Power semiconductor device and manufacturing method
By using a molded body to directly attach the support to the heat sink, the power semiconductor devices improve thermal conductivity and mechanical stability, addressing thermal resistance issues and reducing costs associated with traditional attachment methods.
Patent Information
- Application Number
- JP2023551215
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-02-24
- Filing Date
- 2022-01-19
- Publication Date
- 2024-10-03
- Estimated Expiration
- 2042-01-19
AI Technical Summary
Existing power semiconductor devices face challenges in thermal management due to the use of connection methods like soldering, sintering, gluing, or screwing, which introduce thermal resistance and increase system costs.
The power semiconductor devices utilize a molded body made of electrically insulating material to directly press the support onto a heat sink, eliminating the need for additional attachment means and providing a direct thermal path without thermal interface materials, while also serving as a seal for coolant.
This approach enhances thermal conductivity and mechanical stability, reducing costs by eliminating the need for additional clamping, sealing, and bonding materials, and simplifying the manufacturing process.
Smart Images

Figure 0007561286000001 
Figure 0007561286000002 
Figure 0007561286000003
Abstract
Description
[Technical field]
[0001] A power semiconductor device and a method for manufacturing such a power semiconductor device are provided. [Background technology]
[0002] The document US Patent Application Publication No. 2018 / 0114740(A1) refers to a transistor package.
[0003] The document WO2018 / 202615A1 discloses a resin encapsulated power semiconductor module having exposed terminal areas.
[0004] The documents KR2003 0080900A, US Pat. No. 5,105,259(A), US Patent Application Publication No. 2014 / 0332951(A1), US Patent Application Publication No. 2015 / 0137344(A1), US Patent Application Publication No. 2005 / 0082690(A1) and EP 0577966 A1 refer to electrical devices. Summary of the Invention [Problem to be solved by the invention]
[0005] The problem to be solved is to provide a power semiconductor device with improved thermal behavior without using connection methods such as, for example, soldering, sintering, gluing or screwing. [Means for solving the problem]
[0006] This object is achieved, inter alia, by a power semiconductor device and by a method as defined in the independent patent claims. Exemplary further developments form the subject matter of the dependent claims.
[0007] For example, the power semiconductor device described herein comprises a support, a heat sink, and a molded body. The support is pressed directly onto the heat sink by the molded body, such that no additional means are needed to mount or hold the support on the heat sink. In this way, there may be a direct thermal path from the support to the heat sink without additional thermal resistance due to, for example, thermal paste, solder, or sinter joints.
[0008] In at least one embodiment, the power semiconductor device comprises at least one support, and at least one power semiconductor chip is arranged on the support top surface of the at least one support. Furthermore, the power semiconductor device includes a heat sink having a heat sink top surface, and at least one support is arranged on the heat sink top surface. A mold body of an electrically insulating material is in direct contact with the at least one support and with the heat sink. The mold body fixes and presses the at least one support onto the heat sink. Optionally, the mold body is the only component in the power semiconductor device adhesively bonded to the heat sink, and the at least one support is fixed to the heat sink with the mold body in a press-fit manner, and at least one recess is in the mold body from the mold body top surface facing away from the heat sink to the support top surface, and at least one electrical wiring passes through the at least one recess.
[0009] Power semiconductor devices are key components of inverters that generate heat during operation. Dissipating the heat is important for efficient operation of the inverter. For this purpose, supports carrying the power semiconductor chips are attached to heat sinks and air or liquid is often utilized as the cooling medium or coolant. Moreover, power semiconductor devices operate at high voltages. This requires efficient electrical isolation of the devices, typically by encapsulating the power device structure with silicone gel or with potting or molding compounds that are often epoxy-based.
[0010] An alternative possibility for fixing the support on the heat sink is to clamp the power semiconductor device to the heat sink using screws or the like and to apply a thermal interface material, TIM for short, in between to ensure proper thermal contact. To overcome the relatively low thermal conductivity of the TIM, it is possible to manufacture the power semiconductor device with an integrated cooling structure. Thus, the power semiconductor device needs to be attached, for example, by screws, and also needs to be sealed, for example, by a rubber gasket, to a cooler housing for utilizing liquid cooling.
[0011] That is, the use of a TIM limits the thermal path and thus the performance of the power semiconductor device, ultimately resulting in higher system costs. The use of an integral cooling structure requires an additional seal against the coolant liquid, adding the cost of additional components and process steps.
[0012] In the power semiconductor device described herein, an encapsulation material, i.e. a mold body, is also used to attach the support to the heat sink and possibly also as a sealing material. For this purpose, an open non-encapsulated power module, i.e. a support carrying a power semiconductor chip, is assembled on a heat sink, which may be an open or closed cooler. The assembly is performed, for example, by a pick-and-place process. Alignment features may optionally be used to precisely define the lateral position of the support on the heat sink. The support is then firmly pressed onto the heat sink during an encapsulation process, which is, for example, transfer molding or compression molding of at least one hard mold compound.
[0013] As a result, in addition to the mold body's purpose of electrical insulation, the mold body also serves as an encapsulant, securing the support onto the heat sink and permanently applying pressure to the support-heat sink interface. The heat sink can include features to maximize the bond strength to the mold compound to provide reliable and strong thermal and mechanical contact.
