Buffer member, power storage module, and method for manufacturing buffer member
The introduction of a buffer member with offset softened layers in power storage modules addresses the challenge of increased expansion in high-capacity devices, enhancing reliability by distributing loads and maintaining device positioning without requiring stronger bind bars.
Patent Information
- Application Number
- JP2021548898
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2019-09-27
- Filing Date
- 2020-09-18
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2040-09-18
AI Technical Summary
Conventional power storage modules face challenges in maintaining reliability as higher capacity power storage devices increase expansion, leading to excessive loads on bind bars, which can result in damage and decreased positioning accuracy.
Incorporation of a buffer member with layered structures featuring offset softened portions in the form of through holes or recesses, allowing for differential deformation to absorb and distribute loads more effectively, reducing stress on bind bars while maintaining device positioning.
The buffer member enhances the reliability of power storage modules by absorbing increased expansion, preventing bind bar damage, and ensuring precise positioning of power storage devices, thereby reducing the need for stronger and more costly bind bars.
Smart Images

Figure 0007595281000001 
Figure 0007595281000002 
Figure 0007595281000003
Abstract
Description
[Technical field]
[0001] The present disclosure relates to a cushioning member, an electricity storage module, and a method for manufacturing the cushioning member. [Background technology]
[0002] For example, as a power source that requires a high output voltage for vehicles, etc., a power storage module in which a plurality of power storage devices (e.g., batteries) are connected in series is known. In general, a power storage module includes a plurality of power storage devices, a plurality of separators disposed between adjacent power storage devices, a pair of end plates disposed at both ends in the arrangement direction of the power storage devices, and a bind bar that is stretched between the pair of end plates and binds the plurality of power storage devices in the arrangement direction (see, for example, Patent Document 1). [Prior art documents] [Patent documents]
[0003] [Patent Document 1] JP 2015-99648 A Summary of the Invention [Problem to be solved by the invention]
[0004] In general, energy storage devices expand due to various factors. In conventional energy storage modules, this expansion is suppressed by end plates and bind bars. In addition, in energy storage modules, the energy storage devices are fixed in place by the binding force of the bind bars to maintain electrical connections between the energy storage devices and to prevent the energy storage devices from popping out due to external impacts, etc.
[0005] In recent years, there has been a demand for even higher capacity energy storage modules, and to meet this demand, energy storage devices are being made higher in capacity. As the capacity of an energy storage device increases, the amount of expansion of the energy storage device increases, and the load on the bind bar also increases. Therefore, measures are required to prevent damage to the bind bar and maintain the reliability of the energy storage module. By weakening the binding force of the bind bar, the load on the bind bar can be reduced, and therefore damage to the bind bar can be suppressed. However, weakening the binding force of the bind bar may result in poor positioning of the energy storage device, which may reduce the reliability of the energy storage module.
[0006] The present disclosure has been made in light of these circumstances, and has a purpose to provide a technique for improving the reliability of an energy storage module. [Means for solving the problem]
[0007] One aspect of the present disclosure is an energy storage module. The energy storage module includes at least one energy storage device and a buffer member arranged in a first direction together with the energy storage device and receiving a load from the energy storage device in the first direction. The buffer member has at least a first layer portion and a second layer portion arranged in the first direction. The first layer portion has a first softened portion configured with a through hole penetrating the first layer portion in the first direction or a recessed portion recessed in the first direction. The second layer portion has a second softened portion configured with a through hole penetrating the first layer portion in the first direction or a recessed portion recessed in the first direction. The first softened portion and the second softened portion are at least partially misaligned when viewed from the first direction.
[0008] Another aspect of the present disclosure is a buffer member arranged in a first direction together with at least one power storage device and receiving a load from the power storage device in the first direction. The buffer member includes at least a first layer and a second layer arranged in the first direction. The first layer has a first softened portion configured with a through hole penetrating the first layer in the first direction or a recess recessed in the first direction. The second layer has a second softened portion configured with a through hole penetrating the first layer in the first direction or a recess recessed in the first direction. The first softened portion and the second softened portion are at least partially misaligned when viewed from the first direction.
[0009] Another aspect of the present disclosure is a method for manufacturing a buffer member arranged in a first direction together with at least one power storage device and receiving a load in the first direction from the power storage device. This manufacturing method includes stacking a first sheet having a first softened portion configured with a through hole penetrating the first sheet in the thickness direction or a recessed portion recessed in the thickness direction, and a second sheet having a second softened portion configured with a through hole penetrating the first sheet in the thickness direction or a recessed portion recessed in the thickness direction, such that at least a portion of the first softened portion and the second softened portion are misaligned.
[0010] Any combination of the above components and any conversion of the expression of the present disclosure between a method, an apparatus, a system, etc. are also valid as aspects of the present disclosure. Effect of the Invention
[0011] According to the present disclosure, the reliability of the energy storage module can be improved. [Brief description of the drawings]
[0012] [Figure 1] 1 is a perspective view of an electricity storage module according to an embodiment; [Diagram 2] FIG. 2 is an exploded perspective view of the electricity storage module. [Diagram 3] 5A to 5C are cross-sectional views each showing a schematic state in which each power storage device expands. [Figure 4] FIG. 2 is a front view of the cushioning member according to the first embodiment. [Diagram 5] Fig. 5(A) is a front view of a first layer of the cushioning material, and Fig. 5(B) is a front view of a second layer of the cushioning material. [Figure 6] 6(A) to 6(D) are cross-sectional views of a portion of the cushioning member. [Figure 7] Fig. 7(A) is a perspective view of a cushioning member according to Modification 1. Fig. 7(B) is a front view of the cushioning member. [Figure 8] Fig. 8(A) is a perspective view of a cushioning member according to Modification 2. Fig. 8(B) is a front view of the cushioning member. [Figure 9]Fig. 9(A) is a perspective view of a cushioning member according to Modification 5. Fig. 9(B) is a cross-sectional perspective view taken along line AA in Fig. 9(A). DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0013] The present disclosure will be described below with reference to the drawings based on preferred embodiments. The embodiments are illustrative and do not limit the present disclosure, and all features and combinations thereof described in the embodiments are not necessarily essential to the present disclosure. The same or equivalent components, members, and processes shown in each drawing are given the same reference numerals, and duplicated descriptions are omitted as appropriate. In addition, the scale and shape of each part shown in each drawing are set for convenience to facilitate explanation, and are not to be interpreted as being limiting unless otherwise specified. In addition, when terms such as "first" and "second" are used in this specification or claims, unless otherwise specified, these terms do not represent any order or importance, but are intended to distinguish one configuration from another. In addition, some of the members that are not important in explaining the embodiment in each drawing are omitted.
