Lead plate cutting method and lead plate cutting device
Infrared heating of a lead plate with a Bi and Sn alloy allows for efficient and safe cutting of lead plates, addressing contamination and fume issues in existing methods.
Patent Information
- Application Number
- JP2022135004
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2022-08-26
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2042-08-26
AI Technical Summary
Existing methods for cutting lead plates in nuclear power plant decommissioning, such as using cutting oil or thermal cutting, result in contamination or harmful metal fumes, and require significant time due to the heating of the alloy material.
A method involving the application of a low melting point alloy of Bi and Sn to the lead plate, combined with infrared heating to soften the area, allowing for efficient cutting by an ultrasonic cutter.
The method significantly reduces cutting time and prevents the generation of metal fumes, enabling safe and efficient cutting of lead plates.
Smart Images

Figure 0007589923000001 
Figure 0007589923000002 
Figure 0007589923000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a method and device for cutting lead plates, and more particularly to a method and device for cutting lead plates that can cut lead plates easily, reliably, and inexpensively without generating metal fumes. [Background technology]
[0002] Conventionally, one of the decommissioning procedures for nuclear power plants is the cutting of lead sheets used as radiation shielding material.
[0003] One method for cutting lead sheets is to use a large amount of cutting oil in a machining center, but this method requires transporting the lead sheet 1 containing radioactive materials to the machining center, and even if a machining center is set up nearby, the radioactive materials contained in the cutting oil used during cutting will contaminate the cutting site, making this method unrealistic.
[0004] Another possible method for cutting lead sheets is thermal cutting using a burner, but this has problems such as the generation of harmful metal fumes.
[0005] Therefore, as a method for cutting a lead plate without generating metal fumes, Patent Document 1 discloses a cutting method in which the blade tip of an ultrasonic cutter is applied to a lead plate heated by an electric heater, an alloy material made of Bi and Sn is supplied to the part of the lead plate where the blade tip is applied, softening the part of the lead plate as a low melting point alloy made of Bi, Pb and Sn, and the ultrasonic cutter is moved together with the supply of the alloy material to cut the lead plate. Similarly, Patent Document 2 discloses a cutting method in which the blade tip of an ultrasonic cutter is heated by an electric heater to cut the lead plate. [Prior art documents] [Patent documents]
[0006] [Patent Document 1] Patent No. 6688816 [Patent Document 2] Patent No. 6688817 Summary of the Invention [Problem to be solved by the invention]
[0007] However, in the cutting methods of Patent Documents 1 and 2, a lead plate or a blade is heated with an electric heater, and an alloy material is supplied to the portion of the lead plate where the cutting edge of the blade is placed, thereby melting the alloy material. However, there is a problem in that it takes time to heat the lead plate or the blade to a temperature at which the alloy material melts, and therefore cutting takes a long time.
[0008] Therefore, the object of this invention is to provide a method and device for cutting lead plates, which supply molten alloy material consisting of Bi and Sn to the portion of the lead plate where the cutting edge is placed, softening that portion of the lead plate as a low melting point alloy consisting of Bi, Pb and Sn, and cutting the lead plate by moving the blade as the alloy material is supplied, thereby making it possible to shorten the time required to cut the lead plate by making the alloy material more efficient. [Means for solving the problem]
[0009] The present invention has been made to achieve the above object and has the following features.
[0010] The invention described in claim 1 is a method for cutting a lead plate, which comprises applying the cutting edge of a blade to a lead plate, supplying an alloy material consisting of Bi and Sn to the portion of the lead plate where the cutting edge is applied, thereby softening the portion of the lead plate where the cutting edge is applied as a low-melting point alloy consisting of Bi, Pb and Sn, and then moving the blade together with the supply of the alloy material to cut the lead plate, and is characterized in that infrared rays are irradiated to the portion of at least one of the lead plate and the blade where black paint is applied, to heat at least one of the lead plate and the blade.
[0011] The invention described in claim 2 is the method for cutting a lead plate described in claim 1, characterized in that at least a part of the portion irradiated with the infrared rays is shielded with aluminum foil.
[0012] The invention described in claim 3 is a method for cutting a lead plate described in claim 1, characterized in that the alloy material heated and melted by infrared rays is supplied to the lead plate in the portion where the cutting edge is applied.
