Energy Storage Module
The power storage module addresses the challenge of increasing parts and pressure release by using a seal portion with communication holes and a sheet member for individual, irreversible space opening, enhancing efficiency and reliability.
Patent Information
- Application Number
- JP2021088518
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-05-26
- Publication Date
- 2024-10-23
- Estimated Expiration
- 2041-05-26
AI Technical Summary
Existing power storage devices face an increase in the number of parts required as the number of laminated bipolar electrodes increases, and they struggle to efficiently release pressure when internal pressure rises.
A power storage module with a seal portion containing communication holes and a sheet member that seals and opens internal spaces individually through a stress concentration point, allowing irreversible pressure release without increasing the number of parts.
The module effectively suppresses the need for additional parts and ensures individual, irreversible opening of internal spaces when pressure increases, maintaining structural integrity and preventing reuse.
Smart Images

Figure 0007571661000001 
Figure 0007571661000002 
Figure 0007571661000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to an energy storage module. [Background technology]
[0002] Patent Document 1 describes an electric storage device. The electric storage device has a plurality of bipolar electrodes stacked with a separator interposed therebetween. The bipolar electrodes have a current collector, a positive electrode layer formed on one surface of the current collector, and a negative electrode layer formed on the other surface of the current collector. The electric storage device has a spacer that maintains the interval between the current collectors of the bipolar electrodes adjacent to each other and forms a storage space between the current collectors. The spacer includes a first seal portion and a second seal portion. The first seal portion has a communication portion that communicates the storage space with the outside. The second seal portion is inserted into the communication portion without a gap, thereby sealing the storage space together with the first seal portion. The second seal portion has a lower pressure resistance against the pressure of the storage space compared to the first seal portion. As a result, when the pressure of the storage space rises to a predetermined threshold value, the second seal portion is pushed out from the storage space side toward the outside of the storage space, thereby releasing the pressure of the storage space. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2018-092717 A Summary of the Invention [Problem to be solved by the invention]
[0004] In the electricity storage device described in Patent Document 1, since the second seal portion is inserted into each of the communication portions, the pressure is released when the internal pressure in each of the storage spaces increases. On the other hand, if the number of bipolar electrodes is increased, it is necessary to prepare the same number of parts such as the second seal portion, which is not preferable.
[0005] Therefore, an object of the present disclosure is to provide an energy storage module that suppresses an increase in the number of parts even when multiple electrodes are stacked, and that is capable of releasing pressure when the internal pressure in each internal space increases. [Means for solving the problem]
[0006] The electricity storage module according to the present disclosure is configured by stacking a plurality of electrodes, each including a current collector and an active material layer formed on the current collector, and includes a laminate having a plurality of internal spaces each including the plurality of active material layers; a sealing portion provided on the current collector so as to seal the plurality of internal spaces, the sealing portion having a plurality of communication holes formed therein for connecting each of the plurality of internal spaces to the outside; and a sheet member provided in the sealing portion across the plurality of communication holes, individually sealing each of the plurality of communication holes and opening each of the plurality of internal spaces to the outside through each of the plurality of communication holes by cleaving, the sheet member including a plurality of opposing portions facing first openings on the opposite side to each of the internal spaces of the plurality of communication holes, and a joint portion provided around each of the plurality of opposing portions so as to surround each of the first openings and joined to the sealing portion, each of the opposing portions being provided with a stress concentration portion that serves as a starting point for cleavage, and a cleavage pressure which is the internal pressure applied to the opposing portions when the stress concentration portions cleave is lower than a peel pressure which is the internal pressure applied to the opposing portions when the joint portion and the sealing portion peel off.
[0007] In this energy storage module, a laminate is formed by stacking a plurality of electrodes including a current collector and an active material layer, and a seal portion is formed on each of the current collectors. A communication hole communicating with an internal space including the active material layer is formed in each of the seal portions. A sheet member is provided collectively across the communication holes in the seal portion, and each of the communication holes is individually sealed. The sheet member includes an opposing portion facing a first opening on the opposite side of the communication hole from the internal space, and a stress concentration portion serving as a starting point of cleavage is formed in the opposing portion. The cleavage pressure, which is the internal pressure applied to the opposing portion when the stress concentration portion cleaves, is lower than the peeling pressure, which is the internal pressure applied to the opposing portion when the joint portion and the seal portion of the sheet member are peeled off. Therefore, when the internal pressure of a certain internal space rises, the sheet member is cleaved starting from the stress concentration portion of the opposing portion facing the communication hole communicating with the internal space, and the internal space is individually and irreversibly opened. In this way, with this energy storage module, by sealing multiple internal spaces at the same time, it is possible to suppress an increase in the number of parts even when multiple electrodes are stacked, and it is possible to release pressure in each internal space when the internal pressure increases.
[0008] In the energy storage module according to the present disclosure, the sheet member may include a first resin layer joined to the sealing portion, and a metal layer laminated on the first resin layer on a side of the first resin layer opposite the sealing portion, in which case the first resin layer ensures adhesion to the sealing portion, and the metal layer suppresses moisture permeation.
[0009] In the energy storage module according to the present disclosure, the sheet member may include a second resin layer laminated on the metal layer on a side of the metal layer opposite the first resin layer, in which case the second resin layer suppresses corrosion and short circuits of the metal layer.
[0010] In the energy storage module according to the present disclosure, the stress concentration portion may include a groove portion formed in at least one of the first resin layer and the second resin layer. In this case, the stress concentration portion can be formed while maintaining the breaking strength of the entire sheet member. In particular, when the groove portion is formed in the second resin layer located relatively outside, when the sheet member is deformed to bulge outward due to an increase in internal pressure in the internal space, pressure can be concentrated more in the groove portion.
[0011] In the energy storage module according to the present disclosure, the stress concentrating portion may include a bent portion formed in the metal layer, In this case, the stress concentrating portion can be formed with a simple configuration.
