Tunneling magnetoresistance sensor
The tunnel magnetoresistive sensor addresses hysteresis-induced errors by synchronizing adjacent elements with shared electrode layers, enhancing sensitivity and reducing measurement errors.
Patent Information
- Application Number
- JP2019030127
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2019-02-22
- Publication Date
- 2024-11-27
- Estimated Expiration
- 2039-02-22
AI Technical Summary
Magnetic measurement devices using tunnel magnetoresistive elements suffer from hysteresis-induced measurement errors and reduced sensitivity due to differences in TMR response when the magnetic field changes direction.
The tunnel magnetoresistive sensor design includes a fixed layer and a free layer with a tunnel barrier layer, where adjacent tunnel magnetoresistive elements share a first electrode layer and are arranged in close proximity (0.5 μm or less) to synchronize their magnetization, reducing hysteresis and increasing sensitivity.
The sensor reduces measurement errors caused by hysteresis and enhances sensitivity by synchronizing adjacent tunnel magnetoresistive elements through close proximity, leading to improved magnetic field detection accuracy.
Smart Images

Figure 0007590705000001 
Figure 0007590705000002 
Figure 0007590705000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a tunneling magnetoresistance (TMR) sensor. [Background technology]
[0002] In recent years, devices having magnetic sensors including tunnel magnetoresistance (TMR) elements have been used in fields such as medicine, non-destructive testing, and electric vehicles, where high sensitivity, low power consumption, and portability are essential (see, for example, Patent Document 1). In this magnetic measurement device, in order to reduce noise such as 1 / f noise, the magnetic sensor is composed of a tunnel magnetoresistance element array in which multiple tunnel magnetoresistance elements are arranged in a lattice.
[0003] Recently, research has been conducted on mutual device synchronization in spin Hall nano-oscillators and its advantages (see, for example, Non-Patent Document 1). In addition, in tunnel magnetoresistance elements, 1 / f noise is the most dominant noise in the low frequency band, and it has been found that the magnetic fluctuation is related to the switching state of the magnetization orientation at the interface between the fixed layer and the free layer (see, for example, Non-Patent Document 2). [Prior art documents] [Patent documents]
[0004] [Patent Document 1] International Publication No. WO2012 / 032962 [Non-patent literature]
[0005] [Non-Patent Document 1] Awad, AA et al., “Long-range mutual synchronization of spin Hall nano-oscillators”. Nat. Phys., 2016, 13, p.292-299 [Non-Patent Document 2] ZQ Lei, et al., “Review of Noise Sources in Magnetic Tunnel Junction Sensors”, IEEE Transactions on Magnetics, March 2011, Volume 47, Issue 3, p.602-612 Summary of the Invention [Problem to be solved by the invention]
[0006] In a magnetic measurement device such as that described in Patent Document 1, the TMR response of the tunnel magnetoresistance element differs when the magnetic field changes from positive to negative and from negative to positive, i.e., the device has so-called hysteresis, which causes measurement errors and reduces sensitivity.
[0007] The present invention has been made in view of the above-mentioned problems, and has an object to provide a tunnel magnetoresistance sensor capable of reducing measurement errors due to hysteresis and increasing sensitivity. [Means for solving the problem]
[0008] The inventors of the present invention came up with the idea that the magnetic fluctuations of the tunneling magnetoresistance element described in Non-Patent Document 2 are caused by the direction of internal magnetization, and that the maximum value of the output density always appears when the free layer of the tunneling magnetoresistance element is changing the direction of magnetization, and therefore that mutual synchronization of each tunneling magnetoresistance element in a tunneling magnetoresistance element array may reduce noise.
[0009] That is, in order to achieve the above object, the tunneling magnetoresistance sensor according to the present invention has a plurality of tunneling magnetoresistance elements, each of which has a fixed layer whose magnetization direction is fixed, a free layer whose magnetization direction is changeable, a tunnel barrier layer disposed between the fixed layer and the free layer, a first electrode layer disposed on the side of the fixed layer opposite to the tunnel barrier layer, and a second electrode layer disposed on the side of the free layer opposite to the tunnel barrier layer, and each of the tunneling magnetoresistance elements is arranged in a row or a lattice array, and adjacent Two Tunneling magnetoresistance element of between the free layer and the second electrode layer and each island is formed independently, and adjacent tunnel magnetoresistance elements are formed between adjacent islands. The first electrode layer is shared to form a tunneling magnetoresistance element array, and the distance between the free layers of adjacent tunneling magnetoresistance elements that share the first electrode layer is 0.5 μm or less.
