Bipolar Plates for Fuel Cell Stacks
Reinforcing the bipolar plate material in areas facing apertures with additional thickness or materials addresses the issue of damage from ice and pressure, enhancing durability and longevity.
Patent Information
- Application Number
- JP2023562530
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-04-21
- Filing Date
- 2022-04-19
- Publication Date
- 2024-11-21
- Estimated Expiration
- 2042-04-19
AI Technical Summary
Bipolar plates in fuel cells are prone to damage due to ice formation and pressure differentials, leading to cracks and potential destruction.
Reinforcing the material of the bipolar plate in areas facing apertures with a greater material thickness or additional reinforcing materials, such as fibers, to enhance mechanical strength and prevent damage.
The reinforcement significantly increases the service life of the bipolar plate by preventing cracks and damage, while maintaining efficient coolant flow.
Smart Images

Figure 0007588251000001 
Figure 0007588251000002 
Figure 0007588251000003
Abstract
Description
[Technical field]
[0001] The invention relates to a bipolar plate for a fuel cell stack comprising two layers according to the type more particularly defined in the preamble of claim 1. [Background technology]
[0002] Bipolar plates for fuel cells are known in principle from the general prior art. They are used in the fuel cells, on the one hand, for the electrical contact of the electrodes of the fuel cell and, on the other hand, for the supply and removal of media to and from the fuel cell. They also typically contain coolant flow fields for the combined cooling of the fuel cell stack.
[0003] In general, bipolar plates are known, for example from DE 199 1 02 13 56 A1. There, two layers or halves are combined into an actual bipolar plate. The medium is fed into the plate via a medium inlet and a medium outlet. In this connection, passages are formed between both layers, by means of which the medium is guided, so to speak, into the interior of the bipolar plate. From there, the medium reaches the corresponding flow areas for the medium on the cathode and anode sides of the bipolar plate from the interior of the bipolar plate via openings, also called backfeed slots or backfeed channels. The coolant flow typically still takes place inside the bipolar plate, so that the openings are only formed in one half towards the anode side flow area and in the other half towards the cathode side flow area. [Patent Document 1] WO 2008 / 061094 A1
[0004] Equivalent structures which also use this technology are known from US Pat. No. 5,393,633, US Pat. No. 5,493,663, US Pat. No. 5,529,471 and US Pat. No. 5,613,666. [Patent Document 2] WO 03 / 083979 A2 [Patent Document 3] WO 2015 / 145233 A1 [Patent Document 4] US 9,105,883 B2 [Patent Document 5] US 2007 / 0117001 A1
[0005] Regarding further prior art, reference may also be made to US Pat. No. 5,399,633. [Patent Document 6] US 8,927,170 B2
[0006] This structure has now been demonstrated in principle in practice. However, it has also been shown that in some circumstances it is highly susceptible to failures: if ice forms, for example in the region of the openings, the freezing water expands its volume accordingly and presses so hard against the material of the half or layer of the bipolar plate adjacent to the openings that damage to the adjacent bipolar plate can occur up to its destruction. In the worst case scenario, cracks form here, which destroy the bipolar plate. Also, in the case of particularly strong pressure differences in these regions, cracks can appear in the underlying material of the bipolar plate in the abovementioned regions if pressure propagates through the openings and the opposite sides of the adjacent layers of the bipolar plate are damaged in the event of an extreme pressure event. Summary of the Invention [Problem to be solved by the invention]
[0007] The object of the invention is therefore to provide an improved bipolar plate. [Means for solving the problem]
[0008] According to the invention, this problem is solved by a bipolar plate having the features of claim 1. Advantageous configurations and variants are evident from the dependent claims which depend thereon.
