Formation of high carbon content flowable dielectric films with low processing damage.

The use of high carbon content carbosiloxane precursors and nitrogen treatment forms a porous dielectric film with smaller pores and improved mechanical stability, addressing processing damage issues in semiconductor devices and enhancing film performance.

JP7560216B2Active Publication Date: 2024-10-02INTERNATIONAL BUSINESS MACHINE CORPORATION
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2021540574
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2019-01-18
Filing Date
2019-12-12
Publication Date
2024-10-02
Estimated Expiration
2039-12-12

AI Technical Summary

Technical Problem

Existing ultra-low k dielectric films in semiconductor devices are susceptible to processing damage during etching and patterning, leading to increased capacitance and reliability issues due to high porosity and mechanical instability.

Method used

A method involving the deposition of cyclic and linear carbosiloxane precursors with high carbon content, followed by exposure to nitrogen-containing precursors and energy sources, forms a porous dielectric film with smaller pore sizes and improved mechanical stability, reducing susceptibility to machining damage.

Benefits of technology

The resulting dielectric film exhibits lower capacitance, improved mechanical properties, and enhanced resistance to etching, with a carbon content that stabilizes the film structure, providing better conformal coverage and reduced plasma-induced damage.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007560216000016
    Figure 0007560216000016
  • Figure 0007560216000017
    Figure 0007560216000017
  • Figure 0007560216000018
    Figure 0007560216000018
Patent Text Reader

Abstract

A method for fabricating a dielectric film includes depositing a first precursor on a substrate. The first precursor includes a cyclic carbosiloxane group having a six-membered ring. The method also includes depositing a second precursor on the substrate. The first precursor and the second precursor form a preliminary film on the substrate, the second precursor including silicon, carbon, and hydrogen. The method further includes exposing the preliminary film to energy from an energy source to form a porous dielectric film.
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates generally to fabrication methods and resulting structures for semiconductor devices. More specifically, the present invention relates to fabrication methods and resulting structures for high carbon content flowable dielectric films formed with low processing damage.

[0002] Integrated circuits in electronic devices entail semiconductor device fabrication. A series of photolithographic and chemical processing steps creates electronic circuits on semiconductor wafers. The semiconductor wafers are subjected to front-end-of-line (FEOL) and back-end-of-line (BEOL) processes. FEOL processes involve forming transistors directly in silicon. BEOL processes involve interconnecting the respective semiconductor devices to form electrical circuits. In particular, interconnect metal lines separated by insulating layers are created. The insulating dielectric material is, for example, silicon dioxide or a low dielectric constant (k) material. Summary of the Invention

[0003] An embodiment of the present invention is directed to a method for making a dielectric film. A non-limiting example of the method includes depositing a first precursor on a substrate. The first precursor includes a cyclic carbosiloxane group with a six-membered ring. The method also includes depositing a second precursor on the substrate. The first precursor and the second precursor form a preliminary film on the substrate, the second precursor includes silicon, carbon, and hydrogen. The method further includes exposing the preliminary film to energy from an energy source to form a porous dielectric film. Advantages of the method include providing smaller pore sizes than the eight-membered ring carbosiloxane counterpart, which reduces the k value and provides lower capacitance.

[0004] Another non-limiting example of the method includes depositing a first precursor on a substrate, the first precursor having the following structure:

[0005] [ka]

[0006] and a, b, c, d, e, and f are each independently an alkyl or alkenyl group. The method also includes depositing a second precursor on the substrate. The first precursor and the second precursor form a pre-film on the substrate, the second precursor comprising a linear carbosiloxane. The method further includes exposing the pre-film to an energy source to form a porous dielectric film. Advantages of the method include smaller pore sizes than the eight-membered carbosiloxane counterpart, which lowers the k value providing lower capacitance.

[0007] Another non-limiting example of the method includes depositing a first precursor on a substrate. The first precursor includes a cyclic carbosiloxane group. The method also includes depositing a second precursor on the substrate. The first precursor and the second precursor form a preliminary film on the substrate, the second precursor includes a carbosilane with a carbon to silicon ratio greater than 3:1. The method further includes exposing the preliminary film to an energy source to form a porous dielectric film. Advantages of the method include increased carbon content and smaller pore size, thus stronger and more stable bonds within the film, which provides improved mechanical properties (e.g., density) and reduced susceptibility to processing damage, for example, by etching and planarization.

[0008] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS The present invention is directed to dielectric films. Non-limiting examples of dielectric films include covalently bonded networks that include atoms of silicon, oxygen, carbon, and hydrogen. The dielectric films include cyclic carbosiloxane groups and bridged Si-CH 2 Advantages of the dielectric films include increased carbon content and smaller pore size, and therefore stronger and more stable bonds within the film, which provides improved mechanical properties (e.g., density) and reduced susceptibility to processing damage, e.g., by etching and planarization.

[0009] Another non-limiting example of a dielectric film includes a covalent network containing atoms of silicon, oxygen, carbon, hydrogen, and nitrogen. The dielectric film includes cyclic carbosiloxane groups and bridged Si-CH 2 Advantages of the dielectric films include increased carbon content and smaller pore size, and therefore stronger and more stable bonds within the film, which provides improved mechanical properties (e.g., density) and reduced susceptibility to processing damage, e.g., by etching and planarization.