[0010] In the tunneling magnetoresistance sensor according to the present invention, among the tunneling magnetoresistance elements of the tunneling magnetoresistance element array, the free layers of adjacent tunneling magnetoresistance elements that share the first electrode layer, i.e., adjacent tunneling magnetoresistance elements that do not share a free layer, are close to each other with a distance of 0.5 μm or less, so that the tunneling magnetoresistance elements can be synchronized with each other to reduce hysteresis, thereby reducing measurement errors due to hysteresis and increasing sensitivity.
[0011] In the tunneling magnetoresistance sensor according to the present invention, the distance between the free layers of adjacent tunneling magnetoresistance elements sharing the first electrode layer is preferably 0.35 μm or less. In this case, by bringing the free layers of adjacent tunneling magnetoresistance elements closer to each other, it is possible to further reduce measurement errors and increase sensitivity. The distance between the free layers of adjacent tunneling magnetoresistance elements varies greatly depending on the manufacturing method, but can be narrowed to about 0.2 μm to 0.35 μm, for example, when lithography and ion milling are used.
[0012] In the tunneling magnetoresistive sensor according to the present invention, it is preferable that the first electrode layer is an upper electrode and the second electrode layer is a lower electrode. In this case, during manufacturing, layers are stacked starting from the second electrode layer of the lower electrode, so that the distance between the free layers of adjacent tunneling magnetoresistive elements can be easily set to a desired distance. Effect of the Invention
[0013] According to the present invention, it is possible to provide a tunnel magnetoresistance sensor capable of reducing measurement errors due to hysteresis and increasing sensitivity. [Brief description of the drawings]
[0014] [Figure 1] 1 is a side view showing a tunnel magnetoresistive sensor according to an embodiment of the present invention; [Diagram 2] 2 is a front view showing a layer configuration of a tunneling magnetoresistive element of the tunneling magnetoresistive sensor shown in FIG. [Diagram 3] 2A is a plan view showing the distribution of independent islands having a free layer and a lower electrode layer of a tunneling magnetoresistance element of the tunneling magnetoresistance sensor shown in FIG. 1, and FIG. 2B is a cross-sectional view taken along line A-A' in FIG. 2A. [Figure 4] 1 is an optical microscope photograph in plan view showing a state in which an independent island has been manufactured in the tunnel magnetoresistive sensor according to the embodiment of the present invention. [Diagram 5] 1A is a graph showing the magnetoresistance curves of a tunnel magnetoresistance sensor according to an embodiment of the present invention (island spacing is 0.3 μm) and a comparative example tunnel magnetoresistance sensor in which the island spacing is 5 μm, and FIG. 1B is a graph showing an enlarged view of the area near zero magnetic field in FIG. [Figure 6] 1 is a graph showing the relationship between the distance between free islands (Distance Between Free Islands) and the normalized TMR difference at zero field (Hc) and normalized TMR sensitivity (TMRS) of a tunnel magnetoresistive sensor according to an embodiment of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0015] Hereinafter, an embodiment of the present invention will be described with reference to the drawings. 1 to 6 show a tunnel magnetoresistive sensor according to an embodiment of the present invention. As shown in FIG. 1, a tunneling magnetoresistive sensor 10 has a plurality of tunneling magnetoresistive elements 11, which are arranged in a row.
[0016] As shown in Figure 2, each tunnel magnetoresistance element 11 has a substrate 12, and an undercoat layer 13, a lower electrode layer 14, a free layer 15, a tunnel barrier layer 16, a fixed layer 17, a fixation promotion layer 18, and an upper electrode layer 19 stacked in that order on the substrate 12.
