Method and system for producing hexafluorobutadiene
A continuous production method using a supported metal nanocatalyst for trifluoroethylene and controlled bromination processes addresses safety and yield issues in hexafluorobutadiene production, enhancing industrial suitability and efficiency.
Patent Information
- Application Number
- JP2023032771
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2022-08-18
- Filing Date
- 2023-03-03
- Publication Date
- 2024-12-05
- Estimated Expiration
- 2043-03-03
AI Technical Summary
The production of hexafluorobutadiene is hindered by safety issues such as disproportionation explosions of trifluoroethylene, low yield, and inefficient dehydrobromation processes, which affect industrial scalability and market competitiveness.
A continuous production method using a supported metal nanocatalyst for hydrodechlorination of chlorotrifluoroethylene to trifluoroethylene, followed by controlled bromination and coupling reactions, employing specific catalyst compositions and conditions to suppress disproportionation and enhance yield.
The method achieves high safety, improved yield, and reduced waste emissions, making it suitable for industrial-scale hexafluorobutadiene production.
Smart Images

Figure 0007595103000006 
Figure 0007595103000007 
Figure 0007595103000008
Abstract
Description
[Technical field]
[0001] The present invention relates to the preparation of fluorine-containing olefins, and in particular to a safe method for producing trifluoroethylene, and a production method and system for preparing hexafluorobutadiene by bromination of trifluoroethylene, solid alkaline dehydrobromination and coupling. [Background technology]
[0002] Hexafluorobutadiene is primarily used in plasma media etching of semiconductors, with an ODP of 0 and a GWP of 1. 100 It is a dry etching gas with excellent environmental and etching performance, with a surface area of 290 nm and a residence time in the atmosphere of only 1.9 d. It has a higher etching rate, etching options, and a higher aspect ratio than conventional electronic etching gases such as tetrafluoromethane (CF4), hexafluoroethane (C2F6), octafluoropropane (C3F8), and octafluorocyclobutane (c-C4F8).
[0003] In the preparation process of hexafluorobutadiene, as disclosed in patents CN101031529A and CN110590495A, the most common process is to use chlorotrifluoroethylene as raw material, hydrodechlorination, bromination, dehydrobromination, preparation of zinc reagent and coupling of zinc reagent to prepare hexafluorobutadiene. This process flow has easy access to raw materials and mild conditions, and is most suitable for industrial application.
[0004] However, in actual production, it was found that 1) trifluoroethylene is prone to disproportionation reactions, particularly when coexisting with hydrogen, which makes it prone to disproportionation explosions, posing a major safety hazard, and 2) the liquid alkali dehydrobromination process produces a low and unstable yield of bromotrifluoroethylene.
[0005] Regarding the safety issues of trifluoroethylene, a document published by DuPont in 1997 (Trifluoroethylene deflagration, Andrew E. Feiring; Jon D. Hulburt, American Chemical Society: Chemical & Engineering Safety Letters) states that trifluoroethylene undergoes a disproportionation reaction, releasing a large amount of heat, leading to a pressure rise and explosion.
[0006] Lisochkin et al. (Explosive-hazard estimates for several fluorine-containing monomers and their mixtures, based on the minimum ignition pressure with a fixed igniter energy, Combustion, Explosion and Shock Waves volume 42, pages 140-143 (2006)) point out that when trifluoroethylene coexists with hydrogen, a disproportionation explosion is likely to occur, releasing a large amount of heat.
[0007] At present, research into the safety of trifluoroethylene mainly focuses on such links as refining, transportation, and mixtures, and the safety of the trifluoroethylene production process has not been considered. However, achieving the reaction safety of the preparation of trifluoroethylene by hydrodechlorination of 1,1,2-chlorotrifluoroethylene directly determines the industrialization prospects and market size of hexafluorobutadiene.
[0008] Regarding the liquid alkali dehydrobromination process, the method of removing hydrogen halide using an aqueous solution or alcohol solution of sodium hydroxide or potassium hydroxide is one of the methods commonly used in the preparation of olefins. For example, Patent CN104844411A discloses the preparation of bromotrifluoroethylene by dehydrobromination of 1,2-dibromo-1,1,2-trifluoroethane in the presence of 10% sodium hydroxide solution. Patent CN107032946A also discloses the dehydrobromination reaction of 1,2-dibromo-1,1,2-trifluoroethane using an aqueous solution or alcohol solution of potassium hydroxide or sodium hydroxide under the action of a phase transfer catalyst to produce bromotrifluoroethylene.
[0009] Here, the preparation of bromotrifluoroethylene by dehydrobromination of 1,2-dibromo-1,1,2-trifluoroethane is a key step that restricts the synthesis yield of hexafluorobutadiene. The liquid alkali dehydrobromination reaction has problems of low yield, long reaction time, poor efficiency, and large amounts of three waste products, which significantly restrict the production cost and scale of hexafluorobutadiene, and ultimately affect the market competitiveness of hexafluorobutadiene products. Therefore, it is necessary to develop a new method for preparing bromotrifluoroethylene by dehydrobromination of 1,2-dibromo-1,1,2-trifluoroethane. Summary of the Invention [Means for solving the problem]
[0010] In order to solve the above problems, the present invention proposes a method and system for producing hexafluorobutadiene, which has high production safety, a high total product yield, and is suitable for industrialized production.
[0011] The first aspect of the present invention provides a method for the continuous and safe production of trifluoroethylene, which is realized by the following technical solution:
[0012] A method for continuously producing trifluoroethylene, the method comprising the step of subjecting chlorotrifluoroethylene and hydrogen to a hydrodechlorination reaction in a first reactor under the action of a supported metal nanocatalyst to obtain a mixture, the mixture containing 0.8% to 2.0% of 1,2-dichlorotrifluoroethane (HCFC-123a) and / or 1-chloro-1,2,2-trifluoroethane (HCFC-133), the supported metal nanocatalyst containing at least one first component selected from ruthenium, palladium, or platinum, at least one second component selected from copper, bismuth, and cerium, and an activated carbon carrier.
[0013] Additionally, the mixture further comprises 20% to 50% trifluoroethylene, 43% to 77% chlorotrifluoroethylene, and 2% to 5% 1,1,2-trifluoroethane (HFC-143).
[0014] The temperature of the hydrodechlorination reaction of chlorotrifluoroethylene with hydrogen is 100-200°C, the reaction pressure is 0-2 MPa, and the total volumetric space velocity of hydrogen and chlorotrifluoroethylene is 200-500 h -1 and the molar ratio of hydrogen to chlorotrifluoroethylene is (1.2-2.5):1.
[0015] In the supported metal nanocatalyst of the present invention, the loading amount is based on the carrier mass of the catalyst, and the loading amount of the first component is 0.05 wt% to 5.0 wt%, and the loading amount of the second component is 0.01 wt% to 3.0 wt%, and preferably the loading amount of the first component is 0.1% to 3.0%, and the loading amount of the second component is 0.01% to 2.0%.
[0016] Furthermore, the first component and the second component satisfy the following requirements: The mass ratio of the first component to the second component is 1:(0.1 to 5). Preferably, the mass ratio of the first component to the second component is 1:(0.1 to 2).
[0017] The activated carbon carrier according to the present invention is granular activated carbon or columnar activated carbon, and its material is selected from coconut shell, wood or coal activated carbon. Preferably, the specific surface area of the activated carbon carrier is 1000 m 2 / g or more, and the ash content is 3.0 wt% or less. More preferably, the specific surface area of the activated carbon carrier is 1100 m 2 / g or more, and the ash content is 2.8 wt% or less.
