Heat exchanger manufacturing method and manufacturing device

JP7594877B2Active Publication Date: 2024-12-05LISSENOK PACKAGING CO LTD
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
JP2020170398
Authority / Receiving Office
JP · JP
Patent Type
Patents
Current Assignee / Owner
Filing Date
2020-10-08
Publication Date
2024-12-05
Estimated Expiration
2040-10-08

AI Technical Summary

Benefits of technology

【0021】 発明[1]の熱交換器の製造方法によれば、外包体の内部を減圧してインナーフィンを外包体に融着しているため、減圧による外包体の収縮作用により、外包体がインナーフィンの凹凸部に追従して密着し、その密着部を融着部として融着することができる。このため外包体およびインナーフィン間における所定の融着部全域を隙間なく融着できて、接着不良や接着不足の発生を確実に防止することができる。その結果、熱融着時の接着信頼性を格段に向上させることができ、熱交換性能を向上させることができる。

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 0007594877000002
    Figure 0007594877000002
  • Figure 0007594877000003
    Figure 0007594877000003
  • Figure 0007594877000004
    Figure 0007594877000004
Patent Text Reader

Abstract

To provide a manufacturing method for a heat exchanger securely enabling thermal fusion between an outer envelope body and a fin.SOLUTION: This invention relates to a manufacturing method for a heat exchanger including: an outer envelope body 1 constituted by outer envelope laminate materials L1 in which thermal fusion layers 52 are provided in heat transfer layers 51; and an inner fin 2 provided in the outer envelope body and constituted by an inner core laminate material L2 in which a thermal fusion layer 62 is provided in a heat transfer layer 61. The manufacturing method includes: an outer envelope body fusing process of thermally fusing the outer envelope laminate materials L1 to each other to seal an outer peripheral edge part of the outer envelope body 1; and a fin fusing process of thermally fusing projecting and recessed parts 25, 26 provided in the inner fin 2 to the outer envelope body 1 after the outer envelope body fusing process is performed. The fin fusing process is performed while inside of the outer envelope body 1 is decompressed relative to outside.SELECTED DRAWING: Figure 6B
Need to check novelty before this filing date? Find Prior Art

Description

[Technical field]

[0001] The present invention relates to a method and an apparatus for manufacturing a heat exchanger produced using a laminate material in which a resin heat-sealing layer is laminated on a metal heat-conductive layer. [Background technology]

[0002] As electronic devices such as smartphones and personal computers become smaller and more powerful, measures to prevent heat generation around the CPU of the electronic device have become important. Some models incorporate water-cooling devices or heat pipes to reduce the thermal load on electronic components such as the CPU and prevent heat from building up inside the housing, and technologies have been proposed to avoid the adverse effects of heat.

[0003] In addition, the battery modules installed in electric vehicles and hybrid vehicles generate a lot of heat in the battery packs due to repeated charging and discharging. For this reason, technology has been proposed to incorporate water-cooling devices and heat pipes into battery modules, just like the above electronic devices, to avoid the adverse effects of heat.

[0004] Furthermore, for power modules made of silicon carbide (SiC) and the like, measures such as installing cooling plates or heat sinks have been proposed to prevent heat generation.

[0005] Conventionally, thin coolers such as heat pipes incorporated into small electronic devices have predominantly been made of metal, with multiple metal components joined by brazing or the like (Patent Documents 1 to 3).

[0006] Such metal coolers are difficult to make thinner than current models because each component is manufactured using laborious metal processing (machining) methods such as plastic processing, such as casting or forging, and removal processing, such as cutting.

[0007] In view of this, a cooler has been proposed in which the outer envelope as a casing and the inner fin (inner core material) are made of a laminate material. The laminate material is made by laminating a resin heat-sealing layer on a metal foil layer. For example, the laminate material for the outer envelope (outer envelope laminate material) is stacked vertically via the laminate material for the inner core material (inner fin), and the outer peripheral edges of the outer envelope laminate material are heat-sealed to form the outer envelope, and the intermediate region of the upper and lower outer envelope laminate materials is heat-sealed to the uneven portion of the inner fin, thereby fixing the inner fin inside the outer envelope.

[0008] Coolers made of such laminated materials have been attracting attention in recent years because they do not require troublesome metal processing, are easy to manufacture, reduce costs, and can be made thinner. [Prior art documents] [Patent documents]

[0009] [Patent Document 1] JP 2015-59693 A [Patent Document 2] JP 2015-141002 A [Patent Document 3] JP 2016-189415 A Summary of the Invention [Problem to be solved by the invention]

[0010] When manufacturing a cooler made of the above-mentioned laminate material, the outer envelope (outer envelope laminate material) and the inner fin are bonded by heat fusion as described above. However, if the outer envelope and the inner fin are not bonded sufficiently, the heat transfer coefficient between the refrigerant flowing inside the outer envelope and the member to be cooled, such as a battery, that is in contact with the outer surface of the outer envelope decreases, resulting in a problem of reduced heat exchange performance.

[0011] The present invention has been made in consideration of the above-mentioned problems, and aims to provide a method and apparatus for manufacturing a heat exchanger that can reliably heat seal between the outer casing and the inner fin, thereby producing a heat exchanger with excellent heat exchange performance. [Means for solving the problem]

[0012] In order to solve the above problems, the present invention comprises the following means.

[0013] [1] A method for manufacturing a heat exchanger, comprising: an outer envelope made of an outer laminate material having a resin heat-sealing layer provided on the inner surface side of a metal heat transfer layer; and an inner fin provided inside the outer envelope and made of an inner core laminate material having a resin heat-sealing layer provided on both sides of the metal heat transfer layer, the method comprising: an outer envelope fusion step of heat-fusing the outer envelope laminate materials to seal an outer peripheral edge of the outer envelope; and a fin fusion step of heat-fusing the concave and convex portions of the inner fin to the outer envelope after the outer envelope fusion step, The method for manufacturing a heat exchanger, wherein the fin fusion step is performed under a condition in which the inside of the outer casing is reduced in pressure relative to the outside.

[0014] [2] The outer envelope has an opening for introducing and removing a heat exchange medium into and from the inside thereof, 2. The method for manufacturing a heat exchanger according to claim 1, wherein in the fin fusing step, the inside of the outer casing is depressurized by utilizing the inlet / outlet.

[0015] [3] A header made of heat-sealing resin is provided in the outer envelope in correspondence with the inlet and outlet, a header fusion step of heat-sealing an outer surface of the header to the outer envelope after the outer envelope fusion step is performed, 3. The method for manufacturing a heat exchanger according to item 1 or 2, wherein the header fusion step is performed in a state where the inside of the outer envelope is reduced in pressure relative to the outside.

[0016] [4] The method for manufacturing a heat exchanger according to item 3 above, wherein the fin fusion step and the header fusion step are carried out simultaneously.

[0017] [5] A pipe portion is provided in the header and extends through the entrance and exit to the outside. 5. The method for manufacturing a heat exchanger according to item 3 or 4, wherein in the fin fusing step, the inside of the outer casing is depressurized by utilizing the pipe portion.

[0018] [6] The method for producing a heat exchanger according to any one of items 1 to 5, wherein in the fin fusing step, the internal pressure of the outer casing is set to 1 / 15 to 1 / 2 of the external pressure.

