Wiring board and method for manufacturing the same
By designing openings with recesses for larger bumps on the wiring board, the uneven heights of bumps with different diameters are addressed, enhancing connection reliability through equalized bump heights and preventing defects.
Patent Information
- Application Number
- JP2023076685
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2023-05-08
- Publication Date
- 2024-10-02
- Estimated Expiration
- 2039-04-26
AI Technical Summary
Bumps with different diameters on a wiring board result in uneven heights, leading to reduced connection reliability due to potential open failures for smaller bumps and short-circuit failures for larger bumps when semiconductor chips are mounted.
The wiring board design includes openings of varying diameters with recesses in the larger openings to accommodate a two-layer metal structure, ensuring the second metal layer is partially stored in the recess, maintaining equal heights for all bumps.
This design enhances connection reliability by ensuring consistent bump heights, preventing open defects and short-circuits, thereby improving the connection between the wiring board and semiconductor chips.
Smart Images

Figure 0007560603000001 
Figure 0007560603000002 
Figure 0007560603000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a wiring board and a method for manufacturing a wiring board. [Background technology]
[0002] Generally, a wiring board on which a semiconductor chip is mounted may have bumps formed as connection terminals with the semiconductor chip. A bump is a metal protrusion that connects to the conductor layer of the wiring board and protrudes outward from an opening provided in a solder resist layer that covers the conductor layer. Such a bump may have a two-layer structure formed by plating two different types of metal, for example.
[0003] Specifically, a first metal layer, such as copper, is plated in and around an opening in the solder resist layer, and a second metal layer, such as tin or solder, is plated on the first metal layer. Then, only the second metal layer is melted and solidified by a reflow process to form a bump with a spherical surface. That is, since the melting point of the second metal layer is lower than that of the first metal layer, by setting an appropriate reflow temperature, it is possible to form a bump by melting only the second metal layer without melting the first metal layer. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2007-103878 A [Patent Document 2] JP 2017-152646 A Summary of the Invention [Problem to be solved by the invention]
[0005] Incidentally, a wiring board and a semiconductor chip may be connected via a plurality of bumps. That is, for example, a connection terminal for inputting and outputting electric signals and a connection terminal for applying a power supply voltage may be provided separately. In such a case, the diameters of the bumps as the connection terminals are not necessarily all the same, and bumps of different diameters may be provided. Specifically, for example, the diameter of the bump for inputting and outputting electric signals may be relatively small, while the diameter of the bump for applying a power supply voltage may be relatively large, and so on, resulting in a mixture of small and large diameter bumps.
[0006] When these bumps are formed by the above-mentioned two-layer plating, the large-diameter bumps are higher than the small-diameter bumps. In other words, in the process of plating the first and second metal layers, the small and large-diameter bumps are plated to the same thickness, so the volume of the second metal layer in the large-diameter bump is larger than the volume of the second metal layer in the small-diameter bump. Then, when these second metal layers are melted and solidified, the surface becomes spherical. In this state, the large-diameter bumps protrude higher than the small-diameter bumps.
[0007] When bumps of different heights are mixed, there is a problem that the connection reliability between the wiring board and the semiconductor chip is reduced. Specifically, in the case of small-diameter bumps with low height, the bump tops may not make sufficient contact with the electrodes of the semiconductor chip, resulting in open defects. In addition, in the case of large-diameter bumps with high height, the bump tops may be pressed and stretched laterally when the semiconductor chip is mounted, resulting in contact with neighboring bumps, resulting in short defects.
[0008] Such a decrease in connection reliability does not only occur when a semiconductor chip is mounted on a wiring board, but can also occur when other electronic components are mounted on the wiring board via a plurality of bumps.
