Method for manufacturing sealing structure
The sealing structure addresses the inefficiencies of conventional sealing methods by using a diffusion joint with a plastic fluidized layer formed through forge welding, enhancing bonding strength and reliability while reducing production time and costs.
Patent Information
- Application Number
- JP2023539558
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-08-06
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2041-08-06
AI Technical Summary
Existing sealing methods for structures require multiple parts and processes, are heavy, costly, and lack high productivity, with potential issues in sealing quality and reliability, especially when dealing with dissimilar metals.
A sealing structure using a diffusion joint between metals with a plastic fluidized layer formed by forge welding at low temperatures, eliminating liquid phases and reducing metal thickness to enhance bonding strength and reliability.
The sealing structure achieves high bonding strength and reliability with a simple process, reducing production time and costs, and is applicable to various industrial fields.
Smart Images

Figure 0007586449000001 
Figure 0007586449000002 
Figure 0007586449000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a sealing structure whose interior is sealed, and a method for manufacturing the same. [Background technology]
[0002] For example, sealed structures (sealed structures) are used in a variety of fields, such as battery cases for secondary batteries in the automotive industry, control boxes for accommodating electronic components and circuit boards for control, housings for accommodating hydraulic components and control components, and sealed structures for heat exchangers such as heat sinks. Conventionally, sealing means have been used in which a sealing member is fastened with a bolt or pin via a sealing material such as a gasket or an O-ring, a mechanical means is used in which the sealing member is fastened to the housing by crimping, or a fusion joining means such as brazing or welding is used. These conventional methods require a large number of parts and steps, which results in problems in terms of weight and productivity. Furthermore, the process can be complicated, which can cause problems with the sealing quality (reliability). In the field of electronic equipment, a so-called packaging process is carried out in which a mounting board, various devices, elements, etc. are built in and hermetically sealed. In such fields, as a means of sealing and airtightness A sealing structure is required to seal the various parts, devices, electronic boards, etc. inside. These sealing structures are required to have excellent airtightness and watertightness as well as high strength and durability. In recent years, there has been a demand for smaller, thinner and lighter devices, as well as for cheaper and more productive manufacturing methods.
[0003] For example, Patent Document 1 discloses a battery case in which the opening of the tray that houses the battery is closed with a top cover that is bolted, and Patent Document 2 discloses a heat sink structure that is water-sealed with a packing material. These are mechanical sealing structures and are not high productivity assembly processes. In the field of electronic devices, for example, Patent Document 3 discloses a technology in which one side of a joint is gold-plated and the other side is tin-plated, and then a gold-tin alloy is formed by heating to seal the joint. However, this technology is expensive and has low productivity. In addition, sealing at low temperatures is difficult, and the material is not suitable for use in devices that are susceptible to heat damage. Patent Document 4 discloses a package structure including a substrate having a device disposed on its main surface, and a lid having a recess that opens toward the substrate and is disposed on the substrate so as to cover the device, and the joint is formed by a brazing material formed by plating or printing. Patent Document 5 discloses a sealing technology in which a metallized layer having a nickel or gold surface plating is formed on a ceramic case, a metal lid having a silver alloy or aluminum alloy film formed on one side is placed on top, and localized heating is performed using an electron beam; however, the process is complicated and productivity is low. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] Japanese Patent Publication No. 2021-41783 [Patent Document 2] Japanese Patent Application Publication No. 2006-296074 [Patent Document 3] Japanese Patent Publication No. 2017-85000 [Patent Document 4] Japanese Patent Publication No. 2004-202604 [Patent Document 5] Japanese Patent Publication No. 9-246415 Summary of the Invention [Problem to be solved by the invention]
[0005] An object of the present invention is to provide a sealing structure which has excellent bonding strength and reliability and can be bonded in a short time through a simple process, and a method for manufacturing the same. [Means for solving the problem]
[0006] The sealing structure of the present invention is a sealing structure for sealingly holding an internal structure or a component provided inside, and is characterized in that it comprises a case body and a sealing member sealed and joined to the case body by a sealing joint, the sealing joint being a diffusion joint between the same or dissimilar metals, and a plastic flow layer being formed in the diffusion joint. Here, the internal structure refers to sealing the inside of the case body obtained by pressing, casting, machining, etc., and the parts installed inside refers to sealing the opening of the case body in which a battery, electronic parts, functional parts, etc. are attached.
