Battery, battery module, and method for manufacturing battery

By implementing a curved shape and precise radius of curvature at the bent portion of the fused laminate film, the battery design addresses the issue of film damage, enhancing structural integrity and reliability.

JP7567879B2Active Publication Date: 2024-10-16TOYOTA JIDOSHA KK
View PDF 12 Cites 0 Cited by

Patent Information

Application Number
JP2022139559
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-09-01
Publication Date
2024-10-16
Estimated Expiration
2042-09-01

AI Technical Summary

Technical Problem

The existing battery manufacturing process often results in damage to the laminate film at the bent portion of the fused portion due to the dimensional mismatch between the side member and the electrode body, leading to potential structural weaknesses.

Method used

The battery design incorporates a curved shape at the bent portion of the fused portion on the side surface member, with specific radius of curvature calculations to prevent damage, and uses a laminate film with a metal and resin layer combination to enhance sealing and prevent gaps.

Benefits of technology

This design effectively suppresses damage to the laminate film at the bent portion, ensuring improved structural integrity and reliability of the battery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007567879000001
    Figure 0007567879000001
  • Figure 0007567879000002
    Figure 0007567879000002
  • Figure 0007567879000003
    Figure 0007567879000003
Patent Text Reader

Abstract

To provide a battery capable of suppressing damage at a bent part in the laminate film at the starting point on the side member side of a welded part.SOLUTION: The battery includes an electrode body, a side member 20, and a laminate film 30 covering the electrode body and the side member 20. In the battery, when the battery is viewed from the side member side, the outer edge of the side member 20 is located inside the outer edge of the electrode body. The laminate film 30 is arranged to cover the surface that forms the outer edge of the side member 20 and the surface forming the outer edge of the electrode body. A fused portion X where the inner surfaces of the laminate film 30 are fused is placed on the side member 20. A bent part at the starting point on the side member side of the fused part X has a curved shape.SELECTED DRAWING: Figure 4
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present disclosure relates to a battery, a battery module, and a method for manufacturing a battery. [Background technology]

[0002] Batteries such as lithium ion secondary batteries usually include an electrode body having a positive electrode current collector, a positive electrode active material layer, an electrolyte layer, a negative electrode active material layer, and a negative electrode current collector. The electrode body is sealed in an internal space surrounded by an exterior material, for example. Patent Document 1 discloses a lithium polymer secondary battery including an electrode assembly, an exterior material surrounding the outside of the electrode assembly, and first and second covers sealing the exterior material, with the first electrode terminal and the second electrode terminal being drawn out to the outside through the first cover and the second cover, respectively. Patent Document 1 also describes a laminate film as the exterior material. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2011-108623 A Summary of the Invention [Problem to be solved by the invention]

[0004] As shown in Figures 3A and 3B described later, the dimensions of the side member may be made smaller than the dimensions of the electrode body. When sealing a side member having such a dimensional relationship with a laminate film, one method of sealing is to fold the excess part of the laminate film covering the side member and fuse the inner faces together to form a fused part. However, there have been cases where the laminate film has been damaged at the bent part at the starting point of the fused part on the side member side.

[0005] The present disclosure has been made in consideration of the above-mentioned situation, and aims to provide a battery in which breakage at the bend at the starting point of the fused portion of the laminate film on the side member side is suppressed, a battery module having such a battery, and a method for manufacturing such a battery. [Means for solving the problem]

[0006] <1> An electrode body; A side surface member disposed on a side surface portion of the electrode body; a laminate film covering the electrode body and the side surface member; A battery comprising: When the battery is viewed from the side of the side member, an outer edge of the side member is located inside an outer edge of the electrode body, the laminate film is disposed so as to cover a surface constituting the outer edge of the side member and a surface constituting the outer edge of the electrode body; A fusion portion in which inner surfaces of the laminate film are fused to each other is disposed on the side surface member, A battery, wherein a bent portion at a starting point of the fused portion on the side member side has a curved shape. <2> The laminate film has a metal layer and a fusion resin layer on the inner surface side forming the fusion portion, and the side member has a coating resin layer on the surface that contacts the laminate film. <1> 2. The battery according to claim 1 . <3> The radius of curvature R of the curved shape at the bent portion satisfies the following formulas (1) and (3), <2> 2. The battery according to claim 1 . R<(((2Δt(a+b+4t1)) / (4-π)) 1 / 2 )-r...Formula (1) R In addition, the symbols in formulas (1) and (3) represent the following. a: width of the side member (mm) b: Thickness of the side member (mm) t1: the sum (mm) of the average thickness of the fusion resin layer and the average thickness of the coating resin layer before fusion ​t2: the sum (mm) of the average thickness of the fusion resin layer and the average thickness of the coating resin layer after fusion in the fusion portion Δt: t1-t2 (mm) r: average thickness of the laminate film (mm) R: radius of curvature of the curved shape at the bent portion (mm) <4> The radius of curvature R of the curved shape at the bent portion satisfies the following formulas (2) and (3): <2> or <3> 2. The battery according to claim 1 . R<(((((a+2t1)(b+2t1)-ab)×0.05) / (4-π)) 1 / 2 )-r...Formula (2) R In addition, the symbols in formulas (2) and (3) represent the following. a: width of the side member (mm) b: Thickness of the side member (mm) t1: the sum of the average thickness of the fusion resin layer and the average thickness of the coating resin layer before welding (mm) r: average thickness of the laminate film (mm) R: radius of curvature of the curved shape at the bent portion (mm) <5> The radius of curvature R of the curved shape at the bent portion is equal to or greater than the average thickness of the metal layer. <2> ~ <4> 13. The battery according to any one of claims 1 to 12. <6> The fused portion does not have a crease mark in an area other than the bent portion. <1> ~ <5> 13. The battery according to any one of claims 1 to 12. <7> When the battery is viewed in a plan view from the thickness direction, the fusion portion is continuously disposed from an end position α of the laminate film on the side surface member side to a position β of the laminate film corresponding to the boundary between the side surface member and the electrode body. <1> ~ <6> 13. The battery according to any one of claims 1 to 12. <8> The fused portion is disposed at a corner portion constituting the outer edge of the side member. <1> ~ <7> 13. The battery according to any one of claims 1 to 12. <9> ​When the battery is viewed from the side of the side member, the shape of the side member is rectangular. <1> ~ <8> 13. The battery according to any one of claims 1 to 12. <10> A plurality of the fused portions are disposed on the side member. <1> ~ <9> 13. The battery according to any one of claims 1 to 12. <11> The side member is a current collecting terminal. <1> ~ <10> 13. The battery according to any one of claims 1 to 12. <12> The battery includes a pair of the side members, The pair of side members are disposed to face each other with respect to the electrode body. <1> ~ <11> 13. The battery according to any one of claims 1 to 12. <13> A battery module having a plurality of batteries stacked in a thickness direction, The battery comprises: <1> ~ <12> 2. A battery module comprising the battery according to claim 1. <14> In a pair of side members adjacent to each other in the thickness direction, a main surface of the laminate film arranged on one of the side members is not in contact with a main surface of the laminate film arranged on the other side member. <13> The battery module described in <15> <1> ~ <12> A method for producing the battery according to any one of claims 1 to 4, a preparation step of preparing a structure having the electrode body and the side surface member, wherein when the battery is viewed from the side of the side surface member, the shape of the side surface member is quadrangle, the quadrangle having a first side, a second side adjacent to the first side, a third side adjacent to the second side and facing the first side, and a fourth side adjacent to the third side and facing the second side; a first covering step of covering a surface constituting the outer edge of the electrode body in the structure with the laminate film; A second covering step of covering a surface constituting the outer edge of the side member in the structure with the laminate film; having The second covering step includes: a first adhesion process in which a first jig and a third jig are pressed into the first side and the third side of the side member, respectively, to adhere the laminate film to the first side and the third side, respectively; a second adhesion process in which a second jig and a fourth jig are pressed into the second side and the fourth side of the side member, respectively, after the first adhesion process, to adhere the laminate film to the second side and the fourth side, respectively; having A method for manufacturing a battery, wherein at least one of the first jig and the third jig has a chamfered shape at a location that forms the curved shape of the bent portion in the fused portion. <16> After the preparation step and before the first coating step, A folding process is provided for forming a folding line in advance on the laminate film at a position opposite to a corner of the electrode body, In the folding step, no folding line is provided at a position of the laminate film facing the side member. <15> A method for manufacturing the battery according to claim 1. Effect of the Invention