[0010] Additional technical features and advantages are realized through the techniques of the present invention. Embodiments and aspects of the present invention are described in detail herein and are considered a part of the claimed subject matter. For a better understanding, refer to the detailed description and drawings.

[0011] The appended claims particularly point out and distinctly claim the exclusive rights set forth herein. The foregoing and other features and advantages of embodiments of the present invention will become apparent from the following detailed description taken in conjunction with the accompanying drawings.

[0012] 1-6 depict a process flow for fabricating a dielectric film in a semiconductor device according to an embodiment of the present invention. [Brief description of the drawings]

[0013] [Figure 1] 1 depicts a cross-sectional side view of a patterned substrate of a semiconductor device. [Diagram 2] 1 depicts a cross-sectional side view of a patterned substrate after flowing a first precursor and a second precursor onto the patterned substrate. [Diagram 3] 1 depicts a cross-sectional side view of a patterned substrate after forming a pre-dielectric film on the patterned substrate. [Figure 4] 1 depicts a cross-sectional side view of a patterned substrate after exposing the pre-dielectric film to a nitrogen-containing precursor. [Diagram 5] 1 depicts a cross-sectional side view of a patterned substrate after exposing the pre-dielectric film to an energy source. [Figure 6] 1 depicts a cross-sectional side view of a porous dielectric film formed on a patterned substrate. [Figure 7] 1 shows an exemplary electron microscope image depicting a dielectric film arranged in a trench in accordance with an embodiment of the present invention. [Figure 8] 1 depicts a graph comparing the dielectric constant of dielectric films formed with and without ultraviolet (UV) light curing. [Figure 9A] 1 depicts a graph showing atomic % carbon in dielectric films according to embodiments of the present invention. [Figure 9B] 1 depicts a graph showing atomic % carbon in comparative dielectric films. [Figure 10] 1 depicts a graph showing % shrinkage of a dielectric film after ammonia exposure according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0014] The diagrams depicted herein are illustrative. There may be many variations in the diagrams or the operations described therein without departing from the spirit of the invention. For example, actions may be performed in a different order, or actions may be added, removed, or modified. Also, the term "coupled" and variations thereof describe having a communication path between two elements, and do not imply a direct connection with no other intervening elements / connections between the elements. All of these variations are considered part of this specification.

[0015] In the accompanying drawings and the following detailed description of the described embodiments, the various elements shown in the drawings are provided with two- to three-digit reference numerals. With minor exceptions, the left-most digit(s) of each reference numeral corresponds to the figure in which the element is first shown.

[0016] For the sake of brevity, conventional techniques relating to semiconductor device and integrated circuit (IC) fabrication may or may not be described in detail herein. Moreover, various tasks and process steps described herein may be incorporated into a more comprehensive procedure or process having additional steps or functionality not described in detail herein. In particular, the various steps in the manufacture of semiconductor devices and semiconductor-based ICs are well known, and thus, for the sake of brevity, many conventional steps will be described only briefly herein or omitted entirely without providing details of well-known processes.

[0017] Turning now to an overview of the technology more specifically related to embodiments of the present invention, insulation requirements become more stringent as line dimensions shrink to increase the speed and memory storage capacity of microelectronic devices (e.g., computer chips). As size and dimensions shrink in these devices, lower k materials are needed to minimize the RC time constant, where R is the resistance of the conductive line and C is the capacitance of the insulating dielectric interlayer, and C is inversely proportional to the spacing and proportional to the k of the ILD.

[0018] Many of the fabrication steps of very large scale integration (VLSI) and ultra-large scale integration (ULSI) chips are performed by plasma enhanced chemical or physical vapor deposition techniques. The ability to fabricate ultra-low k materials by plasma enhanced chemical vapor deposition (PECVD) techniques using pre-installed and available processing equipment therefore facilitates manufacturing process integration, reduces manufacturing costs, and reduces hazardous waste.

[0019] Additionally, as the size of electronic devices decreases, the thickness of dielectric insulating layers decreases, and as a result, dielectric layers become increasingly susceptible to degradation, or wear-out failure, known as time-dependent dielectric breakdown (TDDB).

[0020] Ultra-low k dielectric films (SiCOH), which contain atoms of silicon (Si), carbon (C), oxygen (O), and hydrogen (H), can be non-porous or porous. Generally, porous SiCOH films have a lower dielectric constant (k) (e.g., k below 3.0) than the corresponding non-porous SiCOH films. Porous SiCOH films typically have k values ​​between about 1.8 and about 2.95, with lower k films having higher porosity. For example, porous films can be formed by introducing labile porogen groups during deposition of a pre-film structure that are subsequently removed by curing.

[0021] Porous ultra-low k SiCOH films, however, may have suboptimal mechanical properties compared to the corresponding non-porous dielectrics, e.g., high fracture rate and stress, and low modulus and hardness. SiCOH dielectric films may also degrade as k decreases. As a result, many ultra-low k SiCOH films are susceptible to processing damage. For example, the carbon contained in standard SiCOH films can be removed during patterning and etching processes (e.g., plasma reactive ion etching and oxygen-based plasma ashing processes). As a result, the film may behave like porous silicon oxide and be quickly removed by standard wet etches, which may affect dimensional control during patterning. In addition, the k value of porous silicon oxide readily absorbs moisture and has a much higher k value (e.g., k greater than 4.2). Porous oxide films result in higher overall k value and final device capacitance and reliability. Plasma Induced Damage (PID) is a parameter that describes this type of degradation in dielectric films.

