Battery manufacturing method and battery
Patent Information
- Application Number
- JP2022043977
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-03-18
- Publication Date
- 2024-10-23
- Estimated Expiration
- 2042-03-18
AI Technical Summary
【0013】 本開示によれば、集電端子と外装体との間に空隙が発生することを抑制し、熱溶着不良を抑制することができる。
Smart Images

Figure 0007571757000001 
Figure 0007571757000002 
Figure 0007571757000003
Abstract
Description
[Technical field]
[0001] The present application relates to a method for manufacturing a battery and to a battery. [Background technology]
[0002] Conventionally, laminated batteries have been known in which a power generating element is sealed with a laminate film. A laminated battery has a structure in which a current collector terminal connected to the power generating element extends to the outside, and the current collector terminal is sandwiched between the laminate films and heat-welded.
[0003] In recent years, in order to meet the demand for high performance batteries, it has been considered to increase the thickness of the current collector terminal. However, when the thickness of the current collector terminal is increased, there is a problem that a gap occurs between the current collector terminal, particularly the end of the current collector terminal in the width direction, and the laminate film. When a gap occurs, the airtightness of the laminated battery is impaired, moisture enters from the outside, and the power generating element deteriorates. In addition, in the case of a liquid battery, there is a problem that the internal electrolyte leaks to the outside through the gap. Therefore, it is necessary to suppress such poor thermal welding.
[0004] To address this problem, Patent Document 1 discloses a laminated battery having current collector terminals whose thickness gradually decreases toward the outside in the width direction. With such a laminated battery, gaps are less likely to occur between the ends of the current collector terminals and the laminate film. [Prior art documents] [Patent documents]
[0005] [Patent Document 1] JP 2006-164784 A Summary of the Invention [Problem to be solved by the invention]
[0006] The laminated battery described in Patent Document 1 certainly makes it difficult for gaps to occur between the end of the current collector terminal and the laminate film. However, due to manufacturing tolerances, there is a possibility that gaps may occur between the end of the current collector terminal and the laminate film during thermal welding. Therefore, the technology disclosed in Patent Document 1 has room for improvement.
[0007] Therefore, a main object of the present application is to provide a battery manufacturing method and a battery capable of suppressing thermal welding defects. [Means for solving the problem]
[0008] The present disclosure provides, as one aspect for solving the above-mentioned problems, a manufacturing method for a battery including a power generating element, an exterior body that houses the power generating element, and a current collecting terminal that is electrically connected to the power generating element and disposed so as to extend outward from the exterior body, the manufacturing method including an arrangement step of arranging a resin layer along at least one surface in a thickness direction of the current collecting terminal connected to the power generating element, an accommodation step of accommodating the power generating element in the exterior body, and a sealing step of sealing the power generating element in the exterior body by thermal welding, wherein in the sealing step, the resin layer and the exterior body are thermally welded, and the current collecting terminal has a terminal flat portion having a constant thickness and a terminal flat portion connected to the terminal flat portion. and a terminal inclined portion whose thickness decreases toward the outside in the width direction, the terminal inclined portion being formed on at least one end of the current collecting terminal, the resin layer having a resin layer flat portion arranged along the surface of the terminal flat portion, and a resin layer inclined portion connected to the resin layer flat portion and arranged along the surface of the terminal inclined portion, wherein in an arrangement step, when an angle formed by a straight line extending from the terminal flat portion and the terminal inclined portion is θ1, and an angle formed by a straight line extending from the resin layer flat portion and the resin layer inclined portion is θ2, the resin layer is arranged on the current collecting terminal such that θ1>θ2.
[0009] The above manufacturing method may be such that, in the sealing step, when the angle formed by the terminal flat portion and a straight line extending from the terminal inclined portion is θ3, and the angle formed by the resin layer flat portion and a straight line extending from the resin layer inclined portion is θ4, the power generating element is sealed in the exterior body such that θ3 and θ4 satisfy θ3>θ4. Alternatively, in the above manufacturing method, the resin layer has, in the length direction, a first region that is welded to the outer casing and a second region that is not welded to the outer casing, the first region of the resin layer comprises a first region flat portion arranged along the surface of the terminal flat portion, and a first region inclined portion connected to the first region flat portion and arranged along the surface of the terminal inclined portion, and the second region of the resin layer comprises a second region flat portion arranged along the surface of the terminal flat portion and a second region inclined portion connected to the second region flat portion and arranged along the surface of the terminal inclined portion, and in the sealing process, when the angle formed by the first region flat portion and a straight line extending through the first region inclined portion is θ5, and the angle formed by the second region flat portion and a straight line extending through the second region inclined portion is θ6, the power generating element may be sealed in the outer casing such that θ5>θ6.
[0010] As one aspect for solving the above-mentioned problems, the present disclosure provides a battery comprising: a power generating element; an exterior body that houses the power generating element; a current collecting terminal that is electrically connected to the power generating element and arranged to extend outward from the exterior body; and a resin layer that is arranged along at least one surface in a thickness direction of the current collecting terminal and is arranged between the current collecting terminal and the exterior body, wherein the resin layer and the exterior body are heat-welded, the current collecting terminal comprises a terminal flat portion having a constant thickness, and a terminal inclined portion that is connected to the terminal flat portion and whose thickness decreases toward the outside in the width direction, the terminal inclined portion is formed on at least one end of the current collecting terminal, and the resin layer comprises a resin layer flat portion that is arranged along the surface of the terminal flat portion, and a resin layer inclined portion that is connected to the resin layer flat portion and arranged along the surface of the terminal inclined portion, wherein θ3 is an angle formed by the terminal flat portion and the terminal inclined portion, and θ4 is an angle formed by the resin layer flat portion and the resin layer inclined portion, and θ3 and θ4 satisfy θ3>θ4.
