Solid polymer fuel cell

The polymer electrolyte fuel cell addresses electrolyte deterioration by employing a counterflow structure and a strategically positioned third catalyst layer with hydrogen peroxide decomposition and redox abilities to enhance durability and performance.

JP7593047B2Active Publication Date: 2024-12-03KK TOYOTA CHUO KENKYUSHO
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
JP2020175301
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-10-19
Publication Date
2024-12-03
Estimated Expiration
2040-10-19

AI Technical Summary

Technical Problem

Existing polymer electrolyte fuel cells suffer from electrolyte deterioration due to hydrogen peroxide radicals generated during operation, which reduces durability and power generation performance, and existing solutions like platinum deposition or hydrogen peroxide decomposition catalysts are insufficient or inefficient due to fixed placement without considering in-plane environmental distribution.

Method used

A polymer electrolyte fuel cell design with a counterflow structure and a third catalyst layer inside the electrolyte membrane, having hydrogen peroxide decomposition, hydrogen redox, and oxygen redox abilities, positioned according to the in-plane environmental distribution to effectively decompose hydrogen peroxide and suppress radical generation.

Benefits of technology

The design effectively suppresses hydrogen peroxide and radical generation, thereby enhancing the durability and power generation performance of the fuel cell by strategically placing the third catalyst layer based on the flow direction of oxidizing and fuel gases.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007593047000001
    Figure 0007593047000001
  • Figure 0007593047000002
    Figure 0007593047000002
  • Figure 0007593047000003
    Figure 0007593047000003
Patent Text Reader

Abstract

To suppress deterioration of an electrolyte due to hydrogen peroxide in a solid polymer fuel cell.SOLUTION: A solid polymer fuel cell 10 comprises: a membrane electrode assembly 20 consisting of an anode catalyst layer 24a, an electrolyte membrane 22 and a cathode catalyst layer 24b; an anode gas diffusion layer 26a; a cathode gas diffusion layer 26b; an anode separator 28a; a cathode separator 28b; and a third catalyst layer 32 formed inside of the electrolyte membrane 22. The anode separator 28a and the cathode separator 28b include counterflow structures. The third catalyst layer 32 contains a third catalyst having hydrogen peroxide decomposition ability, hydrogen oxidation reduction ability and oxygen oxidation reduction ability and satisfies a relation of ydown>yup, however ydown and yup are average distances from the anode catalyst layer 24a to an anode side end of the third catalyst layer 32 at a downstream side and an upstream side of an oxidant passage.SELECTED DRAWING: Figure 1
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a polymer electrolyte fuel cell, and more particularly to a polymer electrolyte fuel cell capable of suppressing deterioration of an electrolyte caused by radicals. [Background technology]

[0002] A polymer electrolyte fuel cell includes a membrane electrode assembly (MEA) in which catalyst layers are bonded to both sides of an electrolyte membrane. Typically, a gas diffusion layer is further disposed on the outer side of the catalyst layer. Separators (also called current collectors) having gas flow paths are further disposed on both sides of the gas diffusion layer. A polymer electrolyte fuel cell typically includes a structure (fuel cell stack) in which a plurality of unit cells, each including such an MEA, gas diffusion layer, and separator, are stacked together.

[0003] During the operation of a polymer electrolyte fuel cell, hydrogen peroxide is generated in the anode catalyst layer, which turns into OH radicals through the Fenton reaction. It is known that the OH radicals deteriorate the electrolyte in the MEA. The deterioration of the electrolyte reduces the durability of the fuel cell or reduces the power generation performance of the fuel cell. Therefore, various proposals have been made to solve this problem.

[0004] For example, Patent Document 1 states: providing a mixture layer containing platinum-containing ions and / or platinum-containing complexes and a proton-conductive material on the anode catalyst layer side of the electrolyte membrane; A step of precipitating platinum contained in the platinum-containing ions and / or platinum-containing complexes; A method for manufacturing a fuel cell comprising the steps of:

[0005] The same document states: (A) By using such a method, a fuel cell having a platinum deposit layer disposed between the electrolyte membrane and the anode catalyst layer can be obtained; (B) If there is no platinum deposit layer between the electrolyte membrane and the anode catalyst layer, the permeated oxygen comes into contact with the carbon rather than the platinum in the anode catalyst layer, and undergoes two-electron reduction on the carbon, resulting in the production of a large amount of hydrogen peroxide; and (C) When a platinum deposit layer is present between the electrolyte membrane and the anode catalyst layer, the permeated oxygen undergoes four-electron reduction on the platinum in the platinum deposit layer, suppressing the production of hydrogen peroxide, thereby suppressing the production of OH radicals and the deterioration of the electrolyte membrane caused by OH radicals. is stated.