[0022] Improved mechanical properties of low k or ultra-low k SiCOH dielectric films can be achieved by post-deposition treatment of the SiCOH films. Curing or treatment using, for example, heat, ultraviolet (UV) light, electron beam irradiation, chemical energy or a combination of these energy sources has been used to stabilize low or ultra-low k dielectric materials and improve their mechanical properties. While such post-deposition treatments are possible, they add extra processing steps, and thus costs, to the manufacture of low k or ultra-low k dielectric films. Therefore, there is a need for improved ultra-low k dielectric film materials that are less susceptible to mechanical damage after processing and can be used to fill devices with reduced sizes and dimensions.

[0023] SiCOH films can be formed by using a CVD process to deposit precursors onto patterned regions of a substrate. Precursors used to form the films include, for example, cyclic and linear organosilicon compounds (e.g., octamethylcyclotetrasiloxane ([(CH 3 ) 2 SiO] 4 ), and linear tetramethoxysilane (Si(OCH 3 ) 4 )) The precursors form a film that flows over the substrate during deposition to facilitate filling of confined geometries.

[0024] Although ultra-low k SiCOH films are desirable, porous SiCOH films with lower k values ​​can have suboptimal mechanical properties compared to corresponding non-porous materials, e.g., high fracture rates and stresses, and low modulus and hardness. These ultra-low k films are therefore susceptible to processing damage, e.g., from chemical mechanical planarization (CMP). There is therefore a need for improved ultra-low k dielectric film materials that are less susceptible to post-processing mechanical damage and can be used to fill devices with reduced sizes and dimensions.

[0025] Turning now to an overview of aspects of the invention, one or more embodiments of the invention address the above-mentioned shortcomings of the prior art by providing a method for depositing low k dielectric films with high carbon content (e.g., greater than 20%) and the resulting films. Two precursors are used to deposit the dielectric film. The first precursor is a cyclic organosilicon compound containing a cyclic carbosiloxane group with a six-membered ring in which three silicon atoms alternate with three oxygen atoms, or an eight-membered ring in which four silicon atoms alternate with four oxygen atoms. The first precursor contains a high carbon content. The second precursor is a high carbon content linear carbosiloxane or carbosilane. Compared to a cyclic precursor with four silicon atoms (e.g., octamethylcyclotetrasiloxane), the six-membered cyclic carbosiloxane precursor has a higher carbon content. In some embodiments of the invention, the ratio of C:Si is greater than 4:1 and the ratio of C:O is greater than 1. Once the first and second precursors are deposited on the patterned substrate, a pre-film is prepared by ionizing the precursor with a nitrogen-containing precursor (e.g., ammonia (NH)) to form a nitrogen-containing SiCONH film and to reduce film shrinkage. 3 )) The pre-membrane is cured to form the final porous membrane.

[0026] The above aspects of the invention address the shortcomings of the prior art by providing flowable, porous SiCOH and SiCONH films with high carbon content and low k values ​​(e.g., less than 3.0 according to one or more embodiments of the invention). Cyclic carbosiloxanes with three silicon atoms provide smaller pore sizes than their four silicon atom counterparts, which provides reduced pore sizes that lower the k value and provide lower capacitance. Due to the combination of higher carbon content and smaller pore sizes, and therefore stronger and more stable bonds within the film, the film has improved mechanical properties (e.g., density) and reduced susceptibility to processing damage, for example, by etching and planarization. The film also has improved conformal coverage for filling small gaps in patterned substrates.

[0027] Turning now to a more detailed description of aspects of the invention, FIGS. 1-6 depict a process flow for forming a dielectric film on a patterned substrate 101 including one or more trenches 102 according to an embodiment of the invention. FIG. 1 depicts a cross-sectional side view of the patterned substrate 101. The patterned substrate 101 includes single or multiple layers of materials including, but not limited to, semiconductor materials, insulating materials, conductive materials, or any combination thereof. Non-limiting examples of semiconductor materials include Si, SiGe, SiGeC, SiC, GaAs, InAs, InP, and other III / V or II / VI compound semiconductors. The patterned substrate 101 can also include layered substrates such as, for example, Si / SiGe, Si / SiC, silicon-on-insulator (SOI), or silicon germanium-on-insulator (SGOI).

[0028] When the patterned substrate 101 includes an insulating material, the insulating material can be an organic insulator, an inorganic insulator, or a combination thereof, including multiple layers. When the patterned substrate 101 includes a conductive material, the patterned substrate 101 can include, for example, polysilicon, elemental metals, alloys of elemental metals, metal silicides, metal nitrides, and combinations thereof, including multiple layers. The patterned substrate 101 can include a combination of a semiconducting material and an insulating material, a combination of a semiconducting material and a conductive material, or a combination of a semiconducting material, an insulating material, and a conductive material.