[0007] According to the present disclosure, it is possible to provide a battery in which breakage at a bent portion at the starting point of the fused portion of the laminate film on the side of the side member is suppressed, a battery module having the battery, and a method for manufacturing the battery. [Brief description of the drawings]

[0008] [Figure 1A] 1 is a schematic perspective view illustrating an electrode body according to the present disclosure. [Figure 1B] 1 is a schematic perspective view illustrating an electrode body and a side member according to the present disclosure. [Figure 2A] 1 is a schematic perspective view illustrating an electrode body, a side member, and a laminate film in the present disclosure in a state before sealing. FIG. [Figure 2B] 1 is a schematic perspective view illustrating a state after sealing of an electrode body, a side member, and a laminate film in the present disclosure. FIG. [Figure 3A] 3 is a schematic side view illustrating an electrode body and a side member according to the present disclosure. FIG. [Figure 3B] 3A to 3C are schematic cross-sectional views illustrating an electrode body and a side member according to the present disclosure. [Figure 3C] 2 is a schematic side view illustrating an electrode body, a side member, and a laminate film in the present disclosure. FIG. [Figure 3D] 2 is a schematic cross-sectional view illustrating an electrode body, a side member, and a laminate film in the present disclosure. FIG. [Figure 4] FIG. 2 is a schematic side view illustrating a portion of a battery in the present disclosure. [Diagram 5] FIG. 2 is a schematic side view illustrating a portion of a battery in the present disclosure. [Figure 6] FIG. 2 is a schematic cross-sectional view illustrating a portion of a battery according to the present disclosure. [Figure 7] FIG. 2 is a schematic plan view illustrating a portion of a battery according to the present disclosure. [Figure 8A] FIG. 2 is a schematic cross-sectional view illustrating a portion of a battery according to the present disclosure. [Figure 8B] FIG. 2 is a schematic cross-sectional view illustrating a portion of a battery according to the present disclosure. [Figure 9A] FIG. 2 is a schematic side view illustrating a portion of a battery in the present disclosure. [Figure 9B] FIG. 2 is a schematic side view illustrating a portion of a battery in the present disclosure. [Figure 9C] FIG. 2 is a schematic side view illustrating a portion of a battery in the present disclosure. [Figure 10] 1 is a schematic cross-sectional view illustrating an electrode body according to the present disclosure. [Figure 11] FIG. 1 is a schematic perspective view illustrating a battery module according to the present disclosure. [Figure 12] 1 is a schematic cross-sectional view illustrating a battery module according to the present disclosure. [Figure 13] FIG. 1 is a schematic plan view illustrating a laminate film in the present disclosure. [Figure 14A] FIG. 2 is a schematic side view illustrating a second coating step in the present disclosure. [Figure 14B]FIG. 2 is a schematic side view illustrating a second coating step in the present disclosure. [Figure 14C] FIG. 2 is a schematic side view illustrating a second coating step in the present disclosure. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] The battery of the present disclosure will be described in detail below with reference to the drawings. Each of the drawings shown below is a schematic illustration, and the size and shape of each part are appropriately exaggerated to facilitate understanding. In addition, in this specification, when expressing an aspect in which another member is arranged relative to a certain member, the term "above" or "below" simply refers to both a case in which another member is arranged directly above or below a certain member so as to be in contact with the certain member, and a case in which another member is arranged above or below a certain member via another member, unless otherwise specified.

[0010] A.Battery 1A and 1B are schematic perspective views illustrating an electrode body and a side surface member in the present disclosure. The electrode body 10 shown in FIG. 1A has a top surface portion 11, a bottom surface portion 12 facing the top surface portion 11, and four side surfaces (a first side surface portion 13, a second side surface portion 14, a third side surface portion 15, and a fourth side surface portion 16) connecting the top surface portion 11 and the bottom surface portion 12. In FIG. 1B, a first side surface member 20A is disposed on the first side surface portion 13 of the electrode body 10, and a second side surface member 20B is disposed on the third side surface portion 15 of the electrode body 10. For example, the first side surface member 20A is a positive electrode current collector terminal, and the second side surface member 20B is a negative electrode current collector terminal.