[0014] Fig. 1 is a perspective view of an electricity storage module according to an embodiment. Fig. 2 is an exploded perspective view of the electricity storage module. In Fig. 2, the illustration of a cushioning member 40 is simplified. The electricity storage module 1 includes, as an example, a battery stack 2, a pair of restraining members 6, and a cooling plate 8. The battery stack 2 has a plurality of electricity storage devices 10, a plurality of separators 12, a plurality of cushioning members 40, and a pair of end plates 4.
[0015] Each of the power storage devices 10 is, for example, a rechargeable secondary battery such as a lithium ion battery, a nickel-hydrogen battery, or a nickel-cadmium battery, or a capacitor such as an electric double layer capacitor. The power storage device 10 of this embodiment is a so-called prismatic battery, and has a housing 13 in the shape of a flat rectangular parallelepiped. The housing 13 is composed of an outer can 14 and a sealing plate 16. The outer can 14 has a substantially rectangular opening on one side, and an electrode assembly 38 (see FIG. 3) including a positive electrode 38a, a negative electrode 38b, and a porous separator 38d, an electrolyte, and the like are accommodated in the outer can 14 through this opening. The outer can 14 is covered with an insulating film (not shown) such as a shrink tube. By covering the surface of the outer can 14 with an insulating film, it is possible to suppress short circuits between adjacent power storage devices 10 and between the power storage device 10 and each of the end plate 4, the restraining member 6, and the cooling plate 8. A sealing plate 16 is provided at the opening of the outer can 14 to close the opening and seal the outer can 14. The sealing plate 16 constitutes a first surface 13 a of the housing 13 .
[0016] The electrode body 38 has a structure in which a plurality of sheet-shaped positive electrodes 38a and a plurality of sheet-shaped negative electrodes 38b are alternately stacked with porous separators 38d interposed therebetween (see FIG. 3). The positive electrodes 38a and the negative electrodes 38b are aligned in the first direction X. Therefore, the electrodes located at both ends in the stacking direction face the long side surface of the case 13, which will be described later. The electrode body 38 may be a flat-wound electrode body in which a strip-shaped positive electrode and a strip-shaped negative electrode are wound with a porous separator interposed therebetween, and which has a flat portion where the positive electrode and the negative electrode spread out flatly, and a bent portion where the positive electrode and the negative electrode are bent. In this case, the electrode body 38 is arranged so that the flat portion spreads in a direction intersecting (for example, perpendicular to) the first direction X. In other words, the electrode body 38 is arranged so that the thickness direction of the flat portion is parallel to the first direction X.
[0017] An output terminal 18 electrically connected to the positive electrode 38a of the electrode body 38 is provided on the sealing plate 16, i.e., the first surface 13a of the housing 13, near one end in the longitudinal direction, and an output terminal 18 electrically connected to the negative electrode 38b of the electrode body 38 is provided near the other end. Hereinafter, the output terminal 18 connected to the positive electrode 38a will be referred to as the positive electrode terminal 18a, and the output terminal 18 connected to the negative electrode 38b will be referred to as the negative electrode terminal 18b. In addition, when it is not necessary to distinguish the polarity of the pair of output terminals 18, the positive electrode terminal 18a and the negative electrode terminal 18b will be collectively referred to as the output terminal 18. The outer can 14 and the sealing plate 16 are conductors, and are made of metals such as aluminum, iron, and stainless steel. The sealing plate 16 and the outer can 14 are joined together, for example, by laser, friction stir welding, brazing, or the like. Alternatively, the outer can 14 and the sealing plate 16 are made of insulating resin.
[0018] The exterior can 14 has a bottom surface facing the sealing plate 16. The exterior can 14 also has four side surfaces connecting the opening and the bottom surface. Two of the four side surfaces are a pair of long side surfaces connected to two opposing long sides of the opening and the bottom surface. Each long side surface is the surface with the largest area among the surfaces of the exterior can 14, i.e., the main surface. Each long side surface is a side surface that extends in a direction intersecting (for example, perpendicular to) the first direction X. The remaining two side surfaces excluding the two long side surfaces are a pair of short side surfaces connected to two opposing short sides of the opening and bottom surface of the exterior can 14. The bottom surface, long side surfaces, and short side surfaces of the exterior can 14 correspond to the bottom surface, long side surfaces, and short side surfaces of the housing 13, respectively.
[0019] In the description of the present embodiment, for convenience, the first surface 13a of the housing 13 is the upper surface of the energy storage device 10. The bottom surface of the housing 13 is the bottom surface of the energy storage device 10, the long side surface of the housing 13 is the long side surface of the energy storage device 10, and the short side surface of the housing 13 is the short side surface of the energy storage device 10. In the energy storage module 1, the surface on the upper side of the energy storage device 10 is the upper surface of the energy storage module 1, the surface on the bottom side of the energy storage device 10 is the bottom surface of the energy storage module 1, and the surface on the short side of the energy storage device 10 is the side surface of the energy storage module 1. In addition, the upper surface side of the energy storage module 1 is vertically upward, and the bottom surface side of the energy storage module 1 is vertically downward. These directions and positions are defined for convenience. Therefore, for example, a portion defined as the upper surface in this disclosure does not necessarily mean that it is located above a portion defined as the bottom surface. Therefore, the sealing plate 16 is not necessarily located above the bottom surface of the exterior can 14.
[0020] A safety valve (not shown) is provided on the sealing plate 16 between the pair of output terminals 18. The safety valve is configured to open when the internal pressure of the housing 13 rises to or above a predetermined value, thereby allowing the gas inside the housing 13 to be released. The safety valve is configured, for example, by a thin-walled portion that is provided in a portion of the sealing plate 16 and is thinner than other portions, and a linear groove formed in the surface of the thin-walled portion. In this configuration, when the internal pressure of the housing 13 rises, the thin-walled portion tears starting from the groove, opening the safety valve.
