Insulating wall material for building ventilation ducts
A lightweight, self-supporting heat insulating material for ventilation ducts is achieved by using a stacked and compressed glass fiber structure with an inorganic binder, addressing molding and dehydration challenges of existing materials.
Patent Information
- Application Number
- JP2020183505
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2020-11-02
- Publication Date
- 2024-11-14
- Estimated Expiration
- 2040-11-02
AI Technical Summary
Existing insulation materials for ventilation ducts, such as glass fiber felt and calcium silicate, are difficult to mold into desired shapes, lack self-supporting capabilities, are heavy, and have poor dehydration properties after moisture absorption.
A heat insulating molded body composed of stacked and compressed defibrated glass fibers with an inorganic binder, having a density of 190-370 kg/m³, which is lightweight, easy to mold, and ensures dehydration properties, with a clamping strength maintained by a density of 250 kg/m³ or less.
The solution provides a heat insulating wall material that can maintain its shape, is lightweight, and effectively dehydrates, ensuring a weight loss of 6-9% within 25 hours post-water absorption.
Smart Images

Figure 0007583405000003 
Figure 0007583405000004 
Figure 0007583405000005
Abstract
Description
[Technical field]
[0001] The present invention relates to an insulating wall material for ventilation ducts in buildings. [Background technology]
[0002] Generally, ventilation ducts such as kitchen exhaust ducts, air conditioning ducts, and chimneys in buildings are provided with heat-resistant and heat-retaining insulation materials. This type of ventilation duct insulation material is made of glass fiber felt or calcium silicate. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2018-112329 A [Patent Document 2] JP 2020-003105 A Summary of the Invention [Problem to be solved by the invention]
[0004] Fiberglass felt insulation for ventilation ducts is difficult to form into a desired wall shape, and even if it is formed, it is difficult to make it stand on its own and maintain that wall shape. Calcium silicate ventilation duct insulation is relatively dense and heavy, and has poor dehydration properties after absorbing moisture, so it takes a long time to dry. In view of the above circumstances, an object of the present invention is to provide an insulating wall material for ventilation ducts which can be easily formed into a desired wall shape, can stand on its own and retain its shape, is lightweight, and has good dewatering properties. [Means for solving the problem]
[0005] In order to solve the above problems, the present invention provides a heat insulating wall material for a ventilation duct of a building, a heat insulating shaped body formed into a predetermined wall shape along a flow path of the ventilation duct, the heat insulating shaped body including a stacked compressed body in which defibrated glass fiber bodies are stacked and compressed, and a cured inorganic binder that is diffused in the stacked compressed body and bonds the defibrated bodies together, The density of the stacked compressed body in the heat insulating molded body is 190 kg / m 3 ~370kg / m 3 It is characterized by being about. This makes it possible to obtain a heat insulating wall material for ventilation ducts which can be easily formed into a desired wall shape, can stand on its own and retain its shape, is lightweight, and has a certain degree of dewatering properties.
[0006] It is preferable that the thickness reduction degree when the insulating wall material for ventilation ducts is sandwiched between backing plates on both sides and a bolt is inserted through the insulating wall material and a tightening torque of 20 Nm is applied is 60% or less. This ensures the tightening resistance and thus the self-supporting shape retention of the insulating wall material. From the viewpoint of ensuring the tightening resistance and thus the self-supporting shape retention of the insulating wall material, the density is 250 kg / m 3 Super 370kg / m 3 It is more preferable that the amount is less than that. In the insulating wall material for ventilation ducts, the weight loss ratio after 25 hours from the start of dehydration after absorbing water, relative to the weight at the time of substantially complete water absorption, is preferably more than 6%, more preferably 8% or more, and even more preferably 9% or more, at a temperature of 20°C to 30°C and a relative humidity of 60% RH to 80% RH. This ensures the dehydration of the insulating wall material. From the viewpoint of weight reduction of the insulating wall material or ensuring dehydration, the density is preferably 190 kg / m 3 More than 200kg / m 3 Less than 100% is preferable. From the viewpoint of ensuring dewatering, 250 kg / m 3 Super 370kg / m 3 It can be less than stomach. The time when the insulation wall material is substantially completely absorbed is not limited to the time when the insulation wall material is completely absorbed, but may be the time when the insulation wall material is almost completely absorbed, specifically, the time when the insulation wall material is at least 90% of the time when the insulation wall material is completely absorbed. Usually, when the insulation wall material is immersed in water, it will be almost completely absorbed in a few minutes, and even if the insulation wall material continues to absorb water after that, there will be almost no increase in weight due to water absorption.
