How to recycle lead wires for barrel plating equipment
The method for recycling lead wires in barrel plating equipment by replacing worn electrode components and applying new coverings maintains performance and extends the life of lead wires, addressing the issue of reduced plating effectiveness.
Patent Information
- Application Number
- JP2024070124
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2024-04-23
- Publication Date
- 2024-11-14
- Estimated Expiration
- 2044-04-23
AI Technical Summary
Existing methods for replacing electrode portions in lead wires for barrel plating equipment risk reducing the plating effect due to decreased applied power, and there is a need for efficient recycling of lead wires to maintain performance.
A method for recycling lead wires involves removing old electrode balls and coverings, applying new coverings and electrode balls, and optionally adding a curl or marking for tracking usage, ensuring airtightness and maintaining electrical performance.
The method allows for the reuse of lead wires with improved performance, ensuring consistent plating quality by replacing worn components and tracking usage, thus extending the life and efficiency of the lead wires.
Smart Images

Figure 0007583419000001_ABST
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for recycling lead wires for a barrel plating apparatus, which are used when performing an electroplating process in the barrel plating apparatus. [Background technology]
[0002] Nickel plating, tin plating, zinc plating, alloy plating, etc. (hereinafter simply referred to as "plating") are highly corrosion resistant and have good color tones, and are therefore used for various purposes such as corrosion prevention, decoration, etc. There are various methods for plating products, but when plating a large number of small items, small components, etc., the barrel plating method using a barrel plating machine is preferable and widely used.
[0003] A barrel plating device comprises a processing liquid tank (plating tank) filled with processing liquid, a barrel container rotatably arranged within the processing liquid tank, and electricity is passed from an anode inserted into the processing liquid tank to a cathode on a lead wire, and electroplating is performed on the workpiece while the plating barrel is rotated around its central axis.
[0004] When plating is performed using a lead wire, the plating metal is deposited on the electrode (cathode), but if electroplating is continued in this state in the barrel plating method, the contact between the workpiece and the electrode will deteriorate due to a drop in the applied power, and the workpiece may come into contact with the deposited metal, causing scratches on the workpiece and reducing the value of the product. Therefore, when a certain amount of metal deposition is found on the electrode, the lead wire needs to be replaced, but in order to make effective use of the lead wire, it is common to replace only the electrode part.
[0005] There are various known inventions and devices that, when plating metal adheres to the electrode of a lead wire, replace it with a new electrode and reuse the lead wire itself (lead wire body), for example, the "cathode part for electroplating barrel" described in Patent Document 1. The device in Patent Document 1 is a cathode part for electroplating barrel characterized by comprising an insulating lead wire, a stainless steel bolt attached to the tip of the lead wire, a zinc or zinc alloy cap detachably screwed onto the tip side of the bolt, and an acid-resistant, alkali-resistant packing and a hard resin sleeve attached to the middle part of the bolt between the cap and the lead wire.
[0006] Patent Document 1 states that "plated metal 16 adheres to the surface of cathode portion 11 and gradually grows. When plated metal 16 has become a certain amount of mass...the cap 23 with plated metal 16 adhered thereto is twisted and removed from stainless steel bolt 17 and separated as shown in Figure 6. A new cap 23 is then screwed onto bolt 17 to complete the replacement procedure" (page 7).
[0007] Also, there is a "contact terminal for barrel plating" described in Patent Document 2. The device according to Patent Document 2 is a contact terminal for barrel plating, characterized in that the cathode contact terminal is disposed inside the barrel body and comes into contact with the product, and is composed of a base part to be soldered to the lead wire and a front part connected to the base part and freely removable, and the plating film grown on the outer periphery can be freely removed by removing only the front part, without removing the lead wire from the barrel body.
[0008] Patent Document 2 states that "a plating film forms on the contacts, and when this grows to a certain thickness, the top part of the contact can be reversed and removed, and easily replaced with a new top part" (page 4).