[0021] The multiple energy storage devices 10 are arranged side by side at a predetermined interval such that the long sides of adjacent energy storage devices 10 face each other. In this embodiment, the direction in which the multiple energy storage devices 10 are arranged is defined as a first direction X. Furthermore, the output terminals 18 of each energy storage device 10 are arranged to face the same direction. In this embodiment, the output terminals 18 of each energy storage device 10 are arranged to face vertically upward for convenience. However, the output terminals 18 of each energy storage device 10 may be arranged to face different directions.
[0022] Two adjacent energy storage devices 10 are arranged (stacked) such that the positive electrode terminal 18a of one energy storage device 10 and the negative electrode terminal 18b of the other energy storage device 10 are adjacent to each other. The positive electrode terminal 18a and the negative electrode terminal 18b are connected in series via a bus bar (not shown). Note that the output terminals 18 of the same polarity in a plurality of adjacent energy storage devices 10 may be connected in parallel with each other via a bus bar to form an energy storage device block, and the energy storage device blocks may be connected in series to each other.
[0023] The separator 12 is also called an insulating spacer, and is disposed between two adjacent power storage devices 10 to electrically insulate the two power storage devices 10. The separator 12 is made of, for example, an insulating resin. Examples of the resin that constitutes the separator 12 include thermoplastic resins such as polypropylene (PP), polybutylene terephthalate (PBT), polycarbonate (PC), and Noryl (registered trademark) resin (modified PPE). A plurality of power storage devices 10 and a plurality of separators 12 are stacked alternately. In addition, the separator 12 is also disposed between the power storage device 10 and the end plate 4.
[0024] The separator 12 has a flat portion 20 and a wall portion 22. The flat portion 20 is interposed between the opposing long side surfaces of two adjacent energy storage devices 10. This ensures that the outer casings 14 of the adjacent energy storage devices 10 are insulated from each other more reliably.
[0025] The wall portion 22 extends from the outer edge of the flat portion 20 in a first direction X in which the power storage devices 10 are arranged, and covers a part of the top surface, the side surface, and a part of the bottom surface of the power storage device 10. This ensures a creepage distance between adjacent power storage devices 10 or between the power storage device 10 and the end plate 4. Also, the housing 13 of the power storage device 10 is more reliably insulated from the restraining member 6. Also, the position of the power storage device 10 can be restricted or fixed in a second direction Y in which the output terminals 18 are arranged, and in a third direction Z in which the top surface and the bottom surface of the power storage device 10 are arranged. The first direction X, the second direction Y, and the third direction Z are perpendicular to each other.
[0026] The wall portion 22 has a cutout 24 to expose the bottom surface of the power storage device 10. Providing the cutout 24 makes it possible to prevent the separator 12 from impeding the thermal connection between the power storage device 10 and the cooling plate 8. In addition, the separator 12 has upwardly facing biasing receiving portions 26 at both ends in the second direction Y.
[0027] The buffer members 40 are arranged in the first direction X together with the multiple power storage devices 10. The buffer members 40 are sheet-shaped and are interposed, for example, between the long side surface of each power storage device 10 and the flat surface portion 20 of each separator 12. The number of buffer members 40 arranged between two adjacent power storage devices 10 may be one or more. The buffer members 40 may be fixed to the surface of the flat surface portion 20 by adhesion or the like. Alternatively, a recess may be provided in the flat surface portion 20, and the buffer members 40 may be fitted into the recess. The structure and function of the buffer members 40 will be described in detail later.
[0028] The multiple electricity storage devices 10, multiple separators 12, and multiple buffer members 40 arranged in parallel are sandwiched in the first direction X by a pair of end plates 4. Separators 12 are arranged between the pair of end plates 4 and the electricity storage devices 10 arranged at both ends in the first direction X. This more reliably insulates the outer casing 14 of the electricity storage device 10 from the end plate 4. The end plate 4 is made of, for example, a metal plate or a resin plate. The end plate 4 is provided with a screw hole 4a that penetrates the end plate 4 in the first direction X and into which a screw 28 is screwed.
[0029] The pair of restraining members 6, also called bind bars, are elongated members with the first direction X as their longitudinal direction. The pair of restraining members 6 are arranged to face each other in the second direction Y. The battery stack 2 is interposed between the pair of restraining members 6. Each of the restraining members 6 includes a main body portion 30, a support portion 32, multiple biasing portions 34, and a pair of fixing portions 36.
[0030] The main body 30 is a rectangular portion extending in the first direction X. The main body 30 extends parallel to the side surfaces of each power storage device 10. The support portion 32 extends in the first direction X and protrudes from the lower end of the main body 30 in the second direction Y. The support portion 32 is a plate-like body continuing in the first direction X, and supports the battery stack 2.
[0031] The multiple urging portions 34 are connected to the upper end of the main body portion 30 and protrude in the second direction Y. The support portion 32 and each urging portion 34 face each other in the third direction Z. The multiple urging portions 34 are arranged in the first direction X at predetermined intervals. Each urging portion 34 is disposed corresponding to each power storage device 10. Each urging portion 34 is in the shape of a leaf spring and urges each power storage device 10 toward the support portion 32.
[0032] The pair of fixing portions 36 are plate-like bodies that protrude in the second direction Y from both ends of the main body 30 in the first direction X. The pair of fixing portions 36 face each other in the first direction X. Each fixing portion 36 is provided with a through hole 36a through which the screw 28 is inserted. The pair of fixing portions 36 fix the restraining member 6 to the battery stack 2.
[0033] The cooling plate 8 is a mechanism for cooling the multiple power storage devices 10. The cooling plate 8 is made of a thermally conductive material such as metal. The battery stack 2 is placed on a main surface of the cooling plate 8 while being restrained by a pair of restraining members 6, and is fixed to the cooling plate 8 by inserting fastening members such as screws (not shown) into through holes 32a of the supports 32 and through holes 8a of the cooling plate 8. Each power storage device 10 is cooled by heat exchange with the cooling plate 8. The cooling plate 8 may be provided with refrigerant pipes (not shown) through which a refrigerant flows.
