Reactor manufacturing method

The frame body with vertical sides addresses the challenge of burr formation and enhances heat dissipation by closely contacting the coil's surfaces, ensuring resin does not intrude, thus maintaining coil integrity and insulation.

JP7577173B2Active Publication Date: 2024-11-01TAMURA KK
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
JP2023135089
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2023-08-22
Publication Date
2024-11-01
Estimated Expiration
2039-09-06

AI Technical Summary

Technical Problem

Existing methods for manufacturing resin-coated reactors face challenges in exposing both flat and curved surfaces of coils without causing burrs, as the coil's irregularities lead to gaps and unevenness, risking resin intrusion and coil damage.

Method used

A frame body with vertical sides is used to sandwich and closely contact the coil's flat and curved surfaces, ensuring the mold resin does not enter the gaps, while maintaining insulation and heat dissipation by exposing the coil's surfaces.

Benefits of technology

The method effectively suppresses burr formation and enhances heat dissipation by ensuring the mold resin does not enter the coil's curved surfaces, while maintaining coil integrity and insulation properties.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007577173000001
    Figure 0007577173000001
  • Figure 0007577173000002
    Figure 0007577173000002
  • Figure 0007577173000003
    Figure 0007577173000003
Patent Text Reader

Abstract

To suppress generation of burrs of a mold resin on a surface of a coil in a reactor in which a part of surface of the coil is exposed from the mold resin.SOLUTION: With respect to a coil 5 in which four flat faces and four curved faces are alternately arranged, an upper frame body 6 is disposed on one of the flat faces. A lower frame body 7 including a pair of longitudinal side parts 71 along a cylinder axis of the coil 5 is disposed on the opposite flat face. Therein, the pair of longitudinal side parts 71 is disposed so as to interpose the flat face therebetween, and the flat face is exposed over an entire lateral width range from one to the other lower curved faces 53 to which the pair of longitudinal side parts 71 is configured to adhere. The coil 5 is pressed with a metal mold via the upper frame body 6 and the lower frame body 7. Therein, the upper frame body 6 is pressed with an upper mold, so as to cause the pair of longitudinal side parts 71 to adhere to the two lower curved faces 53. Then, while the pressing with the metal mold is being performed, the coil 5 is molded with a resin except inside a frame of the lower frame body 7 and inside a frame of the upper frame body 6.SELECTED DRAWING: Figure 6
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method for manufacturing a reactor having a coil molded with resin. [Background technology]

[0002] Reactors are used in various applications, including drive systems for hybrid vehicles, electric vehicles, and fuel cell vehicles. For example, reactors are used in in-vehicle boost circuits. Resin-molded reactors, in which the periphery of the core and coil is covered with resin, are widely used. In this type of reactor, a part of the coil surface may be exposed without being covered with molded resin in order to ensure heat dissipation. In order to expose the coil surface, a proposal has been made to fill the surrounding area with molded resin while a mold is pressed against the coil surface (see Patent Documents 1 to 3). [Prior art documents] [Patent documents]

[0003] [Patent Document 1] Patent No. 5869518 [Patent Document 2] JP 2015-130410 A [Patent Document 3] JP 2018-011019 A Summary of the Invention [Problem to be solved by the invention]

[0004] The coil is made into a cylindrical shape by winding a conductive wire in a spiral shape while shifting the winding position for each turn along the winding axis, and has an outer shape in which four flat surfaces and four curved surfaces are arranged alternately. For reasons of manufacturing precision, the surface of the coil has irregularities and is not necessarily smooth. Therefore, even if the coil is to be closely attached to the mold, a gap will occur between the mold and the surface of the coil. If this happens, resin may seep in through this gap and cause burrs to form on the surface that is to be exposed.

[0005] In order to improve heat dissipation, it is useful to expose not only the flat surfaces of the coil but also the curved surfaces, but because the curved surfaces of the coil must maintain a constant curvature within one turn and the curvature must be the same for all turns, unevenness is particularly likely to occur and the unevenness tends to become large, making it difficult to expose the curved surfaces from the mold resin.

[0006] One way to prevent burrs from occurring is to press the die firmly against the coil surface. By pressing the die firmly against the coil surface, it is possible to eliminate the gap between the die and the coil surface and to straighten out any twists in the coil surface using the die.