[0029] One or more trenches 102 (or gaps) in a patterned substrate 101 are formed, for example, by etching. When viewed from the surface, the trenches 102 can have any shape or dimensions. The trenches 102 can be circular, elliptical, polygonal, rectangular, or a variety of other shapes. The trenches 102 have a height and width that define a height-to-width aspect ratio of greater than 1:1 (e.g., 5:1 or more, 6:1 or more, 7:1 or more, 8:1 or more, 9:1 or more, 10:1 or more, 11:1 or more, 12:1 or more, etc.). In some embodiments of the invention, the high aspect ratio results from a small gap width of less than 32 nanometers (nm), less than 28 nm, less than 22 nm, or less than 16 nm. Although FIGS. 1-6 show an embodiment of a patterned substrate 101, according to other embodiments, the substrate is unpatterned. The films described herein can be deposited onto any substrate having any surface topology, including flat or substantially flat.

[0030] 2 depicts a cross-sectional side view of the patterned substrate 101 after flowing a first precursor 204 and a second precursor 206 onto the surface of the patterned substrate 101. The patterned substrate 101 is placed in a reactor chamber. The first precursor 204 and the second precursor 206, which may be in liquid, gas, or vapor form, may then be introduced into the chamber. Any deposition method may be used, such as spin-on coating, plasma-enhanced chemical vapor deposition (PECVD), thermal chemical vapor deposition, evaporation, or other methods.

[0031] The first precursor 204 is a cyclic carbosiloxane containing atoms of silicon (Si), carbon (C), oxygen (O), and hydrogen (H). The first precursor 204 is a six-membered ring with three silicon atoms alternating with three oxygen atoms according to some embodiments of the invention. The first precursor 204 is an eight-membered ring with four silicon atoms alternating with four oxygen atoms according to other embodiments of the invention.

[0032] In accordance with one or more embodiments of the present invention, the first precursor 204 has the following structure:

[0033] [ka]

[0034] and a, b, c, d, e, and f are each independently an alkyl or alkenyl group. According to one or more embodiments of the present invention, the alkyl group is a methyl group, an ethyl group, a propyl group, a butyl group, or a pentyl group. According to some embodiments of the present invention, the alkenyl group is an ethenyl group, a propenyl group, a butenyl group, or a pentenyl group.

[0035] In accordance with one or more embodiments of the present invention, the first precursor 204 has the following structure:

[0036] [ka]

[0037] and a, c, and e are each a methyl group, and b, d, and f are each an ethenyl group.

[0038] According to some embodiments of the present invention, the first precursor 204 has the following structure:

[0039] [ka]

[0040] and a, b, c, d, e, f, g, and h are each independently an alkyl or alkenyl group. According to one or more embodiments of the present invention, the alkyl group is a methyl group, an ethyl group, a propyl group, a butyl group, or a pentyl group. According to some embodiments of the present invention, the alkenyl group is an ethenyl group, a propenyl group, a butenyl group, or a pentenyl group.

[0041] In one or more embodiments of the invention, the first precursor 204 has a carbon to silicon (C:Si) ratio of greater than 2: 1. According to other embodiments, the first precursor has a C:Si ratio of about 3:1 to about 9:1.

[0042] The second precursor 206 is a linear carbosiloxane according to one or more embodiments of the present invention and includes atoms of silicon (Si), carbon (C), oxygen (O), and hydrogen (H). The second precursor 206 is a carbosilane according to other embodiments of the present invention and includes atoms of silicon (Si), carbon (C), and hydrogen (H).

[0043] The second precursor 206 also includes a high carbon content. In some embodiments of the invention, the ratio of C:Si in the second precursor 206 is greater than 3:1. According to other embodiments, the ratio of C:Si in the second precursor 206 is from about 4:1 to about 8:1. In one or more embodiments of the invention, the second precursor 406 has a carbon to oxygen (C:O) ratio of greater than 4:1. In other embodiments of the invention, the second precursor 406 has a C:O ratio of greater than 1.

[0044] In accordance with one or more embodiments of the present invention, the second precursor 206 has the following structure:

[0045] [ka]

[0046] and g, h, i, j, k, and l are each independently an alkyl group, an alkenyl group, or an alkoxyl group. The alkyl group is a methyl group, an ethyl group, a propyl group, a butyl group, or a pentyl group in some embodiments of the invention. The alkenyl group is an ethenyl group, a propenyl group, a butenyl group, or a pentenyl group according to one or more embodiments of the invention. The alkoxyl group is a methoxyl group, an ethoxyl group, a propoxyl group, or a butoxyl group according to some embodiments of the invention.

[0047] In accordance with one or more embodiments of the present invention, the second precursor 206 has the following structure:

[0048] [ka]

[0049] According to another embodiment of the present invention, the second precursor 206 has the following structure:

[0050] [ka]

[0051] According to some embodiments of the present invention, the second precursor 206 has the following structure:

[0052] [ka]

[0053] and m, n, o, and p are each independently hydrogen, an alkyl group, an alkenyl group, or an alkoxyl group. The alkyl group is a methyl group, an ethyl group, a propyl group, a butyl group, or a pentyl group in some embodiments of the invention. The alkenyl group is an ethenyl group, a propenyl group, a butenyl group, or a pentenyl group in accordance with one or more embodiments of the invention. The alkoxyl group is a methoxyl group, an ethoxyl group, a propoxyl group, or a butoxyl group in accordance with some embodiments of the invention.