[0013] The invention described in claim 4 is a method for cutting a lead plate described in claim 3, characterized in that the infrared rays are irradiated to a portion of a container for storing the alloy material that is coated with black paint, thereby melting the alloy material.
[0015] Claim 5 The invention described in A method for cutting a lead plate, comprising: applying the cutting edge of a blade to a lead plate; supplying an alloy material consisting of Bi and Sn to the lead plate at the portion where the cutting edge is applied; softening the lead plate at the portion where the cutting edge is applied as a low melting point alloy consisting of Bi, Pb and Sn; and moving the blade together with the supply of the alloy material to cut the lead plate, comprising: supplying the molten alloy material to the lead plate at the portion where the cutting edge is applied; The method is characterized in that infrared rays are irradiated onto a portion of a container for storing the alloy material, which is coated with black paint, to melt the alloy material.
[0016] Claim 6 The invention described in claims 1 to 5 The method is characterized in that the low melting point alloy in the lead plate cut by the lead plate cutting method described in any one of the above is brought into contact with hydrochloric acid or dilute sulfuric acid to separate Bi and Sn from the lead plate.
[0017] Claim 7 The invention described in the above is characterized by comprising a blade whose cutting edge is placed against a lead plate, an alloy material supplying means for supplying an alloy material consisting of Bi and Sn to the portion of the lead plate where the cutting edge is placed, and an infrared ray irradiating means for irradiating an area of at least one of the lead plate and the blade where black paint is applied with infrared rays to heat at least one of the lead plate and the blade.
[0018] Claim 8 The invention described in claim 7 The lead plate cutting device described in the above is characterized in that at least a part of the area where the infrared rays are irradiated is shielded with aluminum foil.
[0019] Claim 9 The invention described in claim 7 The lead plate cutting device described in the above is characterized in that the infrared ray irradiation means irradiates the infrared ray to a portion of a container for storing the alloy material that is coated with black paint, thereby melting the alloy material, and the alloy material supply means supplies the molten alloy material to the portion of the lead plate to which the cutting edge is applied.
[0020] Claim 10 The invention described in claim 9 The lead plate cutting device described in the above is characterized in that the alloy material supplying means has a pipeline through which the molten alloy material passes inside the blade, and the pipeline is connected to the cutting edge.
[0021] Claim 11 The invention described in the above comprises a blade whose cutting edge is applied to a lead plate, an alloy material supplying means for supplying molten alloy material consisting of Bi and Sn to the portion of the lead plate to which the cutting edge is applied, and a driving means for moving the blade, wherein the alloy material supplying means includes a container for storing the alloy material, and comprises infrared irradiating means for irradiating an area of the container which is coated with black paint with infrared rays to melt the alloy material.
[0022] Claim 12 The invention described in claim 9 or claims 11 The lead plate cutting device described in the above is characterized in that the container is provided above the portion to which the cutting edge is applied, and has an alloy material supply port formed at the bottom for dripping the alloy material, and further comprises a pressure control means for making the inside of the container a positive pressure relative to the outside of the container. Effect of the Invention
[0023] According to this invention, by irradiating infrared rays to the areas of at least one of the lead plate and the blade where black paint is applied, and heating at least one of the lead plate and the blade, the area to which the alloy material is supplied can be efficiently heated, which in turn makes the melting of the alloy material more efficient and shortens the time required to cut the lead plate. [Brief description of the drawings]
[0024] [Figure 1] FIG. 11 is a perspective view showing a state in which a lead plate is heated by an infrared heater in this embodiment. [Diagram 2] FIG. 1 is a perspective view showing an example of a measurement point in an experimental example for measuring a temperature change in a lead plate heated by an infrared heater. [Diagram 3] 1 is a graph showing an example of the results of an experiment measuring the temperature change of a lead plate heated by an infrared heater. [Figure 4] FIG. 2 is a perspective view showing an example of a lead plate cutting device in the present embodiment. [Diagram 5] 4 is a flowchart showing an example of a method for cutting a lead plate in the present embodiment. [Figure 6] FIG. 2A is a schematic cross-sectional view showing a state in which a lead plate is being cut, and FIG. 2B is a schematic cross-sectional view showing a state in which cutting of the lead plate has progressed. [Figure 7] FIG. 2A is a perspective view showing an example of a blade as an alloy material supplying means, and FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0025] An embodiment of the present invention will now be described with reference to the drawings.
