Method for fabricating a semiconductor structure including a high resistivity layer, and related semiconductor structure - Patents.com
The DLT method addresses RF losses in RF CMOS devices by forming a high resistivity layer with an average resistivity greater than 10000 ohm cm, improving RF performance by replacing initial substrates with more suitable final substrates.
Patent Information
- Application Number
- JP2023101912
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2016-01-15
- Filing Date
- 2023-06-21
- Publication Date
- 2024-11-06
- Estimated Expiration
- 2037-01-12
AI Technical Summary
Residual thickness of initial substrates in RF CMOS devices fabricated from standard bulk substrates creates low resistivity paths, leading to RF losses and reduced performance.
A method involving double layer transfer (DLT) to replace the initial substrate with a final substrate suitable for enhanced RF performance, including forming a high resistivity layer by removing a portion of the initial substrate and attaching a final substrate to vias, ensuring the high resistivity layer has an average electrical resistivity greater than 10000 ohm cm.
The method enhances RF performance by eliminating low resistivity paths, ensuring optimal performance of RF devices through the formation of a high resistivity layer that maintains device integrity and reduces conductive interference.
Smart Images

Figure 0007578762000001 
Figure 0007578762000002 
Figure 0007578762000003
Abstract
Description
[Technical field]
[0001] SUMMARY OF THE DISCLOSURE Embodiments of the present disclosure relate to methods that may be used to fabricate semiconductor structures that include high resistivity layers, as well as semiconductor structures and devices fabricated using such methods. [Background technology]
[0002] The performance of radio frequency (RF) electronic switching devices, such as RF CMOS devices, can depend on the electrical resistivity of the substrate from which they are fabricated. Recently, advanced semiconductor-on-insulator (SeOI) substrates, such as high resistivity silicon-on-insulator (HR-SOI), have been utilized to fabricate RF CMOS devices with enhanced performance. For example, RF devices fabricated from HR-SOI have been demonstrated to have reduced RF losses.
[0003] Double (or dual) layer transfer (DLT) of the active layers of a device can allow for the replacement of an initial substrate with a final substrate that is better suited to provide improved RF performance of the device formed thereon.
[0004] Briefly, a device layer, including, for example, multiple RF CMOS devices, may be fabricated in or on an initial substrate. The device layer may then be attached to a temporary substrate. Once the device layer is attached to the temporary substrate, portions of the initial substrate may be removed and replaced with a final substrate that is more suitable for enhanced RF performance. Once the device layer is attached to the final substrate, the temporary substrate may be removed, completing the DLT process of the device layer. For example, DLT for RF CMOS has been demonstrated utilizing an initial SOI type substrate.
[0005] When utilizing an initial SOI type substrate, the bulk silicon carrier portion of the SOI type substrate is completely removed during DLT processing to eliminate undesirable low resistivity paths that can degrade RF performance. However, for RF CMOS devices fabricated from standard bulk substrates, residual thickness of the initial substrate may remain adjacent to the RF CMOS device as a result of the fabrication process. The remaining residual thickness of the initial substrate may act as a low resistivity path, resulting in RF losses and degradation of the RF performance of the device layer. Summary of the Invention [Problem to be solved by the invention]
[0006] Thus, the present invention provides an improved method for fabricating semiconductor structures that include high resistivity layers, and related semiconductor structures. [Means for solving the problem]
[0007] This Summary is provided to introduce a selection of concepts in a simplified form. These concepts are described in more detail below in the Detailed Description of Exemplary Embodiments of the Disclosure. This Summary is not intended to identify key features or essential features of the claimed subject matter, nor is it intended to be used to limit the scope of the claimed subject matter.
[0008] In some embodiments, the present disclosure includes a method of fabricating a semiconductor structure. A method of forming a semiconductor structure includes: - forming a device layer on an initial substrate; - attaching a first surface of the device layer to a temporary substrate; - forming a high resistivity layer, where forming the high resistivity layer comprises removing a portion of the initial substrate, the high resistivity layer comprising a remaining portion of the initial substrate; - attaching the final substrate (132, 232) to the high resistivity layer (136, 236); - removing the temporary substrate (114, 214); Includes.
