package

The package design with a via electrode having specific dimensions and inverse taper angles addresses the challenge of forming fine electrodes while ensuring airtightness and preventing brazing material ingress, enhancing mechanical and electrical reliability.

JP7562767B2Active Publication Date: 2024-10-07NGK ELECTRONICS DEVICES INC +1
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
JP2023098406
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-08-09
Filing Date
2023-06-15
Publication Date
2024-10-07
Estimated Expiration
2043-06-15

AI Technical Summary

Technical Problem

Conventional methods struggle to form fine via electrodes in ceramic packages while ensuring airtightness and preventing brazing material from flowing into the cavity, especially as packages become smaller, leading to potential mechanical and electrical issues.

Method used

The package design includes a via electrode with specific dimensions and inverse taper angles, ensuring a larger ceramic interface area and maintaining a distance from the cavity to prevent brazing material ingress, while allowing for miniaturization.

Benefits of technology

This design effectively prevents brazing material from entering the cavity, maintains airtightness, and enhances mechanical and electrical reliability of the package, even as the frame dimensions shrink.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007562767000001
    Figure 0007562767000001
  • Figure 0007562767000002
    Figure 0007562767000002
  • Figure 0007562767000003
    Figure 0007562767000003
Patent Text Reader

Abstract

To provide a package which can prevent a brazing material from flowing into a cavity while ensuring airtightness.SOLUTION: A frame part 120 made of ceramic has a first surface SF1 and a second surface SF2. The second surface SF2 has: an inner edge surrounding a cavity CV; and an outer edge EO surrounding the inner edge. A substrate part 110 made of ceramic has a third surface SF3 which has: a portion supporting the second surface SF2 of the frame part 120; and a portion facing the cavity CV. An electrode layer 200 is provided on the third surface SF3 of the substrate part 110. A via electrode 510 has: an end surface SFA which has a diameter DA on the first surface SF1; and a bottom surface SFB which comes into contact with the electrode layer 200 and has a diameter DB on the second surface SF2. An inequality DA<DB is satisfied. In plan view, the bottom surface SFB of the via electrode has: a minimum dimension LI from the inner edge of the second surface SF2 of the frame part 120; and a minimum dimension LO from the outer edge EO of the second surface SF2 of the frame part 120. Here, an inequality LO>LI is satisfied.SELECTED DRAWING: Figure 11
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a package, and more particularly to a package having a frame portion penetrated by via electrodes. [Background technology]

[0002] Packages for quartz crystal resonators are known as ceramic components manufactured using ceramic green sheets. A typical quartz crystal resonator has a quartz crystal blank, a package having a cavity in which the quartz crystal blank is housed, and a lid for sealing the cavity. The package has a substrate portion that forms the bottom of the cavity, a frame portion that surrounds the cavity, and a metallized layer provided on the frame portion. The lid is joined to the metallized layer using brazing material, thereby ensuring the airtightness of the cavity.

[0003] The metallization layer on the frame of the package is usually electrically shorted to an electrode pad for ground potential. This electrical path can typically be secured through a via electrode penetrating the frame. However, as the size of the package decreases, the material width of the frame (the dimension between the inner edge and the outer edge of the frame) becomes smaller, and it becomes difficult to form a fine via electrode corresponding to this. Specifically, it becomes difficult to form a fine via hole for a fine via electrode in a green sheet that becomes the frame by firing. When a pin-shaped die is used as a typical method for forming a via hole, the mechanical strength of the pin is likely to be insufficient if the pin shape is made fine to make the via hole finer. Therefore, according to the technology disclosed in, for example, JP 2007-27592 A, a castellation electrode having a roughly crescent shape is provided on the inner wall surface of the frame instead of a via electrode.

[0004] When castellation electrodes are provided on the side walls of the cavity instead of via electrodes as in the technology of the above publication, electrodes having higher wettability to the brazing material than the ceramic frame section run vertically along the thickness direction of the inner wall of the cavity. Therefore, in the process of joining the lid using the brazing material, the brazing material is likely to flow into the cavity along the castellation electrodes. If the flowed brazing material comes into contact with the crystal blank, it may adversely affect the mechanical performance of the crystal unit. Such adverse effects on mechanical properties are of particular concern when the element mounted in the package is a crystal blank, but may also occur in the case of other piezoelectric elements. Furthermore, as long as the element mounted in the package is an electrical element, there is concern about adverse effects on electrical properties, such as unintended short circuits. Therefore, it is sometimes important to avoid the flow of the brazing material, and from that perspective, via electrodes are more suitable than castellation electrodes. Since there is such a demand even for small packages, a technology is desired that can form minute via holes for via electrodes in response to the small material width of the frame section.

[0005] Japanese Patent Application Laid-Open No. 2009-234074 discloses a method for forming a minute through hole as a via hole in a ceramic green sheet by laser processing technology. Specifically, a through hole with a diameter of 30 μm to 50 μm is formed in a ceramic green sheet with a thickness of 250 μm or less by using an ultraviolet laser. It is pointed out that when a through hole with a small diameter relative to the thickness is formed by laser processing, the through hole tends to have a tapered shape. In the above publication, the tapered shape of the through hole is considered to be problematic as it makes it difficult to fill the through hole with a conductive paste. Therefore, in the technology of the above publication, laser light irradiation conditions that can make the taper rate 60% or more are considered. Here, the taper rate is defined by the taper diameter ratio, and a taper rate of 100% means that the through hole does not have a tapered shape, and a smaller taper rate means a more rapid tapered shape. [Prior art documents] [Patent documents]

[0006] [Patent Document 1] JP 2007-27592 A [Patent Document 2] JP 2009-234074 A Summary of the Invention [Problem to be solved by the invention]

[0007] According to the study by the present inventors, when the above-mentioned laser processing technology is simply applied for the purpose of providing a via electrode on the frame of the package, it may be difficult to sufficiently ensure the airtightness of the cavity. This problem becomes more serious as the width of the material of the frame becomes smaller with the progress of miniaturization of the package. Therefore, from the viewpoint of ensuring airtightness, the above-mentioned castellation electrode may be more preferable. On the other hand, as described above, when the castellation electrode is provided, the flow of the brazing material into the cavity may become a problem. From the above, it is difficult to prevent the flow of the brazing material into the cavity while ensuring sufficient airtightness of the cavity with the conventional technology.

[0008] The present invention has been made to solve the above-mentioned problems, and its object is to provide a package that can prevent the flow of brazing material into the cavity while ensuring sufficient airtightness of the cavity. [Means for solving the problem]

[0009] Aspect 1 is a package provided with a cavity, comprising a frame portion made of ceramic. The frame portion has a first surface and a second surface opposite to the first surface in the thickness direction. The second surface has an inner edge surrounding the cavity and an outer edge surrounding the inner edge. The package further comprises a substrate portion made of ceramic. The substrate portion has a third surface having a portion that supports the second surface of the frame portion and a portion that faces the cavity. The package further comprises an electrode layer provided on the third surface of the substrate portion and a via electrode that penetrates the frame portion between the first surface and the second surface. The via electrode has an end face having a diameter DA at the first surface and a bottom face having a diameter DB that is in contact with the electrode layer at the second surface, and DA < DB is satisfied. In a plan view, the bottom face of the via electrode has a minimum dimension LI from the inner edge of the second surface of the frame portion and a minimum dimension LO from the outer edge of the second surface of the frame portion, and LO > LI is satisfied.

[0010] Aspect 2 is the package of Aspect 1, wherein the diameter DA is 50 μm or less.

[0011] Aspect 3 is the package of Aspect 1 or 2, wherein the minimum dimension between the inner edge and the outer edge of the second surface of the frame portion is 200 μm or less.

[0012] Aspect 4 is the package of any one of Aspects 1 to 3, wherein LO ≧ LI × 1.5 is satisfied.