[0019] [7] A heat exchanger manufacturing apparatus for manufacturing a heat exchanger including an outer envelope made of an outer envelope laminate material having a resin heat-sealing layer provided on the inner surface side of a metal heat transfer layer, and an inner fin provided inside the outer envelope and made of an inner core laminate material having a resin heat-sealing layer provided on both sides of the metal heat transfer layer, comprising: an outer envelope fusion mold for heat-fusing the outer envelope laminate materials by sandwiching them together and heating them to seal the outer periphery of the outer envelope; a fin fusion die for heat-sealing the concave-convex portion of the inner fin to the outer shell by heating the outer shell while pressing the outer shell against the inner fin, The fin fusion mold is characterized in that it is provided with a pressure reduction means for reducing the pressure inside the outer casing relative to the outside while pressing the outer casing toward the inner fin.

[0020] [8] The outer envelope has an opening for introducing and removing a heat exchange medium into and from the inside thereof, the suction means includes a suction pump and a suction section having one end connected to the suction pump and disposed so as to pass through the fin fusion die and cover the inlet / outlet with the other end; 8. The heat exchanger manufacturing apparatus according to item 7, wherein the inside of the outer casing is depressurized through the suction pipe by driving the suction pump. Effect of the Invention

[0021] According to the method for manufacturing a heat exchanger of the invention [1], the pressure inside the outer envelope is reduced to fuse the inner fin to the outer envelope, so that the outer envelope shrinks due to the reduced pressure, and the outer envelope conforms to the unevenness of the inner fin and adheres to the inner fin, and the adhered area can be fused as the fused area. Therefore, the entire area of ​​the fused area between the outer envelope and the inner fin can be fused without any gaps, and poor or insufficient adhesion can be reliably prevented. As a result, the reliability of the heat fusion can be significantly improved, and the heat exchange performance can be improved.

[0022] According to the manufacturing method of the heat exchanger of invention [2], the pressure is reduced during the fin fusion process by utilizing the inlet and outlet of the outer casing, so that the internal pressure of the outer casing can be easily reduced without adopting any special configuration.

[0023] According to the manufacturing method of a heat exchanger of invention [3], the inside of the outer casing is reduced pressure and the header is fused to the outer casing. As a result, as described above, the outer casing can be fused to the header in a tight contact state, which reliably prevents poor adhesion or insufficient adhesion and improves heat exchange performance.

[0024] According to the method for manufacturing a heat exchanger of the invention [4], the fin fusion process and the header fusion process are carried out simultaneously, thereby improving production efficiency.

[0025] According to the manufacturing method of the heat exchanger of invention [5], the pressure is reduced during the fusion process by utilizing the pipe portion protruding outward, so that the internal pressure of the outer casing can be easily reduced without adopting any special configuration.

[0026] According to the method for manufacturing a heat exchanger of the invention [6], the above-mentioned effects can be obtained even more reliably.

[0027] According to the heat exchanger manufacturing apparatus of the inventions [7] and [8], an apparatus capable of carrying out the above-mentioned method invention is specified, so that the same effects as those described above can be reliably obtained. [Brief description of the drawings]

[0028] [Figure 1] FIG. 1 is a perspective view showing a heat exchanger manufactured by a manufacturing method according to an embodiment of the present invention. [Diagram 2] FIG. 2 shows a heat exchanger of an embodiment, where FIG. 2(a) is a plan view, FIG. 2(b) is a side cross-sectional view corresponding to the cross-section along line BB in FIG. 2(a), and FIG. 2(c) is a front cross-sectional view corresponding to the cross-section along line CC in FIG. 2(a). [Diagram 3] FIG. 3 is an exploded perspective view of the heat exchanger according to the embodiment. [Figure 4] FIG. 4 is a front cross-sectional view illustrating an outer shell and an inner fin applied to the heat exchanger of the embodiment. [Figure 5A] FIG. 5A is a front cross-sectional view illustrating an inner fin according to an embodiment. [Figure 5B] FIG. 5B is a front cross-sectional view illustrating an inner fin according to a modified example. [Figure 6A] FIG. 6A is a schematic cross-sectional view for explaining an outer package fusion mold capable of carrying out the outer package fusion step of the embodiment. [Figure 6B] FIG. 6B is a schematic cross-sectional view for explaining a fin / header fusion die capable of carrying out the fin / header fusion step of the embodiment. [Figure 7A] FIG. 7A is a plan view of a heat exchanger illustrating the areas fused by the outer envelope fusion step according to an embodiment. [Figure 7B] FIG. 7B is a plan view of the heat exchanger illustrating the areas fused by the fin / header fusion process. [Figure 8] FIG. 8 shows a coupler of a pressure reducing means in a fin / header fusion die of an embodiment, where FIG. 8(a) is a side view and FIG. 8(b) is a bottom view. [Figure 9A]FIG. 9A is a plan view showing a tray member employed in a heat exchanger of an example related to a manufacturing method of the embodiment. [Figure 9B] FIG. 9B is a cross-sectional view of an end portion of the tray member of the embodiment. [Figure 10A] FIG. 10A is a schematic cross-sectional view for explaining a batch fusion die used in manufacturing the heat exchanger of Comparative Example 1. [Figure 10B] FIG. 10B is a schematic cross-sectional view for explaining a batch fusion die used in manufacturing the heat exchanger of Comparative Example 2. [Figure 10C] FIG. 10C is a schematic cross-sectional view for explaining a fin / header fusion die used in manufacturing the heat exchanger of Comparative Example 3. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS

[0029] 1 to 3 are diagrams showing a heat exchanger according to an embodiment of the present invention. In the following description, in order to facilitate understanding of the invention, the left-right direction in Fig. 2(a) will be referred to as the "front-rear direction", and the up-down direction in Fig. 2(b) will be referred to as the "up-down direction (thickness direction)".

[0030] As shown in Figures 1 to 3, the heat exchanger of this embodiment is used as a heat transfer panel, a heat transfer tube, etc., and comprises an outer casing 1 as a casing (container), an inner fin (inner core material) 2 housed inside the outer casing 1, and a pair (both sides) of headers (joint members) 3, 3 housed within both end portions of the outer casing 1.

[0031] The outer envelope 1 is composed of a tray member 10 having a rectangular shape in a plan view, and a cover member 15 having a rectangular shape in a plan view.

[0032] The tray member 10 is composed of a molded product of an outer laminate material L1, and using cold forming techniques such as deep drawing or extrusion molding, the entire middle region except for the outer peripheral edge is recessed downwardly to form a recessed portion 11 that is rectangular in plan view, and an outwardly protruding flange portion 12 is integrally formed on the outer periphery of the opening edge of the recessed portion 11.

[0033] Further, the cover member 15 is formed with a pair of openings 16, 16 corresponding to the front and rear ends of the recessed portion 11 in the tray member 10. Needless to say, in this embodiment, of the pair of openings 16, one opening 16 is configured as an entrance, and the other opening 16 is configured as an exit.

[0034] The tray member 10 and the cover member 15 are made of an outer laminate material L1 which is a laminate sheet or film having flexibility and suppleness.