[0034] The energy storage module 1 is assembled, for example, by the following method. That is, the energy storage devices 10, the buffer members 40, and the separators 12 are repeatedly arranged in this order and sandwiched between a pair of end plates 4 in the first direction X to form a battery stack 2. The battery stack 2 is sandwiched between a pair of restraining members 6 in the second direction Y. Each restraining member 6 is aligned so that the through hole 36a overlaps with the screw hole 4a of the end plate 4. In this state, a screw 28 is inserted into the through hole 36a and screwed into the screw hole 4a. In this way, the pair of restraining members 6 engage with the pair of end plates 4 to restrain the multiple energy storage devices 10. The battery stack 2 is fastened by the restraining members 6 with a predetermined pressure applied in the first direction X.
[0035] Each energy storage device 10 is fastened in the first direction X by the restraining member 6, and thereby positioned in the first direction X. Furthermore, the bottom surface of each energy storage device 10 is supported by the support portion 32. The wall portion 22 of the separator 12 is interposed between the bottom surface of each energy storage device 10 and the support portion 32. Furthermore, the urging portion 34 abuts against the urging receiving portion 26 corresponding to each energy storage device 10. Each urging portion 34 urges each energy storage device 10 toward the support portion 32 via the urging receiving portion 26. That is, each energy storage device 10 is sandwiched in the third direction Z by the support portion 32 and the multiple urging portions 34. As a result, the position of each energy storage device 10 in the third direction Z is determined.
[0036] As an example, after these positioning steps are completed, a bus bar is attached to the output terminal 18 of each power storage device 10, and the output terminals 18 of the multiple power storage devices 10 are electrically connected to each other. For example, the bus bar is fixed to the output terminal 18 by welding. The top surface of the battery stack 2 is then covered with a cover member (not shown). The cover member prevents condensed water, dust, and the like from coming into contact with the output terminals 18, bus bar, safety valve, and the like of the power storage devices 10. The cover member is made of, for example, insulating resin, and can be fixed to the top surface of the battery stack 2 by a well-known fixing structure (not shown) including screws or a well-known locking mechanism.
[0037] The battery stack 2 with the restraining members 6 and cover members attached is placed on the cooling plate 8, and fastening members are inserted through the through holes 8a and through holes 32a to secure the battery stack 2 to the cooling plate 8. Through the above steps, the energy storage module 1 is obtained. Note that the battery stack 2 may be placed on the cooling plate 8, and then the battery stack 2 and cooling plate 8 may be secured together with the restraining members 6 to produce the energy storage module 1. In this case, the cooling plate 8 is placed inside the pair of restraining members 6.
[0038] FIG. 3 is a cross-sectional view that shows a schematic state of the expansion of each energy storage device 10. In FIG. 3, the number of energy storage devices 10 is thinned out. Also, the internal structure of the energy storage device 10 and the separator 12 are simplified, and the cushioning member 40 is not shown. As shown in FIG. 3, an electrode body 38 is housed inside each energy storage device 10. In the energy storage device 10, the exterior can 14 repeatedly expands and contracts with charging and discharging. The expansion of the exterior can 14 is mainly caused by the expansion of the electrode body 38. When the exterior can 14 of each energy storage device 10 expands, a load G1 toward the outside in the first direction X is generated in the battery stack 2. Meanwhile, a load G2 corresponding to the load G1 is applied to the battery stack 2 by the restraining member 6. This suppresses the expansion of each energy storage device 10.
[0039] In a structure in which the restraining members 6 restrain a plurality of energy storage devices 10, expansion of the energy storage devices 10 places a load on the restraining members 6. When the amount of expansion increases due to an increase in the capacity of the energy storage devices 10, the load on the restraining members 6 also increases. If the load on the restraining members 6 becomes excessive, the restraining members 6 may be damaged. If an attempt is made to increase the strength of the restraining members 6 to prevent damage, this may lead to an increase in the size and cost of the restraining members 6 and in turn the energy storage module 1. Furthermore, if the restraining members 6 are used to suppress the expansion of the energy storage devices 10, the electrode body 38 (particularly the porous separator 38d) may be excessively pressed, which may result in a decrease in performance and a shortened lifespan of the energy storage devices 10.
[0040] If the restraint of the energy storage devices 10 by the restraining members 6 is loosened, the load on the restraining members 6 can be reduced. However, in order to position the energy storage devices 10 within the energy storage module 1, a certain amount of load needs to be applied to each energy storage device 10. For this reason, the restraint of the energy storage devices 10 cannot be simply loosened.
[0041] In contrast, the electricity storage module 1 according to the present embodiment includes a buffer member 40. FIG. 4 is a front view of the buffer member 40 according to the first embodiment. FIG. 5(A) is a front view of a first layer portion included in the buffer member 40. FIG. 5(B) is a front view of a second layer portion included in the buffer member 40. FIGS. 6(A) to 6(D) are cross-sectional views of a portion of the buffer member 40. FIG. 4 illustrates the buffer member 40 arranged in the first direction X together with the electricity storage device 10. Also, the separator 12 is not illustrated. Also, the first layer portion 42 is arranged on the rear side of the paper, and the second layer portion 44 is arranged on the front side of the paper.
[0042] The cushioning member 40 is arranged in the first direction X together with the power storage device 10, and is a member that receives a load from the power storage device 10 in the first direction X. The cushioning member 40 is in the form of a sheet extending in the second direction Y and the third direction Z. The cushioning member 40 has at least a first layer 42 and a second layer 44 arranged in the first direction X. The cushioning member 40 of the present embodiment is composed of only the first layer 42 and the second layer 44. The number of layers of the cushioning member 40 is not limited to two layers, and may be three or more layers. The cushioning member 40 may also include a layer that is composed of the same material as the first layer 42 and the second layer 44 and has no through-holes or recesses. The first layer 42 and the second layer 44 are both in the form of a sheet. The first layer 42 is composed of a first sheet 42a, and the second layer 44 is composed of a second sheet 44a.
[0043] The first layer 42 has a plurality of first softened parts 46 and a first remaining part 47. Similarly, the second layer 44 has a plurality of second softened parts 48 and a second remaining part 49. The first softened part 46 and the second softened part 48 may each be one. As shown in FIG. 6(A) to FIG. 6(C), the first softened part 46 of the present embodiment is configured with a through hole penetrating the first sheet 42a in the first direction X. Similarly, the second softened part 48 of the present embodiment is configured with a through hole penetrating the second sheet 44a in the first direction X. As shown in FIG. 6(D), the first softened part 46 and the second softened part 48 may be configured with a recess recessed in the first direction X, or a through hole and a recess may be combined. The softened part may be called a hollow part from its shape. The first remaining part 47 is a solid part excluding the plurality of first softened parts 46. The second remaining portion 49 is a solid portion excluding the multiple second softened portions 48 .