[0006] In Patent Document 2, A composite membrane in which an ion exchange material is impregnated into the pores of expanded polytetrafluoroethylene; an electrically insulating layer formed on one surface of the composite film; Platinum-supported carbon particles dispersed in the electrically insulating layer; A solid polymer electrolyte membrane comprising: The document describes that dispersing platinum-loaded carbon particles in the electrical insulating layer extends the life of the electrolyte membrane.

[0007] Patent Document 3 discloses a solid polymer electrolyte fuel cell in which a hydrogen peroxide decomposition catalyst coated with a hydrogen ion conductive polymer electrolyte is added to at least one of the anode catalyst layer or the cathode catalyst layer. The same document states: (A) Peroxides not only deteriorate the electrolyte membrane but also the proton-conductive polymer electrolyte in the catalyst layer; and (B) The addition of a hydrogen peroxide decomposition catalyst to the catalyst layer improves the decomposition of hydrogen peroxide. is stated.

[0008] In Non-Patent Document 1, it is stated that, of the platinum that dissolves from the catalyst layer and deposits in the electrolyte membrane during the operation of the fuel cell, (a) Star-shaped and dendritic particles with high particle density and high specific surface area have high catalytic activity for scavenging peroxides and consuming crossover gases (i.e., have a positive effect on the durability of the electrolyte membrane), whereas (b) Small and dispersed cubic particles either have no effect or have a negative effect on the durability of the electrolyte membrane. It is stated that:

[0009] Furthermore, Non-Patent Document 2 describes that during an oxygen reduction reaction in an environment with a low potential, the production rate of hydrogen peroxide tends to increase.

[0010] During operation of a polymer electrolyte fuel cell, most of the oxygen supplied to the cathode is reduced at the cathode, but some crosses over within the electrolyte membrane and is transported from the cathode to the anode. The oxygen that reaches the anode is reduced at the anode. However, the anode is in a low potential state during operation of a polymer electrolyte fuel cell. When an oxygen reduction reaction occurs in a low potential environment, a relatively large amount of hydrogen peroxide is generated. Furthermore, when the generated hydrogen peroxide becomes a radical through the Fenton reaction, the radical decomposes the polymer electrolyte, causing the deterioration of the electrolyte membrane and catalyst layer.

[0011] To solve this problem, a method of forming a platinum deposit layer between the electrolyte membrane and the anode catalyst layer has been proposed in Patent Document 1. However, since the platinum deposit layer is in a hydrogen-rich environment (low potential environment), the generation of hydrogen peroxide is unavoidable, and the effect is thought to be limited. Furthermore, Patent Document 3 proposes adding a hydrogen peroxide decomposition catalyst to the catalyst layer. However, even if the method described in this document can suppress the deterioration of the catalyst layer to some extent, its effect of suppressing the deterioration of the electrolyte membrane is considered to be limited.

[0012] In addition, during the operation of a polymer electrolyte fuel cell, the fuel gas and oxidant gas flow in one direction from the inlet to the outlet of the gas flow channel, and the concentrations of fuel (hydrogen) and oxygen decrease toward the downstream side of the fuel gas and oxidant gas flow. As a result, a distribution occurs in the in-plane environment of the MEA, and the amount and location of hydrogen peroxide generation change depending on this in-plane environment distribution. Therefore, if a hydrogen peroxide decomposition catalyst is placed at a fixed position in the MEA without considering the in-plane environment distribution, a sufficient hydrogen peroxide decomposition effect cannot be obtained. Furthermore, there have been no conventional proposals for a fuel cell in which a catalyst having hydrogen peroxide decomposition ability, hydrogen oxidation-reduction ability, and oxygen oxidation-reduction ability is arranged at an appropriate position according to the in-plane environment distribution of the MEA. [Prior art documents] [Patent documents]

[0013] [Patent Document 1] JP 2006-351320 A [Patent Document 2] JP 2017-054819 A [Patent Document 3] JP 2003-123777 A [Non-patent literature]

[0014] [Non-Patent Document 1] N. Macauley et al., J. Power Sources 299(2015) 139-148 [Non-Patent Document 2] K. Ke, et al., Rlectrochimica Acta 56(2011) 2098-2104 Summary of the Invention [Problem to be solved by the invention]

