MEMS (Micro Electro Mechanical Systems) Resonators
By forming metallic glass on the piezoelectric film in the MEMS resonator structure, stress variations are minimized, allowing for effective annealing to tune the resonance frequency and enhance performance.
Patent Information
- Application Number
- JP2021139946
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Filing Date
- 2021-08-30
- Publication Date
- 2024-12-04
- Estimated Expiration
- 2041-08-30
AI Technical Summary
Existing MEMS resonators face challenges in achieving desired resonance frequencies and characteristics due to stress variations in metallic glass when the piezoelectric film is formed at temperatures exceeding the annealing temperature of the metallic glass, preventing effective stress control.
The MEMS resonator structure is redesigned with the metallic glass formed on the piezoelectric film instead of the conventional approach, allowing for annealing treatments to adjust the resonance frequency by controlling stress after film formation, ensuring desired characteristics are met.
This structure enables precise tuning of the resonance frequency and improves the MEMS resonator's performance by reducing stress variations, thereby achieving the desired characteristics.
Smart Images

Figure 0007594259000001 
Figure 0007594259000002 
Figure 0007594259000003
Abstract
Description
[Technical field]
[0001] The present invention relates to a MEMS resonator configured with a semiconductor device having a MEMS structure. [Background technology]
[0002] Conventionally, Patent Document 1 has proposed improving the characteristics of MEMS sensors by using metallic glass with a high elastic modulus as a membrane material. Specifically, Patent Document 1 proposes a structure in which metallic glass is produced by sputtering on a substrate made of silicon, and then a piezoelectric film is formed on the metallic glass.
[0003] On the other hand, it is known that annealing metallic glasses can control the stress generated in the metallic glasses to a value that depends on the annealing temperature. By utilizing this, it is possible to reduce the variation in the stress generated in metallic glasses by performing annealing individually after stress measurement. [Prior art documents] [Patent documents]
[0004] [Patent Document 1] JP 2008-155333 A Summary of the Invention [Problem to be solved by the invention]
[0005] However, in the structure described in Patent Document 1, since a piezoelectric film is disposed on a metallic glass, for example, when aluminum nitride (AlN) is used as the piezoelectric film, the film formation temperature is 350°C or higher, which exceeds the annealing temperature of the metallic glass. Therefore, the metallic glass cannot be annealed to control the stress, and the stress variation cannot be reduced. Specifically, in the case of manufacturing a MEMS resonator, the metallic glass cannot be annealed to match the desired resonant frequency, and the desired characteristics cannot be obtained.
[0006] In view of the above, an object of the present invention is to provide a MEMS resonator having a structure that can be matched to a target resonant frequency and can achieve desired characteristics. [Means for solving the problem]
[0007] In order to achieve the above object, the MEMS vibrator described in claim 1 has a substrate (10) in which an opening (11) is formed and which has a base portion (12) constituting a peripheral wall surrounding the opening, a lower electrode (20) formed on one side of the substrate so as to cover the opening, a piezoelectric film (30) formed on the lower electrode, and metallic glass (40) formed on the piezoelectric film, and a membrane is formed including the lower electrode, the piezoelectric film, and the metallic glass.
[0008] In this way, instead of forming a piezoelectric film on metallic glass, the MEMS resonator has a structure in which metallic glass is formed on a piezoelectric film. This makes it possible to prevent temperatures higher than the deposition temperature of the piezoelectric film from being applied to the metallic glass. Therefore, after forming the metallic glass, it is possible to anneal it according to the desired characteristics, thereby adjusting the resonant frequency. This makes it possible to obtain a MEMS resonator with a structure that can achieve the desired characteristics.
[0009] Note that the reference symbols in parentheses attached to each component indicate an example of the correspondence between the component and specific components described in the embodiments described below. [Brief description of the drawings]
[0010] [Figure 1] 1 is a cross-sectional view of a MEMS resonator according to a first embodiment of the present invention. [Diagram 2] FIG. 2 is a top view of the MEMS resonator shown in FIG. [Figure 3A] 2A to 2C are cross-sectional views showing the MEMS resonator shown in FIG. 1 during a manufacturing process. [Figure 3B] 3B is a cross-sectional view showing a state of the MEMS resonator during the manufacturing process subsequent to FIG. 3A. [Figure 3C] 3C is a cross-sectional view showing the state of the MEMS resonator during the manufacturing process subsequent to FIG. 3B. [Figure 4] FIG. 4 is a cross-sectional view of a MEMS resonator according to a second embodiment of the present invention. [Diagram 5] FIG. 5 is a top view of the MEMS resonator shown in FIG. [Figure 6] FIG. 11 is a cross-sectional view of a MEMS resonator according to a third embodiment of the present invention. [Figure 7] FIG. 7 is a top view of the MEMS resonator shown in FIG. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0011] Hereinafter, embodiments of the present invention will be described with reference to the drawings. In the following embodiments, parts that are the same or equivalent to each other will be denoted by the same reference numerals.