[0054] In accordance with one or more embodiments of the present invention, the second precursor 206 has the following structure:

[0055] [ka]

[0056] According to another embodiment of the present invention, the second precursor 206 has the following structure:

[0057] [ka]

[0058] and Each of q and r is independently hydrogen, an alkyl group, an alkenyl group, or an alkoxyl group. The alkyl group is a methyl group, an ethyl group, a propyl group, a butyl group, or a pentyl group in some embodiments of the present invention. The alkenyl group is an ethenyl group, a propenyl group, a butenyl group, or a pentenyl group in accordance with one or more embodiments of the present invention. The alkoxyl group is a methoxyl group, an ethoxyl group, a propoxyl group, or a butoxyl group in accordance with some embodiments of the present invention.

[0059] In accordance with one or more embodiments of the present invention, the second precursor 206 has the following structure:

[0060] [ka]

[0061] An oxidizing gas or an inert gas can be included in the chamber while the first precursor 204 and the second precursor 206 are being deposited. Non-limiting examples of oxidizing gases include carbon dioxide, oxygen, nitrous oxide, or any combination thereof. The oxidizing gas can be used to stabilize the reactants in the reactor and to improve the uniformity of the dielectric film deposited on the substrate. The oxidizing gas is optional and can be used to promote reactivity and uniformity.

[0062] The conditions for depositing the first precursor 204 and the second precursor 206 may vary depending on the desired final dielectric constant of the dielectric film. However, using a lower temperature allows at least a portion of the unstable organic porogen groups to remain in the final film, thereby providing a film with a high carbon content. In accordance with one or more embodiments of the present invention, the temperature used may be in the range of about 10 to about 300° C. In another aspect, the temperature may be set at a temperature in the range of about 25 to about 200° C. Additionally, in other embodiments of the present invention, the temperature may be set at a temperature in the range of about 60 to about 120° C.

[0063] 3 depicts a cross-sectional side view of the patterned substrate 101 after forming a pre-dielectric film 303 from the first and second precursors 204, 206 on the patterned substrate 101. The pre-film 303 includes a covalently bonded network of silicon (Si), oxygen (O), carbon (C), and hydrogen (H) with cyclic carbosiloxane structures. The pre-film 303 includes cross-linked Si-CH from the second precursor 206 according to some embodiments of the present invention. 2 Also includes -Si group.

[0064] The pre-dielectric film 303 forms a generally uniform conformal layer over the surface of the patterned substrate 101. The pre-dielectric film 303 fills the trenches 102 without forming air gaps or voids therein, even with high aspect ratios.

[0065] The preliminary dielectric film 303 also includes unstable porogens, portions of which will be subsequently removed to produce a porous final dielectric film. Porogens are unstable, removable functional groups present in and covalently bonded to the preliminary film. At least a portion of the porogens are subsequently removed by an energetic treatment step (see FIG. 5) to provide a porous final low k film. As referred to herein, the porous dielectric film includes a plurality of pores or openings within the film formed from the removal of the plurality of unstable porogens.

[0066] 4 depicts a cross-sectional side view of the patterned substrate 101 after exposing the pre-dielectric film 303 to a nitrogen-containing precursor 410. The nitrogen-containing precursor 410 is, in accordance with one or more embodiments of the present invention, ammonia (NH 3 ). The nitrogen-containing precursor 410, according to some embodiments of the present invention, includes nitrous oxide (N 2 O).

[0067] Exposure of the pre-dielectric film 303 to the nitrogen-containing precursor 410 may or may not add small amounts of nitrogen (N) to the film. Thus, after exposure to the nitrogen-containing precursor 410, the resulting film contains silicon, carbon, oxygen, and hydrogen (SiCOH), or silicon, carbon, oxygen, hydrogen, and nitrogen (SiCONH). Exposure of the pre-dielectric film 303 to the nitrogen-containing precursor 410 reduces film shrinkage, allowing the film to maintain greater physical strength than an otherwise similar film that has not been treated. Without being bound by theory, exposure to the nitrogen-containing precursor 410 may increase the effectiveness of a subsequent curing process that can remove undesirable components and crosslink the film matrix to establish a rigid material lattice.

[0068] FIG. 5 depicts a cross-sectional side view of the nitrogen-treated pre-dielectric film 303a during curing by an energy source 505. Energy 505 is applied to the nitrogen-treated pre-dielectric film 303a in the form of thermal energy, UV light, microwave, electron beam, ion beam, or other energy sources such as catalytic species to form a porous final low k film (303b as shown in FIG. 6). In some embodiments of the present invention, a combination of two or more of these energy sources is employed. These energy inputs convert the nitrogen-treated pre-dielectric film 303a into a final porous low k film (as shown in FIG. 6). In particular, removal of at least a portion of the labile porogen groups from the pre-film provides a porous film as described below. Due to the structure of the first precursor 204, which has a cyclic carbosiloxane structure, smaller and substantially non-interconnected pores are provided, for example, compared to other cyclic tetrasilane precursors, such as octamethyl cyclotetrasilane (OMCTS). Also, due to the high carbon content of the second precursor, the carbon content of the final porous film is higher.

