Pulse wave sensor

The pulse wave sensor design with a cross-shaped beam and gapless connecting portion effectively prevents foreign matter entry, enhancing detection accuracy and sensitivity by using a Cr multiphase film resistor to detect resistance changes.

JP7571976B2Active Publication Date: 2024-10-23MINEBEAMITSUMI INC
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
JP2021146128
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-09-08
Publication Date
2024-10-23
Estimated Expiration
2041-09-08

AI Technical Summary

Technical Problem

Pulse wave sensors are prone to electrical short circuits and flexibility obstructions due to foreign matter entering through openings in the pressure receiving plate, which is in direct contact with the subject's skin.

Method used

A pulse wave sensor design featuring a strain-generating body with a beam portion intersecting in a cross shape, a connecting portion without gaps, and a load portion protruding from the intersection, utilizing a Cr multiphase film resistor to detect pulse waves based on resistance changes.

Benefits of technology

Prevents foreign matter entry, improving pulse wave detection accuracy and sensitivity by enhancing the S/N ratio and reducing the risk of electrical short circuits.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007571976000001
    Figure 0007571976000001
  • Figure 0007571976000002
    Figure 0007571976000002
  • Figure 0007571976000003
    Figure 0007571976000003
Patent Text Reader

Abstract

To provide a pulse wave sensor preventing foreign objects from entering.SOLUTION: A pulse wave sensor comprises a strain generating body, and a strain gage provided on the strain generating body and using a Cr-mixed phase film as a resistor. The strain generating body includes a frame part, a beam part for bridging the inside of the frame part, and a connecting part for connecting, in plan view, the inside of the frame part and the outside of the beam part without any gap, where the connecting part is thinner than the frame part and the beam part. The pulse wave sensor detects the pulse wave based on change in a resistance value of the resistor due to deformation of the beam part.SELECTED DRAWING: Figure 2
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a pulse wave sensor. [Background technology]

[0002] Pulse wave sensors are known that detect pulse waves generated when the heart pumps blood. One example is a pulse wave sensor that includes a pressure-receiving plate that is a strain-generating body supported so that it can flex under the action of an external force, and a piezoelectric conversion means that converts the flexure of the pressure-receiving plate into an electrical signal. In this pulse wave sensor, the flexible area of ​​the pressure-receiving plate is formed in a dome shape that is a convex curved surface facing outward, and a pressure detection element is provided on the inner surface of the top of the pressure-receiving plate as the piezoelectric conversion means (see, for example, Patent Document 1). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2002-78689 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, in the above-mentioned pulse wave sensor, the roughly fan-shaped through-openings are arranged radially from the center position of the pressure-receiving plate. Because the pulse wave sensor is in direct contact with the subject's skin, foreign matter such as dust or moisture may enter the pulse wave sensor through the through-openings, causing problems such as an electrical short circuit or impeded flexibility due to foreign matter being trapped inside the sensor.

[0005] The present invention has been made in consideration of the above-mentioned points, and has an object to provide a pulse wave sensor which is prevented from entering with foreign matter. [Means for solving the problem]

[0006] This pulse wave sensor has a strain gauge provided on the strain body, the strain gauge having a Cr mixed phase film as a resistor, the strain body having a frame portion, a beam portion bridging the inside of the frame portion, and a connection portion connecting the inside of the frame portion and the outside of the beam portion without any gaps in a plan view, the connection portion being thinner than the frame portion and the beam portion, The beam portion has a first beam and a second beam that intersect in a cross shape in a plan view, and a load portion that protrudes from the beam portion is provided in a region where the first beam and the second beam intersect, A pulse wave is detected based on a change in the resistance value of the resistor caused by the deformation of the beam portion. Effect of the Invention

[0007] According to the disclosed technique, it is possible to provide a pulse wave sensor that is resistant to the intrusion of foreign matter. [Brief description of the drawings]

[0008] [Figure 1] 1 is a plan view illustrating a pulse wave sensor according to a first embodiment. [Diagram 2] 2 is a bottom view illustrating the pulse wave sensor according to the first embodiment. FIG. [Diagram 3] 1 is a cross-sectional view (part 1) illustrating a pulse wave sensor according to a first embodiment. [Figure 4] 4 is a cross-sectional view (part 2) illustrating the pulse wave sensor according to the first embodiment. FIG. [Diagram 5] FIG. 2 is a cross-sectional view illustrating a housing to which a strain generating body is attached. [Figure 6] FIG. 2 is a plan view illustrating the strain gauge according to the first embodiment. [Figure 7] 1 is a cross-sectional view illustrating a strain gauge according to a first embodiment. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0009] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. In the drawings, the same components are denoted by the same reference numerals, and duplicated explanations may be omitted.

[0010] First Embodiment FIG. 1 is a plan view illustrating the pulse wave sensor according to the first embodiment. FIG. 2 is a bottom view illustrating the pulse wave sensor according to the first embodiment. FIG. 3 is a cross-sectional view (part 1) illustrating the pulse wave sensor according to the first embodiment, showing a cross-section along line AA in FIG. 1. FIG. 4 is a cross-sectional view (part 2) illustrating the pulse wave sensor according to the first embodiment, showing a cross-section along line BB in FIG. 1. Note that here, a view seen from the direction in which load portion 14 protrudes is shown as a plan view, and a view seen from the direction in which strain gauge 100 is provided is shown as a bottom view.