[0012] (First embodiment) A MEMS vibrator according to a first embodiment will be described. The MEMS vibrator described in this embodiment is applied to, for example, an ultrasonic transducer. The MEMS vibrator according to this embodiment will be described below with reference to Figs. 1 and 2. Note that the MEMS vibrator 1 shown in Figs. 1 and 2 shows, for example, an element portion of an ultrasonic transducer, and is provided with a wiring structure, a control unit, and the like (not shown) to configure the ultrasonic transducer.
[0013] The MEMS vibrator 1 is formed using MEMS technology, and as shown in FIG. 1, has a configuration in which a membrane is formed on a substrate 10 by providing a lower electrode 20, a piezoelectric film 30, metallic glass 40, and an upper electrode 50.
[0014] The substrate 10 is made of, for example, silicon (Si), and is made of a Si substrate with one surface on which the lower electrode 20 and the like are arranged as the front surface and the opposite surface as the back surface. As shown in FIG. 2, the substrate 10 has a rectangular top surface shape, a square shape in this case, an opening 11 is formed inside, and the substrate 10 is structured with a pedestal portion 12 formed by a peripheral wall surrounding the periphery of the opening 11. The opening 11 is formed by drilling a hole in the substrate 10 from the back surface side in the direction of the central axis, with the normal direction to one surface of the substrate 10 being the central axis direction. Here, the opening 11 is formed by drilling a cylindrical hole from the back surface of the substrate 10 around the central axis. The dimensions of the opening 11 are arbitrary, but are designed to correspond to the intended resonant frequency of the membrane.
[0015] The lower electrode 20 is composed of a metal film composed of a single layer film or a multi-layer film of, for example, platinum (Pt), aluminum (Al), gold (Au), titanium (Ti), etc. The lower electrode 20 is formed on one surface of the front side of the base material 10 in a portion corresponding to at least a part of the opening 11, and in this embodiment, is formed so as to cover the opening 11. In other words, the lower electrode 20 is formed so as to extend from the outer circumferential end of the pedestal portion 12 to the inner end and further to the entire area inside the opening 11, and in this embodiment, the upper surface shape is a square shape.
[0016] The piezoelectric film 30 is formed on the lower electrode 20 and below the metallic glass 40, and similar to the lower electrode 20, is formed on the entire front surface side of the substrate 10 so as to cover the opening 11. That is, the piezoelectric film 30 is also formed so as to extend from the outer circumferential end of the pedestal portion 12 to the inner end and further to the entire area inside the opening 11, and in this embodiment, the upper surface shape is rectangular. The piezoelectric film 30 is made of a piezoelectric material such as AlN or lead zirconate titanate (PZT).
[0017] The metallic glass 40 is formed on the piezoelectric film 30, and in this embodiment, is formed so as to cover at least the entire opening 11 and reach the boundary line between the opening 11 and the pedestal 12. The metallic glass 40 may be formed so as to cover the opening 11 on the entire front surface side of the substrate 10, similar to the lower electrode 20, and this is the configuration adopted in this embodiment. The metallic glass 40 may also be extended to a position not reaching the outer edge of the substrate 10, that is, to stop at a position inside the outer edge of the substrate 10.
[0018] The metallic glass 40 is a non-crystalline alloy mainly composed of metal elements, and is an amorphous metal in which a glass transition is observed. The raw material of the metallic glass 40 is a metal, but when cooled rapidly from a molten state, it solidifies into an amorphous state in which atoms are irregularly arranged like glass, and is also called an amorphous metal. The material of the metallic glass 40 is arbitrary as long as it can obtain the above characteristics. For example, a Ni-Nb-Zr alloy containing nickel (Ni), niobium (Nb), and zirconium (Zr), or a Pd-Cu-Si alloy containing palladium (Pd), copper (Cu), and Si can be used as the metallic glass 40.
[0019] The upper electrode 50 is formed on the metallic glass 40, and is formed at a position corresponding to the opening 11 so as to cover the inside of the opening 11 or almost the entire area of the opening 11. The upper electrode 50 may also be formed so as to cover the entire area of one surface side of the substrate 10, but it is sufficient that the upper electrode 50 is formed so as to cover at least a part of the opening 11. The upper electrode 50 can be made of the same material as the lower electrode 20, for example.