[0011] As one aspect for solving the above-mentioned problems, the present disclosure provides a battery comprising: a power generating element; an exterior body that houses the power generating element; a current collecting terminal that is electrically connected to the power generating element and disposed so as to extend outward from the exterior body; and a resin layer that is disposed along at least one surface in a thickness direction of the current collecting terminal and disposed between the current collecting terminal and the exterior body, the resin layer being heat welded to the exterior body, the current collecting terminal comprising: a terminal flat portion having a constant thickness; and a terminal inclined portion that is connected to the terminal flat portion and has a thickness that decreases toward the outside in the width direction, the terminal inclined portion being formed on at least one end portion of the current collecting terminal, and the resin layer has a first region that is welded to the exterior body in the longitudinal direction; and a second region that is not welded to the outer casing, wherein the first region of the resin layer comprises a first region flat portion arranged along the surface of the terminal flat portion, and a first region inclined portion connected to the first region flat portion and arranged along the surface of the terminal inclined portion, and the second region of the resin layer comprises a second region flat portion arranged along the surface of the terminal flat portion, and a second region inclined portion connected to the second region flat portion and arranged along the surface of the terminal inclined portion, wherein θ5 is the angle formed by the first region flat portion and a straight line extending through the first region inclined portion, and θ6 is the angle formed by the second region flat portion and a straight line extending through the second region inclined portion, such that θ5 and θ6 satisfy θ5>θ6.
[0012] As one aspect for solving the above-mentioned problems, the present disclosure provides a battery intermediate comprising: a power generating element; a current collecting terminal electrically connected to the power generating element; and a resin layer arranged along at least one surface in a thickness direction of the current collecting terminal, wherein the current collecting terminal comprises a terminal flat portion having a constant thickness; and a terminal inclined portion connected to the terminal flat portion and having a thickness that decreases outward in the width direction, the terminal inclined portion being formed on at least one end of the current collecting terminal, and the resin layer has a resin layer flat portion arranged along the surface of the terminal flat portion, and a resin layer inclined portion connected to the resin layer flat portion and arranged along the surface of the terminal inclined portion, wherein θ1 is the angle formed by a straight line extending from the terminal flat portion and the terminal inclined portion, and θ2 is the angle formed by the resin layer flat portion and the straight line extending from the resin layer inclined portion, and θ1 and θ2 satisfy θ1>θ2. Effect of the Invention
[0013] According to the present disclosure, it is possible to prevent the occurrence of gaps between the current collecting terminal and the exterior body, and to prevent poor thermal welding. [Brief description of the drawings]
[0014] [Figure 1] 1 is a flowchart of a method for manufacturing a battery according to one embodiment. [Diagram 2] FIG. 1 is a perspective view of a battery 100 manufactured by a battery manufacturing method according to one embodiment. [Diagram 3] FIG. 2 is an exploded perspective view of the battery 100. [Figure 4] 2 is a perspective view simply illustrating a state in which a resin layer 40 is disposed on a current collecting terminal 20. FIG. [Diagram 5] 1 is a perspective view of a battery intermediate 90 produced in a placement step S1. FIG. [Figure 6] (a) is a cross-sectional view taken along line VI-VI in Fig. 5. (b) is an exploded cross-sectional view of (a). [Figure 7] 11 is another embodiment of the current collecting terminal 30. [Figure 8] 1A to 1C are diagrams showing, in time sequence, how a resin layer 40 is thermally welded to a current collecting terminal 30 using a heat bar 50. [Figure 9] 1A to 1C are diagrams showing, in time sequence, how a resin layer 40 and an exterior body 20 are thermally welded together using a heat bar 60. [Figure 10] 1A is a schematic diagram showing a case where a sealing step is performed using a battery intermediate body where θ1≦θ2, and FIG. 1B is a cross-sectional view of the battery after the sealing step. [Figure 11] 2 is an exploded cross-sectional view of a portion where the resin layer 40 and the exterior body 20 are thermally welded together. FIG. [Figure 12] 2 is a perspective view of the vicinity of a current collecting terminal 30 of the battery 100. FIG. [Figure 13] 12(a) is an exploded cross-sectional view taken along line aa in Fig. 12 (an exploded cross-sectional view of the first region 40a), and (b) is an exploded cross-sectional view taken along line bb in Fig. 12 (an exploded cross-sectional view of the second region 40b). DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] [Battery manufacturing method] The manufacturing method of the battery of the present disclosure will be described with reference to one embodiment of the manufacturing method. Fig. 1 shows a flow chart of the manufacturing method of one embodiment. Fig. 2 shows a perspective view of a battery 100 manufactured by the manufacturing method of one embodiment. Fig. 3 shows an exploded perspective view of the battery 100. Here, in this specification, the x direction shown in Fig. 2 is defined as the length direction (length direction of the battery 100), the y direction is defined as the width direction (width direction of the battery 100), and the z direction is defined as the thickness direction (thickness direction of the battery 100). The x, y, and z directions are perpendicular to each other.
[0016] One embodiment of the manufacturing method is a method for manufacturing a battery 100 including a power generating element 10, an outer casing 20 that houses the power generating element 10, and a current collecting terminal 30 that is electrically connected to the power generating element 10 and arranged to extend outward from the outer casing 20, and includes an arrangement process S1, an accommodation process S2, and a sealing process S3, as shown in Figure 1.
[0017] 3, in one embodiment of the manufacturing method, a predetermined resin layer 40 is disposed on a current collecting terminal 30 to manufacture a battery 100. Each step will be described below.
[0018] <Placement process S1> The arrangement step S1 is a step of arranging the resin layer 40 along at least one surface in the thickness direction of the current collector terminal 20 connected to the power generating element 10. The arrangement step S1 makes it possible to manufacture a battery intermediate 90.
[0019] Fig. 4 shows a perspective view illustrating in a simplified manner how the resin layer 40 is disposed on the current collecting terminal 20. Fig. 5 shows a perspective view of a battery intermediate body 90. Fig. 6(a) shows a cross-sectional view taken along line VI-VI in Fig. 5, and Fig. 6(b) shows an exploded cross-sectional view of Fig. 6(a).
[0020] (Power generation element 10) The power generating element 10 may be a power generating element of a chemical battery such as a lithium ion battery, a nickel metal hydride battery, or a nickel cadmium battery. The power generating element 10 may also be a power generating element of a physical battery such as a capacitor. Furthermore, the power generating element 10 may be a laminated type or a wound type. The power generating element 10 may also be a solid-state battery or a liquid battery. An example of a power generating element 10 for a laminated type lithium ion secondary battery is shown below. However, the power generating element of the present disclosure is not limited thereto.
[0021] The power generating element 10 is formed by stacking a positive electrode current collector foil, a positive electrode active material layer, an electrolyte layer, a negative electrode active material layer, and a negative electrode current collector foil (hereinafter, these may be collectively referred to as "electrode elements"). The electrode elements are stacked in the thickness direction. The number of each electrode element to be stacked is not particularly limited. The electrode elements may be stacked so as to be electrically connected in series, or so as to be electrically connected in parallel.