[0009] The bipolar plate according to the invention, like the bipolar plates described in the prior art cited at the outset, is composed of two layers with a connection between the flow field and the interior of the bipolar plate via suitable openings. Here, according to the invention, the material of each layer of the bipolar plate is reinforced in the area facing the openings of the other layer. It was clear to the inventor that in practice, cracks or even damage to the bipolar plate due to openings almost always occurs in the area facing the openings. Here, this can be effectively remedied by the reinforcement of the material of the bipolar plate, by correspondingly strengthening the layer of the bipolar plate facing the openings in the area facing the openings, without the need to change the entire structure of the bipolar plate or carry out other adaptations.
[0010] In this respect, the reinforcement of the corresponding areas of the bipolar plate can be carried out in various ways. A particularly simple and efficient solution provides for the reinforcement to be realized by a larger material thickness. Other possibilities, such as the introduction of reinforcing materials, paints, resins or the like that reinforce the layer structure, are also conceivable and possible in principle.
[0011] A preferred embodiment of this reinforcement by a larger material thickness provides that the reinforcement is realized by a larger material thickness based on a very advantageous variant of the bipolar plate according to the invention. This material thickness is typically greater than the material thickness between the innermost part of the flow field formed by the recess in the surface of the respective layer, in which the flow-dispersing and / or flow-guiding structures protruding from the bottom of the recess are arranged. The maintained remaining thickness of the respective layer of the bipolar plate refers to the minimum material thickness of the respective layer between the innermost part of the flow field and the opposite surface of the same layer. If this minimum material thickness in the area facing the openings of the adjacent layer is accordingly reinforced, then an increase in the service life of the bipolar plate can be achieved simply and very efficiently. Since the opening area is relatively small in relation to the entire surface of the bipolar plate or its flow area, i.e. if a small surface area is accordingly reinforced, then it is already sufficient to obtain the above-mentioned advantages.
[0012] According to one very preferred variant of this idea, this can be realised, for example, in that the greater material thickness is achieved by a zone of reduced depth of the flow field, i.e. in this reinforced zone the remaining wall thickness of the flow field is slightly increased, thereby reducing the depth in the flow field in this small zone and thus the flow cross-sectional area, nevertheless, since the reinforced zone is typically very small and in the edge zone of the flow field, this has almost no or at least not a significant effect on the flow itself.
[0013] In this respect, reinforcement areas with a smaller depth of the flow field can in principle be realized independently in the flow field, for example by the creation of a kind of pedestal around the flow-dispersing or flow-guiding structures in this area, however, it is particularly advantageous if the reinforcement areas are correspondingly connected to the edges of the flow field, since in this case a connection of the reinforcement areas to the edge areas of the flow field, which is present at least on one side or also on two sides if arranged at a corner, can achieve even better reinforcement with even more suitable force distribution.
[0014] An alternative to this may also contemplate that a larger material thickness is realized by offsetting the flow area from the reinforced area, i.e. in this variation the complete flow area in the reinforced area is abandoned, so that the flow area is made a little smaller, and in the reinforced area the full thickness of the layer opposite the apertures of the adjacent layer remains.
[0015] A further embodiment may also provide that a greater material thickness is achieved by a smaller depth of the passages or by the omission of passages in the layer with the reinforced zone, i.e. the passages internal between both layers of the bipolar plate are, as it were, shifted towards the layer with the opening, which automatically results in a reinforced zone with a greater material thickness in the region of the adjacent layer opposite the respective opening.
[0016] The greater material thickness in the reinforced zone can then be 1.5 to 2.5 times, preferably 2 to 2.5 times, the material thickness between the innermost part of the flow field in this layer and the opposite surface of the same layer, i.e. the remaining material thickness of the respective layer is multiplied, for example by a factor of 1.75, to provide a corresponding reinforced zone. Thus, for typical bipolar plate dimensions and flow field depths, the flow field depth is reduced by half or a little more than half, which in principle does indeed impede the flow, but does not, however, have a significant effect on the uniform distribution of the flow and the flow of the medium through the flow field of the bipolar plate, due to the arrangement of reinforced zones, which are very small in area relative to the area of the flow field, typically at the edge of the flow field.