[0020] 1 and 2, the MEMS resonator 1 is provided with a wiring structure and a control unit (not shown) as described above. This makes it possible to extract the potential difference generated between the lower electrode 20 and the upper electrode 50 based on the piezoelectric effect of the piezoelectric film 30 when ultrasonic waves are applied to vibrate the membrane, and to output ultrasonic waves to the outside. It is also possible to apply a potential difference for ultrasonic vibration between the lower electrode 20 and the upper electrode 50, vibrate the membrane based on the piezoelectric effect of the piezoelectric film 30, and output ultrasonic waves to the outside. This makes it possible to configure an ultrasonic transducer that can transmit and receive ultrasonic waves or both with the MEMS resonator 1.
[0021] In the MEMS resonator 1 configured in this manner, the piezoelectric film 30 is not formed on the metallic glass 40, but the metallic glass 40 is formed on the piezoelectric film 30. This makes it possible to prevent the deposition temperature of the piezoelectric film 30, for example, a temperature of 350° C. or higher if the piezoelectric film 30 is made of AlN, from being applied to the metallic glass 40. Therefore, after the metallic glass 40 is formed, the annealing temperature and annealing time can be adjusted according to the desired resonance frequency, thereby making it possible to match the resonance frequency. This makes it possible to obtain a MEMS resonator 1 having a structure that can achieve the desired characteristics.
[0022] Next, a method for manufacturing the MEMS resonator 1 having the above-mentioned structure will be described with reference to FIGS. 3A to 3C.
[0023] First, as shown in FIG. 3A, the lower electrode 20, the piezoelectric film 30, the metallic glass 40, and the upper electrode 50 are sequentially formed on the wafer-shaped substrate 10. After the metallic glass 40 and the upper electrode 50 are formed, they are patterned by photoetching to have a desired shape as necessary. This produces the structure shown in FIG. 3A. For example, the substrate 10 is made of Si, the lower electrode 20 and the upper electrode 50 are made of Pt, the piezoelectric film 30 is made of AlN, and the metallic glass 40 is made of a Ni-Nb-Zr alloy. The lower electrode 20 and the upper electrode 50 are made to have a thickness of several tens of nm to several μm, the piezoelectric film 30 is made to have a thickness of several μm, and the metallic glass 40 is made to have a thickness of several tens of nm to several tens of μm. In this configuration, in the initial state before the annealing process, compressive stress occurs due to the stress of the metallic glass 40, and the part that becomes the membrane is in a state of shrinking toward the center as shown in FIG. 3A.
[0024] After that, annealing is performed at 200 to 400° C. for several tens of minutes to several hours, for example, 1 hour at 300° C. This relieves the compressive stress generated in the metallic glass 40 and changes it to, for example, tensile stress, and the contraction of the part that will become the membrane is eliminated, as shown in FIG.
[0025] Then, a photomask having openings at positions where the openings 11 are to be formed is formed on the back surface of the substrate 10, and then dry etching is performed to form the openings 11 in the substrate 10 as shown in Fig. 3C. As a result, a membrane is formed of the lower electrode 20, the piezoelectric film 30, the metallic glass 40, and the upper electrode 50 at positions corresponding to the openings 11. Thereafter, dicing is performed along the scribe lines to manufacture the MEMS resonator 1 shown in Figs. 1 and 2.
[0026] In this example, a case where compressive stress occurs in the initial state and is changed to tensile stress by annealing is given. This is just one example of the form of stress, and it is not always the case that the form is this. In other words, it is sufficient if the stress generated in the metallic glass 40 can be adjusted to a stress that can obtain the target resonance frequency of the membrane. For example, tensile stress generated in the initial state may be changed to compressive stress by annealing. Also, compressive stress generated in the initial state may be weakened by annealing.
[0027] As described above, in this embodiment, the piezoelectric film 30 is not formed on the metallic glass 40, but the MEMS resonator 1 has a structure in which the metallic glass 40 is formed on the piezoelectric film 30. This makes it possible to prevent a temperature equal to or higher than the deposition temperature of the piezoelectric film 30 from being applied to the metallic glass 40. Therefore, after the metallic glass 40 is formed, it is possible to anneal the metallic glass 40 in accordance with a desired resonant frequency, thereby making it possible to tune the resonant frequency to the desired frequency. This makes it possible to provide the MEMS resonator 1 with a structure that can achieve the desired characteristics.