[0007] However, if the die is pressed strongly against the surface of the coil, problems occur such as damaging the coil or damaging the coating of the coil's conductive wire, impairing its insulation, etc. Thus, in a resin-molded type reactor in which the coil is coated with molding resin except for a portion of the coil's surface, there is a demand for preventing the occurrence of burrs without damaging the coil, but the above-mentioned conventional technology cannot meet such demands.

[0008] The present invention has been proposed to solve the problems of the conventional technology as described above. An object of the present invention is to provide a manufacturing method for a reactor in which a part of the coil surface is exposed from the molding resin, which suppresses the generation of burrs in the molding resin on the coil surface. [Means for solving the problem]

[0009] The reactor of the present invention comprises a core made of a magnetic material, a cylindrical coil attached to the core and having an outer shape in which four flat surfaces and four curved surfaces are arranged alternately, a frame body placed on the surface of the coil, and molded resin covering the coil except for the inside of the frame body, wherein the frame body has a pair of vertical side portions along the cylindrical axis of the coil, the pair of vertical side portions sandwich one of the flat surfaces and are in close contact with two of the curved surfaces adjacent to the flat surfaces, and the flat surfaces sandwiched between the pair of vertical side portions are exposed from the molded resin over the entire width range from one of the curved surfaces where the pair of vertical side portions are in close contact to the other of the curved surfaces.

[0010] The flat surface sandwiched between the pair of vertical side portions is a first flat surface, and the flat surface perpendicular to the first flat surface is a second flat surface, and the vertical side portions of the frame body have a contact surface that is in close contact with the curved surface of the coil, an end surface on the second flat surface side that is adjacent to the contact surface, extends along the cylindrical axis of the coil and expands in a direction away from the contact surface, and an outer surface that is adjacent to the end surface and is the opposite side of the contact surface, and the end surface has a length that is covered with the molded resin and has a length that reaches or exceeds the surface of the molded resin, and the outer surface is not covered by the molded resin.

[0011] The end face may have a length that reaches a surface of the molding resin, and the outer surface may be flush with the surface of the molding resin.

[0012] The angle formed between the contact surface and the end surface may be approximately a right angle, and the angle formed between the end surface and the outer surface may be approximately a right angle. Effect of the Invention

[0013] According to the present invention, even if the exposed area of ​​the coil is expanded to include a curved surface where burrs are likely to occur when the coil is directly pressed with a mold, the occurrence of burrs can be suppressed and heat dissipation is also excellent. [Brief description of the drawings]

[0014] [Figure 1] FIG. 2 is a perspective view of the reactor in the embodiment, in which members covering each portion are omitted. [Diagram 2] FIG. 2 is a perspective view showing a core coating resin that coats the core. [Diagram 3] FIG. [Figure 4] FIG. [Diagram 5] FIG. 2 is a top perspective view of the reactor, omitting the molding resin that covers the reactor body. [Figure 6] FIG. 2 is a bottom perspective view of the reactor, omitting the molding resin that covers the reactor body. [Figure 7] A cross-sectional view of the vertical side portion of the lower frame body. [Figure 8] FIG. 2 is an enlarged perspective view of an end face and a horizontal side portion of the coil, with the molding resin that covers the reactor body omitted. [Figure 9] 5A to 5C are schematic diagrams showing a process of forming a molding resin that covers a reactor body. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0015] (composition) Hereinafter, a reactor according to an embodiment of the present invention will be described with reference to the drawings. FIG. 1 is a perspective view of the reactor of this embodiment, and for convenience of explanation, the members covering each part are omitted. The reactor 100 is incorporated in the drive systems of hybrid cars, electric cars, and fuel cell cars, for example, and used in boost circuits. The reactor 100 includes a reactor body 10. The reactor body 10 is an electromagnetic component that converts electric energy into magnetic energy and stores and releases it, and includes two coils 5, 5 and a core 1.

[0016] The core 1 is made of a magnetic material such as a powder magnetic core, a ferrite magnetic core, or a laminated steel plate, and has a ring shape. The coil 5 is a cylindrically wound body made of a conductive wire such as a copper wire, and is formed by winding the conductive wire in a spiral shape while shifting the winding position for each turn along the winding axis. The two coils 5, 5 are insulated from the core 1 and fitted side-by-side into one core 1. In this reactor 100, when a current is conducted through the coil 5, the core 1 becomes a passage for the magnetic flux generated by the coil 5, forming a closed magnetic circuit.