[0009] According to further non-limiting features of the invention, the following are incorporated, either alone or in any technically feasible combination:
[0010] the step of removing the portion of the initial substrate comprises thinning the portion of the initial substrate; The step of removing the portion of the initial substrate includes forming a plurality of vias extending through the remaining portion of the initial substrate; forming a plurality of vias through the remaining portion of the initial substrate (102) forming a masking layer on the exposed surface of the remaining portion of the initial substrate; Etching vias through the remaining unmasked portions of the initial substrate; Including, the masking layer includes a plurality of masking elements, the method including the step of selecting a total surface area of the plurality of masking elements to be less than 75 percent of a total surface area of the exposed sides of the remaining portion of the initial substrate; Attaching the final substrate to the high resistivity layer includes attaching the final substrate to a plurality of vias to form a plurality of cavities between the final substrate and the device layer; The method includes forming a high resistivity material over the plurality of vias; The method includes selecting a high resistivity material to have an electrical resistivity greater than 10,000 ohm-cm; The method includes selecting the high resistivity material to include at least one of silicon oxide, silicon nitride, a high resistivity polymer, a polyimide, or a ceramic glue.
[0011] The present disclosure relates to - The final board, - a high resistivity layer disposed on the final substrate, the high resistivity layer comprising a remaining portion of the initial substrate; and a plurality of vias extending through said remaining portion; a high resistivity layer comprising: - a radio frequency electronic device disposed on the high resistivity layer; The semiconductor structure further comprises:
[0012] According to further non-limiting features of the invention, the following are incorporated, either alone or in any technically feasible combination:
[0013] A high resistivity layer includes a layer having an average electrical resistivity greater than approximately 10,000 ohm cm; the high resistivity layer includes a remaining portion of the initial substrate and a plurality of cavities; the high resistivity layer includes a high resistivity material disposed between the plurality of vias; The high resistivity material includes one or more of silicon oxide, silicon nitride, high resistivity polymer, polyimide, or ceramic adhesive; A high resistivity material has an electrical resistivity greater than approximately 10,000 ohm cm. [Brief description of the drawings]
[0014] While the specification concludes with claims particularly pointing out and distinctly claiming what are regarded as embodiments of the present disclosure, the advantages of the embodiments of the present disclosure may be more readily ascertained from the following description of certain examples of the embodiments of the present disclosure when read in conjunction with the accompanying drawings. [Figure 1A] FIG. 1 is a simplified schematic diagram illustrating the fabrication of semiconductor structures and devices that may be utilized in accordance with embodiments of the present disclosure, showing an initial substrate with device layers formed thereon. [Figure 1B] FIG. 1 is a simplified schematic diagram illustrating the fabrication of semiconductor structures and devices that may be utilized in accordance with embodiments of the present disclosure, showing a temporary substrate bonded to an exposed surface of a device layer opposite an initial substrate. [Figure 1C]1A-1C are simplified schematic diagrams illustrating the fabrication of semiconductor structures and devices that may be utilized in accordance with embodiments of the present disclosure, illustrating the thinning of a portion of an initial substrate. [Figure 1D] FIG. 1 is a simplified schematic diagram illustrating the fabrication of semiconductor structures and devices that may be utilized in accordance with embodiments of the present disclosure, showing the formation of a masking layer over remaining portions of an initial substrate. [Figure 1E] FIG. 1 is a simplified schematic diagram illustrating the fabrication of semiconductor structures and devices that may be utilized in accordance with embodiments of the present disclosure, showing a plan view of a remaining portion of an initial substrate having a masking layer thereon. [Figure 1F] FIG. 1 is a simplified schematic diagram illustrating the fabrication of semiconductor structures and devices that may be utilized in accordance with embodiments of the present disclosure, showing the formation of a high resistivity layer by forming a number of vias through remaining portions of an initial substrate. [Figure 1G] FIG. 1 is a simplified schematic diagram illustrating the fabrication of semiconductor structures and devices that may be utilized in accordance with embodiments of the present disclosure, showing attachment to a high resistivity layer of a final substrate. [Figure 1H] 1A-1C are simplified schematic diagrams illustrating the fabrication of semiconductor structures and devices that may be utilized in accordance with embodiments of the present disclosure, showing removal of the temporary substrate. [Figure 2A] FIG. 1 is a simplified schematic cross-sectional view illustrating the fabrication of a semiconductor structure and device that may be utilized in accordance with another embodiment of the present disclosure, showing a semiconductor structure including a temporary substrate, a device layer, and a remaining portion of an initial substrate including a plurality of vias. [Figure 2B] FIG. 1 is a simplified schematic cross-sectional view illustrating the fabrication of a semiconductor structure and device that may be utilized in accordance with another embodiment of the present disclosure, showing the application of a high resistivity material over a plurality of vias to form a high resistivity layer. [Figure 2C]1A-1C are simplified schematic cross-sectional views illustrating the fabrication of semiconductor structures and devices that may be utilized in accordance with another embodiment of the present disclosure, showing attachment to a high resistivity layer of a final substrate. [Figure 2D] 2D is a simplified schematic cross-sectional view illustrating the fabrication of a semiconductor structure and device that may be utilized in accordance with another embodiment of the present disclosure, showing removal of a temporary substrate from the semiconductor structure of FIG. 2C. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] The diagrams presented herein are not intended to be actual diagrams of any particular semiconductor structures, devices, systems, or methods, but merely idealized representations used to explain embodiments of the present disclosure.