[0035] 4, the outer laminate material L1 includes a heat transfer layer 51 made of metal (metal foil), a heat fusion layer 52 made of a heat fusion resin film or a heat fusion resin sheet laminated via an adhesive on one surface (inner surface) of the heat transfer layer 51, and a protective layer 53 made of a heat resistant resin film or a heat resistant resin sheet laminated via an adhesive on the other surface (outer surface) of the heat transfer layer 51. In this embodiment, the term "foil" is used to include a film, a thin plate, and a sheet.

[0036] The heat transfer layer 51 in the outer laminate material L1 can be preferably made of copper foil, aluminum foil, stainless steel foil, nickel foil, nickel-plated copper foil, clad metal made of nickel and copper foil, etc., and among them, aluminum foil with JIS aluminum alloy number A8021H can be particularly preferably used. In this embodiment, the terms "copper", "aluminum", "nickel" and "titanium" are used to include their alloys.

[0037] The heat transfer layer 51 is also called a heat collecting layer, and is preferably 30 μm to 200 μm thick, more preferably 40 μm to 180 μm thick. That is, if the heat transfer layer 51 is too thin, it is likely to be deformed by external pressure and its strength may decrease, which is not preferable. Conversely, if the heat transfer layer 51 is too thick, it is likely to be less flexible and less moldable, which is not preferable.

[0038] Furthermore, by subjecting the heat transfer layer 51 to a surface treatment such as a chemical conversion treatment, the durability of the heat transfer layer 51 can be further improved, for example, by preventing corrosion of the heat transfer layer 51 and improving adhesion to the resin.

[0039] As the heat-sealing layer 52, a film or sheet made of a polyolefin resin such as polyethylene or polypropylene, or a modified resin thereof, a fluorine-based resin, a polyester-based resin, a vinyl chloride resin, or the like, can be suitably used.

[0040] Furthermore, it is preferable to use polypropylene, which is heat resistant and inexpensive, for the heat seal layer 52. Among them, it is preferable to use non-oriented polypropylene (CPP). It is more preferable to use a multi-layer film of polypropylenes having different melting points.

[0041] The thermal adhesive layer 52 preferably has a thickness of 20 μm to 500 μm, and more preferably has a thickness of 30 μm to 80 μm.

[0042] For example, a three-layer (random PP / block PP / random PP) co-extruded film as the heat-sealing layer 52 has random PP with a low melting point arranged on the surface layer and block PP with a higher melting point than random PP, a smaller MFR, and low fluidity arranged on the middle layer, and has good heat sealability due to the random PP and ability to suppress extreme thickness reduction during heat sealing due to the block PP, resulting in excellent adhesion and corrosion resistance after sealing. Note that a three-layer co-extruded film with a layer ratio of random PP / block PP / random PP in the range of 1-2 / 6-8 / 1-2 can be suitably used.

[0043] The protective layer 53 can be preferably a film or sheet of a heat-resistant resin such as oriented polyester resin (PET, PBT, etc.) or oriented polyamide resin (ONY) having a melting point 10° C. or higher, more preferably 20° C. or higher, than that of the thermal adhesive layer 52. The protective layer 53 should preferably have a thickness of 6 μm to 100 μm.

[0044] In addition, as an adhesive for bonding between the heat transfer layer 51, the heat fusion layer 52 and the protective layer 53 that constitute the outer laminate material L1, a urethane-based adhesive, an epoxy-based adhesive, an olefin-based adhesive, etc., having a thickness of 1 μm to 5 μm can be suitably used.

[0045] In this embodiment, a three-layered sheet is used as the laminate material L1 constituting the envelope 1, but this is not limited thereto, and in the present invention, a two-layered sheet consisting of a heat transfer layer and a heat fusion layer may be used, or a four-layered sheet may be used. When a four-layered sheet is used, for example, another layer may be interposed between the protective layer and the heat transfer layer, or another layer may be interposed between the heat transfer layer and the heat fusion layer, so that the four-layered sheet is configured to be four or more layers.

[0046] The outer envelope laminate material L1 having the above-mentioned configuration constitutes the tray member 10 and cover member 15 of the outer envelope 1. Then, in an outer envelope fusion step (outer envelope fusion treatment) described below, the cover member 15 is attached to the tray member 10 so as to close the opening of the recessed portion 11, thereby forming the outer envelope 1.

[0047] In this embodiment, a pair of opposing walls 111, 151 is formed by a bottom wall (lower wall) 111 of the recessed portion 11 in the tray member 10 and a top wall (upper wall) 151 of the portion corresponding to the recessed portion 11 in the cover member 15 attached to the tray member 10.

[0048] As shown in Figs. 1 to 4, the inner fin 2 housed in the hollow portion (recessed portion) 11 of the outer envelope 1 is made of an inner core laminate material L2 which is a laminate sheet or film having flexibility or pliability.

[0049] As shown in FIG. 4, the inner core laminate material L2 includes a heat transfer layer 61 made of metal foil, and heat fusion layers 62, 62 made of a resin film or resin sheet laminated on both sides of the heat transfer layer 61 with an adhesive.

[0050] The heat transfer layer 61 in the inner core laminate material L2 may suitably be the same as the heat transfer layer 51 in the outer laminate material L1.

[0051] As the heat-sealing layer 62, a material similar to the heat-sealing layer 52 of the outer laminate material L1 can be suitably used.

[0052] In this embodiment, a three-layered sheet is used as the laminate material L2 constituting the inner fin 2, but the present invention is not limited thereto, and a four-layered sheet may be used in the present invention. For example, a four-layered sheet may be adopted by interposing another layer between the thermal fusion layer and the heat transfer layer.

[0053] The processing method of the inner fin 2 is not particularly limited, but may be, for example, a method in which the inner core laminate material L2 is sandwiched between a pair of embossing rolls or a pair of corrugated rolls and passed between the pair of rolls to form concaves and convexes. Further, a method in which a press machine or a press die is used to form concaves and convexes on the inner core laminate material L2 may be exemplified.

[0054] 2 to 5A, the inner fin 2 is formed in an angular wave shape (rectangular wave shape) in which the recesses 25 and the protrusions 26 are alternately and continuously formed, i.e., in a so-called digital signal waveform. That is, the bottom surfaces (bottom walls) of the recesses and the top surfaces (top walls) of the protrusions in the inner fin 2 of this embodiment are formed flat, and are arranged parallel to the bottom wall (lower wall) 111 of the tray member 10 and the top wall (upper wall) 151 of the cover member 15 in a state where the heat exchanger is assembled. Furthermore, in the inner fin 2, the rising walls connecting the adjacent bottom walls of the recesses and the top walls of the protrusions are arranged perpendicular to the bottom walls of the recesses and the top walls of the protrusions, or to the upper and lower walls 111, 151 of the outer casing 1 in a state where the heat exchanger is assembled.

[0055] In this embodiment, as shown in Fig. 5A, an inner fin 2 having an angular waveform is used, but the present invention is not limited to this, and an inner fin having a general waveform (sine wave shape) in which arc-shaped recesses and protrusions are alternately and continuously formed, i.e., a so-called analog signal waveform, may be used in the present invention, as shown in Fig. 5B. However, in the present invention, an inner fin having any shape may be used as long as it has recesses and protrusions that are bonded to the inner peripheral surface of the outer envelope.