[0026] An example of a method for heating a lead plate by an infrared heater will be described with reference to FIG. 1. The infrared heater 2 heats the lead plate 1 placed on the workbench W in a non-contact state. A halogen heater that emits shortwave infrared rays (wavelength: 1000 nm to 2500 nm) was adopted as the infrared heater 2. The lead plate 1 is coated with black paint on the portion where the infrared heater 2 irradiates infrared rays (in this embodiment, the surface 1a facing the direction of the infrared heater 2). As an example of the black paint, black body paint JSC-3 (emissivity 0.94) made by Japan Sensor Co., Ltd. can be used. As will be described in the experimental example described later, by applying black paint to the portion of the lead plate 1 where the infrared heater 2 irradiates infrared rays, heating can be performed more efficiently than when the black paint is not applied. The black paint may be applied to the side surfaces 1b, 1d and upper surface 1c of the lead plate 1.
[0027] On the other hand, for objects or parts that would be undesirable if heated by infrared irradiation, heating can be prevented by shielding them from the infrared rays with aluminum foil. For example, by shielding the workbench W and surrounding objects with aluminum foil, deterioration of these objects due to heating can be prevented. Also, for example, the side surfaces 1b, 1d and the top surface 1c of the lead plate 1 may be shielded with aluminum foil to control the temperature of the lead plate 1.
[0028] 2 and 3, an experimental example will be described in which the temperature change of a lead plate 1 (width 200 mm, height 50 mm, depth 100 mm) was measured when the lead plate 1 was heated by an infrared heater 2. In this experimental example, temperature measurements were performed at measurement points P1 (front), P2 (middle), and P3 (back) on the lead plate 1 shown in FIG.
[0029] Temperature measurements were performed in the following three patterns: (1)-(3). (1) Pattern 1 Black paint applied to surface 1a: None (plain) Distance between infrared heater 2 and surface 1a: 20 cm (2) Pattern 2 Black paint applied to surface 1a: Yes Distance between infrared heater 2 and surface 1a: 20 cm (3) Pattern 3 Black paint applied to surface 1a: Yes Distance between infrared heater 2 and surface 1a: 10cm
[0030] The measurement results of temperature change are shown in the graph of Figure 3. In pattern 1, the measurement points P1, P2, and P3 reached approximately 75°C to approximately 80°C in about 4,800 seconds. In pattern 2, the measurement points P1, P2, and P3 reached approximately 118°C to approximately 130°C in about 4,800 seconds. In pattern 3, the measurement point P1 reached approximately 160°C, the measurement point P2 reached approximately 150°C, and the measurement point P3 reached approximately 140°C in about 2,400 seconds.
[0031] From these measurement results, it can be seen that by applying black paint to the portion irradiated with infrared rays by the infrared heater 2, the lead plate 1 can be heated more effectively than when no black paint is applied. As will be described later, when cutting the lead plate 1 in this embodiment, the cut portion of the lead plate 1 needs to be heated to 139°C or higher, but under the conditions of pattern 3, it is possible to heat it in about 2,400 seconds (40 minutes). Also, even with lead (see pattern 1), which is generally considered difficult to raise the temperature with radiant heat, it was possible to raise the temperature with radiant heat by applying black paint.
[0032] Generally, metals are said to be difficult to heat with radiant heat because they contain a lot of electrons and reflect far-infrared rays. It is also said that most substances, except metals, absorb far-infrared rays at the surface layer and their temperature rises immediately. Under the condition that it would be sufficient to heat lead plate 1 to about 150°C in order to cut it, we tried heating lead plate 1 with infrared heater 2 and, although it took some time, we were able to reach the desired temperature. Furthermore, when we painted lead plate 1 with black paint and then heated it with infrared heater 2, we were able to heat it more efficiently.
[0033] Next, the lead plate cutting device 10 in this embodiment will be described with reference to Fig. 4. The lead plate cutting device 10 includes an infrared heater 2, a blade 3 and a driving unit 8 (an example of a "driving means") constituting a reciprocating saw, and a supply container 5 that stores an alloy material 6 (melting point: 139°C) made of Bi and Sn and supplies it to a cutting section S of the lead plate 1, which will be described later.
[0034] The lead plate 1 has a surface 1a coated with black paint, and is heated by irradiating the surface 1a with infrared rays from the infrared heater 2. The lead plate 1 is, for example, a radiation shielding material in a nuclear power plant.