[0009] The disclosed technology has been made in view of the above points, and has an object to provide a wiring board and a method for manufacturing a wiring board that can improve the connection reliability with electronic components. [Means for solving the problem]
[0010] In one aspect, the wiring board disclosed in the present application comprises a wiring layer, an insulating layer covering the wiring layer and having a first opening penetrating to the wiring layer and a second opening having a larger diameter than the first opening, a first metal layer formed in the first opening and the second opening and having a deeper recess in the second opening than the first opening, and a second metal layer formed on top of the first metal layer and a portion of which is accommodated in the recess of the first metal layer in the second opening. Effect of the Invention
[0011] According to one aspect of the wiring board and the method for manufacturing the wiring board disclosed in the present application, it is possible to improve the reliability of connection with electronic components. [Brief description of the drawings]
[0012] [Figure 1] FIG. 1 is a diagram showing a configuration of a wiring board according to an embodiment. [Diagram 2] FIG. 2 is a flow diagram showing a method for manufacturing a semiconductor package according to an embodiment. [Diagram 3] FIG. 3 is a diagram showing a specific example of the formation of a core substrate. [Figure 4] FIG. 4 is a diagram showing a specific example of build-up. [Diagram 5] FIG. 5 is a diagram showing a specific example of the formation of a solder resist layer. [Figure 6] FIG. 6 is a diagram showing a specific example of terminal formation. [Figure 7] FIG. 7 is a diagram showing a specific example of mounting a semiconductor chip. [Figure 8] FIG. 8 is a flow chart showing the terminal forming step. [Figure 9] FIG. 9 is a diagram showing openings in the solder resist layer. [Figure 10] FIG. 10 is a diagram illustrating the formation of a seed layer. [Figure 11]FIG. 11 is a diagram illustrating patterning. [Figure 12] FIG. 12 is a diagram illustrating the formation of the first metal layer. [Figure 13] FIG. 13 is a diagram illustrating the formation of the second metal layer. [Figure 14] FIG. 14 is a diagram illustrating lamination. [Figure 15] FIG. 15 is a diagram illustrating polishing. [Figure 16] FIG. 16 is a diagram illustrating resist peeling. [Figure 17] FIG. 17 is a diagram for explaining the reflow. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS Hereinafter, preferred embodiments of a wiring board and a method for manufacturing a wiring board according to the present invention will be described in detail with reference to the accompanying drawings. Note that the present invention is not limited to the preferred embodiments.
[0014] Fig. 1 is a diagram showing a configuration of a wiring board 100 according to an embodiment. Fig. 1 shows a schematic cross section of the wiring board 100. The wiring board 100 shown in Fig. 1 can be used, for example, as a substrate for a semiconductor package on which a semiconductor chip is mounted.
[0015] The wiring board 100 has a layered structure, and includes a core substrate 110, a multilayer wiring structure 120, and solder resist layers 130 and 140. In the following description, the solder resist layer 140 is the bottom layer and the solder resist layer 130 is the top layer as shown in Fig. 1, but the wiring board 100 may be used, for example, upside down, or in any position.
[0016] Core substrate 110 has wiring layers 113 formed by plating on both sides of base material 111, which is a plate-like insulator. The wiring layers 113 on both sides are connected by vias 112 as necessary.
[0017] The multilayer wiring structure 120 is formed by stacking layers including an insulating layer 121 and a conductive wiring layer 122. In Fig. 1, two layers are stacked in the multilayer wiring structure 120 above the core substrate 110, and two layers are stacked in the multilayer wiring structure 120 below the core substrate 110, but the number of stacked layers may be one layer or three or more layers.
[0018] The solder resist layer 130 is a layer that covers the wiring layer 122 on the surface of the multilayer wiring structure 120 and protects the wiring. The solder resist layer 130 is a layer made of an insulating photosensitive resin such as an acrylic resin or a polyimide resin, and is one of the insulating layers. The solder resist layer 130 may be formed using an insulating non-photosensitive resin such as an epoxy resin.
[0019] The solder resist layer 130 side of the wiring board 100 is a surface on which electronic components such as semiconductor chips are mounted. At the position where the semiconductor chip is mounted, openings 131 and 132 are drilled in the solder resist layer 130. That is, the openings 131 and 132 are provided in the solder resist layer 130 to connect the electrodes of the semiconductor chip to the wiring layer 122 of the multilayer wiring structure 120. The openings 131 and 132 have different diameters, and the opening 132 has a larger diameter than the opening 131. When the solder resist layer 130 is formed using a photosensitive resin, the openings 131 and 132 can be formed by exposure and development. When the solder resist layer 130 is formed using a non-photosensitive resin, the openings 131 and 132 can be formed by laser processing.
[0020] Bumps 150, 160, which are connection terminals that connect wiring layer 122 of multilayer wiring structure 120 to electrodes of a semiconductor chip, are formed in openings 131, 132. Since openings 131, 132 have different diameters, bumps 150, 160 also have different diameters. That is, small-diameter bump 150 is formed in small-diameter opening 131, and large-diameter bump 160 is formed in large-diameter opening 132.
