Wafer placement table

The wafer mounting table addresses thermal non-uniformity by optimizing coolant flow path alignment with ceramic protrusions, improving thermal uniformity and heat removal efficiency.

JP7572936B2Active Publication Date: 2024-10-24NGK CORP
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
JP2021192899
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2021-11-29
Publication Date
2024-10-24
Estimated Expiration
2041-11-29

AI Technical Summary

Technical Problem

Conventional wafer mounting tables experience non-uniform thermal distribution due to coolant temperature differences along the flow path, leading to insufficient thermal uniformity of the wafer.

Method used

The wafer mounting table design incorporates ceramic small protrusions on the wafer placement surface, with varying area ratios and distances from a reference plane, aligned with the coolant flow path to enhance thermal conductivity and uniformity. The coolant flow path is optimized to minimize thermal resistance and promote heat exchange.

Benefits of technology

This design achieves improved thermal uniformity of the wafer by reducing temperature differences across the wafer surface, enhancing heat removal efficiency through ceramic protrusions and a metal bonding layer with high thermal conductivity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007572936000001
    Figure 0007572936000001
  • Figure 0007572936000002
    Figure 0007572936000002
  • Figure 0007572936000003
    Figure 0007572936000003
Patent Text Reader

Abstract

To improve the wafer uniformity.SOLUTION: A wafer table 10 includes a ceramic substrate 20 having a wafer mounting surface on which a wafer can be mounted and having electrodes 26 built therein, a cooling substrate 30 that has a coolant channel 32, a metal bonding layer 40 that bonds the ceramic substrate 20 and the cooling substrate 30, and a plurality of small projections 22c supporting the lower surface of the wafer W on the top surface on the reference surface 22d of the wafer mounting surface 22a, The top surfaces of the small projections 22c are coplanar. In a channel overlapping range R10 overlapping the coolant channel 32 in plan view on the wafer mounting surface 22a, the area ratio of the small projections 22c in a small region A1 opposite to the uppermost stream portion 32U in the range overlapping the wafer mounting surface 22a when the coolant channel 32 is planarly viewed is the lowest.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a wafer stage. [Background technology]

[0002] Conventionally, a wafer mounting table is known that includes a ceramic substrate having a wafer mounting surface and an electrode built therein, a cooling substrate having a coolant flow path, and a bonding layer that bonds the ceramic substrate and the cooling substrate. For example, Patent Documents 1 and 2 disclose that such a wafer mounting table uses a cooling substrate made of a metal matrix composite material having a linear thermal expansion coefficient similar to that of the ceramic substrate. They also disclose that the wafer mounting table is provided with a terminal hole through which a power supply terminal for supplying power to the electrode is inserted, a gas hole through which He gas is supplied to the back surface of the wafer, and a lift pin hole through which a lift pin for lifting the wafer from the wafer mounting surface is inserted. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 5666748 [Patent Document 2] Patent No. 5666749 Summary of the Invention [Problem to be solved by the invention]

[0004] However, when the wafer mounting table is in use, the coolant flows from the upstream to the downstream side of the coolant flow path while removing heat from the wafer, so the temperature of the coolant tends to be higher on the downstream side than on the upstream side, resulting in insufficient thermal uniformity of the wafer.

[0005] The present invention has been made to solve these problems, and has as its main object to improve the thermal uniformity of the wafer. [Means for solving the problem]

[0006] The first wafer mounting table of the present invention comprises: a ceramic substrate having an electrode built therein and a wafer mounting surface on an upper surface of the ceramic substrate; A cooling substrate having a refrigerant flow path; a bonding layer that bonds the ceramic substrate and the cooling substrate; a plurality of small protrusions on a reference surface of the wafer mounting surface, the small protrusions supporting the lower surface of the wafer with their top surfaces; A wafer mounting table comprising: The top surfaces of the small projections are coplanar; in a flow passage overlapping range of the wafer mounting surface that overlaps with the refrigerant flow passage in a plan view, an area ratio of the small protrusions is minimum in a portion facing a most upstream portion of the range that overlaps with the wafer mounting surface in a plan view of the refrigerant flow passage, It is something.

[0007] In this first wafer placement table, the area ratio of the small protrusions in the flow path overlapping range is the lowest in the portion facing the most upstream portion. Here, the "area ratio of the small protrusions" refers to the ratio of the total area of ​​the small protrusions to a unit area. When the wafer placement table is in use, the coolant flows from the upstream side of the coolant flow path to the downstream side while taking heat from the high-temperature wafer, so the temperature of the coolant flowing through the coolant flow path is higher on the downstream side than on the upstream side. On the other hand, in this wafer placement table, the area ratio of the small protrusions in the flow path overlapping range is the lowest in the portion facing the most upstream portion, so the thermal resistance from the coolant flow path to the wafer placement surface is lower in other portions than the portion facing the most upstream portion. This is due to the following reason. The small protrusions are ceramic, and ceramics have better thermal conductivity than voids. Therefore, in the portion where the area ratio of the small protrusions is high, the proportion of ceramics in the planar direction is higher than in the portion where the area ratio of the small protrusions is not high, which promotes heat exchange between the wafer and the coolant and promotes heat removal. Therefore, overall, the temperature difference can be reduced in the flow path overlapping range of the wafer placement surface. Therefore, the temperature uniformity of the wafer is improved.

[0008] In the first wafer stage of the present invention, the area ratio of the small protrusions in the flow passage overlapping area may be gradually increased from a portion facing the most upstream portion toward the downstream of the coolant flow passage, thereby improving the temperature uniformity of the wafer.

[0009] In the first wafer mounting table of the present invention, the area ratio of the small protrusions in the flow passage overlapping range, which overlaps with the wafer mounting surface when the refrigerant flow passage is viewed from above, facing the most downstream portion may be 150% or more of the area ratio of the small protrusions in the range facing the most upstream portion, thereby further improving the temperature uniformity of the wafer.

[0010] In the first wafer mounting table of the present invention, the area ratio of the small protrusions may be higher in an adjacent area adjacent to the specified area and outside the flow path overlapping area than in a specified area of ​​the flow path overlapping area. Generally, heat is less easily removed from the adjacent area than in the specified area of ​​the flow path overlapping area. This is because there is no refrigerant flow path directly below. On the other hand, in the wafer mounting table of the present invention, the area ratio of the small protrusions is higher in the adjacent area than in the specified area of ​​the flow path overlapping area. This promotes heat removal in the specific area. This results in higher thermal uniformity of the wafer.