[0069] According to some embodiments of the invention, the temperature of the curing process is about 100 to about 450° C. According to other embodiments, the temperature of the curing process is about 200 to about 400° C. According to one or more embodiments of the invention, the temperature of the curing process is about 250 to about 385° C., or about 300 to about 350° C.

[0070] At least a portion of the porogen is then absent from the final low k film 303b. The energy treatment step creates pores, voids or holes in the final film. The resulting final low k film 303b has nanometer-scale porosity formed by the removal of the porogen groups.

[0071] The thickness of the low k film 303b typically varies and depends on the desired application. According to some embodiments of the invention, the low k film 303b has a thickness of about 5 to about 500 nanometers (nm). In some embodiments of the invention, the low k film 303b has a thickness of about 20 to about 120 nm.

[0072] In accordance with one or more embodiments of the present invention, the dielectric constant (k) of the low k film 303b is less than 3.0. In some embodiments of the present invention, the k value of the low k film 303b is less than 2.7. In yet another aspect, the k value of the low k film 303b is less than about 2.6. In yet another aspect, the k value of the low k film 303b is from about 2.2 to about 2.8.

[0073] In accordance with one or more embodiments of the present invention, the low k film 303b is a SiCOH film, which has a covalently bonded network of atoms Si, C, O, and H. These atoms form a three-dimensional network structure in which the Si, C, O, and H are interconnected in the x, y, and z directions. The low k film 303b contains a high percentage of carbon (C), which enhances cross-linking in the film. Furthermore, the higher carbon content provides favorable properties, including lower plasma-induced damage (PID), smaller average pore size, and improved modulus. In some embodiments of the present invention, the low k film 303b is a cross-linked Si-CH 2 -Contains Si groups.

[0074] In one or more embodiments of the invention, the low k film 303b comprises at least about 30 atomic percent (at. %) carbon (C). In some embodiments of the invention, the low k film 303b comprises at least 35 at. % carbon (C). Moreover, in other embodiments of the invention, the low k film 303b comprises about 35 to about 50 at. % carbon (C).

[0075] According to one or more embodiments, the low k film 303b is a SiCONH film and contains a small amount of nitrogen (N), which improves stability and PID. In some embodiments of the invention, the low k film 303b contains about 1 to about 15 atomic % nitrogen (N). In other embodiments of the invention, the low k film 303b contains about 1 to about 4 atomic % nitrogen (N).

[0076] The chemical structure of the low k film 303b enhances the mechanical properties of the material. According to one or more embodiments of the present invention, the low k film 303b has a modulus of about 3 to about 12 gigapascals (GPa) at a thickness of 400 nm. In some embodiments of the present invention, the low k film 303b has a modulus of about 7 to about 10 GPa at a thickness of 400 nm.

[0077] According to one or more embodiments of the present invention, the low k film 303b has a porosity of about 1 to about 50%. According to some embodiments of the present invention, the low k film 303b has a porosity of about 8 to about 20%.

[0078] The low k films 303b can be used in a variety of applications, such as fully aligned via processes and devices, FEOL gate stack gap fill applications, and magnetic tunnel junction magnetoresistive random-access memory (MTJ MRAM) gap fill and devices. EXAMPLES

[0079] 7 shows an exemplary electron microscope image 700 depicting a dielectric film 702 disposed in a trench of a substrate in accordance with an embodiment of the present invention. The film 702 was a SiCOH film having a thickness of about 80 nm and a k-value of about 2.75. As shown, the film 702 filled the high aspect ratio gap between pillars in the substrate 707. The gap had a 1:1 aspect ratio. The film 702 filled the gap without exhibiting voids.

[0080] 8 depicts a graph 800 comparing the dielectric constant of dielectric films formed with and without ultraviolet (UV) light curing. Measurements were performed at 150° C. In general, the dielectric film without UV curing 802 had a higher k value than the UV cured dielectric film 804. The UV curing reduced the k value from about 2.8 to about 2.6.

[0081] FIG. 9A depicts a graph 900 showing the atomic % (at.%) carbon in a film prepared according to an embodiment of the invention, which was formed from a cyclic carbosiloxane group precursor with a six-membered ring of silicon and oxygen. FIG. 9B depicts a graph 901 showing the atomic % (at.%) carbon in a comparative dielectric film, which was formed from an octamethylcyclotetrasilane (OMCTS) precursor containing an eight-membered ring of silicon and oxygen. As shown in FIGS. 9A and 9B, the at.% carbon 904 of the film of the invention was higher (40-45 at.%) (FIG. 9A) than the at.% carbon 903 of the comparative film, which was about 30 at.% (FIG. 9B).

[0082] 10 depicts a graph 1000 showing the % shrinkage of a dielectric film after ammonia exposure in accordance with an embodiment of the present invention. As shown, treating the film with ammonia reduced the shrinkage of the film.

[0083] Various embodiments of the invention are described herein with reference to the associated drawings. Alternatively, embodiments may be devised without departing from the scope of the invention. Although various connections and relationships (e.g., above, below, adjacent, etc.) are presented between elements in the following description and in the drawings, those skilled in the art will appreciate that many of the relationships described herein are orientation independent as the described functionality is maintained even if the orientation is changed. These connections and / or relationships may be direct or indirect unless otherwise specified, and the invention is not intended to be limited in this respect. Thus, the coupling of entities may refer to either direct or indirect coupling, and the relationship between entities may be a direct or indirect relationship. As an example of an indirect relationship, a statement herein to forming layer "A" on layer "B" includes the situation where one or more intermediate layers (e.g., layer "C") are between layers "A" and "B," so long as the relevant properties and functionality of layers "A" and "B" are not substantially altered by the intermediate layer(s).