[0022] The power generating element 10 has a sheet-like shape and is rectangular in plan view. However, the shape of the power generating element 10 is not particularly limited as long as it has a shape that can be accommodated inside the exterior 20. Each current collecting foil of the power generating element 10 may have a tab for connecting to each current collecting terminal 30. A positive electrode tab is provided on each positive current collecting foil and is electrically connected to the positive current collecting terminal. Similarly, a negative electrode tab is provided on each negative current collecting foil and is electrically connected to the negative current collecting terminal.
[0023] The positive electrode current collector foil and the negative electrode current collector foil are sheet-shaped metal foils. The metal constituting the positive electrode current collector foil and the negative electrode current collector foil is not particularly limited, but examples thereof include Cu, Ni, Cr, Au, Pt, Ag, Al, Fe, Ti, Zn, Co, stainless steel, etc. The metal constituting the positive electrode current collector foil is preferably Al. The material constituting the negative electrode current collector foil is preferably Cu.
[0024] The positive and negative current collector foils may have some coating layer (e.g., a carbon coating layer) on their surfaces to adjust the resistance. The thickness of the positive and negative current collector foils may be, for example, 0.1 μm or more and 1 mm or less.
[0025] The positive electrode active material layer is a sheet-like layer containing a positive electrode active material. The positive electrode active material is not particularly limited as long as it is a positive electrode active material that can be used in a lithium ion secondary battery. For example, various lithium-containing composite oxides such as lithium cobalt oxide, lithium nickel oxide, lithium manganate, lithium nickel cobalt manganate, and spinel-based lithium compounds can be mentioned.
[0026] The positive electrode active material layer may optionally contain a conductive assistant and a binder. The binder is not particularly limited as long as it is a binder that can be used in lithium ion secondary batteries. Examples include butadiene rubber (BR), butylene rubber (IIR), acrylate butadiene rubber (ABR), polyvinylidene fluoride (PVdF), and the like. The conductive assistant is not particularly limited as long as it is a conductive assistant that can be used in lithium ion secondary batteries. Examples include carbon materials such as acetylene black and ketjen black, and metal materials such as nickel, aluminum, and stainless steel.
[0027] When the battery 100 is an all-solid-state battery, the positive electrode active material layer may optionally contain a solid electrolyte. The solid electrolyte is not particularly limited as long as it is a solid electrolyte that can be used in a lithium ion secondary battery. For example, it may be an organic polymer electrolyte or an inorganic solid electrolyte. An inorganic solid electrolyte is preferable. This is because it has higher ionic conductivity and superior heat resistance compared to an organic polymer electrolyte. The inorganic solid electrolyte may be an oxide solid electrolyte or a sulfide solid electrolyte. A sulfide solid electrolyte is preferable. Examples of oxide solid electrolytes include lithium lanthanum zirconate, LiPON, Li 1+X AlXGe 2-X(PO4)3, Li-SiO-based glass, Li-Al-SO-based glass, etc. Examples of sulfide solid electrolytes include Li2S-P2S5, Li2S-SiS2, LiI-Li2S-SiS2, LiI-Si2S-P2S5, Li2S-P2S5-LiI-LiBr, LiI-Li2S-P2S5, LiI-Li2S-P2O5, LiI-Li3PO4-P2S5, Li2S-P2S5-GeS2, etc.
[0028] The content of each component in the positive electrode active material layer may be appropriately set depending on the purpose. The surface of the positive electrode active material may be covered with an oxide layer such as a lithium niobate layer, a lithium titanate layer, or a lithium phosphate layer. The thickness of the positive electrode active material layer may be, for example, 0.1 μm or more and 1 mm or less.
[0029] The negative electrode active material layer is a sheet-like layer containing a negative electrode active material. The negative electrode active material is not particularly limited as long as it is a negative electrode active material that can be used in a lithium ion secondary battery. For example, silicon and Si alloys, silicon-based active materials such as silicon oxide, carbon-based active materials such as graphite and hard carbon, various oxide-based active materials such as lithium titanate, metallic lithium, lithium alloys, etc. can be mentioned.
[0030] The negative electrode active material layer may optionally contain a conductive additive or a binder. The conductive additive and the binder may be appropriately selected from the conductive additives and the binders that can be used in the positive electrode active material layer. In addition, when the battery 100 is an all-solid-state battery, the negative electrode active material layer may optionally contain a solid electrolyte. The solid electrolyte may be appropriately selected from the solid electrolytes that can be used in the positive electrode active material layer.
[0031] The content of each component in the negative electrode active material layer may be appropriately set depending on the purpose. The thickness of the negative electrode active material layer may be, for example, 0.1 μm or more and 1 mm or less.
[0032] When the battery 100 is an all-solid-state battery, the electrolyte layer is a sheet-shaped solid electrolyte layer. The solid electrolyte layer includes a solid electrolyte. The solid electrolyte can be appropriately selected from solid electrolyte layers that can be used in the positive electrode active material layer. The solid electrolyte layer may also include a binder. The binder can be appropriately selected from binders that can be used in the positive electrode active material layer. The content of each component in the solid electrolyte layer may be appropriately set depending on the purpose. The thickness of the solid electrolyte layer may be, for example, 0.1 μm or more and 1 mm or less.
[0033] When the battery 100 is a liquid battery, the electrolyte layer includes an electrolyte and a separator. The electrolyte and the separator are not particularly limited as long as they are electrolyte and separator that can be used in a lithium ion secondary battery. The separator may be, for example, a porous sheet (film) made of polyolefin such as polyethylene (PE) or polypropylene (PP). The thickness of the separator may be, for example, 0.1 μm or more and 1 mm or less. The electrolyte usually contains a non-aqueous solvent and a supporting salt. Examples of the non-aqueous solvent include carbonates, ethers, esters, nitriles, sulfones, lactones, etc. Examples of the supporting salt include LiPF6, LiBF4, lithium bis(fluorosulfonyl)imide (LiFSI), lithium bis(trifluoromethane)sulfonimide (LiTFSI), etc. The concentration of the supporting salt in the electrolyte is not particularly limited, but may be, for example, 0.5 mol / L or more and 5 mol / L or less. In addition, any component such as a gas generating agent, a film forming agent, a dispersing agent, or a thickener may be added to the electrolyte.