[0015] The problem that the present invention aims to solve is to provide a solid polymer fuel cell in which a catalyst having hydrogen peroxide decomposition ability, hydrogen oxidation-reduction ability, and oxygen oxidation-reduction ability is arranged at an appropriate position according to the in-plane environment distribution of the MEA. Another problem to be solved by the present invention is to suppress deterioration of the electrolyte caused by hydrogen peroxide in a polymer electrolyte fuel cell. [Means for solving the problem]

[0016] In order to solve the above problems, the polymer electrolyte fuel cell according to the present invention has the following configuration. (1) The solid polymer electrolyte fuel cell is a membrane electrode assembly in which an anode catalyst layer is bonded to one surface of an electrolyte membrane and a cathode catalyst layer is bonded to the other surface of the electrolyte membrane; an anode gas diffusion layer disposed on the outer side of the anode catalyst layer; a cathode gas diffusion layer disposed on the outer side of the cathode catalyst layer; an anode separator disposed on the outer side of the anode gas diffusion layer; a cathode separator disposed on the outer side of the cathode gas diffusion layer; a third catalyst layer formed inside the electrolyte membrane; It is equipped with: (2) The anode separator and the cathode separator have a counterflow structure in which the fuel gas and the oxidant gas flow in opposite directions. (3) The third catalyst layer includes a third catalyst having a hydrogen peroxide decomposition ability, a hydrogen oxidation-reduction ability, and an oxygen oxidation-reduction ability. (4) The third catalyst layer satisfies the relationship of the following formula (1). y down >y up …(1) however, y down is the average distance from the interface between the anode catalyst layer and the electrolyte membrane to the anode side end of the third catalyst layer on the downstream side of the oxidant flow path of the cathode separator, y upis the average distance from the interface between the anode catalyst layer and the electrolyte membrane to the anode side end of the third catalyst layer on the upstream side of the oxidant flow path. Effect of the Invention

[0017] In a solid polymer electrolyte fuel cell with a counterflow structure, the oxygen partial pressure (p O2 ) becomes higher, and the hydrogen partial pressure in the anode gas (p H2 Conversely, downstream of the oxidizer flow path (upstream of the fuel flow path), the oxygen partial pressure (p O2 ) is lower, and the hydrogen partial pressure in the anode gas (p H2 As a result, if the distance y0 from the anode catalyst layer / electrolyte membrane interface to the position where the potential inside the electrolyte membrane is high enough to suppress the production of hydrogen peroxide, y0 increases toward the downstream side of the oxidant flow path.

[0018] Therefore, when a third catalyst having hydrogen peroxide decomposition ability, hydrogen oxidation-reduction ability, and oxygen oxidation-reduction ability is disposed inside the electrolyte membrane, (a) a third catalyst is disposed closer to the anode on the upstream side of the oxidant flow path, and (b) The third catalyst is arranged closer to the cathode on the downstream side of the oxidant flow path. By changing the position of the third catalyst according to the flow directions of the oxidant gas and the fuel gas, it is possible to suppress the generation of hydrogen peroxide and radicals, as well as the deterioration of the electrolyte due to the radicals. [Brief description of the drawings]

[0019] [Figure 1] 1 is a cross-sectional schematic diagram of a polymer electrolyte fuel cell according to the present invention. [Diagram 2] FIG. 11 is a graph showing the relationship between the position (y) in the membrane thickness direction of the third catalyst layer and the average hydrogen peroxide concentration in the electrolyte membrane. [Diagram 3] FIG. 13 is a diagram showing the relationship between the position (y) in the film thickness direction of the third catalytic layer and the potential of the third catalytic layer. [Figure 4] FIG. 4 is a diagram showing the relationship between the position (x) in the oxidant gas flow direction and the appropriate position (y) in the film thickness direction of a third catalyst layer. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0020] An embodiment of the present invention will be described in detail below. [1. Polymer electrolyte fuel cell] FIG. 1 is a schematic cross-sectional view of a polymer electrolyte fuel cell according to the present invention. In FIG. 1, a polymer electrolyte fuel cell 10 includes: A membrane electrode assembly (MEA) 20 in which an anode catalyst layer 24a is bonded to one surface of an electrolyte membrane 22 and a cathode catalyst layer 24a is bonded to the other surface of the electrolyte membrane 22; an anode gas diffusion layer 26a disposed on the outer side of the anode catalyst layer 24a; a cathode gas diffusion layer 26b disposed on the outer side of the cathode catalyst layer 24b; an anode separator 28a disposed on the outer side of the anode gas diffusion layer 26a; a cathode separator 28b disposed on the outer side of the cathode gas diffusion layer 26b; A third catalyst layer 32 formed inside the electrolyte membrane 22; It is equipped with:

[0021] [1.1. MEA] [1.1.1. Electrolyte membrane] In the present invention, the material of the electrolyte membrane 22 is not particularly limited. Examples of the material of the electrolyte membrane 22 include: (a) perfluorocarbon sulfonic acid polymers such as Nafion®, Flemion®, Aquivion®, and Aciplex®; (b) A highly oxygen-permeable ionomer containing an acid group and a cyclic structure in its molecular structure. etc.