[0044] As shown in Fig. 4 to Fig. 5(B), each of the first softening portions 46 and each of the second softening portions 48 is circular when viewed from the first direction X. Furthermore, each of the first softening portions 46 and each of the second softening portions 48 has a uniform size. Note that the shape and size of the first softening portions 46 and the second softening portions 48 may be varied depending on the location. For example, each of the first softening portions 46 and the second softening portions 48 may be a linear groove or a slit hole.
[0045] In the first layer 42, the portion where the first softened portion 46 is arranged is more easily deformed than the portion where the first softened portion 46 is not arranged, that is, the first remaining portion 47. Similarly, in the second layer 44, the portion where the second softened portion 48 is arranged is more easily deformed than the portion where the second softened portion 48 is not arranged, that is, the second remaining portion 49. In this case, the deformation is a compressive deformation in the first direction X. In each layer, a portion adjacent to the softened portion and abutting against the electricity storage device 10 can be displaced toward the softened portion when compressed by a force from the electricity storage device 10. In other words, a portion of the portion adjacent to the softened portion can escape into the softened portion. Therefore, by providing the first softened portion 46 and the second softened portion 48, the peripheral portion of each softened portion can be easily deformed. In other words, even if the entire layer is made of the same material, the apparent elastic modulus (compressive elastic modulus) in the peripheral region of each softened portion can be reduced.
[0046] The density of the first layer 42 is smaller on the central side than on the outer edge side of the first layer 42 when viewed from the first direction X. In other words, the ratio of the area of the first softened portion 46 to the unit area of the first layer 42 is larger on the central side than on the outer edge side of the first layer 42 when viewed from the first direction X. Similarly, the density of the second layer 44 is smaller on the central side than on the outer edge side of the second layer 44 when viewed from the first direction X. In other words, the ratio of the area of the second softened portion 48 to the unit area of the second layer 44 is larger on the central side than on the outer edge side of the second layer 44 when viewed from the first direction X. In this specification, the "outer edge side" and "center side" are defined as a location closer to the center of the target member as the "center side" and a location farther from the center of the target member as the "outer edge side" when comparing two locations in the target member. The center of the target member is, for example, the geometric center of the outer diameter of the target member when viewed from the first direction X.
[0047] In other words, the first softened portions 46 are provided more in number closer to the center of the first layer 42, and the second softened portions 48 are provided more in number closer to the center of the second layer 44. Therefore, the first layer 42 and the second layer 44 are more likely to deform at the center and less likely to deform at the outer edge. The center of the buffer member 40 is, for example, the geometric center of the outer diameter of the buffer member 40 as viewed from the first direction X. The outer edge of the buffer member 40 is, for example, a region including the end of the buffer member 40 in the second direction Y and the end of the buffer member 40 in the third direction Z.
[0048] As described above, the expansion of the electric storage device 10 is mainly caused by the expansion of the electrode body 38. In addition, the electrode body 38 expands more toward the center 38C. Therefore, when the electric storage device 10 expands, the portion closer to the center 13C of the long side surface of the housing 13 or the portion closer to the center 38C of the electrode body 38 is displaced more in the first direction X, and the portion closer to the outer edge of the long side surface of the housing 13 or the portion closer to the outer edge of the electrode body 38 is displaced less. In contrast, the outer edge side of the buffer member 40 is relatively less likely to deform, and the central side is relatively more likely to deform. For this reason, it is possible to easily arrange the buffer member 40 with respect to the electric storage device 10 so that a large load caused by a large displacement of the electric storage device 10 is received by a portion that is easily deformed, and a small load caused by a small displacement of the electric storage device 10 is received by a portion that is less likely to deform.
[0049] The first layer 42 and the second layer 44 are laminated in the first direction X to obtain the cushioning member 40. The first layer 42 and the second layer 44 are laminated such that their outer edges coincide with each other when viewed from the first direction X. By laminating the first layer 42 and the second layer 44, the cushioning member 40 is formed with a portion where at least one of the first softening portion 46 and the second softening portion 48 is arranged, and a portion where neither the first softening portion 46 nor the second softening portion 48 is arranged, i.e., a laminated portion 45 where the first remaining portion 47 and the second remaining portion 49 overlap.
[0050] As a method for positioning the first layer 42 and the second layer 44, a first softened portion 46 and a second softened portion 48 that overlap each other may be provided near the outer edges of the first layer 42 and the second layer 44, and the first layer 42 and the second layer 44 may be positioned by fitting a protrusion or a separate positioning member provided on the separator 12 into the pair of softened portions. Furthermore, the first layer 42 and the second layer 44 may be fixed to each other only by fastening in the first direction X by the restraining member 6, or may be fixed to each other by a known fixing method such as adhesion.
[0051] In this state, the first softened portion 46 and the second softened portion 48 are arranged in the first layer 42 and the second layer 44 so that they are at least partially misaligned when viewed from the first direction X. "At least partially misaligned when viewed from the first direction X" means that at least a part of the opening edge of one softened portion does not overlap with the opening edge of the other softened portion when viewed from the first direction X. Therefore, it also includes the case where the entire circumference of the opening edge of one softened portion is located inside or outside the opening edge of the other softened portion when viewed from the first direction X.
[0052] For example, as shown in FIG. 6(A), some of the first softening portions 46 are disposed so as to be entirely displaced from the second softening portions 48 when viewed from the first direction X. Also, as shown in FIG. 6(B) and FIG. 6(C), other parts of the first softening portions 46 are disposed so as to be partially displaced from the second softening portions 48 when viewed from the first direction X. Similarly, as shown in FIG. 6(A), some of the second softening portions 48 are disposed so as to be entirely displaced from the first softening portions 46 when viewed from the first direction X. Also, as shown in FIG. 6(B) and FIG. 6(C), other parts of the second softening portions 48 are disposed so as to be partially displaced from the first softening portions 46 when viewed from the first direction X.