[0034] (Collection terminal 30) The current collector terminal 30 is electrically connected to the power generating element 10 and is disposed so as to extend outward from the exterior body 20. The current collector terminal 30 has a positive electrode current collector terminal and a negative electrode current collector terminal, the positive electrode current collector terminal being connected to the positive electrode current collector foil, and the negative electrode current collector terminal being connected to the negative electrode current collector foil. The arrangement of the positive electrode current collector terminal and the negative electrode current collector terminal is not particularly limited, and may be disposed on opposing surfaces of the power generating element 10 as shown in FIG. 2, or may be disposed on the same surface. The material of the current collector terminal 30 is not particularly limited, and may be appropriately selected from metals used for each current collector foil. For example, the current collector terminal 30 may be made of the same metal as each current collector foil. The metal constituting the positive electrode current collector terminal is preferably Al. The metal constituting the negative electrode current collector terminal is preferably Cu.
[0035] The current collecting terminal 30 has a terminal flat portion 31 having a constant thickness and a terminal inclined portion 32 connected to the terminal flat portion 31 and tapering toward the outside in the width direction, and the terminal inclined portion 32 is formed at least on one end of the current collecting terminal 30. This makes it difficult for a gap to occur between the current collecting terminal 30 and the exterior body 20 in the manufactured battery 100. From the viewpoint of further enhancing the effect, the current collecting terminal 30 may have the terminal inclined portion 32 at both ends in the width direction. FIG. 6 shows a form in which the current collecting terminal 30 has the terminal inclined portion 32 at both ends in the width direction. In addition, as another embodiment of the current collecting terminal 30 having the terminal inclined portion 32 at both ends in the width direction, the form shown in FIG. 7(a) and (b) can be mentioned. In this way, the current collecting terminal 30 may have a hexagonal cross section as shown in FIG. 6, may have a trapezoidal cross section as shown in FIG. 7(a), or may have an octagonal cross section as shown in FIG. 7(b). 6 and 7(b), the current collecting terminal 30 may have a terminal inclined portion 32 on both surfaces in the thickness direction of the end portion thereof, which can further suppress the occurrence of voids.
[0036] The length in the longitudinal direction of the current collecting terminal 30 is not particularly limited and may be set as appropriate. The length in the width direction of the current collecting terminal 30 is not particularly limited and may be set as appropriate. The length in the width direction of the terminal flat portion 31 may be 20% or more and 90% or less of the length in the width direction of the current collecting terminal 30. The length in the width direction of the terminal inclined portion 32 may be 10% or more and 80% or less of the length in the width direction of the current collecting terminal 30. When the width direction lengths of the terminal flat portion 31 and the terminal inclined portion 32 are within the above-mentioned ranges, the occurrence of voids can be further suppressed.
[0037] The thickness of the current collecting terminal 30 (thickness of the terminal flat portion 31) is not particularly limited, but may be relatively thick. For example, it may be 1 mm or more and 5 mm or less. If the current collecting terminal 30 is thick, a gap is likely to occur between the current collecting terminal 30 and the exterior body 20, but since the current collecting terminal 30 has the above-mentioned terminal inclined portion 32, the occurrence of the gap can be suppressed. In addition, in combination with the effect of the resin layer 40 described later, the occurrence of the gap can be further suppressed.
[0038] (Resin layer 40) The resin layer 40 is disposed along at least one surface in the thickness direction of the current collecting terminal 30. As shown in Figs. 5 and 6, the resin layer 30 may be disposed along both surfaces in the thickness direction of the current collecting terminal 30. The resin layer 40 is a member that is heat-welded to the exterior body 20, and is therefore made of a thermoplastic resin. Examples of the resin layer 40 include crystalline resins such as polyolefins such as polyethylene (PE) and polypropylene (PP), and polyesters such as polyethylene terephthalate (PET), and non-crystalline resins such as polystyrene and polyvinyl chloride. The length of the resin layer 40 in the width direction may be longer than the length of the current collecting terminal 30 in the width direction. The length of the resin layer 40 in the length direction may be longer than the length of the region to be heat-welded.
[0039] The resin layer 40 has a resin layer flat portion 41 disposed along the surface of the terminal flat portion 31, and a resin layer inclined portion 42 connected to the resin layer flat portion 41 and disposed along the surface of the terminal inclined portion 32. The resin layer 40 may also have a resin layer end portion 43 connected to the resin layer inclined portion 42.
[0040] The thickness of the resin layer 40 is not particularly limited, but a resin layer that is relatively thicker than conventional resin layers (approximately 100 μm) is used. For example, the thickness of the resin layer 40 may be 250 μm or more, or 400 μm or less. The reason for making the resin layer 40 relatively thick is to ensure that θ1 and θ2, which will be described later, satisfy θ1>θ2. In other words, the inclination of the resin layer inclined portion 42 is gentler than the inclination of the terminal inclined portion 32. As a result, the thickness of the resin layer inclined portion 42 increases toward the outside in the width direction.
[0041] (Placement process S1) As shown in FIG. 6(b), the arrangement step S1 is characterized in that, when the angle formed by the straight line extending from the terminal flat portion 31 and the terminal inclined portion 32 is θ1, and the angle formed by the straight line extending from the resin layer flat portion 41 and the resin layer inclined portion 42 is θ2, the resin layer 40 is arranged on the current collecting terminal 30 so that θ1 and θ2 satisfy θ1>θ2. θ2 is the angle of the outer surface of the resin layer 40. If θ1 and θ2 are θ1≦θ2, a gap may occur between the current collecting terminal 30 and the exterior body 20 due to manufacturing tolerances in the sealing step S3 described later. The manufacturing tolerances are the tolerances of the positional deviation of the heat bar in the sealing step S3, the size of the heat bar, the size of the current collecting terminal, etc. In contrast, if θ1 and θ2 satisfy θ1>θ2 after the arrangement step S1, the occurrence of a gap can be suppressed even if a manufacturing tolerance occurs in the sealing step S3. This effect will be described in detail in the sealing step S3 described later.
[0042] θ1 and θ2 are not particularly limited as long as θ1>θ2 is satisfied. For example, θ1 may be 30° or more and 60° or less. θ2 may be 10° or more and 40° or less. In addition, the difference between θ1 and θ2 may be 10° or more and 30° or less.
[0043] The method for disposing the resin layer 40 on the current collecting terminal 30 so that θ1 and θ2 satisfy θ1>θ2 is not particularly limited, but examples thereof include the following: First, the current collecting terminal 30 and the resin layer 40 are molded so that θ1 and θ2 satisfy θ1>θ2, and the resin layer 40 is disposed along the surface of the current collecting terminal 30 as shown in FIG.