[0056] The inner fin 2 is accommodated in the recessed portion 11 of the tray member 10. In this case, the inner fin 2 is accommodated in the middle portion of the recessed portion 11 of the tray member 10, excluding both front and rear ends. Furthermore, the inner fin 2 is arranged so that the direction of the peaks and valleys coincides with the front-rear direction of the tray member 10 (the left-right direction in FIG. 1). As a result, the tunnel portion and the groove portion formed by the peaks and valleys of the inner fin 2 are configured as a heat exchange flow path. The heat exchange flow paths are arranged along the front-rear direction (length direction) of the tray member 10, and a plurality of them are arranged in parallel in the width direction (left-right direction), so that the heat exchange medium (heat medium) can flow smoothly from one end side to the other end side in the front-rear direction of the outer envelope 1 while being evenly distributed through each heat exchange flow path.

[0057] On the other hand, as shown in Figs. 2 and 3, a pair of headers 3, 3 disposed at both ends of the envelope 1 are made of molded products made of heat-sealable resin.

[0058] The resin constituting the header 3 is preferably the same type of resin as that constituting the heat-sealing layers 52, 62 of the outer cover 1 and the inner fin 2. Specifically, polyolefin resins such as polyethylene and polypropylene or modified resins thereof, fluorine-based resins, polyester-based resins, vinyl chloride resins, etc. can be suitably used.

[0059] The header 3 includes a box-shaped mounting box portion 31 having an opening 32 on one side, and a pipe portion 33 provided on the upper wall of the mounting box portion 31. The pipe portion 33 communicates with the inside of the mounting box portion 31, and is configured to allow a heat exchange medium to pass between the inside of the pipe portion 33 and the inside of the mounting box portion 31.

[0060] The method for molding the header 3 is not particularly limited, but a molding method using injection molding, for example, can be suitably adopted.

[0061] The mounting box portions 31 of the header 3 are disposed on both sides of the inner fin 2 in the recessed portion 11 of the tray member 10. Furthermore, the pipe portions 33 of the header 3 are disposed facing upward, and the openings 32 of the mounting box portions 31 are disposed facing inward, that is, facing the inner fins 2.

[0062] In this way, the headers 3, 3 are housed in the tray member 10, and the cover member 15 is placed on the tray member 10 so as to close the opening. In this case, the upward pipe portions 33, 33 of the headers 3, 3 are inserted and placed in the entrance / exit 16 of the cover member 15.

[0063] The heat exchanger assembly is heated to heat-seal the necessary parts of the contacting members to be joined together. This heat sealing includes three heat-sealing steps: an outer envelope sealing step (outer envelope sealing step) for heat-sealing the flange 12 of the tray member 10 and the outer peripheral edge of the cover member 15 via the corresponding heat-sealing layers 52, a fin sealing step (fin sealing step) for heat-sealing the pair of opposing walls 111, 151 and the uneven parts 25, 26 of the inner fin 2 via the corresponding heat-sealing layers 52, 62, and a header sealing step (header sealing step) for heat-sealing the heat-sealing layers 52 of the pair of opposing walls 111, 151 and the header 3.

[0064] In this embodiment, after the outer envelope fusion step, the fin fusion step and the header fusion step are simultaneously performed by a fin / header fusion step (interior item fusion step). Furthermore, in this embodiment, the outer envelope fusion step is performed using an outer envelope fusion die described below, and the fin / header fusion step is performed using a fin / header fusion die (interior item fusion die) described below.

[0065] In this embodiment, the case where the outer shell fusion process is performed followed by the fin / header fusion process is referred to as two-stage sealing (two-stage sealing method), the first fusion process (outer shell fusion process) is referred to as the first (first stage) seal, and the second fusion process (fin / header fusion process) is referred to as the second (second stage) seal.

[0066] In the present invention, the fin fusion step and the header fusion step do not necessarily have to be carried out simultaneously, and may be carried out separately using separate dies or the like.

[0067] For reference, in the present invention, the case where the outer envelope fusion process, fin fusion process and header fusion process are performed simultaneously using a single mold (one-stage fusion mold), as exemplified in the comparative example described below, is referred to as one-stage sealing (one-stage sealing method).

[0068] Fig. 6A is a schematic cross-sectional view for explaining an envelope fusion die D1 for carrying out the envelope fusion step. As shown in the figure, the lower die of this die D1 is provided with a hot plate H for supporting from below the flange 12 of the tray member 10 of the heat exchanger temporary assembly placed in the die, and the upper die is provided with a hot plate H for pressing from above the outer periphery of the cover member 15. The die is then closed, and the overlapping portion of the flange 12 of the tray member 10 and the outer periphery of the cover member 15 is sandwiched and pressed between the upper and lower hot plate H, and in this state, the flange 12 of the tray member 10 and the outer periphery of the cover member 15 are heat-fused and sealed by the heat from the hot plate H, as shown by the diagonal hatching in Fig. 7A.

[0069] 6B is a schematic cross-sectional view for explaining a fin / header fusion die D2 for carrying out the fin / header fusion step. As shown in the figure, the lower die of this die D2 is provided with a seal plate S for supporting from below the bottom wall (opposing wall) 111 of the tray member 10 of the heat exchanger temporary assembly placed in the die, and the upper die is provided with a seal plate S for pressing from above the opposing wall 151 of the cover member 15. After the die is closed, the upper seal plate S is lowered to press the upper and lower seal plates S against the bottom surface of the tray member 10 and the center of the upper surface of the cover 15 to apply pressure, and in this state, the pair of opposing walls 111, 151 can be thermally fused and fixed to the uneven parts 25, 26 of the inner fin 2 and the upper and lower surfaces of the header 3 by heat from the seal plate S, as shown by the diagonal hatching in FIG. 7B.

[0070] In this embodiment, by placing a cushioning material such as silicone rubber, fluororubber, glass cloth, etc. on the outermost surface of the sealing plate S, i.e., the contact surface with the pair of opposing walls 111, 151 of the outer cover 1, the sealing plate S can be pressed with an even pressing force against the entire required area of ​​the outer cover 1, thereby achieving good bonding between the outer cover 1 and the inner fin 2 and the header 3.

[0071] Furthermore, the fin / header fusion mold D2 of this embodiment is provided with a decompression means 8 for reducing the pressure inside the envelope 1 while the fin / header fusion step is being carried out.

[0072] The pressure reduction means 8 comprises a suction pump 81, a main pipe 82 having one end connected to the suction pump 81, a pair of branch pipes 83 each having one end connected to the main pipe 82 and each passing through the upper die of the fin / header fusion die and having the other ends positioned opposite a pair of inlets and outlets 16 in the outer envelope 1, and couplers 9 connected to the other ends of the pair of branch pipes 83 and each connected to a pair of inlets and outlets 16 in the outer envelope 1.

[0073] In this embodiment, the main pipe 82 and the branch pipe 83 form a suction pipe, and the suction pipe and the coupler 9 form a suction section. Furthermore, one end of the main pipe 82 forms one end of the suction section, and the other end of the suction section is formed by the coupler 9.

[0074] As shown in Fig. 8, coupler 9 has a trumpet-like or conical tube-like shape, and its small-diameter end is airtightly connected to the other end of branch pipe 83. Furthermore, an O-ring 91 is attached to the peripheral wall end face at the large-diameter end (connection port). When the fin / header fusion die is closed, the large-diameter end face of coupler 9 comes into airtight contact with the outer periphery of inlet / outlet 16 of envelope 1 via O-ring 91, and pipe section 33 is housed inside coupler 9. In this state, when suction pump 81 is driven, the inside of envelope 1 is sucked through main pipe 82 and branch pipe 83, and a reduced pressure (negative pressure) state is set.

