Manufacturing method of press-molded products
The method addresses mold complexity and buckling issues by forming a step-shaped portion in the intermediate stage, enabling efficient and accurate production of press-formed products with outward flanges.
Patent Information
- Application Number
- JP2023551205
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2022-08-29
- Filing Date
- 2023-05-23
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2043-05-23
AI Technical Summary
Existing methods for manufacturing press-formed products with outward flanges face challenges such as complex mold structures, difficulty in achieving good dimensional accuracy, and buckling at the connection between the ridgeline and corner flange, especially with high-strength materials.
A manufacturing method that includes an intermediate molding step to form a step-shaped portion at the base of the outward flange, followed by a target shape forming step to bend and raise the flange, allowing for simultaneous press molding of the top plate, ridgeline, and vertical wall portions without a complicated mold structure.
This method enables the stable production of press-formed products with good dimensional accuracy and prevents buckling at the corner flange connection, enhancing manufacturing efficiency and product quality.
Smart Images

Figure 0007586339000002 
Figure 0007586339000003 
Figure 0007586339000004
Abstract
Description
[Technical field]
[0001] The present invention relates to a method for manufacturing a press-molded product, and in particular to a method for manufacturing a press-molded product having a top plate portion and a vertical wall portion continuing from the top plate portion via a ridge portion, and having an outward flange portion formed continuously with the ends of the top plate portion, the ridge portion, and the vertical wall portion. [Background technology]
[0002] As automobile crash safety standards become stricter, the crash safety of car bodies is being improved, but in response to carbon dioxide emission regulations, there is also a need to reduce the weight of car bodies in order to improve fuel efficiency and promote the shift to EVs. In order to achieve both improved crash safety and reduced weight of car bodies, the use of high-strength steel plates (also known as high-tensile steel) with a tensile strength of 590 MPa or higher is increasingly being used in car body structural parts.
[0003] As shown in FIG. 4 , an automobile part may be, for example, a press-formed product 1 such as a floor cross member, which has a top plate portion 5, a vertical wall portion 7, and a ridge portion 9 connecting the top plate portion 5 and the vertical wall portion 7, and has an outward flange portion 3 formed continuously with the ends of the top plate portion 5, the ridge portion 9, and the vertical wall portion 7.
[0004] When such a press-formed product 1 is press-formed, the portion of the outward flange portion 3 that continues to the ridge portion 9 (hereinafter referred to as the "corner flange portion") undergoes stretch flange deformation, making it prone to cracks occurring at the tip of the corner flange portion 3b.
[0005] Regarding a conventional method for manufacturing a press-formed product having an outward flange portion formed continuously from the end of such a vertical wall portion 7, Patent Document 1 discloses a method for manufacturing a saddle-shaped press-formed product. In Patent Document 1, press forming is performed by bending the top plate portion of the blank, applying a first force from the inner side to the outer side of the blank, and applying a resultant force of a second force in directions facing each other and a third force in a direction opposite to the first force to each of the outer sides of the vertical wall portions. The method disclosed in Patent Document 1 is a method for simultaneously forming the top plate portion, the vertical wall portion, and the outward flange portion.
[0006] Patent Document 2 also discloses another press forming method in which a metal plate is formed into a U-shaped cross section and then an outward flange is bent up. The method disclosed in Patent Document 2 claims that when bending the outward flange, the forming of the flange starts from the top plate and vertical wall, so that the distortion of the outward flange can be distributed to the top plate and vertical wall.
[0007] Patent document 3 discloses a press molding method for forming an outward flange by a shearing process for forming a step portion in a workpiece having a top plate, a vertical wall, and a flange, and a cutting process for cutting away unnecessary portions in the vicinity of the step portion. [Prior art documents] [Patent documents]
[0008] [Patent Document 1] International Publication No. 2019 / 216317 [Patent Document 2] International Publication No. 2022 / 049916 [Patent Document 3] International Publication No. 2016 / 194963 Summary of the Invention [Problem to be solved by the invention]
[0009] In the method disclosed in Patent Document 1, the die structure is quite complicated, and the die manufacturing costs are high. In addition, because a composite force of a first force and a third force in the opposite direction is applied, it is difficult to press the blank sufficiently and evenly for press forming, and it is also difficult to obtain a press-formed product with good dimensional accuracy.