[0035] The blade 3 cuts the lead plate 1 by applying the cutting edge 4 to the lead plate 1 and sliding downward by the driving unit 8. In this embodiment, the part of the lead plate 1 to which the cutting edge 4 is applied is referred to as a cutting section S.
[0036] The blade 3 is coated with black paint, and is heated by irradiating infrared rays from the infrared heater 2. In this embodiment, the lead plate 1 and the blade 3 are heated, but it is also possible to heat only one of them. For example, when only the blade 3 is heated, the part of the lead plate 1 other than the cut part S that is exposed to infrared rays is shielded with aluminum foil. Also, when only the lead plate 1 is heated, the blade 3 may not be coated with black paint, or may be shielded from infrared rays with aluminum foil (however, even when the blade 3 is heated, there are cases where it is not necessary to apply black paint if the material of the blade 3 itself is black). In this embodiment, the lead plate 1 is cut with a reciprocating saw, but other cutting means (for example, an ultrasonic cutter, etc.) may be used.
[0037] The supply container 5 (an example of an "alloy material supply means") is a metal container (for example, a copper container or an aluminum container can be used) with a triangular cross section in the shape of a trough, and is arranged above the blade 3 along the movement direction D of the blade 3 so that one apex of the triangle faces downward (so that the apex is the lower part of the trough). The supply container 5 is installed on the drive unit 8 of the reciprocating saw via a support 7, and stores an alloy material 6 made of Bi and Sn inside. In addition, black paint is applied to the outer surfaces 5a, 5b, and 5c of the supply container 5, and the supply container 5 is heated by irradiation of infrared rays from the infrared heater 2. When the inside of the supply container 5 is heated to 139°C or higher, the alloy material 6 (melting point: 139°C) melts. Note that, by applying black paint to the outer surfaces 5a, 5b, and 5c of the supply container 5, the supply container 5 and the alloy material 6 can be efficiently heated. Note that it is not necessary to apply black paint to the outer surface 5c if it is not exposed to infrared rays. Furthermore, when the outer surface 5c is to be painted black, another infrared heater 2 may be prepared and placed in a position where infrared rays can be irradiated onto the outer surface 5c.
[0038] A plurality of alloy material supply ports 5d are formed at the bottom of the supply container 5, and the alloy material 6 molten in the supply container 5 drips (is supplied) from the alloy material supply ports 5d onto the cut portion S of the lead plate 1. The lead plate 1 of the cut portion S to which the molten alloy material 6 is supplied is alloyed into a low melting point alloy (melting point: 95°C) made of Bi, Pb, and Sn, and softens into a liquid phase. An appropriate number of alloy material supply ports 5d are provided at appropriate positions so that the alloy material 6 falls evenly onto the cut portion S.
[0039] 4, the top of the supply container 5 is open, but if the amount of alloy material 6 dripping from the alloy material supply port 5d cannot be controlled due to the influence of the viscosity of the alloy material 6, the top of the supply container 5 may be closed with a lid or the like, and a hole may be formed for applying pressure to the inside of the supply container 5, and pressure may be applied from the hole with a cylinder (an example of a "pressure control means") to make the inside of the supply container 5 a positive pressure relative to the outside of the supply container 5. By controlling the pressure inside the supply container 5, the amount of alloy material dripping from the alloy material supply port 5d can be adjusted.
[0040] The infrared heater 2 irradiates infrared rays in a non-contact manner onto the black painted areas of at least one of the lead plate 1 and the blade 3, and heats at least one of the lead plate 1 and the blade 3 by radiant heat. At this time, the infrared heater 2 heats the cut portion S to 95°C or higher, which is the melting point of the low-melting point alloy.
[0041] As the infrared heater 2, a heater that emits infrared rays can be used. For example, a halogen heater that emits short-wave near-infrared rays is preferable because the heating element (generally a tungsten wire) can reach 2,000°C or higher and the temperature rises quickly (within a few seconds).
[0042] In addition, the infrared heater 2 irradiates infrared rays in a non-contact manner onto the portion of the supply container 5 that is coated with black paint, and heats the supply container 5 and the alloy material 6 stored therein by radiant heat. At this time, the infrared heater 2 heats the supply container 5 and the alloy material 6 so that the alloy material 6 reaches its melting point of 139°C or higher. When heating the supply container 5 and the alloy material 6, the infrared heater 2 may heat at least one of the lead plate 1 and the blade 3 to 139°C or higher.