[0028] Second embodiment The second embodiment will be described. This embodiment is different from the first embodiment in that the shape of the metallic glass 40 is changed, but other aspects are similar to the first embodiment, so only the differences from the first embodiment will be described.
[0029] As shown in FIGS. 4 and 5, in this embodiment, the metallic glass 40 is not disposed over the entire surface of the membrane, but is disposed only on a portion of the membrane.
[0030] Specifically, metallic glass 40 is arranged so as to overlap the boundary line between opening 11 and pedestal 12 at two or more points. In this embodiment, metallic glass 40 is configured in the shape of a rectangular strip, and metallic glass 40 is arranged so that one end and the other end in the longitudinal direction of metallic glass 40 overlap the boundary line between opening 11 and pedestal 12. In this way, when metallic glass 40 is arranged so as to overlap the boundary line between opening 11 and pedestal 12 at at least two points, the effect of controlling the stress generated in metallic glass 40 by annealing can be more effectively obtained.
[0031] Third embodiment A third embodiment will be described. This embodiment is the same as the first and second embodiments except that the shape of the metallic glass 40 is changed. Only the parts different from the first and second embodiments will be described. Note that, as in the second embodiment, a case in which the metallic glass 40 is shaped to be disposed only on a part of the membrane will be taken as an example, but the present embodiment can also be applied to a case in which the metallic glass 40 is disposed so as to cover the entire surface of the membrane as in the first embodiment.
[0032] As shown in Fig. 6 and Fig. 7, the metallic glass 40 of this embodiment has a plurality of holes 41 formed therethrough in the thickness direction of the metallic glass 40. The plurality of holes 41 are arranged in an array, and the metallic glass 40 has a mesh-like shape. In this manner, the holes 41 can also be formed in the metallic glass 40. When the metallic glass 40 has a holed shape, the weight of the metallic glass 40 can be reduced accordingly. This makes it possible to improve the design freedom of the MEMS resonator 1.
[0033] Here, the metallic glass 40 is formed in a mesh shape by arranging a plurality of holes 41 in an array, but the shape, number and location of the holes 41 may be arbitrary, and the metallic glass 40 does not necessarily have to be in a mesh shape. In other words, the shape, number and location of the holes 41 may be appropriately set according to the resonant frequency characteristics of the desired membrane.
[0034] (Other embodiments) Although the present disclosure has been described based on the above-described embodiment, it is not limited to the embodiment, and includes various modifications and modifications within the equivalent range. In addition, various combinations and forms, and other combinations and forms including only one element, more than one element, or less than one element, are also within the scope and concept of the present disclosure.
[0035] (1) For example, in each of the above embodiments, the metallic glass 40 and the upper electrode 50 are configured separately, but the metallic glass 40 can also serve as the upper electrode 50. In this way, compared to the case where the upper electrode 50 is configured as a separate member from the metallic glass 40, there is no need to form an upper electrode film, which can reduce costs.
[0036] When the metallic glass 40 and the upper electrode 50 are formed separately, it is effective to make the metallic glass 40 overlap the boundary between the opening 11 and the pedestal 12 at at least two points in order to control the stress caused by the annealing treatment. On the other hand, the upper electrode 50 only needs to be formed on at least a part of the membrane formed in the opening 11, and does not need to overlap the boundary between the opening 11 and the pedestal 12. However, taking into account the resonant frequency characteristics of the membrane, it is preferable that the metallic glass 40 and the upper electrode 50 are laid out in rotational symmetry with respect to the center of the membrane.
[0037] On the other hand, when the metallic glass 40 also serves as the upper electrode 50, it is preferable that the metallic glass 40 overlaps the boundary between the opening 11 and the base portion 12 in at least two places so that the annealing treatment is effective in controlling stress.
[0038] (2) In the above embodiment, the lower electrode 20 is formed using a metal material such as Pt, but at least a portion of it may be made of Si, that is, an impurity layer in which Si is doped with a high concentration of n-type or p-type impurities.
[0039] For example, an insulating film and polysilicon are sequentially formed on the substrate 10 by a commonly performed MOS process, and impurities are doped into the polysilicon to form an impurity layer to form the lower electrode 20. Then, when forming the opening 11, etching is performed so that the lower electrode 20 remains, making it possible to form the lower electrode 20 from Si.
[0040] Moreover, the surface layer on the front surface side of the base material 10 may be made of an impurity layer as the lower electrode 20, and the lower electrode 20 may be left when the opening 11 is formed, so that the lower electrode 20 is made of Si.