[0007] Conventionally, packing materials, brazing, welding, etc. have been used as a means for sealing and joining, but the present invention is characterized in that it uses a diffusion joining method that forms a plastic flow layer at the joint. The means for forming this plastic flow layer is a manufacturing method for a sealing structure for sealingly holding an internal structure or a part installed inside, in which the case body and the sealing member are superimposed and heated and pressurized to a level that does not create a liquid phase at the joint. For example, when joining similar metals such as aluminum-based materials, copper-based materials, or iron-based materials, applying pressure to the joint using a press or the like creates a plastic flow layer at the joint interface, removing contaminant layers such as oxide films that were present on the joining surfaces of the two materials, and joining the newly formed surfaces together, thereby increasing the joint strength.
[0008] Furthermore, when the sealing joint is made of dissimilar metals, a brittle intermetallic compound (IMC) is easily formed at the joint interface. For example, in the case of Fe-Al, it is generally known that if the thickness of this IMC exceeds 1 μm, the bonding strength decreases significantly. With fusion welding methods such as laser and arc welding, it is practically impossible to weld combinations of dissimilar materials that generate IMC. In contrast, the present invention involves heating to a relatively low temperature within a range in which no liquid phase is generated at the joint interface, and applying pressure in a short period of time using a press or the like in a direction that reduces the thickness of the overlapping portion between the case body and the sealing member. In this specification, this type of construction method is referred to as forge welding as necessary. As an index for evaluating the thickness reduction of the sealing joint, the total thickness of the metal on both sides of the pressurized joint before joining is defined as "T 0」 mm, and the total thickness of the metal on both sides after pressure bonding is "T 1」 mm, then "T0 / T 1」 The value of this is defined as the reduction ratio R. The larger the reduction ratio R, the easier it is for a plastic flow layer to form at the joining interface. The increase in plastic flow at the bond interface leads to an increase in the number of newly formed surfaces. This enables more efficient diffusion reactions, resulting in low-temperature, short-time bonding that suppresses the growth of intermetallic compounds. The applicant has previously filed an international application (PCT / JP2021 / 3018) for a method of joining metal materials by forge welding, which involves applying spot pressure. The present invention further develops this method, making it possible to form linear, planar, or frame-shaped joints by forge welding.
[0009] Examples of metal combinations suitable for forge welding include the following: Examples of alloys between the same metal include Al-Al, Cu-Cu, Fe-Fe, Mg-Mg, Ni-Ni, and Ti-Ti. Examples of dissimilar metals include Al-Fe, Al-Cu, Al-Ti, Al-Ni, and Al-Mg. The above metals also include their alloys.
[0010] The sealing structure of the present invention may have an insert layer made of metal between the case body and the sealing member, in which case the case body and the sealing member are bonded by heating and pressure with the insert layer made of metal between them. Alternatively, pressure bonding is also possible, in which the insert material is heated separately and the heat is used to ensure an appropriate bonding temperature at the bonding interface. Here, the insert layer (insert material) may be a so-called metal gasket, and if the case body and sealing member are not made of metal, for example, glass, ceramics, semiconductor substrates such as silicon, etc., a metal layer may be formed at the joint by plating, vapor deposition, etc. Effect of the Invention
[0011] The sealing structure according to the present invention has excellent joint strength and joint reliability because the joints are formed by forge welding. Such joints can be obtained using a versatile press or the like, and can be formed at relatively low temperatures and in a much shorter time than conventional welding or brazing, resulting in high productivity. In addition, the forge welding process according to the present invention can be easily incorporated into the process of press-forming the case body, etc. Furthermore, the use of auxiliary materials such as brazing material, welding rods, packing materials, and auxiliary equipment can also be reduced. [Brief description of the drawings]
[0012] [Figure 1] (a) shows an example of the component configuration of a sealing structure, and (b) shows the forge welding process. [Diagram 2] This shows an example in which the case body is made of a housing with flow channels formed inside. (a) shows an example of the part configuration, and (b) shows the forge welding process. [Diagram 3] Examples of packaging for electronic components are shown. (a) shows an example of the component configuration, and (b) shows the forge welding process. [Figure 4] (a) shows a cross-sectional photograph of the bonded interface of an Al-Al combination, and (b) shows a cross-sectional photograph of the bonded interface of an Fe-Al combination. BEST MODE FOR CARRYING OUT THEINVENTION
[0013] Examples of the sealing structure according to the present invention will be described below with reference to the drawings, but the present invention is not limited thereto.
[0014] FIG. 1 shows an example of a case body 11, which is a housing in which various components are arranged and attached. A flange portion 11a is formed along the entire circumference of the opening of the case body 11, and is forge-welded to the sealing member 12 at this portion. A sealing member 12 made of a plate-shaped metal material may be placed on the flange portion 11a of the case body 11 and directly sealed and joined, but the embodiment shown in Figure 1 is an example in which a metal gasket is used as an insert material 13, and this insert material 13 is sandwiched between the flange portion 11a and the sealing member 12 and forge-welded. As shown in FIG. 1(b), the overlapped flanges are preheated and pressed with a press or the like using upper and lower pressure jigs so that the reduction ratio becomes R=1.3 or more.