[0017] The substrate 12 may be made of any material, for example, Si or SiO2, as long as it is non-magnetic and can withstand the deposition of each layer and heat treatment. The undercoat layer 13 is provided on the surface of the substrate 12 to smooth out the surface roughness. The undercoat layer 13 may be made of any material as long as it can smooth out the surface roughness of the substrate 12. The undercoat layer 13 preferably has a layer thickness of about 2 nm to 10 nm.
[0018] The lower electrode layer 14 is provided so as to be in contact with the surface of the undercoat layer 13 opposite to the substrate 12. The lower electrode layer 14 may be made of any conductive material, and may have a structure in which a plurality of metal materials are laminated. The lower electrode layer 14 preferably has a layer thickness of about 2 nm to 20 nm. The lower electrode layer 14 forms a second electrode layer.
[0019] The free layer 15 is provided on the surface of the lower electrode layer 14 opposite to the undercoat layer 13. The free layer 15 has a structure in which a first ferromagnetic layer 21, a first non-magnetic layer 22, and a second ferromagnetic layer 23 are laminated in this order on the lower electrode layer 14. The magnetization direction of the first ferromagnetic layer 21 is changeable under the influence of an external magnetic flux. The first ferromagnetic layer 21 is made of a soft magnetic material, such as NiFe, CoFeSiB, or the like, and preferably has a layer thickness of about 30 nm to 200 nm.
[0020] The first non-magnetic layer 22 is provided to magnetically couple the first ferromagnetic layer 21 and the second ferromagnetic layer 23, and to separate the first ferromagnetic layer 21 from the crystal structure of the second ferromagnetic layer 23. The first non-magnetic layer 22 is preferably made of, for example, Ru or Ta, and has a layer thickness of about 0.2 to 1 nm. The magnetization direction of the second ferromagnetic layer 23 is changeable under the influence of an external magnetic flux. The second ferromagnetic layer 23 is preferably made of, for example, CoFeB, and has a layer thickness of about 1.4 nm to 5.0 nm.
[0021] The tunnel barrier layer 16 is provided on the surface of the free layer 15 opposite to the lower electrode layer 14. The tunnel barrier layer 16 is made of an insulating material such as MgO, Mg-Al-O, AlOx, etc. The tunnel barrier layer 16 preferably has a layer thickness of, for example, about 1 nm to 10 nm.
[0022] The fixed layer 17 is provided on the surface of the tunnel barrier layer 16 opposite to the free layer 15, and sandwiches the tunnel barrier layer 16 between the tunnel barrier layer 16 and the free layer 15. The fixed layer 17 has a structure in which a third ferromagnetic layer 24, a second non-magnetic layer 25, and a fourth ferromagnetic layer 26 are laminated in this order on the tunnel barrier layer 16. The magnetization direction of the third ferromagnetic layer 24 is fixed. The third ferromagnetic layer 24 is preferably made of CoFeB, for example, and has a layer thickness of about 1.4 nm to 10 nm.
[0023] The second nonmagnetic layer 25 is provided to magnetically couple the third ferromagnetic layer 24 and the fourth ferromagnetic layer 26, and to separate the third ferromagnetic layer 24 from the crystal structure of the fourth ferromagnetic layer 26. The second nonmagnetic layer 25 is preferably made of, for example, Ru or Ta, and has a thickness of about 0.2 to 1 nm. The fourth ferromagnetic layer 26 has a fixed magnetization direction. The fourth ferromagnetic layer 26 is preferably made of, for example, CoFe, and has a thickness of about 1 nm to 10 nm.
[0024] The fixation promotion layer 18 is provided on the surface of the fixed layer 17 opposite to the tunnel barrier layer 16 in order to promote fixation of the fourth ferromagnetic layer 26. The fixation promotion layer 18 is made of an antiferromagnetic material such as IrMn or PtMn, and has a layer thickness of about 5 nm to 20 nm.
[0025] The upper electrode layer 19 is provided on the surface of the immobilization promotion layer 18 opposite to the immobilization layer 17. The upper electrode layer 19 may be made of any conductive material, and may have a structure in which a plurality of metal materials are laminated. The upper electrode layer 19 preferably has a layer thickness of about 2 nm to 20 nm. The upper electrode layer 19 forms a first electrode layer.