[0021] The bumps 150 and 160 have a two-layer structure of two different kinds of metals. Specifically, the bump 150 has a first metal layer 151 of, for example, copper and a second metal layer 152 of, for example, tin, and a layer of, for example, nickel is interposed between the bonding surface of the first metal layer 151 and the second metal layer 152. In the small-diameter bump 150, the upper surface of the first metal layer 151 is flat, and the second metal layer 152 protrudes upward in a spherical shape from the flat upper surface. On the other hand, the bump 160 also has a first metal layer 161 of, for example, copper and a second metal layer 162 of, for example, tin, and a layer of, for example, nickel is interposed between the bonding surface of the first metal layer 161 and the second metal layer 162. In the large diameter bump 160, a recess is formed in the center of the upper surface of the first metal layer 161, the center of the upper surface of the first metal layer 161 is lower than the surrounding area, and the second metal layer 162 protrudes upward in a spherical shape from this upper surface.
[0022] Since the bump 160 has a larger diameter than the bump 150, the second metal layer 162 has a larger volume than the second metal layer 152, but a part of the second metal layer 162 is stored in a recess formed in the first metal layer 161. Therefore, the height of the top of the second metal layer 162 from the surface of the solder resist layer 130 is lower. Furthermore, the height of the periphery of the recess on the top surface of the first metal layer 161 is lower than the height of the top surface of the first metal layer 151. In other words, the bottom surface of the second metal layer 162 is located lower than the bottom surface of the second metal layer 152. Therefore, even if the second metal layer 162, which has a larger volume than the second metal layer 152, protrudes upward significantly, the top of the bump 150 and the top of the bump 160 are equal in height. Then, for example, when a semiconductor chip is mounted above the bumps 150 and 160, the tops of the bumps 150 and 160 are reliably in contact with the electrodes of the semiconductor chip, and the connection reliability can be improved.
[0023] The solder resist layer 140, like the solder resist layer 130, is a layer that covers the wiring layer 122 on the surface of the multilayer wiring structure 120 and protects the wiring. The solder resist layer 140 is a layer made of an insulating photosensitive resin such as an acrylic resin or a polyimide resin, and is one of the insulating layers. The solder resist layer 140 may be formed using an insulating non-photosensitive resin such as an epoxy resin.
[0024] The solder resist layer 140 side of the wiring board 100 is the surface to be connected to external components and devices. At the positions where external connection terminals for electrically connecting to external components and devices are to be formed, openings 141 are formed in the solder resist layer 140, and the wiring layer 122 of the multilayer wiring structure 120 is exposed through the openings 141. External connection terminals such as solder balls are formed in the openings 141. When the solder resist layer 140 is formed using a photosensitive resin, the openings 141 can be formed by exposure and development. When the solder resist layer 140 is formed using a non-photosensitive resin, the openings 141 can be formed by laser processing.
[0025] Next, a method for manufacturing a semiconductor package having wiring substrate 100 configured as described above will be described with reference to a specific example and a flow chart of FIG.
[0026] First, a core substrate 110 that becomes a support member of the wiring substrate 100 is formed (step S101). Specifically, as shown in FIG. 3, for example, vias 112 that penetrate the substrate 111, which is a plate-shaped insulator, are formed, and wiring layers 113 of metal such as copper are formed on both sides of the substrate 111 by, for example, copper foil or copper plating. The wiring layers 113 on both sides of the substrate 111 are connected by vias 112 formed by plating of metal such as copper, as necessary. As the substrate 111, for example, a reinforcing material such as glass woven fabric impregnated with insulating resin such as epoxy resin can be used. As the reinforcing material, glass nonwoven fabric, aramid woven fabric, aramid nonwoven fabric, etc. can be used in addition to glass woven fabric. As the insulating resin, polyimide resin, cyanate resin, etc. can be used in addition to epoxy resin.
[0027] Then, the multilayer wiring structure 120 is formed on the upper and lower surfaces of the core substrate 110 by a build-up method (step S102). Specifically, as shown in Fig. 4, for example, an insulating layer 121 is formed on the upper and lower surfaces of the core substrate 110, and a wiring layer 122 is formed on the surface of the insulating layer 121. The insulating layer 121 is formed using an insulating resin such as an epoxy resin or a polyimide resin. The wiring layer 122 is formed by plating a metal such as copper.
[0028] Between wiring layer 113 and wiring layer 122 of core substrate 110, or between wiring layers 122 of adjacent layers, vias 123 formed by plating with a metal such as copper are connected as necessary. Insulating layer 121 and wiring layer 122 may be laminated in multiple layers on the upper and lower surfaces of core substrate 110, respectively.
[0029] When the multilayer wiring structure 120 is formed, the wiring layer 122 on the surface of the multilayer wiring structure 120 is covered with the solder resist layers 130 and 140 (step S103). For example, the wiring layer 122 on the surface of the multilayer wiring structure 120 laminated on the upper surface of the core substrate 110 is covered with the solder resist layer 130, and the wiring layer 122 on the surface of the multilayer wiring structure 120 laminated on the lower surface of the core substrate 110 is covered with the solder resist layer 140.