[0014] Hence, any costs associated with additional clamping, sealing, bonding materials and process steps may be saved by using the power semiconductor devices described herein.
[0015] In short, in the power semiconductor device described herein, the substrate of the power module, i.e., the support, is mechanically attached to the heat sink by means of an encapsulation material, i.e., a molded body, where no additional interconnection layers, such as solder or sintered layers or adhesives, are required between the substrate and the heat sink. The power module may comprise at least one electrically insulating substrate, at least one power semiconductor device, such as a MOSFET, an IGBT, or a diode, made of silicon or silicon carbide. The encapsulation material may be an epoxy-based molded component or a silicone-based molded compound. The encapsulation material is not directly in the thermal path between the power device and the heat sink. To maximize the mechanical strength of the connection between the support and the heat sink, anchoring features can be manufactured on the top surface of the heat sink, which may be, for example, a T-shaped cross section, an L-shaped cross section, or an angled groove, which is easy to manufacture, filled by the encapsulation material. Open or closed coolers may be used. The insulating support may comprise an integral cooling structure. In that case, the heat sink is an open cooler with at least one inlet and one outlet for the cooling medium and at least one opening per support in which the cooling structure of the support is at least partially immersed. In another embodiment, the heat sink is a closed cooler with at least one inlet and one outlet for the cooling medium and with integrated cooling structures such as fins and / or channels. In that case, the thermal contact between the substrate and the closed cooler may be improved by a thermal interface material or additional non-bonding material such as metal particles. Features may remain in the final structure that are required to achieve strong mechanical contact during the encapsulation process. Possible features may be, for example, insulating posts or exposed areas made by transfer or compression molding.
[0016] According to at least one embodiment, at least one support is provided with one or more power semiconductor chips. Hence, the support may be a substrate of a power semiconductor module. For example, the one or more power semiconductor chips of the power semiconductor device are configured for a voltage of at least 400V, or at least 650V, or at least 1.0kV, or at least 1.2kV, or at least 1.6kV. Additionally, the at least one power semiconductor chip may be configured for a current of at least 1A, or at least 10A, or at least 50A.
[0017] According to at least one embodiment, the at least one power semiconductor chip is selected from the following group: metal-oxide-semiconductor field effect transistor (MOSFET), metal-insulator-semiconductor field effect transistor (MISFET), insulated gate bipolar transistor (IGBT), bipolar junction transistor (BJT), thyristor, gate turn-off thyristor (GTO), gate commutated thyristor (GCT), junction gate field effect transistor (JFET), and diode. In case of multiple power semiconductor chips, all the semiconductor chips may be of the same type, or there are different types of semiconductor chips.
[0018] According to at least one embodiment, the top surface of the support is of a generally planar type. In other words, the support may be a parallel plate board. This does not include that the top surface of the support may be provided with conductor tracks structured in a metal layer on the top surface of the support.
[0019] According to at least one embodiment, the mold body is the only component adhesively bonded to or on the heat sink top surface in the power semiconductor device. For example, there may be no adhesive bond between the heat sink and the support, and the support may be directly attached to the heat sink top surface. It is possible that the only metallic and / or conductive connection between the support and the heat sink is through the support itself, so that no solder, sintered layer or conductive particles in the paste are used. Otherwise, there may be an intermediate layer between the heat sink and the support, which may be, for example, a TIM layer. With the intermediate layer, unevenness or roughness of the heat sink top surface and / or the support bottom surface may be filled in order to enhance the thermal contact between the heat sink and the support.
[0020] According to at least one embodiment, the at least one support is fixed to the heat sink by means of a mold body in a press-fit manner, in other words, by means of the mold body the support may be pressed very hard onto the heat sink such that lateral movement of the support relative to the heat sink is prevented by friction.
[0021] According to at least one embodiment, the heat sink top surface is of a flat type. That is, the heat sink top surface may not have any curvature. Moreover, the heat sink top surface may be smooth. For example, the average roughness, also called Ra, of the heat sink top surface is at least 0.5 μm or at most 10 μm or at most 5 μm. For example, the heat sink top surface is a polished surface. The same may be true for the substrate bottom surface that contacts the heat sink top surface. Otherwise, the heat sink top surface and / or the support bottom surface may have some roughness to improve thermal contact with or without additional intermediate layers such as paste or TIM.
[0022] According to at least one embodiment, a top view of the heat sink top surface is seen where the heat sink top surface protrudes from the mold body at least at certain locations or over the entire surface. For example, a top view of the heat sink top surface is seen where the mold body protrudes from the heat sink. Laterally, it is possible that the heat sink and the mold body may be terminated flush with one another.
[0023] Alternatively, the mold body can partially surround the heat sink such that the mold body may extend to the sides or bottom surface of the heat sink, said bottom surface being opposite the heat sink top surface.
[0024] According to at least one embodiment, the bottom surface of at least one support, opposite the respective top surface of the support, is a flat, continuous surface. The bottom surface of the support may be free of any curvature and may be a polished surface. For example, the bottom surface of the support is free of holes so that screws or the like cannot pass through the bottom surface of the support.