[0017] Instead of, or in principle also in addition to, such reinforcement by larger material thicknesses, it may be provided for the introduction of reinforcing materials, such as fibers, wovens, knits or the like, into the reinforced areas, which can be realized relatively simply in the production, especially when producing the individual layers from a plastic matrix filled with graphite or another carbon-containing material.
[0018] The flow region itself can then preferably have one flow field and two dispersion regions with openings. In this regard, according to an advantageous variant, it may be provided that the flow field has channels and the dispersion region has an open flow dispersion structure, especially in the form of a nodule. In particular, in such a type of flow region, the openings typically face the dispersion region of the adjacent layer. This dispersion region can be reinforced relatively simply by slightly increasing the material thickness here, so that, for example, the nodules of the dispersion region are no longer located at the bottom of the flow region, but on a kind of base in the reinforced area. The flow is only slightly affected thereby, and the mounting of the bipolar plate can be realized efficiently, achieving high mechanical reliability and a long service life.
[0019] This applies in principle to all types of bipolar plates. However, according to a particularly preferred embodiment of the bipolar plate according to the invention, it is provided that the two layers are each formed from a carbon-containing material in a plastic matrix. Structures in which graphite as a filler in a suitable matrix is cured are often also called graphite bipolar plates or carbon bipolar plates.
[0020] Further advantageous configurations of the bipolar plate according to the invention are evident from the exemplary embodiments which are explained in more detail below with reference to the figures. [Brief description of the drawings]
[0021] [Figure 1] FIG. 2 shows a bipolar plate according to the prior art with two opposing surfaces of the bipolar plate before assembly of the layers of the bipolar plate. [Diagram 2] FIG. 4 is a schematic cross-sectional view according to the line II-II after assembly of the layers according to FIG. [Diagram 3] FIG. 2 shows a bipolar plate with two opposing surfaces of the bipolar plate before assembly of the layers of the bipolar plate. [Figure 4] FIG. 4 is a schematic cross-sectional view according to the line IV-IV after assembly of the layers according to FIG. [Diagram 5]FIG. 5 shows an alternative embodiment of a bipolar plate according to the invention in a representation similar to that in FIG. [Figure 6] FIG. 5 shows a further alternative form of bipolar plate according to the invention in a representation similar to that in FIG. 4. [Figure 7] FIG. 5 shows a further alternative form of bipolar plate according to the invention in a representation similar to that in FIG. 4. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0022] In the representation of Fig. 1 one can see a plan view of two still separate layers 2, 3 which are subsequently assembled into a bipolar plate 1 according to the curved arrows. In this respect, the upper layer 2 represents the cathode side and the lower layer 3 the anode side of the subsequent bipolar plate 1. On the respective rear side of both layers 2, 3 of the bipolar plate 1, flow fields for the coolant are arranged which are not shown in more detail here but are known in principle.
[0023] The layer 2 on the anode side here has a medium inlet 4 and a medium outlet 5. These medium inlet 4 and medium outlet 5 are formed in such a way that they are aligned in both layers 2, 3 and in such a way that they are aligned with the other bipolar plate 1 that is subsequently stacked in the fuel cell stack, not shown here. Between the two layers 2, 3, i.e. here on the back side according to the representation in FIG. 1, both the medium inlet 4 and the medium outlet 5 are connected via channels marked 6 to apertures marked 7, respectively. The apertures 7 connect the channels 6, which are on the back side of the layer 2 in the representation in FIG. 1, and thus the medium inlet 4 or the medium outlet 5, with a flow distribution area 8 arranged adjacent to the medium inlet 4. In the distribution area 8, the flow is distributed as uniformly as possible over the entire cross section of the flow area marked 9 and is accordingly concentrated adjacent to the medium outlet 5. For this purpose, open, non-blocking and non-guiding structures 10, which are formed here, for example, in the form of lumps, are arranged in the respective distribution area 8. Between these distribution regions 8, as the largest area-wise part of the flow region 9, there are so-called flow fields 11 in which flow-guiding structures, e.g. ribs 12, ensure uniform guidance of the flow along the gas diffusion layer of the membrane electrode assembly which is subsequently placed on the cathode-side layer 2 of the bipolar plate 1.