[0022] [1.1.2. Anode catalyst layer and cathode catalyst layer] An anode catalyst layer 24a is bonded to one surface of the electrolyte membrane 22, and a cathode catalyst layer 24b is bonded to the other surface. The anode catalyst layer 24a and the cathode catalyst layer 24b are reaction fields for the electrode reaction. There are no particular limitations on the materials for the anode catalyst layer 24a and the cathode catalyst layer 24b, as long as they are capable of causing the electrode reaction to proceed. In general, in the solid polymer fuel cell 10, the anode catalyst layer 24a and the cathode catalyst layer 24b each use a composite of an electrode catalyst containing platinum or a platinum alloy and a catalyst layer ionomer.

[0023] [1.2. Anode gas diffusion layer and cathode gas diffusion layer] An anode gas diffusion layer 26a is disposed on the outer side of the anode catalyst layer 24a. A cathode gas diffusion layer 26b is disposed on the outer side of the cathode catalyst layer 24b. The anode gas diffusion layer 26a and the cathode gas diffusion layer 26b are provided to supply reactant gases (fuel gas, oxidant gas) supplied from the anode separator 28a and the cathode separator 28b to the anode catalyst layer 24a and the cathode catalyst layer 24a, respectively.

[0024] In the present invention, the materials for the anode gas diffusion layer 26a and the cathode gas diffusion layer 26b are not particularly limited as long as they are capable of supplying reactant gas to the catalyst layer and capable of transferring electrons between the catalyst layer and the material. The anode gas diffusion layer 26a and the cathode gas diffusion layer 26b may be made of a material such as a porous metal body or a carbon fiber nonwoven fabric.

[0025] [1.3. Anode separator and cathode separator] An anode separator 28a is disposed on the outer side of the anode gas diffusion layer 26a. A fuel flow passage 30a is provided within the anode separator 28a. A cathode separator 28b is disposed on the outer side of the cathode gas diffusion layer 26b. An oxidant flow path 30b is provided in the cathode separator 28b. The anode separator 28a and the cathode separator 28a are for supplying reactant gases to the anode gas diffusion layer 26a and the cathode gas diffusion layer 26a, respectively.

[0026] In the present invention, the anode separator 28a and the cathode separator 28b have a counterflow structure in which the fuel gas and the oxidant gas flow in opposite directions. Other aspects of the structures of the anode separator 28a and the cathode separator 28b are not particularly limited, and an optimal structure can be selected depending on the purpose. The material of the anode separator 28a and the cathode separator 28b is not particularly limited as long as it is capable of supplying reactive gas and transferring electrons, and an optimum material can be selected according to the purpose. Examples of the material of the anode separator 28a and the cathode separator 28b include stainless steel, titanium, and titanium alloy.

[0027] [1.4. Third catalyst layer] [1.4.1. Third catalyst] In the present invention, a third catalyst layer 32 containing a third catalyst is formed inside the electrolyte membrane 22. This is different from the conventional technology. Here, the "third catalyst" refers to a catalyst having the ability to decompose hydrogen peroxide, the ability to oxidize and reduce hydrogen, and the ability to oxidize and reduce oxygen.

[0028] The third catalyst is required to have the ability to decompose hydrogen peroxide in order to decompose hydrogen peroxide produced as a by-product in the MEA 20 into water and oxygen in the third catalyst layer 32 . The reason why the third catalyst is required to have hydrogen oxidation-reduction ability and oxygen oxidation-reduction ability is that oxygen crossed over from the cathode catalyst layer 24b is converted into water by reacting with protons or hydrogen diffused or crossed over from the anode catalyst layer 24a in the third catalyst layer 32. In general, the less crossover oxygen that reaches the anode catalyst layer 24a, the less hydrogen peroxide is produced in the anode catalyst layer 24a.