[0025] According to at least one embodiment, the mold body is attached to the heat sink using at least one form-locked joint. In other words, the mold body penetrates the heat sink top surface and the interlocking features in the heat sink are filled during the molding process. For example, the mold body includes one or more projections as form-locked joints that pass through the heat sink top surface and into the heat sink. Additionally or alternatively, the heat sink can include at least one projection as an anchoring element formed by molding the mold body at or around the anchoring element to achieve improved mechanical contact.
[0026] According to at least one embodiment, the form-locked joint comprises at least one of the following elements, seen in a cross section of the heat sink perpendicular to the heat sink top surface, but reaching into the heat sink: T-shaped anchoring elements, L-shaped anchoring elements, V-shaped protrusions, trapezoidal protrusions, rectangular protrusions. Hence, each protrusion may be relatively thin directly at the heat sink top surface and thicken inside the heat sink. Also, at least one roughening is possible as an anchoring structure. The same may apply to the protrusions of the heat sink and, consequently, to the recesses in the molded body.
[0027] Otherwise, the width of each protrusion may decrease monotonically or strictly monotonically along the direction inward of the heat sink, thus moving away from the support. "Form-locked" may mean that each protrusion of the mold body is in direct contact with the heat sink over its entire surface. There may be different types of protrusions in combination, or all of the protrusions may be of the same shape.
[0028] According to at least one embodiment, there are one or more recesses in the mold body, for example at least one recess extending from a top surface of the mold body facing away from the heat sink to a top surface of the support, such that the top surface of the support may be partially free of the mold body.
[0029] For example, as seen in a top view of the support upper surface, the at least one recess amounts to at most 20% or 10% of the area of the respective support upper surface. Hence, the at least one recess is only on a relatively small portion of the support upper surface. Other portions of the support upper surface that are not affected by the at least one recess are preferably covered by the mold body.
[0030] Although the at least one recess ends directly in the carrier top surface, as seen in a top view of the carrier top surface, it is not necessary that there is no material of the mould body on the carrier top surface in the area of the at least one recess, i.e. the at least one recess may also reach up to the at least one power semiconductor chip.
[0031] According to at least one embodiment, the power semiconductor device further comprises one or more pillars. The at least one pillar is partially or completely placed in the at least one recess. For example, the at least one pillar touches the support top surface or the at least one power semiconductor chip. The at least one pillar may terminate flush with the molded body top surface or may otherwise protrude from the molded body top surface in a direction away from the heat sink. Laterally, parallel to the support top surface, the at least one pillar may be in direct contact with the molded body over the entire surface. Hence, the molded body may be molded on the at least one pillar or vice versa.
[0032] For example, the at least one support post is made of a hard material, i.e. a material that is more rigid than the mold body. The at least one support post can be made of hard plastic or metal or ceramic. Otherwise, the at least one support post can be made of a soft material, i.e. a material that is less rigid than the mold body. In the latter case, the at least one mold body can be made of soft plastic, such as silicone resin or silicone rubber, in order to close the at least one recess.
[0033] Furthermore, it is possible that there are electrical wiring in at least one recess, through which at least one support may be electrically contacted, in which case, for electrical insulation purposes, the recess may be filled with an electrically insulating material, such as a silicone-based material.
[0034] According to at least one embodiment, the heat sink is an open cooler, so that the coolant supplied through the heat sink is configured to circulate in the support. That is, the support is supplied with coolant by the heat sink. For this reason, the support may be provided with at least one channel for the coolant. Otherwise, the coolant may flow directly at the bottom of the support but may not penetrate the support, or in the case of a closed cooler, the coolant may be restricted to the inside of the heat sink and / or may not be in direct contact with the support. For example, the coolant may be a gas such as air or a liquid such as water or oil.
[0035] According to at least one embodiment, the mold body provides a seal for the coolant. In other words, due to the mold body, there is no leakage of the coolant between the support and the heat sink, even if the coolant is in direct contact with the support. For example, the mold body is the only seal for the coolant at the support-heat sink interface. Hence, there is no need for additional gaskets or the like. In this respect, it is possible that the mold body may be fabricated in a multi-step molding process, for example using two steps with two different materials, one material for sealing and another material for insulation and mechanical strength.
[0036] According to at least one embodiment, the support comprises an electrically insulating body, which may be a part of the support that mechanically carries the support and thus the at least one power semiconductor chip. For example, the electrically insulating body is made of ceramic.
[0037] According to at least one embodiment, the electrically insulating body is provided with at least one metallization layer, for example, the electrically insulating body is placed between two metallization layers, such that the carrier top surface may be formed by one of the metallization layers and the carrier bottom surface may be formed by the other of the metallization layers.
[0038] According to at least one embodiment, the support is an insulated substrate, e.g., a direct bond copper substrate, an active metal brazing substrate, an insulated metal substrate, which includes a central electrically insulating body, e.g., made of a ceramic, such as Al2O3, SiN, or AlN, and at least one metallization layer on each major surface of the electrically insulating body. Hence, the support may be optimized for low thermal resistance between the heat sink and the at least one power semiconductor chip.