[0041] Furthermore, an SOI (Silicon on Insulator) substrate may be used, with the active layer side being made a thin film, and impurities may be doped at a high concentration to form an impurity layer, which may be used as the lower electrode 20. In this case, the opening 11 may be formed until the buried oxide film disposed between the active layer and the support layer is removed, or the buried oxide film may be left so as to become a part of the membrane.
[0042] (3) Furthermore, in each of the above embodiments, the opening 11 is made to have a circular shape when viewed from above the MEMS vibrator 1, and the membrane shape is made to be circular, but it may also be a regular polygon shape such as a hexagon or octagon.
[0043] Even in this case, as in the second and third embodiments, it is preferable that metallic glass 40 is arranged so as to overlap the boundary line between opening 11 and pedestal 12 in two or more places. This makes it possible to more effectively obtain the effect of controlling the stress generated in metallic glass 40 by annealing. That is, in either case where the membrane is circular or polygonal, metallic glass 40 is preferably arranged so as to equally divide the membrane with the central axis of opening 11 as the center.
[0044] For example, when the membrane shape is a regular n-gon, the metallic glass 40 may be laid out so as to divide the regular n-gon into n parts or into multiples or divisors of n. For example, when the membrane shape is an octagon and the membrane is to be divided into n parts, the metallic glass 40 is laid out in a shape radiating in eight directions in the radial direction from the center of the membrane. When the membrane shape is an octagon and the membrane is to be divided into multiples of n, the metallic glass 40 is laid out in a shape radiating in 16 directions in the radial direction from the center of the membrane, and when the membrane is to be divided into divisors of n, the metallic glass 40 is laid out in a shape radiating in four or two directions in the radial direction from the center of the membrane. When the membrane is divided into four directions, the metallic glass 40 has a cross shape, and when the membrane is divided into two directions, the metallic glass 40 has a rectangular shape.
[0045] Furthermore, it is not necessary to arrange the metallic glass 40 so as to divide the membrane equally around the central axis of the opening 11. For example, the metallic glass 40 may be arranged in an L-shape, extending in two directions from the central axis of the opening 11.
[0046] In addition, the number and materials of each part are merely examples in each of the above embodiments. For example, the metallic glass 40 may be arranged in a stripe shape of two or more stripes, or may be divided into a plurality of stripes radially around the central axis of the opening 11. [Explanation of symbols]
[0047] 1 MEMS resonator 10 Base material 11 Opening 12 Pedestal 20 Lower electrode 30 Piezoelectric film 40 Metallic Glasses 41 holes 50 Upper electrode
Claims
1. A substrate (10) having an opening (11) formed therein and a base portion (12) constituting a peripheral wall surrounding the opening; a lower electrode (20) formed on one surface side of the substrate in a portion corresponding to at least a portion of the opening; a piezoelectric film (30) formed on the lower electrode; A metallic glass (40) formed on the piezoelectric film, A MEMS vibrator, wherein a membrane is formed including the lower electrode, the piezoelectric film, and the metallic glass.
2. The MEMS vibrator according to claim 1 , wherein the metallic glass is disposed to cover the entire opening.
3. The MEMS resonator of claim 1 , wherein the metallic glass is disposed to cover only a portion of the opening.
4. The MEMS vibrator according to claim 3 , wherein the metallic glass is disposed so as to overlap a boundary line between the opening and the base at two or more points.
5. The opening is formed with a central axis aligned in a normal direction to one surface of the base material, The MEMS vibrator according to claim 3 , wherein the metallic glass is arranged so as to equally divide the membrane with respect to the central axis.
6. A top electrode (50) is provided on the metallic glass; 6. The MEMS vibrator according to claim 1, wherein a membrane is formed by including the upper electrode in addition to the lower electrode, the piezoelectric film, and the metallic glass.
7. The MEMS resonator of claim 1 , wherein the metallic glass also functions as a top electrode (50).
8. The MEMS vibrator according to claim 1 , wherein at least a portion of the lower electrode is made of silicon.
9. 9. The MEMS vibrator according to claim 1, wherein the metallic glass has a hole (41) formed therein, the hole penetrating the metallic glass in a thickness direction.
Citation Information
Patent Citations
Micromachine using metal glass and sensor using same, and manufacturing method thereof
JP2008155333A
Acceleration sensor and method for manufacturing the same
JP2009192379A
Liquid ejecting head, liquid ejecting apparatus, and piezoelectric element
JP2010017984A
Micromirror device and fabrication method of the same
JP2014134642A
Film structure and manufacturing method of the same
JP2019216181A