[0018] The supported metal nanocatalyst described in the present invention has a particle diameter of 2-50 nm, and the proportion of metal particles having a particle diameter of 2-10 nm is 90% or more, and has a uniform particle size distribution. The specific particle size is calculated by the following method. Two or three points are randomly selected from a transmission electron microscope (TEM) photograph, enlarged, and then statistically analyzed using Image-Pro Plus software. The calculation formula for the surface average particle diameter is ds=Σnidi3 / Σnidi2, where ni represents the number of metal particles with a diameter of di, and the number of selected metal particles is 200 or more.
[0019] The present invention has a small catalyst particle size and a small active phase particle diameter, which reduces the number of chlorotrifluoroethylene and trifluoroethylene adsorbed on local active sites, lowers the coupling probability between the two, improves the selectivity for trifluoroethylene, and effectively alleviates deactivation due to catalyst carbon accumulation, while reducing the amount of dissociated H formed around the main product trifluoroethylene, making desorption easier.
[0020] The disproportionation explosion during the reaction process of trifluoroethylene is caused by three aspects: 1) disproportionation reaction due to polymerization of trifluoroethylene, 2) disproportionation reaction due to high temperature and pressure, and 3) chain propagation due to the disproportionation of trifluoroethylene, rapid reaction, rapid increase in pressure, and large amount of heat release.
[0021] When the supported metal nanocatalyst described in any one of the above aspects of the present invention is applied to the reaction process of hydrodechlorinating chlorotrifluoroethylene to prepare trifluoroethylene, it can effectively inhibit the disproportionation reaction of trifluoroethylene and greatly improve the safety of the reaction, which can be seen from the following three aspects:
[0022] (1) The supported metal nanocatalyst of the present invention can control the production of trace amounts of HCFC-123a and / or HCFC-133, and utilizes the chlorine atoms in the HCFC-123a and HCFC-133 molecules to capture intermediate radicals in the trifluoroethylene reaction, thereby preventing chain propagation and suppressing the occurrence of trifluoroethylene disproportionation reactions.
[0023] (2) The supported metal nanocatalyst of the present invention controls the production of a small amount of the by-product HFC-143 and suppresses the disproportionation reaction of trifluoroethylene by utilizing the thermal dilution effect of HFC-143.
[0024] (3) The supported metal nanocatalyst of the present invention controls the conversion rate of the raw material chlorotrifluoroethylene to 50% or less, and prevents the occurrence of hot spots in the reactor, i.e., prevents the disproportionation reaction of trifluoroethylene caused by high temperatures.
[0025] The supported metal nanocatalyst according to the present invention is prepared by the following steps.
[0026] A1. Carrier reduction modification: The activated carbon carrier is reduced using a reducing agent at 200 to 800° C. for 1.5 to 3 hours, and then cooled to room temperature. The reducing agent is at least one selected from hydrogen, nitrogen, and ammonia.
[0027] A2. Nanoparticle deposition: The mixture of nanoparticle stabilizer, potassium bromide and potassium chloride is heated to 80-110°C under stirring, and refluxed for 1-2 hours. Then, the first component soluble salt and the second component soluble salt are added, and the reaction is continued by keeping the temperature at 80-110°C for 1.5-2.5 hours. Then, the temperature is lowered to room temperature, and an excess amount of liquid phase reducing agent is dripped in while stirring. Then, the activated carbon carrier reduced and modified in step A1 is added, and an alkaline solution is continuously dripped in, and the pH value is controlled to 6-10.5, preferably 9-10.5, to deposit metal nanoparticles on the surface of the activated carbon carrier.
[0028] A3. Washing and calcination: Filter, wash with deoxygenated deionized water or ethanol until neutral, dry, and calcinate in an inert atmosphere at 300-400°C for 1.0-4.0 hours to obtain a catalyst precursor. Preferably, the calcination temperature is about 350°C, and the calcination time is about 1.5-2.5 hours.
[0029] A4. Reductive activation: The catalyst precursor is placed in a mixed atmosphere of hydrogen and nitrogen, heated to 250-450°C at a rate of 0.1-2.0°C / min, and kept at that temperature for 1-5 hours to obtain the supported metal nanocatalyst.
[0030] In step A1, the reducing agent is preferably a combination of hydrogen and nitrogen, or a combination of ammonia and nitrogen. In the modified activated carbon carrier, the acidic functional groups are decomposed to reduce the oxygen content, and at the same time, the basic functional groups are increased, and the carrier surface is coated with nitrogen-containing functional groups. The adsorption capacity of the reduced and modified activated carbon carrier for non-polar substances is improved.
[0031] In step A2, the first component soluble salt is at least one selected from the chloride, hydrochloride, or organic salt of the first component, such as ruthenium trichloride, ruthenium acetate, chloride or hydrochloride of palladium or platinum, an ethanol solution of sodium chloropalladate (Na2PdCl4), ammonium chloroplatinate, or potassium chloroplatinate (K2PtCl4), and the second component soluble salt is at least one selected from the chloride, nitrate, sulfate, or organic salt of the second component, such as copper chloride, copper nitrate, copper sulfate, bismuth chloride or bismuth nitrate, cerium sulfate, or cerium chloride heptahydrate.
[0032] In step A2, the nanoparticle stabilizer is at least one selected from polyvinylpyrrolidone (PVP), polyacrylate, and hexadecyltrimethylammonium bromide (CTAB), and the molar amount used is 4 to 6 times the sum of the molar amounts of the first component and the second component.
[0033] In step A2, the liquid-phase reducing agent is at least one selected from L-ascorbic acid, NaBH4, citric acid, and ethylene glycol, and the molar amount used is 2 to 4 times the total molar amount of the first component and the second component.
[0034] In step A2, the alkaline solution is a NaOH or KOH solution, and the mass concentration is 2 to 10 wt %.
[0035] In step A2, in the mixture of potassium bromide and potassium chloride, the molar ratio of potassium chloride / potassium bromide is 1:0.01 to 1:0.3.
[0036] The supported metal nanocatalyst of the present invention contains a (111) crystal face and a (100) crystal face, and the inventors have found through research that the depth of the catalytic hydrogenation reaction of chlorotrifluoroethylene and the distribution of the products can be controlled by changing the crystal face ratio. Specifically, the (111) crystal face is favorable for the production of the target product trifluoroethylene TrFE, and produces a small amount of HCFC-123a (reaction route: CTFE → HCFC-123a → TrFE), while the (100) crystal face has a high adsorption capacity for chlorotrifluoroethylene and is favorable for the production of the by-products HCFC-133 and HFC-143.
[0037] In the present invention, by changing the ratio of potassium bromide and potassium chloride, the ratio of the (111) crystal face to the (100) crystal face can be adjusted, and the depth of the catalytic hydrogenation reaction and the distribution of the products can be controlled. The reason for this is presumed to be as follows.
[0038] (i)Br - preferentially adsorbs on the (100) crystal face of the metal cation, i.e., crystal growth in the (100) direction is promoted. (ii) Cl - Br - The use of potassium chloride favors the creation of a (111) crystalline surface for the alloy because it has weaker interactions with metal cations than (100) and the (111) metal surface has the lowest surface energy, and the nanoparticles will attempt to minimize the total surface energy [Note: (111)<(100)<(110)].
[0039] In step A3, to prevent the nanoparticle stabilizer and liquid-phase reducing agent from being adsorbed on the catalyst surface, which weakens the contact between the reactants and the active sites, i.e., reduces the catalytic activity, alcohol washing and roasting are used to remove the nanoparticle stabilizer and liquid-phase reducing agent.