[0013] Aspect 5 is the package of any one of Aspects 1 to 4, wherein the via electrode has a diameter of (DA + DB) / 2 or less at an intermediate position between the end face and the bottom face in the thickness direction.

[0014] Aspect 6 is the package of any one of Aspects 1 to 5, wherein the via electrode has a portion that extends in an inverted taper shape from the end face in the thickness direction.

[0015] A seventh aspect is the package of the sixth aspect, wherein the inverted tapered shape has a taper angle of 5 degrees or more.

[0016] Behavior 8 is a package according to any one of embodiments 1 to 7, wherein the via electrode has a portion extending in an inverted tapered shape from the end face toward the bottom face over a thickness greater than half the thickness of the frame portion.

[0017] Behavior 9 is a package of any one of embodiments 1 to 8, wherein the via electrode has a side surface connecting the end surface and the bottom surface, and the side surface has at least one bending point when viewed in a cross-section parallel to the thickness direction.

[0018] Example 10 is the package of Example 9, wherein the at least one flex point includes two flex points that bend in opposite directions.

[0019] Example 11 is a package of any one of Examples 1 to 10, wherein the frame has an outer wall surface connecting the first surface and the outer edge of the second surface, and the outer wall surface has an as-fired surface connected to the first surface and a fracture surface connected to the second surface.

[0020] Aspect 12 is a package according to any one of aspects 1 to 11, in which LI>0 is satisfied.

[0021] Example 13 is a package of any one of Examples 1 to 11, wherein the via electrode has an outer periphery on the second surface, and the outer periphery consists of an arc portion along a circular shape of diameter DB and a missing portion along part of the inner edge of the second surface of the frame portion.

[0022] A fourteenth aspect is the package of the thirteenth aspect, wherein the missing portion of the outer periphery of the via electrode has a convex shape extending inwardly from the bottom surface of the via electrode.

[0023] A fifteenth aspect is any one of the packages described in the first to fourteenth aspects, wherein the electrode layer is locally thickened in a portion contacting the bottom surface of the via electrode.

[0024] Behavior 16 is a package described in embodiments 1 to 15, wherein the second surface of the frame portion has a first region directly connected to the bottom surface of the via electrode and a second region connected to the bottom surface of the via electrode via the first region, the second region being perpendicular to the thickness direction, and the first region being inclined relative to the second region so that the thickness of the frame portion becomes smaller the closer it is to the bottom surface of the via electrode. Effect of the Invention

[0025] According to the first aspect, firstly, the bottom surface of the via electrode is arranged so that LO>LI is satisfied, and therefore, between the outer edge of the bottom surface of the via electrode and the outer edge of the second surface of the frame, the area where the lamination interface between the ceramics is arranged can be secured large. Here, the lamination interface between the ceramics has higher airtightness than the lamination interface between the metal and the ceramic. Therefore, it is possible to suppress the decrease in airtightness of the cavity caused by the leak along the lamination interface. Secondly, since the diameter DA of the end surface of the via electrode is smaller than the diameter DB of the bottom surface of the via electrode, even if the via electrode is located so close to the cavity that the bottom surface of the via electrode reaches the cavity, the end surface of the via electrode can be located away from the cavity. This prevents the side surface of the via electrode from being exposed to the cavity near the end surface of the via electrode. Therefore, it is possible to prevent the brazing material from flowing into the cavity due to the via electrode. From the above, it is possible to prevent the brazing material from flowing into the cavity while ensuring sufficient airtightness of the cavity.

[0026] According to the second aspect, the diameter DA of the via electrode is a minute dimension of 50 μm or less. This allows the width dimension of the frame to be made finer. As this miniaturization progresses, leakage along the lamination interface between the substrate part and the frame part becomes more likely to become a problem, but this problem is effectively suppressed for the reasons described above.

[0027] According to aspect 3, the minimum dimension between the inner edge and the outer edge of the second surface of the frame is 200 μm or less. As miniaturization advances, leakage along the lamination interface between the substrate and frame becomes more likely to become a problem, but this problem is effectively suppressed for the reasons described above.

[0028] According to the fourth aspect, LO≧LI×1.5 is satisfied, which makes it possible to more sufficiently suppress the decrease in airtightness of the cavity caused by leakage along the lamination interface between the substrate portion and the frame portion.

[0029] According to aspect 5, the via electrode has a diameter of (DA+DB) / 2 or less at a middle position between the end face and the bottom face in the thickness direction. This makes it possible to ensure a sufficient distance between the middle position of the via electrode and the outer wall surface of the frame. This makes it possible to improve the airtightness reliability between the via electrode and the frame.

[0030] According to the sixth aspect, the via electrode has a portion extending in an inverse tapered shape from the end face in the thickness direction. This makes it easier to ensure the distance between the end face of the via electrode and the cavity. This makes it possible to more sufficiently prevent the brazing material from flowing into the cavity due to the via electrode.

[0031] According to the seventh aspect, the inverse tapered shape extending from the end face of the via electrode has a taper angle of 5 degrees or more. This makes it easier to ensure the distance between the end face of the via electrode and the cavity. This makes it possible to more sufficiently prevent the brazing material from flowing into the cavity due to the via electrode.

[0032] According to the eighth aspect, the inverted tapered shape extending from the end face of the via electrode has a thickness equal to or more than half the thickness of the frame portion. This makes it easier to ensure the distance between the end face of the via electrode and the cavity. This makes it possible to more sufficiently prevent the brazing material from flowing into the cavity due to the via electrode.

[0033] According to the ninth aspect, the side surface of the via electrode has at least one bending point, which can suppress peeling between the side surface of the via electrode and the frame portion caused by sintering shrinkage during package production.

[0034] According to the tenth aspect, the side surface of the via electrode has two bending points that bend in opposite directions, which makes it possible to more sufficiently suppress peeling between the side surface of the via electrode and the frame portion caused by sintering shrinkage during package manufacturing.

[0035] According to the eleventh aspect, the outer wall surface of the frame has a fired surface connected to the first surface and a fractured surface connected to the second surface. The fractured surface is formed by a breaking process, and the distance between the outer edge of the second surface of the frame and the bottom surface of the via electrode may become small due to the influence of process variations. However, as described above, since LO>LI is satisfied, the distance is unlikely to become too small. Therefore, it is possible to prevent insufficient airtightness caused by the distance being too small.

[0036] According to the twelfth aspect, LI>0 is satisfied. This prevents the side surface of the via electrode from being exposed to the cavity even in the vicinity of the bottom surface of the via electrode. This makes it possible to more reliably prevent the brazing material from flowing into the cavity.

[0037] According to the thirteenth aspect, the outer periphery of the via electrode has a missing portion along a part of the inner edge of the second surface of the frame. This makes it easier to arrange the via electrode close to the cavity. Therefore, it is possible to more sufficiently suppress the decrease in airtightness of the cavity caused by leakage along the lamination interface between the substrate portion and the frame.

[0038] According to the fourteenth aspect, the missing portion of the outer periphery of the via electrode has a convex shape toward the inside of the bottom surface of the via electrode. This allows the via electrode to be disposed at the corner of the cavity. This makes it easier to ensure a large minimum dimension LO. This makes it possible to more sufficiently suppress the decrease in airtightness of the cavity caused by leakage along the lamination interface between the substrate portion and the frame portion.

[0039] According to the fifteenth aspect, the electrode layer is locally thickened at a portion in contact with the bottom surface of the via electrode. This allows the obtuse angle between the side surface of the via electrode and the second surface of the frame to be increased while roughly maintaining the configuration of the via electrode. This allows the thermal stress caused by the difference in thermal expansion between the via electrode, which is mainly made of metal, and the frame, which is made of ceramic, to be alleviated. This allows the cracks or peeling between the via electrode and the frame, which are caused by the thermal stress, to be prevented.