[0029] The type of the third catalyst is not particularly limited as long as it has the above-mentioned function. Examples of the third catalyst include platinum and platinum alloys. The third catalyst may exist alone in the third catalyst layer 32, or may exist in a state supported on the surface of a carrier. When the third catalyst is supported on the surface of a carrier, the carrier does not necessarily need to be an electron conductor and may be an insulator.

[0030] [1.4.2. Structure of the third catalyst layer] The structure of the third catalyst layer 32 is as follows: (a) hydrogen peroxide produced in the anode catalyst layer 24a can be effectively decomposed; (b) capable of effectively reducing crossover oxygen; and (c) It does not impede power generation by the polymer electrolyte fuel cell 10 (i.e., it does not impede proton transport from the anode catalyst layer 24a to the cathode catalyst layer 24b). As far as possible, there is no particular limitation. For example, the third catalyst layer 32 may be a layer in which a particulate third catalyst or a particulate carrier carrying the third catalyst is dispersed discretely or continuously in the in-plane direction of the electrolyte membrane 22. Alternatively, the third catalyst layer 32 may be a thin film made of a third catalyst formed by sputtering or the like, so long as it does not impede power generation.

[0031] [1.5. Shape and arrangement of the third catalyst layer] [1.5.1. Formula (1)] In the present invention, the third catalyst layer 32 must at least satisfy the relationship of the following formula (1). y down >y up …(1) however, y down is the average distance from the interface between the anode catalyst layer 24a and the electrolyte membrane 22 to the anode side end of the third catalyst layer 32 on the downstream side of the oxidant flow path 30b of the cathode separator 28b, y upis the average distance from the interface between the anode catalyst layer 24a and the electrolyte membrane 22 to the anode side end of the third catalyst layer 32 on the upstream side of the oxidant flow path 30b.

[0032] Here, the "downstream side of the oxidant flow channel 30b" refers to the region from the center to the outlet of the oxidant flow channel 30b provided in the cathode separator 28b. The "upstream side of the oxidant flow channel 30b" refers to the region from the inlet to the center of the oxidant flow channel 30b provided in the cathode separator 28b.

[0033] As described later, the potential in the electrolyte membrane 22 increases from the anode catalyst layer 24a toward the cathode catalyst layer 24b. When the distance (y) in the membrane thickness direction from the interface between the anode catalyst layer 24a and the electrolyte membrane 22 to the anode side end of the third catalyst layer 32 exceeds a certain critical value, the potential in the electrolyte membrane 22 increases abruptly. If the critical value of y when the potential increases abruptly is "y0", y0 increases toward the downstream side of the oxidant flow path 30b.

[0034] Furthermore, when the third catalyst layer 32 is closer to the anode catalyst layer 24a than y0, the third catalyst layer 32 is exposed to a low potential environment, and the third catalyst may actually promote the production of hydrogen peroxide. On the other hand, when the third catalyst layer 32 is closer to the cathode catalyst layer 24b than y0, the third catalyst layer 32 is exposed to a high potential environment, and the third catalyst promotes the decomposition of hydrogen peroxide. In any potential environment, in the presence of crossover hydrogen, the third catalyst reduces crossover oxygen. Therefore, in order to suppress the production of hydrogen peroxide, the third catalyst layer 32 must at least satisfy formula (1).

[0035] The shape and arrangement of the third catalyst layer 32 are not particularly limited as long as they satisfy formula (1). In Fig. 1, the third catalyst layer 32 is composed of a flat region with a constant thickness, and is arranged in the electrolyte membrane 22 so that y increases linearly toward the downstream side of the oxidant flow path 30b, but this is merely an example. For example, the third catalyst layer 32 may consist of a flat region of non-uniform thickness, and may be disposed within the electrolyte membrane 22 such that y increases linearly, curvedly, or stepwise toward the downstream side of the oxidant flow path 30b. Alternatively, the third catalyst layer 32 may consist of a bent or curved plate-like region having a uniform or non-uniform thickness, and may be disposed within the electrolyte membrane 22 such that y increases curvilinearly or stepwise toward the downstream side of the oxidant flow path 30b.

[0036] [1.5.2. Position in the electrolyte membrane along the membrane thickness] The above-mentioned critical value y0 depends on the operating conditions (particularly the cathode oxygen partial pressure and the anode hydrogen partial pressure) of the polymer electrolyte fuel cell 10. However, when air is used as the oxidant gas, it is highly unlikely that y0 will be equal to or less than half the thickness δ of the electrolyte membrane 22. Therefore, the third catalyst layer 32 is preferably disposed in the region from the center of the electrolyte membrane 12 in the thickness direction to the interface between the cathode catalyst layer 24b and the electrolyte membrane 22.