[0075] The coupler 9 may be made of metal such as stainless steel or aluminum, or may be made of resin such as ABS resin.

[0076] Also, the O-ring 91 is preferably selected from the shapes specified in JIS B 2401. It is further preferable to select it from O-rings for vacuum flanges.

[0077] The O-ring 91 can be made of a material such as fluororubber, silicone rubber, or nitrile rubber.

[0078] As the suction pump 81 of the pressure reducing means 8, a rotary pump, a diffusion pump, or the like can be used.

[0079] In this embodiment, the above-mentioned heat exchanger preliminary assembly is subjected to an outer body fusion process using an outer body fusion die (see Figure 6A) to seal the outer peripheral edge portion of the outer body 1, and then a fin / header fusion process is performed using a fin / header fusion die (see Figure 6B) in the following steps (1) to (5).

[0080] (1) The heat exchanger subassembly in which the outer casing 1 is sealed is set in the lower die of a fin / header fusion die.

[0081] (2) The upper mold is lowered to close the mold, and the lower end (large diameter end) of coupler 9 of pressure reducing means 8 provided on the upper mold is brought into close contact with the outer periphery of inlet / outlet 16 in outer envelope 1.

[0082] (3) The vacuum pump 81 is operated to reduce the pressure inside the outer cover 1 to a predetermined level, and then the upper sealing plate S is lowered to press the upper and lower sealing plates S against the opposing walls 111, 151 of the outer cover 1, and the outer cover 1 is heat-sealed to the inner fin 2 and the header 3 as described above.

[0083] (4) After heat sealing, the suction pump 81 is stopped to release the reduced pressure (negative pressure) inside the envelope, and the upper seal plate S is raised to open the mold.

[0084] (5) The heat-sealed heat exchanger is then removed from mold D2, completing the fin / header fusion process.

[0085] In this embodiment, when reducing the pressure inside the outer envelope 1, suction is performed from both sides of the pair of inlets and outlets 16, but this is not limited to this, and in the present invention, it is sufficient to configure it so that suction can be performed from at least one of the pair of inlets and outlets 16.

[0086] The heat exchanger obtained by the manufacturing method of this embodiment is used as a cooler (cooling device) for cooling a battery or the like as a member to be cooled (member to be heat exchanged). That is, an inlet pipe for introducing a cooling liquid (cooling water, antifreeze, etc.) as a heat exchange medium (refrigerant) is connected to one pipe section 33 of the heat exchanger, and an outlet pipe for discharging the cooling liquid is connected to the other pipe section 33. Furthermore, a battery as a member to be cooled is placed in contact with the lower wall 111 and / or the upper wall 151 of the outer casing 1 of the heat exchanger. In this state, the cooling liquid flows from one pipe section 33 into the inside of the outer casing 1 through one header 3, flows through the inner fin 2, and flows out of the other pipe section 33 through the other header 3. By circulating the cooling liquid through the outer casing 1 in this way, heat is exchanged between the cooling liquid and the battery through the inner fin 2 and the upper and lower walls of the outer casing 1, and the battery is cooled.

[0087] The heat exchanger of this embodiment is not particularly limited in the manner of use, and may be used alone or in combination of two or more. When using one, as described above, the heat exchanger is used by contacting the upper and lower surfaces of the heat exchanger with the heat exchange target material. When using two, for example, the two heat exchangers may be arranged to sandwich the heat exchange target material. Furthermore, when using two or more, the heat exchangers and the heat exchange target material may be arranged to overlap each other.

[0088] As described above, in the method for manufacturing a heat exchanger according to the present embodiment, the pressure inside the outer envelope 1 is reduced to fuse the inner fin 2 to the outer envelope 1, so that the outer envelope 1 can be sufficiently adhered to the bottom surface of the recessed portion and the top surface of the protruding portion of the inner fin 2 by the shrinkage of the outer envelope 1 due to the reduced pressure, and the adhered portion can be fused as a fused portion. Therefore, the entire area of ​​the predetermined fused portion between the outer envelope 1 and the inner fin 2 can be fused without any gaps, and the occurrence of poor adhesion or insufficient adhesion can be reliably prevented. As a result, the adhesion reliability during heat sealing (thermal fusion) can be significantly improved, and the heat transfer and thus the heat exchange performance can be improved, and defects such as leakage and swelling can be prevented, so that a laminated type heat exchanger with no problems in appearance can be provided.

[0089] Similarly, since the header 3 is fused to the outer envelope 1 while shrinking the outer envelope 1 by reducing the pressure, the outer envelope 1 conforms to the required area of ​​the outer surface of the header 3 and adheres sufficiently, and the adhered area can be fused as a fused area. Therefore, even if the outer surface of the header 3 has a recess such as a sink mark, the outer envelope 1 can be reliably adhered to the sink mark area and the entire predetermined fused area between the outer envelope 1 and the header 3 can be fused without any gaps. Therefore, in this respect as well, it is possible to reliably prevent the occurrence of poor adhesion or insufficient adhesion, and to prevent defects such as leakage and swelling, and it is possible to provide a high-quality laminate-type heat exchanger.

[0090] In addition, in this embodiment, the pressure reduction means 8 of the fin / header fusion mold D2 utilizes the inlet / outlet 16 of the outer cover 1, in other words the pipe section 33 of the header 3, to reduce the pressure inside the outer cover 1, so that the pressure inside the outer cover 1 can be easily and reliably reduced without using any new components or adopting any special configuration.

[0091] In this embodiment, the decompression conditions as the fusion conditions in the fin / header fusion step are preferably set so that the internal pressure of the outer body 1 is 1 / 15 to 1 / 2 of the atmospheric pressure (external pressure of the outer body 1), in other words, 5 cmHg to 38 cmHg. That is, if the internal pressure of the outer body 1 is too low, the outer body 1 and the inner fin 2 are strongly sucked toward the inlet / outlet 16 (the suction part) and deformed, which is undesirable as this may cause the outer body 1 to become molded or wrinkled. Conversely, if the internal pressure of the outer body 1 is too high, the outer body 1 may not be able to be sufficiently tightly attached to the inner fin 2 and the header 3, which may make it difficult to reliably obtain the above-mentioned effects of the decompression, which is undesirable.

[0092] The sealing temperature (heat fusion temperature) is preferably set to 160°C to 250°C, and more preferably to 170°C to 210°C.

[0093] Furthermore, in this embodiment, the fin fusion process and the header fusion process are performed simultaneously, so that the fusion process can be performed more efficiently than when they are performed separately, thereby improving the production efficiency of the heat exchanger.

[0094] In addition, in this embodiment, since the inner fin 2 has a rectangular waveform, the bottom wall of the recess and the top wall of the protrusion are flat, and the contact area with the pair of opposing walls 111, 151 of the outer cover 1 can be increased. This further improves the heat transfer between the inner fin 2 and the outer cover 1, and further improves the heat exchange performance. Furthermore, since a large contact area between the inner fin 2 and the outer cover 1 can be secured, the attachment strength of the inner fin 2 to the outer cover 1 can be improved, and the occurrence of poor contact and the like can be more reliably prevented.