[0012] In the energy storage module according to the present disclosure, the sealing portion may include an outer surface on which the first opening is formed and a frame portion protruding from the outer surface so as to surround the first opening, and the joining portion may be joined to the frame portion. In this case, the joining portion between the sealing portion of the sheet member and the sealing portion is limited to the frame portion, making joining easier.
[0013] In the electricity storage module according to the present disclosure, a groove extending from one end of the active material layer to the other end of the active material layer may be formed in the active material layer, and a second opening on the internal space side of each of the plurality of communication holes may be formed in a portion of the seal portion facing one end of the active material layer. In this case, gas generated in the internal space is smoothly introduced into the communication hole along the groove of the active material layer, making it possible to cause the sheet member to be quickly torn open.
[0014] In the energy storage module according to the present disclosure, the stack is restrained by a restraining plate along the stacking direction of the electrodes, a groove extending from one end of the restraining plate to the other end of the restraining plate is formed in the restraining plate, and the second opening on the internal space side of each of the plurality of communication holes may be formed in a portion of the seal portion facing one end of the restraining plate as viewed from the stacking direction. In this case, gas generated in the internal space is smoothly introduced into the communication hole along the groove of the restraining plate, making it possible to cause the sheet member to quickly tear.
[0015] In the energy storage module according to the present disclosure, the plurality of communication holes include a first communication hole which is a through hole communicating with an internal space including an active material layer of an electrode of the outermost layer of the laminate, and a second communication hole different from the first communication hole, and the cleavage pressure of the stress concentration portion formed in the facing portion of the plurality of facing portions facing the first opening of the first communication hole may be different from the cleavage pressure of the stress concentration portion formed in the facing portion of the plurality of facing portions facing the first opening of the second communication hole. In general, the manner of internal pressure rise may be different between the internal space corresponding to the electrode of the outermost layer of the laminate and the internal space corresponding to the electrode on the inside of the laminate. Therefore, it may be effective to use stress concentration portions with different cleavage pressures in the outermost layer and the other portions of the laminate. Effect of the Invention
[0016] According to the present disclosure, it is possible to provide an electricity storage module capable of sealing a plurality of internal spaces collectively while individually and irreversibly opening each of the plurality of internal spaces. [Brief description of the drawings]
[0017] [Figure 1] FIG. 1 is a schematic side view showing an electricity storage device according to one embodiment. [Diagram 2] FIG. 2 is a schematic cross-sectional view showing the electricity storage module shown in FIG. [Diagram 3] FIG. 3 is a perspective view of the power storage module shown in FIG. [Figure 4] FIG. 4 is an exploded perspective view (including a partial cross-sectional view) showing a part of FIG. 3 in an enlarged scale. [Diagram 5] FIG. 5 is a schematic cross-sectional view showing a state in which a sheet member is attached to the seal portion shown in FIGS. [Figure 6] FIG. 6 is a plan view showing an example of the sheet member shown in FIG. [Figure 7] FIG. 7 is a plan view showing an example of the sheet member shown in FIG. [Figure 8] FIG. 6 is a cross-sectional view showing an example of the sheet member shown in FIGS. [Figure 9]FIG. 4 is a schematic plan view illustrating the positional relationship between an active material layer and a sheet member. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] Hereinafter, a detailed description will be given of an electric storage device according to an embodiment with reference to the drawings. In each drawing, an orthogonal coordinate system defined by an X-axis, a Y-axis, and a Z-axis may be illustrated. In addition, in the description of each drawing, the same reference numerals may be used to designate the same elements or corresponding elements, and duplicate descriptions may be omitted.
[0019] Fig. 1 is a schematic side view showing an energy storage device according to one embodiment. The energy storage device 1 shown in Fig. 1 is a device used as a battery for various vehicles such as a forklift, a hybrid vehicle, an electric vehicle, etc. The energy storage device 1 includes a module stack 2 including an energy storage module 11, connection members 3 and 4 electrically connected to the module stack 2, a pair of end plates 5 for restraining the module stack 2, and a fastening member 6 for fastening the end plates 5 and 5 together.
[0020] The module stack 2 is configured by stacking a plurality of power storage modules 11 and a plurality of conductive plates P in the Z-axis direction. In the example of FIG. 1, the module stack 2 includes two power storage modules 11 and three conductive plates P. The three conductive plates P are disposed between the power storage modules 11 and at both ends of the module stack 2 in the stacking direction. These conductive plates P are electrically connected to electrodes that constitute the power storage modules 11. Here, the two power storage modules 11 are connected in series by the conductive plates P.
[0021] A plurality of flow paths (not shown) for circulating a cooling medium such as air may be provided inside the conductive plate P. By circulating a cooling medium through the flow paths in the conductive plate P, the conductive plate P functions not only as a connection member for electrically connecting the plurality of power storage modules 11 to each other, but also as a heat dissipation plate for dissipating heat generated in the power storage modules 11. In the example of FIG. 1, the area of the conductive plate P is slightly smaller than the area of the power storage modules 11. From the viewpoint of improving heat dissipation, the area of the conductive plate P may be equal to the area of the power storage modules 11, or may be slightly larger than the area of the power storage modules 11.
[0022] The connection members 3 and 4 are conductive members (bus bars) that function as a positive terminal and a negative terminal of the energy storage device 1. The connection member 3 is electrically connected to the conductive plate P that is the positive electrode side, and the connection member 4 is electrically connected to the conductive plate P that is the negative electrode side. The connection members 3 and 4 are formed of, for example, a metal material or an alloy material. Examples of the metal material include copper, aluminum, titanium, and nickel. Examples of the alloy material include stainless steel plates (SUS301, SUS304, etc.) and alloys of the above-mentioned metal materials. At least one of the connection members 3 and 4 may be provided with a heat dissipation fin (not shown) that has excellent thermal conductivity. In this case, heat generated in the energy storage module 11 can be effectively dissipated through the conductive plate P, the connection members 3 and 4, and the heat dissipation fin.