[0011] 1 to 4, pulse wave sensor 1 has a strain generating body 10 and a strain gauge 100. Pulse wave sensor 1 may also have a shielded cable, a flexible board, etc. for inputting and outputting electrical signals to and from the outside. X, Y, and Z indicate an orthogonal coordinate system.

[0012] The flexure body 10 has a frame portion 11, beam portions 12, connection portions 13, and a load portion 14. However, the load portion 14 is provided as necessary. The flexure body 10 is, for example, in the shape of a flat plate, and each component is, for example, formed integrally. The flexure body 10 has, for example, a two-fold symmetric shape in a plan view.

[0013] The flexure body 10 is, for example, rectangular in plan view, but may also be circular or elliptical in plan view. When the flexure body 10 is rectangular in plan view, for example, the flexure body 10 has two sides parallel to the X direction and two sides parallel to the Y direction in plan view. In this case, the outer diameter of the flexure body 10 may be, for example, 20±2 mm (X direction)×15±2 mm (Y direction). The material of the flexure body 10 may be, for example, SUS (stainless steel), copper, aluminum, or the like.

[0014] The frame portion 11 is, for example, a rectangular frame-like region provided on the outermost side of the flexure body 10 in a plan view. The width W1 of the frame portion 11 is, for example, 1 mm or more and 5 mm or less. The width W1 of the frame portion 11 may be constant or may not be constant.

[0015] The beam portion 12 is provided so as to bridge the inside of the frame portion 11. The beam portion 12 has, for example, a first beam 12a and a second beam 12b that intersect in a cross shape in a plan view. The region where the first beam 12a and the second beam 12b intersect is a common portion between them and includes the center of the frame portion 11. In the example of Figs. 1 to 4, the first beam 12a, which is one beam constituting the cross, has a longitudinal direction in the X direction, and the second beam 12b, which is the other beam constituting the cross, has a longitudinal direction in the Y direction, and the two are perpendicular to each other.

[0016] The width W2 of the first beam 12a and the second beam 12b other than the intersecting region is constant, for example, 1 mm or more and 5 mm or less. It is not essential that the width W2 be constant, but making the width W2 constant is preferable in terms of being able to detect strain linearly.

[0017] The connection portions 13 are four portions that connect the inside of the frame portion 11 and the outside of the beam portion 12 without any gaps in a plan view. The planar shape of each of the connection portions 13 is, for example, rectangular. Each of the connection portions 13 is thinner than the frame portion 11 and the beam portion 12. The thicknesses t1 of the frame portion 11 and the beam portion 12 are, for example, the same, and are, for example, not less than 0.1 mm and not more than 0.2 mm. The thickness t2 of the connection portions 13 can be, for example, about 1 / 2 of the thickness t1.

[0018] The load portion 14 can be provided on the beam portion 12. The load portion 14 is provided, for example, in the region where the first beam 12a and the second beam 12b constituting the beam portion 12 intersect. The load portion 14 protrudes from the upper surface of the beam portion 12. The amount of protrusion of the load portion 14 based on the upper surface of the beam portion 12 is, for example, about 0.1 mm. The beam portion 12 is flexible, and elastically deforms when a load is applied to the load portion 14.

[0019] The strain gauge 100 is provided on the strain generating body 10. The strain gauge 100 can be provided, for example, on the lower surface side of the beam portion 12. Since the beam portion 12 is flat, the strain gauge can be easily attached. One or more strain gauges 100 may be provided, but in this embodiment, four strain gauges 100 are provided. By providing four strain gauges 100, strain can be detected by a full bridge.

[0020] Two of the four strain gauges 100 are arranged on the side of the first beam 12a, whose longitudinal direction is the X direction, close to the frame portion 11, so as to face each other across the load portion 14 in a plan view. The other two of the four strain gauges 100 are arranged on the side of the second beam 12b, whose longitudinal direction is the Y direction, close to the load portion 14 (toward the center of the frame portion 11), so as to face each other across the load portion 14 in a plan view. With this arrangement, compressive force and tensile force can be effectively detected, and a large output can be obtained by the full bridge.

[0021] The pulse wave sensor 1 is used by being fixed to the arm of a subject so that the load section 14 abuts against the radial artery of the subject. When a load is applied to the load section 14 in accordance with the pulse wave of the subject and the beam section 12 elastically deforms, the resistance value of the resistor 130 (described later) of the strain gauge 100 changes. The pulse wave sensor 1 can detect the pulse wave based on the change in the resistance value of the resistor 130 of the strain gauge 100 that accompanies the deformation of the beam section 12. The pulse wave is output as a periodic change in voltage from a measurement circuit connected to, for example, an electrode 150 (described later) of the strain gauge 100.

[0022] Although it is possible to detect pulse waves without providing load portion 14, providing load portion 14 protruding from beam portion 12 toward the subject improves the S / N ratio when detecting pulse waves, thereby improving the accuracy of pulse wave detection.