[0044] In addition, a method of thermally welding the resin layer 40 to the current collecting terminal 30 using a heat bar 50 is also available. FIGS. 8(a) to 8(c) are a time series diagram showing how the resin layer 40 is thermally welded to the current collecting terminal 30 using the heat bar 50. As shown in FIG. 8(a), the resin layer 40 is disposed on the outside of the current collecting terminal 30, and the heat bar 50 is further disposed on the outside of the resin layer 40. Next, as shown in FIG. 8(b), the current collecting terminal 40 and the resin layer 40 are sandwiched between two heat bars 50 and heated. This allows the resin layer 40 to be disposed in close contact with the current collecting terminal 30. In addition, the resin layer ends 43 are thermally welded to each other, and the resin layer 40 can be fixed to the current collecting terminal 30. Then, as shown in FIG. 8(c), the heat bar 50 is separated from the resin layer 40. The current collecting terminal 30 sandwiched between the resin layers 40 in this way is further sandwiched between the heat bars 50, allowing the resin layer 40 to be disposed on the current collecting terminal 30.
[0045] Here, the shape of the heat bar 50 is set so that θ2 of the resin layer 40 is a predetermined angle. The heat bar 50 has a heat bar flat portion 51 with a constant thickness and a heat bar inclined portion 52 connected to the heat bar flat portion 51. The heat bar flat portion 51 is a portion corresponding to the resin layer flat portion 41, and the heat bar inclined portion 52 is a portion corresponding to the resin layer inclined portion 42. The shape of the heat bar 50 is set so that θx=θ2 when the angle formed by a straight line extending from the heat bar flat portion 51 and the heat bar inclined portion 52 is θx. θx is the angle of the inner surface of the heat bar 50. By using such a heat bar 50, the resin layer 40 can be disposed on the current collecting terminal 30 while θ2 of the resin layer 40 is formed to a predetermined angle. The heat bar 50 may also have a heat bar end 53 connected to the heat bar inclined portion 52. The heat bar end 53 is a portion corresponding to the resin layer end 43.
[0046] 8, an already molded resin layer 40 is used, but the resin layer 40 that can be used in the arrangement step S1 is not limited to this, and a flat resin layer may be used. This is because even if a flat sheet-like resin layer is used, it can be molded into a desired shape by the heat bar 50.
[0047] The temperature of the heat bar 50 is not particularly limited, and is set appropriately according to the melting temperature of the resin layer 40. For example, it may be 150°C or higher, or 200°C or lower. The pressure of the heat bar 50 when sandwiching the current collecting terminal 30 and the resin layer 40 is not particularly limited, and it is sufficient that the current collecting terminal 30 and the resin layer 40 can be appropriately thermally welded. It is also sufficient that the resin layer 40 can be formed into a desired shape. For example, it may be 0.1 MPa or higher, or 1 MPa or lower. The heat bar 50 may be a known heat bar made of, for example, silicone rubber.
[0048] <Accommodation process S2> The accommodation step S2 is a step of accommodating the power generating element 10 on which the resin layer 40 is disposed, in the exterior body 20. At this time, the power generating element 10 is accommodated in the exterior body 20 so that the current collector 30 extends outward from the exterior body 20. In addition, the exterior body 20 is disposed so that the resin layer 40 is disposed between the current collecting terminal 30 and the exterior body 20. This is for the purpose of thermally welding the resin layer 40 and the exterior body 20 in the sealing step S3 described later.
[0049] (Exterior body 20) An exterior body having a thermally welded layer is used as the exterior body 20. For example, a metal laminate film is used. In general, a metal laminate film includes a metal layer and a resin layer that covers the metal layer.
[0050] The metal layer of the metal laminate film functions as a gas barrier layer. The gas barrier layer is a layer that blocks the entry and exit of moisture, air, or gas generated inside the battery 100 between the inside and outside of the battery 100. The metal layer may be made of a metal material such as aluminum, iron, or stainless steel.
[0051] Resin layers are provided on both sides of the metal layer, but the functions of the resin layers differ depending on the side of the metal layer. For example, a heat-sealed layer is used for the resin layer provided on the side where heat welding is performed (usually the inner side). The heat-sealed layer includes a thermoplastic resin. Examples of thermoplastic resins include crystalline resins such as polyolefins such as polyethylene (PE) and polypropylene (PP); polyesters such as polyethylene terephthalate (PET); and non-crystalline resins such as polystyrene and polyvinyl chloride. On the other hand, a protective layer is used for the resin layer provided on the side where heat welding is not performed (usually the outer side). A resin that functions as a protective layer is appropriately used for the protective layer. Examples include polyesters such as PET, and polyamide (nylon).
[0052] When a metal laminate film is used for the exterior body 20, the power generating element 10 is sandwiched between two metal laminate films as shown in Figs. 2 and 3. Alternatively, one metal laminate film is folded to sandwich the power generating element 10. At this time, the metal laminate films are arranged so that the thermally welded layers overlap each other. In addition, a convex portion may be provided on the metal laminate film to accommodate the power generating element 10. The convex portion may be provided on the two metal laminate films, or on one of the metal laminate films. In this manner, the power generating element 10 can be accommodated in the exterior body 20.
[0053] 9(a), the end of the exterior body 20 on the collector terminal 30 side may be shaped as shown in FIG. 9(a). In this case, the end of the exterior body 20 on the collector terminal 30 side may have an exterior body flat portion 21 and an exterior body inclined portion 22 connected to the exterior body flat portion 21. The exterior body flat portion 21 is a portion corresponding to the resin layer flat portion 41, and the exterior body inclined portion 22 is a portion corresponding to the resin layer inclined portion 42. In addition, the end of the exterior body 20 on the collector terminal 30 side may have an exterior body end portion 23 connected to the exterior body inclined portion 22. The exterior body end portion 23 is a portion corresponding to the resin layer end portion 43.
[0054] (Sealing process S3) The sealing step S3 is a step of sealing the power generating element 10 in the exterior body 20 by thermal welding. Specifically, it is a step of thermally welding the ends of the exterior body 20 to seal the power generating element 10 inside the exterior body 20. At this time, since the resin layer 40 is disposed between the current collecting terminal 30 and the exterior body 20, the resin layer 40 and the exterior body 20 are thermally welded together in the sealing step S3.