[0009] [Patent Document 1] Practical application 1984-193865 [Patent Document 2] Actual development Showa 63-98379 Summary of the Invention [Problem to be solved by the invention]
[0010] However, as in the devices related to References 1 and 2, if the electrode part is replaced easily, there is a risk that the plating effect will decrease due to a decrease in the applied power. [Means for solving the problem]
[0011] Therefore, the present invention provides a method for recycling lead wires for barrel plating equipment.
[0012] The invention of claim 1 is a method for recycling lead wires for a barrel plating apparatus which applies electric current from an anode to a cathode in a plating solution stored in a plating tank of the barrel plating apparatus to electroplating an object to be treated, comprising the steps of: removing an old electrode ball screwed onto the lead wire body of the barrel plating apparatus; removing an old coating covering the tip end of the lead wire body; coating the tip end of the lead wire body with a new coating; and screwing a new electrode ball onto the lead wire body to form a new lead wire. forming the new lead by heating and / or cooling; A method for recycling lead wires for a barrel plating apparatus comprising the steps of: It is.
[0013] The invention of claim 2 is a method for recycling lead wires for use in a barrel plating apparatus as described in claim 1, which includes a process of coating the tip side of the lead wire body with a coating material instead of the process of coating the tip side of the lead wire body with a new coating.
[0014] The invention of claim 3 is a method for recycling lead wires for a barrel plating apparatus according to claim 1 or 2, further comprising a step of applying marking processing to new lead wires in accordance with the number of times they have been recycled. Effect of the Invention
[0017] According to the invention described in claims 1 and 2 of the present application, the lead wire body can be used as is, and by replacing the old electrode balls, etc. with new electrode balls, etc., it is possible to recycle it into a new lead wire with maintained or even improved performance.
[0018] According to the invention described in claim 3 of the present application, the number of times replacement work has been performed can be easily visually confirmed from the outside, so that the time to replace the lead wire body can be estimated.
[0019] According to the invention as set forth in claims 4 and 5 of the present application, the plate can be adapted to the shape of a barrel plating device or the like, enabling efficient plating work. [Brief description of the drawings]
[0020] [Figure 1] 1 is a flow chart showing the steps of the present invention. [Diagram 2] This is a photograph of the lead wire. [Diagram 3] This is a photograph of the free end of the lead wire. [Figure 4] This is a photograph of the free end side of the lead wire body. [Diagram 5] This is a photograph of a lead wire with a buffer material interposed therebetween. [Figure 6] This is a photograph of the free end side of a lead wire with a buffer material interposed therebetween. [Figure 7] This is the first disassembly photo of the lead wire with the electrode ball and cushioning material removed. [Figure 8] This is the second disassembly photo with the electrode ball and cushioning material removed from the lead wire body. [Figure 9] 1 is a photograph of the proximal end of the lead body. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0021] The barrel plating method using a barrel plating device (not shown) involves placing a large number of objects to be plated (small items such as screws, nuts, etc.) in a container called a barrel, immersing this barrel container in plating liquid in a plating tank, and rotating the barrel container to move the objects to be plated inside the barrel container while passing a direct current from an anode plate (anode) placed in the plating tank to a lead wire 1 (cathode), thereby forming a plating coating on the surface of the objects to be plated.
[0022] The present invention is a method for recycling lead wires 1 that serve as cathodes immersed in plating solution during electroplating in a barrel plating device, i.e., lead wires for barrel plating devices (hereinafter simply referred to as "lead wires") 1. Even if plating metal is deposited on the electrode balls 20 of the lead wires 1 during plating, the lead wires 1 can be recycled and reused as new lead wires 1 by going through the steps of the present invention.
[0023] The lead wire 1 is fixed to a well-known barrel plating device. An example of the barrel plating device and plating process will be briefly described below.