[0011] The first wafer mounting table of the present invention may have a hole penetrating the cooling base material in the vertical direction, and the cross-sectional area of ​​the coolant flow path may be smaller in the peripheral region of the hole than in the region outside the peripheral region of the hole, and the area ratio of the small protrusions may be higher in the region directly above the hole than in the peripheral region outside the region directly above the hole on the wafer mounting surface. Generally, the region directly above such a hole on the wafer is prone to becoming a hot spot. On the other hand, the area ratio of the small protrusions is higher in the region directly above than in the peripheral region. Therefore, heat removal from the region directly above is promoted. Therefore, the thermal uniformity of the wafer is improved.

[0012] The second wafer mounting table of the present invention is a ceramic substrate having an electrode built therein and a wafer mounting surface on an upper surface of the ceramic substrate; A cooling substrate having a refrigerant flow path; a bonding layer that bonds the ceramic substrate and the cooling substrate; a plurality of small protrusions on a reference surface of the wafer mounting surface, the small protrusions supporting the lower surface of the wafer with their top surfaces; A wafer mounting table comprising: The top surfaces of the small projections are coplanar; in a flow passage overlapping range of the wafer mounting surface that overlaps with the refrigerant flow passage in a plan view, a distance from a top surface of the small protrusion to the reference surface is longest at a portion facing a most upstream portion of the range that overlaps with the wafer mounting surface in a plan view of the refrigerant flow passage, It is something.

[0013] In this second wafer mounting table, the distance from the top surface of the small protrusion to the reference surface in the flow path overlapping range is longest at the portion facing the most upstream portion. When the wafer mounting table is in use, the coolant flows from the upstream side of the coolant flow path to the downstream side while removing heat from the high-temperature wafer, so the temperature of the coolant flowing through the coolant flow path is higher on the downstream side than on the upstream side. On the other hand, in this wafer mounting table, the distance from the top surface of the small protrusion to the reference surface in the flow path overlapping range is In the area facing the most upstream part Since the small protrusions are the longest, the thermal resistance from the coolant flow path to the wafer placement surface is lower in areas other than the area facing the most upstream portion. This is for the following reason. The small protrusions are made of ceramic, which has a better thermal conductivity than voids. Top surface of In the area where the distance from the reference plane is short, Top surface of Compared to the portion where the distance from the wafer to the reference surface is not shortened, the proportion of voids in the thickness direction is low, which promotes heat exchange between the wafer and the refrigerant and promotes heat removal. Therefore, overall, it is possible to reduce the temperature difference in the flow path overlap area of ​​the wafer placement surface. This improves the thermal uniformity of the wafer.

[0014] In the second wafer stage of the present invention, the distance from the top surface of the small protrusion to the reference plane in the flow passage overlapping area may be gradually shortened from the portion facing the most upstream portion toward the downstream of the coolant flow passage, thereby improving the temperature uniformity of the wafer.

[0015] In the second wafer stage of the present invention, in the flow path overlapping range, the distance from the top surface of the small protrusion to the reference plane in the portion facing the most downstream portion may be 80% or less of the distance from the top surface of the small protrusion to the reference plane in the portion facing the most upstream portion, thereby further improving the temperature uniformity of the wafer.

[0016] In the second wafer mounting table of the present invention, the distance from the top surface of the small protrusion to the reference surface may be shorter in an adjacent area adjacent to the specified area and outside the flow path overlap area than in a specified area of ​​the flow path overlap area. Generally, heat is less easily removed from the adjacent area than in the specified area of ​​the flow path overlap area. This is because there is no refrigerant flow path directly below. On the other hand, in the wafer mounting table of the present invention, the distance from the top surface of the small protrusion to the reference surface is shorter in the adjacent area than in the specified area of ​​the flow path overlap area. This promotes heat removal in a specific area. This results in higher thermal uniformity of the wafer.

[0017] The second wafer mounting table of the present invention may have a hole penetrating the cooling base material in the vertical direction, and the cross-sectional area of ​​the coolant flow path may be smaller in the peripheral region of the hole than in the region outside the peripheral region of the hole, and the distance from the top surface of the small protrusion to the reference plane may be shorter in the region directly above the hole than in the peripheral region outside the region directly above the hole on the wafer mounting surface. Generally, the region directly above such a hole on the wafer is prone to becoming a hot spot. On the other hand, the distance from the small protrusion to the reference plane is shorter in the region directly above than in the peripheral region. Therefore, heat removal from the region directly above is promoted. Therefore, the thermal uniformity of the wafer is improved.

[0018] In the first and second wafer mounting tables of the present invention, the cooling base material may be made of a metal matrix composite material, and the bonding layer may be a metal bonding layer. In a structure in which the cooling base material is a metal matrix composite material and the bonding layer is a metal bonding layer, the thermal resistance from the coolant flow path to the wafer mounting surface is small, so the wafer temperature is easily affected by the temperature gradient of the coolant. Therefore, it is highly meaningful to apply the present invention. In addition, the metal bonding layer has a high thermal conductivity and is therefore suitable for heat extraction. Furthermore, the thermal expansion difference between the ceramic base material and the cooling base material made of a metal matrix composite material can be reduced, so that even if the stress relaxation property of the metal bonding layer is low, problems are unlikely to occur. [Brief description of the drawings]