[0037] [1.5.3. Optimal Position] The third catalyst layer 32 preferably satisfies the following formula (2). {0.23(x / L)+0.73}δ≦y≦{0.06(x / L)+0.94}δ …(2) however, L is the total distance from the inlet to the outlet of the oxidant flow path 30b, x is the position in the oxidant gas flow direction, δ is the thickness of the electrolyte membrane 22, y is the distance from the interface between the anode catalyst layer 24a and the electrolyte membrane 22 to the anode side end of the third catalyst layer 32 when the position in the oxidant gas flow direction is x. Here, the "position in the flow direction of the oxidant gas" refers to the distance from the inlet of the oxidant flow passage 30b, which is the origin, to an arbitrary position on the outlet side of the oxidant flow passage 30b.

[0038] Equation (2) represents the range of variation of the critical value y0 when air is used as the oxidant gas and the operating conditions of the polymer electrolyte fuel cell 10 are varied within a realistic range. This range does not depend on the active species of the third catalyst layer 32. In other words, "the third catalyst layer 32 satisfies formula (2)" means that the entire third catalyst layer 32 is disposed within the region represented by formula (2). When the entire third catalyst layer 32 is within the region represented by formula (2), all the third catalysts are placed in a high potential environment, so that the third catalysts suppress the generation of hydrogen peroxide and promote the reduction of crossover oxygen. The process of deriving formula (2) will be described later.

[0039] [2. Manufacturing method of polymer electrolyte fuel cells] The polymer electrolyte fuel cell 10 including the third catalyst layer 32 can be manufactured by various methods.

[0040] [2.1. First Method] For example, after preparing a polymer electrolyte fuel cell 10' that does not include a third catalyst layer 32, a potential fluctuation is applied under conditions where the stoichiometric ratio is 1.0 to 2.0 and / or the anode inlet pressure is greater than the cathode inlet pressure. This causes an electrode catalyst component (e.g., platinum) to dissolve from the cathode catalyst layer 24b, and the dissolved component precipitates in the electrolyte membrane to become the third catalyst. At this time, by optimizing the operating conditions of the polymer electrolyte fuel cell 10', the third catalyst layer can be precipitated at a position that satisfies formula (1) or formula (2).

[0041] [2.2. Second Method] Alternatively, an electrolyte membrane 22a having a non-uniform thickness in the in-plane direction is prepared. Next, a third catalyst layer 32 is formed on the surface of the electrolyte membrane 22a by using a method such as spray coating or transfer. Furthermore, a thin electrolyte membrane 22b is laminated on the surface of the third catalyst layer 32 to obtain an electrolyte membrane 22 consisting of an electrolyte membrane 22a / third catalyst layer 32 / electrolyte membrane 22b laminate. At this time, by optimizing the thicknesses of the electrolyte membranes 22a and 22b, the third catalyst layer 32 can be disposed at a position that satisfies formula (1) or formula (2).

[0042] An anode catalyst layer 24a and a cathode catalyst layer 24b are bonded to both sides of the electrolyte membrane 22 obtained in this manner to obtain the MEA 20. Furthermore, an anode gas diffusion layer 26a and a cathode gas diffusion layer 26b are laminated on both sides of the MEA 20, and an anode separator 28a and a cathode separator 28b are further laminated on the outsides thereof to obtain the polymer electrolyte fuel cell 10 according to the present invention.

[0043] [3. Derivation of Equation (2)] [3.1. Appropriate position (y0)] When electricity was generated under various conditions using a solid polymer electrolyte fuel cell with a third catalyst layer in the electrolyte membrane, the average hydrogen concentration in the electrolyte membrane and the potential of the third catalyst layer in the electrolyte membrane were calculated by numerical simulation. The third catalyst was assumed to be platinum, but the same argument can be applied to the case of other active species. The third catalyst layer was disposed at a certain position from the interface between the electrolyte membrane 22 and the anode catalyst layer 24a. The position in the membrane thickness direction of the third catalyst layer was set to any position between the anode catalyst layer / electrolyte membrane interface and the electrolyte membrane / cathode catalyst layer interface. Furthermore, the H2 partial pressure of the anode catalyst layer (aCL) was set to 50 kPa or 100 kPa, and the O2 partial pressure of the cathode catalyst layer (cCL) was set to 10.5 kPa or 21.0 kPa.