[0016] Any headings used herein should not be construed as limiting the scope of the embodiments of the invention, which is defined by the following claims and their legal equivalents. Concepts described under any particular heading may generally be applicable in other sections throughout this specification.
[0017] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS An embodiment of the present invention will now be described with reference to Figures 1A to 1H. Referring to Figure 1A, an embodiment may include forming a device layer 100 on an initial substrate 102.
[0018] More specifically, the device layer 100 may include a plurality of electronic devices 104, which may include additional electronic device types in addition to switching devices, such as, for example, logic devices, light emitting devices, and light receiving devices. In an embodiment, the plurality of electronic devices 104 may include a plurality of radio frequency devices, such as RF CMOS devices. The device layer 100 may also include an interconnect layer 106, which may include conductive elements 108 disposed within an interlayer dielectric material 110. The plurality of electronic devices 104 may be formed on and / or in the initial substrate 102 using standard electronic fabrication methods known in the art.
[0019] An embodiment may include selecting the initial substrate 102 to include at least one of silicon, germanium, silicon germanium, silicon carbide, a III-V material, or a II-VI material. Further embodiments may include selecting the initial substrate to exhibit a resistivity between approximately 5 ohm cm and approximately 30 ohm cm. The initial substrate 102 may have a diameter of, for example, 300 mm, 200 mm, or other diameters may be utilized, depending on its end use.
[0020] The device layer 100 may include an exposed surface 112 that may be attached to a temporary substrate 114 to form a semiconductor structure 118, as shown in FIG. 1B. An embodiment may include selecting the temporary substrate 114 to include at least one of silicon, germanium, silicon germanium, silicon carbide, a III-V or II-VI material, glass, or the like. In an embodiment, the initial substrate 102 and the temporary substrate 114 may include essentially the same material. Such matching of the materials of the initial substrate 102 and the temporary substrate 114 may improve the process for attaching the device layer 100 to the temporary substrate 114. For example, the coefficient of thermal expansion of the initial substrate 102 and the coefficient of thermal expansion of the temporary substrate 114 may be selected to be essentially the same value to prevent undesirable stress during the attachment process. In a further embodiment, the difference between the coefficient of thermal expansion of the initial substrate 102 and the coefficient of thermal expansion of the temporary substrate 114 may be selected to be less than about 10 percent.
[0021] The attachment of the device layer 100 to the temporary substrate 114 may be preformed using a bonding process. For example, the exposed surface 112 of the device layer 100 may be bonded to the surface 116 of the temporary substrate 114. The bonding of the device layer 100 to the temporary substrate 114 may be performed by bonding them together via a molecular adhesion process at room temperature (e.g., between approximately 20° C. and 30° C.).
[0022] As known in the art, the principle of bonding by molecular adhesion, called direct bonding, is based on the principle of contacting two surfaces (e.g. the exposed surface 112 of the device layer 100 and the surface 116 of the temporary substrate 114) directly, i.e. without the use of specific bonding materials (glue, wax, solder, etc.). Such a bonding process requires that the surfaces to be bonded are sufficiently smooth and free of particles or contaminants, and that they are brought close enough together to be able to initiate contact at a distance generally less than a few nanometers. In this case, the attractive forces between the two surfaces are large enough to cause molecular adhesion (bonding caused by the sum of the attractive forces of electronic interactions (van der Waals forces) between two atoms or molecules of the two surfaces to be bonded).