[0055] The heat welding of the outer casing 20 can be carried out by known methods, but the heat welding between the resin layer 40 and the outer casing 20, i.e., the heat welding of the end of the outer casing 20 on the collector terminal 30 side, is carried out using an angled heat bar 60.
[0056] 9(a) to 9(c) show the time series of the process of thermally welding the resin layer 40 and the exterior body 20 using the heat bar 60. As shown in FIG. 9(a), the exterior body 20 is disposed on the outside of the current collecting terminal 30 on which the resin layer 40 is disposed, and the heat bar 60 is further disposed on the outside of the exterior body 20. Next, as shown in FIG. 9(b), the end of the exterior body 20 on the current collecting terminal 30 side is sandwiched between the two heat bars 60 and heated. As a result, the resin layer 40 disposed on the current collecting terminal 30 and the exterior body 20 are thermally welded. In addition, the exterior bodies 20 disposed in the portions on the widthwise outer side of the resin layer end 40 are thermally welded to each other. Then, as shown in FIG. 9(c), the heat bar 60 is separated from the exterior body 20. In this way, the end of the exterior body 20 on which the current collecting terminal 30 is disposed is sandwiched between the heat bars 60, whereby the resin layer 40 and the exterior body 20 are thermally welded to each other.
[0057] Here, similar to the heat bar 50, the heat bar 60 has a heat bar flat portion 61 with a constant thickness and a heat bar inclined portion 62 connected to the heat bar flat portion 61. The heat bar flat portion 61 is a portion corresponding to the exterior body flat portion 21, and the heat bar inclined portion 62 is a portion corresponding to the exterior body inclined portion 22. When the angle formed by the straight line extending from the heat bar flat portion 61 and the heat bar inclined portion 62 is θy, the shape of the heat bar 60 is set so that θ1 ≧ θy > θ2. θy is the angle of the inner surface of the heat bar 60. By setting the angle to satisfy this relationship, it becomes difficult for a gap to occur between the current collecting terminal 30 (resin layer 40) and the exterior body 20.
[0058] FIG. 10 shows a schematic diagram of a sealing process using a battery intermediate body with θ1≦θ2. FIG. 10(a) is a diagram corresponding to FIG. 9(a). As shown in FIG. 10(a), the position of the upper heat bar is shifted from the specified position, and a manufacturing tolerance d occurs. When heat welding is performed in this state, as shown by dotted line A in FIG. 10(b), the resin layer melts due to the heat of the heat bar at the upper part of the inclined resin layer and flows outward in the width direction, so that the resin layer is heat-welded to the exterior body, but as shown by dotted line B, a gap C occurs between the resin layer and the exterior body at the lower part of the inclined resin layer. In this way, if θ1≦θ2, a gap may occur due to manufacturing tolerance.
[0059] On the other hand, when θ1>θ2, the resin layer inclined portion 42 has a structure in which the thickness increases toward the outside in the width direction. Therefore, even if the manufacturing tolerance as described above occurs, the generation of voids is suppressed in the outer part of the resin layer inclined portion 42 in the width direction.
[0060] The heat bar 60 may also include a heat bar end 63 connected to the heat bar inclined portion 62. This allows the resin layer end 43 and the exterior body end 23 to be thermally welded together, and allows the exterior body ends 23 located outside the resin layer end 43 to be thermally welded together.
[0061] 9, an exterior body 20 with an end portion on the side of the current collecting terminal 30 already shaped is used, but the shape of the end portion of the exterior body 20 that can be used in the sealing step S3 is not limited to this, and an exterior body having a flat end portion may be used. This is because even if such an exterior body is used, it can be shaped into a desired shape by the heat bar 60.
[0062] The temperature of the heat bar 60 is not particularly limited, and is set appropriately according to the heat welding temperature between the exterior body 20 and the resin layer 40. For example, it may be 150°C or higher, or 200°C or lower. The pressure of the heat bar 50 when sandwiching the current collecting terminal 30, the resin layer 40, and the exterior body 20 is not particularly limited, and it is sufficient that the exterior body 20 and the resin layer 40 are appropriately heat welded. It is also sufficient that the exterior body 20 can be molded into a desired shape. For example, it may be 0.1 MPa or higher, or 1 MPa or lower. The heat bar 60 can be a known heat bar made of, for example, silicone rubber.
[0063] (100 batteries) The sealing step S3 allows the manufacture of the battery 100. As described above, the generation of voids is suppressed in the battery 100. Such a battery 100 has the following structural features.
[0064] FIG. 11 shows an exploded cross-sectional view of the part where the resin layer 40 and the exterior body 20 are heat-welded in the battery 100 manufactured by the sealing step S3. Also, the metal layer 2a inside is shown only in the exterior material 20 arranged on the upper side. As shown in FIG. 11, the angle between the terminal flat portion 31 and the straight line extending from the terminal inclined portion 32 is θ3, and the angle between the resin layer flat portion 41 and the straight line extending from the resin layer inclined portion 42 is θ4. At this time, the relationship between θ3 and θ4 may change depending on the conditions of the sealing step S3. This is because, when the resin layer 40 and the resin layer arranged on the inner surface of the exterior body 20 are heat-welded in the sealing step S3, the boundary between the resin layer 40 and the resin layer of the exterior body 20 is often not clear in the manufactured battery 100. Therefore, the angle of the inner surface of the metal layer 20a of the exterior body 20 may be regarded as θ4. Specifically, as shown in FIG. 11, θ4 may be regarded as the angle of the inner surface of metal layer 20a of exterior body 20, which is the angle formed by the inner surface of metal layer 20a of exterior body flat portion 21 and a straight line extending from the inner surface of metal layer 20a of exterior body inclined portion 22.
[0065] In the sealing step S3, when θy of the heat bar 60 satisfies θ1>θy>θ2, θ3 and θ4 of the battery 100 satisfy θ3>θ4. This is the same as the relationship between θ1 and θ2. However, θ1 and θ3 have almost the same value, but θ2 and θ4 may have completely different values. This is because the resin layer 40 melts due to thermal welding using the heat bar 60, and the angle between the resin layer flat portion 41 and the straight line extending the resin layer inclined portion 42 may change. Therefore, θ1 and θ3 are θ1≒θ3, and θ2 and θ4 are θ4≧θ2. When the angle between the resin layer flat portion 41 and the straight line extending the resin layer inclined portion 42 changes, θ2 and θ4 are θ4>θ2. When θ4>θ2, the battery 100 has the following structural characteristics.