[0007] The density of the stack of defibrated materials before compression is 100 kg / m 3 ~200kg / m 3 It is preferable that the amount is about 100%. It is preferable that the compressed stack has a large number of streaks extending in the thickness direction and distributed in the in-plane direction, and that the defibrated bodies are intertwined with each other in each streaky portion. The thickness direction refers to a direction connecting an inner surface (a surface facing the flow path) and an outer surface of the insulating wall material. The in-plane direction refers to a direction along a surface perpendicular to the thickness direction, or a direction along the inner surface or the outer surface. Preferably, the stack is compressed in the thickness direction to become the stack compressed body.
[0008] It is preferable that the heat insulating wall material for ventilation ducts further comprises a surface layer sheet covering the surface of the heat insulating molded body, and the surface layer sheet is directly bonded to the heat insulating molded body by the inorganic binder cured product on the surface. The surface may be the outer surface, inner surface, or flow path defining surface of the heat insulating molded body. Effect of the Invention
[0009] According to the present invention, it is possible to obtain a heat insulating wall material for ventilation ducts which can be easily formed into a desired wall shape, can be self-supporting and shape-retaining, is lightweight, and has a certain degree of dewatering property. [Brief description of the drawings]
[0010] [Figure 1] FIG. 1 is a cross-sectional view of a ventilation duct for a building according to one embodiment of the present invention. [Diagram 2] FIG. 2 is a perspective view of the building ventilation duct. [Diagram 3] FIG. 3 is an exploded perspective view of the air duct for a building. [Figure 4] FIG. 4 is an explanatory diagram illustrating an enlarged cross-sectional structure of the insulating wall material of the building ventilation duct. [Diagram 5] 5(a) to (h) are explanatory diagrams of the manufacturing process of the heat insulating wall material. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Hereinafter, one embodiment of the present invention will be described with reference to the drawings. 1 and 2 show a building ventilation duct 1. The building may be a house, an office building, or a factory. The building ventilation duct 1 may be a kitchen exhaust duct, an air conditioning duct, or a chimney (smoke exhaust duct). The building ventilation duct 1 has, for example, a cylindrical shape.
[0012] As shown in Figures 1 and 3, the building ventilation duct 1 includes a heat insulating wall material 2 and an inner surface member 3. The heat insulating wall material 2 includes a pair of heat insulating molded bodies 10 and a surface sheet 4. The heat insulating molded bodies 10 are molded to match the wall shape of the building ventilation duct 1. For example, each heat insulating molded body 10 has a half-cylinder shape. Two heat insulating molded bodies 10 are joined together to form the cylindrical heat insulating wall material 2. Although not shown in the drawings, adhesive tape or adhesive is used as a means for joining the heat insulating bodies 10 together.
[0013] 4, the heat insulating molded body 10 includes a compressed laminate 11 and a cured inorganic binder 12. The compressed laminate 11 is obtained by compressing a laminate 11x in which a large number of defibrated glass fiber bodies 11a are stacked. The glass fibers contain SiO2 as a main component, and may also contain Al2O3, Fe2O3, TiO2, CaO, Na2O, etc. The SiO2 content in the glass fibers is preferably about 50 to 98 wt%, more preferably about 60 to 95 wt%, and even more preferably about 70 to 95 wt%. The defibrated glass fiber material 11a is preferably long fiber, and its average length is usually 10 mm or more, preferably 20 mm or more, more preferably 30 mm or more, and even more preferably 50 mm or more. The average diameter of the defibrated glass fiber material 11a is usually about 2 to 30 μm, preferably about 5 to 30 μm, more preferably about 5 to 20 μm, and even more preferably about 5 to 15 μm. The density of the stack 11x (FIG. 5(d)) in which the defibrated bodies 11a are stacked before compression is preferably 100 kg / m 3 ~200kg / m 3 That's about it. The density of the stacked compressed body 11 in the heat insulating molded body 10 is 190 kg / m 3 ~370kg / m 3 That's about it.