[0023] Bonding by molecular adhesion may be initiated by application of a pressure point on at least one location of the semiconductor structure 118 (of FIG. 1B) formed by the initial substrate 102, the device layer 100, and the temporary substrate 114. A bond wave between the temporary substrate 114 and the device layer 100 is then propagated from the point where the pressure was applied. The application of such pressure is not, however, necessary to initiate propagation of the bond wave.
[0024] After bonding by molecular adhesion, annealing may be performed on the semiconductor structure 118 at a suitable temperature (preferably below 100° C.) to strengthen the bond between the temporary substrate 114 and the device layer 100 .
[0025] In a further embodiment, the bonding process for attaching the temporary substrate 114 to the exposed surface 112 of the device layer 100 may be performed under pressure at room temperature. In yet a further embodiment, the bonding process may be performed under pressure at a temperature of 100° C. or less.
[0026] In a further embodiment, a bonding layer (not shown) may be disposed between the temporary substrate 114 and the device layer 100. The bonding layer may be formed on one or both bonding surfaces of the device layer 100 and the temporary substrate 114, i.e., on the exposed surfaces 112 and 116. The bonding layer may include one or more of silicon oxide, silicon nitride, or silicon oxynitride. The bonding layer may be utilized to improve the reliability of the bonding process for attaching the device layer 100 to the temporary substrate 114.
[0027] Once the temporary substrate 114 is attached to the device layer 100, further processing may be utilized to form a high resistivity layer to improve the RF performance of the devices 104 that make up the device layer 100. The formation of the high resistivity layer may include removing a portion of the initial substrate 102 opposite the device layer 100. For example, with reference to FIG. 1C, the portion of the initial substrate 102 opposite the device layer 100 may be removed by utilizing a thinning process to leave a remaining portion 102′ of the initial substrate 102. The thinning of the portion of the initial substrate 102 may include one or more of an etching, grinding, and polishing process. For example, the initial substrate 102 may have an initial thickness approximately less than 1000 microns, or even less than 800 microns, or in an embodiment, less than 500 microns. The thinning process may be used to remove a portion of the exposed rear surface of the initial substrate 102, thereby reducing the thickness of the initial substrate 102 to less than approximately 100 microns, or less than 20 microns, or in one embodiment, less than approximately 5 microns.
[0028] Upon thinning the portion of the initial substrate 102, a masking layer 122 may be formed on the exposed rear surface 120 of the remaining portion 102′ of the initial substrate opposite the device layer 100, as shown in FIG 1D. The masking layer 122 may be formed on the exposed rear surface 120 of the remaining portion 102′ of the initial substrate 102 using methods well known in the semiconductor industry, such as standard photolithography methods. For example, the masking layer 122 may include one or more of a polymer, silicon oxide, silicon nitride, or metal layer.
[0029] As shown in Figure 1D, the masking layer 122 includes a plurality of masking elements 124 and a plurality of mask openings 126 disposed on the rear surface 120 of the remaining portion 102' of the initial substrate 102. An exemplary embodiment of the layout of the masking layer 122 on the rear surface 120 of the remaining portion 102' of the initial substrate 102 is shown in the plan cross-sectional view of Figure 1E. For example, as in the illustrated example of Figure 1E, the plurality of masking elements 124 making up the masking layer 122 may have a selected geometric shape, such as a rectangle, a circle, or other suitable masking geometric shape. In some embodiments of the present invention, the total surface area of the multiple masking elements 124 is less than 75 percent of the total area of the rear surface 120 of the remaining portion 102' of the initial substrate 102, in other embodiments, the total surface area of the multiple masking elements 124 is less than 60 percent of the total area of the rear surface 120 of the remaining portion 102' of the initial substrate 102, or in some embodiments, the total surface area of the multiple masking elements 124 is less than 50 percent of the total area of the rear surface 120 of the remaining portion 102' of the initial substrate 102.