[0026] In a specific example shown in FIG. 2, the undercoat layer 13 is made of Ta and has a thickness of 5 nm. The lower electrode layer 14 is made of Ta / Ru, with the Ru layer having a thickness of 10 nm and the Ta layer having a thickness of 5 nm. The first ferromagnetic layer 21 of the free layer 15 is made of CoFeSiB and has a thickness of 100 nm. The first non-magnetic layer 22 of the free layer 15 is made of Ru and has a thickness of 0.8 nm. The second ferromagnetic layer 23 of the free layer 15 is made of CoFeB and has a thickness of 3 nm. The tunnel barrier layer 16 is made of MgO and has a thickness of 1.6 nm. The third ferromagnetic layer 24 of the fixed layer 17 is made of CoFeB and has a thickness of 3 nm. The second non-magnetic layer 25 of the fixed layer 17 is made of Ru and has a thickness of 0.85 nm. The fourth ferromagnetic layer 26 of the pinned layer 17 is made of CoFe and has a thickness of 5 nm. The pinning promotion layer 18 is made of IrMn and has a thickness of 6 nm. The upper electrode layer 19 is made of Ru / Ta, with the Ta layer being 5 nm thick and the Ru layer being 8 nm thick.
[0027] The tunnel magnetoresistance element 11 can be manufactured by depositing each layer on the substrate 12 using a physical vapor deposition method such as sputtering or molecular beam epitaxy (MBE). The tunnel magnetoresistance element 11 may be heat-treated after each layer is deposited in order to obtain a desired crystal structure. The temperature for the heat treatment is preferably 325°C to 450°C.
[0028] 1, adjacent two tunneling magnetoresistance elements 11 are grouped together, and the free layer 15 and the lower electrode layer 14 are shared between the two tunneling magnetoresistance elements 11, forming each independent island 31. In addition, adjacent tunneling magnetoresistance elements 11 between adjacent islands 31 share the upper electrode layer 19. In this way, each tunneling magnetoresistance element 11 constitutes a tunneling magnetoresistance element array.
[0029] As shown in FIG. 1 and FIG. 3(a), the tunneling magnetoresistance sensor 10 has a distance between adjacent islands 31, i.e., a distance between the free layers 15 of adjacent islands 31, of 0.5 μm or less. It is particularly preferable that the distance between adjacent islands 31 is 0.1 μm to 0.35 μm. In a specific example shown in FIG. 3(a), the tunneling magnetoresistance sensor 10 has a plurality of tunneling magnetoresistance element arrays arranged in parallel at a predetermined distance. In the figure, a represents the distance between adjacent islands 31, and b represents the distance between the plurality of tunneling magnetoresistance element arrays. In addition, when there is no external magnetic field, the magnetization direction of the fixed layer 17 (the direction of the arrow "Pin" in the figure) is parallel to the hard magnetization axis, and the magnetization direction of the free layer 15 (the direction of the arrow "Free" in the figure) is parallel to the easy magnetization axis. Furthermore, as shown in FIG. 3(b), if the height of the island 31 in the film thickness direction is h, then the ratio of the interval (groove width) a between adjacent islands 31 to the film thickness h can be expressed as Q (=h / a).
[0030] In the tunneling magnetoresistance sensor 10, the distance between the islands 31 in which the adjacent tunneling magnetoresistance elements 11 share the free layer 15 and the lower electrode layer 14 among the tunneling magnetoresistance elements 11 in the tunneling magnetoresistance element array is 0.5 μm or less, so that the tunneling magnetoresistance elements 11 are synchronized with each other, thereby reducing hysteresis. This makes it possible to reduce measurement errors due to hysteresis and increase sensitivity. EXAMPLES
[0031] Using magnetron sputtering, each layer of the tunneling magnetoresistance element 11 was deposited on the substrate 12 in an ultra-high vacuum chamber to manufacture the tunneling magnetoresistance sensor 10 shown in FIG. 1. In the manufacturing process, after the free layer 15 was deposited, a groove was formed from the free layer 15 to the surface of the substrate 12 using lithography and ion milling to form an independent island 31. The interval between adjacent islands 31 (a in FIG. 3(a)), i.e., the width of the formed groove, was 0.3 μm. FIG. 4 shows an optical microscope photograph in plan view after the islands 31 were formed and the resist was removed. The thin vertical groove in FIG. 4 is the groove a in FIG. 3(a). Also, Q (=h / a) shown in FIG. 3(b) was close to 1.