[0019] [Figure 1] FIG. 2 is a vertical cross-sectional view of the wafer mounting table 10 installed in the chamber 94. [Diagram 2] FIG. [Diagram 3] 3 is a cross-sectional view of a cooling substrate 30 cut by a horizontal plane passing through a refrigerant flow path 32 as viewed from above. FIG. [Figure 4] An enlarged view of a small area Ai and an adjacent area Qi. [Diagram 5] 4 is an enlarged view of the directly above region R30 and the surrounding region R40. [Figure 6] 5A to 5C are diagrams showing the manufacturing process of the wafer mounting table 10. [Figure 7] FIG. 2 is an explanatory diagram showing the distance from the top surface of the small protrusion 22c to the reference surface 22d in the small areas A1 and Ak. [Figure 8] FIG. 4 is a plan view of another example of the wafer mounting table 10. [Figure 9] 4 is a cross-sectional view of the cooling substrate 30 cut by a horizontal plane passing through a refrigerant flow path 82, as viewed from above. FIG. [Figure 10] FIG. 4 is a plan view of another example of the wafer mounting table 10. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0020] A preferred embodiment of the present invention will be described below with reference to the drawings. Fig. 1 is a vertical cross-sectional view of the wafer mounting table 10 installed in the chamber 94 (a cross-sectional view when cut along a plane including the central axis of the wafer mounting table 10), Fig. 2 is a plan view of the wafer mounting table 10, Fig. 3 is a cross-sectional view of the cooling substrate 30 cut along a horizontal plane passing through the refrigerant flow path 32 as viewed from above, Fig. 4 is an enlarged view of the small region Ai and the adjacent region Qi, and Fig. 5 is an enlarged view of the directly above region R30 and the peripheral region R40. For convenience of explanation, the flow path overlap range R10 is hatched in Figs. 2 and 4, and the terminal hole 51, the power supply terminal 54, and the insulating tube 55 are omitted in Fig. 3.

[0021] The wafer mounting table 10 is used for performing CVD, etching, and the like on a wafer W using plasma, and is fixed to a mounting plate 96 provided inside a semiconductor process chamber 94. The wafer mounting table 10 includes a ceramic base 20, a cooling base 30, and a metal bonding layer 40.

[0022] The ceramic base 20 has a central portion 22 having a circular wafer mounting surface 22a, and an outer peripheral portion 24 having an annular focus ring mounting surface 24a on the outer periphery of the central portion 22. Hereinafter, the focus ring may be abbreviated as "FR." A wafer W is mounted on the wafer mounting surface 22a, and a focus ring 78 is mounted on the FR mounting surface 24a. The ceramic base 20 is made of a ceramic material such as alumina or aluminum nitride. The FR mounting surface 24a is one step lower than the wafer mounting surface 22a.

[0023] The center portion 22 of the ceramic base material 20 incorporates a wafer adsorption electrode 26 on the side close to the wafer mounting surface 22a. The wafer adsorption electrode 26 is formed of a material containing, for example, W, Mo, WC, MoC, etc. The wafer adsorption electrode 26 is a disk-shaped or mesh-shaped monopolar electrostatic adsorption electrode. The layer of the ceramic base material 20 above the wafer adsorption electrode 26 functions as a dielectric layer. A wafer adsorption DC power source 52 is connected to the wafer adsorption electrode 26 via a power supply terminal 54. The power supply terminal 54 is inserted into a terminal hole 51 provided between the lower surface of the wafer adsorption electrode 26 and the lower surface of the cooling base material 30 of the wafer mounting table 10. The power supply terminal 54 is provided so as to pass through an insulating tube 55 arranged in a through hole of the terminal hole 51 that vertically penetrates the cooling base material 30 and the metal bonding layer 40, and reach the wafer adsorption electrode 26 from the lower surface of the ceramic base material 20. A low pass filter (LPF) 53 is provided between the wafer attracting DC power supply 52 and the wafer attracting electrode .

[0024] As shown in FIG. 2, a seal band 22b is formed along the outer edge of the wafer mounting surface 22a, and a plurality of small protrusions 22c are formed on the entire surface. The seal band 22b and the plurality of small protrusions 22c are formed on a reference surface 22d of the wafer mounting surface 22a. In this embodiment, the small protrusions 22c are flat cylindrical protrusions. The top surface of the seal band 22b and the top surfaces of the plurality of small protrusions 22c are located on the same plane. The heights of the seal band 22b and the small protrusions 22c (i.e., the distances from the reference surface 22d to these top surfaces) are several μm to several tens of μm. The wafer W is mounted on the wafer mounting surface 22a in a state of contact with the top surface of the seal band 22b and the top surfaces of the plurality of small protrusions 22c.

[0025] The cooling substrate 30 is a disk member made of a metal matrix composite material (also called metal matrix composite (MMC)). The cooling substrate 30 has a cooling medium flow path 32 through which a cooling medium can circulate inside. The cooling medium flow path 32 is connected to a cooling medium supply path 36 and a cooling medium discharge path 38, and the cooling medium discharged from the cooling medium discharge path 38 is returned to the cooling medium supply path 36 after temperature adjustment. Examples of MMC include materials containing Si, SiC, and Ti, and materials in which a porous SiC body is impregnated with Al and / or Si. A material containing Si, SiC, and Ti is called SiSiCTi, a material in which a porous SiC body is impregnated with Al is called AlSiC, and a material in which a porous SiC body is impregnated with Si is called SiSiC. When the ceramic substrate 20 is an alumina substrate, the MMC used for the cooling substrate 30 is preferably AlSiC or SiSiCTi, which has a thermal expansion coefficient close to that of alumina. The cooling substrate 30 is connected to an RF power source 62 via a power supply terminal 64. A high-pass filter (HPF) 63 is disposed between the cooling base 30 and the RF power supply 62. The cooling base 30 has a flange portion 34 used for clamping the wafer stage 10 to a mounting plate 96 on the lower surface side.

[0026] As shown in FIG. 3, when the cross section of the refrigerant flow path 32 cut on a horizontal plane is viewed from above, the refrigerant flow path 32 is formed in a single stroke from the inlet 32a to the outlet 32b over the entire region of the cooling substrate 30 except for the flange portion 34. In this embodiment, the refrigerant flow path 32 is formed in a zigzag shape. Specifically, the refrigerant flow path 32 has straight portions 32c and folded portions 32d alternately provided from the inlet 32a connected to the refrigerant supply path 36 to the outlet 32b connected to the refrigerant discharge path 38. Here, when the most upstream portion 32U and the most downstream portion 32L are defined in the region of the refrigerant flow path 32 overlapping with the wafer placement surface 22a in a plan view, the most upstream portion 32U and the most downstream portion 32L are located as shown in FIG. 3. The cross-sectional area of ​​the refrigerant flow path 32 gradually increases from the most upstream portion 32U to the most downstream portion 32L of the refrigerant flow path 32 except for the peripheral region of the terminal hole 51. A distance d from the ceiling surface of the coolant flow path 32 to the top surface of the small protrusion 22c provided on the wafer mounting surface 22a is constant from the most upstream part 32U to the most downstream part 32L, as shown in FIG.