[0040] The present invention provides a method for continuous production of 1,2-dibromotrifluoroethane, the method comprising the steps of feeding the above-obtained mixture to a rectification apparatus for separation, feeding the trifluoroethylene obtained by rectification to a second reactor and continuously reacting with bromine under light irradiation to obtain 1,2-dibromotrifluoroethane, and returning the chlorotrifluoroethylene obtained by rectification to the first reactor for recycling.
[0041] The rectification apparatus includes at least two rectification columns, with trifluoroethylene being taken from the top of the first rectification column and chlorotrifluoroethylene being taken from the reflux tube of the last rectification column.
[0042] In a specific embodiment, two rectification towers are used to separate the mixture, the first rectification tower has a tower bottom temperature of 20°C to 40°C, a condenser temperature of -10°C to 0°C, and a tower bottom pressure of 0.5 to 1.5 MPa, and the second rectification tower has a tower bottom temperature of 40 to 60°C, a condenser temperature of 0°C to 10°C, and a tower bottom pressure of 0.3 to 0.8 MPa.
[0043] Due to safety issues with trifluoroethylene, the rectified trifluoroethylene must be immediately fed to a second reactor to react continuously with bromine under light irradiation to obtain 1,2-dibromotrifluoroethane. The complete reaction scheme is as follows:
[0044] [ka]
[0045] The bromine is bromine vapor, and the molar ratio of trifluoroethylene to bromine vapor is 1:(0.3 to 3). Preferably, the molar ratio of trifluoroethylene to bromine vapor is 1:(0.9 to 1.1).
[0046] The reaction temperature between trifluoroethylene and bromine vapor is 0° C. to 150° C., and the pressure is 0 to 1 MPa. Preferably, the reaction temperature between trifluoroethylene and bromine vapor is 20° C. to 80° C., and the pressure is 0 to 0.3 MPa.
[0047] The second aspect of the present invention provides a continuous method for producing bromotrifluoroethylene, the method includes the steps of continuously adding 1,2-dibromotrifluoroethane and a solid alkali reaction to a third reactor containing 1,2-dibromotrifluoroethane in advance to obtain bromotrifluoroethylene, the reaction formula of which is as follows:
[0048] [ka]
[0049] Specifically, the reaction includes the following steps: B1. Pre-add 1,2-dibromotrifluoroethane (as a solvent) to the third reactor, turn on the external circulation pump, and allow the 1,2-dibromotrifluoroethane to flow out of the third reactor and back into the third reactor via the filtration device. B2. The temperature is raised to the reaction temperature, 1,2-dibromotrifluoroethane and solid alkali are continuously added, bromotrifluoroethylene gas is collected and condensed to obtain bromotrifluoroethylene liquid, and the by-product is discharged from the reaction system through a filtration device to realize a continuous reaction.
[0050] In step B1, the volume of 1,2-dibromotrifluoroethane pre-entered into the third reactor is 1 / 4 to 1 / 2 the volume of the third reactor. The flow rate per hour of the external circulation pump is 1 / 5 to 5 times the volume of the third reactor.
[0051] In step B2, 1,2-dibromotrifluoroethane is continuously added, and the amount charged per hour is (0.01 to 0.1) of the amount previously charged.
[0052] The molar ratio of the supply rates of the solid alkali to 1,2-dibromotrifluoroethane is 1:(0.8 to 1.2). Preferably, the molar ratio of the supply rates of the solid alkali to 1,2-dibromotrifluoroethane is 1:1.
[0053] The temperature of the dehydrobromination reaction is 30°C to 80°C, and preferably the reaction temperature is 60°C to 70°C.
[0054] The solid alkali is at least one selected from lithium hydroxide, sodium hydroxide, potassium hydroxide, calcium hydroxide, sodium carbonate, and potassium carbonate. Preferably, the solid alkali is at least one selected from sodium hydroxide, potassium hydroxide, sodium carbonate, and potassium carbonate.
[0055] In order to improve the reaction efficiency, the particle size of the solid alkali is in the range of 10 μm to 5 mm, and preferably, the particle size of the solid alkali is in the range of 100 μm to 1 mm.
[0056] The bromotrifluoroethylene enters a condenser from the gas phase outlet of the third reactor and is condensed and collected, and the condenser temperature is selected from -15°C to -5°C.
[0057] A third aspect of the present invention provides a method for producing hexafluorobutadiene, said method comprising the steps of:
[0058] (1) Any of the above-described methods for continuous production of trifluoroethylene is employed, and the mixture containing trifluoroethylene is prepared in a first reactor. From the mixture, 1,2-dibromotrifluoroethane is prepared in a second reactor by any of the above-described methods for continuous production of 1,2-dibromotrifluoroethane.
[0059] (2) Any of the above-mentioned processes for continuous production of bromotrifluoroethylene is employed, and bromotrifluoroethylene is prepared in a third reactor.
[0060] (3) Add bromotrifluoroethylene to the fourth reactor containing zinc powder, initiator and organic solvent to react, obtain trifluorovinyl zinc bromide, filter and feed to the fifth reactor, add coupling agent to couple and obtain hexafluorobutadiene, the reaction equation is as follows:
[0061] [ka]
[0062] In the fourth reactor, first, an organic solvent, an initiator and zinc powder are added and stirred, and the temperature is raised to 0 to 100°C (preferably 30 to 60°C), and then bromotrifluoroethylene is added and reacted to obtain a trifluorovinyl zinc bromide solution. The zinc powder in the trifluorovinyl zinc bromide solution is removed by filtration, and the solution is supplied to a fifth reactor, and a coupling agent is added at -20 to 50°C (preferably -10 to 10°C) to react with the solution to obtain hexafluorobutadiene.
[0063] The organic solvent is at least one selected from N,N-dimethylformamide (DMF), N,N-dimethylacetamide (DMAc), dimethylsulfoxide (DMSO) and tetrahydrofuran (THF), and the water content in the organic solvent is 200 ppm or less.
[0064] The initiator is at least one selected from bromomethane, 1,2-dibromoethane, simple iodine, chlorotrimethylsilane, and a trifluorovinyl zinc bromide solution.
[0065] The coupling agent is at least one selected from copper iodide, copper bromide, copper chloride, ferric chloride, and ferric bromide.
[0066] A fourth aspect of the present invention provides a system for producing hexafluorobutadiene, the system comprising: (1) A subsystem X for producing 1,2-dibromotrifluoroethane, comprising a first reactor, a water alkali washing device, a rectification device and a second reactor connected in sequence, the first reactor being a gas-solid phase reactor filled with the supported metal nanocatalyst according to any one of claims 1 to 10, and having a raw material gas inlet and a mixture outlet, the mixture outlet being connected to the inlet of the rectification device, the top of the rectification device being connected to the trifluoroethylene inlet of the second reactor, the second reactor being a photobromination reactor, and further comprising a bromine vapor inlet, a 1,2-dibromotrifluoroethane outlet and a non-condensable gas outlet; (2) Subsystem Y for producing bromotrifluoroethylene, comprising a third reactor, the third reactor being a dehydrobromination reactor, and equipped with a solid alkali continuous supply device, a 1,2-dibromotrifluoroethane inlet connected to the 1,2-dibromotrifluoroethane outlet of the second reactor, an outlet, and a bromotrifluoroethylene outlet, the outlet being connected to a filtration device for filtering by-products, and the bromotrifluoroethylene outlet being connected in turn to a condenser A for refluxing 1,2-dibromotrifluoroethane and a condenser B for condensing bromotrifluoroethylene; (3) Subsystem Z for producing hexafluorobutadiene, the Subsystem Z including a fourth reactor, a fifth reactor, and a hexafluorobutadiene collection device connected in series, the fourth reactor being connected to the bromotrifluoroethylene outlet of the third reactor.