[0024] The barrel container, which is rotatably supported within the plating tank by an arm that can move up and down and which contains the objects to be plated, is a polygonal container body such as a hexagon, and has many holes drilled therein for immersing the objects to be plated in the plating liquid. A second gear that meshes with a first gear connected to the rotating shaft of the drive unit (motor) is fixedly provided on both the left and right side surfaces of the barrel container.
[0025] One or more lead wires 1 (cathode) are inserted into the barrel container, and the electrode balls 20 of the lead wires 1 are in contact with the object to be plated. With electricity flowing from the anode plate (anode) in the plating tank to the cathode in the barrel container, the drive unit operates to rotate the first gear and the second gear meshing with the first gear, thereby rotating the barrel container. As a result, electricity flows from the anode plate (anode) connected to the positive terminal of the power source to the lead wire 1 (cathode) connected to the negative terminal of the power source, and the object to be plated in contact with the cathode is electroplated. As an example of the arrangement of the multiple lead wires 1, there are an arrangement in which two pairs of lead wires 1 are inserted from through holes at both ends in the left and right direction of the barrel container, and an arrangement in which two or more lead wires 1 are suspended from above into the barrel container. Here, in the case of an example in which two pairs of lead wires 1 are inserted from the left and right of the barrel container, it is desirable to reverse the direction of the screw grooves of the electrode balls 20 of the left and right lead wires 1. Specifically, it is desirable to form the screw hole 22 of the electrode ball 20 of one lead wire 1 into a forward thread, and the screw hole 22 of the electrode ball 20 of the other lead wire 1 into a reverse thread. By providing electrode balls 20 with reverse threads in this manner, the electrode balls 20, 20 can be fastened together by frictional contact, rotational contact, etc., between the electrode balls 20, 20 and the inner surface of the barrel container as the barrel container rotates.
[0026] Next, a description will be given of the lead wire 1 that is used in the barrel plating apparatus and is recycled. In the embodiment, the same reference numerals are given to old components and corresponding new components.
[0027] The lead wire 1 can be broadly divided into a lead wire body 2 and electrode balls 20. The lead wire body 2 mainly comprises a conductive wire 3 that conducts electricity, a connection base 6 connected to one end (free end) of the conductive wire 3, and a terminal 13 connected to the other end (base end) of the conductive wire 3. The length of the lead wire 1 (lead wire body 2 and electrode balls 20) is not important.
[0028] The material of the conductor 3 is not particularly limited, but may be soft twisted copper wire, flexible twisted copper wire, etc. The conductor 3 is covered with an insulator 5.
[0029] The material of the insulator 5 may be soft vinyl or the like, and any insulating material may be used.
[0030] The tip of the lead wire body 2 is provided with a connection base 6. The connection base 6 is a member that connects the conductor 3 and the electrode ball 20, and the connection base 6 is connected to one end of the conductor 3. Specifically, a connection hole (not shown) is opened at the rear end of the body 7 of the connection base 6, and the free end side of the conductor 3 inserted into this connection hole is clamped and held. The connection base 6 is connected to the centering portion of the conductor 3 that is centered from the free end of the insulator 5. The clamping portion may be one or more. Although the internal structure is not shown, for example, there may be a configuration in which the free end side of the lead wire 1 is clamped and held at two points, namely, the insulator crimping portion 15, which is a portion that crimps the conductor 3 together with the insulator 5, and the conductor crimping portion 17, which is a portion that crimps the conductor 3 (centering portion) in a state in which the conductor 3 is centered from the insulator 5. In such an example, the connection hole of the connection base 6 is configured with two stages of different diameters, the first stage (large diameter) being the insulator crimping portion 15 and the second stage (small diameter) being the conductor crimping portion 17. A bolt portion 8 stands upright from the front end of the main body 7, and this bolt portion 8 is threaded with a screw groove that screws into the screw groove of the electrode ball 20.