[0023] The length L1 of the first beam 12a and the length L2 of the second beam 12b may be the same, but it is preferable that the first beam 12a is longer than the second beam 12b. For example, when the flexure body 10 is rectangular in a plan view and the outer diameter of the flexure body 10 is 20 mm (X direction) × 15 mm (Y direction), the length L1 of the first beam 12a can be set to 18 mm, and the length L2 of the second beam 12b can be set to 13 mm.

[0024] By fixing the pulse wave sensor 1 to the subject's arm so that the long first beam 12a is aligned along the radial artery, the component along the radial artery can be acquired at a large signal level, improving the S / N ratio and increasing the detection accuracy of the pulse wave. Also, by fixing the pulse wave sensor 1 to the subject's arm so that the long first beam 12a is aligned along the radial artery, it is preferable in that the low-frequency line component of the pulse wave can be acquired efficiently.

[0025] When the first beam 12a is made longer than the second beam 12b, the flexure body 10 can be made elliptical in plan view. It is also possible to make the flexure body 10 circular in plan view and to make the first beam 12a longer than the second beam 12b by partially changing the width of the frame portion 11. However, making the flexure body 10 rectangular in plan view is preferable in terms of ease of manufacture compared to making the flexure body 10 circular or elliptical in plan view.

[0026] The flexure body 10 may be attached to one side of a housing 20, for example, as shown in Fig. 5. The housing 20 is a portion that holds the flexure body 10. The housing 20 is, for example, square-shaped, with a closed bottom side and an open top side. The flexure body 10, for example, rectangular in shape, is fixed with an adhesive or the like so as to close the opening on the top side of the housing 20.

[0027] The housing 20 can be made of, for example, metal or resin. However, in order to prevent deterioration in the accuracy of strain detection due to the influence of thermal expansion, it is preferable that the strain body 10 and the housing 20 are made of materials with the same thermal expansion coefficient. The material that can be used for the strain body 10 and the housing 20 can be, for example, SUS (stainless steel).

[0028] 1 to 4, one side in the thickness direction of frame 11, beams 12, and connection parts 13 (upper side in FIG. 3) are flush, load part 14 is provided on one side, and strain gauges are provided on the other side opposite to the one side (lower side in FIG. 3). In this case, the flush side of frame 11, beams 12, and connection parts 13 is the side that comes into contact with the subject.

[0029] However, the load section 14 may be provided on the other side (upper side in FIG. 3) and the strain gauge may be provided on one side (upper side in FIG. 3). In this case, the side where the frame section 11, the beam section 12, and the connection section 13 are not flush is the side that comes into contact with the subject. A structure in which the side where the frame section 11, the beam section 12, and the connection section 13 are flush is the side that comes into contact with the subject (example in FIG. 3) is preferable in that it is less likely to cause discomfort to the subject.

[0030] In this way, in the pulse wave sensor 1, the strain generating body 10 has the connection portion 13 that connects the inside of the frame portion 11 and the outside of the beam portion 12 without any gaps in a plan view, so there is no opening (gap) through which foreign matter can get into the inside of the pulse wave sensor as in the conventional case. This makes it possible to prevent problems such as an electrical short circuit caused by foreign matter such as dust or moisture getting into the inside of the pulse wave sensor 1 or a reduction in flexibility due to the foreign matter being trapped inside.

[0031] In addition, since the connection portion 13 is formed thinner than the frame portion 11 and the beam portion 12, it does not significantly impede the deformation of the beam portion 12. Therefore, the pulse wave sensor 1 can detect the pulse wave with high sensitivity based on the change in the resistance value of the resistor 130 that accompanies the deformation of the beam portion 12.

[0032] In addition, the pulse wave sensor 1 has a highly sensitive strain gauge 100 having a gauge factor of 10 or more and using a Cr mixed phase film described below as the resistor 130, so that the pulse wave can be detected with particularly high sensitivity based on the change in the resistance value of the resistor 130 that accompanies the deformation of the beam portion 12.

[0033] [Strain gauge 100] Fig. 6 is a plan view illustrating the strain gauge according to the first embodiment. Fig. 7 is a cross-sectional view illustrating the strain gauge according to the first embodiment, showing a cross section along line CC in Fig. 6. Referring to Figs. 6 and 7, the strain gauge 100 has a substrate 110, a resistor 130, wiring 140, electrodes 150, and a cover layer 160. For convenience, only the outer edge of the cover layer 160 is shown by a dashed line in Fig. 6. The cover layer 160 may be provided as necessary.

[0034] In the explanation of the strain gauge 100 in FIG. 6 and FIG. 7, for convenience, the side of the substrate 110 on which the resistor 130 is provided is referred to as the upper side or one side, and the side on which the resistor 130 is not provided is referred to as the lower side or the other side. In addition, the surface on which the resistor 130 is provided in each part is referred to as the one side or the upper surface, and the surface on which the resistor 130 is not provided is referred to as the other side or the lower surface. However, the strain gauge 100 can be used upside down or placed at any angle. For example, in FIG. 5, the strain gauge 100 is attached to the beam 12 in a state in which it is upside down compared to FIG. 7. That is, the substrate 110 in FIG. 7 is attached to the lower surface of the beam 12 with an adhesive or the like. In addition, the planar view refers to the object being viewed from the normal direction of the upper surface 110a of the substrate 110, and the planar shape refers to the shape of the object being viewed from the normal direction of the upper surface 110a of the substrate 110.