[0011] 2A and 2B are schematic perspective views illustrating an electrode body, a side member, and a laminate film in the present disclosure. As shown in FIG. 2A, the laminate film 30 is, for example, a single film. As shown in FIGS. 2A and 2B, the laminate film 30 is folded so as to cover the entire bottom surface portion 12, the second side surface portion 14, the top surface portion 11, and the fourth side surface portion 16 of the electrode body 10. Meanwhile, in FIG. 2B, at least a part of the first side surface member 20A and at least a part of the second side surface member 20B are located inside the folded laminate film 30.

[0012] FIG. 3A is a schematic side view illustrating an electrode body and a side member in the present disclosure, and FIG. 3B is a cross-sectional view taken along line AA in FIG. 3A. As shown in FIG. 3A and FIG. 3B, when the electrode body 10 and the side member 20 are observed from the side member 20 side, the outer edge E2 of the side member 20 is located inside the outer edge E1 of the electrode body 10. In other words, the dimensions of the side member 20 are smaller than the dimensions of the electrode body 10. By adopting such a dimensional relationship, for example, when a plurality of batteries are stacked, it is possible to prevent adjacent side members 20 from contacting each other. By preventing contact between adjacent side members 20, damage to the battery is less likely to occur.

[0013] FIG. 3C is a schematic side view illustrating an electrode body, a side member, and a laminate film in the present disclosure, and FIG. 3D is a cross-sectional view taken along the line AA in FIG. 3C. FIG. 3D and FIG. 3C show the state before the side member is sealed with the laminate film. As shown in FIG. 3C and FIG. 3D, when the electrode body 10, the side member 20, and the laminate film 30 are observed from the side member 20 side, a space S is generated between the laminate film 30 and the side member 20. Therefore, when sealing the side member 20 with the laminate film 30, there is a method of sealing by folding the excess part of the laminate film 30 and fusing the inner surfaces together to form a fused part X, as shown in FIG. 4. However, by forming the fused part X, a bent part is formed at the starting point of the fused part X on the side member 20 side, and the laminate film 30 may be damaged at this bent part.

[0014] In contrast, in the battery according to the present disclosure, as shown in FIG. 5, a bent portion 34 at the starting point of the fused portion X on the side surface member 20 side has a curved shape. According to the present disclosure, since the bent portion 34 at the starting point of the fused portion X on the side member 20 side has a curved shape, concentration of stress at a specific point in the bent portion 34 is suppressed, resulting in a battery in which breakage at the bent portion 34 of the fused portion X in the laminate film 30 is suppressed.

[0015] 1. Battery configuration The battery according to the present disclosure comprises at least an electrode body, a side member, and a laminate film.

[0016] (1) Electrode body The electrode body in the present disclosure functions as a power generating element of a battery. The shape of the electrode body is not particularly limited, but for example, as shown in FIG. 1A, the electrode body has a top surface portion 11, a bottom surface portion 12 facing the top surface portion 11, and four side surfaces (a first side surface portion 13, a second side surface portion 14, a third side surface portion 15, and a fourth side surface portion 16) connecting the top surface portion 11 and the bottom surface portion 12. The top surface portion 11 and the bottom surface portion 12 both correspond to the main surface of the electrode body, and the normal direction of the main surface can be defined as the thickness direction. In addition, the first side surface portion 13 and the third side surface portion 15 are arranged to face each other. Similarly, the second side surface portion 14 and the fourth side surface portion 16 are arranged to face each other.

[0017] The shape of the top surface portion is not particularly limited, but examples thereof include quadrilaterals such as a square, a rectangle, a rhombus, a trapezoid, and a parallelogram. The shape of the top surface portion 11 in FIG. 1A is a rectangle. The shape of the top surface portion may be a polygon other than a quadrilateral, or may be a shape having a curve such as a circle. The shape of the bottom surface portion is the same as that of the top surface portion. The shape of the side surface portion is not particularly limited, but examples thereof include quadrilaterals such as a square, a rectangle, a rhombus, a trapezoid, and a parallelogram.

[0018] (2) Side members The side surface member in the present disclosure is disposed on the side surface of the electrode body. The battery in the present disclosure may include one side surface member for one electrode body, or may include two or more side surface members. In the latter case, for example, as shown in FIG. 1B, a pair of side surface members 20 (a first side surface member 20A and a second side surface member 20B) may be disposed to face the electrode body 10. Also, in FIG. 1B, the pair of side surface members 20 are disposed to face each other in the longitudinal direction of the electrode body 10. On the other hand, although not particularly shown, the pair of side surface members may be disposed to face each other in the lateral direction of the electrode body.

[0019] The shape of the side member is not particularly limited, but examples thereof include quadrilaterals such as squares, rectangles, rhombus, trapezoids, and parallelograms. The shape of the side member 20 in FIG. 3A is a rectangle. In this rectangle, the thickness direction D T The short side extends along a direction parallel to the thickness direction D T The long side extends along a direction perpendicular to the . The shape of the side surface member may be a polygon other than a rectangle, or may be a shape having a curve such as a circle. The side surface member may have a corner where two sides (straight sides) intersect.

[0020] When the battery is viewed from the side from the side member side, the outer edge of the side member is located inside the outer edge of the electrode body. For example, as shown in FIG. 3A, the outer edge E2 of the side member 20 is located inside the outer edge E1 of the electrode body 10. In other words, the outer edge E2 of the side member 20 is included in the outer edge E1 of the electrode body 10 over the entire circumference. The dimensions of the side member 20 are smaller than the dimensions of the electrode body 10.

[0021] 3A, for example, the length (total circumferential length) of the outer edge E1 of the electrode body 10 is L1, and the length (total circumferential length) of the outer edge E2 of the side member 20 is L2. The ratio of L2 to L1 (L2 / L1) may be, for example, 0.7 or more and less than 1, or 0.8 or more and 0.95 or less. T The length of the outer edge E1 in the thickness direction D TThe length of the outer edge E2 in the thickness direction D is Lb. The ratio of Lb to La (Lb / La) may be, for example, 0.5 or more and less than 1, or 0.8 or more and 0.95 or less. T The length of the outer edge E1 in the direction perpendicular to the thickness direction D is Lc. T The length of the outer edge E2 in the direction perpendicular to the direction of the arrow A is defined as Ld. The ratio of Ld to Lc (Ld / Lc) is, for example, 0.5 or more and less than 1, and may be 0.8 or more and 0.95 or less. Also, for example, in FIG. 3A, the length of the gap between the outer edges E1 and E2 is defined as δ. δ is greater than 0 mm, and may be 0.3 mm or more, or 0.5 mm or more. On the other hand, δ is, for example, 1.5 mm or less.