[0023] The pair of end plates 5 and the fastening members 6 constitute restraining members that apply a restraining load to the module stack 2 in the stacking direction. The pair of end plates 5 are provided to sandwich the module stack 2 in the stacking direction. The end plates 5 are formed, for example, from metal plates. Examples of materials for forming the end plates 5 include alloys such as copper, aluminum, titanium, nickel, and stainless steel. As shown in Figs. 1 and 2, the end plates 5 have a rectangular shape that is one size larger than the shape (rectangular in this case) of the module stack 2 when viewed from the stacking direction. The end plates 5 are arranged concentrically with the module stack 2 when viewed from the stacking direction. As a result, the edges of the four sides of the end plates 5 form protruding portions 5a that protrude outward beyond the sandwiched portion of the module stack 2.
[0024] The fastening members 6 are composed of, for example, bolts 6A and nuts 6B. The bolts 6A are passed through insertion holes 5b provided in the protruding portions 5a of each of the pair of end plates 5, and the pair of end plates 5 are fastened together by screwing in the nuts 6B. As a result, a restraint load is applied to the module stack 2 in the stacking direction via the pair of end plates 5. In this embodiment, when viewed from the stacking direction, the fastening members 6 are disposed at equal intervals on the edges of the four sides of the protruding portions 5a of the end plates 5 so as to include positions corresponding to the corners of the end plates 5.
[0025] 2 is a schematic cross-sectional view showing a layer structure of the power storage module shown in FIG. 1. The power storage module 11 is a single cell having a rectangular parallelepiped shape that is flattened in the Z-axis direction. In this embodiment, a bipolar type lithium ion secondary battery is exemplified as the power storage module 11. The power storage module 11 includes an electrode stack (stack) 12 including a plurality of bipolar electrodes (electrodes) 14, and a sealing portion 13. The bipolar electrodes 14 in the electrode stack 12 are stacked along the Z-axis direction. The stacking direction of the bipolar electrodes 14 is along the Z-axis direction and coincides with the stacking direction of the power storage modules 11 in the module stack 2.
[0026] The bipolar electrode 14 includes a current collector 21, a positive electrode active material layer (active material layer) 22 provided on a first surface 21a of the current collector 21, and a negative electrode active material layer (active material layer) 23 provided on a second surface 21b of the current collector 21. The current collector 21 and the positive electrode active material layer 22 provided on the first surface 21a of the current collector 21 constitute the positive electrode of the bipolar electrode 14, and the current collector 21 and the negative electrode active material layer 23 provided on the second surface 21b of the current collector 21 constitute the negative electrode of the bipolar electrode 14.
[0027] The current collector 21 is a sheet-like conductive member having a rectangular shape in a plan view, and has a first surface 21a and a second surface 21b located on the opposite side of the first surface 21a. The current collector 21 is made of, for example, a metal foil or an alloy foil. Examples of the metal foil include copper foil, aluminum foil, titanium foil, and nickel foil. Examples of the alloy foil include stainless steel foil (e.g., SUS304, SUS316, SUS301, etc., as specified in JIS G 4305:2015), plated steel plate (e.g., cold-rolled steel plate (SPCC, etc.) as specified in JIS G 3141:2005), and plated stainless steel plate. The alloy foil may be an alloy foil of the metals exemplified as the material of the metal foil. The current collector 21 may be formed by integrating a plurality of metal foils, or may be formed by plating another metal on the surface of a metal foil.
[0028] The positive electrode active material layer 22 is a layered member containing a positive electrode active material, a conductive assistant, and a binder. Examples of the positive electrode active material include a composite oxide, metallic lithium, and sulfur. The composition of the composite oxide includes at least one of iron, manganese, titanium, nickel, cobalt, and aluminum, and lithium. Examples of the composite oxide include olivine-type lithium iron phosphate (LiFePO 4 ) are mentioned.
[0029] The binder serves to bind the active material or the conductive assistant to the surface of the current collector 21 and maintain the conductive network in the electrode. Examples of the binder include fluorine-containing resins such as polyvinylidene fluoride, polytetrafluoroethylene, and fluorine rubber, thermoplastic resins such as polypropylene and polyethylene, imide resins such as polyimide and polyamideimide, alkoxysilyl group-containing resins, acrylic resins containing monomer units such as acrylic acid and methacrylic acid, styrene-butadiene rubber (SBR), carboxymethyl cellulose, alginates such as sodium alginate and ammonium alginate, water-soluble cellulose ester crosslinked bodies, and starch-acrylic acid graft polymers. These binders can be used alone or in combination. Examples of the conductive assistant include acetylene black, carbon black, and graphite. The positive electrode active material layer 22 may contain a viscosity adjusting solvent such as N-methyl-2-pyrrolidone (NMP).
[0030] The negative electrode active material layer 23 is a layered member containing a negative electrode active material, a conductive assistant, and a binder. Examples of the negative electrode active material include graphite, artificial graphite, highly oriented graphite, mesocarbon microbeads, hard carbon, soft carbon, and other carbon, metal compounds, elements that can be alloyed with lithium or compounds of such elements, and boron-added carbon. Examples of elements that can be alloyed with lithium include silicon and tin. The conductive assistant and binder may be the same as those used in the positive electrode active material layer 22.
[0031] In the electrode laminate 12, the bipolar electrodes 14 adjacent in the stacking direction are arranged so that the positive electrode active material layer 22 and the negative electrode active material layer 23 face each other. A separator 15 is arranged between the bipolar electrodes 14. In this embodiment, the separator 15 is a sheet-like member having a rectangular shape in a plan view, and prevents short-circuiting between the bipolar electrodes 14 adjacent in the stacking direction. The separator 15 is composed of a porous film made of a polyolefin resin such as polyethylene (PE) or polypropylene (PP). The separator 15 may be composed of a woven or nonwoven fabric made of polypropylene, methylcellulose, or the like. The separator 15 may be reinforced with a vinylidene fluoride resin compound.