[0031] The electrode ball 20 is screwed to the connection base 6 at the free end of the lead wire body 2. The electrode ball 20 is a cylindrical member with a hole drilled from the base end, and a screw groove is threaded on the inner peripheral surface of the hole. That is, a screw hole 22 is provided in the central axis direction. The shape of the tip side may be any shape such as a bullet shape (spherical shape) or a flat shape, and is not particularly limited. In addition, a collar may be press-fitted to the tip side of the electrode ball 20, or a collar may be welded (not shown). The electrode ball 20 may be made of any material such as brass, copper, iron, stainless steel, etc., as long as it is electrically conductive. Titanium may also be used. The diameter, length, etc. of the electrode ball 20 can be selected arbitrarily.
[0032] The conductor 3 is covered with an insulator 5, and the free end side of the lead wire body 2 is further covered with a coating 10. Specifically, it is covered up to the edge (tip surface 7a) of the body 7 of the connection base 6. The coating 10 may be made of any material. For example, it may be made of a material that is stretchable and adheres to the insulator 5 covering the lead wire 1, a material that adheres to the insulator 5 covering the lead wire 1 by thermal contraction, or a material that is resistant (chemical resistant) to the chemical solution used for plating.
[0033] A terminal 13 having a terminal hole 13a is connected to the base end of the lead body 2 (see FIG. 9, etc.). The terminal 13 and the conductor 3 may be connected by any method, such as soldering or spot welding (resistance welding). The area between the base end side of the lead body 2 and the terminal 13 is preferably covered with a covering 10 and further provided with a sealing structure.
[0034] The electrode balls 20 are screwed into the connection base 6, and a buffer material 30 may be interposed between the electrode balls 20 and the connection base 6 (see FIG. 5, etc.). Specifically, the buffer material 30 is fitted onto the bolt portion 8 of the connection base 6 that connects the conductor 3 and the electrode balls 20, and is finally crimped by the electrode balls 20. The buffer material 30 may be any material that can provide a buffer seal between the electrode balls 20 and the connection base 6, and examples of the buffer material include an O-ring (made of resin, etc.) and a packing (made of rubber, etc.).
[0035] Electrically conductive grease can be applied to the bolt portion 8 of the connection base 6. Any electrically conductive grease may be used as long as it has an electrically conductive effect, and examples of such grease include grease or other oils mixed with metal powder having low electrical resistance, such as copper, and containing antioxidants, corrosion inhibitors, and other additives. The consistency, dropping point, oil separation rate, and other properties of the grease composition can be appropriately selected.
[0036] By applying conductive grease to the bolt 8, when the electrode ball 20 is screwed into the connection base 6, a thin film is formed between the thread groove of the bolt 8 and the thread groove of the electrode ball 20, reducing the electrical resistance at the contact point between the connection base 6 and the electrode ball 20, enabling smooth and stable electrical conduction. In addition, oxidation and corrosion of the contact point between the connection base 6 and the electrode ball 20 are prevented.
[0037] The present invention relates to a method for recycling lead wires 1, in which an electric current is applied from an anode to a cathode in a plating solution stored in a plating tank using the barrel plating apparatus described above to electroplating an object to be treated. Each step of the recycling method of the present invention will be described below. Various types of plating can be used for the electroplating, such as nickel plating, tin plating, zinc plating, and alloy plating, but in the following embodiment, a method for recycling lead wires 1 in the case where lumps of plated metal have adhered to electrode balls or the like due to nickel electroplating will be described.
[0038] First, as a pre-process of the present invention, the lead wire 1 with plated metal lumps attached to the cathode electrode ball 20 is removed from the barrel plating device and collected. After a certain period of plating work, old electrode balls 20 need to be replaced due to adhesion of plated metal lumps to the electrode ball 20 of the lead wire 1. To do this, in order to facilitate recycling of the lead wire 1 to maintain or improve its performance, the lead wire 1 with plated metal lumps attached to the electrode ball 20 is removed from the barrel plating device. For example, if the lead wire 1 is fixed to the barrel plating device via a fastener such as a bolt or nut in the terminal hole 13a of the terminal 13 at the base end of the lead wire 1, the lead wire 1 can be removed from the barrel plating device by loosening the fastener. The removal is performed manually or using a tool. From here on, the steps of the present invention are carried out.