[0084] The following definitions and abbreviations will be used for the interpretation of the claims and the specification. As used herein, the terms "comprises," "comprising," "includes," "including," "has," "having," "contains," "containing," or other variations thereof, are intended to cover a non-exclusive inclusion. For example, a composition, mixture, process, method, article, or device that comprises a list of elements is not necessarily limited to only those elements and can include other elements not expressly listed or inherent to such composition, mixture, process, method, article, or device.

[0085] Additionally, the term "exemplary" is used herein to mean "serving as an example, instance, or illustration." Any embodiment or design described herein as "exemplary" is not necessarily to be construed as preferred or advantageous over other embodiments or designs. The terms "at least one" and "one or more" are understood to include any integer number greater than or equal to one, i.e., 1, 2, 3, 4, etc. The term "a plurality" is understood to include any integer number greater than or equal to two, i.e., 2, 3, 4, 5, etc. The term "connection" can include an indirect "connection" and a direct "connection."

[0086] References herein to "one embodiment," "an embodiment," "an example embodiment," and the like indicate that the embodiment being described may include a particular feature, structure, or characteristic, but that all embodiments may or may not include that particular feature, structure, or characteristic. Moreover, such phrases do not necessarily refer to the same embodiment. Furthermore, it is submitted that when a particular feature, structure, or characteristic is described in connection with one embodiment, it is within the knowledge of one of ordinary skill in the art to affect such feature, structure, or characteristic that is described in connection with other embodiments, whether or not explicitly stated.

[0087] For purposes of the following description, the terms "upper," "lower," "right," "left," "vertical," "horizontal," "top," "bottom," and their derivatives should refer to the structures and methods being described as oriented during drawing. The terms "overlying," "atop," ("on top"), "positioned on," or "positioned atop" mean that a first element, such as a first structure, is on a second element, such as a second structure, and there may be an intervening element, such as an interface structure, between the first and second elements. The term "direct contact" means that a first element, such as a first structure, and a second element, such as a second structure, are connected without an intermediate conductive, insulating, or semiconducting layer at the interface of the two elements.

[0088] The phrase "selective to," e.g., "a first element selective to a second element," means that the first element can be etched and the second element can act as an etch stop.

[0089] The terms "about," "substantially," "approximately," and variations thereof are intended to include the degree of error associated with the measurement of a particular quantity based on equipment available at the time of filing. For example, "about" can include ±8% or 5%, or 2% of a given value.

[0090] As noted earlier herein, for the sake of brevity, the prior art related to semiconductor device and integrated circuit (IC) fabrication may or may not be described in detail herein. By way of background, however, a more general description of a semiconductor device fabrication process that may be utilized in implementing one or more embodiments of the present invention will now be provided. While the specific fabrication operations used in implementing one or more embodiments of the present invention may be individually known, the described combination of inventive operations and / or resulting structures is unique. Thus, the unique combination of operations described in connection with the fabrication of semiconductor devices in accordance with the present invention utilizes a variety of individually known physical and chemical processes performed on a semiconductor (e.g., silicon) substrate, some of which are described in the immediately following paragraphs.

[0091] In general, the various processes used to form microchips that will be packaged into ICs fall into four general categories: film deposition, removal / etching, semiconductor doping, and patterning / lithography. Deposition is any process that grows, coats, or otherwise transfers material onto a wafer. Available techniques include physical vapor deposition (PVD), chemical vapor deposition (CVD), electrochemical deposition (ECD), molecular beam epitaxy (MBE), and more recently, atomic layer deposition (ALD), among others. Removal / etching is any process that removes material from the wafer. Examples include etch processes (either wet or dry), and chemical mechanical planarization (CMP), and the like. Semiconductor doping is generally the modification of electrical properties by doping, for example, the source and drain of a transistor, by diffusion or ion implantation, or both. These doping processes are followed by furnace annealing or rapid thermal annealing (RTA). The annealing serves to activate the implanted dopants. Both conductor (e.g., polysilicon, aluminum, copper, etc.) and insulator (e.g., various forms of silicon dioxide, silicon nitride, etc.) films are used to connect and separate transistors and their components. Selective doping of various regions of a semiconductor substrate allows the conductivity of the substrate to change with the application of voltage. By creating structures of these various components, millions of transistors can be constructed and wired together to form the complex circuit elements of modern microelectronic devices. Semiconductor lithography is the formation of a three-dimensional relief image or pattern on a semiconductor substrate for subsequent transfer of the pattern to a substrate. In semiconductor lithography, the pattern is formed by a light-sensitive polymer called a photoresist.Lithography and etch pattern transfer steps are repeated multiple times to build the intricate structures that make up the transistors and the many wires that connect the circuit's millions of transistors. To form the final device, each pattern printed on the wafer is aligned with previously formed patterns, gradually building up conductors, insulators, and selectively doped regions.