[0039] According to at least one embodiment, the electrically insulating body and / or at least one metallization layer comprises at least one fastener at a side of the support. The fastener may be of a small thickness compared to other parts of the respective support. The fastener may protrude into the mold body to enhance the mechanical connection between the mold body and the support. For example, the fastener comprises at least one protrusion and / or roughening towards the mold body.
[0040] According to at least one embodiment, the mold body is made of a relatively hard material, for example an epoxy mold compound, for example based on an epoxy resin, for example a polyaromatic or multifunctional resin, which contains a high content, for example at least 70% and / or at most 95%, of a filler material, for example silicon oxide, aluminum oxide or silicon nitride. For example, the mold body has a flexural modulus of at least 5 GPa or at least 10 GPa and / or at most 40 GPa or at most 30 GPa, for example at a temperature of 297 K. Alternatively or additionally, the mold body is made of a relatively soft material, for example based on a silicone resin, and has a flexural strength of at least 5 MPa or at least 10 MPa and / or at most 100 MPa or at most 70 MPa.
[0041] According to at least one embodiment, the support upper surface comprises or consists of at least one of Cu, Al and Ni. For example, the metallization layer forming the support upper surface is a copper layer. By using such a material, improved adhesion between the metallization layer and the mold body may be realized. It is also possible that a thin coating is applied on the metallization layer, such as a thick copper layer, to avoid, for example, an oxide layer that inhibits the electrical connection. In this context, "thin" can mean at most 1 μm, and "thick" can mean at least 10 μm.
[0042] According to at least one embodiment, the mold body comprises at least one filler. The filler may be made of an inorganic material such as silicon dioxide, aluminum oxide or silicon nitride. However, organic and inorganic fillers may be combined in the mold body. With the at least one filler, the thermal expansion coefficient, or CTE for short, of the mold body may be adapted to correspond to the CTE of the support and / or of the heat sink.
[0043] According to at least one embodiment, at least one filler is provided in the form of particles distributed in the mold body. For example, the particles are distributed in a uniform manner throughout the mold body. Otherwise, the filler or at least one of the fillers may be provided in a non-uniform manner, for example only near the support or with a certain gradient of mass fraction. In the case of multiple fillers, each type of particle may have different shapes and / or sizes.
[0044] According to at least one embodiment, the mass fraction of at least one filler, or of all fillers together, for the entire mold body is at least 20%, or at least 70%, or at least 80%. Alternatively or additionally, said mass fraction is at most 60%, or at most 90%, or at most 95%.
[0045] According to at least one embodiment, the edge length, such as the average edge length or maximum edge length, of at least one support parallel to the upper surface of the support, as viewed in a cross section perpendicular to the upper surface of the support, is at least 2 cm, or at least 3 cm, and / or at most 10 cm.
[0046] According to at least one embodiment, the thickness of the mold body, as seen in a cross section perpendicular to the upper surface of the support, is at least 0.2 cm or at least 0.3 cm and / or at most 2 cm or at most 1 cm. For example, the thickness of the mold body exceeds the thickness of the support by at least 2 times and / or by at most 10 times or at most 5 times.
[0047] According to at least one embodiment, the projected length of the mold body across the respective upper surface of the support, as viewed in a cross section perpendicular to the upper surface of the support, but parallel to the upper surface of the support, is at least 1 mm or at least 2 mm and / or at most 8 mm or at most 6 mm.
[0048] According to at least one embodiment, for example at a temperature of 297 K, the at least one support is pressed onto the heat sink top surface by the mold body with a pressure of at least 0.05 MPa or at least 0.2 MPa and / or at most 5 MPa or at most 2 MPa. The pressure may be an average pressure averaged over the entire bottom surface of the support. For example, the average pressure is the ratio of the force with which the support is pressed onto the heat sink due to the mold body and the area content of the bottom surface of the support.
[0049] According to at least one embodiment, the power semiconductor device comprises a plurality of supports. All supports may be arranged at a distance from each other on the heat sink top surface. In this way, adjacent supports may not touch each other. The supports may be arranged in a regular grid. For example, there are at least two or at least four supports and / or there are at most 64 or at most 16 supports.
[0050] According to at least one embodiment, all supports are located between the heat sink and the mold body, e.g., all supports only contact the heat sink and the mold body, not counting the optional at least one recess and the optional coolant.
[0051] A power semiconductor device is, for example, a power module that converts direct current from a battery into alternating current for an electric motor in a vehicle, such as, for example, a hybrid vehicle or a plug-in electric vehicle.
[0052] A method for manufacturing a power semiconductor device is additionally provided, by means of which the power semiconductor device is fabricated as indicated in relation to at least one of the above-mentioned embodiments. Features of the power semiconductor device are therefore further disclosed for the method and vice versa.
[0053] In at least one embodiment, a method for manufacturing a power semiconductor device includes, for example, in the order stated: A) providing a heat sink; B) placing at least one support directly on the top surface of the heat sink; C) pressing at least one support onto the heat sink and simultaneously forming a mold body on the at least one support and on the heat sink upper surface; Includes.