[0032] The electrode laminate 12 has a positive terminal electrode (electrode) 16 and a negative terminal electrode (electrode) 17 in addition to the bipolar electrode 14. The positive terminal electrode 16 is composed of a current collector 21 and a positive electrode active material layer 22 provided on a first surface 21a of the current collector 21. The positive terminal electrode 16 is disposed on one end side in the lamination direction of the electrode laminate 12 so that the positive electrode active material layer 22 on the first surface 21a faces the negative electrode active material layer 23 of the terminal bipolar electrode 14. In the positive terminal electrode 16, the negative electrode active material layer 23 is not provided on the second surface 21b of the current collector 21, and the second surface 21b is electrically connected to the adjacent conductive plate P.
[0033] The negative terminal electrode 17 is composed of a current collector 21 and a negative electrode active material layer 23 provided on a second surface 21b of the current collector 21. The negative terminal electrode 17 is disposed on the other end side in the stacking direction of the electrode laminate 12 so that the negative electrode active material layer 23 on the second surface 21b faces the positive electrode active material layer 22 of the terminal bipolar electrode 14. In the negative terminal electrode 17, the positive electrode active material layer 22 is not provided on the first surface 21a of the current collector 21, and the first surface 21a is electrically connected to the adjacent conductive plate P.
[0034] The separators 15 are arranged between the bipolar electrodes 14 adjacent to each other in the stacking direction, as well as between the bipolar electrodes 14 and the positive terminal electrode 16, and between the bipolar electrodes 14 and the negative terminal electrode 17. The arrangement of the separators 15 prevents short circuits between the bipolar electrodes 14 and the positive terminal electrode 16, and between the bipolar electrodes 14 and the negative terminal electrode 17.
[0035] The sealing portion 13 is a portion that seals a side portion of the electrode laminate 12 extending in the stacking direction. When viewed in the stacking direction, the sealing portion 13 has a rectangular frame shape that follows the outer shape of the current collector 21. The sealing portion 13 is welded to the first surface 21a side of the edge portion 21c of the current collector 21. The sealing portion 13 may be further welded to the second surface 21b side of the edge portion 21c of the current collector 21 of another bipolar electrode 14 adjacent to one bipolar electrode 14 in the stacking direction.
[0036] In the positive terminal electrode 16, the sealing portion 13 is welded to both the first surface 21a side and the second surface 21b side of the edge portion 21c of the current collector 21. In the negative terminal electrode 17, the sealing portion 13 is welded to the first surface 21a of the edge portion 21c of the current collector 21.
[0037] The sealing portion 13 is made of, for example, a resin having heat resistance and corrosion resistance against the electrolyte. Examples of such resins include polyimide, polypropylene (PP), polyphenylene sulfide (PPS), and modified polyphenylene ether (modified PPE). An electrolyte (not shown) is accommodated in the internal space S surrounded by the sealing portion 13 and the current collectors 21 adjacent to each other in the stacking direction. The electrolyte is, for example, a carbonate-based or polycarbonate-based electrolyte. A lithium salt is used as a supporting salt contained in the electrolyte. The lithium salt is, for example, LiBF 4 , LiPF 6 , LiN(SO 2 CF 3 ) 2 , LiN(SO 2 C 2 F 5 ) 2 , or a mixture thereof may be used.
[0038] The sealing portion 13 has a protruding portion 13a that protrudes outward beyond the edge of the current collector 21. The protruding portions 13a of the sealing portions 13 adjacent to each other in the stacking direction are welded to each other. As a result, in the electricity storage module 11, the multiple sealing portions 13 form seal portions 30 for sealing each of the internal spaces S.
[0039] In this manner, the electricity storage module 11 is configured by stacking a plurality of bipolar electrodes 14, a positive terminal electrode 16, and a negative terminal electrode 17, and includes an electrode stack 12 having a plurality of internal spaces S including a plurality of active material layers (positive electrode active material layers 22 and / or negative electrode active material layers 23). The electricity storage module 11 also includes a sealing portion 13 (sealing portion 30) provided on the current collector 21 so as to seal the plurality of internal spaces S. In particular, the sealing portion 30 is provided with a configuration for adjusting the internal pressure of the internal space S. This point will be described in more detail below.
[0040] FIG. 3 is a perspective view of the electricity storage module shown in FIG. 2. FIG. 4 is an exploded perspective view (including a partial cross-sectional view) showing an enlarged portion of FIG. 3. As shown in FIGS. 3 and 4, one wall portion 30a constituting the seal portion 30 is provided with a plurality of (four in this case) mounting regions 24 for mounting a sheet member 40 for adjusting the internal pressure of the internal space S. The wall portion 30a is a wall portion including one outer side surface 13b of the sealing portion 13. A plurality of (six in this case) communication holes 30H are provided (opened) in each of the mounting regions 24. Each of the communication holes 30H communicates each of the internal spaces S with the outside. Each of the communication holes 30H communicates with each of the different internal spaces S. Each of the communication holes 30H is provided in each of the sealing portions 13. Each of the communication holes 30H penetrates the sealing portion 13 and reaches each of the internal spaces S. As a result, each of the communication holes 30H communicates with each of the internal spaces S. The communication holes 30H are arranged in three rows and two columns (three rows in the Y-axis direction and two columns in the Z-axis direction) in each of the mounting regions 24. Therefore, the communication holes 30H are arranged in 12 rows and two columns in the wall portion 30a.
[0041] The communication hole 30H has an opening (first opening) 30Ha on one outer side surface 13b of the sealing portion 13 (i.e., the outer surface of the wall portion 30a of the seal portion 30). The opening 30Ha is an opening on the opposite side of the communication hole 30H to the internal space S, and opens to the outer side surface 13b. Each of the mounting regions 24 is provided with a frame portion 27 protruding from the outer surface of the wall portion 30a of the seal portion 30. The frame portion 27 is provided so as to surround each of the openings 30Ha of the communication hole 30H. As a result, the frame portion 27 forms a plurality of (here, six) space portions 30s connected to each of the communication holes 30H. The space portions 30s are separated from each other by the partition wall of the frame portion 27 and are independent. The communication hole 30H and the space portion 30s connected to the communication hole 30H form a flow path 28 for gas from the internal space S.