[0067] It is common knowledge and well known to those skilled in the art that each piece of equipment is connected by piping, that valves and pumps are installed at the inlets and outlets, and that storage tanks are often used for temporary storage of raw materials and products (e.g., chlorotrifluoroethylene storage tanks, bromine storage tanks, bromotrifluoroethylene storage tanks, hexafluorobutadiene storage tanks, etc.), and therefore will not be repeated here.
[0068] Furthermore, the rectification apparatus includes a first rectification column and a second rectification column, and the trifluoroethylene-containing mixture passes through a water alkali washing device, is compressed and supplied to the first rectification column (excess hydrogen that cannot be compressed is discharged), trifluoroethylene is collected from the top of the column and supplied to the second reactor, the remainder is supplied to the second rectification column, and chlorotrifluoroethylene is collected from the reflux pipe and returned to the first reactor for recycling.
[0069] Furthermore, 1,2-dibromotrifluoroethane from which by-products have been removed by filtration in the filtration device is returned to the third reactor.
[0070] Furthermore, the fourth reactor has an inlet connected to an organic solvent supply device, a zinc powder supply device and a bromotrifluoroethylene supply device, and an outlet connected to an excess zinc powder filter device; the fifth reactor has an inlet connected to the outlet of the zinc powder filter device and is equipped with a coupling agent supply device, and an outlet connected to a hexafluorobutadiene collector, which includes a condenser and a storage tank.
[0071] The material of the first reactor of the present invention is one selected from 316L, Inconel 600 alloy, Monel 400 alloy, and Hastelloy C alloy, the material of the second reactor is one selected from silicate glass, quartz glass, and silicon carbide, the material of the third reactor is one selected from glass lining, silicon carbide, and Teflon-lined carbon steel, the material of the fourth reactor is one selected from glass lining, silicon carbide, 316L, and Teflon-lined carbon steel, and the material of the fifth reactor is one selected from glass lining, silicon carbide, 316L, and Teflon-lined carbon steel. Effect of the Invention
[0072] The present invention has the following advantageous effects compared to the prior art:
[0073] 1. It is possible to control certain reaction by-products. By utilizing the action of the by-products HCFC-123a and HCFC-133 to capture trifluoroethylene radicals, it is possible to remove the energy source and block the chain reaction to avoid the occurrence of the disproportionation reaction of trifluoroethylene. By utilizing the thermal dilution effect of the by-product HFC-143, it is possible to control the reaction conversion rate and avoid the occurrence of hot spots, thereby realizing the safety of trifluoroethylene production.
[0074] 2. The supported metal nanocatalyst of the present invention has a long life, good stability, and good resistance to carbon deposition and sintering while maintaining a low conversion rate of chlorotrifluoroethylene.
[0075] 3. The present invention adopts a solid alkali continuous dehydrobromination process, which prevents the product bromotrifluoroethylene from contacting with proton-type solvents, not only improving the production efficiency and reaction yield, but also reducing the discharge of three waste products. [Brief description of the drawings]
[0076] [Figure 1a] This is a 1,2-dibromotrifluoroethane process subsystem X in a hexafluorobutadiene production system according to an embodiment of the present invention, and includes: 1: chlorotrifluoroethylene cylinder, 2: hydrogen cylinder, 3: first reactor, 4: water alkali washing device, 5: compressor, 6: condenser, 7: first fractionator, 8: second fractionator, 9: second reactor, 10: bromine evaporation tank, 11: 1,2-dibromotrifluoroethane storage tank, and 12: chlorotrifluoroethylene storage tank. [Figure 1b] This is a bromotrifluoroethylene process subsystem Y in a hexafluorobutadiene production system according to an embodiment of the present invention, and includes: 13: a 1,2-dibromotrifluoroethane storage tank; 14: a third reactor; 15: a solid alkali storage tank; 16: a condenser; 17: a condenser; 18: a bromotrifluoroethylene storage tank; 19: a by-product filtration tank; and 20: a by-product filtration tank. [Figure 1c]This is a hexafluorobutadiene process subsystem Z in a hexafluorobutadiene production system according to an embodiment of the present invention, and includes 21: a bromotrifluoroethylene cylinder, 22: a fourth reactor, 23: a zinc powder storage tank, 24: a condenser, 25: a zinc powder filtration device, 26: a fifth reactor, 27: a coupling agent storage tank, 28: a condenser, 29: a condenser, and 30: a hexafluorobutadiene storage tank. [Diagram 2] 1 is a curve of the safety test of the Cat1 hydrogenation product prepared in Preparation Example 1 of the present invention. [Diagram 3] 4 is a curve of the safety test of the Cat-DB2 hydrogenation product prepared in Comparative Preparation Example 2 of the present invention. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0077] The present invention will be further described below with reference to specific examples, but the present invention is not limited to these specific embodiments. Those skilled in the art should recognize that the present invention includes all alternatives, improvements and equivalents that may be included within the scope of the claims.
[0078] Preparation Example 1 This preparation example provides the preparation of a supported metal nanocatalyst, and specifically includes the following steps:
[0079] A1. Carrier reduction modification: 20g of activated carbon carrier is placed in a mixed gas atmosphere of ammonia and nitrogen (V NH3 :V N2 =1:5) and treated at 450°C for 2 hours, after which it was cooled to room temperature before use.
[0080] A2. Nanoparticle deposition: 7mL of platinum chloride hydrochloric acid solution (Pt 3.8%), 0.6g BiCl3, and 5mL of hydrochloric acid solution (concentration 37%) were weighed and dissolved in 40mL deionized water for use. Polyvinylpyrrolidone (PVP), a mixture of potassium chloride and potassium bromide (molar ratio of KCl to KBr is 1:0.2) was packed in a round-bottom flask, magnetic stirring was adopted, and the mixture was heated at 85°C and refluxed for 1h. Next, the above-mentioned mixed solution of platinum chloride and BiCl3 was added, heated at 85°C for 2h, and then cooled to room temperature. Then, excess liquid-phase reducing agent NaBH4 was added dropwise. While continuing the stirring state, the activated carbon carrier reduced and modified in step A1 was added, a 3% concentration NaOH solution was added dropwise, the pH value was controlled to 9, and metal nanoparticles were deposited on the surface of the carrier.
[0081] A3. Washing and calcination: After filtration, the filter cake was washed with deoxygenated deionized water and ethanol until neutral, and then vacuum dried at 100°C for 8 hours. Then, it was placed in an atmosphere furnace and calcined at 350°C for 2 hours under a nitrogen atmosphere to obtain the catalyst precursor.
[0082] A4. Reductive activation: The catalyst precursor is heated under a mixed atmosphere of hydrogen and nitrogen (V 水素 :V 窒素 =1:3), and the temperature was increased to 250 °C at a rate of 2.0 °C / min and kept at that temperature for 2 h to obtain a supported metal nanocatalyst, which was designated Cat1.
[0083] Preparation Example 2 This preparation example provides the preparation of a supported metal nanocatalyst, and specifically includes the following steps:
[0084] A1. The carrier reduction modification step was the same as in Preparation Example 1.
[0085] A2. Nanoparticle deposition: 6.1 mL of palladium chloride solution in hydrochloric acid (concentration 0.033 g Pd / mL) and 2.3 g Cu(NO3)2·3H2O were weighed and dissolved in 40 mL of deionized water. Polyvinylpyrrolidone (PVP), a mixture of potassium chloride and potassium bromide (molar ratio of KCl to KBr is 1:0.2) were charged into a round-bottom flask, and the flask was heated to reflux at 85 °C for 1 h under magnetic stirring.