[0095] In this embodiment, the inner fin 2 is formed in an angular wave shape, so that a large number of rising walls connecting the bottom wall of the recess and the top wall of the protrusion are arranged perpendicular to the opposing upper and lower walls 111, 151 of the outer envelope 1. As a result, the inner fin 2 acts to brace against the compressive stress caused by external pressure and acts to pull against the expanding stress caused by internal pressure, so that high strength can be ensured against both internal and external pressure, deformation can be prevented, a stable shape can be reliably maintained, and operational reliability can be further improved. In particular, when multiple heat exchangers are used in a stacked manner, sufficient pressure resistance can be ensured, a stable form (shape) can be reliably maintained, and high heat exchange performance can be reliably obtained.

[0096] Furthermore, in this embodiment, it is preferable to install a reinforcing member such as a spacer that maintains the distance between the pair of opposing walls 111, 151 inside the envelope 1, so that deformation of the space in which the inner fin 2 is housed can be reliably prevented during vacuum sealing or fin placement. Although not shown in the figures, the reinforcing member is preferably made of the same type of resin as the resin that constitutes the interior of the envelope 1, so that it can be bonded to the envelope 1, and its shape is preferably a rectangular parallelepiped. In addition, it is preferable that the reinforcing member is placed in a direction that passes through the center of the envelope 1 and is parallel to the flow of the heat exchange medium. For this reason, it is preferable that the inner fin 2 is placed in the space in a divided manner.

[0097] In the above embodiment, an unmolded sheet-like material is used as the cover member 15 of the outer envelope 1, but this is not limited thereto, and in the present invention, the cover member 15 may be molded. For example, the cover member may be formed of a molded product having a hat-shaped cross section with a central portion recessed upward, and the outer periphery of the hat-shaped cover member may be joined and integrated with the above-mentioned tray-shaped tray member 10 to cover it from above, thereby forming the outer envelope. Furthermore, in the present invention, the outer envelope may be formed by overlapping two unmolded sheet-like outer envelope laminate materials L1 and heat-sealing their outer peripheries.

[0098] In addition, in the above embodiment, an example has been described in which the outer case 1 is formed by bonding two sheets of outer case laminate material L1 together, but this is not limited to this. In the present invention, the number of sheets of outer case laminate material that form the outer case is not limited. For example, the outer case may be formed by folding one sheet of outer case laminate material in half, or three or more sheets of outer case laminate material may be bonded together to form the outer case. EXAMPLES

[0099] <Preparation of heat exchanger components> (1) Preparation of outer laminate material L1 As shown in Table 1, a 120 μm thick aluminum foil made of A8021H-O material was prepared as the metal foil for the heat transfer layer 51 of the outer packaging laminate material (outer packaging material) L1 of Example 1. This aluminum foil was used as the heat transfer layer 51, and a 40 μm thick three-layer (random PP / block PP / random PP: layer ratio of each layer 1 / 8 / 1) unstretched co-extruded film was bonded to one side (inner surface) of the aluminum foil via a urethane adhesive, and a 12 μm thick polyethylene terephthalate (PET) film was bonded to the other side (outer surface) of the heat transfer layer (aluminum foil) via a urethane adhesive to produce the outer packaging laminate material L1.

[0100] (2) Preparation of inner core laminate material L2 As shown in Table 1, an aluminum foil similar to that described above was prepared as the metal foil for the heat transfer layer 61 of the inner core laminate material (inner core material) L2 of Example 1. This aluminum foil was used as the heat transfer layer 61, and a 40 μm-thick three-layer (random PP / block PP / random PP: layer ratio of each layer 1 / 8 / 1) unstretched co-extruded film was bonded to both sides of the aluminum foil via a urethane adhesive to produce the inner core laminate material L2.

[0101] (3) Preparation of Tray Member 10 and Cover Member 15 In accordance with the embodiment shown in Figures 1 to 3, the sheet material obtained by cutting the outer laminate material L1 was subjected to deep drawing molding using a press die to produce a tray member 11 having a recess 11 of width (Wr) 90 mm × length (Lr) 140 mm × depth (Dr) 4 mm and a flange portion 12 of width (Wf) 10 mm formed around the entire periphery of the opening edge of the recess 11, as shown in Figures 9A and 9B.

[0102] In this embodiment, in order to obtain high dimensional accuracy, the tray member 10 was fabricated with a sharp shape. Specifically, the four corner radii (R1) of the recessed portion 11 were 2.0 mm, the die shoulder radius (R2) was 1.0 mm, the punch shoulder radius (R3) was 1.0 mm, and the clearance between the die and punch was 0.25 mm.

[0103] The outer laminate material L1 was also cut to produce a sheet-like cover member 15 of a size (110 mm x 160 mm) corresponding to the upper surface of the tray member 11, with entrance / exit ports 16 (see Figures 1 to 3) formed corresponding to both sides of the recessed portion 11 of the tray member 11.

[0104] (4) Making the inner fin 2 The inner core laminate material L2 was corrugated to produce two types of inner fins, one with a square wave shape and the other with a sinusoidal wave shape, as shown in Figs. 5A and 5B.

[0105] The corrugated inner fin 2 was fabricated by forming the inner core laminate material L2 into a corrugated shape with a fin height (Hf) of 4.1 mm, a fin pitch (Pf) of 4 mm, and a fin thickness (Tf) of 0.2 mm as shown in Fig. 5A, and cutting the corrugated sheet to a length of 100 mm and a width of 90 mm. The crest and valley directions of the inner fin 2 are arranged along the length direction (vertical direction). Furthermore, in the inner fin 2, as in the tray member 11, the outer corner radius (R4) was set to 0.5 mm to give it a sharp shape.

[0106] The sinusoidal wave-shaped inner fin 2 was produced by forming the inner core laminate material L2 into a sinusoidal wave shape with a fin height (Hf) of 4.1 mm, a fin pitch (Pf) of 4 mm, and a fin thickness of 0.2 mm, as shown in Figure 5B, and then cutting the sinusoidal wave sheet to a length of 100 mm and a width of 90 mm.

[0107] (5) Making Header 3 As shown in Figures 2 and 3, a header 3 was produced by injection molding a PP resin material, in which a mounting box portion 31 with a height of 4 mm, a length of 90 mm, and a width of 20 mm was integrally formed with a pipe portion 33 with an inner diameter of φ10 mm, an outer diameter of φ12 mm, and a length of 3 mm.

[0108] <Example 1>

[0109] [Table 1]

[0110] As shown in Table 1, the heat exchanger of Example 1 was produced using the above-mentioned tray member 10, cover member 15, sinusoidal inner fin 2, and header 3. That is, the headers 3, 3 were placed at both ends of the recessed portion 11 of the tray member 10 with each pipe portion 33 facing upward. Furthermore, a sinusoidal inner fin 2 was placed between the headers 3, 3 within the recessed portion 11.

[0111] Next, the cover member 15 was placed on the tray member 10 so as to close the recessed portion 11 from above. At this time, the pipe portions 33, 33 of the headers 3, 3 were inserted into the inlets 16, 16 of the cover member 15 and protruded above the cover member 15.

[0112] This resulted in the creation of a heat exchanger mock-up. This mock-up was then heat-sealed using the following two-stage sealing method.