[0042] FIG. 5 is a schematic cross-sectional view showing a state where a sheet member is attached to the sealing portion shown in FIGS. 3 and 4. FIGS. 6 and 7 are plan views showing an example of the sheet member shown in FIG. 5. As shown in FIGS. 5 to 7, the sheet member 40 is attached to the sealing portion 30 via the frame portion 27. The sheet member 40 is joined to the sealing portion 30 (here, the frame portion 27) by, for example, welding or adhesion. More specifically, the sheet member 40 includes a plurality of facing portions 40a facing the respective openings 30Ha of the communication holes 30H (i.e., facing the space portion 30s), and a joining portion 40b provided around each of the plurality of facing portions 40a so as to surround each of the openings 30Ha and joined to the sealing portion 30 (here, the frame portion 27). That is, the sealing portion 30 includes an outer surface 13b in which an opening 30Ha is formed, and a frame portion 27 protruding from the outer surface 13b so as to surround the opening 30Ha when viewed from a direction intersecting the outer surface 13b, and the joining portion 40b is joined to the frame portion 27.
[0043] The number of opposing portions 40a in one sheet member 40 is the same as the number of communication holes 30H in one mounting region 24, for example, six. As a result, one opposing portion 40a and a joint portion 40b provided around the opposing portion 40a cooperate to seal one communication hole 30H and the space portion 30s connected to the communication hole 30H. In this way, one sheet member 40 is provided in the seal portion 30 across multiple (here, six) communication holes 30H, and individually seals each of the multiple communication holes 30H.
[0044] Here, the sheet member 40 is composed of a plurality of layers. More specifically, the sheet member 40 includes a first resin layer 41, a metal layer 42, and a second resin layer 43, which are laminated on one another. The first resin layer 41 is bonded to the seal portion 30 (frame portion 27). That is, the first resin layer 41 is the layer located closest to the seal portion 30, and also serves as an adhesive layer with the seal portion 30. Therefore, the material of the first resin layer 41 can be arbitrarily selected in consideration of the adhesiveness of the seal portion 30 with the resin material of the frame portion 27.
[0045] The metal layer 42 is laminated on the first resin layer 41 on the side of the first resin layer 41 opposite the seal portion 30. The metal layer 42 is bonded to and integrated with the first resin layer 41. The metal layer 42 maintains the overall pressure resistance strength of the sheet member 40 and has a function of, for example, suppressing moisture penetration into the internal space S in the sheet member 40.
[0046] The second resin layer 43 is laminated on the metal layer 42 on the side of the metal layer 42 opposite to the first resin layer 41. The second resin layer 43 is bonded to and integrated with the metal layer 42. As a result, the first resin layer 41, the metal layer 42, and the second resin layer 43 are integrated as a whole into a laminate film. The second resin layer 43 covers at least the metal layer 42, thereby contributing to suppression of corrosion and short circuits of the metal layer 42.
[0047] The sheet member 40 as described above has a function of opening the internal space S to the outside irreversibly by selectively breaking a portion corresponding to the internal space S when the internal pressure of the internal space S rises. More specifically, in the sheet member 40, a stress concentration portion 50 is formed in each of the facing portions 40a. When the internal pressure of the internal space S, the communication hole 30H, and the space portion 30s rises due to gas generation in the internal space S, and internal pressure is applied to the facing portion 40a so that the facing portion 40a is deformed to bulge outward, the stress concentration portion 50 is a portion that becomes a starting point of rupture of the facing portion 40a due to concentration of tensile stress caused by deformation caused by the internal pressure. The tensile stress generated in the stress concentration portion 50 is proportional to the internal pressure applied to the facing portion 40a. Here, the internal pressure applied to the facing portion 40a when the stress concentration portion 50 ruptures (i.e., the internal pressure at which such tensile stress that the stress concentration portion 50 ruptures) is defined as the rupture pressure.
[0048] In this way, by providing a stress concentration portion 50 in each of the opposing portions 40a of the sheet member 40, when the internal pressure of a certain internal space S rises, the portion corresponding to that internal space S (the opposing portion 40a) is selectively destroyed, making it possible to adjust only the internal pressure of that internal space S.
[0049] As an example, the stress concentration portion 50 may include a groove portion 53g formed in the second resin layer 43 of the sheet member 40, as shown in (a) of FIG. 8. The groove portion 53g may penetrate the second resin layer 43, but may be provided so as not to penetrate the second resin layer 43 from the viewpoint of the corrosion and short circuit suppression function by covering the metal layer 42 of the second resin layer 43. In such a case, the shape of the portion of the second resin layer 43 of the sheet member 40 where the groove portion 53g is provided changes abruptly, and therefore the portion is likely to crack due to stress concentration. Moreover, the strength of at least the portion where the groove portion 53g is provided is relatively reduced compared to other portions.
[0050] As another example, the stress concentration portion 50 may include a groove portion 51g formed in the first resin layer 41 of the sheet member 40, as shown in (b) of FIG. 8. The groove portion 51g may or may not penetrate the first resin layer 41. The facing portion 40a in which the groove portion 51g is provided is not a portion that contributes to the joining of the sheet member 40 to the seal portion 30, so even if the groove portion 51g penetrates the first resin layer 41, the function related to the adhesiveness of the first resin layer 41 is not impaired. In such a case, the shape of the portion in the first resin layer 41 in the sheet member 40 in which the groove portion 51g is provided changes abruptly, so that it is likely to be torn due to stress concentration. Also, at least the portion in which the groove portion 51g is provided has a relatively reduced strength compared to other portions.
[0051] As another example, the stress concentrating portion 50 may include a bent portion 52b formed in the metal layer 42 by bending the entire sheet member 40 as shown in FIG. 8(c). In this case, the shape of the buckled portion of the bent portion 52b of the metal layer 42 changes abruptly, so that the metal layer 42 is more likely to split due to stress concentration. The buckled portion of the bent portion 52b of the metal layer 42 has a relatively lower strength than the other portions. The stress concentrating portion 50 may include a mixture of the grooves 51g, 53g and the bent portion 52b.