[0066] Fig. 12 shows a perspective view of the battery 100 in the vicinity of one current collecting terminal 30. As shown in Fig. 12, the resin layer 40 has, in the longitudinal direction, a first region 40a that is welded to the exterior body 20 and a second region 40b that is not welded to the exterior body 20. In other words, the first region 40a is a portion where the resin layer 40 and the exterior body 20 are thermally welded by the heat bar 60. In other words, the second region 40b is a portion that is not affected by the heat bar 60 and where the resin layer 40 and the exterior body 20 are not thermally welded.
[0067] Next, Figure 13(a) shows an exploded cross-sectional view taken along line aa in Figure 12 (an exploded cross-sectional view of the first region 40a), and Figure 13(b) shows an exploded cross-sectional view taken along line bb in Figure 12 (an exploded cross-sectional view of the second region 40b).
[0068] As shown in FIG. 13(a), the first region 40a of the resin layer 40 includes a first region flat portion 41a arranged along the surface of the terminal flat portion 31, and a first region inclined portion 42a connected to the first region flat portion 41a and arranged along the surface of the terminal inclined portion 32. The first region 40a may also include a first region end portion 43a connected to the first region inclined portion 42a. As shown in FIG. 13(b), the second region 40b of the resin layer 40 includes a second region flat portion 41b arranged along the surface of the terminal flat portion 31, and a second region inclined portion 42b connected to the second region flat portion 41b and arranged along the surface of the terminal inclined portion 32. The second region 40b may also include a second region end portion 43b connected to the second region inclined portion 42b. The first region flat portion 41a and the second region flat portion 41b correspond to the resin layer flat portion 41, the first region inclined portion 42a and the second region inclined portion 42b correspond to the resin layer inclined portion 42, and the first region end portion 43a and the second region end portion 43b correspond to the resin layer end portion 43.
[0069] Then, when the angle between the first region flat portion 41a and the straight line extending from the first region inclined portion 42a is θ5, and the angle between the second region flat portion 41b and the straight line extending from the second region inclined portion 42b is θ6, θ5 and θ6 satisfy θ5>θ6. At this time, θ5 corresponds to θ4, and θ6 corresponds to θ2. However, as described above, in the manufactured battery 100, the boundary between the resin layer 40 and the resin layer of the exterior body 20 is often unclear due to thermal welding. Therefore, the angle of the inner surface of the metal layer 20a of the exterior body 20 may be regarded as θ5. Specifically, as shown in FIG. 13(a), θ5 may be regarded as the angle of the inner surface of metal layer 20a (shown only in the upper exterior body 20) of exterior body 20, which is formed by a straight line extending from the inner surface of metal layer 20a of exterior body flat portion 21 corresponding to first region flat portion 41a to the inner surface of metal layer 20a of exterior body inclined portion 22 corresponding to first region inclined portion 42a.
[0070] On the other hand, in the sealing step S3, when θy of the heat bar 60 satisfies θ1=θy>θ2, θ3 and θ4 of the battery 100 may be θ3=θ4. Even in such a case, θ5 and θ6 satisfy θ5>θ6.
[0071] In this manner, the battery 100 manufactured by the sealing step S3 has a predetermined structural feature at the angle of the resin layer 40.
[0072] Here, θ3 may be, for example, 30° or more and 60° or less. θ4 and θ5 may be 10° or more, 20° or more, 40° or less, or 30° or less. θ6 may be 10° or more and 40° or less. The difference between θ3 and θ4 may be 10° or more, 15° or more, 30° or less, or 25° or less. The difference between θ5 and θ6 may be 10° or more, 15° or more, 30° or less, or 25° or less.
[0073] To summarize the above, when θy of the heat bar 60 satisfies θ1>θy>θ2, the power generating element 10 can be sealed in the exterior body 20 in the sealing step S3 such that θ3 and θ4 satisfy θ3>θ4. On the other hand, when θy of the heat bar 60 satisfies θ1=θy>θ2, the power generating element 10 can be sealed in the exterior body 20 in the sealing step S3 such that θ5 and θ6 satisfy θ5>θ6. However, other conditions of the heat bar 60 need to be set appropriately.
[0074] The method for manufacturing a battery according to the present disclosure has been described above using one embodiment. According to the method for manufacturing a battery according to the present disclosure, it is possible to reduce the occurrence of voids between the current collecting terminal and the exterior body.
[0075] [Battery intermediates] The present disclosure provides a battery intermediate comprising: a power generating element; a current collecting terminal electrically connected to the power generating element; and a resin layer arranged along at least one surface in the thickness direction of the current collecting terminal, wherein the current collecting terminal comprises a terminal flat portion of a constant thickness and a terminal inclined portion connected to the terminal flat portion and having a thickness that decreases outward in the width direction, the terminal inclined portion being formed on at least one end of the current collecting terminal, and the resin layer has a resin layer flat portion arranged along the surface of the terminal flat portion, and a resin layer inclined portion connected to the resin layer flat portion and arranged along the surface of the terminal inclined portion, wherein θ1 is the angle formed by a straight line extending from the terminal flat portion and the terminal inclined portion, and θ2 is the angle formed by the resin layer flat portion and the straight line extending from the resin layer inclined portion, and θ1 and θ2 satisfy θ1>θ2.
[0076] The battery intermediate of the present disclosure can be manufactured by the arrangement step in the battery manufacturing method of the present disclosure. According to the battery intermediate of the present disclosure, when the battery intermediate is sealed in the outer casing, the generation of a gap between the current collecting terminal and the outer casing can be suppressed, and thermal welding defects can be suppressed. A detailed description of the battery intermediate of the present disclosure has been given above, and will not be repeated here.
[0077] [battery] The present disclosure provides a battery comprising: a power generating element; an exterior body that houses the power generating element; a current collecting terminal electrically connected to the power generating element and arranged to extend outward from the exterior body; and a resin layer arranged along at least one surface in a thickness direction of the current collecting terminal and arranged between the current collecting terminal and the exterior body, wherein the resin layer and the exterior body are heat-welded, the current collecting terminal comprises a terminal flat portion having a constant thickness, and a terminal inclined portion connected to the terminal flat portion and having a thickness that decreases toward the outside in the width direction, the terminal inclined portion is formed on at least one end of the current collecting terminal, and the resin layer comprises a resin layer flat portion arranged along the surface of the terminal flat portion, and a resin layer inclined portion connected to the resin layer flat portion and arranged along the surface of the terminal inclined portion, wherein θ3 is an angle formed by the terminal flat portion and the terminal inclined portion, and θ4 is an angle formed by the resin layer flat portion and the resin layer inclined portion, such that θ3>θ4.