[0017] The coil 5 has an outer shape in which four curved surfaces and four flat surfaces parallel to the cylindrical axis are alternately connected. That is, the coil 5 has an upper surface 51 which is a flat surface parallel to the surface on which the annular shape of the core 1 appears, and a flat lower surface 52 opposite to the upper surface 51. The coil 5 has a side surface 54 which is a flat surface perpendicular to the upper surface 51 and the lower surface 52. The coil 5 has a lower curved surface 53 between the lower surface 52 and the side surface 54. The coil 5 has annular end surfaces 55 which are located at the start and end of the winding, through which the core 1 passes and which are perpendicular to the cylindrical axis.

[0018] The flat surface of the coil 5 is a surface that is flat in comparison with a curved surface, and also includes a surface that forms a large arc with a gentle curvature due to the swelling of the conductive wire. The top and bottom refer to the upper and lower molds that house the reactor body 10 when covering the reactor body 10 by molding, and do not refer to the positional relationship or direction when the reactor 100 is mounted on the actual device to be installed.

[0019] As shown in Figs. 2 to 4, each part of such a reactor 100 is coated with a core coating resin 2 and a molded resin 4. The core coating resin 2 and the molded resin 4 are molded articles that maintain a certain shape and have insulating properties and heat resistance. For example, the core coating resin 2 and the molded resin 4 are made of epoxy resin, unsaturated polyester resin, urethane resin, BMC (Bulk Molding Compound), PPS (Polyphenylene Sulfide), PBT (Polybutylene Terephthalate), or a combination of these materials. The core coating resin 2 and the molded resin 4 may be made of the same type of material or different materials. A thermally conductive filler may be mixed into the core coating resin 2 and the molded resin 4.

[0020] Fig. 2 is a perspective view showing the core coating resin 2. As shown in Fig. 2, the reactor body 10 includes the core 1, the coils 5, 5, and the core coating resin 2. The core coating resin 2 coats the core 1. The coils 5, 5 are fitted into the core 1 from above the core coating resin 2, and the coils 5, 5 and the core 1 are insulated by the core coating resin 2.

[0021] Fig. 3 is a top perspective view showing the molded resin 4, and Fig. 4 is a bottom perspective view showing the molded resin 4. As shown in Fig. 3 and Fig. 4, the reactor 100 includes the molded resin 4, and the molded resin 4 covers the reactor body 10 including the coils 5, 5. This molded resin 4 is formed so as to cover the reactor body 10 by placing the reactor body 10 in a mold and injecting the resin into the mold and solidifying it.

[0022] 3, the reactor 100 is provided with a sensor unit 3. The sensor unit 3 is, for example, a thermistor that detects temperature. The molded resin 4 is provided with terminals 44 for connecting the coils 5, 5 to an electric circuit, and has fastening holes 45 for fixing the reactor 100 to an installation target.

[0023] 3 and 4, the coils 5, 5 are not entirely covered by the molded resin 4, but rather have a portion of their surface exposed from the molded resin 4. An opening 56 that is not covered by the molded resin 4 is formed in an upper surface 51 of each of the coils 5, 5, and an opening 57 that is not covered by the molded resin 4 is formed in a lower surface 52 of each of the coils 5, 5.

[0024] In detail, the reactor 100 has an upper frame 6 and a lower frame 7, each of which is open to the inside, disposed on the surface of the coils 5, 5. One upper frame 6 is disposed on the upper surface 51 of each coil 5, 5. One lower frame 7 is disposed on each coil 5, 5 so that the entire width range of the lower surface 52 of each coil 5, 5 is included within the frame. The width of the lower surface 52 refers to the direction perpendicular to the cylindrical axis of the coil 5. The molded resin 4 fills the outer periphery of the upper frame 6 and the lower frame 7 without any gaps, but does not enter the frame of the upper frame 6 and the lower frame 7, and covers the reactor main body 10.

[0025] With the upper frame 6 and lower frame 7 blocking the molded resin 4, each coil 5, 5 has an opening 56 on the upper surface 51 side and an opening 57 on the lower surface 52 side. The opening 56 on the upper surface 51 side is contained within the upper surface 51. The opening 57 on the lower surface 52 side exposes the lower surface 52 over the entire width range from one lower curved surface 53 to the other lower curved portion 53. Furthermore, the opening 57 on the lower surface 52 side exposes not only the lower surface 52 but also a part of the lower curved portion 53 from the molded resin 4 in the width direction perpendicular to the cylindrical axis of the coil 5.