[0092] The flow charts and block diagrams in the figures illustrate possible implementations of methods of making and / or operating according to various embodiments of the present invention. In the flow diagrams, various functions / operations of the method are represented by blocks. In some alternative implementations, the functions noted in the blocks may occur out of the order noted in the figures. For example, two blocks shown in succession may in fact be executed substantially simultaneously, or the blocks may sometimes be executed in the reverse order, depending on the functionality involved.

[0093] Although the description of various embodiments of the present invention has been presented for the purpose of explanation, these descriptions are not intended to be exhaustive or limited to the described embodiments. Many modifications and variations will be apparent to those skilled in the art without departing from the spirit of the described embodiments. Terminology has been selected herein to best explain the principles of the embodiments, practical applications, or technical improvements beyond the art found in the market, or to allow other skilled in the art to understand the embodiments described herein.

Claims

1. 1. A method of making a dielectric film, the method comprising: depositing a first precursor on a substrate, the first precursor comprising a cyclic carbosiloxane group having a six-membered ring and having a carbon to silicon ratio (C:Si) greater than 2:1; depositing a second precursor on the substrate, the first precursor and the second precursor forming a pre-film on the substrate, the second precursor comprising silicon, carbon, and hydrogen; exposing the pre-film to energy from an energy source to form a porous dielectric film; A method comprising:

2. 1. A method of making a dielectric film, the method comprising: depositing a first precursor on a substrate, the first precursor including a cyclic carbosiloxane group having a six-membered ring; depositing a second precursor on the substrate, the first precursor and the second precursor forming a pre-film on the substrate, the second precursor comprising silicon, carbon, and hydrogen; exposing the pre-film to energy from an energy source to form a porous dielectric film; wherein the porous dielectric film comprises at least 30 atomic % carbon.

3. The method of claim 1 or 2, wherein the substrate is a patterned substrate and the porous dielectric film is deposited in trenches in the patterned substrate.

4. The method of any one of claims 1 to 3, further comprising exposing the pre-film to a nitrogen-containing precursor.

5. The method of any one of claims 1 to 4, wherein the porous dielectric film further comprises about 1 to about 4 atomic % nitrogen.

6. 1. A method of making a dielectric film, the method comprising: depositing a first precursor on a substrate, the first precursor having the structure: [Formula 1] ,and depositing, wherein a, b, c, d, e, and f are each independently an alkyl or alkenyl group, and the first precursor has a carbon to silicon ratio (C:Si) of greater than 2:1; depositing a second precursor on the substrate, the first precursor and the second precursor forming a pre-film on the substrate, the second precursor comprising a linear carbosiloxane; exposing the pre-film to an energy source to form a porous dielectric film; A method comprising:

7. 1. A method of making a dielectric film, the method comprising: depositing a first precursor on a substrate, the first precursor having the structure: [Case 2] ,and wherein a, b, c, d, e, and f are each independently an alkyl or alkenyl group; depositing a second precursor on the substrate, the first precursor and the second precursor forming a pre-film on the substrate, the second precursor comprising: having the following structure: [C3] ,and wherein g, h, i, j, k, and l are each independently an alkyl group, an alkenyl group, or an alkoxyl group; exposing the pre-film to an energy source to form a porous dielectric film; A method comprising:

8. 1. A method of making a dielectric film, the method comprising: depositing a first precursor on a substrate, the first precursor having the structure: [C4] ,and a, b, c, d, e, and f are each independently an alkyl or alkenyl group, and the alkenyl group is an ethenyl group, a propenyl group, a butenyl group, or a pentenyl group; depositing a second precursor on the substrate, the first precursor and the second precursor forming a pre-film on the substrate, the second precursor comprising a linear carbosiloxane; exposing the pre-film to an energy source to form a porous dielectric film; A method comprising:

9. The method of any one of claims 6 to 8, further comprising exposing the pre-film to a nitrogen-containing precursor.

10. 1. A method of making a dielectric film, the method comprising: depositing a first precursor on a substrate, the first precursor including cyclic carbosiloxane groups, the first precursor having a carbon to silicon ratio (C:Si) greater than 2:1; depositing a second precursor on the substrate, the first precursor and the second precursor forming a pre-film on the substrate, the second precursor comprising a carbosilane with a carbon to silicon ratio of greater than 3:1; exposing the pre-film to an energy source to form a porous dielectric film; A method comprising:

11. The method of claim 10, further comprising exposing the preliminary film to a nitrogen-containing precursor.

12. 1. A method of making a dielectric film, the method comprising: depositing a first precursor on a substrate, the first precursor comprising a cyclic carbosiloxane group; depositing a second precursor on the substrate, the first precursor and the second precursor forming a pre-film on the substrate, the second precursor comprising a carbosilane with a carbon to silicon ratio of greater than 3:1; exposing the pre-film to an energy source to form a porous dielectric film; wherein the porous dielectric film comprises at least 30 atomic % carbon.

Citation Information

Patent Citations

  • Organic siloxane copolymer film, its manufacturing method, growth apparatus, and semiconductor device using same

    JP2004047873A

  • Method for curing low dielectric constant film by electron beam

    JP2005524983A

  • Sicoh dielectric and its manufacturing method

    JP2007194639A

  • Thin film resistor with current density enhancement layer (cdel)

    JP2008530820A

  • Method for forming si-containing film, insulator film, and semiconductor device

    JP2010067810A