[0027] The metal bonding layer 40 bonds the lower surface of the ceramic base material 20 and the upper surface of the cooling base material 30. The metal bonding layer 40 may be, for example, a layer formed of solder or a metal brazing material. The metal bonding layer 40 is formed, for example, by TCB (thermal compression bonding). TCB refers to a known method in which a metal bonding material is sandwiched between two members to be bonded, and the two members are pressure-bonded while being heated to a temperature equal to or lower than the solidus temperature of the metal bonding material.

[0028] The area of ​​the wafer mounting surface 22a that overlaps with the refrigerant flow passage 32 in a plan view is called the flow passage overlap area R10. The flow passage overlap area R10 is the hatched area in FIG. 2. The area ratio of the small protrusions 22c in the flow passage overlap area R10 is the ratio of the total area of ​​the top faces of the small protrusions 22c to a unit area, and is calculated as follows. That is, first, as shown in FIG. 2, the flow passage overlap area R10 is divided into n areas (n is an integer of 2 or more). Here, among the n areas, the i-th area (i is an integer of 1 to n) from the upstream side of the refrigerant flow passage 32 is called the small area Ai. The areas of the small areas A1 to An are all the same. Next, the area of ​​the small area Ai is calculated, and the total area of ​​the top faces of the small protrusions 22c provided in the small area Ai is calculated. Then, the total area of ​​the small protrusions 22c in the small area Ai is divided by the area of ​​the small area Ai to calculate the area ratio of the small protrusions 22c in the small area Ai. The area ratio of the small protrusions 22c in the flow passage overlapping range R10 is lowest in the portion facing the most upstream portion 32U, that is, in the small area A1.

[0029] The area ratio of the small protrusions 22c in the flow passage overlapping range R10 gradually increases from the small region A1 toward the downstream of the refrigerant flow passage 32 (from the small region A1 toward the small region An). The small region An is the portion facing the most downstream portion 32L. The area ratio of the small protrusions 22c in the small region An facing the most downstream portion 32L in the flow passage overlapping range R10 is gradually increased compared to the area ratio of the small region An facing the most upstream portion 32U. A1 It is preferable that the area ratio of the small protrusions 22c in the area is 150% or more.

[0030] The area ratio of the small protrusions 22c is higher in an adjacent area Qi adjacent to a small area Ai and outside the flow path overlapping range R10 than in a small area Ai in the flow path overlapping range R10. For example, as shown in FIG 4, the area ratio of the small protrusions 22c in the adjacent areas Qi on both sides of a small area Ai (e.g., a small area A6) is higher than the area ratio of the small protrusions 22c in the small area Ai.

[0031] Here, the area directly above the terminal hole 51 on the wafer placement surface 22a is defined as the direct-above region R30, and the area around the direct-above region outside the direct-above region R30 is defined as the peripheral region R40. The direct-above region R30 is a circular region with a predetermined radius (e.g., a radius of 25 mm), and the peripheral region R40 is an annular region surrounding the direct-above region R30. The area ratio of the small protrusions 22c is higher in the direct-above region R30 than in the peripheral region R40. For example, as shown in FIG. 5, the small protrusions 22c are provided so that the arrangement density of the small protrusions 22c is higher in the direct-above region R30 than in the peripheral region R40. The area ratio of the small protrusions 22c in the direct-above region R30 is preferably at least twice the area ratio of the small protrusions 22c in the peripheral region R40.

[0032] The side surface of the outer periphery 24 of the ceramic substrate 20, the outer periphery of the metal bonding layer 40, and the side surface of the cooling substrate 30 are covered with an insulating film 42. The insulating film 42 may be, for example, a thermally sprayed film of alumina, yttria, or the like.

[0033] The wafer mounting table 10 is attached to a mounting plate 96 provided inside a chamber 94 by using a clamp member 70. The clamp member 70 is an annular member having a cross section in a substantially inverted L-shape, and has an inner peripheral step surface 70a. The wafer mounting table 10 and the mounting plate 96 are integrated by the clamp member 70. With the inner peripheral step surface 70a of the clamp member 70 placed on the flange portion 34 of the cooling substrate 30 of the wafer mounting table 10, a bolt 72 is inserted from the upper surface of the clamp member 70 and screwed into a screw hole provided on the upper surface of the mounting plate 96. The bolt 72 is attached to a plurality of locations (e.g., 8 locations or 12 locations) that are provided at equal intervals along the circumferential direction of the clamp member 70. The clamp member 70 and the bolt 72 may be made of an insulating material or a conductive material (metal, etc.).

[0034] Next, a manufacturing example of the wafer mounting table 10 will be described with reference to FIG. 6. FIG. 6 is a manufacturing process diagram of the wafer mounting table 10. First, a disk-shaped ceramic sintered body 120, which is the base of the ceramic base material 20, is produced by hot-pressing and firing a ceramic powder compact (FIG. 6A). The ceramic sintered body 120 has a wafer adsorption electrode 26 built in. Next, a terminal hole upper portion 151a is formed between the lower surface of the ceramic sintered body 120 and the wafer adsorption electrode 26 (FIG. 6B). Then, a power supply terminal 54 is inserted into the terminal hole upper portion 151a to join the power supply terminal 54 and the wafer adsorption electrode 26 (FIG. 6C).

[0035] In parallel with this, two MMC disk members 131 and 136 are fabricated (FIG. 6D). Then, holes penetrating in the vertical direction are drilled in both MMC disk members 131 and 136, and a groove 132 that will eventually become the coolant flow path 32 is formed in the lower surface of the upper MMC disk member 131 (FIG. 6E). Specifically, a terminal hole intermediate portion 151b is drilled in the upper MMC disk member 131. The groove 132 is formed by machining the upper MMC disk member 131 so as to have the same shape as the coolant flow path 32. In addition, a terminal hole lower portion 151c, a through hole 133 for the coolant supply path, and a through hole 134 for the coolant discharge path are drilled in the lower MMC disk member 136. When the ceramic sintered body 120 is made of alumina, the MMC disk members 131 and 136 are preferably made of SiSiCTi or AlSiC. This is because the thermal expansion coefficient of alumina is roughly the same as that of SiSiCTi and AlSiC.