[0040] According to the sixteenth aspect, the second surface of the frame has a first region directly connected to the bottom surface of the via electrode and a second region connected to the bottom surface of the via electrode through the first region, the second region being perpendicular to the thickness direction, and the first region being inclined with respect to the second region such that the thickness of the frame becomes smaller as it approaches the bottom surface of the via electrode. This makes it possible to increase the obtuse angle between the side surface of the via electrode and the second surface of the frame while roughly maintaining the configuration of the via electrode. This makes it possible to alleviate thermal stress caused by the difference in thermal expansion between the via electrode mainly made of metal and the frame made of ceramic. This makes it possible to prevent cracks or peeling between the via electrode and the frame caused by thermal stress. [Brief description of the drawings]

[0041] [Figure 1] 1 is a plan view illustrating a schematic configuration of a quartz crystal resonator according to a first embodiment. [Diagram 2] FIG. 2 is a schematic cross-sectional view taken along line II-II in FIG. [Diagram 3] 2 is a plan view illustrating a schematic process of a method for manufacturing the quartz crystal resonator of FIG. 1. [Figure 4] FIG. 4 is a schematic cross-sectional view taken along line IV-IV in FIG. [Diagram 5] FIG. 2 is a plan view illustrating a schematic configuration of a package in the first embodiment. [Figure 6] FIG. 6 is a schematic cross-sectional view taken along line VI-VI in FIG. 5. [Figure 7] 6 is a plan view in which the metallized layer and the frame in FIG. 5 are omitted. [Figure 8] 8 is a plan view showing a schematic diagram of the substrate portion and via electrodes in FIG. 7, with package electrode pads indicated by dashed lines. FIG. [Figure 9] 6 is a plan view in which the metallized layer on the frame in FIG. 5 is omitted. [Figure 10] FIG. 10 is a partially enlarged view of FIG. [Figure 11] FIG. 6 is a schematic partial cross-sectional view taken along line XI-XI in FIG. 5. [Figure 12] 3 is a partial plan view roughly showing a configuration of a substrate green body in the method for manufacturing a package in the first embodiment. FIG. [Figure 13] 13 is a partial plan view that shows, in a simplified manner, a substrate portion and substrate via electrodes in the substrate green body shown in FIG. 12, with package electrode pads shown by dashed lines. FIG. [Figure 14] FIG. 14 is a schematic partial cross-sectional view taken along line XIV-XIV in FIGS. 12 and 13. [Figure 15] 3 is a partial cross-sectional view illustrating a schematic step of a method for manufacturing the package in the first embodiment. [Figure 16] 3 is a partial cross-sectional view illustrating a schematic step of a method for manufacturing the package in the first embodiment. [Figure 17] 3 is a partial cross-sectional view illustrating a schematic step of a method for manufacturing the package in the first embodiment. [Figure 18] 3 is a partial cross-sectional view illustrating a schematic step of a method for manufacturing the package in the first embodiment. [Figure 19] 3 is a partial cross-sectional view illustrating a schematic step of a method for manufacturing the package in the first embodiment. [Figure 20] 3 is a partial cross-sectional view illustrating a schematic step of a method for manufacturing the package in the first embodiment. [Figure 21] 3 is a partial cross-sectional view illustrating a schematic step of a method for manufacturing the package in the first embodiment. [Figure 22] 3 is a partial cross-sectional view illustrating a schematic step of a method for manufacturing the package in the first embodiment. [Figure 23] 12 is a partial cross-sectional view showing the configuration of a package of a first comparative example in the same field of view as in FIG. 11. [Figure 24] 12 is a partial cross-sectional view showing the configuration of a package of a second comparative example in the same field of view as in FIG. 11. [Diagram 25] 12 is a partial cross-sectional view showing a schematic view of a package configuration in a modified example of the first embodiment, taken in the same field of view as in FIG. 11. [Figure 26] 11 is a partial plan view roughly showing the configuration of a package in a modified example of the first embodiment in the same field of view as in FIG. 10. [Figure 27] 27 is a plan view illustrating the configuration of the bottom surface of a via electrode of the package of FIG. 26. [Figure 28] 12 is a diagram for explaining details of the configuration of the via electrode shown in FIG. 11. FIG. [Figure 29] 11 is a diagram for explaining details of the configuration of via electrodes included in a package according to a second embodiment of the present invention. FIG. [Diagram 30] 13 is a diagram for explaining details of the configuration of via electrodes included in a package according to a third embodiment of the present invention. FIG. [Diagram 31] 10 is a partial plan view showing a schematic view of a package configuration according to a fourth embodiment, in the same field of view as in FIG. 10 of the first embodiment. [Diagram 32] FIG. 32 is a schematic partial cross-sectional view taken along line XXXII-XXXII in FIG. 31. [Diagram 33] 8 is a partial plan view generally illustrating the configuration of a package in a fourth embodiment, in the same field of view as in FIG. 7 of the first embodiment. FIG. [Diagram 34]17 in the first embodiment, in a method of manufacturing a package according to the fourth embodiment. FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0042] Hereinafter, an embodiment of the present invention will be described based on the drawings. In some drawings, an xyz orthogonal coordinate system is shown to facilitate understanding of the directions, and the z direction corresponds to the thickness direction. In this specification, the terms "tapered shape" and "reverse taper shape" have different meanings. When a certain direction is defined, a "tapered shape" extending in the direction is a shape that gradually narrows toward the direction, for example, a shape in which the diameter gradually decreases toward the direction. On the other hand, an "reverse taper shape" extending in the direction is a shape that gradually narrows toward the opposite direction to the direction, for example, a shape in which the diameter gradually decreases toward the opposite direction to the direction. In other words, an "reverse taper shape" extending in the direction is a shape that gradually widens toward the direction, for example, a shape in which the diameter gradually increases toward the direction.

[0043] <Embodiment 1> Fig. 1 is a plan view that shows a schematic configuration of a quartz crystal resonator 900 (electrical component) in the first embodiment. Fig. 2 is a schematic cross-sectional view taken along line II-II in Fig. 1. Fig. 3 is a plan view that shows a schematic configuration immediately after mounting a quartz crystal blank 890 (electrical element) in a manufacturing method of the quartz crystal resonator 900 (Fig. 1). Fig. 4 is a schematic cross-sectional view taken along line IV-IV in Fig. 3.

[0044] The crystal unit 900 includes a package 701, a crystal blank 890, a brazing material 960, and a lid 980. The package 701 is provided with a cavity CV. The crystal blank 890 is housed in the cavity CV and is mounted on the element electrode pads 211 and 212 of the package 701. The lid 980 is joined to the metallization layer 600 of the package 701 by the brazing material 960, thereby sealing the cavity CV. The brazing material 960 is typically preferably made of an alloy containing gold, for example, an alloy containing gold and tin, in other words, an Au-Sn alloy. The lid 980 is made of a metal, for example, an alloy containing iron and nickel. In this specification, an alloy is considered to be a type of metal.

[0045] The metallization layer 600 is made of, for example, a metal containing at least one of molybdenum and tungsten. A plating layer, typically a gold plating layer, may be provided on the surface of the metallization layer 600 (the surface facing the brazing material 960). A nickel plating layer may be provided as a base for the gold plating layer. In this embodiment, the metallization layer 600 provided directly on the frame upper surface SF1 of the frame portion 120 of the package 701 and the lid 980 are joined together only by the brazing material 960.

[0046] Fig. 5 is a plan view that shows a schematic configuration of a package 701. Fig. 6 is a schematic cross-sectional view along line VI-VI in Fig. 5. The package 701 has a ceramic part 100, an element electrode pad 211, an element electrode pad 212, and package electrode pads 301 to 304. Although described in detail later, the package 701 has a configuration for electrical wiring that is provided in the ceramic part 100.