[0043] In this way, the infrared heater 2 can heat the lead plate 1, the blade 3, and the supply container 5 simultaneously in a non-contact state by radiating heat. In contrast, even if you try to heat the objects using a ribbon heater or the like, it is not possible to heat the objects in a non-contact state, and if you want to heat each of them simultaneously, you have to heat them individually in a contact state.
[0044] Note that parts that should not be irradiated with infrared rays or heated (for example, parts not painted black such as the lead plate 1, the blade 3, and the supply container 5, as well as the support 7 and the drive unit 8) may be shielded from infrared rays with aluminum foil. In particular, it is preferable to shield objects and parts that are easily deteriorated by heating with aluminum foil.
[0045] According to the lead plate cutting device 10 of this embodiment, the alloy material 6 in the supply container 5 heated by the infrared heater 2 melts and drips (is supplied) from the alloy material supply port 5d to the cutting section S, so that the lead plate 1 at the cutting section S becomes a low-melting point alloy made of Bi, Pb, and Sn and softens. Then, while the cutting section S is heated by the infrared heater 2 to a temperature equal to or higher than the melting point of the low-melting point alloy, the alloy material 6 is supplied to the cutting section S, and the blade 3 moves with the blade tip 4 placed on the cutting section S, thereby cutting the lead plate 1.
[0046] Next, a method for cutting the lead plate 1 will be described with reference to Fig. 5 and Fig. 6(A) and (B). In Fig. 6(A) and (B), the alloy material supplying means 5Z sequentially supplies, for example, the alloy material 6 wound in a coil shape to the lead plate 1 at the portion (cutting portion S) where the blade tip 4 is applied.
[0047] First, black paint is applied to at least one of the lead plate 1 and the blade 3, and infrared rays are irradiated onto the part where the black paint is applied to heat at least one of the lead plate 1 and the blade 3 (step S1). Note that an infrared heater 2 or the like can be used for irradiating the infrared rays.
[0048] Also, the cutting edge 4 of the blade 3 is placed on the cutting portion S of the lead plate 1 where the cutting edge 4 is to be placed (step S2, FIG. 6(A)).
[0049] Also, an alloy material 6 made of Bi and Sn is supplied to the cut portion S (step S3, FIG. 6(A)). The purpose of supplying the alloy material 6 to the cut portion S is to bring the molten alloy material 6 into contact with the cut portion S, thereby softening the lead plate 1 of the cut portion S into a low-melting-point alloy (melting point of 95° C.) made of Bi, Pb, and Sn.
[0050] As a method of making the cut portion S into a low melting point alloy, there is a method of heating at least one of the lead plate 1 and the blade 3 to heat the cut portion S to 139°C or more, and supplying (contacting) the unmelted alloy material 6 by, for example, the alloy material supply means 5Z to melt the alloy material 6 at the cut portion S, and a method of supplying the alloy material 6 melted in advance in the supply container 5 or the like to the cut portion S, and either method may be adopted in step S3. However, when cutting the lead plate 1 at the cut portion S, it is necessary to heat the cut portion S to 95°C or more, which is the melting point of the low melting point alloy, so at least one of the lead plate 1 and the blade 3 is heated to 95°C or more. Therefore, as in the lead plate cutting device 10 described above, it is preferable to apply black paint to at least one of the lead plate 1 and the blade 3 and heat them with the infrared heater 2.
[0051] Then, while supplying the alloy material 6 to the cutting portion S, the blade 3 is moved with the cutting edge 4 placed on the cutting portion S to cut the lead plate 1 (step S4, FIG. 6(B)). It is preferable to move the blade 3 downward (lower) while sliding it in the movement direction D of the blade 3. The order of steps S1 to S3 can be changed as appropriate.
[0052] As explained with respect to the lead plate cutting device 10, it is preferable to block infrared rays with aluminum foil in areas where it is inconvenient to be irradiated with infrared rays or heated.
[0053] As described above, according to the lead plate cutting device 10 and lead plate cutting method of this embodiment, by irradiating infrared rays to the areas on at least one of the lead plate 1 and the blade 3 where black paint is applied, the area where the alloy material 6 is supplied (the cutting area S) can be efficiently heated, which in turn makes it possible to efficiently melt the alloy material 6 and shortens the time required to cut the lead plate 1.