[0036] The SiSiCTi disk member can be manufactured, for example, as follows. First, silicon carbide, metal Si, and metal Ti are mixed to produce a powder mixture. Next, the obtained powder mixture is uniaxially pressed to produce a disk-shaped compact, which is then hot-press sintered in an inert atmosphere to obtain the SiSiCTi disk member.

[0037] Next, a metal bonding material is placed between the lower surface of the upper MMC disk member 131 and the upper surface of the lower MMC disk member 136, and a metal bonding material is placed on the upper surface of the upper MMC disk member 131. Each metal bonding material has a through hole at a position opposite to each hole. Then, the power supply terminal 54 of the ceramic sintered body 120 is inserted into the terminal hole intermediate part 151b and the terminal hole lower part 151c, and the ceramic sintered body 120 is placed on the metal bonding material placed on the upper surface of the upper MMC disk member 131. This results in a laminate in which the lower MMC disk member 136, the metal bonding material, the upper MMC disk member 131, the metal bonding material, and the ceramic sintered body 120 are laminated in this order from below. The laminate is heated and pressurized (TCB) to obtain the bonded body 110 (FIG. 6F). The bonded body 110 is formed by bonding the ceramic sintered body 120 to the upper surface of the MMC block 130, which is the base of the cooling base material 30, via the metal bonding layer 40. The MMC block 130 is formed by bonding an upper MMC disk member 131 and a lower MMC disk member 136 via a metal bonding layer 135. The MMC block 130 has a coolant flow path 32, a coolant supply path 36, a coolant discharge path 38, and a terminal hole 51. The terminal hole 51 is a hole in which an upper terminal hole portion 151a, a middle terminal hole portion 151b, and a lower terminal hole portion 151c are connected to each other.

[0038] For example, TCB is performed as follows. That is, the laminate is pressed and bonded at a temperature equal to or lower than the solidus temperature of the metal bonding material (for example, a temperature equal to or higher than the solidus temperature minus 20°C and equal to or lower than the solidus temperature), and then returned to room temperature. This causes the metal bonding material to become the metal bonding layer 40. As the metal bonding material at this time, an Al-Mg based bonding material or an Al-Si-Mg based bonding material can be used. For example, when TCB is performed using an Al-Si-Mg based bonding material, the laminate is pressed in a heated state under a vacuum atmosphere. It is preferable to use a metal bonding material having a thickness of about 100 μm.

[0039] Next, the outer periphery of the ceramic sintered body 120 is cut to form a step. Next, a mask for forming the seal band 22b and small protrusions 22c is attached to the upper surface of the ceramic sintered body 120, and a blasting process is performed by spraying a blasting medium, and then the mask is removed. The small protrusions 22c are formed by the blasting process. As a result, the ceramic sintered body 120 becomes a ceramic base material 20 having a central portion 22, an outer periphery 24, and a wafer mounting surface 22a. Also, by cutting the outer periphery of the MMC block 130 to form a step, twist , and the cooling substrate 30 is provided with a flange portion 34. An insulating tube 55 is disposed in the terminal hole 51, through which the power supply terminal 54 is inserted, from the underside of the ceramic substrate 20 to the underside of the cooling substrate 30. Furthermore, the insulating film 42 is formed by thermally spraying the side surface of the outer periphery 24 of the ceramic substrate 20, the periphery of the metal bonding layer 40, and the side surface of the cooling substrate 30 with ceramic powder (FIG. 6G). In this manner, the wafer mounting table 10 is obtained.

[0040] Although the cooling substrate 30 in FIG. 1 is shown as an integrated component, it may have a structure in which two components are joined with a metal joining layer as shown in FIG. 6G, or it may have a structure in which three or more components are joined with a metal joining layer.

[0041] Next, an example of use of the wafer stage 10 will be described with reference to Fig. 1. As described above, the wafer stage 10 is fixed to the mounting plate 96 of the chamber 94 by the clamp members 70. A shower head 98 is disposed on the ceiling surface of the chamber 94, which ejects process gas into the chamber 94 from a number of gas injection holes.

[0042] A focus ring 78 is placed on the FR mounting surface 24a of the wafer mounting table 10, and a disk-shaped wafer W is placed on the wafer mounting surface 22a. The focus ring 78 has a step along the inner circumference of the upper end so as not to interfere with the wafer W. In this state, a DC voltage from the wafer suction DC power supply 52 is applied to the wafer suction electrode 26 to suction the wafer W onto the wafer mounting surface 22a. Then, the interior of the chamber 94 is set to a predetermined vacuum atmosphere (or reduced pressure atmosphere), and an RF voltage from the RF power supply 62 is applied to the cooling substrate 30 while a process gas is supplied from the shower head 98. Then, plasma is generated between the wafer W and the shower head 98. Then, the plasma is used to perform CVD film formation or etching on the wafer W. The focus ring 78 is also worn out as the wafer W is plasma-processed, but since the focus ring 78 is thicker than the wafer W, the focus ring 78 is replaced after processing a plurality of wafers W.

[0043] When processing the wafer W with high-power plasma, it is necessary to efficiently cool the wafer W. In the wafer mounting table 10, a metal bonding layer 40 with high thermal conductivity is used as a bonding layer between the ceramic base material 20 and the cooling base material 30, instead of a resin layer with low thermal conductivity. Therefore, the ability to draw heat from the wafer W (heat extraction ability) is high. In addition, since the difference in thermal expansion between the ceramic base material 20 and the cooling base material 30 is small, even if the stress relaxation of the metal bonding layer 40 is low, problems are unlikely to occur. When the wafer mounting table 10 is used, the coolant flows from the most upstream part 32U of the coolant flow path 32 to the most downstream part 32L while removing heat from the high-temperature wafer W, so that the temperature of the coolant flowing through the coolant flow path 32 is higher in the most downstream part 32L than in the most upstream part 32U. On the other hand, compared to the small region A1, which is a portion of the flow passage overlapping range R10 facing the most upstream portion 32U, the area ratio of the small protrusions 22c is higher in the portion other than the small region A1, so the thermal resistance from the refrigerant flow passage 32 to the wafer mounting surface 22a is lower in the small regions A2 to An than in the small region A1. Therefore, overall, it is possible to reduce the temperature difference within the flow passage overlapping range R10 of the wafer mounting surface 22a. The flow rate of the refrigerant flowing through the refrigerant flow passage 32 is preferably 20 to 40 L / min, and more preferably 15 to 35 L / min.