[0047] The ceramic part 100 is made of ceramic, preferably contains an oxide as a main component, more preferably contains alumina as a main component, and is, for example, substantially made of alumina. The ceramic part 100 includes a substrate part 110 and a frame part 120. The material of the substrate part 110 and the material of the frame part 120 may be the same. The frame part 120 is laminated on the substrate part 110 in the thickness direction (z direction in FIG. 6). The frame part 120 has a frame upper surface SF1 (first surface) and a frame lower surface SF2 (second surface opposite to the first surface in the thickness direction). The frame part 120 also has an inner wall surface connecting the frame upper surface SF1 and the frame lower surface SF2 to each other, and the inner wall surface is a side wall of the cavity CV. The substrate part 110 has a substrate upper surface SF3 (third surface). The substrate upper surface SF3 has a support surface portion SF3S that supports the frame lower surface SF2 of the frame portion 120, and a cavity surface portion SF3C that faces the cavity CV. The cavity surface portion SF3C forms the bottom surface of the cavity CV.

[0048] The element electrode pads 211 and 212 (FIG. 5) are disposed on the ceramic part 100 (FIG. 6) facing the cavity CV. Specifically, the element electrode pads 211 and 212 are disposed on the upper surface (surface facing the cavity CV) of the substrate part 110 (FIG. 6). The package electrode pads 301-304 (FIG. 5) are disposed on the ceramic part 100 (FIG. 6) outside the cavity CV. Specifically, the package electrode pads 301-304 are disposed on the lower surface (surface opposite to the surface facing the cavity CV) of the substrate part 110 (FIG. 6).

[0049] The relay electrode 220 (FIG. 5) is provided on the substrate upper surface SF3 of the substrate portion 110 (FIG. 6). The relay electrode 220 is at least partially disposed on the support surface portion SF3S (FIG. 6). Thus, the relay electrode 220 (FIG. 5) is at least partially covered by the frame portion 120. The relay electrode 220 may further have a portion that is not covered by the frame portion 120 and is disposed on the bottom surface of the cavity CV. In other words, the relay electrode 220 may be only partially covered by the frame portion 120.

[0050] Fig. 7 is a plan view in which the metallization layer 600 (Fig. 5) and the frame portion 120 (Fig. 6) are omitted. Fig. 8 is a plan view that diagrammatically shows the substrate portion 110 and substrate via electrodes 411-414 in Fig. 7, with package electrode pads 301-304 indicated by dashed lines.

[0051] Wiring layers 401-403 are embedded in the substrate 110 of the ceramic part 100 near its upper surface. The wiring layer 401 is in contact with the element electrode pad 211, the wiring layer 402 is in contact with the element electrode pad 212, and the wiring layer 403 is in contact with the relay electrode 220. The wiring layers 401-403 may be covered with an insulating film 110i (see FIG. 11) as part of the substrate 110 to the extent that this contact is not hindered, and in particular, the element electrode pad 211 and the wiring layer 403 are insulated by the insulating film 110i. The wiring layer 403 and the relay electrode 220 form an electrode layer 200.

[0052] The package 701 has substrate via electrodes 411-414 embedded in the substrate portion 110 of the ceramic portion 100. The substrate via electrode 411 connects the wiring layer 402 and the package electrode pad 301 to each other. The substrate via electrode 412 connects the wiring layer 403 and the package electrode pad 302 to each other. The substrate via electrode 413 connects the wiring layer 401 and the package electrode pad 303 to each other. The substrate via electrode 414 connects the wiring layer 403 and the package electrode pad 304 to each other.

[0053] With the above configuration, the element electrode pad 211 is electrically connected to the package electrode pad 303, the element electrode pad 212 is electrically connected to the package electrode pad 301, and the relay electrode 220 is electrically connected to the package electrode pad 302 and the package electrode pad 304.

[0054] Fig. 9 is a plan view in which the metallization layer 600 in Fig. 5 is omitted. Fig. 10 is a partially enlarged view of Fig. 9. Fig. 11 is a schematic cross-sectional view taken along line XI-XI in Fig. 5.

[0055] The frame bottom surface SF2 of the frame 120 has an inner edge EI surrounding the cavity CV and an outer edge EO surrounding the inner edge EI. The minimum dimension WD (FIG. 10) between the inner edge EI and the outer edge EO may be 200 μm or less, and is typically 20 μm or more and 110 μm or less. The frame 120 has an outer wall surface SF4 connecting the frame top surface SF1 and the outer edge EO of the frame bottom surface SF2. The frame 120 also has an inner wall surface (the left surface in FIG. 11) connecting the frame top surface SF1 and the inner edge EI of the frame bottom surface SF2, and the inner wall surface faces the cavity CV. In this embodiment, the outer wall surface SF4 has a firing surface SF4A connected to the frame top surface SF1 and a fractured surface SF4B connected to the frame bottom surface SF2. The fractured surface SF4B may be a surface that is approximately perpendicular to the frame top surface SF1 (a surface parallel to the z direction in FIG. 11). The firing surface SF4A may be a beveled surface that chamfers between the frame top surface SF1 and the fractured surface SF4B, as shown in Figure 11. In other words, the normal direction of the firing surface SF4A may be different from and may be between the normal directions of the frame top surface SF1 and the fractured surface SF4B.

[0056] As described above, the electrode layer 200 is configured on the substrate upper surface SF3 of the substrate part 110 by the wiring layer 403 and the relay electrode 220. Also, as described above, the substrate part 110 has the insulating film 110i (FIG. 11) as a part thereof. As a modification, the insulating film 110i may be omitted depending on the package design. Also, the electrode layer 200 may be configured by only one of the wiring layer 403 and the relay electrode 220. For example, the electrode layer 200 may have the wiring layer 403 while omitting the relay electrode 220, and in that case, the boundary position between the wiring layer 403 and the insulating film 110i (the right end position of the wiring layer 403 in FIG. 11) may be shifted to the end position of the relay electrode 220 on the support surface part SF3S (the right end position of the relay electrode 220 in FIG. 11), and the relay electrode 220 may be omitted. Also, the end of the insulating film 110i facing the cavity CV may be deformed to reach the frame 120, and in that case, the electrode layer 200 may be separated from the cavity CV by the insulating film 110i. Also, the electrode layer 200 typically spans the support surface portion SF3S and the cavity surface portion SF3C as shown in FIG. 11, but as a modified example, it may be disposed only on the support surface portion SF3S. Also, as shown in FIG. 11, the electrode layer 200 preferably has an end (the right end in FIG. 11) away from the outer edge EO of the frame lower surface SF2 of the frame 120. In other words, it is preferable that this end does not reach the outer edge EO. As a result, the lamination interface between the metal constituting the electrode layer 200 and the ceramic does not reach the outer edge EO. As a result, the interface between the metal and the ceramic, which has lower airtightness compared to the airtightness of the interface between ceramics, does not reach the outer edge EO. Therefore, it is possible to suppress a decrease in airtightness caused by the electrode layer 200.

[0057] Package 701 has via electrodes 510. The via electrodes 510 penetrate through the frame portion 120 between the upper frame surface SF1 and the lower frame surface SF2. The via electrode 510 has an end face SFA on the upper frame surface SF1 and a bottom face SFB on the lower frame surface SF2. In a plan view, the center position of the end face SFA and the center position of the bottom face SFB may be approximately the same. The bottom face SFB is in contact with the electrode layer 200 and, in the present embodiment, is in contact with the relay electrode 220. As described above, the relay electrode 220 is in contact with the wiring layer 403, and the substrate via electrodes 412 and 414 are connected to the wiring layer 403 (FIG. 7). Therefore, the substrate via electrodes 412 and 414 are electrically connected to the via electrode 510. Further, the end face SFA of the via electrode 510 is in contact with the metallization layer 600 (FIG. 6). Therefore, the metallization layer 600 is electrically connected to the package electrode pads 302 and 304 via the substrate via electrodes 412 and 414, respectively (see FIG. 8).