[0032] After each layer of the tunneling magnetoresistance element 11 was formed, a heat treatment was performed at 350° C. with a magnetic field applied, thus producing the tunneling magnetoresistance sensor 10 shown in FIG. 1. As a comparative example, a tunneling magnetoresistance sensor 10 in which the interval between islands 31 was 5 μm was also produced by the same method.
[0033] The magnetoresistance curves of the tunneling magnetoresistance sensor 10 with the island 31 spaced apart by 0.3 μm and the comparative tunneling magnetoresistance sensor with the island 31 spaced apart by 5 μm were measured by the four-terminal method. The measurement results are shown in FIG. 5(a). FIG. 5(b) is an enlarged view of the area near zero magnetic field in FIG. 5(a). As shown in FIGS. 5(a) and (b), it was confirmed that the tunneling magnetoresistance sensor 10 with the island 31 spaced apart by 0.3 μm has a smaller deviation between the curve when the magnetic field changes from positive to negative and the curve when the magnetic field changes from negative to positive, and has a smaller hysteresis, compared to the comparative example with the island 31 spaced apart by 5 μm. This is considered to be because the tunneling magnetoresistance elements 11 of adjacent islands 31 are more strongly synchronized with each other by placing the independent islands 31 closer to each other.
[0034] Based on Fig. 5, the relationship between the distance between islands 31 (Distance Between Free Islands) and the amount of deviation in the TMR ratio at zero magnetic field (Normalized TMR Difference at zero field; Hc) and the TMR sensitivity (Normalized TMR Sensitivity; TMRS) was obtained and is shown in Fig. 6. As shown in Fig. 6, it was confirmed that the smaller the distance between islands 31, the smaller the deviation in the TMR ratio and the smaller the hysteresis. It was also confirmed that this reduces the measurement error and therefore increases the TMR sensitivity. [Explanation of symbols]
[0035] 10 Tunneling magnetoresistance sensor 11 Tunneling magnetoresistance element 12 Substrate 13 Undercoat layer 14 Lower electrode layer 15 Free layer 21 First ferromagnetic layer 22 First non-magnetic layer 23 Second ferromagnetic layer 16 Tunnel Barrier Layer 17 Fixed layer 24 Third ferromagnetic layer 25 Second non-magnetic layer 26 Fourth ferromagnetic layer 18 Immobilization promotion layer 19 Upper electrode layer 31 islands
Claims
1. a plurality of tunnel magnetoresistance elements each including a fixed layer whose magnetization direction is fixed, a free layer whose magnetization direction is changeable, a tunnel barrier layer disposed between the fixed layer and the free layer, a first electrode layer disposed on the opposite side of the fixed layer to the tunnel barrier layer, and a second electrode layer disposed on the opposite side of the free layer to the tunnel barrier layer; the tunneling magnetoresistive elements are arranged in a row or in a lattice array, the free layer and the second electrode layer are shared between two adjacent tunneling magnetoresistive elements, and each tunneling magnetoresistive element forms an independent island, and the first electrode layer is shared between adjacent islands by adjacent tunneling magnetoresistive elements, thereby constituting a tunneling magnetoresistive element array; Among the tunneling magnetoresistive elements, the distance between the free layers of adjacent tunneling magnetoresistive elements sharing the first electrode layer is 0.5 μm or less. A tunnel magnetoresistive sensor.
2. 2. The tunneling magnetoresistive sensor according to claim 1, wherein the distance between the free layers of adjacent tunneling magnetoresistive elements sharing the first electrode layer is 0.35 [mu]m or less.
3. 3. The tunneling magnetoresistive sensor according to claim 1, wherein the first electrode layer is an upper electrode, and the second electrode layer is a lower electrode.
Citation Information
Patent Citations
Magnetic resistance element, magnetic sensor and current sensor
JP2016021518A
Biomagnetism measuring device, biomagnetism measuring system, and biomagnetism measuring method
WO2012032962A1
Magnetic sensor
WO2016047782A1