[0044] In the wafer mounting table 10 of the present embodiment described above, the area ratio of the small protrusions 22c in the flow passage overlap range R10 is the lowest in the small region A1, which is the portion facing the most upstream portion 32U. When the wafer mounting table 10 is in use, the coolant flows from the upstream side of the coolant flow passage 32 to the downstream side while removing heat from the high-temperature wafer W, so that the temperature of the coolant flowing through the coolant flow passage 32 is higher on the downstream side than on the upstream side. On the other hand, in the wafer mounting table 10, the area ratio of the small protrusions 22c in the flow passage overlap range R10 is the lowest in the small region A1 facing the most upstream portion 32U, so that the thermal resistance from the coolant flow passage 32 to the wafer mounting surface 22a is lower in the areas other than the small region A1 (small regions A2 to An) than in the small region A1. This is for the following reason. The small protrusions 22c are ceramic, and ceramic has better thermal conductivity than voids. Therefore, in the portion where the area ratio of the small protrusions 22c is high, the proportion of ceramic in the planar direction is high compared to the portion where the area ratio of the small protrusions 22c is not high, and heat exchange between the wafer W and the refrigerant is promoted, and heat removal is promoted. Therefore, overall, the temperature difference can be reduced within the flow passage overlap range R10 of the wafer mounting surface 22a. Therefore, the temperature uniformity of the wafer W is improved.

[0045] Furthermore, in the wafer mounting table 10, the area ratio of the small protrusions 22c in the flow passage overlapping range R10 gradually increases from the small area A1 toward the downstream of the coolant flow passage 32. Therefore, the temperature uniformity of the wafer W is improved.

[0046] Furthermore, when the flow passage overlapping range R10 is viewed from above, the wafer mounting table 10 is The coolant flow path 32 is The area ratio of the small protrusions 22c in the portion facing the most downstream portion 32L in the range overlapping with Most upstream section 32U In the part facing small protrusion 22c Therefore, the temperature uniformity of the wafer W is further improved.

[0047] Furthermore, in the wafer mounting table 10, the adjacent region Qi adjacent to the small region Ai and outside the flow path overlapping range R10 has a higher area ratio of the small protrusions 22c than the small region Ai in the flow path overlapping range R10. Generally, heat is less easily removed from the adjacent region Qi than from the small region Ai in the flow path overlapping range R10. This is because there is no refrigerant flow path 32 directly below. On the other hand, the adjacent region Qi has a higher area ratio of the small protrusions 22c than from the small region Ai in the flow path overlapping range R10. This promotes heat removal from the adjacent region Qi. This improves the thermal uniformity of the wafer W.

[0048] The wafer mounting table 10 has a terminal hole 51 that penetrates the cooling substrate 30 in the vertical direction, and the cross-sectional area of ​​the coolant flow path 32 is smaller in the peripheral region of the terminal hole 51 than in the region outside the peripheral region of the terminal hole 51, and the area ratio of the small protrusions 22c is higher in the direct-above region R30 than in the peripheral region R40 outside the direct-above region R30 of the wafer mounting surface 22a. In general, the direct-above region R30 of the terminal hole 51 of the wafer W is prone to become a hot spot. However, the direct-above region R30 has a higher area ratio of the small protrusions 22c than the peripheral region R40. Therefore, heat removal from the direct-above region R30 is promoted. Therefore, the thermal uniformity of the wafer W is improved.

[0049] In addition, in the wafer mounting table 10, the cooling substrate 30 is made of a metal matrix composite material, and the ceramic substrate 20 and the cooling substrate 30 are bonded with a metal bonding layer 40. In a structure in which the cooling substrate 30 is made of a metal matrix composite material and the bonding layer is a metal bonding layer 40, the thermal resistance from the coolant flow path 32 to the wafer mounting surface 22a is small, so the wafer temperature is easily affected by the temperature gradient of the coolant. Therefore, it is highly meaningful to apply the present invention. In addition, the metal bonding layer 40 has a high thermal conductivity and is therefore suitable for heat extraction. Furthermore, since the thermal expansion difference between the ceramic substrate 20 and the cooling substrate 30 made of a metal matrix composite material can be reduced, even if the stress relaxation property of the metal bonding layer 40 is low, no problems are likely to occur.

[0050] Furthermore, the coolant flow paths 32 are formed in a zigzag shape when the cooling substrate 30 is viewed from above. This makes it easier to route the coolant flow paths 32 over the entire cooling substrate 30.

[0051] It goes without saying that the present invention is not limited to the above-described embodiment, and can be embodied in various forms within the technical scope of the present invention.

[0052] For example, in the above embodiment, in the flow passage overlap range R10, the area ratio of the small protrusions 22c in the small area A1, which is the portion facing the most upstream portion 32U, is set to be the lowest, but this is not limited to this. For example, as shown in FIG. 7, if the distance h1 from the top surface of the small protrusions 22c in the small area A1 to the reference surface 22d is smaller than the area ratio of the small protrusions 22c in the other small areas Ak (k is an integer between 2 and n), Top surface of The distance from the top surface of the small protrusion 22c to the reference surface 22d may be longer than the distance hk from the small region A1 to the reference surface 22d. In this case, the distance from the top surface of the small protrusion 22c to the reference surface 22d may be gradually shorter from the small region A1 to the downstream of the refrigerant flow path 32. Specifically, when the relationship between the position of the flow path overlap range R10 and the distance from the top surface of the small protrusion 22c to the reference surface 22d is represented in a graph, Top surface of The distance from the small protrusion 22c to the reference surface 22d may be continuously shorter from the small region A1 to the small region An, or may be stepped. However, it is preferable that the distance is continuously shorter. For example, the distance from the small protrusion 22c to the reference surface 22d may be continuously shorter from the small region A1 to the small region An. Top surface of The distance from the small protrusion 22c to the reference surface 22d may decrease continuously at a constant gradient, or may decrease in a downward convex curve, or may decrease in an upward convex curve. Top surface of The distance from the small protrusion 22c in the small area A1 facing the most upstream portion 32U to the reference surface 22d is Top surface of It is preferable that the distance be 80% or less of the distance from the reference surface 22d to the reference surface 22d.