[0058] The end face SFA of the via electrode 510 has a diameter DA (FIG. 10). The diameter DA is smaller than the minimum dimension WD and may be 50 μm or less. The bottom face SFB of the via electrode 510 has a diameter DB (FIG. 10) that is larger than the diameter DA. In other words, DA < DB is satisfied. The ratio of the diameter DA to the diameter DB may be 30% or more and 70% or less. When the thickness of the frame portion 120 is 20 μm or more and 250 μm or less, the above ratio is particularly suitable. The via electrode 510 preferably has a diameter of (DA + DB) / 2 or less at an intermediate position (average position between the position of the end face SFA and the position of the bottom face SFB) in the thickness direction (z direction in FIG. 11). The taper ratio (percentage of the diameter DA to the diameter DB) may be less than 60%.

[0059] In plan view (FIG. 10), the bottom surface SFB has a minimum dimension LI from an inner edge EI of the frame bottom surface SF2 of the frame portion 120, and a minimum dimension LO from an outer edge EO of the frame bottom surface SF2 of the frame portion 120. LO>LI is satisfied, and preferably, LO≧LI×1.5 is satisfied. In this embodiment, LI>0.

[0060] In the planar layout shown in Fig. 10, the shapes of the end surface SFA and the bottom surface SFB are approximately circular, but these shapes may be slightly different from a geometrically strict circular shape due to manufacturing errors. In this case, the diameters DA and DB may be calculated by approximating the end surface SFA and the bottom surface SFB with a circular shape. Also, when a missing portion is provided in the circular shape as in a modified example described later, the diameters may be determined by ignoring the missing portion.

[0061] 10, the inner edge EI of the frame bottom surface SF2 (see FIG. 11) has a first straight line portion (a straight line portion along the x direction in FIG. 10), a second straight line portion (a straight line portion along the y direction in FIG. 10) extending perpendicular to the first straight line portion, and a corner portion connecting these straight lines to each other. The minimum dimension LI may be the dimension to this corner portion.

[0062] 12 to 22 are diagrams for explaining a manufacturing method for manufacturing a plurality of packages 701 at once. Note that FIGS. 12 to 21 show a state before the firing process that changes the state of FIG. 21 to the state of FIG. 22. Therefore, each component in FIGS. 12 to 21 is made of unfired material, unlike the components in the completed package 701. However, for convenience of explanation, the same reference numerals as those representing the components of the package 701 obtained through the firing process are used in FIGS. 12 to 21, which show the process before the firing process. Also, for convenience of explanation, the names of the components in the package 701 obtained through the firing process may be used for the names of the above components made of unfired materials.

[0063] FIG. 12 is a partial plan view that shows a schematic configuration of the substrate green body GS in the above manufacturing method. FIG. 13 is a partial plan view that shows a schematic configuration of the substrate portion 110 and the substrate via electrodes 411-414 in the substrate green body GS, while the package electrode pads 301-304 are shown by dashed lines. FIG. 14 is a schematic partial cross-sectional view along the line XIV-XIV in FIG. 12 and FIG. 13. The substrate green body GS includes a plurality of regions UN0-UN4, each of which will eventually become the substrate portion 110 of the package 701 (FIG. 6) and its neighboring structure. The regions UN1-UN4 are all disposed so as to be adjacent to the region UN0. Note that in FIG. 12 and FIG. 13, a specific configuration is shown only for the region UN0, but the regions UN1-UN4 may have a similar configuration.

[0064] In this specification, the term "green body" means an unfired structure to be fired in a later step. The green body is typically a powder compact. In order to facilitate handling, the green body may contain a glass component and an organic component as additives in addition to the main component. The organic component may include, for example, polyvinyl butyral or acrylic. The green body may be formed by any method, but a green sheet as at least a part of the green body may be formed, for example, by a doctor blade method. A further green body may be added onto this green sheet, and this addition is typically performed by printing on the green sheet or laminating another green sheet. The printing is typically performed by a screen printing method. The main component of the green body that will become the ceramic part 100 (FIG. 6) by firing may be, for example, alumina powder. The main component of the green body that will become a wiring structure such as via electrode 510 and electrode layer 200 (see FIG. 11) when fired may be, for example, tungsten (W) powder, molybdenum (Mo) powder, a mixed powder of W powder and Mo powder, or a W-Mo alloy powder.

[0065] To obtain the substrate green body GS, first, a green sheet that will become the substrate portion 110 is formed. This green sheet is subjected to punching to form via holes and printing of electrode paste into the via holes to form green bodies that will become the substrate via electrodes 411-414. For example, at least one of tungsten and molybdenum powder is dispersed in the electrode paste. Next, this green sheet is printed with electrode paste to form green bodies that will become the wiring layers 401-403. Next, this green sheet is printed with ceramic paste to form green bodies that will become the insulating film 110i. Next, this green sheet is printed with electrode paste to form green bodies that will become the element electrode pads 211, 212 and the relay electrode 220. Also, at any timing after the green bodies that will become the substrate via electrodes 411-414 are formed as described above, this green sheet is printed with electrode paste to form green bodies that will become the package electrode pads 301-304.

[0066] 15 to 19 are partial cross-sectional views sequentially showing steps related to the frame green body GF for constructing the frame 120 (FIG. 11) and its surrounding structure. In the figures, the breaking surface BR is shown by a dashed line, along which the breaking step described below will be carried out.

[0067] 15, first, a simple green sheet including a portion that will become the frame 120 is formed as the frame green body GF. This formation may be performed by, for example, a doctor blade method.

[0068] 16, via holes VH are formed in frame portion 120 by laser processing. Laser light for laser processing is irradiated so as to proceed from frame lower surface SF2 to frame upper surface SF1. As a result, via holes VH tend to have a tapered shape in the direction from frame lower surface SF2 to frame upper surface SF1. The hole diameter at frame lower surface SF2 is larger than the hole diameter at frame upper surface SF1.

[0069] 17, via electrodes 510 (FIG. 17) are formed in the via holes VH (FIG. 16) of the frame green body GF. Specifically, the via holes VH are filled with electrode paste by screen printing. This filling is preferably performed from the frame lower surface SF2 to the frame upper surface SF1.

[0070] Referring to Fig. 18, a metallized layer 600 is formed. Specifically, an electrode paste is applied. Note that, although the electrode paste is applied to the entire frame upper surface SF1 in Fig. 18, it is not necessary to apply the metallized layer 600 to the area that will be removed by the cavity CV forming process described later. Therefore, a screen printing method may be applied that does not apply the paste to at least a part of the area.

[0071] 19, a cavity CV is formed by punching. The cavity CV may be formed in the frame green body GF at an earlier timing. In this manner, a frame green body GF having a frame shape surrounding the cavity CV is completed.

[0072] 20, a green sheet 700G is formed by laminating a frame green body GF (FIG. 19) on a substrate green body GS (FIG. 14). The green sheet 700G includes a plurality of regions 701G, each of which will eventually become a package 701 (see FIG. 11).

[0073] 21, a trench TR1 (FIG. 13) is formed on a frame upper surface SF1 of the green sheet 700G. A trench TR2 is formed on the surface of the green sheet 700G opposite to the frame upper surface SF1. The trenches TR1 and TR2 are disposed so as to face each other in the thickness direction. The trenches TR1 and TR2 are formed, for example, by pressing a blade tip against the green sheet 700G. Then, a firing step is performed to fire the green sheet 700G. After the firing step, a plating step may also be performed as necessary.

[0074] With reference to FIG. 22, the sintered sheet 700F is formed by the sintering process. In the sintering process, the inner surface of the trench TR1 is exposed to a sintering atmosphere. Thus, the inner surface of the trench TR1 of the sintered sheet 700F becomes a sintered surface. The sintered surface becomes the sintered surface SF4A (FIG. 11) of the package 701. A breaking process is performed in which a crack is generated from the trench TR1 by applying stress to the sintered sheet 700F. The breaking process breaks the frame portion 120 to form a fracture surface. The fracture surface becomes the fracture surface SF4B (FIG. 11) of the package 701. The breaking process may be a process in which a crack is generated between the trench TR1 and the trench TR2. A plurality of packages 701 are cut out from the sintered sheet 700F by the breaking process. In the above manner, the package 701 (FIG. 11) is obtained.