[0086] Next, the mixed solution of palladium chloride and copper nitrate was added, heated at 85°C for 2 hours, and then cooled to room temperature. Excess liquid-phase reducing agent NaBH4 was then added dropwise. While continuing to stir, the activated carbon carrier reduced and modified in step A1 was added, and a 3% NaOH solution was added dropwise, controlling the pH value to 9.5, and metal nanoparticles were deposited on the surface of the carrier.
[0087] A3. The washing and calcination steps were the same as in Preparation 1.
[0088] A4. The reductive activation step was the same as in Preparation Example 1, and a supported metal nanocatalyst was obtained, which was designated as Cat2.
[0089] Preparation Example 3 This preparation example provides the preparation of a supported metal nanocatalyst, and specifically includes the following steps:
[0090] A1. The carrier reduction modification step was the same as in Preparation Example 1.
[0091] A2. Nanoparticle deposition: 0.7 g ruthenium trichloride hydrate (Ru 43%) and 3.1 g Ce(NO3)3·6H2O were weighed and dissolved in 40 mL deionized water. Hexadecyltrimethylammonium bromide (CTAB), a mixture of potassium chloride and potassium bromide (molar ratio of KCl to KBr is 1:0.2) were charged into a round-bottom flask and heated to reflux at 85 °C for 1 h under magnetic stirring.
[0092] Next, the mixed solution of the ruthenium trichloride hydrate and cerium nitrate was added, heated at 85°C for 2 hours, and then cooled to room temperature. Then, excess liquid-phase reducing agent NaBH4 was added dropwise. While continuing to stir, the activated carbon carrier modified by step reduction in A1 was added, and a 3% NaOH solution was added dropwise, the pH value was controlled to 9.5, and metal nanoparticles were deposited on the surface of the carrier.
[0093] A3. The washing and calcination steps were the same as in Preparation 1.
[0094] A4. The reductive activation step was the same as in Preparation Example 1, and a supported metal nanocatalyst was obtained, which was designated as Cat3.
[0095] Preparation Example 4 This preparation example provides the preparation of a supported metal nanocatalyst, and specifically includes the following steps:
[0096] A1. The carrier reduction modification step was the same as in Preparation Example 1.
[0097] A2. Nanoparticle deposition: 5.2g of platinum chloride in hydrochloric acid (Pt 3.8%) and 1.3g Ce(NO3)3·6H2O were weighed and dissolved in 40mL deionized water. Hexadecyltrimethylammonium bromide (CTAB), a mixture of potassium chloride and potassium bromide (molar ratio of KCl to KBr is 1:0.2) were packed in a round-bottom flask, and magnetic stirring was adopted, and the mixture was heated to 85℃ and refluxed for 1h. Next, the above-mentioned mixture of platinum chloride and cerium nitrate was added, heated at 85℃ for 2h, and then cooled to room temperature. Then, excess liquid-phase reducing agent NaBH4 was added dropwise. While continuing the stirring state, the activated carbon carrier reduced and modified in step A1 was added, and a 3% NaOH solution was added dropwise, and the pH value was controlled to 10, and metal nanoparticles were deposited on the surface of the carrier.
[0098] A3. The washing and calcination steps were the same as in Preparation 1.
[0099] A4. The reductive activation step was the same as in Preparation Example 1, and a supported metal nanocatalyst was obtained, which was designated as Cat4.
[0100] Preparation Example 5 This preparation example provides the preparation of a supported metal nanocatalyst, and specifically includes the following steps:
[0101] A1. The carrier reduction modification step was the same as in Preparation Example 1.
[0102] A2. Nanoparticle deposition: 6.1 mL of palladium chloride hydrochloric acid solution (concentration 0.033 g Pd / mL), 0.9 g BiCl3, and 5 mL of hydrochloric acid solution (concentration 37%) were weighed and dissolved in 40 mL of deionized water. Polyvinylpyrrolidone (PVP), a mixture of potassium chloride and potassium bromide (molar ratio of KCl to KBr is 1:0.2) were charged into a round-bottom flask, and heated to reflux at 85 °C for 1 h under magnetic stirring.
[0103] Next, the mixed solution of palladium chloride and BiCl3 was added, heated at 85°C for 2 hours, and then cooled to room temperature. Then, excess liquid-phase reducing agent NaBH4 was added dropwise. While continuing to stir, the activated carbon carrier reduced and modified in step A1 was added, a 3% NaOH solution was added dropwise, the pH value was controlled to 10, and metal nanoparticles were deposited on the surface of the carrier.
[0104] A3. The washing and calcination steps were the same as in Preparation 1.
[0105] A4. The reductive activation step was the same as in Preparation Example 1, and a supported metal nanocatalyst was obtained, which was designated as Cat5.
[0106] Comparative Preparation Example 1 This comparative example provides the preparation of a supported metal nanocatalyst, specifically including the following steps:
[0107] B1. The support reduction modification step was the same as in Preparation Example 1.
[0108] B2. Impregnation: 0.6g BiCl3, 5mL hydrochloric acid solution (38wt%) and 7mL hydrochloric acid solution of platinum chloride (Pt 3.8%) were weighed, and 80.0mL distilled water was added to dilute thoroughly. 20g of the reduced and modified activated carbon carrier was added, impregnated for 2h, and dried at 110℃ for 8h.
[0109] B3. Reductive activation: The catalyst precursor obtained in B1 was placed in a mixed atmosphere of hydrogen and nitrogen, heated to 250°C at a rate of 2.0°C / min, and kept at that temperature for 2 hours to obtain hydrodechlorination catalyst Cat-DB1.
[0110] Comparative Preparation Example 2 This comparative example provides the preparation of a supported metal nanocatalyst. The specific operation is the same as that of Preparation Example 1, except that in the A2 nanoparticle deposition step, only potassium bromide was used instead of potassium chloride, and hydrodechlorination catalyst Cat-DB2 was obtained.
[0111] Comparative Preparation Example 3 This comparative example provides the preparation of a supported metal nanocatalyst. The specific operation is the same as that of Preparation Example 1, except that in the A2 nanoparticle deposition step, the molar ratio of the mixture of potassium chloride and potassium bromide is 0.2:1, to obtain hydrodechlorination catalyst Cat-DB3.
[0112] Example 1 This embodiment provides a hexafluorobutadiene production system, which includes a 1,2-dibromotrifluoroethane process subsystem X shown in FIG. 1a, a bromotrifluoroethylene process subsystem Y shown in FIG. 1b, and a hexafluorobutadiene process subsystem Z shown in FIG. 1c, and is specifically as follows.
[0113] The 1,2-dibromotrifluoroethane process subsystem X includes a chlorotrifluoroethylene cylinder 1, a hydrogen cylinder 2, a first reactor 3, a water alkali washing device 4, a compressor 5, a condenser 6, a first rectification column 7, a second rectification column 8, a second reactor 9, a bromine evaporation tank 10, a 1,2-dibromotrifluoroethane storage tank 11, and a chlorotrifluoroethylene storage tank 12.
[0114] Bromotrifluoroethylene process subsystem Y includes 1,2-dibromotrifluoroethane storage tank 13, third reactor 14, solid alkali storage tank 15, condenser 16, condenser 17, bromotrifluoroethylene storage tank 18, by-product filtration tank 19 and by-product filtration tank 20.
[0115] Hexafluorobutadiene process subsystem Z includes a bromotrifluoroethylene cylinder 21, a fourth reactor 22, a zinc powder storage tank 23, a condenser 24, a zinc powder filtration device 25, a fifth reactor 26, a coupling agent storage tank 27, a condenser 28, a condenser 29 and a hexafluorobutadiene storage tank 30.