[0026] The upper frame 6 and the lower frame 7 are molded products that retain a fixed shape, and have heat resistance and insulating properties that make them resistant to softening when exposed to heat during the molding process that forms the molded resin 4. For example, the upper frame 6 and the lower frame 7 may be made of PPS (Polyphenylene Sulfide), epoxy resin, unsaturated polyester resin, urethane resin, BMC (Bulk Molding Compound), PPS (Polyphenylene Sulfide), PBT (Polybutylene Terephthalate), or a combination of these. The upper frame 6 and the lower frame 7 may be made of the same type of material, or may be made of different materials. A thermally conductive filler may be mixed into the material of the upper frame 6 and the lower frame 7.

[0027] Fig. 5 is a top perspective view of reactor 100, omitting molded resin 4. As shown in Fig. 5, upper frame 6 is a plate whose outer and inner circumferential shapes are elliptical, and is large enough to fit on upper surface 51 of coil 5. A long, thin, plate-like tongue portion 61 having a circular hole 62 is extended from upper frame 6. Upper frame 6 has two tongue portions 61. Tongue portions 61 are provided at diagonal corners of upper frame 6, and extend parallel to the elliptical plate.

[0028] A pin 21 that serves as a positioning portion for the upper frame 6 is provided in the core coating resin 2 that coats the core 1. The upper frame 6 is positioned by fitting the pin 21 into a circular hole 62 in a tongue portion 61, and is placed on the upper surface 51 of the coil 5. The molded resin 4 fills the outer peripheral side surface of the upper frame 6 without any gaps, and further covers the outer peripheral edge of the upper frame 6 except for the inside of the frame and the inner peripheral edge of the upper frame 6, covering the core 5 (see FIG. 3).

[0029] 6 is a bottom perspective view of reactor 100, omitting molded resin 4. As shown in FIG. 6, lower frame 7 has a generally rectangular shape. One side of lower frame 7 is the same as the axial length of coil 5, and the other side perpendicular to the one side completely crosses lower surface 52 and reaches both lower curved surfaces 53. Here, the direction along the axis of coil 5 is called vertical, and the direction perpendicular to the axis of coil 5 is called horizontal, but these do not refer to the positional relationship or direction when reactor 100 is mounted on an actual device to be installed.

[0030] Each lower frame 7 has a pair of vertical side portions 71 extending along the axial direction of the coil 5, and a pair of horizontal side portions 72 extending perpendicular to the axis of the coil 5. The vertical side portions 71 extend across the lower surface 52, which is an exposed flat surface exposed from the molded resin 4. The vertical side portions 71 have the same length as the axial length of the coil 5. The vertical side portions 71 are in close contact with the lower curved surface 53 of the coil 5. The horizontal side portions 72 run along the end surface 55 of the coil 5 and completely cross the end surface 55.

[0031] FIG. 7 is a cross-sectional view of the vertical side portion 71 including the coil 5 and the molded resin 4. As shown in FIG. 7, the vertical side portion 71 has a curved portion 73 and a vertical portion 74. The curved portion 73 is in close contact with the lower curved surface 53. The vertical portion 74 extends from the lower end of the curved portion 73 and extends perpendicular to the plane in which the lower surface 52 of the coil 5 extends. The curved portion 73 and the vertical portion 74 are seamlessly connected. The curved portion 73 is defined by a contact surface 731, an upper end surface 732, and an outer surface 733, except for the connection area with the vertical portion 74 and the connection area with the horizontal side portion 72. When going around the vertical side portion 71, there is the contact surface 731, the contact surface 731 followed by the upper end surface 732, the upper end surface 732 followed by the outer surface 733, the outer surface 733 followed by the vertical portion 74, and the vertical portion 74 followed by the contact surface 731.

[0032] The contact surface 731 is the inner peripheral surface of the lower frame 7. The contact surface 731 is curved to coincide with a partial arc range of the lower curved surface 53 of the coil 5. The upper end surface 732 is an upper end surface adjacent to the contact surface 731. The upper end surface 732 is adjacent to the contact surface 731 and is located on the side surface 54 side, which is an orthogonal flat surface perpendicular to the lower surface 52, extends along the cylindrical axis of the coil 5, and expands in a direction away from the lower curved surface 53. The outer surface 733 is adjacent to the upper end surface 732 and constitutes the outer peripheral surface of the lower frame 7. The outer surface 733 is the opposite surface to the contact surface 731.