[0010] In this regard, as disclosed in Patent Document 2, a press forming method in which a metal plate is formed into a U-shaped cross section and then the outward flange portion is bent up can use a simple die and improve dimensional accuracy. However, in press forming of high-tensile steel with even higher strength, a problem arises in that the connection portion between the ridge portion and the corner flange portion of the outward flange portion (hereinafter sometimes simply referred to as the "connection portion of the corner flange portion") is prone to buckling (wrinkling, folding).
[0011] Furthermore, the method disclosed in Patent Document 3 has the problem that the mold structure is complicated and a cutting step is necessary.
[0012] The present invention has been made in consideration of the above-mentioned problems, and its object is to provide a method for manufacturing a press-molded product that can stably produce a press-molded product with good dimensional accuracy without using a mold with a complex structure and without causing buckling at the connection portion of the corner flange portion when manufacturing a press-molded product that has a top plate portion and a vertical wall portion that is continuous with the top plate portion via a ridge portion, and has an outward flange portion formed continuous with the ends of the top plate portion, the ridge portion, and the vertical wall portion. [Means for solving the problem]
[0013] In order to solve the above problems and achieve the objectives, (1) The manufacturing method of a press-molded product of the present invention is a manufacturing method of a press-molded product having at least a main body portion having a top plate portion and a vertical wall portion formed via a ridge portion, and an outward flange portion formed at an end of the main body portion so as to be continuous with the top plate portion, the ridge portion, and the vertical wall portion, and is characterized in that it includes an intermediate molding process for molding an intermediate molded product having the top plate portion and the vertical wall portion formed via the ridge portion, and having a step-shaped portion that bulges outward at a base portion of an outward flange equivalent portion molded to the outward flange portion, and a target shape molding process for bending the outward flange equivalent portion in the intermediate molded product outward to mold the outward flange portion into a target shape.
[0014] (2) The manufacturing method of a press-molded product according to the present invention, in the invention described in (1) above, is characterized in that the intermediate molding process press-moldes the top plate portion, the ridge portion, the vertical wall portion and the step-shaped portion in a single process.
[0015] (3) The manufacturing method of a press-molded product according to the present invention, in the invention described in (1) above, is characterized in that the intermediate molding process press-moldes the step-shaped portion after press-molding the top plate portion, the ridge portion, and the vertical wall portion. Effect of the Invention
[0016] The manufacturing method of a press-molded product according to the present invention has an advantage that when manufacturing a press-molded product having a top plate portion and a vertical wall portion continuing from the top plate portion via a ridge portion, and having an outward flange portion formed continuously with the ends of the top plate portion, the ridge portion and the vertical wall portion, it is possible to stably manufacture a press-molded product with good dimensional accuracy without using a mold with a complex structure and without causing buckling at the connection portion of the corner flange portion. [Brief description of the drawings]
[0017] [Figure 1] FIG. 1 is an explanatory diagram of a method for producing a press-molded product according to an embodiment. [Diagram 2] FIG. 2 is a diagram showing an analysis result of the forming process of the target shape forming step according to the embodiment. [Diagram 3] FIG. 3 is a diagram showing a model of the forming process of the target shape forming step according to the embodiment. [Figure 4] FIG. 4 is an explanatory diagram of an example of a press-molded product to which the present invention is directed. [Diagram 5] FIG. 5 is an explanatory diagram of a conventional method for manufacturing a press-formed product. [Figure 6] FIG. 6 is a diagram showing the analysis results of the molding process for molding an outward flange portion in a conventional example. [Figure 7] FIG. 7 is a diagram showing a typical process for forming an outward flange portion in a conventional example. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0018] Hereinafter, an embodiment of the method for producing a press-molded product according to the present invention will be described. Note that the present invention is not limited to the embodiment.