[0052] The shape of the stress concentrating portion 50 in plan view may be of various shapes as shown in Figures 6 and 7. For example, in the example shown in Figure 6(a), the stress concentrating portion 50 is formed such that two straight lines (diagonal lines) extending obliquely with respect to the outer edge of the facing portion 40a intersect near the center of the facing portion 40a. Note that the straight lines shown here are at least one of the groove portion 51g, the groove portion 53g, and the bent portion 52b described above (the same applies below).
[0053] In the example shown in Fig. 6(b), the stress concentrating portion 50 is formed such that two straight lines along the outer edge of the facing portion 40a intersect near the center of the facing portion 40a. In the example shown in Fig. 6(c), the stress concentrating portion 50 is formed by a circular (here, elliptical) curve that surrounds the center of the facing portion 40a. Note that, like the straight lines, the curve here is at least one of the groove portion 51g, the groove portion 53g, and the bent portion 52b.
[0054] Further, in the example shown in Fig. 7(a), the stress concentrating portion 50 is formed by one straight line extending in one direction along one of the outer edges of the facing portion 40a, and in the example shown in Fig. 7(b), the stress concentrating portion 50 is formed by another straight line extending in another direction along another outer edge of the facing portion 40a. In this way, various shapes are assumed for the stress concentrating portion 50, and can be appropriately selected according to the required cleavage pressure (ease of cleavage, ease of stress concentration). In other words, in the sheet member 40, the cleavage pressure can be controlled by selecting the shape of the stress concentrating portion 50.
[0055] For example, when a lower cleavage pressure (easy to cleave, high degree of stress concentration) is required, the stress concentration portion 50 may be configured to include two straight lines intersecting each other as shown in (a) and (b) of Figure 6, or when a higher cleavage pressure (hard to cleave, low degree of stress concentration) is required, the stress concentration portion 50 may be configured to include a closed curve (circle, ellipse) without discontinuities or ends as shown in (c) of Figure 6. Alternatively, when a medium cleavage pressure between these is required, the stress concentration portion 50 may be configured to include one straight line as shown in (a) and (b) of Figure 7, or may be configured by appropriately mixing each shape.
[0056] The peeling force generated at the joint 40b is proportional to the internal pressure applied to the facing portion 40a. Here, the internal pressure applied to the facing portion 40a when the joint 40b and the seal portion 30 are peeled off (i.e., the internal pressure that generates a peeling force that breaks the bond between the joint 40b and the seal portion 30) is defined as the peeling pressure. In the sheet member 40, the cleavage pressure of the stress concentration portion 50 is adjusted to be lower than the peeling pressure of the joint 40b so that the cleavage starting from the stress concentration portion 50 of the facing portion 40a is more likely to occur than the bond between the joint 40b and the seal portion 30 being broken. As a result, when the internal pressure of a certain internal space S rises and internal pressure is applied to the facing portion 40a facing the communication hole 30H communicating with that internal space S, the bond between the seal portion 30 and the joint 40b around the facing portion 40a is broken, and the communication between the problematic internal space S and another internal space S is prevented. Furthermore, the internal pressure acting on the facing portion 40a when the sheet member 40 (the portion of the facing portion 40a where the stress concentration portion 50 is not present) breaks is higher than the cleavage pressure and the peeling pressure.
[0057] In general, the manner of internal pressure increase may be different between the internal space S (internal space S including the active material layer of the positive terminal electrode 16 or the active material layer of the negative terminal electrode 17) corresponding to the outermost layer positive terminal electrode 16 and the negative terminal electrode 17 of the electrode laminate 12 and the internal space S (internal space S including only the active material layer of the bipolar electrode 14) corresponding to the inner bipolar electrode 14 of the electrode laminate 12. This is considered to be due to the fact that, since the electrode laminate 12 is restrained by the conductive plate (restraint plate) P along the lamination direction, the positive terminal electrode 16 and the negative terminal electrode 17 of the outermost layer are not easily deformed in the portion overlapping the conductive plate P, but the portion outside the conductive plate P may be more easily deformed in response to the internal pressure increase than the inner bipolar electrode 14. For this reason, the shape of the stress concentration portion 50 may be changed between the outermost layer and the inner layer.
[0058] That is, the plurality of communication holes 30H include a first communication hole 31H, which is a communication hole 30H communicating with an internal space S including an active material layer of the positive electrode terminal electrode 16 (or the negative electrode terminal electrode 17) of the outermost layer of the electrode laminate 12, and a second communication hole 32H different from (other than) the first communication hole 31H (see FIG. 6(c)), and the cleavage pressure of the stress concentration portion 50 formed in the facing portion 40a facing the opening 30Ha of the first communication hole 31H among the plurality of facing portions 40a can be made different from the cleavage pressure of the stress concentration portion 50 formed in the facing portion 40a facing the opening 30Ha of the second communication hole 32H among the plurality of facing portions 40a. In the example of FIG. 7(c), the stress concentration portion 50 corresponding to the outermost layer has a relatively large cleavage pressure, but conversely, the stress concentration portion 50 corresponding to the outermost layer may have a relatively small cleavage pressure.
[0059] 9, in the electricity storage module 11, for example, the positive electrode active material layer 22 is provided with a groove 22g extending from one end 22a to the other end 22b of the positive electrode active material layer 22 in a direction intersecting with the stacking direction. The opening (second opening) 30Hb on the internal space S side of each of the communication holes 30H is formed in a portion of the seal part 30 (sealing part 13) facing one end 22a of the positive electrode active material layer 22. That is, among the sides of the rectangular frame-shaped seal part 30 (sealing part 13), the communication hole 30H is provided on the side that intersects with the extending direction of the groove 22g and faces one end 22a of the positive electrode active material layer 22. Note that, although the positive electrode active material layer 22 is shown in the illustrated example, the negative electrode active material layer 23 (or only the negative electrode active material layer 23) may also have a similar configuration.