[0014] The hardened inorganic binder 12 is formed by hardening the inorganic binder 12a (FIG. 5(e)) that is applied to and impregnated into the stack 11x. The defibrated bodies 11a are bonded together via the hardened inorganic binder 12. The hardened inorganic binder 12 is dispersed almost uniformly over the entire area of the heat insulating molded body 10. Preferably, the inorganic binder 12a is a thermosetting inorganic binder that is in a liquid state when applied or impregnated and is irreversibly hardened by heating. Examples of the main components of the inorganic binder 12a include silica, aluminum silicate, and other clay minerals. The weight ratio of silica to aluminum silicate is, for example, silica:aluminum silicate=50:50 to 10:90. Furthermore, the inorganic binder 12a before hardening also contains water and other liquids. The viscosity of the inorganic binder 12a can be adjusted by the amount of liquid such as water. The aluminum silicate may be hydrated aluminum silicate.
[0015] The proportion of the defibrated body 11a in the heat insulating formed body 10 is preferably about 80 wt % to 90 wt %. The proportion of the inorganic binder cured product 12 in the heat insulating molded body 10 is preferably 10 wt % to 20 wt %. In the heat insulating molded body 10, the remainder excluding the defibrated body 11a and the inorganic binder cured product 12 is mostly occupied by voids (gaps or air layers). The volume ratio of the voids (gaps) in the heat insulating molded body 10 is preferably about 0.1 vol% to 10 vol%, and more preferably about 0.5 vol% to 5 vol%. The voids are almost uniformly dispersed inside the heat insulating molded body 10.
[0016] A large number of streak-like portions 13 are formed in the stacked compressed body 11 and thus in the heat insulating molded body 10. These streak-like portions 13 each extend in the thickness direction (radial direction, vertical direction in Fig. 4) of the heat insulating molded body 10, and are disposed in a dispersed manner in the in-plane direction of the heat insulating molded body 10 (circumferential direction and axial length direction, horizontal direction in Fig. 4 and perpendicular direction to the paper surface), preferably at substantially uniform intervals. In each streak-like portion 13, the defibrated bodies 11a are intertwined with each other. The arrangement interval d of the streak-like portions 13 is 13 is preferably d 13 = 0.1 mm to 10 mm, and more preferably d 13 = 0.5mm to 5mm.
[0017] The outer peripheral surface (surface) of the heat insulating molded body 10 is covered with a surface sheet 4 such as an aluminum glass cloth. The surface sheet 4 is directly bonded and integrated with the heat insulating molded body 10 by an inorganic binder that appears on the outer peripheral surface of the heat insulating molded body 10. No separate adhesive is used to bond the surface sheet 4. When both sides of the heat insulating wall material 2 are sandwiched between backing plates made of steel plates and bolts are inserted through the material and tightened with a tightening torque of 20 Nm, the degree of thickness reduction is preferably 60% or less. The weight loss ratio of the insulating wall material 2 after 25 hours from the start of dehydration after water absorption to the weight at the time of substantially complete water absorption is preferably more than 6%, more preferably 8% or more, and even more preferably 9% or more, in an environment of a temperature of 20°C to 30°C and a relative humidity of 60% RH to 80% RH.
[0018] An inner surface member 3 is provided on the inner peripheral surface of the heat insulating wall material 2. The inner surface member 3 is made of, for example, a metal pipe with a circular cross section. The internal space of the inner surface member 3 serves as a flow path for the fluid to be circulated, such as kitchen exhaust air, air conditioning air, and chimney exhaust gas. The metal pipe may be a spiral pipe of a galvanized steel sheet or a stainless steel pipe. The material of the inner surface member 3 is not limited to metal, and may be resin, ceramics, paper, wood, etc. The inner surface member 3 may be formed of a sheet similar to the surface sheet 4, and may be directly bonded and integrated with the heat insulating molded body 10 by an inorganic binder that appears on the inner peripheral surface (surface) of the heat insulating molded body 10.
[0019] The building ventilation duct 1 is manufactured as follows. As shown in FIG. 5(a), glass fiber 2a as a material is prepared. 5(b), the glass fibers 2a are defibrated to obtain a defibrated body 11a. The defibrated body 11a is piled up to form a stack 11x. As shown in Fig. 5(c), the stack 11x is needle-punched by a needle punch device 5 having many needles 5a. The needles 5a have protruding barbs 5c. The high-speed reciprocating motion of the needles 5a causes the defibrated bodies 11a to intertwine with each other. As a result, as shown in Fig. 5(d), the stack 11x becomes mat-like, and many streaky portions 13 extending in the thickness direction of the stack 11x are formed. The stack 11x at this stage has no shape retention and can be easily deformed by gravity or other external forces.