[0053] In the above-described embodiment, the area ratio of the small protrusions 22c is changed by changing the arrangement density of the small protrusions 22c, but this is not limiting. For example, as shown in Fig. 8, the area ratio of the small protrusions 22c may be changed by changing the area of ​​the top surface of the small protrusions 22c. Also, the area ratio of the small protrusions 22c may be changed by changing both the area of ​​the top surface of the small protrusions 22c and the arrangement density of the small protrusions 22c. In Fig. 8, the same components as those in Fig. 2 are denoted by the same reference numerals, and the description thereof is omitted.

[0054] In the above embodiment, the adjacent region Qi has a higher area ratio of the small protrusions 22c than the small region Ai, but this is not limited to the above. For example, the distance from the top surface of the small protrusions 22c to the reference surface 22d may be shorter in the adjacent region Qi than in the small region Ai of the flow path overlap range R10.

[0055] In the above embodiment, the area ratio of the small protrusions 22c is higher in the direct-above region R30 than in the peripheral region R40, but this is not limited thereto. For example, the distance from the top surface of the small protrusions 22c to the reference surface 22d may be shorter in the direct-above region R30 than in the peripheral region R40. In this case, it is preferable that the distance from the top surface of the small protrusions 22c to the reference surface 22d in the direct-above region R30 is shorter by a distance L than the distance from the top surface of the small protrusions 22c to the reference surface 22d in the peripheral region R40. The distance L is about 25% of the distance from the top surface of the small protrusions 22c to the reference surface 22d in the peripheral region R40.

[0056] In the above-described embodiment, in the flow passage overlap range R10, the small region A1 facing the most upstream portion 32U may have the smallest area ratio of the small protrusions 22c, and the distance from the top surface of the small protrusions 22c to the reference surface 22d may be the longest. Also, the area ratio of the small protrusions 22c increases as one moves downstream of the refrigerant flow passage 32 from the small region A1 (from the small region A1 to the small region An). Top surface ofThe distance from the small protrusions 22c to the reference surface 22d may be gradually shortened. In this case, the area ratio of the small protrusions 22c in the small region An facing the most downstream portion 32L may be 150% or more of the area ratio of the small protrusions 22c in the small region A1 facing the most upstream portion 32U, and the distance from the top surface of the small protrusions 22c in the small region An to the reference surface 22d may be 80% or less of the distance from the top surface of the small protrusions 22c in the small region A1 to the reference surface 22d. Furthermore, in the above-mentioned embodiment, the area ratio of the small protrusions 22c is higher in the adjacent region Qi than in the small region Ai, and the small protrusions 22c Top surface of In the above embodiment, the area ratio of the small protrusions 22c is higher in the immediate-above region R30 than in the peripheral region R40. Top surface of The distance from the reference surface 22d to the reference surface 22d may be short.

[0057] In the above-described embodiment, instead of the coolant flow passage 32 having a zigzag shape in plan view, a coolant flow passage 82 having a spiral shape in plan view may be used as shown in Fig. 9. The coolant flow passage 82 is formed in a spiral shape from the inlet 82a to the outlet 82b in a single stroke over the entire portion of the cooling substrate 30 except for the flange portion 34. In this case, when the most upstream portion 82U and the most downstream portion 82L are defined in the region of the coolant flow passage 82 that overlaps with the wafer placement surface 22a in plan view, the most upstream portion 82U and the most downstream portion 82L are positioned as shown in Fig. 9. Note that the outer periphery of the coolant flow passage 82 may be the inlet, and the center portion may be the outlet.

[0058] In the above-described embodiment, the cooling substrate 30 is made of MMC, but is not limited to this. The cooling substrate 30 may be made of a metal (for example, aluminum, titanium, molybdenum, tungsten, and alloys thereof).

[0059] In the above-described embodiment, the ceramic base 20 and the cooling base 30 are joined via the metal joining layer 40, but this is not particularly limited. For example, instead of the metal joining layer 40, a resin joining layer may be used.

[0060] In the above-described embodiment, the wafer attracting electrode 26 is built into the central portion 22 of the ceramic base material 20, but instead of or in addition to this, an RF electrode for generating plasma or a heater electrode (resistance heating element) may be built in. Also, a focus ring (FR) attracting electrode, an RF electrode, or a heater electrode may be built in the outer circumferential portion 24 of the ceramic base material 20.

[0061] In the above-described embodiment, the wafer mounting table 10 may have a plurality of holes penetrating the wafer mounting table 10 in the vertical direction. Such holes include a plurality of gas holes opening in the wafer mounting surface 22a and lift pin holes for inserting lift pins for moving the wafer W up and down relative to the wafer mounting surface 22a. A plurality of gas holes are provided at appropriate positions when the wafer mounting surface 22a is viewed from above. A thermally conductive gas such as He gas is supplied to the gas holes. Usually, the gas holes are provided so as to open at positions on the wafer mounting surface 22a on which the seal band 22b and the small protrusions 22c are provided, where the seal band 22b and the small protrusions 22c are not provided. When the thermally conductive gas is supplied to the gas holes, the thermally conductive gas fills the space on the back side of the wafer W mounted on the wafer mounting surface 22a. A plurality of lift pin holes are provided at equal intervals along the concentric circles of the wafer mounting surface 22a when the wafer mounting surface 22a is viewed from above. When the wafer mounting table 10 has gas holes or lift pin holes, as shown in FIG. R30 The area ratio of the small protrusions 22c may be higher in the directly above region R30 than in the peripheral region R40 outside the directly above region R30 of the hole. Alternatively, the distance from the top surface of the small protrusions 22c to the reference surface 22d may be shorter in the directly above region R30 than in the peripheral region R40 outside the directly above region R30 of the hole. Also, the area ratio of the small protrusions 22c may be higher in the directly above region R30 than in the peripheral region R40 outside the directly above region R30 of the hole, and the distance from the top surface of the small protrusions 22c to the reference surface 22d may be shorter. In this way, the thermal uniformity of the wafer W is further improved.

[0062] In the above-described embodiment, the ceramic sintered body 120 in FIG. 6A was produced by hot-press sintering a ceramic powder compact. However, the compact may be produced by stacking a plurality of tape compacts, by a mold casting method, or by compressing ceramic powder.

[0063] In the above-described embodiment, the flow path overlapping range R10 is divided into n small regions A1 to An having the same area, where n is preferably 5 or more.