[0060] Furthermore, the conductive plate P that restrains the electrode stack 12 may be configured in a similar manner. That is, a groove extending from one end to the other end of the conductive plate P in a direction intersecting the stacking direction may be formed in the conductive plate P, and the opening 30Hb on the internal space S side of each of the communication holes 30H may be formed in a portion of the seal portion 30 facing the one end of the conductive plate P when viewed from the stacking direction. That is, the communication hole 30H may be provided in one of the sides of the rectangular frame-shaped seal portion 30 (sealing portion 13) that intersects with the extending direction of the groove and is close to the one end of the conductive plate P.
[0061] As described above, the energy storage module 11 is configured by stacking a plurality of electrodes (bipolar electrode 14, positive terminal electrode 16, and negative terminal electrode 17) including a current collector and an active material layer formed on the current collector, and is equipped with an electrode stack 12 having a plurality of internal spaces S including each of the plurality of active material layers, a sealing portion 30 provided on the current collector so as to seal the plurality of internal spaces S and having a plurality of communication holes 30H formed therein for connecting each of the plurality of internal spaces S to the outside, and a sheet member 40 provided in the sealing portion 30 across the plurality of communication holes 30H, individually sealing each of the plurality of communication holes 30H and opening each of the plurality of internal spaces S to the outside via each of the plurality of communication holes 30H when opened. The sheet member 40 includes a plurality of facing portions 40a facing the openings 30Ha on the opposite side to the internal spaces S of the respective communication holes 40H, and a joint portion 40b provided around each of the facing portions 40a so as to surround each of the openings 30Ha and joined to the seal portion 30. Each of the facing portions 40a is provided with a stress concentration portion 50 which serves as a starting point for cleavage. A cleavage pressure, which is an internal pressure applied to the facing portions 40a when the stress concentration portion 50 cleaves, is lower than a peeling pressure, which is an internal pressure applied to the facing portions 40a when the joint portion 40b of the sheet member 40 and the seal portion 30 are peeled off.
[0062] Therefore, in this storage module 11, when the internal pressure of a certain internal space S rises, the sheet member 40 is torn from the stress concentration portion 50 of the facing portion 40a facing the communication hole 30H communicating with the internal space S as a starting point, and the internal space S is individually released. In this way, according to this storage module 11, by sealing a plurality of internal spaces S collectively, it is possible to suppress an increase in the number of parts even if a plurality of electrodes are stacked, and to release the pressure when the internal pressure rises in each of the internal spaces. In addition, when a lithium ion secondary battery is used as the storage module 11, there is a risk that moisture may enter the internal space S after the sealing is released and the internal pressure is released, so that it may not be preferable to reuse the storage module 11 after it is released. In contrast, in the storage module 11, the internal pressure is irreversibly released by the tearing of the sheet member 40, so that it is possible to suppress the reuse of the storage module 11 in such a case.
[0063] Moreover, in the electricity storage module 11, the sheet member 40 includes a first resin layer 41 joined to the seal portion 30, and a metal layer 42 laminated on the first resin layer 41 on the side of the first resin layer 41 opposite the seal portion 30. Therefore, the first resin layer 41 ensures adhesion to the seal portion 30, and the metal layer 42 suppresses moisture penetration into the internal space S.
[0064] Furthermore, in the electricity storage module 11, the sheet member 40 includes a second resin layer 43 laminated on the metal layer 42 on the side of the metal layer 42 opposite to the first resin layer 41. Therefore, the second resin layer 43 suppresses corrosion and short-circuiting of the metal layer 42.
[0065] Furthermore, in the power storage module 11, the stress concentrating portion 50 may include groove portions 51g, 53g formed in at least one of the first resin layer 41 and the second resin layer 43. In this case, the stress concentrating portion 50 can be formed while maintaining the breaking strength of the entire sheet member 40. In particular, when the groove portion 53g is formed in the second resin layer 43 located relatively outside, when the sheet member 40 is deformed so as to bulge outward due to an increase in the internal pressure of the internal space S, the tensile stress can be further concentrated in the groove portion 53g.
[0066] In the electricity storage module 11, the stress concentrating portion 50 may include a bent portion 52b formed in the metal layer 42. In this case, the stress concentrating portion 50 can be formed with a simple structure.
[0067] Moreover, in the electricity storage module 11, the seal portion 30 includes the outer side surface 13b in which the opening 30Ha is formed, and a frame portion 27 protruding from the outer side surface 18a so as to surround the opening 30Ha, and the joint portion 40b is joined to the frame portion 27. For this reason, the joint portion between the sheet member 40 and the seal portion 30 is limited to the frame portion 27, making it easier to join.
[0068] Furthermore, in the electricity storage module 11, a groove 22g extending from one end 22a to the other end 22b of the positive electrode active material layer 22 (or the negative electrode active material layer 23) is formed, and the opening 30Hb on the internal space S side of each of the multiple communication holes 30H is formed in a portion facing the one end 22a in the seal portion 30. As a result, gas generated in the internal space S is smoothly introduced into the communication hole 30H along the groove 22g, and the sheet member 40 can be quickly torn open.
[0069] Furthermore, in the electricity storage module 11, the electrode stack 12 is restrained by the conductive plate P along the stacking direction of the bipolar electrodes 14, etc., and a groove extending from one end to the other end of the conductive plate P may be formed in the conductive plate P. In this case, the opening 30Hb on the internal space S side of each of the multiple communication holes 30H may be formed in a portion of the seal portion 30 facing that end of the conductive plate P when viewed from the stacking direction. In this case, gas generated in the internal space S is smoothly introduced into the communication hole 30H along the groove of the conductive plate P, making it possible to cause the sheet member 40 to split quickly.