[0019] Before describing the embodiment of the present invention, the shape of the press-formed product to which the present invention is applied will be described with reference to FIG. 4, which shows an example thereof. The present invention is applied to a press-formed product 1 having an outward flange portion 3, as shown in FIG. 4, and including a main body portion 11 having a top plate portion 5, a vertical wall portion 7, and a ridge portion 9 connecting the top plate portion 5 and the vertical wall portion 7. The press-formed product 1 has an outward flange portion 3 formed at an end of the main body portion 11 and continuing to the top plate portion 5, the ridge portion 9, and the vertical wall portion 7. In the example shown in FIG. 4, the press-formed product 1 has a horizontal flange portion 13 at the lower end of the vertical wall portion 7. In the following description, the portions of the outward flange portion 3 continuing to the top plate portion 5, the ridge portion 9, and the vertical wall portion 7 are referred to as a top plate flange portion 3a, a corner flange portion 3b, and a vertical wall flange portion 3c, respectively.
[0020] FIG. 5 is a diagram showing a conventional molding method of a press-molded product 1. Conventionally, first, as shown in FIG. 5(a), an intermediate molded product 15 having a top plate portion 5, a ridge portion 9, a vertical wall portion 7, and a horizontal flange portion 13 at the lower end of the vertical wall portion 7 is molded. The intermediate molded product 15 has the top plate portion 5, the ridge portion 9, and the vertical wall portion 7 extending from its end, and these extending portions become the outward flange portion 3 (top plate flange portion 3a, corner flange portion 3b, and vertical wall flange portion 3c) in the target shape. Therefore, in this embodiment, the extending portions are referred to as outward flange equivalent portions 17. Each portion of the intermediate molded product 15 may be press-molded simultaneously, or each portion may be press-molded separately. Thereafter, as shown in FIG. 5(b), the outward flange equivalent portions 17 in the intermediate molded product 15 are bent outward to form the outward flange portion 3, resulting in the press-molded product 1 having the target shape.
[0021] In a forming method for bending and raising the outward flange equivalent portion 17, for example, as disclosed in Patent Document 2, a bending force is first applied to the top plate flange equivalent portion 17a and the vertical wall flange equivalent portion 17c. Then, in a forming method for bending and raising the outward flange equivalent portion 17, a bending force is applied to the corner flange equivalent portion 17b.
[0022] Fig. 6 shows the results of an FEM analysis using a steel plate with a thickness of 1.4 mm and a tensile strength of 590 MPa, where the target shape is a height of the outward flange portion 3 of 18 mm and a radius of 3 mm at the boundaries between the top plate portion 5, ridge portion 9 and vertical wall portion 7 and the outward flange portion 3. Fig. 6 shows the process from the state of intermediate formed product 15 before the forming of the outward flange portion 3 (Fig. 6(a)) to the state of the outward flange portion 3 after it has been bent and raised to the bottom dead center of forming (Fig. 6(d)), including intermediate stages.
[0023] A tension acts on the tip of the outward flange portion 3, reducing the plate thickness. Meanwhile, a large compression force acts on the connection portion 35 of the corner flange portion 3b (see FIG. 4). This compression force increases the plate thickness, and the maximum plate thickness increase rate at the bottom dead center of forming is 47%, causing wrinkles and folds (see FIG. 6(d)). Here, the plate thickness increase rate is calculated by finding the difference between the plate thickness at the relevant portion and the plate thickness of the blank metal plate, and calculating the ratio to the plate thickness of the blank metal plate.
[0024] Fig. 7 is a diagram showing a schematic diagram of the results of a more detailed study of the process by which wrinkles and folds occur in conventional press forming. Fig. 7 shows the state of the punch 19, die 20, lower pad 21, and metal plate 23 from midway through forming (38 mm up) (Fig. 7(a)) to near the bottom dead point of forming (4 mm up) (Fig. 7(e)) for a cut surface cut in the direction of arrow A along the ridge line 9 of the press-formed product 1 shown in Fig. 5. Note that values such as [30 mm up] are distances in the press forming direction taking into account the plate thickness up to the bottom dead point of forming of the die 20 at that position. Therefore, for example, the position of the die 20 at "30 mm up" is +30 mm in the reverse direction of press forming from the bottom dead point of pressing.
[0025] As shown in Fig. 7, at [38 mm up], the outward flange equivalent portion 17, which is the end portion of the metal sheet 23, begins to come into contact with the punch 19, and at [30 mm up], the outward flange equivalent portion 17 of the metal sheet 23 is bent toward the die 20. Thereafter, at [24 mm up], the outward flange equivalent portion 17 is bent at a position away from the die 20, and is folded so that its tip approaches the die 20. As forming further progresses, a fold occurs between the lower pad 21 and the forming surface of the punch 19 at [10 mm up], and the fold remains even when forming progresses to [4 mm up], causing wrinkles or remaining folds at the bottom dead point of forming.