[0033] The contact surface 731 contacts the lower curved surface 53. The upper end surface 732 is completely covered by the molded resin 4. The outer surface 733 is exposed and not covered by the molded resin 4. That is, the width d1 of the upper end surface 732 is equal to the thickness d2 of the molded resin 4 and reaches the surface of the molded resin 4. The outer surface 733 is connected to the molded resin 4 without any steps and is flush with the molded resin 4. The width of the upper end surface 732 is the length in the direction away from the lower curved surface 53. The thickness of the molded resin 4 compared to the upper end surface 732 is the connection part with the curved portion 73, and other thicknesses are not limited to this.

[0034] The angle between the contact surface 731 and the upper end surface 732 is approximately a right angle, and the angle between the upper end surface 732 and the outer surface 733 is also approximately a right angle. These approximately right angles are angles at which an external force acting on the boundary between the upper end surface 732 and the outer surface 733 is efficiently transmitted to the boundary between the contact surface 731 and the upper end surface 732. In other words, the approximately right angle means a predetermined angle range including 90 degrees as long as the contact surface 731 is corrected along the lower curved surface 53 and the separation of the contact surface 731 and the lower curved surface 53 due to the injection pressure of the molding resin 4 can be prevented, as will be described later.

[0035] The vertical portion 74 extends perpendicular to the plane in which the lower surface 52 of the coil 5 extends. The vertical portion 74 protrudes from the lower surface 72 so that the opening 57 has depth. The molding resin 4 is blocked by the upper end surface 732 of the curved portion 73, and does not reach the outer surface 733 of the curved portion 73 or the vertical portion 74.

[0036] Fig. 8 is an enlarged perspective view of end surface 55 of coil 5 and horizontal side portion 72, without molded resin 4. As shown in Fig. 8, horizontal side portion 72 has a wall portion 75 and an edge portion 76. Wall portion 75 extends parallel to end surface 55 of coil 5, and edge portion 76 has an inverted and inside-out L shape. Wall portion 75 and edge portion 76 are seamlessly connected, and edge portion 76 is seamlessly connected to vertical side portion 71 at both ends.

[0037] Wall portion 75 extends along end surface 55 of coil 5. Wall portion 75 may be in close contact with end surface 55 or may be close to end surface 55 with a small gap therebetween. Wall portion 75 has a bow shape surrounded by a roughly arc portion along lower surface 52 of coil 5 and the lower portions of both lower curved surfaces 53, and a chord connecting both ends of the arc. The position of the chord does not reach core coating resin 2 that coats core 1.

[0038] The edge portion 76 has a contact portion 761 that comes into close contact with the coil 5. The contact portion 761 comes into close contact with the entire edge area on the end face 55 side of the lower surface 52 of the coil 5, and with partial edge areas on the end face 55 side of both lower curved surfaces 53. The edge portion 76 also has a vertical portion 762 that extends perpendicular to the plane on which the lower surface 52 of the coil 5 extends.

[0039] The vertical portion 762 protrudes from the lower surface 72 so that the opening 57 has depth, and extends to the same height as the vertical portion 74 of the vertical side portion 71. The horizontal side portion 72 is covered with the molded resin 4 except for the portion that constitutes the inner peripheral surface of the lower frame 7 and the end face of the vertical portion 74.

[0040] (action) FIG. 9 is a schematic diagram showing the process of forming the molded resin 4. As shown in FIG. 9, the lower frame 7 is set in the lower mold K1, and then the reactor body 10 is set in the lower frame 7. The vertical parts 74 and 762 of the vertical side parts 71 and horizontal side parts 72 of the lower frame 7 are higher than the lower surface 52, and the coil 5 is floating with respect to the lower mold K1. The upper frame 6 is set in advance on the reactor body 10. After the reactor body 10 is set on the lower frame 7, the upper mold is placed on the reactor body 10, and the molded resin 4 is injected. The upper mold has a pressing part that is slightly smaller than the upper frame 6, and presses the reactor body 10 toward the lower mold K1 via the upper frame 6.