[0116] This embodiment further provides a method for producing hexafluorobutadiene using the above-mentioned system for producing hexafluorobutadiene, the method comprising: S1. Preparation of trifluoroethylene and 1,2-dibromo-1,1,2-trifluoroethane: under the action of supported metal nano catalyst, chlorotrifluoroethylene and hydrogen are hydrodechlorinated in the first reactor to obtain a mixture, the mixture is fed to the first and second rectification towers for separation, trifluoroethylene is collected from the top of the first rectification tower and fed to the second reactor, and reacted with bromine under light irradiation to obtain 1,2-dibromotrifluoroethane, and chlorotrifluoroethylene is collected from the reflux tube of the second rectification tower and returned to the first reactor for recycling; S2. Preparation of bromotrifluoroethylene: pre-adding 1,2-dibromotrifluoroethane as a solvent to the third reactor, turning on the external circulation pump, flowing 1,2-dibromotrifluoroethane out of the third reactor, and returning it to the third reactor via a filtration device, heating to a reaction temperature, continuously adding 1,2-dibromotrifluoroethane and solid alkali, collecting bromotrifluoroethylene gas, and condensing it to obtain bromotrifluoroethylene liquid; S3. Add bromotrifluoroethylene to the fourth reactor containing zinc powder, initiator and organic solvent to react, obtain trifluorovinyl zinc bromide, filter and feed to the fifth reactor, add coupling agent to couple and obtain hexafluorobutadiene.
[0117] Example 1-1 Cat1 and Cat-DB2 were used as supported metal nano catalysts, respectively, and chlorotrifluoroethylene and hydrogen were reacted in the first reactor. The reaction temperature was 85°C, the reaction pressure was normal pressure, and the total volumetric space velocity of the raw materials, hydrogen and chlorotrifluoroethylene, was 300 h -1 and n (H2) :n (CTFE) The ratio of the mixture to the total mixture was 2:1, and the mixture obtained in the reaction was collected and subjected to safety testing. The test method was that the mixture test pressure environment was 1.8 MPa and the mixture was ignited at 30°C.
[0118] As shown in FIG. 2, when the Cat 1 hydrodechlorination product was used for the test, no obvious changes were observed in the vessel, i.e., trifluoroethylene did not explode.
[0119] As shown in FIG. 3, when a test was conducted using a hydrodechlorination product of Cat-DB2, the pressure inside the vessel rose rapidly, that is, it was found that a TrFE mixture of this composition may cause branching explosion.
[0120] Example 2-1 This example provides a preparation of 1,2-dibromotrifluoroethane, specifically including the following steps:
[0121] Subsystem X is used to produce 1,2-dibromotrifluoroethane. The first reactor is a fixed-bed reactor made of Inconel 600 alloy, with an inner diameter of 0 mm and a length of 550 mm. It is filled with 10.0 g of Cat1 to Cat5 and Cat-DB1 to Cat-DB3, respectively. The reaction temperature is 80 to 150 °C, the operating pressure is normal pressure, and the raw material space velocity is 200 to 500 h -1 , the ratio of raw materials is V H2 :V TrFE The ratio was 2:1, and the reaction product was washed with water and alkali, compressed, and supplied to the first fractionator (column volume 5 L, column diameter 20 mm, column height 3 m, column temperature 30°C, condenser temperature -5°C, column pressure 0.8 MPa), and the excess hydrogen that could not be compressed was discharged from the top of the condenser.
[0122] The reaction mixture gas is separated through the first fractionator, and trifluoroethylene is collected from the top gas phase of the condenser of the first fractionator and supplied to a photobromination reactor, where it reacts with bromine vapor under light irradiation (the molar ratio of trifluoroethylene to bromine is 1:0.95) to obtain 1,2-dibromotrifluoroethane. The column material of the first fractionator is supplied to the second fractionator (column volume 5L, column diameter 20mm, column height 3m, column temperature 50℃, condenser temperature 0℃, column pressure 0.5MPa), and chlorotrifluoroethylene is collected from the reflux pipe of the second fractionator in a storage tank, and supplied from the storage tank to the raw material supply piping of the first reactor.
[0123] The reaction mixture gases of different catalysts were sampled and analyzed before being fed to the first fractionator, and the results are shown in Table 1 below.
[0124] [Table 1]
[0125] The results of the sampling analysis of trifluoroethylene for each batch before it entered the photobromination reaction via separation in the first fractionator and the analysis results of 1,2-dibromoethane, the product of photobromination, are shown in the table below.
[0126] [Table 2]
[0127] Example 3-1 This example provides a preparation of bromotrifluoroethylene, specifically including the following steps:
[0128] Subsystem Y for producing bromotrifluoroethylene was replaced with high purity nitrogen until the oxygen content was 0.1% or less. 9600 kg (40 mol) 1,2-dibromotrifluoroethane was added to a 10 L glass reactor, the stirring and reactor jacket heating devices were turned on to control the reactor internal temperature at 60°C, the inlet and outlet valves of the 1,2-dibromotrifluoroethane condensing reflux 16 were opened to control the jacket temperature at 5°C, the inlet and outlet valves of the bromotrifluoroethylene condensing reflux 17 were opened to control the jacket temperature at -15°C, the reactor bottom valve was opened to connect to a 2 L external filtration device, and the external circulation pump was turned on to control the flow rate at 2 L / h.
[0129] The 1,2-dibromotrifluoroethane feed pump was turned on and the flow rate was controlled at 400 g / h, and the solid feed was turned on to add sodium hydroxide pellets to the reaction kettle at 66.4 g / h.
[0130] The 1,2-dibromotrifluoroethane vapor was returned to the reaction vessel via the condenser 16, and the bromotrifluoroethylene was collected in a low-temperature refrigerator via the condenser 17. The reaction was continued for 24 hours, and 9600.5 g of 1,2-dibromotrifluoroethane and 1600.5 g of sodium hydroxide were added in total. The theoretical yield was 6414 g, and 6188.1 g of the product bromotrifluoroethylene was collected, which was an anhydrous liquid with a chromatographic purity of 98.5% and a yield of 95.0% (calculated as sodium hydroxide).
[0131] Example 3-2 The operation of this example was the same as that of Example 3-1, except that potassium hydroxide was used instead of sodium hydroxide and the charging rate was 93 g / h. The charging amount and charging rate of 1,2-dibromotrifluoroethane were the same. The reaction was continued for 24 hours, and 9600.5 g of 1,2-dibromotrifluoroethane and 2232 g of potassium hydroxide were charged in total. The theoretical yield was 6414 g. 6125.0 g of the product bromotrifluoroethylene was collected, which was an anhydrous liquid, and the chromatography showed a purity of 98.2% and a yield of 93.8% (based on potassium hydroxide).
[0132] Example 3-3 The operation of this example was the same as that of Example 3-1, except that sodium carbonate was used instead of sodium hydroxide and the charging rate was 88 g / h. The charging amount and charging rate of 1,2-dibromotrifluoroethane were the same. The reaction was continued for 24 hours, and 9600.5 g of 1,2-dibromotrifluoroethane and 2112 g of sodium carbonate were charged in total, the theoretical yield was 6414 g, and 5120.7 g of the product bromotrifluoroethylene was collected, which was an anhydrous liquid, had a chromatographic purity of 98.2%, and a yield of 78.4% (calculated as sodium carbonate).
[0133] Examples 3-4 The operation of this example was the same as that of Example 3-1, except that the reaction temperature was lowered from the original 60° C. to 50° C. The reaction was continued for 24 hours, and 9600.5 g of 1,2-dibromotrifluoroethane and 1588.8 g of sodium hydroxide were added in total. The theoretical yield was 6414 g, and 5355.8 g of the product bromotrifluoroethylene was collected, which was an anhydrous liquid with a chromatographic purity of 98.8% and a yield of 82.5% (calculated as sodium hydroxide).