[0020] 5(e), an inorganic binder 12a is applied to both sides (upper and lower sides in the figure) of the stack 11x. The application is preferably performed with a roller, but may also be performed with a spray. Instead of applying the inorganic binder, the stack 11x may be immersed in an inorganic binder tank to impregnate the stack 11x with the inorganic binder 12a. In this case, it is preferable to immerse the upper and lower portions of the stack 11x in the inorganic binder tank by half or less of the thickness of the stack 11x. It is preferable to form a non-impregnated layer of the inorganic binder 12a in the central portion of the stack 11x in the thickness direction. This ensures a void (air layer) in the stack 11x. For this reason, in the stages from application or impregnation to compression molding described later, the content of the inorganic binder 12a in the stack 11x is high in both side portions (upper and lower portions) of the stack 11x and low in the central portion of the stack 11x in the thickness direction. In addition, the presence rate of voids (air gaps) in the stack 11x is low in both side portions of the stack 11x and high in the central portion of the stack 11x in the thickness direction.
[0021] As shown in FIG. 5(f), the upper surface of the stack 11x after coating or impregnation (the outer periphery of the ventilation duct 1) A surface sheet 4 is attached to the upper surface (the surface facing the side) of the stack 11x. The surface sheet 4 is directly bonded to the stack 11x by the inorganic binder 12a that appears on the upper surface of the stack 11x.
[0022] As shown in Fig. 5(f), molds 6 and 7 having mold surfaces 6a and 7a corresponding to the finished shape (half-cylinder shape) of the heat-insulating molded body 10 are prepared separately. A heater 8 is built into at least one of the molds 6 and 7. In the figure, the heater 8 is composed of multiple rod-shaped heaters, but is not limited to this and may be a plate heater or the like.
[0023] The stack 11x is set between the molds 6 and 7. 5(g), the molds 6 and 7 are closed, and the stack 11x is compression molded by applying pressure while being heated by a heater 8. For the application of pressure, an air cylinder is preferably used. The pressure in the heating and compression molding step is preferably about 0.1 MPa to 0.7 MPa. The heating temperature is preferably about 100° C. to 400° C. The molding time (duration of application of the pressure and heating) is preferably about 3 minutes to 30 minutes. As a result, the stack 11x is compressed in the thickness direction to become the compressed stack body 11. Preferably, the compressed stack body 11 is compression molded so that the thickness of the compressed stack body 11 is about 1 / 2 to 4 / 5 of the thickness of the stack 11x before compression. In addition, the fluidity of the inorganic binder 12a increases due to heating, and the liquid component of the inorganic binder 12a boils, vaporizes, and dissipates. In this process, the solid component of the inorganic binder 12a diffuses throughout the entire stack 11x and becomes the cured inorganic binder 12. Furthermore, the voids (air gaps or air layers) in the stack 11x are reduced in volume by the compression of the stack 11x, and the voids are diffused throughout the compressed stack 11 as the inorganic binder 12a diffuses and the liquid components evaporate and dissipate. As shown in FIG. 5(h), the mold is then removed.
[0024] This forms a heat insulating molded body 10 having at least a part of the wall shape (semi-cylinder shape) of the duct 1. The defibrated bodies 11a throughout the entire heat insulating molded body 10 are bonded evenly via the inorganic binder cured product 12, thereby ensuring the self-supporting shape retention of the heat insulating molded body 10. Furthermore, since the defibrated bodies 11a are entangled with each other in the streak-like portions 13, it is possible to more reliably prevent the stacked compressed body 11 from coming apart, and the self-supporting shape retention of the heat insulating molded body 10 can be further improved. By using glass fiber as the main material of the heat insulating molded body 10, the heat insulating property and heat resistance of the heat insulating molded body 10 can be ensured. Furthermore, by using an inorganic binder instead of an organic binder as the binder, it is possible to ensure the heat resistance, fire resistance, and heat insulation of the heat insulating molded body 10. In addition, by uniformly dispersing voids throughout the entire heat insulating molded body 10, the heat insulation properties are further improved. A surface sheet 4 is laminated integrally on the outer peripheral surface (surface) of the heat insulating molded body 10. The surface sheet 4 is directly bonded to the heat insulating molded body 10 by the cured inorganic binder 12 on the outer peripheral surface (surface) of the heat insulating molded body 10. Since the cured inorganic binder 12 serves as a bonding means for the surface sheet 4, no separate bonding means such as an adhesive is required.