[0041] The lower die K1 has a support portion K2 of the lower frame 7. The support portion K2 abuts the curved portion 73 of the vertical side portion 71 of the lower frame 7 against the outer surface 733. This support portion K2 extends beyond the boundary between the upper end face 732 and the outer surface 733, and abuts against the outer surface 733 including the boundary between the upper end face 732 and the outer surface 733. On the other hand, when the upper die is brought into close contact with the lower die K1, the surface of the upper frame 6 presses the reactor body 10 toward the lower die K1.

[0042] When the lower frame 7 is set, it is set so that the outer surface 733 abuts against the support portion K2. Next, the reactor body 10 is set and the upper and lower molds K1 are brought into close contact with each other, and the upper mold presses the reactor body toward the lower mold K1 via the pressing body and the upper frame 6. Then, the curved portion 73 sandwiched between the support portion K2 and the coil 5 is crushed toward the coil 5. Therefore, the contact surface 731 and the lower curved surface 53 are in close contact with each other without any gaps.

[0043] When the reactor body 10 is set in the lower frame 7, the wall 75 of the horizontal side 72 of the lower frame 7 determines the positional relationship between the lower frame 7 and the reactor body 10. Therefore, the contact surface 731 is in contact with the lower curved surface 53 over the entire area, and local gaps are also suppressed.

[0044] When the molding resin 4 is injected, it flows into the gap defined by the coil 5 and the support part K2, and reaches the upper end face 732. The angle between the contact surface 731 and the upper end face 732 and the angle between the upper end face 732 and the outer surface 733 are both right angles, and the external force applied by the support part K2 to the outer surface 733 is efficiently transmitted to the contact surface 731, and the contact surface 731 and the lower curved surface 53 are firmly attached to each other. Therefore, the molding resin 4 cannot get into the gap between the contact surface 731 and the lower curved surface 53 even by the injection pressure, and the occurrence of burrs is suppressed.

[0045] Moreover, the upper end face 732 has a length that reaches the surface of the molded resin 4, and the outer surface 733 is flush with the surface of the molded resin 4. In other words, the support part K2, which is a part of the lower mold K1 that molds the molded resin 4, is in contact with the outer surface 733 including the boundary between the upper end face 732 and the outer surface 733. Therefore, a large pressure force is also applied to the boundary between the contact surface 731 and the lower curved surface 53, and at least the inlet between the contact surface 731 and the lower curved surface 53 is tightly closed. Therefore, the molded resin 4 cannot penetrate further between the contact surface 731 and the lower curved surface 53 even by the injection pressure, and the occurrence of burrs is further suppressed.

[0046] In addition, when the angle between the contact surface 731 and the upper end surface 732 is on the obtuse angle side, the force applied by the support part K2 to the boundary between the upper end surface 732 and the outer surface 733 acts more strongly on the boundary between the contact surface 731 and the lower curved surface 53 due to the principle of leverage. However, the injection pressure acting on the boundary between the contact surface 731 and the lower curved surface 53 also becomes large. In addition, when the angle between the contact surface 731 and the upper end surface 732 is on the acute angle side, the force applied by the support part K2 to the boundary between the upper end surface 732 and the outer surface 733 acts weaker because the boundary between the contact surface 731 and the lower curved surface 53 becomes farther away. However, the injection pressure acting on the boundary between the contact surface 731 and the lower curved surface 53 becomes smaller.

[0047] Therefore, it is desirable that the angle between the contact surface 731 and the upper end surface 732 and the angle between the upper end surface 732 and the outer surface 733 are both right angles, as this achieves the most balance, but the angle may be made to be on the obtuse or acute side rather than a strict right angle depending on the injection pressure of the molding resin 4. For example, the upper end surface 732 may be extended so as to be parallel to the upper surface 51 and the lower surface 52.

[0048] Here, the vertical portions 74 and 762 of the vertical side portions 71 and horizontal side portions 72 of the lower frame body 7 are higher than the lower surface 52, and the coil 5 floats relative to the lower mold K1, but the lower frame body 7 is made of PPS resin or the like and has heat resistance that makes it difficult for it to soften when exposed to the heat received during the molding process to form the molded resin 4.

[0049] Therefore, it does not soften during the molding process, and keeps the coil 5 and the lower die K1 apart, and fully fulfills its role as a cushioning material. In addition, since it does not soften during the molding process, the external force from the support part K2 is not dispersed or absorbed, but is transmitted to the contact surface 731, and the contact surface 731 is brought into contact with the upper end surface 732.