[0035] The substrate 110 is a flexible member that serves as a base layer for forming the resistor 130 and the like. The thickness of the substrate 110 is not particularly limited and can be appropriately selected depending on the purpose, and can be, for example, about 5 μm to 500 μm. In particular, a thickness of 5 μm to 200 μm is preferable in terms of the transferability of strain from the surface of the strain generator bonded to the lower surface of the substrate 110 via an adhesive layer or the like and dimensional stability against the environment, and a thickness of 10 μm or more is even more preferable in terms of insulation.

[0036] The substrate 110 can be formed from an insulating resin film such as PI (polyimide) resin, epoxy resin, PEEK (polyether ether ketone) resin, PEN (polyethylene naphthalate) resin, PET (polyethylene terephthalate) resin, PPS (polyphenylene sulfide) resin, LCP (liquid crystal polymer) resin, polyolefin resin, etc. The film refers to a flexible member having a thickness of about 500 μm or less.

[0037] Here, "formed from an insulating resin film" does not prevent the base material 110 from containing fillers, impurities, etc. in the insulating resin film. The base material 110 may be formed from an insulating resin film containing fillers such as silica or alumina.

[0038] Examples of materials other than resin for the base material 110 include crystalline materials such as SiO2, ZrO2 (including YSZ), Si, Si2N3, Al2O3 (including sapphire), ZnO, perovskite ceramics (CaTiO3, BaTiO3), and amorphous glass. Metals such as aluminum, aluminum alloys (duralumin), and titanium may also be used as the material for the base material 110. In this case, for example, an insulating film is formed on the metal base material 110.

[0039] The resistor 130 is a thin film formed in a predetermined pattern on the substrate 110, and is a sensing part that generates a resistance change when strained. The resistor 130 may be formed directly on the upper surface 110a of the substrate 110, or may be formed on the upper surface 110a of the substrate 110 via another layer. For convenience, the resistor 130 is shown in FIG. 6 with a dark matte pattern.

[0040] The resistor 130 has a structure in which multiple elongated parts are arranged at regular intervals with their longitudinal direction in the same direction (the direction of lines CC in FIG. 6), and the ends of adjacent elongated parts are alternately connected to form a zigzag fold as a whole. The longitudinal direction of the multiple elongated parts is the grid direction, and the direction perpendicular to the grid direction is the grid width direction (the direction perpendicular to lines CC in FIG. 6).

[0041] One end in the longitudinal direction of the two elongated portions located at the outermost sides in the grid width direction is bent in the grid width direction to form terminal ends 130e1 and 130e2 of the resistor 130 in the grid width direction. The terminal ends 130e1 and 130e2 of the resistor 130 in the grid width direction are electrically connected to the electrode 150 via the wiring 140. In other words, the wiring 140 electrically connects the terminal ends 130e1 and 130e2 of the resistor 130 in the grid width direction to the electrodes 150.

[0042] The resistor 130 can be formed, for example, from a material containing Cr (chromium), a material containing Ni (nickel), or a material containing both Cr and Ni. That is, the resistor 130 can be formed from a material containing at least one of Cr and Ni. An example of a material containing Cr is a Cr mixed phase film. An example of a material containing Ni is Cu-Ni (copper nickel). An example of a material containing both Cr and Ni is Ni-Cr (nickel chromium).

[0043] Here, the Cr mixed phase film is a film in which Cr, CrN, Cr2N, etc. are mixed. The Cr mixed phase film may contain inevitable impurities such as chromium oxide.

[0044] The thickness of the resistor 130 is not particularly limited and can be appropriately selected depending on the purpose, and can be, for example, about 0.05 μm to 2 μm. In particular, it is preferable that the thickness of the resistor 130 is 0.1 μm or more in order to improve the crystallinity of the crystals constituting the resistor 130 (for example, the crystallinity of α-Cr). It is further preferable that the thickness of the resistor 130 is 1 μm or less in order to reduce cracks in the film and warping from the substrate 110 caused by internal stress of the film constituting the resistor 130. The width of the resistor 130 can be optimized for required specifications such as resistance value and lateral sensitivity, and can be, for example, about 10 μm to 100 μm in consideration of measures against disconnection.

[0045] For example, when the resistor 130 is a Cr mixed phase film, the stability of the gauge characteristics can be improved by using α-Cr (alpha chromium) which is a stable crystal phase as the main component. In addition, by using α-Cr as the main component of the resistor 130, the gauge factor of the strain gauge 100 can be set to 10 or more, and the gauge factor temperature coefficient TCS and the resistance temperature coefficient TCR can be set within the range of -1000 ppm / °C to +1000 ppm / °C. Here, the main component means that the target substance accounts for 50% by weight or more of the total substance constituting the resistor, but from the viewpoint of improving the gauge characteristics, the resistor 130 preferably contains α-Cr at 80% by weight or more, and more preferably contains 90% by weight or more. Note that α-Cr is Cr with a bcc structure (body-centered cubic lattice structure).