[0054] The power semiconductor device and method described herein will be described in greater detail below using exemplary embodiments with reference to the drawings. Elements that are the same in the different figures are indicated with the same reference numerals. The relationship between elements is not shown to scale, however, individual elements may be shown exaggeratedly large to aid in understanding. [Brief description of the drawings]
[0055] [Figure 1] 1 is a schematic cross-sectional view of an exemplary embodiment of a power semiconductor device as described herein; [Diagram 2] 1 is a schematic cross-sectional view of an exemplary embodiment of a power semiconductor device as described herein; [Diagram 3] 1 is a schematic cross-sectional view of an exemplary embodiment of a power semiconductor device as described herein; [Figure 4] FIG. 2 is a schematic top view of an exemplary embodiment of a power semiconductor device as described herein. [Diagram 5] FIG. 2 is a schematic top view of an exemplary embodiment of a power semiconductor device as described herein. [Figure 6] FIG. 2 is a schematic top view of an exemplary embodiment of a power semiconductor device as described herein. [Figure 7] FIG. 2 is a schematic block diagram of an exemplary embodiment of a method for manufacturing a power semiconductor device as described herein. [Figure 8] 1 is a schematic cross-sectional view of an exemplary embodiment of a power semiconductor device as described herein; [Figure 9] 1 is a schematic cross-sectional view of an exemplary embodiment of a power semiconductor device as described herein; DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0056] In Fig. 1 an exemplary embodiment of a power semiconductor device 1 is depicted. The power semiconductor device 1 comprises a heat sink 3 having a heat sink upper surface 30. The heat sink upper surface 30 is generally of a planar type. Furthermore, the power semiconductor device 1 comprises a support 2 which carries a power semiconductor chip 24. The support 2 with all components thereon, such as the power semiconductor chip 24, may also be referred to as a power module.
[0057] For example, the support 2 is a direct bonded copper substrate and consists of an electrically insulating body 22 having a metallization layer 21 on the support top surface 20 and on the support bottom surface 29. The support top surface 20 as well as the support bottom surface 29 are of a planar type, but optionally the metallization layer 21 on the support top surface 20 may be structured to include electrical contact areas and conductor tracks, not shown.
[0058] Moreover, the power semiconductor device 1 has a molded body 4 with a molded body top surface 40 facing away from the heat sink 3. The molded body 4, for example, seen in cross section, has a rectangular outline. The molded body 4 is in direct contact with the heat sink 3 and with the support 2. With the molded body 4, the support 2 is pressed and fixed directly onto the heat sink, so that no additional means are needed to fasten the support 2. The interface between the support 2 and the heat sink 3 is therefore devoid of any adhesive layer or thermal interface material, such as solder or glue. The pressure of the support bottom surface 29 on the heat sink top surface 30 caused by the molded body 4 is, for example, 1 MPa.
[0059] Optionally, the contact area between the molded body 4 and the heat sink 3 may be roughened 43 to improve adhesion. For example, the roughening 43 has an average roughness Ra of at least 10 μm or at least 30 μm and / or at most 0.3 mm or at most 0.1 mm. For example, the molded body 4 is made of epoxy resin and the metallization layer 21 is made of copper.
[0060] As a further option, the support 2 may have fasteners 23 on the sides to increase adhesion between the mold body 4 and the support 2. Apart from what is shown, such fasteners may also be present at the support top surface 20. Such fasteners 23 may be roughenings or at least one protrusion extending into the mold body 4. For example, the metallization layer 21 is recessed compared to the electrically insulating body 22.
[0061] There may be pillars 45 for pressing the support 2 onto the heat sink 3 during manufacture of the power semiconductor device 1. The pillars 45 may be applied onto the support 2 before the mold body 4 is fabricated. Hence, the molding material for the mold body 4 may be in direct contact with the pillars 45 over the entire surface.
[0062] For example, the pillars 4 may also be made of metal or an electrically insulating material such as a hard epoxy resin. After forming the molded body 4, the pillars 45 may remain within the power semiconductor device 1 and may protrude from the resin body 4. The pillars 45 may be manufactured by a prior molding process or may be made as a separate pre-fabricated part such as a separately molded plastic dowel.
[0063] Moreover, in Fig. 1 it is shown that the power semiconductor device 1 can be provided with electrical terminals 5 which penetrate the moulded body 4. As an option, the electrical terminals 5 may be used instead of or in addition to the posts 45 to press the support 2 onto the heat sink 3 during the manufacture of the moulded body 4. To this end, for example, the electrical terminals 5 may not penetrate the side of the moulded body as illustrated in Fig. 1, but may instead penetrate the top surface of the moulded body.
[0064] Another exemplary embodiment of the power semiconductor device 1 is illustrated in Fig. 2. According to Fig. 2, the heat sink 3 is a closed cooler, i.e. it comprises a channel 31, in which a gas or liquid is routed as a coolant 33 through the heat sink 3. Such a closed cooler may also be used in all other exemplary embodiments.