[0030] Upon forming the masking layer 122, an etching process may be performed to form a plurality of vias 128 extending through the unmasked rear surface of the remaining portion 102' of the initial substrate 102, forming a semiconductor structure 130, as shown in FIG. 1F. For example, the etching process may include one or more of a dry etch process (such as a plasma etch process) or a wet etch process (such as a wet acid etch). In an embodiment of the present invention, the etching process may be performed until the plurality of vias 128 are approximately deeper than 5 microns, or deeper than 20 microns, or even deeper than 100 microns. The etching process is stopped before penetrating the device layer 100, thereby preventing any undesired damage to the plurality of devices 104 that make up the device layer 100. Upon completing the etching process, the masking layer 122 may be removed utilizing well-known methods, such as a chemical etch or a solvent wash.
[0031] After forming the multiple vias 128 extending through the remaining portion 102' of the initial substrate 102, the final substrate 132 may be attached over the multiple vias, forming multiple cavities 134 between the final substrate 132 and the device layer 100, as shown in FIG. 1G, with the multiple cavities 134 and the remaining portion 102' of the initial substrate 102 forming a high resistivity layer 136.
[0032] More specifically, embodiments of the present invention may include selecting the final substrate 132 to include at least one of silicon, germanium, silicon germanium, silicon carbide, a III-V material, or a II-VI material. In further embodiments, the final substrate 132 may include one or more of a ceramic, a dielectric, or an insulator. The final substrate may further include a single crystal material, or alternatively, a polycrystalline or amorphous material. Further embodiments may include selecting the final substrate 132 to exhibit a resistivity of approximately between about 10 ohm cm and about 1,000,000 ohm cm.
[0033] The final substrate 132 may be attached onto the plurality of vias 128 and contacted with the remaining portion 102′ of the initial substrate 102 using a bonding process as described above with reference to bonding of the temporary substrate 114 to the device layer 100 to form the plurality of cavities 134. Additionally, as described above, a bonding layer (not shown) may be formed on one or more of the final substrate 132 and the remaining portion 102′ of the initial substrate 102 to improve the bonding process, for example by molecular bonding as described in detail above.
[0034] The attachment of the final substrate 132 onto the vias 128 extending through the remaining portion 102' of the initial substrate 102 forms a high resistivity layer 136, which is disposed between the final substrate 132 and the device layer 100. The high resistivity layer 136 thus includes the cavities 134 and the remaining portion 102' of the initial substrate 102. In an embodiment, the attachment of the final substrate 132 onto the vias 128 may be performed by a molecular bonding process such that the cavities 134 constitute a number of air gaps, essentially including the atmosphere. In a further embodiment of the invention, the molecular bonding process may be utilized under different gas atmospheres such that the cavities 134 are filled with a selected atmosphere, and there may be different gas pressures within the cavities.
[0035] The high resistivity layer 136 may be fabricated such that it has an average electrical resistivity greater than approximately 10,000 ohm-cm, or greater than approximately 100,000 ohm-cm, or even greater than 1,000,000 ohm-cm. The fabrication of the high resistivity layer 136 disposed between the final substrate 132 and the device layer 100 ensures optimal performance of RF devices fabricated in the device layer 100.
[0036] Upon fabrication of the high resistivity layer 136, an embodiment of the present invention may proceed with removal of the temporary substrate 114, as shown in Figure 1H. The temporary substrate 114 may be removed by one or more of an etching, grinding, or polishing process. The temporary substrate 114 removal process is performed until all of the temporary substrate 114 is removed, thereby re-exposing the device layers 100, and in particular the interlayer dielectric 110 and the interconnect layer 106 including the conductive elements 106.
[0037] The embodiments of the invention as described above teach methods and structures for forming a high resistivity layer that includes a remaining portion of an initial substrate and a plurality of cavities. In further embodiments of the invention described below, the high resistivity layer may include additional high resistivity material formed thereon in addition to the remaining portion of the initial substrate.
[0038] More specifically, with reference to Figure 2A, a semiconductor structure 230 is formed that includes a temporary substrate 214, a device layer 200, a remaining portion of the initial substrate 202', and a plurality of vias 228 extending through the remaining portion of the initial substrate 202'. The semiconductor structure 230 of Figure 2A is essentially the same semiconductor structure as the semiconductor structure 130 of Figure IF and may be formed using essentially the same methods as previously described above in forming the semiconductor structure 130 of Figure IF.