[0046] Furthermore, when the resistor 130 is a Cr mixed-phase film, the Cr mixed-phase film preferably contains 20% by weight or less of CrN and Cr2N. By containing 20% ​​by weight or less of CrN and Cr2N in the Cr mixed-phase film, a decrease in the gauge factor can be suppressed.

[0047] In addition, the ratio of Cr2N in CrN and Cr2N is preferably 80% by weight or more and less than 90% by weight, and more preferably 90% by weight or more and less than 95% by weight. When the ratio of Cr2N in CrN and Cr2N is 90% by weight or more and less than 95% by weight, the decrease in TCR (negative TCR) becomes more significant due to the Cr2N having semiconductor properties. Furthermore, by reducing the formation of ceramics, brittle fracture is reduced.

[0048] On the other hand, if a small amount of N2 or atomic N is mixed into the film, it will escape from the film due to the external environment (for example, a high temperature environment), causing a change in the film stress.By creating chemically stable CrN, it is possible to obtain a stable strain gauge without generating the unstable N mentioned above.

[0049] The wiring 140 is formed on the base material 110 and is electrically connected to the resistor 130 and the electrode 150. The wiring 140 has a first metal layer 141 and a second metal layer 142 laminated on the upper surface of the first metal layer 141. The wiring 140 is not limited to a straight line and can have any pattern. The wiring 140 can have any width and any length. For convenience, the wiring 140 and the electrode 150 are shown in FIG. 6 as having a matte finish that is thinner than the resistor 130.

[0050] The electrodes 150 are formed on the substrate 110 and are electrically connected to the resistor 130 via the wiring 140, and are formed, for example, in a substantially rectangular shape wider than the wiring 140. The electrodes 150 are a pair of electrodes for outputting to the outside a change in the resistance value of the resistor 130 caused by strain, and for example, a lead wire for external connection is joined to the electrodes 150.

[0051] The electrode 150 has a pair of first metal layers 151 and a second metal layer 152 laminated on the upper surface of each of the first metal layers 151. The first metal layers 151 are electrically connected to the ends 130e1 and 130e2 of the resistor 130 via the first metal layers 141 of the wiring 140. The first metal layers 151 are formed in a substantially rectangular shape in a plan view. The first metal layers 151 may be formed to have the same width as the wiring 140.

[0052] Although the resistor 130, the first metal layer 141, and the first metal layer 151 are given different reference numbers for convenience, they can be integrally formed from the same material in the same process. Therefore, the resistor 130, the first metal layer 141, and the first metal layer 151 have approximately the same thickness. Moreover, the second metal layer 142 and the second metal layer 152 are given different reference numbers for convenience, but they can be integrally formed from the same material in the same process. Therefore, the second metal layer 142 and the second metal layer 152 have approximately the same thickness.

[0053] The second metal layers 142 and 152 are formed of a material having a lower resistance than the resistor 130 (the first metal layers 141 and 151). The material of the second metal layers 142 and 152 is not particularly limited as long as it is a material having a lower resistance than the resistor 130, and can be appropriately selected according to the purpose. For example, when the resistor 130 is a Cr mixed phase film, the material of the second metal layers 142 and 152 can be Cu, Ni, Al, Ag, Au, Pt, etc., or an alloy of any of these metals, a compound of any of these metals, or a laminated film in which any of these metals, alloys, and compounds are appropriately laminated. The thickness of the second metal layers 142 and 152 is not particularly limited and can be appropriately selected according to the purpose, and can be, for example, about 3 μm to 5 μm.

[0054] The second metal layers 142 and 152 may be formed on a part of the upper surface of the first metal layers 141 and 151, or may be formed on the entire upper surface of the first metal layers 141 and 151. One or more other metal layers may be laminated on the upper surface of the second metal layer 152. For example, the second metal layer 152 may be a copper layer, and a gold layer may be laminated on the upper surface of the copper layer. Alternatively, the second metal layer 152 may be a copper layer, and a palladium layer and a gold layer may be sequentially laminated on the upper surface of the copper layer. By forming the top layer of the electrode 150 as a gold layer, the solder wettability of the electrode 150 can be improved.

[0055] In this way, the wiring 140 has a structure in which the second metal layer 142 is laminated on the first metal layer 141 made of the same material as the resistor 130. Therefore, the resistance of the wiring 140 is lower than that of the resistor 130, and it is possible to prevent the wiring 140 from functioning as a resistor. As a result, it is possible to improve the accuracy of strain detection by the resistor 130.

[0056] In other words, by providing the wiring 140 having a lower resistance than the resistor 130, the actual sensing portion of the strain gauge 100 can be limited to the local region where the resistor 130 is formed. Therefore, the accuracy of strain detection by the resistor 130 can be improved.