[0065] Moreover, in FIG. 2, the mold body 4 is optionally shown to be attached to the heat sink 3 in a form-locked manner, for example, using a form-locked joint 42 that is embedded during the molding process. The form-locked joint 42 consists of a T-shaped anchoring element that interlocks with the heat sink 2 and thus traverses the heat sink top surface 30. Other than as shown, the form-locked joint 42 can alternatively or additionally include an L-shaped anchoring element, a V-shaped protrusion, a trapezoidal protrusion, or a rectangular protrusion. Such features can facilitate strong bond strength between the support 2 and the heat sink 3.
[0066] Furthermore, according to Fig. 2 there is a recess 41 in the mold body 4 which reaches from the mold body top surface 40 to the support top surface 20. Instead of pressing onto the posts 45 of Fig. 1 it is also possible that features in the mold tool, not shown, press onto the support 2 during the molding process for the mold body 4. An exposed area will then remain on the support top surface 20 and the recess 41 is formed.
[0067] Optionally, the exposed areas may either be used to make auxiliary control contacts for attaching terminals and / or bus bars, or may be fully or partially filled with an encapsulation material in a subsequent process step, not shown. It may be beneficial to fill the recesses 41 with a soft encapsulation material to reduce distortion on the molded body 4. Hence, there may be at least one electrical trace 51 passing through at least one recess 41. Such an electrical trace 51 may also be present in all other exemplary embodiments.
[0068] For example, the thickness T of the mold body 4 is 6 mm and the thickness D of the support 2 from the support bottom surface 29 to the support top surface 20 is 2 mm. Hence, the mold body 4 may be three times thicker than the support 2.
[0069] Besides, the same may be true for FIG. 1 as well for FIG. According to Fig. 3, the mould body 4 may have sloping sides to simplify the removal of the mould tool. To improve the adhesion with the heat sink 3, there may be a number of V-shaped grooves in the heat sink 3 for form-locked joints 42 arranged, for example, in two rows. Such grooves can be easily manufactured in the heat sink 3.
[0070] Alternatively, the recess 41 may be filled with pillars 45 and have the shape of a truncated pyramid or a truncated cone. Hence, the recess 41 may narrow towards the support 2. As a further option, the pillars 45 may be used to electrically contact the support 2 and thus may act as electrical terminals 5. For this purpose, electrical contact areas may be formed on the moulded body top surface 40, not shown.
[0071] For example, the mold body 4 is composed of a matrix 44, such as an epoxy resin, and particles of a filler 46. The filler 46 is, for example, silicon dioxide. In contrast to what is shown in FIG. 3, it is possible for the filler 46 to be uniformly distributed throughout the entire mold body 4.
[0072] Furthermore, the heat sink 3 may be an open cooler. Hence, in contrast to what is illustrated in Fig. 2, the coolant 33 may come into intimate contact with the support 2. In a first variant, the channels 31 guide the coolant to the bottom surface 29 of the support such that it is guided over the entire bottom surface 29 of the support but does not enter the support 2. In a second variant, shown by dashed lines, there is an internal cooling structure 25 in the support 2 to guide the coolant 33 directly through the support 2.
[0073] The molded body 4 here also serves as a seal to avoid leakage of the coolant 33 from the interface between the support 2 and the heat sink 3, so that a dry contact may be maintained, e.g. a contact without additional adhesives such as solder, between the heat sink 3 and the support 2. Such a heat sink 3 may also be used in all other exemplary embodiments.
[0074] Otherwise, the same may be true for FIG. 3 as for FIG. 1 and FIG. 4 illustrates that the form-locked joint 42 may extend partially or even completely around the support 2 when viewed in top view. Optionally, the form-locked joint 42 may act as a sealing means when an optional coolant 33 is used. For example, the maximum edge length L of the support 2 is 55 mm and the projected length P of the mold body 4 beyond the support top surface 20 is 2 mm.
[0075] As an option, there may be alignment marks 35 which allow precise placement of the support 2 on the heat sink 3. This may also be true for all other exemplary embodiments.
[0076] Otherwise, the same may be true for FIG. 4 as for FIG. 1 to FIG. According to figure 5, the heat sink 3 and the support 2, seen in top view, are of square shape. Optionally, form-locked joints 42 are arranged over the entire surface of the support upper surface 20 in a regular grid.
[0077] Moreover, in FIG. 5 it is illustrated that the recess 41 does not necessarily have to be of a circular type, as in FIG. 4, but may also be of a rectangular shape, etc.
[0078] Both configurations, i.e., frame-like or line-like form-locked joints 42 as in FIG. 4 and point-like form-locked joints 42 as in FIG. 5, may further be used in combination in all exemplary embodiments, so that there may be at least one point-like form-locked joint 42 as well as at least one frame-like or line-like form-locked joint 42. Furthermore, if there are multiple point-like form-locked joints 42, these form-locked joints 42 may have different shapes seen in cross section. If there is at least one frame-like or line-like form-locked joint 42, it is possible that along each form-locked joint 42, the cross section may vary, for example, as seen in a top view, each form-locked joint 42 may narrow or widen and may look like a pearl necklace or a diamond line where the diamonds follow one another along a line. The same applies to all other exemplary embodiments.
[0079] Otherwise, the same as for Figures 1 to 4 may also apply to Figure 5, and vice versa.