[0039] 2A, embodiments may proceed with the formation of a high resistivity layer 236 that includes the remaining portion 202' of the initial substrate and additional high resistivity material 238. In some embodiments of the present invention, the high resistivity material 238 may be disposed on the remaining portion 202' of the initial substrate and may fill the plurality of vias 228, as shown in FIG.
[0040] A number of processes may be utilized to form the high resistivity material 238, such as one or more of a deposition process (e.g., chemical vapor deposition, physical vapor deposition, etc.) or a spin-on process. The high resistivity material 238 may be formed using a conformal formation process and subsequent planarization to form an exposed planar high resistivity surface 239. The planarization process to form the high resistivity surface 239 may be performed using one or more of a chemical polishing, scraping, or etching process.
[0041] In some embodiments of the present invention, the high resistivity material 238 may include one or more of a dielectric material such as, for example, silicon oxide, silicon nitride, a high resistivity polymer, a polyimide, or a ceramic adhesive. The high resistivity material 238 may include a high resistivity material having an electrical resistivity value approximately greater than 10,000 ohm cm, approximately greater than 100,000 ohm cm, or having an electrical resistivity value greater than 1,000,000 ohm cm.
[0042] Upon forming the high resistivity layer 236, the final substrate 232 may be attached to the high resistivity layer 236, as shown in Figure 2C. Attachment of the high resistivity layer 236 to the final substrate 232 may be performed utilizing a bonding process as previously described with reference to bonding the temporary substrate 114 to the device layer 100. Additionally, as previously described, a bonding layer (not shown) may be formed on one or more of the final substrate 232 and the high resistivity layer 236 to improve the bonding process, for example, by molecular bonding as previously described in detail above.
[0043] Upon fabrication of the high resistivity layer 236, an embodiment of the present invention may proceed with removal of the temporary substrate 214, as shown in Figure 2D. The temporary substrate 214 may be removed by one or more of an etching, scraping, or polishing process. The temporary substrate 214 removal process is performed until all of the temporary substrate 214 is removed, thereby re-exposing the device layers 200, and in particular the interconnect layers including the interlayer dielectric and conductive elements. EXAMPLES
[0044] According to a first exemplary implementation (described with reference to Figures 1A to 1H), a device layer 100 including an RF switch is produced on an initial substrate 102 made from silicon, with a resistivity of 5 ohm-cm, a diameter of 300 mm, and a thickness of 800 microns (Figure 1A).
[0045] A temporary substrate 114 made of silicon, with a diameter of 300 mm and a thickness of 800 microns, is assembled by molecular adhesion bonding to the exposed surface of the device layer 100. Before bonding, the exposed surface of the device layer 100 may be subjected to chemical mechanical planarization followed by cleaning in order to give it the flatness, low level of roughness and cleanliness required for the purpose of bonding by molecular adhesion. The temporary substrate 114 may then also be subjected to a microelectronic cleaning (for example with ozone + RCA) in order to provide it with suitable surface properties. An assembled semiconductor structure 118 (Figure 1B) is thereby obtained. The rear side of the initial substrate 102 (i.e. the side opposite to the side carrying the device layer 100) is then thinned, for example by mechanical grinding and then by chemical mechanical polishing, until a residual thickness of 5 microns is achieved (Figure 1C). Prior to the thinning stage, the assembled semiconductor structure 118 may be subjected to a heat treatment, for example at about 100-150° C., to enhance the bonding strength at the interface between the temporary substrate 114 and the device layer 100 .
[0046] A photolithography stage then serves to apply a masking layer 122 to the thinned back side of the initial substrate 102 to define masked areas 124 and unmasked areas 126 (FIGS. 1D and 1E). By way of example, the masked areas 124 are squares with side dimensions of 10×20 microns. The surface area of the masked areas 124 is less than 50%, i.e., for example, 40%, of the total surface area of the thinned side of the initial substrate 102. A chemical etching stage is then used to etch the unmasked areas 126 of the initial substrate 102 in order to form vias 128 (FIG. 1F). The masking layer 122 is removed.