[0030] 5, openings 131 and 132 are formed in the solder resist layer 130 on the side on which the semiconductor chip is mounted at positions where connection terminals for the semiconductor chip are to be provided. At this time, the diameter of the opening 131 differs from the diameter of the opening 132 because the size of the connection terminals differs depending on the type of electrode of the semiconductor chip, for example. That is, the opening 131 where the connection terminal for inputting and outputting an electric signal is formed has a relatively small diameter, whereas the opening 132 where the connection terminal for applying a power supply voltage is formed has a relatively large diameter. At the bottom of the openings 131 and 132, the wiring layer 122 on the surface of the multilayer wiring structure 120 is exposed.
[0031] On the other hand, openings 141 are formed in the solder resist layer 140 on the side to be connected to external components or devices at positions where external connection terminals are to be provided. The wiring layer 122 on the surface of the multilayer wiring structure 120 is exposed at the bottom of the openings 141. When a photosensitive resin is used as the solder resist layers 130 and 140, the openings 131, 132, and 141 can be formed by exposure and development. When a non-photosensitive resin is used as the solder resist layers 130 and 140, the openings 131, 132, and 141 can be formed by laser processing.
[0032] Then, connection terminals for connecting a semiconductor chip are formed in the openings 131, 132 of the solder resist layer 130 (step S104). That is, for example, as shown in Fig. 6, a small-diameter bump 150 is formed in the opening 131, and a large-diameter bump 160 is formed in the opening 132. Both of the bumps 150, 160 have a two-layer structure, and second metal layers 152, 162 overlapping the first metal layers 151, 161 protrude upward in a spherical shape. Both of the first metal layers 151, 161 and the second metal layers 152, 162 are formed by plating.
[0033] The first metal layer 151 is formed by, for example, copper plating the opening 131 and its periphery, filling the inside of the opening 131 and forming a flat upper surface above the opening 131. That is, the upper surface of the first metal layer 151 is a flat surface located farther from the wiring layer 122 than the upper surface of the solder resist layer 130. Then, the second metal layer 152 is formed by, for example, tin plating the flat upper surface of the first metal layer 151 via a nickel layer. The second metal layer 152 is melted and solidified by a reflow process, and protrudes upward in a spherical shape.
[0034] On the other hand, the first metal layer 161 is formed by, for example, copper plating the opening 132 and its periphery, and forms an upper surface having a recess in the center. The upper surface of the first metal layer 161 is formed farther from the wiring layer 122 around the recess than the upper surface of the solder resist layer 130. The openings 131 and 132 are simultaneously copper plated, but the first metal layers 151 and 161 are formed in different shapes in the small-diameter opening 131 and the large-diameter opening 132 by adjusting the composition of the copper sulfate plating solution used for plating and the electrolytic copper plating conditions. That is, the upper surface of the first metal layer 151 is flat, whereas the upper surface of the first metal layer 161 has a recess. Then, the second metal layer 162 is formed by, for example, tin plating via a nickel layer on the upper surface having the recess of the first metal layer 161. The second metal layer 162 is melted and solidified by going through a reflow process, and protrudes upward in a spherical shape.
[0035] Since a part of the second metal layer 162 is stored in the recess of the first metal layer 161, the height of the top of the second metal layer 162 is lower than when the second metal layer 162 is formed on a flat surface above the opening 132. Furthermore, the height of the periphery of the recess of the first metal layer 161 is lower than the height of the upper surface of the first metal layer 151. Therefore, the height of the top of the second metal layer 162 is lower than when the second metal layer 162 is formed on a surface at the same height as the upper surface of the first metal layer 151. From the above, even if the volume of the second metal layer 162 of the large diameter bump 160 is larger than the volume of the second metal layer 152 of the small diameter bump 150, the height from the surface of the solder resist layer 130 to the top of the bumps 150 and 160 is the same. The process of forming the bumps 150 and 160 will be described in detail later.