[0015] FIG. 2 shows an example in which a case body 11 is a heat exchange part such as a heat sink having a flow passage groove formed therein, and the opening is forge-welded to a sealing member 12. Although the present embodiment is also an example in which the insert material 13 is interposed, the insert material does not necessarily have to be used depending on the combination of metal materials. Figure 2(b) shows the flow of press welding. In this case, the reduction ratio is evaluated based on the change in thickness of the part where the thickness is substantially reduced. The reduction in thickness is due to plastic flow.
[0016] FIG. 3 shows an example of packaging electronic components by stacking two or more layers of substrates. In the configuration example shown in FIG. 3, a metal layer 14a is formed on the sealing joint of the ceramic plate 14 by plating or vapor deposition. This is an example in which a substrate 15 made of a silicon substrate is packaged between this and a sealing member 16 made of a glass plate. A frame-shaped metal layer 15a is plated or vapor-deposited on the front and back surfaces of the substrate 15. On the opposing surface of the sealing member 16, a metal layer 16a is formed in a frame shape. An insert material 13 made of a metal gasket is disposed between the ceramic plate 14 and the substrate 15, and between the substrate 15 and a sealing member 16 made of a glass plate. The constituent substrates may be, for example, silicon, glass, ceramic, aluminum, iron, Kovar, nickel, copper, magnesium, etc., and may be selected without limitation from among these as long as they are strong enough to withstand the forge welding process and preferably form a plastic flow layer at the joint. In addition, by appropriately designing the metal patterns of, for example, ceramic substrates that are laminated in multiple layers, it is also possible to realize electrical conduction between the substrates. The flow of forge welding is shown in Figure 3(b). When the sealed joint is heated to a predetermined temperature and pressurized with a press or the like, a plastic flow layer is formed in the joint, completing the sealing joint.
[0017] FIG. 4 shows an example of a cross-sectional photograph of a sealed joint obtained by forge welding according to the present invention. In Figure 4(a), the flange part of the case body is made of an aluminum alloy consisting of AA6061, an Al-Mg-Si alloy, and aluminum sheets of AA2024, an Al-Cu alloy, are overlapped and pressed in a press so that the reduction ratio R becomes approximately 2 while the joint is heated (preheated) to approximately 350°C. A cross-sectional photograph of the Al / Al bonded interface is shown in Figure 4(a). Since the main elements are the same, no reaction layer like IMC was observed, and a highly crystalline joint interface was formed with the contaminated layer removed. Figure 4(b) shows an example of forge welding of an Al-Mg aluminum alloy AA5083 and a high-tensile steel plate SPFC980, which is an iron-based material, in the same manner as above. Here, the preheating temperature is about 420℃. The mixture was pressed with a press so that the reduction ratio R was about 2.6. The IMC had a bonding interface thickness of about several nm. It was a high-quality bonding interface that was much thinner than 1 μm, was uniform, and there was no risk of a decrease in strength. [Industrial Applicability]
[0018] The present invention relates to a sealing structure that requires sealing the inside, and can be applied to many industrial fields, including automobiles and electronic devices. [Explanation of symbols]
[0019] 11 Case body 12 Sealing member 13 Insert material (insert layer)
Claims
[Claim 1] A method for manufacturing a sealing structure for hermetically holding an internal structure or a component provided therein, comprising the steps of: The sealing member is formed by overlapping an opening of the case body with the sealing member and applying pressure to the sealing member, the sealing member being a diffusion bonding portion between the same or different metals, and a plastic flow layer being formed in the diffusion bonding portion, The sealing joint is a diffusion joint at a new surface that appears due to plastic flow between the same metals, or a diffusion joint where an intermetallic compound formed at a joint interface between dissimilar metals has a thickness of 1 μm or less, A method for manufacturing a sealing structure, characterized in that the case body and the sealing member are heated in a superposed state within a range in which a liquid phase is not generated at the joint, and the overlapping portion between the case body and the sealing member is pressurized so that a reduction ratio R is 1.3 or more, thereby pressure bonding the case body and the sealing member.
Citation Information
Patent Citations
Package for electronic part
JP1997246415A
Manufacture of aluminum case for battery
JP2000011964A
Electronic component package, lid material thereof, and manufacture thereof
JP2000164746A
Friction stir welding method and part welded by the method
JP2004042117A
Package structure and manufacturing method
JP2004202604A