, wherein the aspect ratio, which is the ratio of the depth to the width of the conductor plug, of the conductor plug formed in the exposed region has a higher aspect ratio than that of the conductor plug connected to the surface electrode or covered by the protective film.

Citation Information

Patent Citations

  • Method for manufacturing semiconductor device

    JP2004363518A

  • Method of manufacturing semiconductor device

    JP2010103310A

  • Method of manufacturing semiconductor device

    JP2010225600A

  • Semiconductor device manufacturing method

    JP2016152317A

  • Semiconductor device and manufacturing method

    JP2017168659A