[0044] FIG. 2 shows the relationship between the position (y) in the membrane thickness direction of the third catalyst layer and the average hydrogen peroxide concentration in the electrolyte membrane. (a) In order to reduce the hydrogen peroxide concentration by the third catalyst layer, it is necessary to form the third catalyst layer at a position closer to the cathode catalyst layer than a certain degree; and (b) The optimal position for forming the third catalyst layer depends on the H2 partial pressure in the anode catalyst layer and the O2 partial pressure in the cathode catalyst layer. You can see that.

[0045] Figure 3 shows the relationship between the position (y) in the film thickness direction of the third catalytic layer and the potential of the third catalytic layer. It can be seen from Figure 3 that the "region where the hydrogen peroxide concentration decreases" in Figure 2 corresponds to the "region where the potential of the third catalytic layer increases." This is thought to be because the generation of hydrogen peroxide can be suppressed in the region where the potential is high (see Non-Patent Document 2).

[0046] The "region where the potential becomes higher" in FIG. 3 is located approximately 3% closer to the cathode catalyst layer than the position where the component of the electrode catalyst (platinum) eluted from the cathode catalyst layer is deposited. Here, the position where the dissolved platinum precipitates (δ Pt ) is the hydrogen partial pressure (p H2 ) and the oxygen partial pressure in the cathode catalyst layer (p O2 ) can be simply calculated using the following formula (3). [Reference 1] J. Zhang, et al., J. Electrochem. Soc., 154, 10, B1006-B1011 (2007)

[0047] δ Pt =K H2 p H2 δ / (K H2 p H2 +2K O2 p O2 ) …(3) however, K H2 is the hydrogen permeability coefficient in the electrolyte membrane, K O2 is the oxygen permeability coefficient in the electrolyte membrane, δ is the thickness of the electrolyte membrane.

[0048] When the electrolyte membrane is made of 1100EW perfluorosulfonic acid (PFSA) membrane and the temperature of the electrolyte membrane is 80°C, K H2 =3.3×10 -13 (cm s kPa) K O2 =1.6×10 -13 (cm s kPa) (See Reference 1.) In addition, K H2 and K. O2 The value of depends on the type of electrolyte membrane, but as shown in equation (4) below, K H2 and K. O2 Only the ratio of K affects the value of y0. H2 and K. O2 The ratio of is not expected to change significantly even when the EW is changed, so equation (4) is not limited to the PFSA of 1100EW.

[0049] The appropriate position (y0) of the third catalyst layer is δ Pt Using the fact that the cathode catalyst layer is located approximately 3% closer to the cathode catalyst layer, this can be expressed as the following formula (4). y0=1.03K H2 p H2 δ / (K H2 p H2 +2K O2 p O2 ) …(4)

[0050] [3.2. In-plane distribution of appropriate positions (y0)] [3.2.1. Cathode inlet pressure>Anode inlet pressure] First, assume that the cathode inlet pressure is greater than the anode inlet pressure. This case corresponds to the case where y0 becomes extremely small.

[0051] In the case where the polymer electrolyte fuel cell has a counterflow structure, (a) The oxygen partial pressure at the cathode inlet is 0.42 atm. (b) The oxygen partial pressure at the cathode outlet is 0.14 atm. (c) The hydrogen partial pressure at the anode inlet is 1.00 atm. (d) The hydrogen partial pressure at the anode outlet is set to 0.50 atm. Then, from equation (4), the optimal position (y0) is obtained as follows: y0=0.73δ at the cathode inlet (=anode outlet) y0=0.96δ at the cathode outlet (=anode inlet)

[0052] The straight line passing through the above two points can be expressed as the following equation (2a). y0={0.23(x / L)+0.73}δ …(2a)

[0053] [3.2.2. Cathode inlet pressure < Anode inlet pressure] Next, consider the case where the cathode inlet pressure is less than the anode inlet pressure. This case corresponds to the case where y0 becomes extremely large.

[0054] In the case where the polymer electrolyte fuel cell has a counterflow structure, (a) The oxygen partial pressure at the cathode inlet is 0.21 atm. (b) The oxygen partial pressure at the cathode outlet is 0.07 atm. (c) The hydrogen partial pressure at the anode inlet is 2.00 atm. (d) The hydrogen partial pressure at the anode outlet is set to 1.00 atm. Then, from equation (4), the optimal position (y0) is obtained as follows: y0=0.94δ at the cathode inlet (=anode outlet) y0=1.00δ at the cathode outlet (=anode inlet)

[0055] The straight line passing through the above two points can be expressed as the following equation (2b). y0={0.06(x / L)+0.94}δ …(2b)

[0056] [3.2.3. Range of appropriate positions (y0)] Equation (2a) represents the condition where y0 becomes extremely small, and equation (2b) represents the condition where y0 becomes extremely large. Therefore, the region between equations (2a) and (2b), that is, the region represented by the above equation (2), is considered to be the appropriate design region. FIG. 4 shows the relationship between the position (x) in the oxidant gas flow direction thus obtained and the appropriate position (y) in the film thickness direction of the third catalyst layer.