[0080] 6 shows a plurality of supports 2 on a common heat sink 3. For example, the supports 2 are arranged in a regular grid. The projected length P may also be maintained between adjacent supports 2.
[0081] Moreover, the molded body 4 may comprise at least one reinforcing structure 47. For example, the reinforcing structure 47 is formed by a thickened portion of the molded body 4 protruding from the remaining part of the molded body top surface 40. It is possible that the reinforcing structure 47 is formed by a cross fixed at the corners of the molded body top surface 40, as seen in top view, or by a perpendicular straight line from one side to the other. With such a reinforcing structure 47, a more uniform pressure of the support 2 on the heat sink 3 may be achieved over the entire surface of the support bottom surface 29.
[0082] Optional recesses 41 may be located within or next to the reinforcement structure 47 in addition to those shown in Fig. 6. Moreover, as a further option, the recesses 41 may not be next to the power semiconductor chip 42 but may be above the power semiconductor chip 24.
[0083] Otherwise, the same may be true for FIG. 6 as for FIG. 1 to FIG. In Fig. 7 a method for producing a power semiconductor device 1 is simply illustrated. In method step S1 a heat sink 3 is provided. According to method step S2 a support 2 or a number of supports 2 are placed directly on the heat sink upper surface 30. In method step S3 at least one support 2 is pressed onto the heat sink 3 and at the same time a moulded body 4 is formed on the at least one support 2 and on the heat sink upper surface 30.
[0084] The mold body 4 is formed, for example, using one-stage or multi-stage compression molding or transfer molding or casting. It is possible that the mold body 4 is fabricated at an elevated temperature, which is significantly higher than the intended operating temperature of the power semiconductor device 1. Hence, when cooling from the fabrication temperature, the mold body 4 can be further pressed onto the support 2 due to thermal contraction of the mold body 4.
[0085] In the exemplary embodiment of Fig. 8, there is an intermediate layer 6 between the support 2 and the heat sink 3. For example, the intermediate layer 6 is made of a thermal interface material. It is possible that the intermediate layer 6 extends completely between the support 2 and the heat sink 3 and may even protrude beyond the support 2.
[0086] For example, with such an intermediate layer 6, the support bottom surface 29 may be intentionally roughened 7. As a further option, not shown in FIG. 8, such roughening 7 may additionally or instead be present on the heat sink top surface 30 to improve adhesion and anchoring between the mold body 4 and the heat sink 3.
[0087] As a further option, the anchoring structures for the form-locked joints 42 can be realized by protrusions from the heat sink top surface 30. The molded body 4 can be molded around these protrusions or, for example in the case of having prestressing, can be pre-molded and then pressed and fixed at the form-locked joints 42.
[0088] Moreover, if the mold body 4 is pre-formed before being applied onto the heat sink 3, the mold body 4 can optionally include a curved mold body top surface 40 seen in cross section, for example to better enable prestressing. Additionally, the heat sink 3 can be equipped with cooling fins.
[0089] Otherwise, the same as for Figures 1 to 7 may also apply to Figure 8, and vice versa.
[0090] According to Fig. 9, the support 2 consists of a base plate 27 and one or more substrates 26. The substrate may be made of a semiconductor material or even a wafer comprising at least one power semiconductor chip 24. The base plate 27 is, for example, a metal plate. There may be several base plates 27 other than the one shown in Fig. 9.
[0091] Further, according to Fig. 9, the mold body 4 is composed of a first part 4a and a second part 4b. For example, the first part 4a is made of a soft material such as silicone resin. With the first part 4a, an improved sealing for a coolant may be established, not shown in Fig. 9. The second part 4b is formed around the first part and may be made of a more rigid material than the first part 4a, for example, epoxy resin.
[0092] There can be multiple recesses in the heat sink top surface 30 for the form-locked joints 42. For example, there is one inner form-locked joint 42 for the first part 4a and one outer form-locked joint 42 for the second part 4b. These form-locked joints 42 can have different shapes. For example, the inner form-locked joint 42 completely surrounds the support 2 in top view, and the outer form-locked joint 42 can be of a multi-point type in top view, as illustrated in FIG. 5.
[0093] Otherwise, what is the same as in Figures 1 to 8 may also apply to Figure 8, and vice versa.
[0094] Components shown in the figures preferably follow one directly above the other in the order specified, unless otherwise indicated. Components that are not touching in the figures are preferably spaced apart from one another. Where lines are drawn parallel to one another, corresponding surfaces are preferably oriented parallel to one another. Similarly, unless otherwise indicated, the positions of the depicted components relative to one another are accurately reproduced in the figures.
[0095] The power semiconductor device described herein is not limited by the description given with reference to the exemplary embodiments, but rather includes any novel feature and any combination of features, including any combination of features specifically claimed, even if the novel feature or combination is not itself explicitly recited in the claims or exemplary embodiments.