[0078] The present disclosure also relates to a power generating element, an exterior body that houses the power generating element, a current collecting terminal that is electrically connected to the power generating element and disposed so as to extend outward from the exterior body, and a resin layer that is disposed along at least one surface in a thickness direction of the current collecting terminal and disposed between the current collecting terminal and the exterior body, the resin layer being heat welded to the exterior body, the current collecting terminal having a terminal flat portion with a constant thickness and a terminal inclined portion that is connected to the terminal flat portion and has a thickness that decreases toward the outside in the width direction, the terminal inclined portion being formed on at least one end of the current collecting terminal, and the resin layer has a first region that is welded to the exterior body in the length direction and a second region that is welded to the exterior body. the first region of the resin layer comprises a first region flat portion arranged along the surface of the terminal flat portion, and a first region inclined portion connected to the first region flat portion and arranged along the surface of the terminal inclined portion; the second region of the resin layer comprises a second region flat portion arranged along the surface of the terminal flat portion, and a second region inclined portion connected to the second region flat portion and arranged along the surface of the terminal inclined portion, wherein when θ5 is an angle formed by the first region flat portion and a straight line extending through the first region inclined portion, and θ6 is an angle formed by the second region flat portion and a straight line extending through the second region inclined portion, θ5 and θ6 satisfy θ5>θ6.
[0079] The battery of the present disclosure can be manufactured by the manufacturing method of the battery of the present disclosure. According to the battery of the present disclosure, the generation of a gap between the current collector terminal and the exterior body is suppressed, and the thermal welding failure is suppressed. Since the detailed description of the battery of the present disclosure has been given above, it will be omitted here. [Explanation of symbols]
[0080] 10 Power generation elements 20 Exterior body 20a metal layer 30 Current collector terminal 31 Terminal flat part 32 Terminal slope 40 Resin layer 40a 1st area 40b 2nd area 41 Flat part of resin layer 41a 1st area flat part 41b 2nd area flat part 42 Resin layer slope part 42a 1st area slope part 42b 2nd area slope part 43 End of resin layer 43a First area end 43b Second area end 50, 60 Heat Bar 51, 61 Heat bar flat part 52, 62 Heat bar inclination 53, 63 Heat bar end 90 Battery intermediates 100 batteries
Claims
1. A method for manufacturing a battery including a power generating element, an exterior body that houses the power generating element, and a current collecting terminal that is electrically connected to the power generating element and extends outward from the exterior body, comprising: a step of disposing a resin layer along at least one surface in a thickness direction of the current collector terminal connected to the power generating element; a housing step of housing the power generating element in the exterior body; and a sealing step of sealing the power generating element to the exterior body by thermal welding. In the sealing step, the resin layer and the exterior body are thermally welded together, The current collecting terminal has a terminal flat portion having a constant thickness and a terminal inclined portion connected to the terminal flat portion and having a thickness that decreases toward an outer side in a width direction, The terminal inclined portion is formed on at least one end of the current collecting terminal, the resin layer has a resin layer flat portion disposed along a surface of the terminal flat portion, and a resin layer inclined portion connected to the resin layer flat portion and disposed along a surface of the terminal inclined portion, The resin layer has, in a longitudinal direction, a first region that is welded to the exterior body and a second region that is not welded to the exterior body, the first region of the resin layer includes a first region flat portion disposed along a surface of the terminal flat portion, and a first region inclined portion connected to the first region flat portion and disposed along a surface of the terminal inclined portion, the second region of the resin layer includes a second region flat portion disposed along a surface of the terminal flat portion, and a second region inclined portion connected to the second region flat portion and disposed along a surface of the terminal inclined portion, In the arrangement step, when an angle between the terminal flat portion and a straight line extending from the terminal inclined portion is defined as θ1, and an angle between the resin layer flat portion and a straight line extending from the resin layer inclined portion is defined as θ2, The resin layer is disposed on the current collecting terminal so that θ1 and θ2 satisfy θ1>θ2; In the sealing step, when an angle between the first region flat portion and a straight line extending from the first region inclined portion is defined as θ5, and an angle between the second region flat portion and a straight line extending from the second region inclined portion is defined as θ6, The power generating element is sealed in the exterior body so that θ5 and θ6 satisfy θ5>θ6. How batteries are manufactured.
2. In the sealing process, when an angle between the terminal flat portion and a straight line extending from the terminal inclined portion is defined as θ3, and an angle between the resin layer flat portion and a straight line extending from the resin layer inclined portion is defined as θ4, The power generating element is sealed in the exterior body so that θ3 and θ4 satisfy θ3>θ4. A method for producing the battery according to claim 1 .
3. A power generation element; an exterior body that houses the power generating element; a current collecting terminal electrically connected to the power generating element and disposed so as to extend outward from the exterior housing; a resin layer disposed along at least one surface of the current collecting terminal in a thickness direction and between the current collecting terminal and the exterior body, the resin layer is heat-welded to the exterior body, The current collecting terminal includes a terminal flat portion having a constant thickness, and a terminal inclined portion connected to the terminal flat portion and having a thickness that decreases toward an outer side in a width direction, The terminal inclined portion is formed on at least one end of the current collecting terminal, The resin layer has, in a longitudinal direction, a first region that is welded to the exterior body and a second region that is not welded to the exterior body, the first region of the resin layer includes a first region flat portion disposed along a surface of the terminal flat portion, and a first region inclined portion connected to the first region flat portion and disposed along a surface of the terminal inclined portion, the second region of the resin layer includes a second region flat portion disposed along a surface of the terminal flat portion, and a second region inclined portion connected to the second region flat portion and disposed along a surface of the terminal inclined portion, When an angle between the flat portion of the first region and a straight line extending from the inclined portion of the first region is defined as θ5, and an angle between the flat portion of the second region and a straight line extending from the inclined portion of the second region is defined as θ6, θ5 and θ6 satisfy θ5>θ6. battery.
Citation Information
Patent Citations
Film-armored electric device
JP2006164784A
Lead tab for laminate type battery, laminate type battery equipped with the same, and manufacturing method of the same
JP2013020758A
Power storage element, manufacturing method for power storage element
JP2020053238A
Lead tabs for battery terminals
JP2020532082A
Manufacturing method of secondary battery
JP2021150231A