[0053] Hereinafter, the first softened portion 46 that is entirely misaligned with respect to the second softened portion 48 as viewed from the first direction X is referred to as a first separated portion 46a, and the first softened portion 46 that is partially misaligned with respect to the second softened portion 48 as viewed from the first direction X is referred to as a first overlapping portion 46b. The first layer portion 42 of this embodiment has a plurality of first separated portions 46a and a plurality of first overlapping portions 46b. The second softened portion 48 that is entirely misaligned with respect to the first softened portion 46 as viewed from the first direction X is referred to as a second separated portion 48a, and the second softened portion 48 that is partially misaligned with respect to the first softened portion 46 as viewed from the first direction X is referred to as a second overlapping portion 48b. The second layer portion 44 of this embodiment has a plurality of second separated portions 48a and a plurality of second overlapping portions 48b.
[0054] That is, the first separated portion 46a does not overlap any of the second softened portions 48 when viewed from the first direction X, and the opening of the first separated portion 46a on the second layer side is blocked by the second remaining portion 49. The first overlapping portion 46b partially overlaps any of the second softened portions 48 when viewed from the first direction X. Similarly, the second separated portion 48a does not overlap any of the first softened portions 46 when viewed from the first direction X, and the opening of the second separated portion 48a on the first layer side is blocked by the first remaining portion 47. The second overlapping portion 48b partially overlaps any of the first softened portions 46 when viewed from the first direction X.
[0055] The first overlapping portion 46b and the second overlapping portion 48b include those having a relatively large amount of deviation, i.e., the overlapping portion between the first overlapping portion 46b and the second overlapping portion 48b is small, as shown in Fig. 6(B), and those having a relatively small amount of deviation, i.e., the overlapping portion between the first overlapping portion 46b and the second overlapping portion 48b is large, as shown in Fig. 6(C). Note that the first softened portion 46 that entirely overlaps with the second softened portion 48 may be included, or the second softened portion 48 that entirely overlaps with the first softened portion 46 may be included.
[0056] In the cushioning member 40, the portion where at least one of the first softening portion 46 and the second softening portion 48 is disposed is more easily deformed than the laminated portion 45. Also, the greater the overlap between the first overlapping portion 46b and the second overlapping portion 48b, the more easily the cushioning member 40 is deformed. That is, by providing the softening portion, the portion adjacent to the softening portion can be easily displaced. And, the greater the overlap between the first overlapping portion 46b and the second overlapping portion 48b, the greater the amount of the portion adjacent to the softening portion included per unit area. In other words, the greater the overlap, the smaller the area of the laminated portion 45 located around the first overlapping portion 46b and the second overlapping portion 48b tends to be. Since the laminated portion 45 is solid, it is less likely to deform than the portion where the first softening portion 46 and the second softening portion 48 are disposed in the cushioning member 40. Therefore, the greater the overlap between the first softening portion 46 and the second softening portion 48, the more easily the cushioning member 40 is deformed in that portion.
[0057] Therefore, as shown in FIG. 6(A), the area of the cushioning member 40 where the first overlapping portion 46b or the second overlapping portion 48b is arranged is more likely to deform than the area where the first separated portion 46a or the second separated portion 48a is arranged, as shown in FIG. 6(B) or FIG. 6(C).
[0058] Therefore, by providing the first separated portion 46a, the second separated portion 48a, the first overlapping portion 46b, and the second overlapping portion 48b in the cushioning member 40, it is possible to finely adjust the ease of deformation of the cushioning member 40 depending on the location. In other words, by arranging the first separated portion 46a, the second separated portion 48a, the first overlapping portion 46b, and the second overlapping portion 48b, it is possible to easily adjust the shape, size, position, and number of the laminated portions 45 arranged around these softened portions.
[0059] Furthermore, in this embodiment, at least one of the multiple first overlapping portions 46b is disposed closer to the center of the cushioning member 40 than the multiple first separated portions 46a when viewed from the first direction X. Similarly, at least one of the multiple second overlapping portions 48b is disposed closer to the center of the cushioning member 40 than the multiple second separated portions 48a when viewed from the first direction X. This makes it easier for the center side of the cushioning member 40 to deform relative to the outer edge side.
[0060] In the present embodiment, at least one of the multiple first overlapping portions 46b is disposed closer to the center 13C of the long side surface of the housing 13 as viewed from the first direction X than the multiple first separated portions 46a. This makes it easier to deform the portion of the cushioning member 40 that overlaps with the center 13C of the housing 13 compared to the portion that overlaps with the outer edge portion of the housing 13. The center 13C of the long side surface of the housing 13 is, for example, the geometric center of the outer shape of the housing 13 as viewed from the first direction X. The outer edge portion of the long side surface of the housing 13 is, for example, a region that includes the end portion of the long side surface in the second direction Y and the end portion in the third direction Z.
[0061] Similarly, at least one of the multiple second overlapping portions 48b is disposed closer to the center 13C of the long side surface of the housing 13 than the multiple second separated portions 48a are when viewed from the first direction X. This makes it possible to make the portion of the cushioning member 40 that overlaps with the center 13C of the long side surface of the housing 13 more easily deformable than the portion that overlaps with the outer edge side of the long side surface of the housing 13.
[0062] In the present embodiment, at least one of the multiple first overlapping portions 46b is disposed closer to the center 38C of the electrode body 38 as viewed from the first direction X than the multiple first separated portions 46a. This makes it easier to deform the portion of the buffer member 40 that overlaps with the center 38C of the electrode body 38 relative to the portion that overlaps with the outer edge portion of the electrode body 38. The center 38C of the electrode body 38 is, for example, the geometric center of the outer shape of the electrode body 38 as viewed from the first direction X. The outer edge portion of the electrode body 38 is, for example, a region that includes the end portion of the electrode body 38 in the second direction Y and the end portion in the third direction Z.
[0063] Similarly, at least one of the multiple second overlapping portions 48b is disposed closer to the central portion 38C of the electrode body 38 than the multiple second separated portions 48a when viewed from the first direction X. This makes it possible to make the portion of the cushioning member 40 that overlaps with the central portion 38C of the electrode body 38 more easily deformable than the portion that overlaps with the outer edge portion of the electrode body 38.