[0054] In addition, by lowering the blade 3 while the cutting portion S is made of a low melting point alloy and the alloy material 6 is being supplied, the low melting point alloy consisting of Bi, Pb and Sn in the cutting portion S to which the alloy material 6 is supplied turns into a liquid phase and softens, thereby making it possible to cut the lead plate 1 easily, reliably and inexpensively without generating metal fumes.
[0055] Furthermore, since the cut surfaces of the lead plates 1 after cutting are bonded via the cooled low melting point alloy, there is no risk of the cut lead plates 1 separating from the uncut lead plates 1. As a result, it is possible to prevent accidents caused by the cut lead plates 1 dropping. Furthermore, since the cooled low melting point alloy has a coarse metal crystal structure and is harder and more brittle than lead, when the cut lead plates 1 are struck with a hammer or the like, the cut lead plates 1 easily peel off from the uncut lead plates 1, making it easy to remove the cut lead plates 1.
[0056] In the lead plate cutting device 10 of this embodiment, the molten alloy material 6 is supplied to the cutting section S using a supply container 5, but it is also possible to heat at least one of the lead plate 1 or the blade 3 to 139°C or higher without providing the supply container 5, and supply unmolten alloy material 6 by directly contacting it with the cutting section S using an alloy material supply means 5Z or the like.
[0057] In addition, when molten alloy material 6 is supplied to the lead plate 1 of the cut portion S to make the cut portion S into a low melting point alloy, instead of heating the cut portion S by irradiating the lead plate 1 or the blade 3 with infrared rays, the lead plate 1 or the blade 3 may be heated by another method (for example, heating with an electric heater) to make the cut portion S into a low melting point alloy at 95°C or higher.
[0058] Next, the blade 11 capable of supplying the molten alloy material 6 to the cutting portion S will be described with reference to Figs. 7(A) and (B).
[0059] The blade 11 (one example of an "alloy material supply means") has a pipeline through which the molten alloy material 6 passes. The pipeline includes a horizontal pipe 12 and a number of vertical pipes 13A-13E, and each of the vertical pipes 13A-13E is connected below the horizontal pipe 12 and leads to the blade tip 4. The horizontal pipe 12 takes in the alloy material 6 molten in a container (not shown) while it is in the molten state, and the alloy material 6 is supplied to the cutting part S from the blade tip 4 through each of the vertical pipes 13A-13E. In order to prevent the alloy material 6 from solidifying in the pipeline, it is preferable to use a metal with high thermal conductivity (e.g., copper) for the blade 3, apply black paint, and heat it by an infrared heater 2 or the like. In addition, as shown in FIG. 7(B), it is preferable to provide a filler (bulge) 14 in the part of the blade 3 where the horizontal pipe 12 is provided to improve strength.
[0060] With the blade 11, there is no need to place the supply container 5 shown in Figure 4 above the blade 3, and the alloy material 6 can be supplied directly to the cutting portion S from the cutting edge 4, thereby preventing the alloy material 6 from scattering to areas other than the cutting portion S when it falls from the supply container 5.
[0061] Next, we will explain how to separate Bi and Sn from the low melting point alloy consisting of Bi, Pb, and Sn at the cut portion S of the cut lead plate 1. Lead is an amphoteric element, and while it dissolves by reacting with an aqueous solution of nitric acid or a strong base, it does not dissolve in hydrochloric acid or dilute sulfuric acid because it forms a poorly soluble coating (a coating of lead chloride PbCl2 or lead sulfate PbSO4) on the surface of the lead. In addition, Bi and Sn dissolve in hydrochloric acid and dilute sulfuric acid. Therefore, Bi and Sn can be separated from the lead plate 1 by bringing hydrochloric acid or dilute sulfuric acid into contact with the low melting point alloy in the cut lead plate 1.