[0134] Examples 3-5 The operation of this example was the same as that of Example 3-1, except that the reaction temperature was increased from the original 60° C. to 70° C. The reaction was continued for 24 hours, and 9600.5 g of 1,2-dibromotrifluoroethane and 1588.8 g of sodium hydroxide were added in total. The theoretical yield was 6414 g, and 6473.8 g of the product bromotrifluoroethylene was collected, which was an anhydrous liquid with a chromatographic purity of 96.6% and a yield of 97.5% (calculated as sodium hydroxide).
[0135] Examples 3-6 The operation of this example was the same as in Example 3-1, except that the feed rate of 1,2-dibromotrifluoroethane was increased from the original 400g / h to 800g / h, and the feed rate of sodium hydroxide was increased from the original 66.2g / h to 132.4g / h. The reaction was continued for 12 hours, and 9600.5g of 1,2-dibromotrifluoroethane and 1588.8g of sodium hydroxide were added in total, the theoretical yield was 6414g, and 5971.0g of the product bromotrifluoroethylene was collected, which was anhydrous liquid, had a chromatographic purity of 97.0%, and a yield of 90.3% (calculated as sodium hydroxide).
[0136] Comparative Example 3-1 The operation of this example was the same as that of Example 3-1, except that 30% sodium hydroxide solution was used instead of solid sodium hydroxide, and the charging rate was 221g / h. The reaction was continued for 12 hours, and 4800g of 1,2-dibromotrifluoroethane and 2652g of 30% sodium hydroxide solution were charged in total, the theoretical yield was 3202.3g, and 2495.0g of the product bromotrifluoroethylene was collected, which was anhydrous liquid, had a chromatographic purity of 97.8%, and a yield of 76.2% (based on 30% sodium hydroxide solution).
[0137] Comparative Example 3-2 Subsystem Y for producing bromotrifluoroethylene was replaced with high purity nitrogen until the oxygen content was below 0.1%. 4000g of 30% sodium hydroxide solution (60mol NaOH, 1.5 equivalents) was added to a 10L glass reactor, and the stirring and reactor jacket heating devices were turned on to control the reactor internal temperature at 60℃. The inlet and outlet valves of 1,2-dibromotrifluoroethane condensation reflux device A were opened to control the jacket temperature at 5℃, and the inlet and outlet valves of bromotrifluoroethylene condensation reflux device B were opened to control the jacket temperature at -15℃. 4800kg (20mol) 1,2-dibromotrifluoroethane was added to the reactor at an addition rate of 1200g / h. After the addition was completed in 4 hours, the reaction was stopped after 1 hour of warming.
[0138] The theoretical yield was 3220 g, and 2636.7 g of the product bromotrifluoroethylene was collected, which was an anhydrous liquid with a chromatographic purity of 95.5% and a yield of 78.2% (based on 1,2-dibromotrifluoroethane).
[0139] Example 4-1 This example provides a preparation of hexafluorobutadiene, specifically including the following steps:
[0140] Preparation of trifluorovinyl zinc bromide solution: Subsystem Z for producing hexafluorobutadiene was replaced with high purity nitrogen until the oxygen content was 0.1% or less. 3000g of N,N-dimethylformamide solution (water content 150ppm), 468g (7.1mol) of 300mesh activated zinc powder, and 300g of N,N-dimethylformamide solution of trifluorovinyl zinc bromide as an initiator were added to the fourth reactor (5L glass reaction vessel), and the temperature was raised to 45°C while stirring, and 886.2g (5.5mol) of bromotrifluoroethylene was continuously added to react, and after the addition was completed, the mixture was kept at 45°C for 1 hour to terminate the reaction. After that, the mixture was left to stand for 3 hours, and the excess zinc powder and the reaction liquid were separated by filtration. The excess zinc powder was used after acid washing, water washing, and vacuum drying treatment. The reaction liquid was transferred to the fifth reactor.
[0141] Preparation of hexafluorobutadiene: The fifth reactor containing the trifluorovinyl zinc bromide solution was cooled to 0°C, and 892.1g (5.5mol) of anhydrous ferric chloride was added to the reactor with a solid feeder under stirring, and the addition rate was controlled to 300g / h, and the internal temperature was maintained in the range of 0-5°C. After the addition was completed, the temperature was raised to 140°C, and all the hexafluorobutadiene was evaporated, condensed, and collected in a low-temperature condenser. The experimental result was that 404.0 g of product was obtained. Gas chromatography analysis revealed that the hexafluorobutadiene content was 97.8%, the theoretical yield was 445.5 g, and the yield was 88.7%.
[0142] Example 4-2 The operation of this example was the same as that of Example 4-1, except that the trifluorovinyl zinc bromide solution used as the initiator was changed to iodine alone, and the amount of iodine used was 42 g.
[0143] The experimental result was that 400.8g of product was obtained. Gas chromatography analysis revealed that the hexafluorobutadiene content was 96.6%, the theoretical yield was 445.5g, and the yield was 86.9%.
[0144] Example 4-3 The procedure of this example was the same as in Example 4-1, except that the solvent N,N-dimethylformamide was replaced with the same amount of tetrahydrofuran. The experimental result was that 383.7g of product was obtained. Gas chromatography analysis showed that the hexafluorobutadiene content was 95.8%, the theoretical yield was 445.5g, and the yield was 82.5%.
[0145] Example 4-3 The procedure of this example was the same as in Example 4-1, except that the coupling agent, ferric chloride, was replaced by copper chloride in an amount of 739.8 g (5.5 mol).
[0146] The experimental result was that 409.6g of product was obtained. Gas chromatography analysis showed that the hexafluorobutadiene content was 98.1%, the theoretical yield was 445.5g, and the yield was 90.2%.
[0147] Example 4-4 The procedure of this example was the same as that of Example 4-1, except that the temperature of the trifluorovinyl zinc bromide solution preparation reaction was changed from the original 45° C. to 60° C.
[0148] The experimental result was that 386.3g of product was obtained. Gas chromatography analysis showed that the hexafluorobutadiene content was 96.3%, the theoretical yield was 445.5g, and the yield was 83.5%.
[0149] Examples 4-5 The operation of this example was the same as that of Example 4-1, except that the temperature of the hexafluorobutadiene preparation reaction was changed from the original (0 to 5° C.) to (5 to 10° C.). The experimental result was that 397.7g of product was obtained. Gas chromatography analysis showed that the hexafluorobutadiene content was 95.0%, the theoretical yield was 445.5g, and the yield was 84.8%.
Claims
1. A method for continuously producing trifluoroethylene, comprising the step of hydrodechlorinating chlorotrifluoroethylene and hydrogen in a first reactor under the action of a supported metal nanocatalyst to obtain a mixture, the mixture containing 0.8% to 2.0% of 1,2-dichlorotrifluoroethane (HCFC-123a) and / or 1-chloro-1,2,2-trifluoroethane (HCFC-133), the supported metal nanocatalyst containing at least one first component selected from ruthenium, palladium, or platinum, at least one second component selected from copper, bismuth, and cerium, and an activated carbon carrier; The supported metal nanocatalyst is prepared by the following steps: A method for the continuous production of trifluoroethylene. A1. Carrier reduction modification: The activated carbon carrier is reduced at 200-800°C for 1.5-3 hours using a reducing agent, and then cooled to room temperature, where the reducing agent is at least one selected from hydrogen, nitrogen, and ammonia; A2. Nanoparticle deposition: the mixture of nanoparticle stabilizer, potassium bromide and potassium chloride is heated to 80-110°C under stirring, and heated under reflux for 1-2h, in which the molar ratio of potassium chloride / potassium bromide in the mixture of potassium bromide and potassium chloride is 1:0.01-1:0.3, then the first component soluble salt and the second component soluble salt are added, and the reaction is continued at 80-110°C for 1.5-2.5h, and then the temperature is lowered to room temperature, and an excess amount of liquid phase reducing agent is dripped in under stirring, and then the activated carbon carrier modified in step A1 is added, and an alkaline solution is continuously dripped in to control the pH value to 6-10.5, and metal nanoparticles are deposited on the surface of the activated carbon carrier; A3. Washing and calcination: Filter, wash with deoxygenated deionized water or ethanol until neutral, dry, and calcinate in an inert atmosphere at 300-400°C for 1.0-4.0h to obtain a catalyst precursor; A4. Reductive activation: The catalyst precursor is placed in a mixed atmosphere of hydrogen and nitrogen, heated to 250-450° C. at a rate of 0.1-2.0° C. / min, and kept at the same temperature for 1-5 hours to obtain the supported metal nanocatalyst.