[0047] A final substrate 132, for example made of aluminum nitride, with a thickness of 500 microns, is then prepared for its assembly onto the thinned rear side of the initial substrate 102. The preparation of the assembled surfaces may include a plasma treatment (under oxygen or nitrogen) that makes it possible to activate the surfaces and provide a high adhesion energy at low temperature for the subsequent bonding. The assembly is carried out using a direct bonding technique under a controlled atmosphere. By way of example, the atmosphere of the bonding chamber may be air at atmospheric pressure or a gas (for example nitrogen or argon, or another gas) at a selected pressure. Following the assembly (FIG. 1G), a high resistivity layer 136 is formed, which consists of the remaining part 102′ of the initial substrate 102 and a cavity 134 filled with air or a selected gas at a selected pressure. To increase the bonding energy between the thinned side of the initial substrate 102 and the final substrate 132, a low-temperature heat treatment (on the order of 100° C., given the large difference between the thermal expansion coefficients of the assembled temporary and final substrates) may be carried out.
[0048] The final stage involves the removal of the temporary substrate 114. It can be performed by removing the latter by mechanical scraping and chemical etching, or preferentially by decomposition, i.e. by applying a mechanical application force to the bonding interface between the temporary substrate 114 and the device layer 100.
[0049] The resulting structure 140 provides good RF performance to the switches contained within layer 100 of the device thanks to the presence of a final substrate having more advantageous electrical insulating properties than those of the initial substrate 102, and furthermore the remaining portion 102' of the initial substrate 102 does not impair the performance of the device by creating conductive paths thanks to the formation of the high resistivity layer 136.
[0050] The manufacturing technique according to the invention therefore makes it possible to use an initial silicon substrate instead of a more expensive SOI substrate and, following the double transfer of layers and the manufacture of a high resistivity layer 136, to obtain a structure whose properties are suitable for RF applications. EXAMPLES
[0051] According to a second exemplary implementation (described with reference to FIGS. 2A to 2D), the device layer 200 including the RF switches is produced on an initial substrate made of silicon with a resistance of 30 ohm cm, a diameter of 300 mm and a thickness of 800 microns. A temporary substrate 214 made of silicon with a diameter of 300 mm and a thickness of 800 microns is assembled by direct bonding to the exposed face of the device layer 200. Before bonding, the exposed face of the device layer 200 may have been subjected to chemical mechanical planarization followed by cleaning in order to give it the flatness, low level of roughness and cleanliness required for the purpose of bonding by molecular adhesion. The temporary substrate 214 may then also have been subjected to a microelectronic cleaning (e.g. with ozone+RCA) in order to provide it with the correct surface properties. The rear side of the initial substrate (i.e. the side opposite to the side carrying the device layer 200) is then thinned, for example by mechanical grinding and then by chemical mechanical polishing, until a residual thickness of 20 microns is achieved.
[0052] A photolithography stage then serves to apply a masking layer to the thinned rear side (remaining portion 202') of the initial substrate to define masked and unmasked areas. By way of example, the masked areas are rectangular with side dimensions of 10x20 microns. The surface area of the masked areas is less than 75% of the total surface area of the thinned side of the initial substrate 202, i.e. for example 55%. A chemical etching stage is then used to etch the unmasked areas of the remaining portion 202' of the initial substrate in order to form vias 228 (FIG. 2A). The masking layer is removed.
[0053] A layer of high resistivity material 238 is then deposited in the via 228 to fill the latter (i.e. to a thickness at least equal to the remaining thickness of the remaining portion 202' of the initial substrate) and, if appropriate, on the remaining portion 202' of the initial substrate (as shown in FIG. 2B). This high resistivity material is, for example, silicon oxide, or alternatively it may be made of a polymer with high resistivity (i.e. a resistivity preferably higher than 10000 ohm cm). It is then possible to prepare the exposed surface 239 of the high resistivity material 238 for the purpose of direct bonding, for example by application of a chemical mechanical planarization followed by an RCA clean.
[0054] A final substrate 232, made of glass, for example with a thickness of 500 microns, is then prepared for its assembly onto the thinned rear side of the initial substrate (remaining part 202'). The preparation of the assembled surfaces may include a plasma treatment (under oxygen or nitrogen) that makes it possible to activate the surfaces and provide a high adhesion energy at low temperature for the subsequent bonding. The assembly is carried out using a direct bonding technique. Following the assembly (FIG. 2C), a high resistivity layer 236 is formed, which consists of the remaining part 202' of the initial substrate and of a high resistivity material 238. To increase the bonding energy between the thinned side of the initial substrate and the final substrate 232, a low-temperature heat treatment (on the order of 100° C., given the large difference between the thermal expansion coefficients of the assembled temporary and final substrates) may be carried out.