[0039] The first step is to remove the old electrode ball 20 screwed into the lead wire body 2 of the lead wire 1 (ST1). Since the old electrode ball 20 is screwed into the connection base 6, the old electrode ball 20 with the plated metal lumps attached thereto is removed from the connection base 6 of the lead wire 1 by turning the screw in the direction opposite to the fastening direction.
[0040] The second step is to remove the old coating 10 that covers the tip side of the lead wire body 2 (ST2). The old coating 10 that covers the tip side of the lead wire body 2 may be scratched during the plating process, and lumps of plated metal may adhere to the old coating 10 as well as to the old electrode ball 20, so the old coating 10 is removed.
[0041] The third step is to coat the tip end of the lead wire body 2 with a new coating 10 (ST3). Specifically, the coating 10 is tightly attached to the insulator 5 of the lead wire body 2. If the coating 10 is a heat shrink tube, the heat shrink tube will shrink when any heat is applied, and this heat-shrinkable heat shrink tube will coat the tip end of the lead wire 1 (insulator 5). It is desirable to coat up to the tip surface 7a of the main body 7 of the connection base 6 (see FIG. 8, etc.). By coating up to the tip surface 7a of the main body 7, the airtightness between the electrode ball 20 and the connection base 6 is further improved.
[0042] The fourth step is to screw new electrode balls 20 into the lead wire body 2 to make a new lead wire 1 (ST4). The new electrode balls 20 are screwed into the connection base 6 and tightened. That is, the new lead wire 1 is completed by screwing and tightening the new electrode balls 20. When screwing the electrode balls 20, by firmly tightening the electrode balls 20, it is possible to prevent the plating liquid from penetrating. The electrode balls 20 may be tightened manually or with the aid of a tool.
[0043] Although the lead wire 1 can be recycled by going through the above steps, some of the steps may be replaced with other steps. For example, instead of the step (ST3) of covering the tip side of the lead wire body 2 with a new covering body 10, a step of covering the insulator 5 of the lead wire body 2 with a coating material may be performed. The coating material may be of any material, and the insulator 5 may be entirely covered, or only a part of the tip side may be covered. If the tip surface 7a of the body 7 of the connection base 6 is also covered with a coating material, it may not be necessary to interpose the buffer material 30 between the electrode ball 20 and the connection base 6.
[0044] In addition to the steps described above, the following steps may be added. When multiple steps are inserted, the order of the steps may be reversed, and the steps may be inserted between any steps.
[0045] For example, the method may further include a step of marking the lead wire 1 according to the number of times of recycling before the step of fixing a new lead wire 1 to the barrel plating device. The replacement time of the lead wire body 2 can be assumed, but the marking may be performed at any location on the lead wire 1 and may be performed by any type of processing. For example, the terminal 13 may be printed, engraved, written with a marking pen or the like, colored, etc. Furthermore, when the rear end side of the lead wire body 2 is covered with a coating 10, marking may be performed by making a cut in this coating 10, etc.
[0046] Prior to the step of fixing the new lead wire 1 to the barrel plating apparatus, a step of heating and / or cooling the new lead wire 1 to form a shape may be included. Examples of steps include a step of forming a shape (shape) of the new lead wire 1 to make it difficult for the electrode balls 20 to float, to conform to the internal shape of the barrel container, to bring the electrode balls 20 into contact with the object to be plated, etc. Examples of the shape of the lead wire 1 include a U-shape, an L-shape, a crank shape, etc. The heating temperature and cooling temperature are not particularly limited, and any method may be used for forming the shape.