[0113] The first stage of sealing was performed using the outer case fusion mold D1 shown in Figure 6A under sealing conditions of 190°C (sealing temperature) x 0.3 MPa (sealing pressure) x 7 seconds (sealing time), and the outer case fusion process was performed to heat-seal the flange portion 12 of the tray member 10 and the outer peripheral edge portion of the cover member 15.

[0114] The second stage sealing was performed using fin / header fusion mold D2 shown in Fig. 6B under sealing conditions of 190°C (sealing temperature) x 0.3 MPa (sealing pressure) x 7 seconds (sealing time), with the external pressure (external pressure of outer cover 1) at 76 cmHg and the internal pressure of outer cover 1 reduced to 21 cmHg (-55 cmHg), to perform a fin / header fusion step, adhesively fixing the inner fin 2 and the header 3 to the pair of opposing walls 111, 151 of the outer cover 1 by heat fusion. In this way, the heat exchanger of Example 1 was produced.

[0115] <Example 2> As shown in Table 1, a heat exchanger temporary assembly was produced in the same manner as in Example 1 using the above tray member 10, cover member 15, corrugated inner fin 2, and header 3.

[0116] The first stage of sealing was carried out on this temporary assembly in the same manner as in Example 1 above, and the outer envelope fusion step was carried out.

[0117] Next, the second stage sealing was carried out in the same manner as in Example 1 above, except that the internal pressure of the outer envelope 1 was reduced to 10 cmHg (-66 cmHg), and the fin / header fusion step was carried out to produce the heat exchanger of Example 2.

[0118] <Example 3> As shown in Table 1, a heat exchanger temporary assembly was produced in the same manner as in Example 1 using the above tray member 10, cover member 15, corrugated inner fin 2, and header 3.

[0119] The first stage of sealing was performed on this mock-assembly in the same manner as in Example 1 above, and then the second stage of sealing was performed in the same manner as in Example 1 above, except that the internal pressure of the outer casing 1 was reduced to 3 cmHg (-73 cmHg), thereby producing the heat exchanger of Example 3.

[0120] <Example 4> As shown in Table 1, a heat exchanger temporary assembly was produced in the same manner as in Example 1 using the above tray member 10, cover member 15, corrugated inner fin 2, and header 3.

[0121] The first stage of sealing was performed on this mock-assembly in the same manner as in Example 1 above, and then the second stage of sealing was performed in the same manner as in Example 1 above, except that the internal pressure of the outer casing 1 was reduced to 50 cmHg (-26 cmHg), thereby producing the heat exchanger of Example 4.

[0122] <Comparative Example 1> As shown in Table 1, a heat exchanger temporary assembly was produced in the same manner as in Example 1 using the above tray member 10, cover member 15, corrugated inner fin 2, and header 3.

[0123] On the other hand, a batch fusion mold D11 shown in Fig. 10A was prepared to perform the heat fusion process in Comparative Example 1. In this batch fusion mold D11, a lower mold is provided with a hot plate part H that supports from below the bottom wall 11 and flange part 12 of the tray member 10 of the heat exchanger temporary assembly placed in the mold, and an upper mold is provided with a hot plate part H that presses the entire area of ​​the cover member 15 from above. The mold is then closed to press the upper and lower hot plate parts H against the bottom surface of the tray member 10 and the entire upper surface of the cover member 15, and in this state, the outer envelope fusion process, the fin fusion process, and the header fusion process can be performed simultaneously by the heat from the hot plate part H.

[0124] Using this batch fusion mold D11, the above-mentioned temporary assembly was subjected to the outer envelope fusion process, the fin fusion process, and the fin fusion process all at once by a one-stage sealing method to produce the heat exchanger of Comparative Example 1. The sealing conditions during this fusion were 190°C (sealing temperature) x 0.3 MPa (sealing pressure) x 7 seconds (sealing time).

[0125] <Comparative Example 2> As shown in Table 1, a heat exchanger temporary assembly was produced in the same manner as in Example 1 using the above tray member 10, cover member 15, corrugated inner fin 2, and header 3.

[0126] On the other hand, in order to carry out the heat fusion treatment in Comparative Example 2, a lump-fusion mold D12 shown in Fig. 10B was prepared. In this lump-fusion mold D12, the lower mold is provided with a seal plate S that supports from below the bottom wall 11 and flange portion 12 of the tray member 10 of the heat exchanger temporary assembly placed in the mold, and the upper mold is provided with a seal plate S that presses the entire area of ​​the cover member 15 from above. The upper mold is further provided with a decompression means 80 for decompressing the inside of the mold. Then, the mold is closed, and the upper and lower seal plates S are pressed against the bottom surface of the tray member 10 and the entire upper surface of the cover member 15, and the decompression means 80 reduces the pressure on both the inside and outside of the envelope 1 in the mold, and in this state, the envelope fusion process, the fin fusion process, and the header fusion process can be carried out simultaneously by heat from the hot plate part H.

[0127] Using this batch fusion mold D12, the above-mentioned temporary assembly was subjected to the outer envelope fusion process, the fin fusion process, and the fin fusion process all at once by a one-stage sealing method to produce the heat exchanger of Comparative Example 1. The sealing conditions during this fusion were 190°C (sealing temperature) x 0.3 MPa (sealing pressure) x 7 seconds (sealing time), and 21 cmHg (pressure inside the mold).

[0128] <Comparative Example 3> As shown in Table 1, a heat exchanger temporary assembly was produced in the same manner as in Example 1 using the above tray member 10, cover member 15, corrugated inner fin 2, and header 3.

[0129] On the other hand, in order to carry out the heat fusion treatment in Comparative Example 3, a fin / header fusion mold D13 shown in FIG. 10C was prepared. This fusion mold D13 has substantially the same configuration as the fusion mold D2 shown in FIG. 6B, except that it does not have a pressure reducing means 8. That is, the lower mold of this mold D13 is provided with a hot plate part H that supports from below the bottom wall 111 of the tray member 10 of the heat exchanger temporary assembly placed in the mold, and the upper mold is provided with a hot plate part H that presses from above the opposing wall 151 of the cover member 15. Then, the mold is closed to press the upper and lower hot plate parts H against the bottom surface of the tray member 10 and the center of the upper surface of the cover 15, and in this state, the fin fusion process and the header fusion process can be carried out simultaneously by the heat from the hot plate part H.

[0130] In Comparative Example 3, the above heat exchanger temporary assembly was subjected to heat fusion treatment by the following two-stage sealing method.

[0131] The first stage of sealing was carried out using the outer package fusion mold D1 shown in FIG. 6A in the same manner as in Example 1 above, and the outer package fusion step was carried out under the same sealing conditions.

[0132] For the second stage sealing, the fin / header fusion mold D13 shown in Figure 10C was used, and the fin / header fusion process was performed under sealing conditions of 190°C (sealing temperature) x 0.3 MPa (sealing pressure) x 7 seconds (sealing time), to produce the heat exchanger of Comparative Example 3.

[0133] <Appearance evaluation test> The appearance (particularly the front and back) of each of the heat exchangers of Examples 1 to 4 and Comparative Examples 1 to 3 was visually observed for the presence or absence of thermal wrinkles (shrinkage wrinkles), and if wrinkles were present, the depth of the wrinkles was measured using a contour shape measuring device (Contracer "CV-2100" manufactured by Mitutoyo Corporation).