[0024] The structure of the layer 3 on the anode side is thereby substantially similar, with the difference that here the medium inlets 13 for hydrogen are obliquely opposite the corresponding medium outlets 14 for the anode exhaust gas. In other respects, the structures of the respective flow regions 9 for the cathode side on the one hand and the anode side on the other hand are equivalent and respectively bear the same reference numerals.
[0025] As is known in principle from the prior art, the coolant is fed and removed again via medium inlets and medium outlets 15, 16, designated 15 and 16, respectively, in both layers 2, 3. The guidance of the coolant is not important for the invention shown here and therefore need not be discussed further.
[0026] The principle of the inner channels 6 and the apertures 7 is shown once again by means of a principle cross-section according to the line II-II in both layers 2, 3 of FIG. 1 in the representation of FIG. 2. The layers 2, 3 are characterized by different hatchings and are connected to each other. The medium inlets 4 are arranged in line through both layers. The medium inlets 4 open laterally into the channels 6, which typically form in both layers a respective part of the cross-section of said channels 6. The apertures 7 then connect the flow area 9, in particular its dispersion area 8 with its nodules 10 on the cathode side, with the medium inlets 4, so that air or oxygen can reach in this way into the dispersion area 8 and from there into the flow field 11 in a manner known per se. In the other layer 3, in the facing area, as can be seen from the representation of FIG. 1, the dispersion area 8 on the anode side there is arranged with its nodules 10.
[0027] In the representation of Fig. 3, a modified version of the bipolar plate 1 is shown here. In order to prevent mechanical damage in those areas of the layers 2, 3 facing the respective apertures 7 of the other layer, reinforcement areas 17 are provided in these areas, which in the representation of Fig. 3, which should otherwise be understood according to the representation in Fig. 1, are respectively facing the respective apertures 7 of the other layers 3, 2, i.e. in the layer 2 on the cathode side, the reinforcement areas 17 are arranged in diagonally opposite corners, here at the lower left and upper right, and accordingly in the layer 3 on the cathode side, adjacent to the respective medium inlet 4 or medium outlet 5 for the medium on the cathode side. In this case, the reinforcement areas 17 are preferably connected to the edges of the flow areas 9, i.e. here at the respective distribution areas 8, in order to ensure a structure that is as stable as possible.
[0028] According to the representation in FIG. 2 of the structure of the bipolar plate 1 according to the prior art, a corresponding schematic cross-section according to the line IV-IV in FIG. 3 is also shown in FIG. 4. This structure corresponds to the structure described in the scope of FIG. 2 to a large extent. Only reinforced areas 17 are additionally present here, unlike the representation in FIG. 2. In the exemplary embodiment shown here, for this purpose, the material of the layer 3 on the cathode side facing the opening 7 of the layer 2 on the anode side is reinforced in such a way that the open depth of the flow area on the side of the hump 10 facing the opening 7 is correspondingly reduced. This achieves a sufficient reinforcement of the bipolar plate 1 in the reinforced area 17 due to the greater material thickness. This may in particular be taken into account directly during the production of the layer 3, i.e. in particular in the form of a carbon-containing material in a plastic matrix being molded and hardened into the layer 3.
[0029] In the following figures, further possibilities are explained, each of which is similarly based on the representation in figure 4. There too, the material thickness is correspondingly increased due to the design construction. Alternatively, it would be conceivable to carry out this reinforcement correspondingly by the introduction of paints, resins, intermediate layers or the insertion of fibrous material during the manufacture of the corresponding layers 2, 3 of the bipolar plate 1.