[0057] [4. Effect] In a solid polymer electrolyte fuel cell with a counterflow structure, the oxygen partial pressure (p O2 ) becomes higher, and the hydrogen partial pressure in the anode gas (p H2 Conversely, downstream of the oxidizer flow path (upstream of the fuel flow path), the oxygen partial pressure (p O2 ) is lower, and the hydrogen partial pressure in the anode gas (p H2 As a result, if the distance y0 from the anode catalyst layer / electrolyte membrane interface to the position where the potential inside the electrolyte membrane is high enough to suppress the production of hydrogen peroxide, y0 increases toward the downstream side of the oxidant flow path.

[0058] Therefore, when a third catalyst having hydrogen peroxide decomposition ability, hydrogen oxidation-reduction ability, and oxygen oxidation-reduction ability is disposed inside the electrolyte membrane, (a) a third catalyst is disposed closer to the anode on the upstream side of the oxidant flow path, and (b) The third catalyst is arranged closer to the cathode on the downstream side of the oxidant flow path. By changing the position of the third catalyst according to the flow directions of the oxidant gas and the fuel gas, it is possible to suppress the generation of hydrogen peroxide and radicals, as well as the deterioration of the electrolyte due to the radicals.

[0059] Although the embodiment of the present invention has been described in detail above, the present invention is not limited to the above embodiment, and various modifications are possible without departing from the gist of the present invention. [Industrial Applicability]

[0060] The polymer electrolyte fuel cell according to the present invention can be used as an on-vehicle power source, a stationary power generator, and the like. [Explanation of symbols]

[0061] 10 Polymer electrolyte fuel cell 20 Membrane electrode assembly (MEA) 22 Electrolyte membrane 24a Anode catalyst layer 24b Cathode catalyst layer 26a Anode gas diffusion layer 26b Cathode gas diffusion layer 28a Anode separator 28b Cathode separator 32 Third catalyst layer

Claims

1. A polymer electrolyte fuel cell having the following configuration. (1) The solid polymer electrolyte fuel cell is a membrane electrode assembly in which an anode catalyst layer is bonded to one surface of an electrolyte membrane and a cathode catalyst layer is bonded to the other surface of the electrolyte membrane; an anode gas diffusion layer disposed on the outer side of the anode catalyst layer; a cathode gas diffusion layer disposed on the outer side of the cathode catalyst layer; an anode separator disposed on the outer side of the anode gas diffusion layer; a cathode separator disposed on the outer side of the cathode gas diffusion layer; a third catalyst layer formed inside the electrolyte membrane; It is equipped with: (2) The anode separator and the cathode separator have a counterflow structure in which the fuel gas and the oxidant gas flow in opposite directions. (3) The third catalyst layer includes a third catalyst having a hydrogen peroxide decomposition ability, a hydrogen oxidation-reduction ability, and an oxygen oxidation-reduction ability. (4) The third catalyst layer satisfies the relationship of the following formula (2). {0.23(x / L)+0.73}δ≦y≦{0.06(x / L)+0.94}δ…(2) however, L is the total distance from the inlet to the outlet of the oxidant channel of the cathode separator, x is the position in the flow direction of the oxidant gas, δ is the thickness of the electrolyte membrane, y is the distance from the interface between the anode catalyst layer and the electrolyte membrane to the anode side end of the third catalyst layer when the position in the oxidant gas flow direction is x.

2. The solid polymer electrolyte fuel cell according to claim 1 , wherein the third catalyst contains platinum or a platinum alloy.

Citation Information

Patent Citations

  • Polymer electrolyte fuel cell

    JP2003123777A

  • Manufacturing method of fuel cell

    JP2006351320A

  • Membrane-electrode assembly for fuel cell, and fuel cell using it

    JP2008204664A

  • Membrane electrode assembly for fuel cell, and fuel cell using the same

    JP2008243378A

  • Solid polymer electrolyte and process for making the same

    JP2017054819A