[0057] In particular, in a highly sensitive strain gauge with a gauge factor of 10 or more that uses a Cr mixed phase film as the resistor 130, making the wiring 140 lower in resistance than the resistor 130 and limiting the actual sensing part to the local region where the resistor 130 is formed has a significant effect on improving the strain detection accuracy. Making the wiring 140 lower in resistance than the resistor 130 also has the effect of reducing the lateral sensitivity.

[0058] The cover layer 160 is formed on the base material 110, covers the resistor 130 and the wiring 140, and exposes the electrodes 150. A part of the wiring 140 may be exposed from the cover layer 160. By providing the cover layer 160 that covers the resistor 130 and the wiring 140, it is possible to prevent mechanical damage and the like from occurring to the resistor 130 and the wiring 140. Furthermore, by providing the cover layer 160, it is possible to protect the resistor 130 and the wiring 140 from moisture and the like. Note that the cover layer 160 may be provided so as to cover the entire portion except for the electrodes 150.

[0059] The cover layer 160 can be formed from an insulating resin such as PI resin, epoxy resin, PEEK resin, PEN resin, PET resin, PPS resin, or composite resin (e.g., silicone resin, polyolefin resin). The cover layer 160 may contain a filler or a pigment. There is no particular limit to the thickness of the cover layer 160 and it can be appropriately selected depending on the purpose, but it can be, for example, about 2 μm to 30 μm.

[0060] To manufacture the strain gauge 100, first, a base material 110 is prepared, and a metal layer (for convenience, referred to as metal layer A) is formed on an upper surface 110a of the base material 110. Metal layer A is a layer that is finally patterned to become resistor 130, first metal layer 141, and first metal layer 151. Therefore, the material and thickness of metal layer A are similar to the material and thickness of resistor 130, first metal layer 141, and first metal layer 151 described above.

[0061] The metal layer A can be formed by, for example, a magnetron sputtering method using a target made of a raw material capable of forming the metal layer A. The metal layer A may be formed by a reactive sputtering method, a vapor deposition method, an arc ion plating method, a pulsed laser deposition method, or the like instead of the magnetron sputtering method.

[0062] From the viewpoint of stabilizing the gauge characteristics, it is preferable to vacuum-deposit a functional layer of a predetermined thickness as a base layer on the upper surface 110a of the base material 110 by, for example, conventional sputtering, before depositing the metal layer A.

[0063] In the present application, the functional layer refers to a layer having a function of promoting the crystal growth of at least the upper layer, metal layer A (resistor 130). The functional layer preferably further has a function of preventing oxidation of metal layer A due to oxygen and moisture contained in the base material 110, and a function of improving adhesion between the base material 110 and metal layer A. The functional layer may further have other functions.

[0064] Since the insulating resin film that constitutes the substrate 110 contains oxygen and moisture, and since Cr forms a self-oxidized film, particularly when the metal layer A contains Cr, it is effective for the functional layer to have the function of preventing oxidation of the metal layer A.

[0065] The material of the functional layer is not particularly limited as long as it has the function of promoting the crystal growth of at least the upper layer, the metal layer A (resistor 130), and can be appropriately selected depending on the purpose. For example, Cr (chromium), Ti (titanium), V (vanadium), Nb (niobium), Ta (tantalum), Ni (nickel), Y (yttrium), Zr (zirconium), Hf (hafnium), Si (silicon), C (carbon), Zn (zinc), Cu (copper), Bi (bismuth), etc. Examples of the metals that can be used include one or more metals selected from the group consisting of copper (II), iron (Fe), molybdenum (Mo), tungsten (W), ruthenium (Ru), Rh (Rhodium), Re (Rhenium), Os (Osmium), Ir (Iridium), Pt (Platinum), Pd (Palladium), Ag (Silver), Au (Gold), Co (Cobalt), Mn (Manganese), and aluminum (Aluminum), an alloy of any of the metals in this group, or a compound of any of the metals in this group.

[0066] Examples of the alloy include FeCr, TiAl, FeNi, NiCr, CrCu, etc. Examples of the compound include TiN, TaN, Si3N4, TiO2, Ta2O5, SiO2, etc.

[0067] When the functional layer is made of a conductive material such as a metal or alloy, the thickness of the functional layer is preferably 1 / 20 or less of the thickness of the resistor. In this range, the crystal growth of α-Cr can be promoted, and a part of the current flowing through the resistor can be prevented from flowing through the functional layer, which reduces the detection sensitivity of strain.

[0068] When the functional layer is made of a conductive material such as a metal or alloy, the thickness of the functional layer is preferably 1 / 50 or less of the thickness of the resistor. In this range, the crystal growth of α-Cr can be promoted, and the strain detection sensitivity can be further prevented from being reduced due to a part of the current flowing through the resistor flowing through the functional layer.

[0069] When the functional layer is made of a conductive material such as a metal or alloy, the thickness of the functional layer is more preferably 1 / 100 or less of the thickness of the resistor, which can further prevent a part of the current flowing through the resistor from flowing through the functional layer, thereby preventing a decrease in the strain detection sensitivity.