[0022] (3) Laminate film The laminate film in the present disclosure covers the electrode body and seals the electrode body together with the side surface member. As shown in Figures 2A and 2B, when the electrode body 10 and the side surface member 20 are observed from the side surface member 20 side, the laminate film 30 is disposed so as to cover the surface constituting the outer edge of the side surface member 20 and the surface constituting the outer edge of the electrode body 10.

[0023] As shown in Fig. 4, a fused portion X is disposed on the side surface member 20, where the inner surfaces of the laminate film 30 are fused together. The fused surface of the fused portion X preferably does not have any gaps. As shown in Fig. 5, the fused portion X has a curved bend 34 at the starting point on the side surface member side. This makes it possible to prevent breakage of the fused portion X of the laminate film 30 at the bend 34. The curved shape refers to a shape that is continuously curved without any corners that can be visually confirmed.

[0024] 4, there is disposed an end adhesion portion Y where the ends of the laminate film 30 are fused together. The end adhesion portion Y may be folded to fit the shape of the side member 20. This is because it is possible to reduce excess space.

[0025] Here, the radius of curvature R of the curved shape of the bent portion 34 of the fused portion X will be described with reference to FIG. It is preferable that the radius of curvature R of the curved shape of the bent portion 34 satisfies the following formula (1). R<(((2Δt(a+b+4t1)) / (4-π)) 1 / 2 )-r...Formula (1) In addition, each symbol in formula (1) represents the following. a: Width of side member 20 (mm) b: Thickness of the side member 20 (mm) t1: the sum (mm) of the average thickness of the fusion resin layer 30A and the average thickness of the coating resin layer 20A before fusion t2: the sum (mm) of the average thickness of the fusion resin layer 30A and the average thickness of the coating resin layer 20A after fusion at the fusion portion Δt: t1-t2 (mm) r: average thickness of laminate film 30 (mm) R: radius of curvature of the curved shape at the bend 34 (mm)

[0026] However, the radius of curvature R of the curved shape at the bent portion 34 satisfies the following formula (3), that is, the radius of curvature R is less than ½ the thickness b of the side surface member 20. R In addition, each symbol in formula (3) represents the following. b: Thickness of the side member 20 (mm) R: radius of curvature of the curved shape at the bend 34 (mm)

[0027] ​The laminate film 30 may have a metal layer and a fusion resin layer 30A on the inner surface side forming the fusion portion. In addition, the side member 20 may have a coating resin layer 20A on the surface in contact with the laminate film 30 to improve the sealing with the laminate film 30. When the bent portion 34 at the start point of the fusion portion X on the side member 20 side is curved, a space S is generated inside the curved shape of the bent portion 34. It is preferable that this space S is filled with resin from the fusion resin layer 30A of the laminate film 30 and the coating resin layer 20A of the side member 20, and no gap is generated. In contrast, when the curvature radius R of the curved shape of the bent portion 34 satisfies the formula (1), the space S is well filled with resin, and the generation of gaps can be suppressed.

[0028] For example, when the width a of the side member 20 is 63 mm, the thickness b of the side member 20 is 2.5 mm, the sum t1 of the average thickness of the fusion resin layer 30A before fusion and the average thickness of the coating resin layer 20A is 0.18 mm, the difference (t1-t2) between the above t1 and the sum t2 of the average thickness of the fusion resin layer 30A after fusion at the fusion part and the average thickness of the coating resin layer 20A is Δt: 0.05 mm, and the average thickness r of the laminate film 30 is 0.153 mm, R<2.62 mm is calculated by substituting into formula (1). However, it is preferable that R<1.25 mm in order to also satisfy formula (3).

[0029] Furthermore, it is more preferable that the radius of curvature R of the curved shape of the bent portion 34 satisfies the following formula (2). R<(((((a+2t1)(b+2t1)-ab)×0.05) / (4-π)) 1 / 2 )-r...Formula (2) In addition, each symbol in formula (2) represents the following. a: Width of side member 20 (mm) b: Thickness of the side member 20 (mm) t1: the sum (mm) of the average thickness of the fusion resin layer 30A and the average thickness of the coating resin layer 20A before fusion r: average thickness of laminate film 30 (mm) R: radius of curvature of the curved shape at the bend 34 (mm)

[0030] However, the radius of curvature R of the curved shape at the bent portion 34 satisfies the following formula (3), that is, the radius of curvature R is less than ½ the thickness b of the side surface member 20. R b: Thickness of the side member 20 (mm) R: radius of curvature of the curved shape at the bend 34 (mm)

[0031] When the bent portion 34 at the starting point of the fusion portion X on the side of the side member 20 is curved, a space S is generated inside the curved shape of the bent portion 34, and this space S is filled with resin from the fusion resin layer 30A and the coating resin layer 20A. However, since resin easily absorbs moisture, it is preferable that the volume of the space S (i.e., the amount of resin filling the space S) is small from the viewpoint of the water barrier property of the battery. Specifically, it is preferable that the increase in the amount of water absorption due to the increase in the volume of the space S is 5% or less. In contrast, by making the radius of curvature R of the curved shape of the bent portion 34 satisfy the formula (2), the amount of water absorption by the resin filling the space S can be reduced and the water barrier property can be maintained.

[0032] For example, if the width a of the side member 20 is 63 mm, the thickness b of the side member 20 is 2.5 mm, the sum t1 of the average thickness of the fused resin layer 30A before fusion and the average thickness of the coating resin layer 20A is 0.18 mm, and the average thickness r of the laminate film 30 is 0.153 mm, it is preferable that R<1.02 mm when calculated by substituting into formula (2).

[0033] On the other hand, the lower limit of the radius of curvature R of the curved shape at the bent portion 34 is preferably equal to or greater than the average thickness of the metal layer in the laminate film. A smaller radius of curvature R (tighter curvature) causes stress concentration, making the laminate film more susceptible to damage, but by making the radius of curvature R equal to or greater than the average thickness of the metal layer, damage to the laminate film can be more effectively suppressed.