[0075] In the breaking step, the crack from the trench TR1 ideally extends along the thickness direction as shown by the solid arrow in FIG. 22. However, in reality, the crack may unintentionally approach the via electrode 510 as shown by the dashed arrow in FIG. 22. As a result, in the package 701 having the one via electrode 510, the minimum dimension LO (FIG. 10) of the frame undersurface SF2 of the frame portion 120 may become small. Since an excessively small minimum dimension LO is likely to lead to leakage from the package 701, it is desirable for the minimum dimension LO to have a certain degree of margin. According to the present embodiment, it is easy to ensure this margin.

[0076] 23 is a partial cross-sectional view that shows a schematic configuration of a package 791 of the first comparative example in the same field of view as FIG. 11. The shape of the via electrode 510 of the package 791 of the first comparative example is a shape obtained by inverting the shape of the via electrode 510 of the package 701 (FIG. 11) in the above-mentioned first embodiment. As a result, in the package 791, unlike the first embodiment, the diameter of the end face SFA is larger than the diameter of the bottom face SFB. Therefore, in a process intended to manufacture the package 791 (FIG. 23), a manufacturing error occurs in which the cavity CV and the via electrode 510 are close to each other, and the probability that the package 792 of the second comparative example shown in FIG. 24 is manufactured becomes non-negligible.

[0077] In the package 792, the end face SFA of the via electrode 510 reaches the cavity CV. As a result, the side of the via electrode 510 is exposed to the cavity CV near the end face SFA of the via electrode 510. In the process of joining the lid 980 (see FIG. 2) to the package 792, the brazing material 960 (see FIG. 2) is likely to flow into the cavity CV as shown by the arrow FL (FIG. 24). The contact between the flowed brazing material and the crystal blank 890 (see FIG. 2) may adversely affect the performance of the crystal unit 900 (see FIG. 2). Note that the adverse effect on the mechanical characteristics due to the flow of the brazing material 960 is a particular concern when the element mounted in the package is the crystal blank 890, but may also occur in the case of other piezoelectric elements. Furthermore, as long as the element mounted in the package is an electrical element, there is a concern that the electrical characteristics may be adversely affected, such as an unintended short circuit.

[0078] According to the package 701 of the present embodiment (FIGS. 10 and 11), firstly, the bottom surface SFB of the via electrode 510 is arranged so that LO>LI (see FIG. 10) is satisfied, so that a large area where a laminated interface between ceramics is arranged can be secured between the bottom surface SFB of the via electrode 510 and the outer edge EO of the frame lower surface SF2 of the frame part 120. Here, the laminated interface between ceramics has higher airtightness than the laminated interface between metal and ceramic. Therefore, it is possible to suppress a decrease in the airtightness of the cavity CV caused by leakage along the laminated interface. Secondly, since the diameter DA of the end surface SFA of the via electrode 510 is smaller than the diameter DB of the bottom surface SFB of the via electrode 510, even if the via electrode 510 is located near the cavity CV so that the bottom surface SFB of the via electrode 510 reaches the cavity CV, the end surface SFA of the via electrode 510 can be located away from the cavity CV. This prevents the side surface of the via electrode 510 from being exposed to the cavity CV in the vicinity of the end surface SFA of the via electrode 510. This makes it possible to prevent the brazing material 960 from flowing into the cavity CV due to the via electrode 510. From the above, it is possible to prevent the brazing material 960 from flowing into the cavity CV while ensuring sufficient airtightness of the cavity CV.

[0079] The diameter DA (FIG. 10) of the via electrode 510 may be 50 μm or less. This allows the minimum dimension WD (FIG. 10) of the frame portion 120 to be miniaturized, for example, to 200 μm or less. As this miniaturization progresses, leakage along the lamination interface between the substrate portion 110 and the frame portion 120 becomes more likely to become a problem, but this problem is effectively suppressed for the reasons described above.

[0080] Referring to FIG. 10, when LO≧LI×1.5 is satisfied, the decrease in airtightness of the cavity due to leakage along the lamination interface between the substrate portion 110 and the frame portion 120 (see FIG. 11) can be more sufficiently suppressed.

[0081] The via electrode 510 may have a diameter of (DA+DB) / 2 or less at an intermediate position between the end face SFA and the bottom face SFB in the thickness direction (z direction in FIG. 11) with reference to FIG. 10. This makes it possible to ensure a sufficient distance between the intermediate position of the via electrode 510 and the outer wall surface SF4 of the frame portion 120. This makes it possible to improve the airtightness reliability between the via electrode 510 and the frame portion 120. For example, as shown by the dashed arrow in FIG. 22, even if a crack unintentionally approaches the via electrode 510, the crack can be prevented from reaching the via electrode 510.

[0082] The via electrode 510 has a portion extending in an inverse tapered shape from the end face SFA in the thickness direction (z direction in FIG. 11). This makes it easier to ensure the distance between the end face SFA of the via electrode 510 and the cavity CV. This makes it possible to more sufficiently prevent the brazing material 960 from flowing into the cavity CV due to the via electrode 510. Particularly in this embodiment, since the entire via electrode 510 extends in an inverse tapered shape, this effect can be more sufficiently obtained.

[0083] The outer wall surface SF4 (FIG. 11) of the frame 120 has a fired surface SF4A that is connected to the frame upper surface SF1, and a fractured surface SF4B that is connected to the frame lower surface SF2. The fractured surface SF4B is formed by a breaking process, and the minimum dimension LO (FIG. 10) may become small due to process variations. However, as described above, since LO>LI is satisfied, the minimum dimension LO is unlikely to become too small. Therefore, it is possible to prevent a lack of airtightness caused by the minimum dimension LO being too small.

[0084] When LI>0 is satisfied (FIG. 10), the side surface of the via electrode 510 is prevented from being exposed to the cavity CV even in the vicinity of the bottom surface SFB of the via electrode 510. This makes it possible to more reliably prevent the brazing material 960 from flowing into the cavity CV. However, LI>0 does not necessarily have to be satisfied. A modified example corresponding to LI=0 will be described below.

[0085] Fig. 25 is a partial cross-sectional view generally showing the configuration of a package 710 in a modification of the present first embodiment, in the same field of view as Fig. 11. Fig. 26 is a partial plan view generally showing the configuration of a package 710, in the same field of view as Fig. 10. Fig. 27 is a plan view for explaining the configuration of the bottom surface SFB of the via electrode 510 shown in Fig. 26. With reference to Fig. 11 (first embodiment), in this modification, LI>0 is not satisfied.

[0086] The via electrode 510 has an outer periphery PR (FIG. 27) on the frame lower surface SF2 (FIG. 25). The outer periphery PR is composed of an arc portion PRa along a circular shape with a diameter DB and a missing portion PRb along a part EIc of the inner edge EI of the frame lower surface SF2. The missing portion PRb is positioned so as to remove the circular shape. In this modification, the inner edge EI of the frame 120 is considered to include a part EIc along the missing portion PRb. In this modification, the bottom surface SFB of the via electrode 510 is in contact with the part EIc of the inner edge EI of the frame 120, so the minimum dimension LI defined in FIG. 11 is zero.

[0087] According to this modification, the outer periphery PR of the via electrode 510 has a missing portion along a part EIc of the inner edge EI of the frame undersurface SF2 of the frame part 120. This makes it easier to arrange the via electrode 510 close to the cavity CV. Therefore, it is possible to more sufficiently suppress a decrease in the airtightness of the cavity caused by leakage along the lamination interface between the substrate part 110 and the frame part 120.