[0070] When the functional layer is made of an insulating material such as an oxide or nitride, the thickness of the functional layer is preferably 1 nm to 1 μm, which can promote the crystal growth of α-Cr and can be easily formed without cracking the functional layer.

[0071] When the functional layer is made of an insulating material such as an oxide or nitride, the thickness of the functional layer is preferably 1 nm to 0.8 μm, which can promote the crystal growth of α-Cr and can be easily formed without cracking the functional layer.

[0072] When the functional layer is made of an insulating material such as an oxide or nitride, the thickness of the functional layer is more preferably 1 nm to 0.5 μm, which can promote the crystal growth of α-Cr and can be more easily formed without cracking the functional layer.

[0073] The planar shape of the functional layer is patterned to be substantially the same as the planar shape of the resistor shown in FIG. 6, for example. However, the planar shape of the functional layer is not limited to being substantially the same as the planar shape of the resistor. When the functional layer is made of an insulating material, it does not have to be patterned to be the same as the planar shape of the resistor. In this case, the functional layer may be formed in a solid shape at least in the region where the resistor is formed. Alternatively, the functional layer may be formed in a solid shape on the entire upper surface of the substrate 110.

[0074] Furthermore, when the functional layer is made of an insulating material, the functional layer is formed relatively thick, at a thickness of 50 nm to 1 μm, and formed in a solid shape, so that the thickness and surface area of ​​the functional layer are increased, and the heat generated by the resistor can be dissipated to the substrate 110. As a result, in the strain gauge 100, a decrease in measurement accuracy due to self-heating of the resistor can be suppressed.

[0075] The functional layer can be formed in vacuum by conventional sputtering, for example, using a raw material capable of forming the functional layer as a target and introducing Ar (argon) gas into a chamber. By using conventional sputtering, the functional layer is formed while etching the upper surface 110a of the substrate 110 with Ar, so that the amount of the functional layer formed can be minimized and the effect of improving adhesion can be obtained.

[0076] However, this is just one example of a method for forming the functional layer, and the functional layer may be formed by other methods. For example, a method may be used in which the upper surface 110a of the substrate 110 is activated by a plasma treatment using Ar or the like before the formation of the functional layer, thereby improving adhesion, and then the functional layer is vacuum-formed by magnetron sputtering.

[0077] There are no particular restrictions on the combination of the material of the functional layer and the material of the metal layer A and can be selected appropriately depending on the purpose. For example, it is possible to use Ti for the functional layer and form a Cr mixed phase film with α-Cr (alpha chromium) as the main component for the metal layer A.

[0078] In this case, for example, the metal layer A can be formed by magnetron sputtering using a raw material capable of forming a Cr mixed phase film as a target and introducing Ar gas into a chamber. Alternatively, the metal layer A can be formed by reactive sputtering using pure Cr as a target and introducing an appropriate amount of nitrogen gas together with Ar gas into a chamber. In this case, the ratio of CrN and Cr2N contained in the Cr mixed phase film, and the ratio of Cr2N in CrN and Cr2N can be adjusted by changing the amount and pressure of the nitrogen gas introduced (nitrogen partial pressure) or by adjusting the heating temperature by providing a heating process.

[0079] In these methods, the growth surface of the Cr mixed-phase film is determined by the functional layer made of Ti, and a Cr mixed-phase film containing α-Cr, which has a stable crystal structure, as a main component, can be formed. Furthermore, the Ti constituting the functional layer is diffused into the Cr mixed-phase film, thereby improving the gauge characteristics. For example, the gauge factor of the strain gauge 100 can be set to 10 or more, and the gauge factor temperature coefficient TCS and the resistance temperature coefficient TCR can be set within the range of −1000 ppm / ° C. to +1000 ppm / ° C. In addition, when the functional layer is formed of Ti, the Cr mixed-phase film may contain Ti and TiN (titanium nitride).

[0080] When the metal layer A is a Cr mixed phase film, the functional layer made of Ti has all of the following functions: promoting the crystal growth of the metal layer A, preventing oxidation of the metal layer A due to oxygen and moisture contained in the base material 110, and improving the adhesion between the base material 110 and the metal layer A. The same applies when Ta, Si, Al, or Fe is used as the functional layer instead of Ti.

[0081] In this way, by providing a functional layer below the metal layer A, it is possible to promote crystal growth of the metal layer A, and to produce a metal layer A consisting of a stable crystal phase. As a result, it is possible to improve the stability of the gauge characteristics of the strain gauge 100. In addition, the material constituting the functional layer diffuses into the metal layer A, thereby improving the gauge characteristics of the strain gauge 100.

[0082] Next, the second metal layer 142 and the second metal layer 152 are formed on the upper surface of the metal layer A. The second metal layer 142 and the second metal layer 152 can be formed by, for example, a photolithography method.

[0083] Specifically, first, a seed layer is formed by, for example, sputtering or electroless plating so as to cover the upper surface of metal layer A. Next, a photosensitive resist is formed on the entire upper surface of the seed layer, and is exposed and developed to form openings that expose the regions in which second metal layer 142 and second metal layer 152 are to be formed. At this time, the pattern of second metal layer 142 can be formed into any shape by adjusting the shape of the openings in the resist. For example, a dry film resist can be used as the resist.

