Rubber molding die, molding method using same, and rubber molded product

The rubber molding mold with intentional burr grooves addresses chip and burr issues, extending mold life and improving efficiency by preventing burr-related damage and reducing material costs.

JP7586859B2Active Publication Date: 2024-11-19MITSUBISHI CABLE INDUSTRIES LTD
View PDF 12 Cites 0 Cited by

Patent Information

Application Number
JP2022107094
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-07-01
Publication Date
2024-11-19
Estimated Expiration
2042-07-01

AI Technical Summary

Technical Problem

Conventional rubber molding dies suffer from chip and burr formation on the cutting edge, which affects product functionality and requires high-strength, expensive materials and increased mold area, leading to decreased efficiency and increased costs.

Method used

The rubber molding mold design incorporates burr grooves on the periphery of the mating surfaces of the upper and lower molds, with dimensions smaller than the required burr finish, allowing for intentional burr formation that does not affect product quality and eliminates the need for burr treatment.

Benefits of technology

This design extends the life of the mold, maintains product quality, and enhances manufacturing efficiency by preventing burrs from becoming starting points for damage, while reducing material costs and mold complexity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007586859000001
    Figure 0007586859000001
  • Figure 0007586859000002
    Figure 0007586859000002
  • Figure 0007586859000003
    Figure 0007586859000003
Patent Text Reader

Abstract

To achieve longevity of a rubber molding die 1 and to eliminate product function deterioration factors.SOLUTION: A rubber molding die includes: an upper die 2 having an upper side molding groove 4a for molding at least one rubber molding 20 and an upper side clearance groove 8a to which an excess rubber from the upper side molding groove 4a flows in; and a lower die 3 having a lower side molding groove 4b for molding at least one rubber molding 20 at a position opposed to the upper side molding groove 4a and a lower side clearance groove 8b to which an excess rubber from the lower side molding groove 4b flows in. A burr groove 11 for intentionally forming a burr part 21 is formed over the whole periphery at at least one of a circumference 5 of the upper side molding groove 4a and the lower side molding groove 4b between the upper side molding groove 4a and the upper side clearance groove 8a and between the lower side molding groove 4b and the lower side clearance groove 8b.SELECTED DRAWING: Figure 1A
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a rubber molding die, a molding method using the same, and a rubber molded product. [Background technology]

[0002] It is known that rubber products are conventionally molded by sandwiching raw rubber 110 between upper mold 102 and lower mold 103 of mold 101 and vulcanizing the rubber by heat and pressure, as shown in Fig. 4 (see, for example, Patent Document 1). Upper mold 102 and lower mold 103 undergo a high-temperature, high-pressure vulcanization process during one molding cycle, which lasts from several minutes to several tens of minutes. [Prior art documents] [Patent documents]

[0003] [Patent Document 1] JP 2000-153534 A Summary of the Invention [Problem to be solved by the invention]

[0004] However, in a conventional rubber molding die 101, as shown in an enlarged view in Figure 4, repeated molding causes chips and burrs 107 to form on the end (periphery 105) of the product groove 104 and on the peripheral edge (also called the cutting edge) of the mating part 106 of the upper die 102 and the lower die 103.

[0005] The occurrence of such chips and burrs 107 affects the product functions, and therefore requires the renewal of the mold 101. For example, in rubber products such as piston packings that are stretched and fitted into mounting grooves, burrs 107 are likely to become the starting point of product damage.

[0006] On the other hand, measures to extend the life of the mold include using a high-strength mold material such as a heat-treated material, or increasing the distance L2 (land) between the product groove 204 and the escape groove 208 to increase the pressure-receiving area, as shown in the mold 201 in Figure 5.

[0007] However, high-strength mold materials have disadvantages, such as being expensive and difficult to process, and if the distance L2 is increased, the area required for one product becomes larger, reducing the number of products that can be made per mold.

[0008] The present invention has been made in view of the above-mentioned points, and an object of the present invention is to extend the life of rubber molding dies and to eliminate factors that deteriorate the functionality of products. [Means for solving the problem]

[0009] In order to achieve the above object, in this invention, the peripheral edge (cutting edge) of the mating portion between the upper and lower dies is provided on the burr portion that is not related to the product.