[0036] When the bumps 150 and 160 are formed on the solder resist layer 130 side, external connection terminals are formed on the solder resist layer 140 side (step S105). Then, a semiconductor chip is mounted on the solder resist layer 130 side (step S106), and the bumps 150 and 160 are connected to the electrodes of the semiconductor chip. Specifically, as shown in FIG. 7, for example, external connection terminals such as solder balls 170 are formed in the openings 141 of the solder resist layer 140. In addition, the semiconductor chip 200 is mounted above the bumps 150 and 160, and the electrodes 210 of the semiconductor chip 200 are bonded to the bumps 150 and the electrodes 220 are bonded to the bumps 160. At this time, the bumps 210a and 220a provided on the electrodes 210 and 220 of the semiconductor chip 200 and the bumps 150 and 160 are melted and solidified by reflow. Therefore, at the joints between the electrodes 210, 220 and the bumps 150, 160, the bumps 210a, 220a and the bumps 150, 160 are mixed together and melted and solidified.
[0037] The joints between the electrodes 210, 220 and the bumps 150, 160 are sealed with underfill resin 230 to form a semiconductor package in which the semiconductor chip 200 is mounted on the wiring substrate 100. The order of the step of forming the external connection terminals and the step of mounting the semiconductor chip may be reversed. That is, after the semiconductor chip 200 is mounted on the wiring substrate 100, external connection terminals such as solder balls 170 may be formed in the openings 141 of the solder resist layer 140.
[0038] Next, the process of forming the bumps 150, 160 which serve as connection terminals with the semiconductor chip 200 will be described more specifically with reference to the flow chart shown in FIG.
[0039] When the multilayer wiring structure 120 is laminated on the upper surface of the core substrate 110, the wiring layer 122 of the multilayer wiring structure 120 is covered with a solder resist layer 130. The solder resist layer 130 is provided with openings 131 and 132, as shown in FIG. 9 for example. The opening 132 has a larger diameter than the opening 131, and the wiring layer 122 is exposed at the bottom of each of the openings 131 and 132. The opening diameter of the opening 131 is, for example, about 20 to 30 μm, and the depth is, for example, about 13 to 23 μm. The opening diameter of the opening 132 is, for example, about 30 to 40 μm, and the same depth as the opening 131 is, for example, about 13 to 23 μm.
[0040] In this state, a seed layer is formed on the surface of the solder resist layer 130 (step S201). That is, as shown in Fig. 10, for example, a seed layer 301 is formed on the entire surface of the surface of the solder resist layer 130 and the wiring layer 122 exposed in the openings 131, 132 by, for example, electroless copper plating or copper sputtering. The thickness of the seed layer 301 is, for example, about 0.40 to 0.60 µm, and it can be formed by, for example, performing electroless copper plating at a bath temperature of 34 ± 2°C for 15 minutes.
[0041] Then, patterning is performed to form a circuit pattern on the surface of the wiring board 100 (step S202). Specifically, for example, as shown in Fig. 11, dry film resist 302 is attached to the surface of the wiring board 100, and then the circuit pattern is exposed and developed, and the dry film resist is removed from the wiring portion including the openings 131 and 132. The opening diameter of the dry film resist 302 around the opening 131 is, for example, about 27 to 47 µm, and the opening diameter of the dry film resist 302 around the opening 132 is, for example, about 60 to 80 µm. The thickness of the dry film resist 302 is, for example, about 30 to 40 µm.
[0042] Then, for example, copper plating is applied to form first metal layers 151, 161 in openings 131, 132 (step S203). At this time, the composition of a copper sulfate plating solution used for copper plating is, for example, as follows. Copper sulfate: 100~200g / L Sulfuric acid: 100~200g / L Chloride ions: 1~20ppm Polymer (inhibitor): 1~10mL / L Brightener: 1.0~5.0mL / L Leveler: 0.1~3.0mL / L
[0043] As the polymer (inhibitor), for example, a nonionic surfactant such as polyethylene glycol (polyether compound) can be used, as the brightener (accelerator), for example, an organic sulfur compound such as bis(3-sulfopropyl) disulfide can be used, and as the leveler, for example, a quaternary amine compound can be used.
[0044] With the copper sulfate plating solution having the above composition, for example, the current density is set to 0.1 to 1.0 ASD (A / dm 2 ) and copper plating is performed under electrolytic copper plating conditions of plating time of 40 to 80 minutes. As a result, for example as shown in Fig. 12, a first metal layer 151 having a flat upper surface is formed in the small diameter opening 131, and a first metal layer 161 having a recess 161a in the center is formed in the large diameter opening 132. The bottom surface of the recess 161a of the first metal layer 161 is curved, and the deepest part is located below the upper surface of the solder resist layer 130. In other words, the recess 161a has a bottom surface that is closer to the wiring layer 122 than the surface of the solder resist layer 130.