[0034] ​As shown in FIG. 5, it is preferable that the fusion part X does not have a crease mark in an area other than the bent part 34. When the electrode body 10 and the side member 20 are sealed with the laminate film 30, a fold line may be provided in advance on the laminate film 30 at a position facing the corner of the electrode body 10. When providing the fold line on the laminate film 30, the fold line may be provided not only at the position facing the corner of the electrode body 10 but also at a position facing the side member 20 on the extension line. However, the fold line provided at the position facing the side member 20 remains as a crease mark in an area other than the bent part 34 when the fusion part X is formed. When the fusion part X has this crease mark, the laminate film 30 may be damaged at the crease mark. Therefore, by providing the fusion part X with no crease mark in an area other than the bent part 34, damage to the laminate film 30 occurring in an area other than the bent part 34 can be suppressed.

[0035] In Fig. 5, when the battery 100 is viewed from the side of the side member 20, the fused portion X is disposed at a corner that constitutes the outer edge E2 of the side member 20. Specifically, the corner that constitutes the outer edge E2 of the side member 20 coincides with an end t of the fused surface of the fused portion X. Also, as shown in Fig. 5, the width of the fused surface of the fused portion X is w. The width w is, for example, 0.1 mm or more, may be 0.3 mm or more, or may be 0.6 mm or more. On the other hand, the width w is, for example, 1.2 mm or less.

[0036] As shown in FIG. 7, when the battery 100 is viewed in plan from the thickness direction, the end position of the laminate film 30 on the side of the side member 20 is α, and the position of the laminate film 30 corresponding to the boundary between the side member 20 and the electrode body 10 is β. The fusion part X in FIG. 7 is continuously disposed from the end position α to the position β. In addition, when the direction in which the side member 20 extends from the electrode body 10 is D1, it is preferable that the fusion part X is disposed along the direction D1. In addition, the fusion part X may be disposed in at least a part of the region from the end position α to the position β in the direction D1. The length of the fusion part X in the direction D1 is, for example, 1 mm or more, may be 3 mm or more, or may be 5 mm or more.

[0037] As shown in FIG. 8A, the end position α of the laminate film 30 on the side of the side member 20 may be closer to the electrode body 10 than the end position γ of the side member 20 opposite the electrode body 10. That is, when the battery is viewed in plan from the thickness direction, the laminate film 30 may cover a part of the side member 20. In this case, a part of the side member 20 (a part not covered by the laminate film 30) is exposed. On the other hand, as shown in FIG. 8B, the end position α may coincide with the end position γ. That is, when the battery is viewed in plan from the thickness direction, the laminate film 30 may cover the entire side member 20.

[0038] 9A to 9C are schematic side views of a part of the battery 100 viewed from the side of the side member 20. As shown in FIG. 9A, the fusion part X is disposed at a corner portion constituting the outer edge of the side member 20. FIG. 9A shows a battery 100 having an end contact part Y and three fusion parts X. However, one fusion part X may be disposed for one side member 20, or two or more fusion parts X may be disposed. In particular, it is preferable that a plurality of fusion parts X are disposed for the side member 20. This is because the surplus part of the laminate film 30 can be dispersed and absorbed. Moreover, the end contact part Y in FIG. 9A is fused by contacting the inner surfaces of the ends of the laminate film 30 with each other.

[0039] In the present disclosure, when the battery 100 has a plurality of fused parts X, the bent part at the starting point on the side surface member 20 side in one or more of the fused parts X has a curved shape. Note that it is preferable that the bent part at the starting point on the side surface member 20 side in the plurality of fused parts X has a curved shape, and it is preferable that the bent part at the starting point on the side surface member 20 side in all of the fused parts X has a curved shape.

[0040] As shown in Fig. 9A, the three fused parts X may be disposed at the corners of each side constituting the outer edge of the side surface member 20. Also, as shown in Fig. 9B, the two fused parts X may be disposed at the two corners of one short side constituting the outer edge of the side surface member 20. Also, as shown in Fig. 9C, the two fused parts X may be disposed at the two corners of one long side constituting the outer edge of the side surface member 20.

[0041] 2. Battery components The battery according to the present disclosure comprises an electrode body, a side member, and a laminate film.

[0042] (1) Electrode body The electrode assembly in the present disclosure usually has a positive electrode current collector, a positive electrode active material layer, an electrolyte layer, a negative electrode active material layer, and a negative electrode current collector, in this order in the thickness direction. For example, the electrode assembly 10 shown in Fig. 10 has a positive electrode current collector 4, a positive electrode active material layer 1, an electrolyte layer 3, a negative electrode active material layer 2, and a negative electrode current collector 5, in this order in the thickness direction.

[0043] The positive electrode active material layer contains at least a positive electrode active material. The positive electrode active material layer may further contain at least one of a conductive material, an electrolyte, and a binder. Examples of the positive electrode active material include oxide active materials. Examples of the oxide active material include LiNi 1 / 3 Co 1 / 3 Mn 1 / 3 Examples of the positive electrode active material include rock salt layer type active materials such as O2, spinel type active materials such as LiMn2O4, and olivine type active materials such as LiFePO4. Sulfur (S) may also be used as the positive electrode active material. The positive electrode active material may be, for example, in the form of particles.

[0044] Examples of the conductive material include carbon materials. The electrolyte may be a solid electrolyte or a liquid electrolyte. The solid electrolyte may be an organic solid electrolyte such as a gel electrolyte, or an inorganic solid electrolyte such as an oxide solid electrolyte or a sulfide solid electrolyte. The liquid electrolyte (electrolytic solution) contains, for example, a supporting salt such as LiPF6 and a solvent such as a carbonate-based solvent. Examples of the binder include a rubber-based binder and a fluoride-based binder.

[0045] The negative electrode active material layer contains at least a negative electrode active material. The negative electrode active material layer may further contain at least one of a conductive material, an electrolyte, and a binder. Examples of the negative electrode active material include metal active materials such as Li and Si, carbon active materials such as graphite, Li4Ti5O 12 The oxide active material may be in the form of, for example, particles or foil. The conductive material, electrolyte and binder are the same as those described above.

[0046] The electrolyte layer is disposed between the positive electrode active material layer and the negative electrode active material layer, and contains at least an electrolyte. The electrolyte may be a solid electrolyte or a liquid electrolyte. The electrolyte is the same as that described above. The electrolyte layer may have a separator.

[0047] The positive electrode current collector collects the current from the positive electrode active material layer. Examples of the material of the positive electrode current collector include metals such as aluminum, SUS, and nickel. Examples of the shape of the positive electrode current collector include a foil shape and a mesh shape. The positive electrode current collector may have a positive electrode tab for connecting to a positive electrode current collector terminal.