[0084] Next, for example, the second metal layer 142 and the second metal layer 152 are formed on the seed layer exposed in the opening by electrolytic plating using the seed layer as a power supply path. The electrolytic plating method is preferable in that it has high tact and can form low-stress electrolytic plating layers as the second metal layer 142 and the second metal layer 152. By making the electrolytic plating layer thick and low-stress, it is possible to prevent warping of the strain gauge 100. The second metal layer 142 and the second metal layer 152 may be formed by electroless plating.

[0085] Next, the resist is removed. For example, the resist can be removed by immersing the resist in a solution that can dissolve the resist material.

[0086] Next, a photosensitive resist is formed on the entire upper surface of the seed layer, and is exposed and developed to be patterned into a planar shape similar to that of the resistor 130, wiring 140, and electrode 150 in Fig. 6. For example, a dry film resist or the like can be used as the resist. Then, the resist is used as an etching mask to remove the metal layer A and the seed layer exposed from the resist, thereby forming the resistor 130, wiring 140, and electrode 150 in the planar shape of Fig. 6.

[0087] For example, unnecessary portions of the metal layer A and the seed layer can be removed by wet etching. If a functional layer is formed below the metal layer A, the functional layer is patterned by etching into the planar shape shown in Fig. 6, similar to the resistor 130, the wiring 140, and the electrode 150. At this point, the seed layer is formed on the resistor 130, the first metal layer 141, and the first metal layer 151.

[0088] Next, the second metal layer 142 and the second metal layer 152 are used as an etching mask to remove unnecessary seed layer exposed from the second metal layer 142 and the second metal layer 152, thereby forming the second metal layer 142 and the second metal layer 152. Note that the seed layer directly below the second metal layer 142 and the second metal layer 152 remains. For example, the unnecessary seed layer can be removed by wet etching using an etching solution that etches the seed layer but does not etch the functional layer, the resistor 130, the wiring 140, and the electrode 150.

[0089] Thereafter, as necessary, a cover layer 160 that covers the resistor 130 and the wiring 140 and exposes the electrodes 150 is provided on the upper surface 110a of the base material 110, thereby completing the strain gauge 100. The cover layer 160 can be produced, for example, by laminating a semi-cured thermosetting insulating resin film on the upper surface 110a of the base material 110 so as to cover the resistor 130 and the wiring 140 and expose the electrodes 150, and then heating and curing the film. The cover layer 160 may also be produced by applying a liquid or paste-like thermosetting insulating resin to the upper surface 110a of the base material 110 so as to cover the resistor 130 and the wiring 140 and expose the electrodes 150, and then heating and curing the resin.

[0090] Although preferred embodiments have been described above in detail, the present invention is not limited to the above-described embodiments, and various modifications and substitutions can be made to the above-described embodiments without departing from the scope of the claims. [Explanation of symbols]

[0091] REFERENCE SIGNS LIST 1 pulse wave sensor, 10 strain generating body, 11 frame portion, 12 beam portion, 12a first beam, 12b second beam, 13 connection portion, 14 load portion, 20 housing, 100 strain gauge, 110 substrate, 110a upper surface, 130 resistor, 130e1, 130e2 termination, 140 wiring, 150 electrode, 160 cover layer

Claims

1. A strain body, A strain gauge having a Cr mixed phase film as a resistor, the strain gauge being provided on the strain generating body, The strain body is A frame portion and A beam portion bridging the inside of the frame portion; A connection portion that connects an inside of the frame portion and an outside of the beam portion without any gaps in a plan view, the connection portion is thinner than the frame portion and the beam portion, The beam portion includes a first beam and a second beam that intersect in a cross shape in a plan view, A load portion protruding from the beam portion is provided in an area where the first beam and the second beam intersect, The pulse wave sensor detects a pulse wave based on a change in resistance value of the resistor accompanying deformation of the beam portion.

2. The pulse wave sensor according to claim 1 , wherein the first beam is longer than the second beam.

3. one side of the frame portion, the beam portion, and the connection portion in a thickness direction is flush with one another, The load portion is provided on the one side, 3. The pulse wave sensor according to claim 1, wherein the strain gauge is provided on the other side opposite to the one side.

4. The strain gauge includes four strain gauges, Two of the four strain gauges are arranged on a side of the first beam closer to the frame portion so as to face each other across the load portion in a plan view, 4. The pulse wave sensor according to claim 1, wherein the other two of the four strain gauges are arranged on a side of the second beam closer to the load portion so as to face each other across the load portion in a planar view.

5. The pulse wave sensor according to claim 1 , wherein the first beam and the second beam have a constant width except for an area where they intersect.

6. The pulse wave sensor according to claim 1 , wherein the strain element has a rectangular shape in a plan view.

Citation Information

Patent Citations

  • Semiconductor pressure difference detector

    JP1984083023A

  • Catheter end pressure converter

    JP1987176430A

  • Semiconductor sensor and manufacture thereof

    JP1993340957A

  • Acceleration sensor

    JP1999183515A

  • Pressure pulse wave sensor

    JP2002078689A