[0045] Furthermore, the thickness a of first metal layer 151 from the upper surface of solder resist layer 130 to the upper surface of first metal layer 151 is, for example, about 5 to 15 μm, whereas the thickness b of first metal layer 161 from the upper surface of solder resist layer 130 to the upper surface of first metal layer 161 is, for example, about 3 to 12 μm, making first metal layer 161 thinner than first metal layer 151. The reason why first metal layer 161 is formed in large-diameter opening 132 in this manner and is thinner than first metal layer 151 and has recesses 161a is as follows.
[0046] That is, the polymer that suppresses the plating deposition action is less likely to be adsorbed in the openings 131 and 132 than around the openings 131 and 132. On the other hand, the brightener that promotes the plating deposition action is uniformly adsorbed around the openings 131 and 132 and inside the openings 131 and 132. As a result, the amount of plating deposition in the openings 131 and 132 is greater than that around the openings 131 and 132, and for example, in the opening 131, a first metal layer 151 that fills the opening 131 is formed. Also, in the opening 132, the amount of plating deposition in the opening 132 is greater than that around the opening 132, and a first metal layer 161 that is thicker in the opening 132 than around the opening 132 is formed.
[0047] Incidentally, since the opening 131 has a small diameter and the opening 132 has a large diameter, the amount of polymer adsorbed is greater in the opening 132 than in the opening 131. Therefore, the plating deposition action is more strongly suppressed in the opening 132 than in the opening 131, and the first metal layer 161 becomes thinner than the first metal layer 151. At the same time, since the plating deposition action is more strongly suppressed near the center of the opening 132 than in the opening 131, the upper surface of the first metal layer 151 becomes flat, whereas a recess 161a is formed in the center of the first metal layer 161. Note that the upper surface of the first metal layer 151 does not necessarily have to be flat, and a recess may also be formed in the center of the first metal layer 151, but this recess is shallower than the recess 161a. This is because the plating deposition action is more strongly suppressed in the opening 132 than in the opening 131, and the recess formed in the center becomes deeper.
[0048] Furthermore, the thickness of first metal layer 161 around opening 132 is thinner than the thickness of first metal layer 151 around opening 131. Therefore, the height from the surface of solder resist layer 130 to the upper surface of first metal layer 161 is lower than the height from the surface of solder resist layer 130 to the upper surface of first metal layer 151. This means that the surface on which second metal layer 162 is formed is lower than the surface on which second metal layer 152 is formed.
[0049] After the first metal layers 151, 161 are formed by copper plating, the second metal layers 152, 162 are formed in the openings 131, 132 by, for example, tin plating (step S204). At this time, for example, as shown in FIG. 13, nickel layers 303, 304 may be interposed between the first metal layers 151, 161 and the second metal layers 152, 162. The nickel layers 303, 304 are formed to a uniform thickness along the surfaces of the first metal layers 151, 161. By interposing the nickel layers 303, 304, it is possible to prevent the copper of the first metal layers 151, 161 from dissolving or diffusing into the tin of the second metal layers 152, 162. The nickel layers 303, 304 have a thickness of, for example, about 1 to 5 μm, and can be formed by applying nickel plating under electrolytic nickel plating conditions, for example, a current density of 1.0 ASD and a plating time of 17.2 minutes. In addition, in order to prevent dissolution and diffusion of copper from the first metal layers 151, 161, a layer of a metal other than nickel having a higher melting point than the metal of the second metal layers 152, 162 may be interposed between the first metal layers 151, 161 and the second metal layers 152, 162.
[0050] In forming the second metal layers 152 and 162, plating of a uniform thickness is applied in the openings 131 and 132. Therefore, the upper surface of the second metal layer 152 is flat like the upper surface of the first metal layer 151, and the upper surface of the second metal layer 162 has a recess 162a like the upper surface of the first metal layer 161. The thickness of the second metal layers 152 and 162 is, for example, about 10 to 20 μm, and can be formed by applying tin plating under electrolytic tin plating conditions of, for example, a current density of 1.5 ASD and a plating time of 23.3 minutes. The second metal layers 152 and 162 may be formed using various solder metals other than tin, such as a tin-silver alloy, a tin-silver-copper alloy, and a tin-bismuth alloy. The thickness of the second metal layers 152 and 162 is uniform, but the opening 132 has a larger diameter than the opening 131, so the second metal layer 162 has a larger volume than the second metal layer 152.
[0051] After the second metal layers 152 and 162 are formed, the entire surface is laminated with a water-soluble resist 305 such as a dry film resist (step S205), as shown in Fig. 14. The water-soluble resist 305 is also filled into the recesses 162a of the second metal layer 162, and prevents the metal (e.g., tin) around the recesses 162a from flowing into the recesses 162a and deforming the recesses 162a.
