A high carbon steel joint pin with decarburized tip and uniform body hardness addresses the durability issues of conventional pins by ensuring crack-free caulking and improved chain strength.
Patent Information
- Application Number
- JP2024013518
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2024-01-31
- Publication Date
- 2024-11-20
- Estimated Expiration
- 2039-04-16
AI Technical Summary
Conventional joint pins for roller chains suffer from low durability due to low hardness in the caulked parts, leading to potential cracking and deformation, especially when made of high carbon steel with surface hardening prevention treatments.
A joint pin made of high carbon steel with a carbon content of 0.5 to 0.6% is used, with the tip portion decarburized to reduce carbon content and hardness to 500 to 650 HV, while the body maintains 550 to 750 HV, featuring a cutting portion and counterbore hole for accurate caulking without cracks.
The joint pin achieves high strength and wear resistance, preventing cracking and deformation during caulking, enhancing the tensile strength and durability of the chain connection.
Smart Images

Figure 0007587720000001 
Figure 0007587720000002 
Figure 0007587720000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a joint pin for connecting chains such as roller chains. N Regarding. [Background technology]
[0002] Generally, when the number of links of a roller chain used to drive a motorcycle stretches with use and needs to be adjusted, or when the roller chain that was being used has worn out and become unusable, the old chain is cut and the number of links is adjusted, and then the old chain or a new roller chain is replaced, and the chain is wound around the drive sprocket and driven sprocket and then connected in an endless manner by coupling links.
[0003] As shown in Figure 3, the joint link 1 has a foot plate 4 with joint pins 3, 3 erected at both ends of the joint plate 2, and one outer plate 5, and the joint pins 3 of the foot plate 4 are inserted into bushings 7, 7 at both ends of a roller chain 6 having ends, and protrude from pin holes in the outer plate 5 arranged to connect the ends of the roller chain 6, and the tips of the protruding pins 3, 3 are crimped to connect the roller chain 6 in an endless manner.
[0004] Conventionally, the joint pin 3 is made of the same carburized steel as the chain body, and holes are formed in the crimped portion to facilitate deformation during crimping. In addition, the pin is heat treated by the same carburized hardening process as the pins of the chain body. Therefore, the area near the crimped portion of the joint pin is pretreated with copper plating or other pretreatment to prevent carburization, i.e., surface hardening prevention treatment, before carburizing and hardening. This gives the area near the crimped portion a lower hardness level than other areas, making it easier to deform.
[0005] The joint pin 3 is subjected to a punching process with a mountain-shaped end face to crimp the end face of the crimped portion of the joint pin 3. However, since the hardness of the crimped portion (the crimped portion) is set to a low value, it can be easily deformed and crimped.
[0006] However, the crimped portion of the above-mentioned joint pin has low hardness because no carburizing treatment is performed on the chain body and any parts other than the crimped portion of the joint pin. As a result, the strength of only the crimped portion of the pin of the joint link is reduced, reducing the durability of the joint pin.
[0007] In addition, when high carbon steel is used for the above-mentioned joint pin 3, even if the part to be crimped is copper plated to prevent carburizing and hardening, the joint pin itself contains a high amount of carbon and has high hardness, so that defects such as cracks may occur at the tip of the pin during the crimping process.
[0008] Therefore, it has been proposed to make the structural material of the joint pins of the joint links from the same high-tensile steel as the pins used in the chain body, that is, steel with 0.3% or more carbon and various alloy elements added, and to form a specified hole in the crimped part of the joint pin material made of this high-tensile steel, and to subject the entire joint pin material including the crimped part to quenching other than surface hardening, such as austempering, to obtain a joint pin with a uniform hardness of HRC45 or more on the inner and outer surfaces (Patent Document 1). [Prior art documents] [Patent documents]
[0009] [Patent Document 1] Japanese Patent Application Publication No. 52-6860 Summary of the Invention [Problem to be solved by the invention]
[0010] The joint pin of Patent Document 1 mentioned above has a predetermined hardness as a whole pin, so although the strength of the joint pin can be maintained, the crimped portion also has the same hardness. Therefore, even if the tip of the pin is crimped using a truncated cone-shaped punch, cracks or the like may occur in the crimped portion of the pin, which may cause issues with the durability of the joint link.