[0055] The final stage involves the removal of the temporary substrate 214 (FIG. 2D), which can be performed by removing the latter by mechanical scraping and chemical etching, or preferentially by peeling, i.e., by applying a mechanical adaptive force to the bonding interface between the temporary substrate 214 and the layer 200 of the device, for example.
[0056] The resulting semiconductor structure 240 provides good RF performance to the switches contained within the device layer 200 thanks to the presence of the final substrate 232, which has more advantageous electrical insulating properties than those of the initial substrate, and furthermore, the remaining thickness of the remaining portion 202' of the initial substrate does not impair the performance of the device by creating conductive paths thanks to the formation of the high resistivity layer 236.
[0057] The exemplary embodiments of the present disclosure described above do not limit the scope of the present invention, as these embodiments are merely examples of embodiments of the present disclosure, which is determined by the scope of the appended claims and their legal equivalents. Any equivalent embodiments are intended to be within the scope of the present invention. Indeed, various modifications of the present disclosure, such as alternative beneficial combinations of the described elements, in addition to those shown and described herein, will become apparent to those skilled in the art from this description. In other words, one or more features of one exemplary embodiment described herein may be combined with one or more features of another exemplary embodiment described herein to provide further embodiments of the present disclosure. Such modifications and embodiments are intended to be encompassed within the scope of the appended claims.
Claims
1. 1. A method of forming a semiconductor structure, comprising: forming a device layer on an initial substrate, the initial substrate being configured as a bulk substrate; attaching a first surface of the device layer to a temporary substrate; A step of forming a high resistivity layer on the initial substrate, the step of forming the high resistivity layer comprising: removing a portion of the initial substrate; forming a plurality of vias extending through a remaining portion of the initial substrate; forming a high resistivity material over the remaining portion of the initial substrate to fill the vias, the high resistivity layer including the remaining portion of the initial substrate, the vias, and the high resistivity material having an electrical resistivity value greater than approximately 10,000 ohm cm; removing the temporary substrate; 23. A method comprising:
2. forming a plurality of vias through the remaining portion of the initial substrate, forming a masking layer on an exposed surface of the remaining portion of the initial substrate; Etching a via through the remaining unmasked portion of the initial substrate; The method of claim 1 further comprising:
3. 3. The method of claim 2 , wherein the masking layer comprises a plurality of masking elements, the method further comprising the step of selecting a total surface area of the plurality of masking elements to be less than 75 percent of a total surface area of the exposed faces of the remaining portion of the initial substrate.
4. 4. The method of claim 1, further comprising the step of attaching a final substrate to the high resistivity layer, the final substrate being attached to the plurality of vias to form a plurality of cavities between the final substrate and the device layer.
5. 10. The method of claim 1, further comprising selecting the high resistivity material to include at least one of silicon oxide, silicon nitride, a high resistivity polymer, a polyimide, or a ceramic adhesive.
6. A final substrate which is a bulk substrate; a high resistivity layer disposed on the final substrate, the high resistivity layer including a remaining portion of an initial substrate, a plurality of vias extending through the remaining portion, and a high resistivity material having an electrical resistivity value greater than approximately 10,000 ohm-cm; a radio frequency electronic device layer disposed on the high resistivity layer; and attaching the final substrate, which has more advantageous electrical insulation than the initial substrate, to the high resistivity layer to form a high resistivity path in the remaining portion of the initial substrate which serves as a low resistivity path.
1. A semiconductor structure comprising:
7. 7. The semiconductor structure of claim 6, wherein the high resistivity layer comprises a remaining portion of the initial substrate and a plurality of cavities.
8. 7. The semiconductor structure of claim 6, wherein the high resistivity material comprises one or more of silicon oxide, silicon nitride, a high resistivity polymer, a polyimide, or a ceramic adhesive.
Citation Information
Patent Citations
Integrated circuit and manufacturing method of integrated circuit and electronic device
CN104681562A
Super-high frequency integrated circuit device
JP1986054674A
Monolithic integrated circuit device for high-frequency, and method for manufacturing the same
JP2003289106A
Manufacturing method for stacked semiconductor structure with reduced resistance loss
JP2007507093A
SOI with gold-doped handle wafer
US20150371905A1