[0048] The negative electrode current collector collects the current from the negative electrode active material layer. Examples of the material for the negative electrode current collector include metals such as copper, SUS, and nickel. Examples of the shape of the negative electrode current collector include a foil shape and a mesh shape. The negative electrode current collector may have a negative electrode tab for connecting to a negative electrode current collector terminal.

[0049] (2) Side members The side member in the present disclosure is disposed on the side surface of the electrode body. The side member is not particularly limited as long as it is a member disposed on the side surface of the electrode body, but is preferably a current collecting terminal. The current collecting terminal refers to a terminal having a current collecting portion at least in a portion thereof. The current collecting portion is, for example, electrically connected to a tab in the electrode body. The current collecting terminal may be the current collecting portion in its entirety, or may be a current collecting portion in its entirety. The side member may also be an exterior member that does not have a current collecting function.

[0050] Examples of the material of the side member include metals such as SUS. In addition, the side member may have a coating resin layer on the surface that contacts the laminate film. Examples of the material of the coating resin layer include olefin resins such as polypropylene (PP) and polyethylene (PE). The thickness of the coating resin layer is, for example, 40 μm or more and 150 μm or less.

[0051] (3) Laminate film The laminate film in the present disclosure has at least a structure in which a fusion resin layer (thermal fusion layer) and a metal layer are laminated, that is, a structure in which a fusion resin layer (thermal fusion layer) is provided on one surface (the inner surface side forming the fusion part) of the metal layer. The laminate film may also have a fusion resin layer (thermal fusion layer), a metal layer, and a resin layer in this order along the thickness direction. Examples of materials for the fusion resin layer (thermal fusion layer) include olefin resins such as polypropylene (PP) and polyethylene (PE). Examples of materials for the metal layer include aluminum, aluminum alloys, and stainless steel. Examples of materials for the resin layer include polyethylene terephthalate (PET) and nylon. The thickness of the fusion resin layer (thermal fusion layer) is, for example, 40 μm or more and 100 μm or less. The thickness of the metal layer is, for example, 30 μm or more and 60 μm or less. The thickness of the resin layer is, for example, 20 μm or more and 60 μm or less. The total thickness of the laminate film is, for example, 70 μm or more and 220 μm or less.

[0052] (4)Battery The battery in the present disclosure is typically a lithium-ion secondary battery. Examples of uses of the battery include power sources for vehicles such as hybrid electric vehicles (HEVs), plug-in hybrid electric vehicles (PHEVs), electric vehicles (BEVs), gasoline-powered vehicles, and diesel-powered vehicles. In particular, the battery is preferably used as a driving power source for hybrid electric vehicles (HEVs), plug-in hybrid electric vehicles (PHEVs), or electric vehicles (BEVs). The battery in the present disclosure may also be used as a power source for moving objects other than vehicles (e.g., railways, ships, and aircraft), and may also be used as a power source for electrical products such as information processing devices.

[0053] B. Battery module 11 is a schematic perspective view illustrating a battery module according to the present disclosure. T The battery 100 has a plurality of batteries 100 stacked in a stacked manner. The batteries 100 are the batteries described above in "A. Battery."

[0054] According to the present disclosure, by using the above-described battery, a battery module is obtained in which breakage at the bent portion at the starting point of the fused portion of the laminate film on the side of the side member is suppressed.

[0055] The battery in the present disclosure is similar to that described in "A. Battery" above, and therefore the description here is omitted. The battery module in the present disclosure may also have a restraining jig that restrains multiple batteries in the thickness direction. The type of restraining jig is not particularly limited, but examples include a jig that applies restraining torque by a bolt. The restraining pressure applied by the restraining jig is, for example, 1 MPa or more and 50 MPa or less.

[0056] As shown in Fig. 12, the laminate film 30 disposed on the side member 20 has a main surface portion 31 and a wall portion 32. The wall portion 32 is located between the main surface portion 31 and a position β of the laminate film 30 that corresponds to the boundary between the side member 20 and the electrode body 10. When a restraining pressure is applied to the battery by the restraining jig, the battery is compressed in the thickness direction. In such a state, the thickness direction D TIn a pair of side members 20 (20C, 20D) adjacent to each other in the side surface member 20, it is preferable that the main surface portion 31 of the laminate film 30 arranged on one side member 20C is not in contact with the main surface portion 31 of the laminate film 30 arranged on the other side member 20D. This is because damage due to contact can be prevented. Furthermore, when a fusion portion is arranged on the main surface portion of the laminate film, the fusion portion is included in the main surface portion of the laminate film. In other words, it is preferable that the fusion portion arranged on the main surface portion of the laminate film is not in contact with the main surface portion of the laminate film arranged on the other side member.

[0057] C. Battery manufacturing method The method for manufacturing a battery according to the present disclosure is the method for manufacturing a battery described above, and includes a preparation step of preparing a structure having the electrode body and the side member, a first covering step of covering the outer edge of the electrode body in the structure with the laminate film, and a second covering step of covering the outer edge of the side member in the structure with the laminate film, and in the second covering step, the fusion portion is formed using a jig capable of surface contact with a surface constituting the outer edge of the side member. Note that in the preparation step, a structure may be prepared in which the shape of the side member is quadrangular when the battery is viewed from the side of the side member, and the quadrangular shape has a first side, a second side adjacent to the first side, a third side adjacent to the second side and facing the first side, and a fourth side adjacent to the third side and facing the second side. In this case, the second covering process includes a first adhesion process in which a first tool and a third tool are pressed into the first side and the third side of the side member, respectively, to adhere the laminate film to the first side and the third side, respectively, and after the first adhesion process, a second adhesion process in which a second tool and a fourth tool are pressed into the second side and the fourth side of the side member, respectively, to adhere the laminate film to the second side and the fourth side, respectively, and it is preferable that at least one of the first tool and the third tool has a chamfered shape at a location that forms the curved shape of the bent portion in the fused portion.

[0058] 1. Preparation process The preparation step in the present disclosure is a step of preparing a structure having the electrode body and the side member. The electrode body and the side member are the same as those described in "A. Battery" above, so a description thereof will be omitted here.

[0059] 2. Folding process In the present disclosure, before the first covering step, a step of previously marking a folding line on the laminate film at a position opposite to a corner of the electrode body, that is, a folding step of previously folding the laminate film to match the shape of the electrode body, may be included.