[0011] The present invention provides a joint pin for a chain that can obtain high hardness by using a joint pin made of high carbon steel, while preventing the occurrence of crimp cracks by decarburizing the crimped portion. N The purpose of this document is to provide [Means for solving the problem]
[0012] The present invention relates to a joint pin (13) for a chain that connects both ends of an end-connected chain to make it endless, The joint pin (13) A tip surface in an axial direction; Tip surface was formed in Crimping holes(19) and a tip portion (B) having , The body portion (A) other than the tip portion (B), The body portion (A) is made of carbon steel having a carbon content of 0.5 to 0.6% at the radial center and outer periphery, and has a uniform hardness of 550 to 750 [HV] throughout. The tip portion (B) has a carbon content uniformly reduced throughout the thickness direction so that the hardness is 500 to 650 [HV], The carbon content of the tip portion (B) is lower than the carbon content of the body portion (A), The hardness of the tip portion (B) is lower than the hardness of the body portion (A); The present invention relates to a joint pin of a chain.
[0013] The joint pin (13) has a cutting portion (20) on its outer peripheral surface at its tip portion (B).
[0014] The cutting portion (20) has a shallow groove or reduced diameter portion (20a).
[0018] The reference characters in parentheses are for the purpose of comparison with the drawings, and do not in any way affect the description of the claims. Effect of the Invention
[0019] The tip of the joint pin has a hardness of 500 to 650 HV, which is lower than the other parts, so that even if a jig is inserted into the hole at the tip surface of the pin and the pin is crimped properly without cracking. Furthermore, the joint pin at the part that connects the two outer links is made of high carbon steel with a hardness of 550 to 750 HV containing 0.5 to 0.6% carbon, and has high strength and wear resistance. This prevents the joint pin from falling off or deforming due to poor crimping of the chain connected by the joint pin, and also improves the tensile strength and durability of the chain.
[0020] If the outer peripheral surface of the tip of the joint pin has a cut portion, it becomes easier to insert the joint pin into the pin hole of the outer plate, and the streaks of the cut portion ensure that the joint pin can be fitted into the pin hole by crimping.
[0021] Forming a shallow groove or a small diameter portion in the cut portion, coupled with the reduction in hardness, makes it possible to easily and accurately crimp the joint pin. [Brief description of the drawings]
[0025] [Figure 1] 3A and 3B show a coupling link according to the present invention, in which FIG. 3A is a plan view and FIG. [Diagram 2] 5A to 5C are diagrams showing a manufacturing method of a joint pin according to the present invention. [Diagram 3] FIG. 4 is a plan view showing a connection of roller chains by a coupling link. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0026] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. As shown in FIG. 1, the joint link 11 has a rising plate 14 and one outer plate 15. The rising plate 14 is formed by pressing and fixing joint pins 13, 13 to both ends of a joint plate 12 consisting of one outer plate, and a countersunk hole 19 is formed from the tip surface of the pin 13, and the outer peripheral surface of the tip portion of the pin is formed by a cut portion 20, and it is preferable that a shallow recessed groove 20a or a small diameter portion is formed in the cut portion 20. In the joint link 11, with the outer plate 15 arranged so as to be connected to both ends of the roller chain having ends, both joint pins 13, 13 of the rising plate 14 are inserted into bushes at both ends of the roller chain and protrude from the pin holes of the outer plate 15, and a truncated cone-shaped punch is inserted into the countersunk hole 19 at the tip of the protruding pin and crimped (22), whereby the roller chain is connected in an endless manner. The crimping 22 has a relatively low hardness, and combined with the presence of the countersunk hole 19, it can be performed accurately without causing damage such as cracks. A seal ring 21 is fitted onto the joint link 11 adjacent to the joint plate 12 and outer plate 15 so as to surround the joint pin 13.
[0027] The joint pin 13 is made of high carbon steel containing 0.5 to 0.6% carbon C, and has a Vickers hardness of 550 to 750 [HV]. The portion A of the joint pin 13 other than the tip portion B to be crimped has a hardness of 550 to 750 [HV], which is the hardness of the joint pin material, but the hardness of the tip portion B where the cutting portion 20 is located is reduced to 500 to 650 [HV] by a decarburization treatment described later.