2. the mixture further comprises 20% to 50% trifluoroethylene, 43% to 77% chlorotrifluoroethylene, and 2% to 5% 1,1,2-trifluoroethane (HFC-143); 2. The method for continuous production of trifluoroethylene according to claim 1.
3. Based on the mass of the catalyst support, the amount of the first component supported is 0.05% to 5.0%, the amount of the second component supported is 0.01% to 3.0%, and the mass ratio of the first component to the second component is 1:(0.1 to 5).
2. The method for continuous production of trifluoroethylene according to claim 1.
4. The supported metal nano catalyst has a particle diameter of 2 to 50 nm, and the proportion of metal particles having a particle diameter of 2 to 10 nm is 90% or more.
2. The method for continuous production of trifluoroethylene according to claim 1.
5. In step A2, the first component soluble salt is at least one selected from the chloride, hydrochloride, or organic salt of the first component, and the second component soluble salt is at least one selected from the chloride, nitrate, sulfate, or organic salt of the second component.
2. The method for continuous production of trifluoroethylene according to claim 1.
6. In step A2, the nanoparticle stabilizer is at least one selected from polyvinylpyrrolidone (PVP), polyacrylate, and hexadecyltrimethylammonium bromide (CTAB), and the molar amount thereof is 4 to 6 times the sum of the molar amounts of the first component and the second component; 2. The method for continuous production of trifluoroethylene according to claim 1.
7. In step A2, the liquid phase reducing agent is L-ascorbic acid, NaBH 4 , citric acid, or ethylene glycol, and the molar amount of the first component used is 2 to 4 times the total molar amount of the first component and the second component; 2. The method for continuous production of trifluoroethylene according to claim 1.
8. In step A2, the alkaline solution is a NaOH or KOH solution, and its mass concentration is 2 to 10 wt%; 2. The method for continuous production of trifluoroethylene according to claim 1.
9. The reaction temperature of chlorotrifluoroethylene and hydrogen is 100-200°C, the reaction pressure is 0-2 MPa, and the raw material volumetric space velocity of hydrogen and chlorotrifluoroethylene is 200-500 h -1 and the molar ratio of hydrogen to chlorotrifluoroethylene is (1.2-2.5):1; 2. The method for continuous production of trifluoroethylene according to claim 1.
10. (1) The method for continuous production of trifluoroethylene according to any one of claims 1 to 9 is adopted, comprising the steps of preparing the mixture containing trifluoroethylene in a first reactor, supplying the mixture to a rectification device for separation, supplying the trifluoroethylene obtained by rectification to a second reactor and continuously reacting it with bromine under light irradiation to obtain 1,2-dibromotrifluoroethane, and returning the chlorotrifluoroethylene obtained by rectification to the first reactor for recycling; (2) continuously adding 1,2-dibromotrifluoroethane and a solid alkali to a third reactor containing 1,2-dibromotrifluoroethane in advance, and obtaining bromotrifluoroethylene by a dehydrobromination reaction; (3) adding bromotrifluoroethylene to a fourth reactor containing zinc powder, an initiator and an organic solvent to react with each other, obtaining trifluorovinyl zinc bromide, filtering the resulting mixture and feeding it to a fifth reactor, adding a coupling agent to carry out a coupling reaction to obtain hexafluorobutadiene; A method for producing hexafluorobutadiene.
11. In a fourth reactor, first, an organic solvent, an initiator and zinc powder are added and stirred, and the temperature is raised to 0 to 100°C, and then bromotrifluoroethylene is added and reacted to obtain a trifluorovinyl zinc bromide solution, and the zinc powder in the trifluorovinyl zinc bromide solution is removed by filtration, and a coupling agent is added and reacted at -20 to 50°C to obtain hexafluorobutadiene. The method for producing hexafluorobutadiene according to claim 10.
12. The organic solvent is at least one selected from N,N-dimethylformamide (DMF), N,N-dimethylacetamide (DMAc), dimethylsulfoxide (DMSO) and tetrahydrofuran (THF), and the water content in the organic solvent is 200 ppm or less. The method for producing hexafluorobutadiene according to claim 10.
13. The initiator is at least one selected from bromomethane, 1,2-dibromoethane, iodine alone, chlorotrimethylsilane, and a trifluorovinyl zinc bromide solution; The method for producing hexafluorobutadiene according to claim 10.
14. The coupling agent is at least one selected from copper iodide, copper bromide, copper chloride, copper sulfate, copper acetate, ferric chloride, and ferric bromide. The method for producing hexafluorobutadiene according to claim 10.
15. In the step (1), the rectification apparatus includes at least two rectification columns, and trifluoroethylene is collected from the top of the first rectification column and chlorotrifluoroethylene is collected from the reflux pipe of the last rectification column. The method for producing hexafluorobutadiene according to claim 10.
16. In the step (1), the bromine is bromine vapor, the molar ratio of trifluoroethylene to bromine vapor is 1:(0.3-3), the reaction temperature of trifluoroethylene and bromine vapor is 0°C-150°C, and the pressure is 0-1 MPa. The method for producing hexafluorobutadiene according to claim 10.
17. In the step (2), the solid alkali is at least one selected from lithium hydroxide, sodium hydroxide, potassium hydroxide, calcium hydroxide, sodium carbonate, and potassium carbonate. The method for producing hexafluorobutadiene according to claim 10.
18. In the step (2), the molar ratio of the supply rate of the solid alkali to 1,2-dibromotrifluoroethane is 1:(0.8-1.2), and the temperature of the dehydrobromination reaction is 30-80°C. The method for producing hexafluorobutadiene according to claim 10.
19. In the step (2), the volume of 1,2-dibromotrifluoroethane previously charged is 1 / 4 to 1 / 2 of the volume of the third reactor. The method for producing hexafluorobutadiene according to claim 10.
20. In the step (2), the method for continuously producing bromotrifluoroethylene comprises: B1. Preliminarily adding 1,2-dibromotrifluoroethane (as a solvent) into the third reactor, turning on the external circulation pump, and allowing the 1,2-dibromotrifluoroethane to flow out of the third reactor and return to the third reactor via a filtration device; B2. Raising the temperature to a reaction temperature, continuously adding 1,2-dibromotrifluoroethane and solid alkali, collecting and condensing bromotrifluoroethylene gas to obtain bromotrifluoroethylene liquid, and discharging the by-products from the reaction system through a filtration device to realize a continuous reaction. The method for producing hexafluorobutadiene according to claim 10.
Citation Information
Patent Citations
Catalyst for hydrodechlorination catalytic synthesis of chlorotrifluoroethylene or trifluoroethylene and preparation method thereof
CN114308085A
Hydrodechlorination catalyst as well as preparation method and application thereof
CN114713244A
JP1971002324B1
Method for the synthesis of trifluoroethylene
JP2013534529A