[0010] Specifically, in the first invention, an upper mold has an upper molding groove for molding at least one rubber molded product and an upper escape groove into which excess rubber from the upper molding groove flows; a lower mold having a lower molding groove for molding the at least one rubber molded product at a position opposite to the upper molding groove and a lower escape groove into which excess rubber from the lower molding groove flows, A burr groove is formed around the entire periphery of at least one of the upper molding groove and the lower molding groove between the upper molding groove and the upper escape groove and between the lower molding groove and the lower escape groove, for intentionally forming a burr portion.

[0011] According to the above configuration, even if chips or burrs form on the sharp portions (also called cutting edges) of the upper and lower dies that form the periphery of the mating surface of the upper and lower dies due to deterioration over time, these portions correspond to the burrs, so no starting point for damage to the product when pulled or the like is generated, and the quality of the product is not affected.

[0012] In the second invention, in the first invention, The width and depth of the burr groove are both smaller than the size of the burr portion of the rubber molded product that requires burr removal.

[0013] According to the above configuration, the width of the burr groove is smaller than the width of the burr portion of the rubber molded product that requires burr finishing, and the depth of the burr groove is smaller than the thickness of the burr portion of the rubber molded product that requires burr finishing, so there is no need to process the burr portion that is intentionally formed around the entire circumference, resulting in high manufacturing efficiency.

[0014] In the third invention, in the second invention, The rubber molded product is an O-ring, The width and depth of the burr groove are both smaller than the size of the burr portion that requires burr removal, as specified in JIS B 2401-3.

[0015] According to the above-mentioned configuration, there is no need to treat any intentionally formed burrs that extend around the entire circumference of the O-ring, and therefore manufacturing efficiency is high.

[0016] In a fourth aspect of the present invention, in the first aspect of the present invention, The width and depth of the burr groove are both 0.02 mm or more and 0.1 mm or less.

[0017] It is difficult to machine a groove shallower than 0.02 mm in a mold, and burrs larger than 0.1 mm require burr removal. However, the above-mentioned configuration makes it possible to obtain a rubber molded product that does not require burr removal, has a burr that is as thin in width and thickness as possible, and achieves a longer life and elimination of factors that reduce product functionality.

[0018] The fifth invention is directed to a method for molding rubber using any one of the first to fourth rubber molding dies, and in this method, The rubber molding mold is prepared, a raw rubber arranging step of arranging preformed raw rubber between the upper molding groove and the lower molding groove; a mold closing process in which the upper mold and the lower mold are closed to allow excess rubber to escape into at least one of the upper escape groove and the lower escape groove, while also pouring the excess rubber into a flash groove provided on a periphery of at least one of the upper molding groove and the lower molding groove; a vulcanization step of vulcanizing the mixture by heating while applying pressure after the mold closing step; After the vulcanization step, a demolding step is performed to remove the rubber product.

[0019] With the above configuration, even if chips or burrs form on the cutting edge of the upper or lower die, which is the periphery of the mating surface of the upper and lower dies, due to deterioration over time, these parts correspond to burrs, so they do not affect the quality of the product. In addition, since the burrs are intentionally formed, there is no need to remove them, making production easy.

[0020] The rubber molded product of the sixth invention is A burr portion having a width and thickness smaller than that of a burr portion requiring burr finishing is formed around the entire circumference of the inner and outer periphery of a ring-shaped rubber molded product in the thickness direction central portion.

[0021] According to the above-mentioned configuration, it is possible to obtain a ring-shaped rubber molded product having flash intentionally formed on the inner and outer peripheries, which allows the mold to be used for a long period of time, is easy to manufacture, and has a long life. Effect of the Invention

[0022] As described above, according to the present invention, by intentionally forming a flash portion around the entire periphery of the rubber molded product, which can absorb mold defects, it is possible to both extend the life of the rubber molding mold and eliminate factors that reduce product functionality. [Brief description of the drawings]

[0023] [Figure 1A] 3 is an enlarged cross-sectional view of a rubber molding die taken along line IB-IB in FIG. 2. [Figure 1B] FIG. [Diagram 2] FIG. [Diagram 3] FIG. 2 is a perspective view showing a rubber molded product placed on a lower die in a broken state. [Figure 4] FIG. 1 is a cross-sectional view showing a conventional mold. [Diagram 5] FIG. 11 is a cross-sectional view showing another conventional mold. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0024] Hereinafter, an embodiment of the present invention will be described with reference to the drawings.