[0050] When releasing from the mold, the outer edge region of the upper surface of upper frame 6 is covered with molding resin 4, and upper frame 6 is attached to reactor 100 simply by placing it on upper surface 51 of coil 5.

[0051] (effect) (1) As described above, the reactor 100 includes a lower frame 7 disposed on the surface of the coil 5, and a molded resin 4 covering the coil 5 except for the inside of the lower frame 7. The lower frame 7 has a pair of vertical side portions 71 along the cylindrical axis of the coil 5. The pair of vertical side portions 71 extend across the lower surface 52 and are in close contact with the two lower curved surfaces 53 adjacent to the lower surface 52. The coil 5 is configured such that the lower surface 52 sandwiched between the pair of vertical side portions 71 is exposed from the molded resin 4 over the entire width range from one lower curved surface 53 where the pair of vertical side portions 71 are in close contact to the other lower curved surface 53.

[0052] As a result, even if the exposed area of ​​the coil 5 is expanded to the curved surface where burrs are likely to occur when the coil 5 is directly pressed by a mold, the occurrence of burrs can be suppressed and heat dissipation is excellent.

[0053] (2) Furthermore, the vertical side portion 71 of the lower frame 7 has a contact surface 731, an upper contact surface 732, and an outer surface 733. The contact surface 731 is in contact with the lower curved surface 53 of the coil 5. The upper end surface 732 is adjacent to the contact surface 731, extends along the cylindrical axis of the coil 5, and expands in a direction away from the contact surface 731. The outer surface 733 is adjacent to the upper end surface 732, and is the opposite surface to the contact surface 731. The upper end surface 732 is covered with the molded resin 4 and has a length that reaches or exceeds the surface of the molded resin 4, and the outer surface 733 is not covered with the molded resin 4.

[0054] As a result, the support portion K2 comes into contact with the outer surface 733 including the boundary between the upper end surface 732 and the outer surface 733, and a large pressure force is also applied to the boundary between the contact surface 731 and the lower curved surface 53. Therefore, the inlet between the contact surface 731 and the lower curved surface 53 is tightly closed, and the occurrence of burrs is further suppressed. In this embodiment, the upper end surface 732 has a length that reaches the surface of the molded resin 4, but the support portion K2 comes into contact with the outer surface 733 including the boundary between the upper end surface 732 and the outer surface 733 as long as the length is longer than the length that reaches the surface of the molded resin 4. Therefore, it is sufficient that the upper end surface 732 has a length longer than the length that reaches the surface of the molded resin 4.

[0055] (3) The angle between contact surface 731 and upper end surface 732 is an approximate right angle, and the angle between upper end surface 732 and outer surface 733 is an approximate right angle. The approximate right angle includes an angle inclined toward the acute angle side from 90° and an angle inclined toward the obtuse angle side from 90°. For example, the angle may be an angle at which upper end surface 732 is parallel to lower surface 52.

[0056] As a result, the external force applied by the support portion K2 to the outer surface 733 is efficiently transmitted to the contact surface 731, and the contact surface 731 and the lower curved surface 53 are firmly attached to each other. Therefore, the molding resin 4 cannot get into between the contact surface 731 and the lower curved surface 53 even when subjected to injection pressure, and the occurrence of burrs is suppressed.

[0057] (4) The lower frame 7 is made of PPS resin. PPS resin is an example of a resin that has heat resistance and does not easily soften when exposed to heat during the molding process in which the mold resin 4 is formed.

[0058] As a result, the lower frame 7 does not soften during the molding process, and can fully fulfill its role as a cushioning material, while allowing the contact surface 731 to be closely adhered to the upper end surface 732 without dispersing or absorbing external forces from the support portion K2.

[0059] (5) Furthermore, lower frame 7 is at least as high as lower surface 52 sandwiched between a pair of vertical side portions 71. As a result, when reactor 100 is installed on a cooling member such as a gap filler or a heat dissipation sheet, lower frame 7 serves to position reactor 100, enabling reactor 100 to be cooled efficiently.

[0060] (6) Furthermore, an upper frame 6 is further provided, and the molded resin 4 covers the coil 5 except for the inside of the upper frame 6, and at least a part of the upper surface 51 of the coil 5 is further exposed from the molded resin 4. This improves the heat dissipation area of ​​the reactor 100. It also becomes an opportunity to pressurize the reactor body 10 with the upper mold without damaging the coil 5.