[0088] The missing portion PRb (FIG. 27) of the outer periphery PR of the via electrode 510 may have a convex shape toward the inside of the bottom surface SFB of the via electrode 510. In this case, the via electrode 510 can be disposed at the corner of the cavity CV. This makes it easier to ensure a large minimum dimension LO (see FIG. 10). This makes it possible to more sufficiently suppress the decrease in airtightness of the cavity caused by leakage along the lamination interface between the substrate part 110 and the frame part 120. In a typical example of this case, the inner edge EI of the frame part 120 has a substantially rectangular shape, and a part EIc of the inner edge EI extends along each corner of the rectangular shape. In the example shown in FIG. 10, each corner is chamfered in an arc shape, and therefore the part EIc of the inner edge EI also extends in an arc shape.

[0089] FIG. 28 is a diagram for explaining the details of the configuration of the via electrode 510 (FIG. 11). The via electrode 510 has an inverse tapered shape from the end face SFA to the bottom face SFB in the entire thickness direction (z direction in FIG. 28). This inverse taper preferably has a taper angle TP of 5 degrees or more with respect to the thickness direction (z direction in the figure). This makes it easier to ensure the distance between the end face SFA of the via electrode 510 and the cavity CV. Therefore, it is possible to more sufficiently prevent the brazing material 960 from flowing into the cavity CV due to the via electrode 510. In this embodiment, the via electrode 510 has an inverse tapered shape in the entire thickness direction as described above, but different forms will be described in the following embodiments 2 and 3.

[0090] <Embodiment 2> FIG. 29 is a diagram for explaining the details of the configuration of the via electrode 520 of the package 702 in the second embodiment. In a cross-sectional view parallel to the thickness direction (FIG. 29), the via electrode 520 has a side surface connecting the end surface SFA and the bottom surface SFB. The points KA and KB indicate the positions of the side surface at the positions of the end surface SFA and the bottom surface SFB in the thickness direction, respectively. The point KV indicates the position of the side surface between the points KA and KB in the thickness direction. The point KW indicates the position of the side surface between the points KV and KB in the thickness direction. The side surface may have at least one bending point, and in this embodiment, the side surface has the points KV and KW as two bending points bending in opposite directions. The via electrode 520 has a portion 521 having a side surface from the point KA to the point KV, a portion 522 having a side surface from the point KV to the point KW, and a portion 523 having a side surface from the point KW to the point KB. Portion 521 extends in a reverse tapered shape from end face SFA in the thickness direction, and the taper angle TP of this reverse tapered shape is preferably 5 degrees or more. Portion 522 has a gentler reverse tapered shape or a cylindrical shape compared to portion 521. Portion 523 has a steeper reverse tapered shape compared to portion 522.

[0091] Since the configuration other than the above is substantially the same as that of the above-mentioned first embodiment or its modified example, the same or corresponding elements are given the same reference numerals and the description thereof will not be repeated.

[0092] According to the second embodiment, the side surface of the via electrode 520 has bending points (specifically, points KV and KW). This makes it possible to suppress separation between the side surface of the via electrode 520 and the frame portion 120 caused by sintering shrinkage during the manufacture of the package 702. This effect is made more sufficient by the bending points KV and KW being bent in opposite directions.

[0093] It is preferable that the via electrode 520 has a portion extending in an inverse tapered shape from the end face SFA toward the bottom face SFB over a thickness greater than half the thickness of the frame part 120. This makes it easier to ensure the distance between the end face SFA of the via electrode 520 and the cavity CV (see FIG. 11). This makes it possible to more sufficiently prevent the brazing material from flowing into the cavity CV due to the via electrode 520.

[0094] <Embodiment 3> FIG. 30 is a diagram for explaining the details of the configuration of the via electrode 530 of the package 703 in the third embodiment. The via electrode 530 has a portion 531 having a side surface from the point KA to the point KV, a portion 532 having a side surface from the point KV to the point KW, and a portion 533 having a side surface from the point KW to the point KB. The portion 531 extends in a reverse taper from the end face SFA in the thickness direction, and the taper angle TP of this reverse taper shape is preferably 5 degrees or more. The portion 532 has a taper shape, not a reverse taper shape, in the direction from the end face SFA to the bottom face SFB. In other words, the portion 532 has a tapered shape in the direction from the end face SFA to the bottom face SFB. The portion 533 has a reverse taper shape in the direction from the end face SFA to the bottom face SFB.

[0095] Since the configuration other than the above is substantially the same as that of the above-mentioned embodiment 2, the same or corresponding elements are denoted by the same reference numerals and the description thereof will not be repeated. According to the present embodiment, the effect of suppressing the peeling between the side surface of the via electrode 520 and the frame portion 120 due to sintering shrinkage is further enhanced as compared to embodiment 2.

[0096] It is preferable that the via electrode 530 has a portion extending in an inverse tapered shape from the end face SFA toward the bottom face SFB, specifically, the portion 531 and the portion 533, over a thickness greater than half the thickness of the frame portion 120. This makes it easier to ensure the distance between the end face SFA of the via electrode 530 and the cavity CV (see FIG. 11). This makes it possible to more sufficiently prevent the brazing material from flowing into the cavity CV due to the via electrode 530.

[0097] <Fourth embodiment> Fig. 31 is a partial plan view generally showing the configuration of a package 720 in the fourth embodiment with a view similar to that of Fig. 10 in the first embodiment. Fig. 32 is a partial cross-sectional view generally showing the configuration of a package 720 along line XXXII-XXXII in Fig. 31. Fig. 33 is a partial plan view generally showing the configuration of a package 720 with a view similar to that of Fig. 7 in the first embodiment.

[0098] In the package 720, the electrode layer 200 is locally thickened at a portion in contact with the bottom surface SFB of the via electrode 510. This is due to the fact that the electrode layer 200 has a protruding portion 222 in contact with the bottom surface SFB of the via electrode 510, for reasons described later with reference to FIG. 34. Also due to this, the frame underside SF2 of the frame part 120 has an inclined region SF2d (first region) directly connected to the bottom surface SFB of the via electrode 510, and a parallel region SF2f (second region) connected to the bottom surface SFB of the via electrode 510 via the inclined region SF2d. The second region SF2f is perpendicular to the thickness direction. The inclined region SF2d is inclined with respect to the parallel region SF2f so that the thickness of the frame part 120 becomes smaller as it approaches the bottom surface SFB of the via electrode 510. The angle of this inclination is, for example, 4° or more and 20° or less.

[0099] In plan view (FIG. 31), raised portion 222 is spaced apart from outer edge EO of frame underside SF2 of frame portion 120. Furthermore, in plan view, the minimum dimension (in other words, the minimum distance) of raised portion 222 from outer edge EO is preferably greater than minimum dimension LI (FIG. 10), and more preferably greater than or equal to LI×1.5.

[0100] In the configurations illustrated in Figures 31 and 32, in plan view, the inclined region SF2d completely surrounds the bottom surface SFB of the via electrode 510, and the parallel region SF2f completely surrounds this inclined region SF2d. However, as a modification, the parallel region SF2f does not need to completely surround the inclined region SF2d. As a further modification, the inclined region SF2d also does not need to completely surround the bottom surface SFB of the via electrode 510. These modifications correspond to, for example, the case where the protruding portion 222 is applied to the configuration in which the via electrode 510 is disposed near the cavity CV as shown in Figures 25 and 26 (modifications of the first embodiment).

[0101] 32, the raised portion 222 is completely separated from the substrate portion 110 (specifically, the insulating film 110i as part of the substrate portion 110) by the relay electrode 220. As a modification, the raised portion 222 may be in contact with the substrate portion 110 (specifically, the insulating film 110i as part of the substrate portion 110).