[0026] One reason for this forming form is that the corner flange equivalent portion 17b, which is an extension of the ridge line portion 9, does not wrap around the die 20 and is folded in at a position away from the die 20 because the ridge line portion 9 passes through it and has high rigidity against bending (see FIG. 7(c)). Also, in this example, the vertical wall flange portion 3c (see FIG. 6) is not perpendicular to the surface of the top plate portion 5 of the press-formed product 1 but is inclined inward. This is because a large gap is generated between the flange forming portion of the punch 19 and the flange forming portion of the die 20 at the beginning of the press forming.
[0027] When considering measures to prevent the fold of the connection portion 35 of the corner flange equivalent portion 17b, the inventor focused on the deformation of the metal plate 23 from [30 mm up] to [24 mm up] in FIG. 7. Since such deformation occurs due to the free deformation of the end of the metal plate 23, which leads to the fold, it is considered that the free deformation of the end of the metal plate 23 should be restrained in order to prevent this. However, since the corner flange equivalent portion 17b needs to be formed into the corner flange portion 3b, it is difficult to completely restrain the end of the metal plate 23 by the die. Therefore, the inventor came up with the idea that if the part of the metal plate 23 corresponding to the base of the outward flange portion 3 can be wrapped around the die 20 at the beginning of the press forming, the above-mentioned fold can be prevented. The present invention is based on such an idea, and is specifically described below.
[0028] As shown in FIG. 1(a), an example is provided at the base of the outward flange equivalent portion 25 (top plate flange equivalent portion 25a, corner flange equivalent portion 25b, and vertical wall flange equivalent portion 25c) of the intermediate molded product 24, with a step 27 that is a step that bulges outward. In such an intermediate molded product 24, the outward flange equivalent portion 25 is molded into the outward flange portion 3 (top plate flange portion 3a, corner flange portion 3b, and vertical wall flange portion 3c) to form a target shape. By providing the step 27, such an intermediate molded product 24 can be easily wrapped around the die 20 in the early stages of press molding, preventing the above-mentioned folding.
[0029] Figures 2(a) to 2(d) are diagrams showing the results of an FEM analysis of the press forming process of an intermediate product 24 into a target shape. Figure 2(a) shows the intermediate product 24 (before flange forming) in which a stepped portion 27 is formed. Figures 2(b) to 2(d) show the forming process of the flange portion.
[0030] A tension acts on the tip of the outward flange portion 3, causing the plate thickness to decrease. A compression force acts on the connection portion 33 (see FIG. 1(b)) between the ridge portion 9 and the corner flange portion 3b, causing the plate thickness to increase. On the other hand, the maximum plate thickness increase rate at the bottom dead center of forming is 28%, which is significantly reduced compared to the maximum plate thickness increase rate of 47% shown in FIG. 6(d) showing the conventional example, and it is understood that wrinkles can be prevented. One of the reasons for the reduction in the maximum plate thickness increase rate is that in the present invention, in the [10mm up] shown in FIG. 2(c), the plate thickness increase portion of the connection portion 31 (see FIG. 1(a)) between the ridge portion 9 and the corner flange equivalent portion 25b is dispersed compared to the conventional [10mm up] shown in FIG. 6(c).
[0031] Fig. 3 is a schematic diagram showing the forming process of forming an intermediate product 24 into a target shape in the press forming of the present invention. Fig. 3 shows the states of the punch 19, die 20, lower pad 21, and metal plate 23 in the process from [38 mm up] to [4 mm up] on a cross section cut in the direction of arrow A along the ridge line 9 as shown in Fig. 1.
[0032] As shown in FIG. 3, at [38 mm up] to [30 mm up], the connection portion 31 between the ridge portion 9 and the corner flange portion 25b wraps around the die 20 because the step-shaped portion 27 is formed. Then, at [30 mm up], the outward flange portion 25 starts to contact the punch 19, and at [24 mm up], the tip of the metal sheet 23 is bent toward the die 20. At that time, the tip of the outward flange portion 25 does not approach the die 20 because the step-shaped portion 27 is formed. Therefore, the connection portion 31 between the ridge portion 9 and the corner flange portion 25b (see FIG. 1(a)) does not bend at an acute angle. In this regard, at [24 mm up] in FIG. 7 showing the conventional example, the tip of the outward flange portion 25 approaches the die 20, and the connection portion 35 between the ridge portion 9 and the corner flange portion 3b (see FIG. 4) is bent at an acute angle.