[0060] However, as shown in FIG. 13, it is preferable that in the folding process, no folding line is provided at the position of the laminate film 30 facing the side member (i.e., the non-folded portion NB is provided). In the folding process, the position facing the corner of the electrode body is folded (i.e., the folding portion B is provided), and a folding line can also be provided at the position facing the side member on the extension line. However, the folding line provided at the position facing the side member remains as a folding mark in the region other than the bent portion when the fusion portion X is formed. If the fusion portion X has this folding mark, the laminate film may be damaged at the folding mark. Therefore, it is preferable that in the folding process, no folding line is provided at the position facing the side member of the laminate film, and as a result, the fusion portion X has a structure that does not have a folding mark in the region other than the bent portion. This makes it possible to suppress damage to the laminate film caused by the folding mark in the region other than the bent portion of the fusion portion X.

[0061] 3. First coating process The first covering step in the present disclosure is a step of covering the outer edge of the electrode body in the structure with the laminate film. For example, as shown in Figs. 2A and 2B, in the first covering step, the surfaces constituting the outer edge of the electrode body 10 (for example, the bottom surface portion 12, the second side surface portion 14, the top surface portion 11, and the fourth side surface portion 16) are covered with the laminate film 30. At this time, the electrode body 10 and the laminate film 30 may be brought into close contact with each other. Also, as shown in Fig. 2B, the end overlap portion Z where the ends of the laminate film 30 overlap is heated. As a result, an end contact portion Y where the ends of the laminate film 30 are fused to each other is formed.

[0062] In the first covering step, a space S is usually formed between the laminate film 30 and the side member 20, as shown in Fig. 3C and Fig. 3D. This space S disappears in the second covering step described below, and a fused portion is formed instead.

[0063] 4. Second coating process The second covering step in the present disclosure is a step of covering the surface constituting the outer edge of the side surface member with the laminate film. Also, in the second covering step, a fused portion is formed.

[0064] In the second covering step, the side member and the laminate film are brought into close contact with a jig capable of surface contact with the surface constituting the outer edge of the side member. FIGS. 14A to 14C are schematic side views illustrating the second covering step in the present disclosure. As shown in FIG. 14A, a space S is formed between the laminate film 30 and the side member 20 by the above-mentioned first covering step. Furthermore, an end contact portion Y is formed by the above-mentioned first covering step. Next, as shown in FIG. 14B, jigs 41, 42, 43 and 44 are pressed into the laminate film 30 and the side member 20. In the thickness direction D, as shown in FIG. 14B, the laminate film 30 and the side member 20 are pressed into the laminate film 30 and the side member 20. TIn this figure, the length of jig 42 (the length in the vertical direction in the drawing) is shorter than the length of side member 20 (the length in the vertical direction in the drawing). Therefore, a gap is generated between jig 41 and jig 42, and the excess portion of laminate film 30 gathers in the gap. As a result, fused portion X is formed as shown in FIG. 14B. The state in which fused portion X has been formed is shown in FIG. 9A. It is preferable that jigs 41 and 43 are heated, and jigs 42 and 44 may also be heated.

[0065] In the jig 44 of the present disclosure, a portion (a portion facing the bent portion) 44A forming the curved shape of the bent portion in the fused portion X is chamfered. That is, as shown in Fig. 14C, the jig 44 is processed so that the corner of the portion 44A forming the curved shape of the bent portion in the fused portion X is curved. This allows the bent portion at the start point on the side of the side member of the formed fused portion X to be curved. Note that in the jig 42 of the present disclosure, a portion (a portion facing the bent portion) 44A forming the curved shape of the bent portion in the fused portion X is also chamfered.

[0066] It is preferable that the curvature radius C of the chamfered portion of the jig satisfies the following formula (1') and formula (3'). C<(((2Δt(a+b+4t1)) / (4-π)) 1 / 2 )-r...expression (1') C In addition, each symbol in formula (1') and formula (3') represents the following. a: Width of side member (mm) b: Thickness of side member (mm) t1: The sum of the average thickness of the fusion resin layer before fusion and the average thickness of the coating resin layer (mm) t2: The sum of the average thickness of the fused resin layer and the average thickness of the coating resin layer after fusion in the fused part (mm) Δt: t1-t2 (mm) r: average thickness of laminate film (mm) C: Radius of curvature of the chamfered part of the jig (mm)

[0067] ​Furthermore, it is more preferable that the curvature radius C of the chamfered portion of the jig satisfy the following formula (2') and formula (3'). C<(((((a+2t1)(b+2t1)-ab)×0.05) / (4-π)) 1 / 2 )-r...expression (2') C In addition, each symbol in formula (2') and formula (3') represents the following. a: Width of side member (mm) b: Thickness of side member (mm) t1: The sum of the average thickness of the fusion resin layer before fusion and the average thickness of the coating resin layer (mm) r: average thickness of laminate film (mm) C: Radius of curvature of the chamfered part of the jig (mm)

[0068] Furthermore, it is preferable that the radius of curvature C of the chamfered portion of the jig is equal to or greater than the average thickness of the metal layer.

[0069] Here, a description will be given of how the jigs 41, 42, 43, and 44 are pressed into the laminate film 30 and the side surface member 20. When the side surface member has a rectangular shape in side view, the second covering step may include a first adhesion treatment and a second adhesion treatment.

[0070] For example, as shown in Fig. 14B, the shape of the side view of the side surface member 20 is a rectangle, and the short sides of the rectangle (sides facing left and right at the outer edge of the side surface member 20 in Fig. 14B) are the first and third sides, and the long sides of the rectangle (sides facing up and down at the outer edge of the side surface member 20 in Fig. 14B) are the second and fourth sides. In other words, the rectangle has a first side, a second side adjacent to the first side, a third side adjacent to the second side and facing the first side, and a fourth side adjacent to the third side and facing the second side. The first side and the third side correspond to the short sides that constitute the outer edge of the side surface member 20, and the second side and the fourth side correspond to the long sides that constitute the outer edge of the side surface member 20.

[0071] ​First, jigs 42 and 44 are pressed into the side member 20 from the first and third sides, respectively. This causes the laminate film 30 to adhere to the first and third sides, respectively (first adhesion process). Next, jigs 41 and 43 are pressed into the side member 20 from the second and fourth sides, respectively. This causes the laminate film 30 to adhere to the second and fourth sides, respectively (second adhesion process). This forms a fused portion X, as shown in FIG. 9A.