[0047] There may be cases where old cushioning material 30 is fitted around the bolt portion 8 of the connection base 6 connected to the conductor 3 of the lead wire 1. In such a case, the old cushioning material 30 fitted around the bolt portion 8 of the connection base 6 connected to the conductor 3 of the lead wire 1 may be removed, and new cushioning material 30 may be fitted around the bolt portion 8 of the connection base 6. By inserting the bolt portion 8 from its tip and fitting the new cushioning material 30 around the bolt portion 8 of the connection base 6, the new cushioning material 30 will be interposed between the connection base 6 and the electrode ball 20.
[0048] A process of spreading the conductive grease evenly over the bolt portion 8 of the connection base 6 may be added. By spreading the conductive grease evenly over the thread groove of the bolt portion 8, it is possible to improve heat resistance and weather resistance and prevent a decrease in conductivity due to oxidation and corrosion. The grease can also be spread over the bolt portion 8 of the connection base 6 by screwing in a new electrode ball 20 several times.
[0049] Before the step of spreading the conductive grease evenly onto the bolt portion 8 of the connection base 6, a step of polishing the bolt portion 8 by hand using a device such as a rotary wire brush or a metal brush may be added. This step makes it possible to remove rust, dust, etc. from the bolt portion 8, further improving the conductive performance.
[0050] In addition, in order to prevent the electrode ball 20 from loosening and to make the screwing stronger, a thread locking agent may be applied between the bolt portion 8 of the connection base 6 and the screw hole 22 of the electrode ball 20.
[0051] After forming the new lead wire 1, the method may further include a step of measuring the resistance of the new lead wire 1 before the step of fixing the new lead wire 1 to the barrel plating device.
[0052] Finally, the new lead wire 1 that has been through each process is fixed to the barrel plating device. For example, when a pair of left and right lead wires 1 are placed in a barrel container, the lead wire 1 that screws into the bolt portion 8 when the electrode ball 20 is rotated forward (rightward), and the lead wire 1 that screws into the bolt portion 8 when the electrode ball 20 is rotated backward (leftward), are fixed to the barrel plating device. For example, when plating work is performed in a barrel container that rotates towards the front, by arranging and fixing a lead wire 1 with an electrode ball 20 that screws in in a forward direction (clockwise) on the right side as viewed from the front, and a lead wire 1 with an electrode ball 20 that screws in in a reverse direction (counterclockwise) on the left side as viewed from the front, it is possible to prevent the two electrode balls 20, 20 from loosening due to the rotation (frictional contact) of the barrel container and maintain a tightly fastened state.
[0053] It is desirable that the new lead wire 1 completed through each process of the recycling method of the present invention should be consistently performed by the manufacturer of the lead wire 1 before it is removed from the barrel plating device. That is, it is desirable that all of the processes, including the process (ST1) of removing the old electrode ball 20 screwed into the lead wire body 2 of the lead wire 1 for use in a barrel plating device of the present invention, the process (ST2) of removing the old coating 10 coating the tip end of the lead wire body 2, the process (ST3) of coating the tip end of the lead wire body 2 with a new coating 10, and the process (ST4) of screwing the new electrode ball 20 into the lead wire body 2 to make a new lead wire 1, should be performed by the manufacturer of the lead wire 1 (including a subcontractor).
[0054] As described in the problem of the invention, if the electrode portion (electrode ball 20) is replaced carelessly, there is a risk that the plating effect will decrease due to a decrease in the electric current passing through the lead wire 1. Therefore, if the manufacturer of the lead wire 1, who is most familiar with the performance, function, safety, effectiveness, etc. of the lead wire 1, carries out each of the recycling steps described above, the new lead wire 1 will also be able to exhibit high performance such as high sealing properties and low electrical resistance.