[0062] As a result, when the lead plate 1 containing radioactive materials is cut into small pieces by the cutting method of this embodiment and disposed of, it can be disposed of in a state in which Bi and Sn are separated (lead only) from the lead plate 1. Moreover, the Bi and Sn separated from the lead plate 1 can be reused for cutting the lead plate 1 by refining them by a conventionally known method. [Explanation of symbols]
[0063] 1: Lead plate 2: Infrared heater 3: Knives 4: Cutting edge 5: Supply container 5Z: Alloy material supply means 6: Alloy material 7: Support 8: Drive unit 10:Lead plate cutting device 11: Knives 12: Horizontal pipe 13A~13E: Vertical pipe 14: Filler D: Movement direction S: Cutting section W: Workbench
Claims
1. A method for cutting a lead plate, comprising the steps of: applying a cutting edge of a blade to a lead plate; supplying an alloy material consisting of Bi and Sn to the portion of the lead plate to which the cutting edge is applied; softening the portion of the lead plate to which the cutting edge is applied as a low melting point alloy consisting of Bi, Pb and Sn; and cutting the lead plate by moving the blade together with the supply of the alloy material, A method for cutting a lead plate, comprising irradiating infrared rays to a portion of at least one of the lead plate and the blade where black paint is applied, thereby heating at least one of the lead plate and the blade.
2. A method for cutting a lead plate according to claim 1, A method for cutting a lead plate, comprising shielding at least a portion of the area irradiated with infrared rays with aluminum foil.
3. A method for cutting a lead plate according to claim 1, A method for cutting a lead plate, comprising: supplying the alloy material heated and melted by infrared rays to the lead plate at a portion where the cutting edge is placed.
4. The method for cutting a lead plate according to claim 3, A method for cutting a lead plate, comprising irradiating a portion of a container for storing the alloy material, which is coated with black paint, with the infrared rays to melt the alloy material.
5. A method for cutting a lead plate, comprising applying a cutting edge of a blade to a lead plate, supplying an alloy material consisting of Bi and Sn to the lead plate at the portion where the cutting edge is applied, thereby softening the lead plate at the portion where the cutting edge is applied as a low melting point alloy consisting of Bi, Pb and Sn, and then moving the blade together with the supply of the alloy material to cut the lead plate, The molten alloy material is supplied to the lead plate at the portion where the cutting edge is applied; A method for cutting a lead plate, comprising irradiating infrared rays onto a portion of a container for storing the alloy material that is coated with black paint, thereby melting the alloy material.
6. A method for separating Bi and Sn, comprising contacting hydrochloric acid or dilute sulfuric acid with a low melting point alloy in a lead plate cut by the method for cutting a lead plate according to any one of claims 1 to 5, thereby separating Bi and Sn from the lead plate.
7. A blade with a cutting edge placed on a lead plate, an alloy material supplying means for supplying an alloy material made of Bi and Sn to a portion of the lead plate to which the cutting edge is applied; an infrared irradiation means for irradiating infrared rays to a portion of at least one of the lead plate and the blade where black paint is applied, to heat at least one of the lead plate and the blade; A driving means for moving the blade; A lead plate cutting device comprising:
8. 8. The lead plate cutting device according to claim 7, A lead plate cutting device characterized in that at least a portion of the area where the infrared rays are irradiated is shielded with aluminum foil.
9. 8. The lead plate cutting device according to claim 7, the infrared ray irradiation means irradiates the infrared ray to a portion of the container storing the alloy material that is coated with black paint, thereby melting the alloy material; A lead plate cutting device characterized in that the alloy material supplying means supplies molten alloy material to the portion of the lead plate to which the cutting edge is attached.
10. 10. The lead plate cutting device according to claim 9, the alloy material supplying means has a pipe through which the molten alloy material passes inside the blade, A lead plate cutting device characterized in that the duct is connected to the cutting edge.
11. A blade with a cutting edge placed on a lead plate, an alloy material supplying means for supplying a molten alloy material made of Bi and Sn to a portion of the lead plate to which the cutting edge is to be applied; A driving means for moving the blade; Equipped with the alloy material supply means includes a container for storing the alloy material, an infrared ray irradiation means for irradiating infrared rays to a portion of the container where black paint is applied, thereby melting the alloy material; A lead plate cutting device comprising:
12. The lead plate cutting device according to claim 9 or 11, The container is provided above the portion to which the cutting edge is applied, and has an alloy material supply port formed at a lower portion thereof for dripping the alloy material, A lead plate cutting device further comprising a pressure control means for making the inside of the container a positive pressure relative to the outside of the container.
Citation Information
Patent Citations
Apparatus for shearing soft steel
JP1979068590A
Means for improving laser-beam machining efficiency of metal
JP1988295093A
Separation of lead, tin and bismuth from lead slag
JP2000109939A
Method for manufacturing gas cylinder
JP2003053257A
Apparatus and method for shaping glass into curved shape
JP2014196235A