[0033] Furthermore, as press forming progresses, at [10 mm up], outward flange equivalent portion 25 is formed without being folded in the gap between die 20 and punch 19. Thereafter, forming progresses to [4 mm up], and outward flange portion 3 is formed at the bottom dead center of forming, and connection portion 33 (see FIG. 1(b)) between ridge portion 9 and corner flange portion 3b does not wrinkle. Thus, in this embodiment, by providing step-shaped portion 27, connection portion 31 between ridge portion 9 and corner flange equivalent portion 25b wraps around die 20 in the early stage of forming. As a result, the connection portion does not enter the gap between lower pad 21 and punch 19 and is not folded, and the occurrence of wrinkles is prevented.
[0034] The step portion 27 formed in the intermediate forming process can be press-formed simultaneously with forming the top plate portion 5, the vertical wall portion 7, and the ridge portion 9. Forming in one process makes the manufacturing efficient. Alternatively, the step portion 27 may be press-formed after forming the top plate portion 5, the vertical wall portion 7, and the ridge portion 9.
[0035] In the target shape forming process for forming the outward flange portion 3, as disclosed in Patent Document 2, a bending force is first applied to the top plate flange corresponding portion 25a and the vertical wall flange corresponding portion 25c. Then, it is preferable to apply a bending force to the corner flange corresponding portion 25b after that. In this way, it is possible to prevent cracks from occurring at the tip of the corner flange portion 3b.
[0036] In the above description, the orthogonal cross section of the ridgeline portion 9 having the vertical wall portions 7 on both sides of the top plate portion 5 and the horizontal flange portion 13 at the lower end of the vertical wall portions 7 is hat-shaped, but the present invention is not limited to this. That is, the orthogonal cross section of the ridgeline portion 9 without the horizontal flange portion 13 may be U-shaped, or may be Z-shaped or L-shaped by splitting the hat-shaped or U-shaped portion in half in the direction of the ridgeline portion 9 in the top plate portion 5. In addition, bending and drawing are suitable for forming the step-shaped portion that bulges outward in the present invention. Since the step-shaped portion is bent to form the outward flange portion 3, it is easy to form the outward flange portion 3 even when the width of the outward flange portion 3 is wide. On the other hand, when the step-shaped portion is formed by shear forming as described in Patent Document 3, the width of the flange portion may be restricted due to the breaking limit of the material, which may not be preferable. EXAMPLES
[0037] In this example, in order to confirm the effect of the present invention, a press forming analysis of the press-formed product 1 shown in FIG. 4, which is the subject of the present invention, and press forming of the actual material were performed. A 980 MPa-class steel plate with a plate thickness of 1.4 mm was used as the high-tensile material. The press-formed product 1 is hat-shaped with a top plate portion 5 having a width of 84 mm, a vertical wall portion 7 having a height of 100 mm, and a ridge portion 9 having a length of 180 mm. For the outward flange portion 3, the outward flange width defined in FIG. 1(b) was set to 16 mm, and the plate inner curvature radius R of the base portion on the cut surface cut along the ridge portion 9 in the direction of the arrow A was set to 3 mm.
[0038] In this embodiment, press forming analysis was performed for forming the outward flange portion 3 for the intermediate formed product 15 (see FIG. 5(a)) press-formed using the blank model of the high tensile steel as a conventional example and an inventive example. As a conventional example, as shown in FIG. 5 and FIG. 6, a press forming analysis was performed for forming the outward flange portion 3 without providing a step-shaped portion 27 at the base of the corner flange equivalent portion 17b. As an inventive example, a press forming analysis was performed for forming the outward flange portion 3 for the intermediate formed product 24 by providing a step-shaped portion 27 at the base of the corner flange equivalent portion 25b as shown in FIG. 1(a). In the inventive example, press forming analysis was performed by changing the height of the step-shaped portion 27, i.e., the difference in height between the step-shaped portion 27 and the top plate portion 5, from 1.0 mm to 2.5 mm, and the effect of the height of the step-shaped portion 27 was also compared. The plate thickness increase rate of the connection portion 33 or the connection portion 35 between the ridge line portion 9 and the corner flange portion 3b was obtained from the plate thickness of the connection portion using the plate thickness of the blank model as a reference. Table 1 shows the analysis results.