[0134] The evaluation criteria were as follows: heat exchangers with no wrinkles or with wrinkles less than 15 μm deep on either the front or back were rated as "○ (good)", those with wrinkles 15 μm or more and less than 50 μm deep on either the front or back were rated as "△ (normal)", and those with wrinkles 50 μm or more deep on either the front or back were rated as "× (bad)". The results are also shown in Table 1.

[0135] <Pressure Test> Three heat exchangers (N=3) were prepared for each of Examples 1 to 4 and Comparative Examples 1 to 3, and a pressure resistance evaluation test was performed for each heat exchanger. That is, cooling water was passed through each heat exchanger, and the internal pressure was maintained at 1 MPa for 5 minutes, and then each heat exchanger was observed for the presence or absence of adhesion failure such as peeling or swelling between the outer shell 1 and the inner fin 2 and header 3. For reference, the presence or absence of adhesion failure was also observed when the internal pressure was excessively increased to 1.5 MPa.

[0136] The evaluation criteria were as follows: when the internal pressure was 1.5 MPa, no peeling or blistering occurred, it was rated as "◎ (excellent)", when the internal pressure was less than 1.0 MPa, no peeling or blistering occurred, but when the internal pressure was 1.0 MPa or more and less than 1.5 MPa, peeling or blistering occurred, it was rated as "○ (good)", and when the internal pressure was less than 1.0 MPa, peeling or blistering occurred, it was rated as "× (poor)". The results are also shown in Table 1.

[0137] <Repeated pressure test> Five heat exchangers each (N=5) of Examples 1 to 4 and Comparative Examples 1 to 3 were prepared, and tap water at room temperature (23°C) was passed through each heat exchanger, and a load of 0 MPa water pressure and a load of 0.2 MPa were alternately and repeatedly applied. The appearance of each heat exchanger was observed after 15,000 cycles and 20,000 cycles to check whether peeling or swelling had occurred in any areas.

[0138] The evaluation criteria were as follows: All five heat exchangers were evaluated as "Excellent" if they did not peel off or swell after 20,000 loads, four out of five heat exchangers were evaluated as "Good" if they did not peel off or swell after 20,000 loads and one heat exchanger was evaluated as "Good" if they did not peel off or swell after 15,000 loads, four out of five heat exchangers were evaluated as "Normal" if they did not peel off or swell after 20,000 loads and one heat exchanger was evaluated as "Normal" if they peeled off or swelled after 15,000 loads, and two or more out of five heat exchangers were evaluated as "Poor" if they peeled off or swelled after 20,000 or 15,000 loads. The results are shown in Table 1.

[0139] As is clear from Table 1, the heat exchangers of Examples 1 to 4 were superior to the heat exchangers of Comparative Examples 1 to 3 in appearance, pressure resistance (repeated pressure resistance) and corrosion resistance. [Industrial Applicability]

[0140] The manufacturing method for a heat exchanger of the present invention can be used when producing heat exchangers such as coolers used to counter heat generation around the CPU or battery in smartphones and personal computers, around displays such as LCD TVs, OLED TVs, and plasma TVs, around the power modules or batteries in automobiles, and around heat generation in stationary heat-generating devices such as supercomputers, as well as heaters used for heat absorption in floor heating, snow melting, and other applications. [Explanation of symbols]

[0141] 1: Outer envelope 16: Entrance / exit 2: Inner fin 3: Header 25: Recess 26: Convex 51: Heat transfer layer 52: Heat-sealing layer 61: Heat transfer layer 62: Heat-sealing layer 8: Pressure reduction means 81: Suction pump 82: Main pipe (suction pipe) 83: Branch pipe (suction pipe) D1: Envelope fusion mold D2: Fin / Header Fusion Mold L1: Outer laminate material L2: Inner core laminate material

Claims

1. A method for manufacturing a heat exchanger, comprising: an outer envelope made of an outer laminate material having a resin heat-sealing layer provided on the inner surface side of a metal heat transfer layer; and an inner fin provided within the outer envelope and made of an inner core laminate material having a resin heat-sealing layer provided on both sides of the metal heat transfer layer, the method comprising: an outer envelope fusion step of heat-fusing the outer envelope laminate materials to seal an outer periphery of the outer envelope; and a fin fusion step of heat-fusing the concave and convex portions of the inner fin to the outer envelope after the outer envelope fusion step, The fin fusion step is performed in a state where the inside of the outer cover is reduced in pressure relative to the outside, The outer envelope has an opening for introducing and removing a heat exchange medium into and from the inside thereof, A header made of heat-sealing resin is provided in the outer envelope in correspondence with the inlet and outlet, a header fusion step of heat-sealing an outer surface of the header to the outer envelope after the outer envelope fusion step is performed, The method for manufacturing a heat exchanger, wherein the header fusion step is performed under a condition in which the inside of the outer casing is reduced in pressure relative to the outside.

2. The method for manufacturing a heat exchanger according to claim 1 , wherein in the fin fusing step, the inside of the outer envelope is depressurized by utilizing the inlet / outlet.

3. 3. The method for manufacturing a heat exchanger according to claim 1, wherein the fin fusion step and the header fusion step are carried out simultaneously.

4. A pipe portion is provided in the header and extends to the outside through the inlet / outlet, The method for manufacturing a heat exchanger according to any one of claims 1 to 3, wherein in the fin fusing step, the inside of the outer envelope is depressurized by utilizing the pipe portion.

5. The method for manufacturing a heat exchanger according to any one of claims 1 to 4, wherein in the fin fusing step, the internal pressure of the outer envelope is set to 1 / 15 to 1 / 2 of the external pressure.

6. A heat exchanger manufacturing apparatus for manufacturing a heat exchanger comprising: an outer envelope made of an outer laminate material having a resin heat-sealing layer provided on the inner surface side of a metal heat transfer layer, and having an opening for introducing and removing a heat exchange medium into and from the inside; an inner fin provided within the outer envelope and made of an inner core laminate material having a resin heat-sealing layer provided on both sides of the metal heat transfer layer; and a heat-sealing resin header provided within the outer envelope corresponding to the opening, an outer envelope fusion mold for heat-fusing the outer envelope laminate materials by sandwiching them together and heating them to seal the outer periphery of the outer envelope; a fin / header fusion die for heating the outer shell while pressing it against the inner fin to heat-seal the concave and convex portions of the inner fin to the outer shell and heat-seal the outer surface of the header to the outer shell, A heat exchanger manufacturing apparatus characterized in that the fin / header fusion mold is provided with a pressure reduction means for reducing the pressure inside the outer casing relative to the outside while pressing the outer casing toward the inner fin.

7. The pressure reducing means comprises a suction pump and a suction section having one end connected to the suction pump and penetrating the fin / header fusion die and disposed so as to cover the inlet / outlet with the other end; 7. The heat exchanger manufacturing apparatus according to claim 6, wherein the inside of the outer envelope is depressurized through the suction unit by driving the suction pump. End

Citation Information

Patent Citations

  • Sheet type heat pipe or portable information terminal

    JP2015059693A

  • Manufacturing method of heat pipe, heat pipe, and electronic apparatus

    JP2015141002A

  • Thermal diffusion plate for portable electronic apparatus

    JP2016189415A

  • Resin fusion type heat exchanger

    JP2020003132A

  • Heat exchanger

    JP2020161449A