[0072] In the present disclosure, it is preferable that the first side and the third side correspond to the short sides constituting the outer edge of the side member 20, and the second side and the fourth side correspond to the long sides constituting the outer edge of the side member 20. In this case, the unheated jigs 42 and 44 may be pressed in the first adhesion process, and the heated jigs 41 and 43 may be pressed in the second adhesion process. By heating the entire outer edge of the side member 20 only with heat input from the jigs (jigs 41 and 43) on the long side, the structure of the sealing machine can be simplified.

[0073] 5.Battery The battery obtained by the above-mentioned steps is similar to that described above in "A. Battery," and therefore will not be described here.

[0074] The present disclosure is not limited to the above-described embodiments. The above-described embodiments are merely examples, and anything that has substantially the same configuration as the technical idea described in the claims of the present disclosure and exhibits similar effects is included in the technical scope of the present disclosure. [Explanation of symbols]

[0075] 1 Cathode active material layer 2 Negative electrode active material layer 3 Electrolyte layer 4 Positive electrode current collector 5 Negative electrode current collector 10 Electrode body 11 Top part 12 Bottom part 13 First side part 14 Second side part 15 Third side part 16 4th side part 20 Side member 30 Laminating Film 34 Bend 100 batteries

Claims

1. An electrode body; A side surface member disposed on a side surface portion of the electrode body; a laminate film covering the electrode body and the side surface member; A battery comprising: When the battery is viewed from the side of the side member, an outer edge of the side member is located inside an outer edge of the electrode body, the laminate film is disposed so as to cover a surface constituting the outer edge of the side member and a surface constituting the outer edge of the electrode body; A fusion portion in which inner surfaces of the laminate film are fused to each other is disposed on the side surface member, A battery, wherein a bent portion at a starting point of the fused portion on the side member side has a curved shape.

2. The battery according to claim 1 , wherein the laminate film has a metal layer and a fusion resin layer on the inner surface side forming the fusion portion, and the side member has a coating resin layer on the surface in contact with the laminate film.

3. The battery according to claim 2 , wherein a radius of curvature R of the curved shape at the bent portion satisfies the following formulas (1) and (3). R < (((2Δt(a + b + 4t 1 )) / (4 - π))) 1/2 ) - r... Equation (1) R<b / 2...Formula (3) In addition, each symbol in formula (1) and formula (3) represents the following. a: width of the side member (mm) b: thickness of the side member (mm) t 1 : The sum (mm) of the average thickness of the fusion resin layer and the average thickness of the coating resin layer before fusion t 2 : The sum (mm) of the average thickness of the fusion resin layer and the average thickness of the coating resin layer after fusion in the fusion portion Δt:t 1 -t 2 (mm) r: average thickness of the laminate film (mm) R: radius of curvature of the curved shape at the bent portion (mm)

4. The battery according to claim 2 , wherein a radius of curvature R of the curved shape at the bent portion satisfies the following formulas (2) and (3). R < (((((a + 2t 1 )(b + 2t 1 )( - ab))×0.05) / (4 - π)) 1/2 - r... Equation (2) R<b / 2...Formula (3) In addition, each symbol in formula (2) and formula (3) represents the following. a: width of the side member (mm) b: thickness of the side member (mm) t 1 : The sum (mm) of the average thickness of the fusion resin layer and the average thickness of the coating resin layer before fusion r: average thickness of the laminate film (mm) R: radius of curvature of the curved shape at the bent portion (mm)

5. The battery according to claim 2 , wherein a radius of curvature R of the curved shape at the bent portion is equal to or greater than an average thickness of the metal layer.

6. The battery according to claim 1 , wherein the fused portion has no crease marks in areas other than the bent portion.

7. 2. The battery according to claim 1, wherein, when the battery is viewed in a plane from the thickness direction, the fusion portion is continuously arranged from an end position α of the laminate film on the side member side to a position β of the laminate film corresponding to the boundary between the side member and the electrode body.

8. The battery according to claim 1 , wherein the fused portion is disposed at a corner portion that constitutes the outer edge of the side member.

9. The battery according to claim 1 , wherein the side member has a rectangular shape when viewed from the side of the battery.

10. The battery according to claim 1 , wherein a plurality of the fused portions are disposed on the side member.

11. The battery of claim 1 , wherein the side member is a current collecting terminal.

12. The battery includes a pair of the side members, The battery according to claim 1 , wherein the pair of side members are disposed so as to face each other relative to the electrode body.

13. A battery module having a plurality of batteries stacked in a thickness direction, The battery module, wherein the battery is the battery according to claim 1 .

14. 14. The battery module according to claim 13, wherein in a pair of side members adjacent in the thickness direction, a main surface of the laminate film arranged on one of the side members is not in contact with a main surface of the laminate film arranged on the other of the side members.

15. A method for producing the battery according to claim 1, comprising the steps of: a preparation step of preparing a structure having the electrode body and the side surface member, wherein when the battery is viewed from the side of the side surface member, the shape of the side surface member is a rectangle, the rectangle having a first side, a second side adjacent to the first side, a third side adjacent to the second side and facing the first side, and a fourth side adjacent to the third side and facing the second side; a first covering step of covering a surface constituting the outer edge of the electrode body in the structure with the laminate film; A second covering step of covering a surface constituting the outer edge of the side member in the structure with the laminate film; having The second covering step includes: a first adhesion process in which a first jig and a third jig are pressed into the first side and the third side of the side member, respectively, to adhere the laminate film to the first side and the third side, respectively; a second adhesion process in which a second jig and a fourth jig are pressed into the second side and the fourth side of the side member, respectively, after the first adhesion process, to adhere the laminate film to the second side and the fourth side, respectively; having A method for manufacturing a battery, wherein at least one of the first jig and the third jig has a chamfered shape at a location that forms the curved shape of the bent portion in the fused portion.

16. After the preparation step and before the first coating step, A folding process is provided for forming a folding line in advance on the laminate film at a position opposite to a corner of the electrode body, The method for manufacturing a battery according to claim 15 , wherein in the folding step, no folding lines are formed in the laminate film at positions facing the side members.

Citation Information

Patent Citations

  • Bendable electrochemical device for storing energy

    EP3139424A1

  • Thin battery

    JP1999260327A

  • Sealed battery

    JP2002319375A

  • Laminated secondary battery, and battery pack of the same

    JP2005317312A

  • Power storage device and method of manufacturing the same

    JP2010192154A