[0039] [Table 1]
[0040] In the case of No. 1, which is a conventional example without the step-shaped portion 27, the maximum thickness increase rate was as large as 47.6%. In the actual pressed material, buckling (wrinkling and folding) occurred at the connection portion 35 between the ridge portion 9 and the corner flange portion 3b. In contrast, in the invention examples No. 2 to No. 5 with the step-shaped portion 27, the analysis results showed that the maximum thickness increase rate was significantly reduced in all cases. In addition, buckling did not occur in these actual pressed materials. In addition, when the height of the step-shaped portion 27 of No. 4 was 2.0 mm, the maximum thickness increase rate was the lowest at 25%, which was almost half of the 47.6% of the conventional example. As described above, it was demonstrated that buckling of the connection portion 33 between the ridge portion 9 and the corner flange portion 3b can be prevented by providing the step-shaped portion 27 in the intermediate formed product 24 of the present invention. [Industrial Applicability]
[0041] The present invention provides a method for manufacturing press-molded products that can stably produce press-molded products with good dimensional accuracy without using a mold with a complex structure and without causing buckling at the connection portion of the corner flange portion. [Explanation of symbols]
[0042] 1 Press-molded products 3 Outward flange 3a Top plate flange 3b Corner flange part 3c Vertical wall flange 5 Top plate 7 Vertical wall section 9 Ridge 11 Main body 13 Horizontal flange 15 Intermediate molded product (conventional example) 17 Outward flange equivalent part (conventional example) 17a Top plate flange equivalent part (conventional example) 17b Corner flange equivalent part (conventional example) 17c Vertical wall flange equivalent part (conventional example) 19 Punch 20 Die 21 Lower pad 23 Metal plate 24 Intermediate molded products (examples of invention) 25 Outward flange equivalent part (example of invention) 25a Top plate flange equivalent part (example of invention) 25b Corner flange equivalent part (example of invention) 25c Vertical wall flange equivalent part (example of invention) 27 Stepped section 31 Connection between the ridgeline and corner flange of an intermediate molded product (example of the invention) 33 Connection between the ridgeline and corner flange of a press-molded product (example of invention) 35 Connection between ridge and corner flange (conventional example)
Claims
1. A method for manufacturing a press-molded product having at least a main body portion having a top plate portion and a vertical wall portion formed via a ridge portion, and an outward flange portion formed at an end of the main body portion and continuous with the top plate portion, the ridge portion, and the vertical wall portion, an intermediate molding step of molding an intermediate molded product having a top plate portion and a vertical wall portion formed via a ridge portion, and having a step-shaped portion that bulges outward at a base portion of an outward flange equivalent portion molded on the outward flange portion; a target shape forming step of bending the outward flange portion of the intermediate molded product outward to form the outward flange portion into a target shape, A method for manufacturing a press-formed product, characterized in that, in an early stage of forming in the target shape forming process, a step-shaped portion which is a connection portion between the ridge portion and a portion equivalent to a corner flange is wrapped around a die.
2. 2. The method for manufacturing a press-formed product according to claim 1, wherein the intermediate forming step comprises press-forming the top plate portion, the ridge portion, the vertical wall portion, and the step portion in a single step.
3. 2. The method for manufacturing a press-formed product according to claim 1, wherein the intermediate forming step includes press-forming the step portion after press-forming the top plate portion, the ridge portion, and the vertical wall portion.
Citation Information
Patent Citations
Production method of press component
JP2022091379A
Production method for press-molded member and press molding device
WO2014148618A1
Press molded product, press molding method, and press molding device
WO2016194963A1
Manufacturing method for saddle-shaped press-molded article, press-molding device, and manufacturing method for manufacturing saddle-shaped press-molded article
WO2019216317A1
Method for manufacturing press-formed article and pressing device
WO2022049916A1