[0025] A pair of the semi-cylindrical heat insulating molded bodies 10 are prepared. The pair of heat insulating molded bodies 10 are placed on both sides of the inner surface member 3 that is separately prepared. The pair of heat insulating formed bodies 10 are joined together by a joining means such as an adhesive tape or an adhesive, thereby obtaining a cylindrical heat insulating wall material 2. In this way, the building ventilation duct 1 is obtained. The inner surface member 3 serves to prevent the defibrated body 11a from scattering from the inner peripheral surface of the insulating wall material 2. The surface sheet 4 serves to prevent the defibrated body 11a from scattering from the outer peripheral surface of the insulating wall material 2. According to this embodiment of the present invention, by preparing a mold corresponding to the wall shape of various building ventilation ducts, the shape of the heat insulating molded body 10, and therefore the shape of the heat insulating wall material 2, can be set as desired. The density of the stacked compressed body 11 in the heat insulating molded body 10 is 190 kg / m 3 ~370kg / m 3 By adjusting the thickness to about 100 mm, it is possible to obtain a heat insulating wall material for ventilation ducts which is self-supporting and capable of retaining its shape, is lightweight, and has a certain degree of dewatering property. The density is 190 kg / m 3 More than 250kg / m 3 By setting the thickness reduction rate to more than 60%, the fastening resistance and thus the self-supporting shape retention of the heat insulating wall material 2 for a ventilation duct can be sufficiently ensured. The density is 370 kg / m 3 below (250kg / m 3 (Even super) , preferably 200 kg / m 3 By setting the weight reduction rate to less than 6%, preferably more than 6%, more preferably 8% or more, and even more preferably 9% or more, the insulating wall material 2 can be made lightweight and its dewatering properties as an insulating wall material 2 for a ventilation duct can be ensured.
[0026] The present invention is not limited to the above-described embodiment, and various modifications can be made without departing from the spirit of the present invention. For example, the building ventilation duct is not limited to a kitchen exhaust hood, an air conditioning duct, or a chimney, but may be a ventilation duct or the like. The shape of the ventilation duct is not limited to a cylindrical shape, but may be a rectangular or other polygonal cylindrical shape, or may be any other shape. The insulating wall material may be a flat plate, a curved plate, or any other shape. The defibrated material 11a is not limited to long fibers, and may be short fibers. The inorganic binder 12a is not limited to a thermosetting binder, and may be, for example, a water-setting binder that hardens by a hydration reaction or the like. The inorganic binder 12a may be melted by heating to bond the defibrated bodies 11a together, and then hardened by cooling. The inorganic binder 12a may contain a dispersion medium or a solvent. The dispersion medium or solvent may be vaporized when heated. The dispersion medium or solvent may be water. A surface layer sheet 4 may be provided on the inner surface (duct flow path defining surface) of the wall-shaped heat insulating molded body. The surface layer sheet 4 may be directly bonded to the heat insulating molded body by an inorganic binder on the inner surface of the heat insulating molded body. The surface layer sheet may be omitted. EXAMPLES
[0027] The present invention is not limited to the following examples. In Example 1, the clamping force resistance according to the density of the insulating wall material was verified. Samples 1 to 4 of a heat insulating wall material were prepared, each of which was made of a heat insulating molded body containing a compressed laminate and a cured inorganic binder. The length and width of the insulating wall material samples 1 to 4 were approximately 100 mm x approximately 100 mm, and the initial thickness (before tightening) was 19.7 mm to 20.7 mm. The thickness was measured at four points on each of the insulating wall material samples 1 to 4, and the average value was used (similar to Example 2). The initial density (before tightening) of the insulation wall material sample was 198 kg / m 3 ~367kg / m 3 It was. Both sides of each of the insulation wall material samples 1 to 4 were sandwiched between a pair of steel plates, a bolt was inserted from one of the plates through the insulation wall material samples 1 to 4 and the other plate, a nut was screwed in, and a tightening torque of 20 Nm was applied to measure the degree of thickness reduction ( (Initial thickness - Fastening thickness ) / initial thickness) was measured. As shown in Table 1, the measurement results were 59%, 50%, 42%, and 30%, respectively, confirming that sufficient self-supporting shape retention was ensured for use as an insulating wall material for ventilation ducts.