[0064] In the above-described embodiment, the flow path overlapping range R10 is divided into a plurality of parts along the way, but is not limited to this. For example, the flow path overlapping range R10 does not have to be divided along the way.

[0065] In the above-described embodiment, the small region Ak may be composed of one continuous region as shown in Fig. 10, or may be composed of two or more separated regions (for example, small region A2, small region A4, etc.). Note that in Fig. 10, the small protrusion 22c is omitted, and the same components as those in Fig. 2 are denoted by the same reference numerals and their explanations are omitted. [Explanation of symbols]

[0066] 10 wafer mounting table, 20 ceramic substrate, 22 center portion, 22a wafer mounting surface, 22b seal band, 22c small protrusion, 22d reference surface, 24 outer periphery, 24a focus ring mounting surface, 26 wafer suction electrode, 30 cooling substrate, 32 coolant flow path, 32L most downstream portion, 32U most upstream portion, 32a inlet, 32b outlet, 32c straight portion, 32d folded portion, 34 flange portion, 36 coolant supply path, 38 coolant discharge path, 40 metal bonding layer, 42 insulating film, 51 terminal hole, 52 wafer suction DC power source, 53 low pass filter, 54 power supply terminal, 55 insulating tube, 62 RF power source, 63 high pass filter, 64 power supply terminal, 70 clamp member, 70a inner peripheral step surface, 72 bolt, 78 focus ring, 82 Coolant flow path, 82L downstream portion, 82U upstream portion, 82a inlet, 82b outlet, 94 chamber, 96 mounting plate, 98 shower head, 110 bonded body, 120 ceramic sintered body, 130 MMC block, 131 MMC disk member, 132 groove, 133 through hole, 134 through hole, 135 metal bonding layer, 136 MMC disk member, 151a upper terminal hole, 151b middle terminal hole, 151c lower terminal hole, W wafer.

Claims

1. a ceramic substrate having an electrode built therein and a wafer mounting surface on an upper surface of the ceramic substrate; A cooling substrate having a refrigerant flow path; a bonding layer that bonds the ceramic substrate and the cooling substrate; a plurality of small protrusions on a reference surface of the wafer mounting surface, the small protrusions supporting the lower surface of the wafer with their top surfaces; A wafer mounting table comprising: The top surfaces of the small projections are coplanar; In a flow path overlap range of the wafer mounting surface that overlaps with the refrigerant flow path in a planar view, the area ratio of the small protrusions is lowest in a portion that faces the most upstream portion of the range that overlaps with the wafer mounting surface when the refrigerant flow path is viewed in a planar view.

2. an area ratio of the small protrusions in the flow passage overlapping range gradually increases from a portion facing the most upstream portion toward the downstream of the refrigerant flow passage; The wafer stage according to claim 1 .

3. In the flow path overlapping range, an area ratio of the small protrusions in a portion facing the most downstream portion in the range overlapping with the wafer placement surface when the refrigerant flow path is viewed in a plan view is 150% or more of an area ratio of the small protrusions in a portion facing the most upstream portion. The wafer stage according to claim 1 .

4. an area ratio of the small protrusions is higher in an adjacent area outside the flow path overlapping range and adjacent to the predetermined area, compared to an area ratio of the small protrusions in the flow path overlapping range; The wafer stage according to any one of claims 1 to 3.

5. The wafer mounting table according to any one of claims 1 to 4, A hole penetrating the cooling substrate in the vertical direction Equipped with The cross-sectional area of ​​the coolant flow path is smaller in a peripheral region of the hole than in a region outside the peripheral region of the hole, The wafer mounting table has a higher area ratio of the small protrusions in the area directly above the hole than in a peripheral area outside the area directly above the hole on the wafer mounting surface.

6. a ceramic substrate having an electrode built therein and a wafer mounting surface on an upper surface of the ceramic substrate; A cooling substrate having a refrigerant flow path; a bonding layer that bonds the ceramic substrate and the cooling substrate; a plurality of small protrusions on a reference surface of the wafer mounting surface, the small protrusions supporting the lower surface of the wafer with their top surfaces; A wafer mounting table comprising: The top surfaces of the small projections are coplanar; In the flow path overlap range of the wafer mounting surface that overlaps with the refrigerant flow path in a planar view, the distance from the top surface of the small protrusion to the reference surface is longest in the portion that faces the most upstream portion of the range that overlaps with the wafer mounting surface when the refrigerant flow path is viewed in a planar view (excluding those in which all the distances from the top surfaces of the small protrusions to the reference surface are the same).

7. a distance from a top surface of the small protrusion to the reference surface in the flow passage overlapping range gradually decreases from a portion facing the most upstream portion toward the downstream of the refrigerant flow passage; The wafer stage according to claim 6 .

8. In the flow path overlapping range, a distance from a top surface of the small protrusion to the reference surface in a portion facing the most downstream portion in a range overlapping with the wafer placement surface when the refrigerant flow path is viewed in a plan view is 80% or less of a distance from a top surface of the small protrusion to the reference surface in a portion facing the most upstream portion. The wafer stage according to claim 6 or 7.

9. a distance from a top surface of the small protrusion to the reference surface is shorter in an adjacent area that is adjacent to the predetermined area and outside the flow path overlapping area than in a predetermined area of ​​the flow path overlapping area; The wafer mounting table according to any one of claims 6 to 8.

10. The wafer mounting table according to any one of claims 6 to 9, A hole penetrating the cooling substrate in the vertical direction Equipped with The cross-sectional area of ​​the coolant flow path is smaller in a peripheral region of the hole than in a region outside the peripheral region of the hole, a distance from a top surface of the small protrusion to the reference surface is shorter in a region directly above the hole than in a peripheral region outside the region directly above the hole on the wafer mounting surface; Wafer placement stage.

11. the cooling substrate is made of a metal matrix composite material; The bonding layer is a metal bonding layer. The wafer mounting table according to any one of claims 1 to 10.

Citation Information

Patent Citations

  • Measuring method of biological activity and its device

    JP1981066748A

  • Measuring method of activity of animal*botanical tissue

    JP1981066749A

  • Electrostatic chuck device

    JP1995018438A

  • Full-area temperature control electrostatic chuck and its manufacturing method

    JP2002110774A

  • Electrostatic chuck

    JP2005191561A