[0070] Furthermore, in the energy storage module 11, the multiple communication holes 30H include a first communication hole 31H that is a communication hole 30H that communicates with an internal space S including an active material layer of an electrode (positive terminal electrode 16 or negative terminal electrode 17) of the outermost layer of the electrode stack 12, and a second communication hole 32H that is different from the first communication hole 31H, and the cleavage pressure of the stress concentration portion 50 formed in the facing portion 40a facing the opening 30Ha of the first communication hole 31H among the multiple facing portions 40a may be different from the cleavage pressure of the stress concentration portion 50 formed in the facing portion 40a facing the opening 30Ha of the second communication hole 32H among the multiple facing portions 40a. In general, the manner of internal pressure increase may be different between the internal space S corresponding to the positive terminal electrode 16 or negative terminal electrode 17 of the outermost layer of the electrode stack 12 and the internal space S corresponding to the bipolar electrode 14 on the inside of the electrode stack 12. Therefore, it may be effective to use the stress concentrating portion 50 having different cleavage pressures in the outermost layer of the electrode laminate 12 and the remaining layers.
[0071] The above embodiment describes one aspect of the present disclosure. Therefore, the present disclosure is not limited to the above description and may be modified in any manner.
[0072] For example, in the above embodiment, the sheet member 40 is illustrated as being composed of three layers, namely, the first resin layer 41, the metal layer 42, and the second resin layer 43. However, the sheet member 40 may be composed of the first resin layer 41 and the metal layer 42, or may include at least one layer of the first resin layer 41, the metal layer 42, and the second resin layer 43.
[0073] In the above embodiment, an example has been described in which the seal portion 30 (sealing portion 13) includes the frame portion 27, and the sheet member 40 is joined to this frame portion 27. However, the seal portion 30 may not be provided with the frame portion 27, and the sheet member 40 may be joined to a flat surface of the seal portion 30.
[0074] Furthermore, in the above embodiment, the groove 22g is provided in the positive electrode active material layer 22, and the positional relationship between the groove 22g and the communicating hole 30H and the sheet member 40 is specified. However, the positive electrode active material layer 22 does not necessarily need to be provided with the groove 22g, and even if the groove 22g is provided, the positional relationship between the communicating hole 30H and the sheet member 40 may be changed. [Explanation of symbols]
[0075] 11...energy storage module, 12...electrode laminate (laminate), 14...bipolar electrode (electrode), 16...positive electrode terminal electrode (electrode), 17...negative electrode terminal electrode (electrode), 21...current collector, 22...positive electrode active material layer (active material layer), 22g...groove, 23...negative electrode active material layer (active material layer), 27...frame portion, 30...seal portion, 30H...communicating hole, 30Ha...opening (first opening), 30Hb...opening (second opening), 31H...first communicating hole, 32H...second communicating hole, 40...sheet member, 40a...opposing portion, 40b...joint portion, 41...first resin layer, 42...metal layer, 43...second resin layer, 50...stress concentration portion, 51g, 53g...groove portion, 52b...bent portion, P...conductive plate (restraint plate), S...internal space.
Claims
1. a laminate including a plurality of electrodes, each of which includes a current collector and an active material layer formed on the current collector, the laminate having a plurality of internal spaces each including a plurality of the active material layers; a seal portion provided on the current collector so as to seal the plurality of internal spaces, the seal portion having a plurality of communication holes for connecting each of the plurality of internal spaces to the outside; a sheet member provided in the seal portion across the plurality of communication holes, for individually sealing each of the plurality of communication holes and for opening each of the plurality of internal spaces to the outside through each of the plurality of communication holes by rupturing; Equipped with the sheet member includes a plurality of opposed portions opposed to first openings on the opposite side of the internal space of each of the plurality of communication holes, and a joining portion provided around each of the plurality of opposed portions so as to surround each of the first openings and joined to the seal portion, Each of the opposing portions is provided with a stress concentration portion that serves as a starting point for the cleavage, a cleavage pressure, which is an internal pressure applied to the opposing portion when the stress concentration portion cleaves, is lower than a peeling pressure, which is an internal pressure applied to the opposing portion when the joint portion and the seal portion peel off from each other; Energy storage module.
2. The sheet member includes a first resin layer joined to the seal portion, and a metal layer laminated on the first resin layer on a side of the first resin layer opposite to the seal portion. The energy storage module according to claim 1 .
3. The sheet member includes a second resin layer laminated on the metal layer on a side of the metal layer opposite to the first resin layer. The power storage module according to claim 2 .
4. The stress concentration portion includes a groove portion formed in at least one of the first resin layer and the second resin layer. The power storage module according to claim 3 .
5. the stress concentration portion includes a bent portion formed in the metal layer, The storage module according to any one of claims 2 to 4.
6. The seal portion includes an outer surface on which the first opening is formed, and a frame portion protruding from the outer surface so as to surround the first opening, The joint portion is joined to the frame portion. The storage module according to any one of claims 1 to 5.
7. A groove is formed in the active material layer, the groove extending from one end of the active material layer to the other end of the active material layer, a second opening of each of the plurality of communication holes on the internal space side is formed in a portion of the seal portion facing the one end of the active material layer; The storage module according to any one of claims 1 to 6.
8. the stack is restrained by a restraint plate along a stacking direction of the electrodes, The restraint plate has a groove formed therein that extends from one end to the other end of the restraint plate, a second opening on the internal space side of each of the plurality of communication holes is formed in a portion of the seal portion facing the one end of the restraint plate as viewed from the stacking direction; The storage module according to any one of claims 1 to 7.
9. the plurality of communicating holes include first communicating holes which are communicating holes communicating with the internal space including the active material layer of the electrode in the outermost layer of the laminate, and second communicating holes different from the first communicating holes, the cleavage pressure of the stress concentrating portion formed in the facing portion of the plurality of facing portions facing the first opening of the first communication hole is different from the cleavage pressure of the stress concentrating portion formed in the facing portion of the plurality of facing portions facing the first opening of the second communication hole, The storage module according to any one of claims 1 to 8.
Citation Information
Patent Citations
Film-packaged electric device and film-packaged electric device aggregate
JP2006179442A
Bipolar battery assembly
JP2014534582A
Power storage device
JP2018092717A
Electrical device with film covering, frame member, and housing system for electrical device with film covering
WO2005096412A1
Power source device
WO2016132404A1