[0064] In the present embodiment, the ratio of the area of the laminated portion 45 to the unit area of the cushioning member 40, as viewed from the first direction X, is smaller on the central portion side than on the outer edge side of the cushioning member 40. Also, the ratio of the area of the laminated portion 45 to the unit area of the cushioning member 40, as viewed from the first direction X, is smaller on the central portion 13C side than on the outer edge side of the long side surface of the housing 13. Also, the ratio of the area of the laminated portion 45 to the unit area of the cushioning member 40, as viewed from the first direction X, is smaller on the central portion 38C side than on the outer edge side of the electrode body 38.
[0065] By reducing the number of laminated portions 45 on the center side of the buffer member 40 from the outer edge side, the center side of the buffer member 40 can be made easier to deform. Also, by reducing the number of laminated portions 45 on the center side of the long side surface of the housing 13 from the outer edge side, the portion of the buffer member 40 that overlaps with the center side of the housing 13 can be made easier to deform. Also, by reducing the number of laminated portions 45 on the center side of the electrode body 38 from the outer edge side, the portion of the buffer member 40 that overlaps with the center side of the electrode body 38 can be made easier to deform. The uneven distribution of the laminated portions 45 in the buffer member 40 can be adjusted by the arrangement of the first softening portion 46 and the second softening portion 48.
[0066] When viewed from the first direction X, the first remainder 47 may have a smaller area than the second remainder 49. In other words, the proportion of the first remainder 47 in the first layer 42 may be smaller than the proportion of the second remainder 49 in the second layer 44. In this case, it is possible to provide more first softened portions 46 in the first layer 42. This reduces the contact area between the first layer 42 and the energy storage device 10, that is, it is possible to increase the gap in contact with the energy storage device 10. As a result, the first layer 42 can more easily absorb the expansion of the energy storage device 10.
[0067] Examples of materials constituting the first layer 42 and the second layer 44 (i.e., the first sheet 42a and the second sheet 44a) include thermosetting elastomers such as natural rubber, synthetic rubber, urethane rubber, silicone rubber, and fluororubber, and thermoplastic elastomers such as polystyrene, olefin, polyurethane, polyester, and polyamide. These materials may be foamed. Examples also include heat insulating materials carrying a porous material such as silica xerogel. Therefore, the buffer member 40 has insulating properties and can function as a part of the separator 12 that insulates the power storage device 10 from the outside (for example, an adjacent power storage device 10, the end plate 4, the binding member 6, etc.).
[0068] (Method of manufacturing the cushioning material) The cushioning member 40 can be manufactured, for example, as follows. That is, first, the first sheet 42a and the second sheet 44a are prepared. The first sheet 42a is provided with a first softening portion 46 in advance, and the second sheet 44a is provided with a second softening portion 48 in advance. For example, a long sheet wound in a roll shape is subjected to a punching process or the like to form a through hole penetrating the sheet in the thickness direction of the sheet. Alternatively, the sheet is subjected to a press process or the like to form a recess that is recessed in the thickness direction of the sheet. Then, the sheet with the through hole or recess formed therein is cut to a predetermined length. This allows a large number of first sheets 42a and second sheets 44a to be manufactured.
[0069] Next, the first sheet 42a and the second sheet 44a are laminated so that at least a part of the first softened portion 46 and the second softened portion 48 are shifted. In this embodiment, the first sheet 42a and the second sheet 44a are the same size. Then, in a state where the outer edge of the first sheet 42a and the outer edge of the second sheet 44a are aligned, that is, in a state where the first sheet 42a and the second sheet 44a are closely aligned, the positions of the first softened portion 46 and the second softened portion 48 are shifted. Therefore, by laminating the first sheet 42a and the second sheet 44a so that the outer edges are aligned, the first softened portion 46 and the second softened portion 48 can be shifted.
[0070] The above steps make it possible to manufacture the cushioning member 40 including the first layer 42 and the second layer 44. According to this manufacturing method, the cushioning member 40 can be manufactured simply by stacking sheets that have been subjected to punching or pressing, so that the cushioning member 40 can be manufactured simply and inexpensively.
[0071] As described above, the energy storage module 1 according to the present embodiment includes the energy storage device 10 and the buffer member 40 that is arranged in the first direction X together with the energy storage device 10 and receives a load from the energy storage device 10 in the first direction X. The buffer member 40 has at least a first layer 42 and a second layer 44 that are arranged in the first direction X. The first layer 42 has a first softened portion 46 that is configured as a through hole penetrating the first layer 42 in the first direction X or a recess that is recessed in the first direction X. The second layer 44 has a second softened portion 48 that is configured as a through hole penetrating the first layer 42 in the first direction X or a recess that is recessed in the first direction X. The first softened portion 46 and the second softened portion 48 are at least partially misaligned when viewed from the first direction X.
[0072] By providing the first softening portion 46 in the first layer 42, it is possible to make the cushioning member 40 more easily deformable in the portion where the first softening portion 46 is provided. Similarly, by providing the second softening portion 48 in the second softening portion 48, it is possible to make the cushioning member 40 more easily deformable in the portion where the second softening portion 48 is provided. In other words, by providing the first softening portion 46 and the second softening portion 48, it is possible to partially reduce the laminated portion 45, in which the first remaining portion 47 in the first layer 42 and the second remaining portion 49 in the second layer 44 overlap, within the plane of the cushioning member 40. This makes it possible to provide a portion that is easily deformed and a portion that is difficult to deform within the plane of the cushioning member 40.
[0073] In addition, by disposing at least a portion of the first softening portion 46 and the second softening portion 48 in a shifted manner, it is possible to precisely set the ease of deformation of the cushioning member 40 within a plane. For example, it is also possible to set the cushioning member 40 to be gradually easier to deform from one side to the other within the plane.
[0074] That is, the buffer member 40 of the present embodiment has a configuration in which a plurality of sheets each having a plurality of through holes or recesses are laminated, and a load is received at an area (pressure receiving portion) where the solid portions of the sheets overlap. This allows the area receiving the load from the power storage device 10 to be partially reduced, and the apparent compression elastic modulus can be reduced. In addition, a pressure receiving portion of a minute area that is difficult to create with a single sheet can be created. In addition, the apparent elastic modulus per macro area can be set arbitrarily by adjusting the position and area of the pressure receiving portion. In addition, a gradation can be given to the magnitude of the elastic modulus. In addition, since a relatively hard sheet can be used, it is easier to handle when assembling the buffer member 40 or the power storage module 1 than when a sheet with a low and uniform elastic modulus is used. In addition, a mold for molding is required when providing a protrusion on the sheet constituting the buffer member 40, but the softened portion composed of the through holes or recesses can be formed by a simple method such as punching the sheet. Therefore, the buffer member 40 can be easily created.