[0028] Next, the manufacturing method of the above-mentioned joint pin will be described with reference to FIG. 2. As described above, the material of the joint pin 13 is made of 550-750 [HV] steel material with a carbon content of 0.5-0.6%, and as shown in (a), a plating process is performed to apply copper plating D to the entire pin material (plating process). The plating process is to prevent decarburization, which will be described later, and copper plating is preferable, but other plating may also be used. The tip of the pin material with the copper plating D is cut (cutting process) as shown in (b) (cutting process). In the cutting process, the copper plating D on the outer peripheral surface of the pin tip is cut and removed by a cutting tool 24, and the cut part 20 is formed where the surface of the pin material is exposed. At this time, a shallow groove 20a or a slight small diameter part may be formed in the cut part 20 by cutting. Furthermore, a countersunk hole 19 with a predetermined depth and a predetermined spread is formed from the pin tip surface by a drill 23. In the cutting process, it is preferable to remove the copper plating from the pin tip surface as well. Moreover, the cut portion 20 on the outer peripheral surface of the tip portion of the pin from which the copper plating has been removed and the countersunk hole 19 portion have approximately the same length (depth).
[0029] In this state, as shown in (c), a decarburization process such as heat treatment in an oxygen environment is performed (decarburization process). The decarburization process is performed only on the cutting portion 20 of the outer peripheral surface of the pin tip from which the copper plating has been removed, and then normal heat treatment such as quenching and annealing is performed. As a result, carbon is bonded to oxygen and emitted from the cutting portion 20, and the decarburized carbon is diffused from the inner portion between the countersunk hole 19 by the normal heat treatment, and the carbon content of the pin tip (see B in FIG. 1(b)) is uniformly reduced throughout the thickness direction, and the hardness is reduced by a predetermined amount (500 to 650 [HV]). Note that the portion other than the pin tip where the copper plating D is present (see A in FIG. 1(b)) is not decarburized on the surface, so the carbon content is maintained as it is (0.5 to 0.6% C) and the heat treatment is performed in that state, and a uniform hardness is maintained throughout (550 to 750 [HV]).
[0030] Then, as shown in (d), a grinding process is carried out in which the entire surface of the pin material is ground by a grindstone 25 (grinding step), and the copper plating D is peeled off from the entire pin, completing the production of the joint pin 13.
[0031] The tip of the joint pin 13 has a reduced carbon content due to the decarburization process, and is therefore lower in hardness than the other portion A that is not crimped. When connecting a roller chain, a punch is inserted into the countersunk hole 19 at the tip of the joint pin 13 to crimp it, but the crimped portion has a low hardness (550 to 650 [HV]), so it can be crimped properly and reliably without cracks. At this time, the cut portion 20 has a slightly smaller diameter, making it easier to insert it into the pin hole of the outer plate 15, and the streaks of the cut portion 20 bite into the inner peripheral surface of the pin hole by crimping, so that it is reliably fitted and fixed. Furthermore, if a groove 20a or a small diameter portion is formed in the cut portion 20 by cutting, crimping can be performed more accurately and easily. The main body portion A of the joint pin 13, which connects the left and right outer plates 14, 15, is made of high carbon steel that has not been decarburized and has a uniform high hardness (550 to 750 [HV]) with high strength and durability. This improves the tensile strength of the roller chain connected by the joint pin, making it suitable for use in motorcycles with high engine displacements.
[0032] Although the joint pin 13 is generally used as the pin of the rising plate 14, it is also possible to use the pin alone as a joint pin. In this case, since both ends of the joint pin are crimped, the copper plating on both ends of the joint pin is cut and removed, and the hardness is reduced by decarburization treatment. Also, this joint pin is suitable as a joint pin for roller chains, but is not limited to this and can be similarly applied to other chains such as bushing chains and silent chains. [Explanation of symbols]
[0033] 11 Connecting link 13 Joint pin 14 Rising plate 19 (countersunk) holes 20 Cutting part 20a Groove or small diameter portion D Copper plating
Claims
1. In a chain joint pin that connects both ends of an endless chain, a tip portion having a tip surface in an axial direction of the joint pin and a crimping hole formed in the tip surface; A body portion other than the tip portion, The body portion is made of carbon steel having a carbon content of 0.5 to 0.6% at the radial center and outer periphery, and has a uniform hardness of 550 to 750 HV throughout. The tip portion has a carbon content that is uniformly reduced throughout the thickness direction so that the tip portion has a hardness of 500 to 650 [HV], The carbon content of the tip portion is lower than the carbon content of the body portion, The hardness of the tip portion is lower than the hardness of the body portion. A chain joint pin comprising:
2. The joint pin has a cutting portion on its outer peripheral surface at its tip. A joint pin for a chain according to claim 1.
3. The cutting portion has a shallow groove or a small diameter portion. A joint pin for a chain according to claim 2.
Citation Information
Patent Citations
Coupling pin for the repair coupling link in a twoowheeler
JP1977006860A
Link plate slip-off preventing process method for connecting pin in friction transmitting chain and device therefor