[0096] This patent application claims priority to European Patent Application No. 21159002.1, the disclosure of which is incorporated herein by reference. [Explanation of symbols]
[0097] List of References 1. Power Semiconductor Devices 2 Support 20 Top surface of support 21 Metallization Layer 22 Electrically insulating body 23 Fasteners 24 Power Semiconductor Chips 25 Internal cooling structure 26 Substrate 27 Base Plate 29 Bottom of support 3. Heat sink 30 Heat sink top 31 Channels 33 Coolant 35 Alignment Mark 4 Molded body 4a First part of molded body 4b Second part of the molded body 40 Molded body top surface 41 Recess 42 Form Locked Join 43 Roughening 44 Base material 45 Post 46 Filler 47 Reinforcement structure 48 Common aspects 5 Electrical terminals 51 Electrical wiring 6. Middle Tier 7. Roughening D Thickness of the support L Edge length of the support P Projected length mold body-support top surface S. Method steps T Molded body thickness
Claims
1. A power semiconductor device (1), at least one support (2), on whose upper surface (20) at least one power semiconductor chip (24) is arranged, a heat sink (3) having a heat sink upper surface (30), said at least one support (2) being arranged on said heat sink upper surface (30); a moulded body (4) of electrically insulating material in direct contact with said at least one support (2) and with said heat sink (3); Equipped with said mold body (4) fastening and pressing said at least one support (2) onto said heat sink (3) so that said at least one support (2) is placed directly on said heat sink upper surface (30); - the moulded body (4) is the only component in the power semiconductor device (1) that is adhesively bonded to the heat sink (3), and the at least one support (2) is fixed to the heat sink (3) by means of the moulded body (4) in a press-fit manner, - there is at least one recess (41) in said mould body (4) extending from a mould body top surface (40) facing away from said heat sink (3) to said support top surface (20), and at least one electrical wiring (51) passing through said at least one recess (41), Power semiconductor device (1).
2. When viewed from above, the heat sink upper surface (30) protrudes from the mold body (4) over its entire surface. A power semiconductor device (1) according to claim 1.
3. the bottom surface (29) of the at least one support (2) is opposite to the respective top surface (20) of the support and is a flat, continuous surface; A power semiconductor device (1) according to claim 1 or 2.
4. The mold body (4) is attached to the heat sink (3) using at least one form-locked joint (42) such that the mold body (4) is recessed into the heat sink top surface (30) or the heat sink (3) is recessed into the mold body (4) bottom surface. A power semiconductor device (1) according to any one of the preceding claims.
5. The form-locked joint (42), when viewed in cross section of the heat sink (3), comprises at least one of the following elements extending into the heat sink (3): T-shaped anchoring element, L-shaped anchoring element, V-shaped projection, trapezoidal projection, rectangular projection, roughening (7). A power semiconductor device (1) according to claim 4.
6. said at least one support (2) is electrically contacted through said at least one recess (41), said at least one recess (41) being filled with an electrically insulating material; A power semiconductor device (1) according to any one of the preceding claims.
7. Further comprising at least one strut (45); the at least one post (45) is located in the at least one recess (41), touches the support top surface (20) and protrudes from the molded body top surface (40) in a direction away from the heat sink (3); A power semiconductor device (1) according to claim 6.
8. an open cooler in which the heat sink (3) is configured such that a coolant (33) supplied through the heat sink (3) circulates within the at least one support (2), The mold body (4) provides a seal for the coolant (33). A power semiconductor device (1) according to any one of the preceding claims.
9. said at least one support (2) comprises an electrically insulating body (22) between two metallization layers (21), said support upper surface (20) being formed by one of the metallization layers (21); A power semiconductor device (1) according to any one of the preceding claims.
10. the electrically insulating body (22) is provided with at least one fastener (23) at a side of the at least one support (2) protruding into the mold body (4); A power semiconductor device (1) according to claim 9.
11. The mold body (4) is made from at least one resin having a flexural modulus between 5 GPa and 30 GPa at a temperature of 297 K. A power semiconductor device (1) according to any one of the preceding claims.
12. the mould body (4) comprises at least one filler (46) which is an inorganic material and is provided in the form of particles dispersed within the mould body (4); the mass fraction of the at least one filler (46) in the entire mold body (4) is between 30% and 70%; A power semiconductor device (1) according to any one of the preceding claims.
13. the heat sink upper surface (30) is in direct contact only with the at least one support (2) and the mold body (4); A power semiconductor device (1) according to any one of the preceding claims.
14. A plurality of said at least one support (2), all of said at least one support (2) are arranged at a distance from each other on said heat sink upper surface (30) and are disposed between said heat sink (3) and said mold body (4); A power semiconductor device (1) according to any one of the preceding claims.
15. A method for manufacturing a power semiconductor device (1) according to any one of claims 1 to 14, comprising the steps of: A) providing said heat sink (3); B) placing said at least one support (2) directly on said heat sink upper surface (30); C) pressing said at least one support (2) onto said heat sink (3) and simultaneously forming said mold body (4) on said at least one support (2) and on said heat sink upper surface (30); A method comprising:
Citation Information
Patent Citations
Resin-sealed power semiconductor module
JP2007184315A
Power module structure
JP2009194212A
Power semiconductor module for preventing chip crackand for improving thermal resistance
KR1020030080900A
Method for producing semiconductor device and semiconductor device
US20050082690A1
Semiconductor device
US20140332951A1