[0028] [Table 1] EXAMPLES
[0029] In Example 2, the dehydration after water absorption according to the density of the insulating wall material was examined. Heat insulating wall material samples 5 to 8 were prepared, each consisting of a heat insulating molded body containing a compressed laminate and a cured inorganic binder. The length and width of each of the heat insulating wall material samples 5 to 8 was approximately 100 mm×approximately 100 mm, and the thickness was 20 mm to 20.8 mm. The initial weight (before water absorption) of the insulating wall material samples was 0.041 kg to 0.073 kg. The density of the insulating wall material sample is 205 kg / m 3 ~347kg / m 3 It was. These insulating wall material samples were immersed in water in a bucket to absorb water (water absorption process). After these insulating wall material samples were substantially completely absorbed in the water absorption process for 1 hour (60 minutes), they were taken out of the bucket and immediately weighed, which was 0.220 kg to 0.244 kg. The removed heat insulating wall material sample was left to stand in an environment at a temperature of 20° C. to 30° C. and a relative humidity of 60% RH to 80% RH to dehydrate. As shown in Table 2, the weight of the heat insulating wall material sample 25 hours after it was taken out (at the end of the water absorption process) was 0.197 kg to 0.221 kg, and the weight loss rate was 9% to 10%.
[0030] [Comparative Example] As a comparative example, a thermal insulation wall material sample made of calcium silicate was prepared. The thermal insulation wall material sample made of calcium silicate had a length and width of 99 mm x 99 mm, a thickness of 26.3 mm, and a density of 440 kg / m3 When the dehydration of the thermal insulating wall material sample made of calcium silicate was examined under the same conditions as in Example 2, the weight loss rate was 6%. It has been confirmed that the insulating wall material according to the present invention is lighter in weight and has superior dewatering properties than insulating wall materials made of calcium silicate.
[0031] [Table 2] [Industrial Applicability]
[0032] The present invention can be applied to ventilation ducts such as kitchen exhaust ducts, air conditioning ducts, and chimneys in buildings, for example. [Explanation of symbols]
[0033] 1. Building ventilation ducts 2. Insulating wall materials 2a Glass Fiber 4. Surface sheet 10. Heat-insulating molded body 11 Stacked compressed body 11a Defibrillator 11x stack 12 Inorganic binder hardened material 12a Inorganic binder 13 Streak
Claims
1. A heat insulating wall material for ventilation ducts in a ventilation duct of a building, a heat insulating shaped body formed into a predetermined wall shape along a flow path of the ventilation duct, the heat insulating shaped body including a stacked compressed body in which defibrated glass fiber bodies are stacked and compressed, and a cured inorganic binder that is diffused in the stacked compressed body and bonds the defibrated bodies together, The density of the stacked compressed body in the heat insulating molded body is 250 kg / m 3 Super 370kg / m 3 is as follows: The insulating wall material for ventilation ducts is characterized in that when both sides of the insulating wall material for ventilation ducts are sandwiched between backing plates, a bolt is inserted through the insulating wall material and a tightening torque of 20 Nm is applied, the degree of thickness reduction is 50% or less.
2. A heat insulating wall material for ventilation ducts in a ventilation duct of a building, a heat insulating shaped body formed into a predetermined wall shape along a flow path of the ventilation duct, the heat insulating shaped body including a stacked compressed body in which defibrated glass fiber bodies are stacked and compressed, and a cured inorganic binder that is diffused in the stacked compressed body and bonds the defibrated bodies together, The density of the stacked compressed body in the heat insulating molded body is 250 kg / m 3 Super 370kg / m 3 is as follows: The insulating wall material for ventilation ducts is characterized in that the weight loss ratio after 25 hours from the start of dehydration after water absorption, relative to the weight when the insulating wall material for ventilation ducts has substantially completely absorbed water, is 9% or more at a temperature of 20°C to 30°C and a relative humidity of 60% RH to 80% RH.
Citation Information
Patent Citations
Core material for vacuum heat insulation material, manufacture thereof and vacuum heat insulation material
JP1996028776A
Duct
JP2018112329A
Chimney and lining member of the same
JP2020003105A
Thermal insulation cover for air conditioning irregular pipe duct and air conditioning irregular pipe duct with thermal insulation cover
JP3005033U