[0052] Then, the entire surface of the water-soluble resist 305 is polished (step S206), and the second metal layer 152 is exposed, as shown in FIG. 15, and the second metal layer 162 is exposed around the recess 162a. The recess 162a is filled with the water-soluble resist 305, and the shape of the recess 162a is maintained. In the polishing process, the second metal layers 152 and 162 are also polished, and the polishing is completed when the volume of the remaining second metal layers 152 and 162 becomes an appropriate size. For example, the second metal layers 152 and 162, the dry film resist 302, and the water-soluble resist 305 are polished until the height of the dry film resist 302 is reduced by about 10 to 15 μm.
[0053] Then, the dry film resist 302 and the water-soluble resist 305 are peeled off (step S207). For example, an alkaline peeling solution such as caustic soda or amine is used for the peeling off. Also, flash etching is performed to remove the seed layer 301 from the portion not plated. As a result, as shown in FIG. 16, for example, in the opening 131, the seed layer 301, the first metal layer 151, the nickel layer 303, and the second metal layer 152 are laminated, and a conductor portion protruding from the surface of the solder resist layer 130 is formed. In addition, in the opening 132, the seed layer 301, the first metal layer 161, the nickel layer 304, and the second metal layer 162 are laminated, and a conductor portion protruding from the surface of the solder resist layer 130 is formed. In the center of the second metal layer 162 in the opening 132, a recess 162a remains.
[0054] In this state, reflow is performed at a reflow temperature that melts the second metal layers 152, 162 (step S208). That is, the second metal layers 152, 162 are melted at a high temperature, and then cooled to solidify the second metal layers 152, 162. At this time, since the melting point of the metal (e.g., copper) forming the first metal layers 151, 161 is higher than the melting point of the metal (e.g., tin) forming the second metal layers 152, 162, the first metal layers 151, 161 do not melt, and only the second metal layers 152, 162 melt and solidify.
[0055] As a result, as shown in FIG. 17, the upper surfaces of the second metal layers 152 and 162 protrude in a spherical shape, forming the bumps 150 and 160. Here, a part of the second metal layer 162 is stored in the recess 161a formed in the first metal layer 161, and the upper surface of the first metal layer 161 is located lower than the upper surface of the first metal layer 151. Therefore, even if the volume of the second metal layer 162 is larger than that of the second metal layer 152, the tops of the second metal layers 152 and 162 are at the same height. That is, the height from the surface of the solder resist layer 130 to the tops of the bumps 150 and 160 is equal, for example, within a range of 25 to 35 μm. As a result, when the semiconductor chip 200 is mounted, the bumps 150 and 160 can be reliably contacted with the electrodes 210 and 220 of the semiconductor chip 200 to avoid open defects. Furthermore, only one of the tops of the bumps 150, 160 is not excessively pressed by the semiconductor chip 200 and stretched in the lateral direction, so that short circuit defects caused by adjacent bumps coming into contact with each other can be avoided.
[0056] As described above, according to the present embodiment, when forming a two-layered bump by plating in an opening of a solder resist layer of a wiring board, the composition of the plating solution and the electrolytic plating conditions are adjusted so that the larger the diameter of the opening, the deeper the recess formed in the center of the first metal layer. Also, the thinner the first metal layer is on the surface of the solder resist layer around the opening, the larger the diameter of the opening. In this way, when the second metal layer overlapping the first metal layer is melted and solidified, in the opening with a large diameter, a part of the second metal layer is stored in the recess of the first metal layer, and the second metal layer is formed at a position with a low height from the surface of the solder resist layer. As a result, even if the diameters of the multiple openings are different and the volumes of the second metal layer are different, the heights from the surface of the solder resist layer to the tops of the bumps formed in each opening can be made equal, and the connection reliability with the electronic components connected to the bumps of the wiring board and mounted thereon can be improved. [Explanation of symbols]
[0057] 100 Wiring board 110 Core Board 111 Base material 112 Via 113, 122 wiring layer 120 Multilayer wiring structure 121 Insulating layer 130, 140 Solder resist layer 131, 132, 141 Openings 150, 160 Bump 151, 161 1st metal layer 152, 162 2nd metal layer 161a, 162a Recess 170 solder balls
Claims
1. A wiring layer; an insulating layer covering the wiring layer and including a first opening penetrating to the wiring layer and a second opening having a larger diameter than the first opening; a first metal layer formed in the first opening and the second opening, the first metal layer having a deeper recess in the second opening than in the first opening; a second metal layer formed on the first metal layer and a portion of the second metal layer being received in the recess of the first metal layer in the second opening; a third metal layer interposed between the first metal layer and the second metal layer, having a melting point higher than that of the second metal layer, formed in a layer shape along the surface of the first metal layer, and a portion of which is accommodated in a recess of the first metal layer in the second opening; having a first connection terminal is formed by the first metal layer, the second metal layer, and the third metal layer in the first opening, a second connection terminal having a larger diameter than the first connection terminal is formed by the first metal layer, the second metal layer, and the third metal layer in the second opening, The height from the surface of the insulating layer to the tops of the first connection terminal and the second connection terminal is set to be within a predetermined range. A wiring board comprising:
2. The first metal layer is 2. The wiring board according to claim 1, wherein the second opening has a lower height from the insulating layer than the first opening.