[0030] In the representation of Fig. 5, in the reinforced zone 17, the flow area 9 on the anode side is, as it were, reduced, whereby the material thickness is brought up to that of the adjacent region of the layer 3. Alternatively, and this can in principle also be done in addition to both described implementation variations, it is also possible to correspondingly reduce the material thickness in the region of the passage 6 in order to provide the reinforced zone 17, which is indicated diagrammatically in the representation of Fig. 6.
[0031] Also, the representation of FIG. 6 suggests reinforcing fibers 18 purely by way of example, and the reinforcing fibers 18 could be introduced within the reinforced section 17, for example as carbon fibers, Kevlar® fibers, glass fibers, or the like.
[0032] A further possibility for strengthening the area 17, which can be seen in FIG. 7, might also be to arrange the entire passage 6 only in one layer 2, i.e., the cathode side in the illustrated place of the bipolar plate 1, so that, unlike the prior art, the full material thickness remains maintained in the bottom region of the flow field 9 of the layer 3 opposite the opening 7 in the layer 2.
Claims
1. A bipolar plate (1) for a fuel cell stack, comprising two layers (2, 3) with anode or cathode side flow areas (9) on their mutually non-facing surfaces, with aligned medium inlets (4, 13, 15) and medium outlets (5, 14, 16) in the two layers (2, 3), each of the medium inlets and outlets (4, 5, 13, 14, 15, 16) communicating with at least one passage (6) on the inner surface of the two layers (2, 3), the passages (6) assigned to the anode side and the cathode side communicating with the anode or cathode side flow area, respectively, via openings (7) in the respective layers (2, 3), the material of each of said layers (2, 3) being reinforced in the area (17) facing the aperture (7) of the respective other of said layers (3, 2); the flow fields (9) are formed by recesses in the surface of each of the layers (2, 3), the recesses having flow dispersing and / or flow directing structures (10, 12) protruding from their bottoms, the reinforced areas (17) having a greater material thickness compared to the material thickness between the innermost part of the flow field (9) in each of the layers (2, 3) and the opposite surface of the same layer (2, 3); A bipolar plate (1), wherein said greater material thickness is achieved by said area (17) of reduced depth of said flow region (9).
2. 2. A bipolar plate (1) according to claim 1, characterized in that the reinforced area (17) of reduced depth is connected to the edge of the flow area (9).
3. 2. The bipolar plate (1) according to claim 1, characterized in that the reinforced areas (17) are free of any part of the flow fields (9).
4. 4. A bipolar plate (1) according to claim 1, characterized in that the greater material thickness of the reinforced zone (17) is realized by a smaller depth of the passages (6) or by the omission of the passages (6) in the layer (2, 3) having the reinforced zone (17).
5. 4. A bipolar plate (1) according to any one of claims 1 to 3, characterized in that the greater material thickness in the reinforced zones (17) has a thickness between 1.5 and 2.5 times, preferably between 2 and 2.5 times, of the material thickness between the innermost part of the flow field (9) in each of the layers (2, 3) and the opposite surface of the same layer (2, 3).
6. 4. A bipolar plate (1) according to claim 1, wherein each of the flow regions (9) has one flow field (11) and two distribution regions (8) comprising the openings (7), the flow fields (11) having flow-guiding structures, in particular in the form of ribs (12), and the distribution regions (8) having open flow-dispersing structures, in particular in the form of humps (10).
7. 4. A bipolar plate (1) according to any one of claims 1 to 3, characterized in that the two layers (2, 3) are each made from a plastic matrix filled with a carbon-containing material.
8. A bipolar plate (1) as described in claim 7, characterized in that the strengthening of the material in the reinforced area (17) is achieved by application or introduction of a further material (18).
Citation Information
Patent Citations
Fuel cell
JP2001148252A
High polymer electrolyte fuel cell
JP2002203578A
Fuel cell stack
JP2006147506A
Integrated seal for fuel cell assembly and fuel cell stack
US20070042254A1
Method for manufacturing fuel-cell separator
WO2012165492A1