[0025] 1A to 2 show a rubber molding die 1 according to a first embodiment of the present invention, which includes an upper mold 2 having an upper molding groove 4a for molding at least one rubber molded product 20, and an upper escape groove 8a into which excess rubber from the upper molding groove 4a flows.

[0026] Similarly, the rubber molding die 1 is equipped with a lower die 3 having a lower molding groove 4b for molding at least one rubber molded product at a position opposite the upper molding groove 4a, and a lower escape groove 8b into which excess rubber from the lower molding groove 4b flows, as shown in Figure 3, for example.

[0027] For example, the material of the upper mold 2 and the lower mold 3 may be NAK55, which is a high-strength prehardened steel, or may be high-carbon steel 55c, which is a normal strength. Furthermore, the raw rubber that is the molding material is not particularly limited, and may be an additive.

[0028] In the figure, for simplicity, one mold is provided with only an upper molding groove 4a and a lower molding groove 4b for producing one rubber molded product 20, but two or more grooves may be provided.

[0029] A burr groove 11 for intentionally forming a burr portion 21 is formed around the entire periphery 5 of at least one of the upper molding groove 4a and the lower molding groove 4b between the upper molding groove 4a and the upper escape groove 8a and between the lower molding groove 4b and the lower escape groove 8b.

[0030] In this embodiment, as shown in the figure, the burr groove 11 is provided only around the entire inner and outer periphery of the lower molding groove 4b, but conversely, it may be provided only on the upper molding groove 4a side, or on both the lower molding groove 4b and the upper molding groove 4a.

[0031] As shown in FIG. 3, a rubber molded product 20 of this embodiment is, for example, an O-ring for piston packing, and a flash portion 21 having a width W and a thickness T smaller than the width and thickness of a flash portion that requires flash finishing is formed around the entire circumference in the thickness-wise central portion of the inner and outer circumferences of the ring-shaped rubber molded product 20.

[0032] For this reason, the width W and depth T of the burr groove 11 are smaller than the width and thickness of the burr portion of the rubber molded product that requires burr finishing. Specifically, when the rubber molded product 20 is an O-ring as shown in Fig. 3, the width W and thickness T of the burr portion 21 (for simplification, these are assumed to be the same as the width W and depth T of the burr groove 11, respectively) are made smaller than the size that requires burr finishing, as specified in JIS B 2401-3. For this reason, for example, the width W and depth T of the burr groove 11 are both 0.02 mm or more and 0.1 mm or less.

[0033] -Rubber molding method- Next, a rubber molding method using the rubber molding die 1 according to this embodiment will be described.

[0034] First, prepare a press machine including the above-mentioned rubber molding die 1. The configuration of the press machine itself is not particularly limited.

[0035] Next, in the raw rubber placement step, an appropriate amount of preformed raw rubber is placed between the upper molding groove 4a and the lower molding groove 4b.

[0036] Next, in the mold closing step, the upper mold 2 and the lower mold 3 are closed and the excess rubber is allowed to escape into the upper escape groove 8a and the lower escape groove 8b while also flowing into the flash groove 11 provided on the periphery 5 of the lower molding groove 4b.

[0037] Next, in the vulcanization step, the mixture is vulcanized by heating while applying pressure. The mixture is pressed at a predetermined pressure for several minutes to several tens of minutes. The vulcanization conditions are not particularly limited.

[0038] After the vulcanization step, the rubber molded article 20 is taken out. At this time, small flash portions 21 are formed all over the inner and outer peripheries of the ring-shaped rubber molded article 20, as shown in FIG.

[0039] The burr portion 21 formed in this burr groove 11 has a width W and a depth T of, for example, 0.02 mm or more and 0.1 mm or less, which is smaller than the size specified in JIS B 2401-3, and therefore does not need to be removed.

[0040] Here, it is difficult to form a groove shallower than 0.02 mm in the rubber molding die 1 by machining, and burrs larger than 0.1 mm require burr removal. However, in this embodiment, a rubber molded product 20 is obtained in which a burr 21 with a width W and thickness T as thin as possible is formed, while eliminating the need for burr removal.

[0041] Of course, the flash portion 21 may be removed in the usual manner.