[0061] (7) Upper frame 6 is provided with positioning portions such as tongue portions 61. This makes it possible to easily leave upper frame 6 on reactor 100 side when reactor 100 is released from the mold.

[0062] In the above, this embodiment has been described taking the lower frame 7 installed on the lower mold K1 as an example. However, the same effect can be obtained even if the upper frame 6 has the same configuration as the lower frame 7 and the upper mold is provided with the support portion K2. In addition to the upper frame 6 and the lower frame 7, the same effect can be obtained even if a frame having the same configuration as the lower frame 7 is installed on the side surface 54 of the coil 5.

[0063] That is, a frame body is provided on any one of the surfaces of the lower surface 52, upper surface 51, or side surface 54 of the coil 5, and this frame body has a pair of vertical side portions 71 along the cylindrical axis of the coil 5, and the pair of vertical side portions 71 extend across the flat surface on which the frame body is provided and are in close contact with two curved surfaces adjacent to the flat surface on which the frame body is provided.

[0064] This makes it possible to suppress the generation of burrs and achieve excellent heat dissipation even if the exposed area of ​​the coil 5 is expanded to the curved surface where burrs are likely to occur when the coil 5 is directly pressed with a mold. Furthermore, a frame may be provided on each side, which can provide a corresponding increase in the heat dissipation effect.

[0065] (Other embodiments) The embodiments of the present invention are presented as examples, and are not limited to the above-mentioned embodiments. The above-mentioned embodiments can be implemented in various other forms, and various omissions, substitutions, and modifications can be made without departing from the scope of the invention. The embodiments and their modifications are included in the scope of the present invention. [Explanation of symbols]

[0066] 100 Reactor 10 Reactor body 1 core 2 Core coating resin 21 pin 3 Sensor section 4. Mold Resin 44 terminals 45 Fastening hole 5 Coil 51 Top side 52 Bottom surface 53 Lower curved surface 54 Side 55 End face 56 Aperture 57 Aperture 6 Upper frame 61 Tongue piece 62 Circular hole 7 Lower frame 71 Vertical side 72 Side part 73 Curved Section 731 Contact surface 732 Upper end face 733 Exterior 74 Vertical section 75 Wall 76 Edge 761 Contact area 762 Vertical section K1 lower mold K2 support part

Claims

1. A method for manufacturing a reactor having a coil molded with resin, comprising the steps of: an upper frame arrangement step of arranging an upper frame on one of the flat surfaces of the cylindrical coil having an outer shape in which four flat surfaces and four curved surfaces are alternately arranged; a lower frame arrangement process for arranging a lower frame having a pair of vertical side portions aligned along a cylindrical axis of the coil on the flat surface opposite to the flat surface on which the upper frame is arranged; a pressing step of pressing the coil through the upper frame and the lower frame with a die including a lower die and an upper die; a coil molding process of injecting resin into the die while pressing the die to mold the coil; Including, In the lower frame body arrangement process, the pair of vertical side portions are arranged to sandwich the flat surface, and the flat surface sandwiched between the pair of vertical side portions is exposed over the entire width range from one of the curved surfaces where the pair of vertical side portions are in close contact to the other of the curved surfaces, In the pressing step, the upper frame body is pressed by the upper mold to bring the pair of vertical side portions into close contact with the two curved surfaces adjacent to the flat surface, In the coil molding step, the lower frame body is molded with the resin except for an inside of the frame. A method for manufacturing a reactor, comprising the steps of:

2. The lower frame has a height equal to or greater than the flat surface sandwiched between the pair of vertical side portions; A method for manufacturing a reactor according to claim 1,

3. In the coil molding step, the upper frame body is molded with the resin except for an inside of the frame. A method for manufacturing a reactor according to claim 1,

4. a mounting step of mounting the coil on a core made of a magnetic material; a core molding step of covering the core with a resin; Further comprising: In the core molding step, a positioning portion for positioning the upper frame is formed in the resin covering the core; 4. A method for manufacturing a reactor according to claim 1, wherein

Citation Information

Patent Citations

  • Mixer

    JP1983069518A

  • Reactor

    JP2010272771A

  • Reactor

    JP2011210812A

  • Bobbin, reactor and method of manufacturing reactor

    JP2015130410A

  • Reactor

    JP2016092200A