3. The second metal layer is 2. The wiring board according to claim 1, wherein the surface farther from the first metal layer protrudes in a spherical shape.
4. The first metal layer is 2. The wiring board according to claim 1, further comprising a surface located farther from the wiring layer than a surface of the insulating layer.
5. The first metal layer is 2. The wiring board according to claim 1, wherein the first opening overlaps the second metal layer via a flat surface.
6. The recess of the first metal layer is the second opening has a bottom surface that is closer to the wiring layer than a surface of the insulating layer; 2. The wiring board according to claim 1, wherein the deepest part of the bottom surface is located below the surface of the insulating layer.
7. The first metal layer is 2. The wiring board according to claim 1, wherein the wiring board is made of a metal having a melting point higher than that of the metal forming the second metal layer.
8. The first metal layer is a first portion formed on the upper surface of the insulating layer in the first opening and around the first opening; a second portion formed on the upper surface of the insulating layer around the second opening; Including, A thickness of the first portion on the upper surface of the insulating layer around the first opening is greater than a thickness of the second portion on the upper surface of the insulating layer around the second opening.
2. The wiring board according to claim 1.
9. a diameter of the first connection terminal is larger than a diameter of the first opening, The diameter of the second connection terminal is larger than the diameter of the second opening.
2. The wiring board according to claim 1.
10. forming a wiring layer; forming an insulating layer that covers the wiring layer and has a first opening that penetrates to the wiring layer and a second opening that is larger in diameter than the first opening; forming a first metal layer in the first opening and the second opening, the first metal layer having a deeper recess in the second opening than in the first opening; forming a second metal layer overlying the first metal layer by plating; The second metal layer is melted and then solidified. The method includes the steps of: In the step of forming the second metal layer, a third metal layer is interposed between the first metal layer and the second metal layer, the third metal layer having a melting point higher than that of the second metal layer, the third metal layer being formed in a layer shape along the surface of the first metal layer, and a part of the third metal layer being stored in the recess of the first metal layer in the second opening; in a step of melting and then solidifying the second metal layer, a first connection terminal is formed by the first metal layer, the second metal layer, and the third metal layer in the first opening, and a second connection terminal having a larger diameter than the first connection terminal is formed by the first metal layer, the second metal layer, and the third metal layer in the second opening, The height from the surface of the insulating layer to the tops of the first connection terminal and the second connection terminal is set to be within a predetermined range.
4. A method for manufacturing a wiring board comprising the steps of:
11. filling a recess formed in the second metal layer by overlapping the recess in the first metal layer with a resist; polishing the second metal layer together with the resist; The resist remaining after polishing is stripped off.
11. The method for manufacturing a wiring board according to claim 10, further comprising the step of:
12. The recess of the first metal layer is the second opening has a bottom surface that is closer to the wiring layer than a surface of the insulating layer; 11. The method for manufacturing a wiring board according to claim 10, wherein the deepest part of the bottom surface is located below the surface of the insulating layer.
13. The first metal layer is a first portion formed on the upper surface of the insulating layer in the first opening and around the first opening; a second portion formed on the upper surface of the insulating layer around the second opening; Including, A thickness of the first portion on the upper surface of the insulating layer around the first opening is greater than a thickness of the second portion on the upper surface of the insulating layer around the second opening.
11. The method for manufacturing a wiring board according to claim 10.
14. a diameter of the first connection terminal is larger than a diameter of the first opening, The diameter of the second connection terminal is larger than the diameter of the second opening.
11. The method for manufacturing a wiring board according to claim 10.
Citation Information
Patent Citations
Flattening of wiring layers
JP1994053660A
Multilayered printed wiring board
JP1999261228A
Wiring board and manufacturing method thereof
JP2007103878A
Wiring board, semiconductor device and wiring board manufacturing method
JP2014107427A
Electronic component, electronic device and electronic apparatus
JP2017152646A