[0042] In this way, even if chips or burrs form due to aging on the cutting edges of the upper die 2 or the lower die 3, which form the periphery of the mating surface between the upper die 2 and the lower die 3, this does not affect the quality of the product, since this portion corresponds to the burr portion 21. In other words, even if there are chips or burrs in the burr portion 21, they will not become the starting point for stretching and breaking of the rubber molded product 20 when the rubber molded product 20 is pulled.

[0043] Furthermore, since there is no need to remove the intentionally molded flash 21, the manufacturing efficiency is high and the manufacturing process is easy.

[0044] In this embodiment, flash portions 21 are intentionally formed on the inner and outer periphery of the rubber molding die 1, allowing the rubber molding die 1 to be used for a long time, and a high-quality ring-shaped rubber molded product 20 that is easy to manufacture is obtained.

[0045] Therefore, according to this embodiment, by intentionally forming a flash portion 21 around the entire periphery 5 of the rubber molded product 20, which can absorb defects in the mold 1, it is possible to achieve both a longer life for the rubber molding mold 1 and elimination of factors that reduce product functionality.

[0046] (Other embodiments) The present invention may be configured as follows with respect to the above embodiment.

[0047] That is, in the above embodiment, the burr groove 11 is provided only on the periphery of the lower molding groove 4b, but it may also be provided on the upper molding groove 4a. In that case, it is sufficient that the width W of the burr groove 11 on both sides is a predetermined value and the sum of the depths T is within a predetermined range.

[0048] In addition, in the above embodiment, the rubber molded product 20 is an O-ring for piston packing, but this is not limited to this, and in some cases the present invention may also be applied to a mold for a resin molded product.

[0049] It should be noted that the above-described embodiments are essentially preferred examples, and are not intended to limit the scope of the present invention, its applications, or uses. [Explanation of symbols]

[0050] 1 Rubber molding mold 2 Upper mold 3 Lower mold 4a Upper molding groove 4b Lower molding groove 5 Periphery 8a Upper undercut 8b Lower undercut 11 Burr groove 20 Rubber molded products 21 Bali Club

Claims

1. an upper mold having an upper molding groove for molding at least one rubber molded product and an upper escape groove into which excess rubber from the upper molding groove flows; a lower mold having a lower molding groove for molding the at least one rubber molded product at a position opposite to the upper molding groove and a lower escape groove into which excess rubber from the lower molding groove flows, a burr groove for intentionally forming a burr portion is formed around the entire periphery of at least one of the upper molding groove and the lower molding groove between the upper molding groove and the upper relief groove and between the lower molding groove and the lower relief groove, The width and depth of the burr groove are both smaller than the size of the burr portion of the rubber molded product that requires burr removal. A rubber molding mold comprising:

2. the rubber molded product is an O-ring, The width and depth of the burr groove are both smaller than the size of the burr portion that requires burr removal as specified in JIS B 2401-3.

2. The rubber molding mold according to claim 1.

3. The width and depth of the burr groove are both 0.02 mm or more and 0.1 mm or less.

2. The rubber molding mold according to claim 1.

4. A method for molding rubber using the rubber molding mold according to any one of claims 1 to 3, comprising the steps of: The rubber molding mold is prepared, a raw rubber arranging step of arranging preformed raw rubber between the upper molding groove and the lower molding groove; a mold closing process in which the upper mold and the lower mold are closed to allow excess rubber to escape into at least one of the upper escape groove and the lower escape groove, while also pouring the excess rubber into a flash groove provided on a periphery of at least one of the upper molding groove and the lower molding groove; a vulcanization step of vulcanizing the mixture by heating while applying pressure after the mold closing step; After the vulcanization step, a demolding step is performed to remove the rubber product. A method for molding rubber comprising the steps of:

5. A burr of a constant width and thickness, smaller than the width and thickness of a burr that requires burr finishing, is formed continuously around the entire thickness center of the inner and outer circumferences of a ring-shaped rubber molded product. A rubber molded product characterized by:

Citation Information

Patent Citations

  • JP1986128011U

  • Deburring molding method of composite rubber molding and mold thereof

    JP1997117919A

  • Mold

    JP1998296760A

  • Molding die for rubber or resin

    JP2000153534A

  • Molding die

    JP2000190331A