[0102] Since the inclined region SF2d (FIG. 32) is inclined as described above, the obtuse angle SH (FIG. 32) between the side surface of the via electrode 510 and the frame lower surface SF2 can be increased while roughly maintaining the configuration of the via electrode 510. This makes it possible to alleviate thermal stress caused by the difference in thermal expansion between the via electrode 510, which is mainly made of metal, and the frame portion 120, which is made of ceramic. This makes it possible to prevent cracks or peeling between the via electrode 510 and the frame portion 120 caused by thermal stress.

[0103] FIG. 34 is a partial cross-sectional view that shows a schematic diagram of a process of manufacturing the package 720, which corresponds to FIG. 17 of the first embodiment. In this process, the via electrodes 510 (FIG. 34) are formed in the via holes VH (FIG. 16) of the frame green body GF. Specifically, the electrode paste is filled into the via holes VH by a screen printing method and then dried. This filling is preferably performed by pouring the electrode paste from the frame lower surface SF2 to the frame upper surface SF1. The electrode paste is supplied with a small amount of margin so that the electrode vias 510 are reliably formed almost entirely in the via holes VH (FIG. 16), and when it is dried, a protruding portion 222p of the electrode paste is formed on the frame lower surface SF2 so as to protrude from the via holes VH, as shown in FIG. 34. The protuberances 222p are pressed toward the via holes VH by the substrate green body GS during the lamination process (see the process from FIG. 19 to FIG. 20), resulting in the package 720 being provided with protuberances 222 (FIG. 32).

[0104] Since the configuration other than the above is substantially the same as that of any one of the above-mentioned embodiments 1 to 3 or the modified examples thereof, the same or corresponding elements are given the same reference characters and the description thereof will not be repeated. [Explanation of symbols]

[0105] 120: Frame section 200: Electrode layer 222: Ridge 510, 520, 530: Via electrodes 600: Metallized layer 701, 710, 720: Package 900: Quartz crystal unit (electrical component) 960: Brazing material 980: Lid CV: Cavity EI: Inner Marriage EO:Outer edge SF1: Top of frame (first surface) SF2: Bottom surface of the frame (second side) SF2d: 1st area SF2f: 2nd area SF4A: Baked noodles SF4B : Broken section SFA : End Face SFB: Bottom

Claims

1. A package having a cavity, a frame made of ceramic, the frame having a first surface and a second surface opposite to the first surface in a thickness direction, the second surface having an inner edge surrounding the cavity and an outer edge surrounding the inner edge, the package further comprising: a substrate portion made of ceramic, the substrate portion having a third surface having a portion supporting the second surface of the frame portion and a portion facing the cavity, the package further comprising: an electrode layer provided on the third surface of the substrate portion; a via electrode penetrating the frame portion between the first surface and the second surface, the via electrode having an end surface with a diameter DA at the first surface and a bottom surface with a diameter DB in contact with the electrode layer at the second surface, where DA<DB is satisfied; In a plan view, the bottom surface of the via electrode has a minimum dimension LI from the inner edge of the second surface of the frame portion and a minimum dimension LO from the outer edge of the second surface of the frame portion, and LO>LI is satisfied; the via electrode has an outer periphery on the second surface, the outer periphery being composed of an arc portion along a circular shape having a diameter DB and a missing portion along a part of the inner edge of the second surface of the frame portion, A package, wherein the end face of the via electrode is away from the cavity.

2. The package according to claim 1 , wherein the missing portion of the outer periphery of the via electrode has a convex shape extending inwardly from the bottom surface of the via electrode.

3. A package having a cavity, a frame made of ceramic, the frame having a first surface and a second surface opposite to the first surface in a thickness direction, the second surface having an inner edge surrounding the cavity and an outer edge surrounding the inner edge, the package further comprising: a substrate portion made of ceramic, the substrate portion having a third surface having a portion supporting the second surface of the frame portion and a portion facing the cavity, the package further comprising: an electrode layer provided on the third surface of the substrate portion; a via electrode penetrating the frame portion between the first surface and the second surface, the via electrode having an end surface with a diameter DA at the first surface and a bottom surface with a diameter DB in contact with the electrode layer at the second surface, where DA<DB is satisfied; In a plan view, the bottom surface of the via electrode has a minimum dimension LI from the inner edge of the second surface of the frame portion and a minimum dimension LO from the outer edge of the second surface of the frame portion, and LO>LI is satisfied; the electrode layer has a protruding portion that is locally thickened at a portion in contact with the bottom surface of the via electrode, the via electrode has a side surface connecting the end surface and the bottom surface, In a cross-sectional view parallel to the thickness direction, a boundary is formed between the frame portion and the raised portion of the electrode layer, the boundary is connected to the side surface of the via electrode so as to form an obtuse angle with the side surface, and the entire boundary is inclined with respect to a horizontal direction perpendicular to the thickness direction so that the obtuse angle becomes larger.

4. A package having a cavity, a frame made of ceramic, the frame having a first surface and a second surface opposite to the first surface in a thickness direction, the second surface having an inner edge surrounding the cavity and an outer edge surrounding the inner edge, the package further comprising: a substrate portion made of ceramic, the substrate portion having a third surface having a portion supporting the second surface of the frame portion and a portion facing the cavity, the package further comprising: an electrode layer provided on the third surface of the substrate portion; a via electrode penetrating the frame portion between the first surface and the second surface, the via electrode having an end surface with a diameter DA at the first surface and a bottom surface with a diameter DB in contact with the electrode layer at the second surface, where DA<DB is satisfied; In a plan view, the bottom surface of the via electrode has a minimum dimension LI from the inner edge of the second surface of the frame portion and a minimum dimension LO from the outer edge of the second surface of the frame portion, and LO>LI is satisfied; the second surface of the frame portion has a first region directly connected to the bottom surface of the via electrode and a second region connected to the bottom surface of the via electrode through the first region, the second region being perpendicular to the thickness direction, and the first region being inclined with respect to the second region such that a thickness of the frame portion becomes smaller toward the bottom surface of the via electrode, the via electrode has a side surface connecting the end surface and the bottom surface, A package, wherein, in a cross-sectional view parallel to the thickness direction, the side surface of the via electrode is connected to the first region of the second surface of the frame portion so as to form an obtuse angle with the first region.

5. 5. The package according to claim 3 or 4, wherein LI>0 is satisfied.

6. 5. The package of claim 1, wherein the diameter DA is 50 μm or less.

7. The package according to claim 1 , wherein the minimum dimension between the inner edge and the outer edge of the second surface of the frame is 200 μm or less.

8. 5. The package according to claim 1, wherein LO≧LI×1.5 is satisfied.

9. The package according to claim 1 , wherein the via electrode has a diameter of (DA+DB) / 2 or less at a middle position between the end surface and the bottom surface in the thickness direction.

10. The package according to claim 1 , wherein the via electrode has a portion extending in an inverse tapered shape from the end face in the thickness direction.

11. The package of claim 10 , wherein the reverse taper shape has a taper angle of 5 degrees or greater.

12. The package according to claim 1 , wherein the via electrode has a portion extending in an inverted tapered shape from the end face toward the bottom face over a thickness greater than half the thickness of the frame portion.

13. The package according to claim 1 , wherein the via electrode has a side surface connecting the end surface and the bottom surface, and the side surface has at least one bending point when viewed in a cross-section parallel to the thickness direction.

14. 14. The package of claim 13, wherein the at least one flex point includes two flex points that bend in opposite directions.

15. the frame portion has an outer wall surface connecting the first surface and the outer edge of the second surface, The outer wall surface has a fired surface connected to the first surface and a fracture surface connected to the second surface. A package according to any one of claims 1 to 4.

Citation Information

Patent Citations

  • Ceramic package

    JP1991283641A

  • Electronic component device

    JP2001156192A

  • Package for storage of electronic component

    JP2004200633A

  • Ceramic package and manufacturing method therefor, ceramic package for taking many pieces, and its manufacture