[0055] An example of the steps before and after each step and the worker will also be described for confirmation. The lead wire 1 with the plated metal lumps attached thereto is removed from the barrel plating device by the plating contractor, and the lead wire 1 removed from the barrel plating device is collected by the dealer (sales agent, etc.) and handed over to the manufacturer of the lead wire 1. After the manufacturer of the lead wire 1 performs each step of the present invention, the new lead wire 1 is handed over to the dealer, who delivers the new lead wire 1 to the plating contractor, and the plating contractor fixes the new lead wire 1 to the barrel plating device. This division of roles can contribute to improving business efficiency and maintaining high performance regarding the new lead wire 1. Alternatively, the plating contractor may directly send the lead wire 1 with the plated metal lumps attached thereto to the manufacturer of the lead wire 1 without going through the dealer, and the manufacturer of the lead wire 1 may send the new lead wire 1 to the plating contractor. The manufacturer of the lead wire 1 may also perform the steps before and after each step.
[0056] The present invention has been described above based on each embodiment, but the present invention is not limited to the above embodiments, and modifications may be made without departing from the spirit of the present invention, and the techniques described in each embodiment or other publicly known or well-known techniques may be combined.
[0057] In order to determine when the lead wire 1 should be recycled, a step of measuring the amount of plated metal lumps deposited on the electrode balls 20 may be added. The amount of precipitation may be measured, for example, by measuring the thickness (width in the short direction) of the old electrode balls 20 to which the plated metal lumps are attached after plating with a vernier caliper, gauge, etc., and subtracting the thickness (width in the short direction) of the electrode balls 20 to which the plated metal lumps are not attached from the thickness of the old electrode ball 20, and if the difference exceeds a certain range, it may be determined that the lead wire 1 should be recycled. The time to recycle may also be determined visually or simply based on the time when the lead wire 1 was installed in a barrel plating device.
[0058] Depending on the type of plating solution, the electrode balls 20 may wear out or dissolve, but even in such a case, by going through the steps of the present invention, the electrode balls 20 can be replaced with new ones to produce a new lead wire 1. In other words, the electrode balls 20 may be replaced to produce a new lead wire 1 even in cases other than when lumps of plating metal are attached to the electrode balls 20.
[0059] Regarding the barrel plating device to which the new lead wire 1 is fixed, it may be a horizontal barrel plating device equipped with a barrel having a horizontal rotation axis, or an inclined barrel plating device equipped with a barrel having an inclined rotation axis. [Explanation of symbols]
[0060] 1: Lead wire 2: Lead wire body 3: Conductor 5: Insulator 6: Connection base 7: Main body 7a: Tip surface 8: Bolt section 10: Covering body 13: Terminal 13a: Terminal hole 15: Insulation crimping part 17: Conductor crimping part 20: Electrode ball 22: Screw hole 30: Cushioning material ST1: First step ST2: Second process ST3: The third step ST4: The fourth step
Claims
1. A method for recycling lead wires for a barrel plating apparatus in which an electric current is passed from an anode to a cathode in a plating solution stored in a plating tank of the barrel plating apparatus to electroplating a workpiece, comprising the steps of: removing an old electrode ball screwed onto a lead body of the lead wire for a barrel plating apparatus; removing an old coating from the tip end of the lead body; applying a new coating to the tip end of the lead body; a step of screwing a new electrode ball into the lead body to make a new lead; and a step of forming a shape on the new lead wire by heating and / or cooling the new lead wire.
2. 2. The method for recycling lead wires for use in a barrel plating apparatus according to claim 1, further comprising the step of covering the tip end of the lead wire body with a coating material instead of the step of covering the tip end of the lead wire body with a new coating.
3. 3. The method for recycling lead wires for use in a barrel plating apparatus according to claim 1, further comprising the step of marking the new lead wires according to the number of times they have been recycled.
Citation Information
Patent Citations
Tongs for straightening wire
CN202239373U
Cable copper wire straightening device
CN211248091U
JP1973050618U
JP1974042174A
Film unit with lens and method for confirming number of recycled times and recycled time
JP1993093950A