[0075] Therefore, according to this embodiment, it is possible to design the arrangement of the buffer member 40 so that the portion of the energy storage device 10 that expands less is pressed by the portion that is less likely to deform, thereby positioning the energy storage device 10, while the portion that is more likely to deform absorbs a large load from the energy storage device 10, thereby reducing the load on the constraint member 6. As a result, even if the amount of expansion of the energy storage device 10 increases as the capacity of the energy storage device 10 increases, the expansion of the energy storage device 10 can be more reliably absorbed while positioning the energy storage device 10, thereby reducing the load on the constraint member 6. Therefore, it is possible to achieve both prevention of damage to the constraint member 6 and positioning the energy storage device 10. As a result, the reliability of the energy storage module 1 can be improved.
[0076] Furthermore, the amount of expansion of the energy storage device 10 generally increases as the period of use passes. In other words, the amount of expansion of the energy storage device 10 changes between the beginning and end of its life. In contrast, according to this embodiment, the restraining force of the restraining members 6 on the battery stack 2 is set in accordance with the small expansion of the energy storage device 10 at the beginning of its life, thereby more reliably positioning the energy storage device 10, and the large expansion of the energy storage device 10 at the end of its life is absorbed by the buffer members 40, thereby reducing the load on the restraining members 6. Therefore, even if the amount of expansion of the energy storage device 10 changes between the beginning and end of its life, the energy storage device 10 can be held with an appropriate restraining force according to the amount of expansion at each stage.
[0077] Moreover, since it is possible to avoid increasing the strength of the restraining member 6, it is possible to suppress increases in size, weight, cost, etc. of the restraining member 6 and, in turn, the electricity storage module 1. It is also possible to suppress an increase in the load on the electricity storage device 10, which would result in a decrease in performance or a shortened lifespan of the electricity storage device 10.
[0078] Moreover, the cushioning member 40 can be manufactured simply by laminating the first sheet 42a having the first softened portion 46 and the second sheet 44a having the second softened portion 48 such that at least a portion of the first softened portion 46 and the second softened portion 48 are misaligned. This allows the cushioning member 40 to be manufactured simply and inexpensively. Also, adjustment of the ease of deformation within a plane can be more easily achieved. Furthermore, a pressure-receiving portion with a minute area that receives a force from the electricity storage device 10 can be more easily formed within the plane of the cushioning member 40.
[0079] Moreover, the first layer 42 of the present embodiment has a plurality of first softened portions 46, and the density of the first layer 42 is smaller on the central side than on the outer edge side of the first layer 42 when viewed from the first direction X. Moreover, the second layer 44 has a plurality of second softened portions 48, and the density of the second layer 44 is smaller on the central side than on the outer edge side of the second layer 44 when viewed from the first direction X. Moreover, the ratio of the area of the laminated portion 45 to the unit area of the cushioning member 40 when viewed from the first direction X is smaller on the central side than on the outer edge side of the cushioning member 40. This makes it possible to obtain a cushioning member 40 in which the central side is easily deformed and the outer edge side is less likely to deform. Therefore, it is possible to more reliably suppress damage to the restraining member 6 and position the electricity storage device 10.
[0080] Also, some of the first softening portions 46 (first separated portions 46a) are disposed so as to be entirely displaced from the second softening portions 48 when viewed from the first direction X, and other parts of the first softening portions 46 (first overlapping portions 46b) are disposed so as to be partially displaced from the second softening portions 48 when viewed from the first direction X. Similarly, some of the second softening portions 48 (second separated portions 48a) are disposed so as to be entirely displaced from the first softening portions 46 when viewed from the first direction X, and other parts of the second softening portions 48 (second overlapping portions 48b) are disposed so as to be partially displaced from the first softening portions 46 when viewed from the first direction X. This allows the ease of deformation of the cushioning member 40 to be more finely adjusted depending on the location, and allows the deformation of the cushioning member 40 to follow the expansion of the power storage device 10 with higher accuracy. Therefore, it is possible to achieve both expansion absorption and positioning of the power storage device 10.
[0081] Furthermore, at least one of the first overlapping portions 46b is disposed closer to the center of the cushioning member 40 than the first separated portions 46a when viewed from the first direction X. Similarly, at least one of the second overlapping portions 48b is disposed closer to the center of the cushioning member 40 than the second separated portions 48a when viewed from the first direction X. This makes it easier for the center side of the cushioning member 40 to deform relative to the outer edge side.
[0082] At least one of the first overlapping portions 46b is disposed closer to the center 13C of the long side surface of the housing 13 than the first spaced portions 46a when viewed from the first direction X. Similarly, at least one of the second overlapping portions 48b is disposed closer to the center 13C of the long side surface of the housing 13 than the second spaced portions 48a when viewed from the first direction X. Also, the ratio of the area of the laminated portion 45 to the unit area of the cushioning member 40 is smaller on the center 13C side than on the outer edge side of the long side surface of the housing 13 when viewed from the first direction X. This makes it easier for the portion of the cushioning member 40 that overlaps with the center 13C side of the long side surface to deform compared to the portion that overlaps with the outer edge side of the long side surface of the housing 13.
[0083] Moreover, at least one of the first overlapping portions 46b is disposed closer to the center 38C of the electrode body 38 than the first separated portions 46a when viewed from the first direction X. Similarly, at least one of the second overlapping portions 48b is disposed closer to the center 38C of the electrode body 38 than the second separated portions 48a when viewed from the first direction X. Moreover, when viewed from the first direction X, the ratio of the area of the laminated portion 45 to the unit area of the buffer member 40 is smaller on the center 38C side than on the outer edge side of the electrode body 38. This makes it easier to deform the portion of the buffer member 40 that overlaps with the center 38C side of the electrode body 38 compared to the portion that overlaps with the outer edge side of the electrode body 38.
[0084] The above describes the embodiments of the present disclosure in detail. The above-mentioned embodiments merely show specific examples of implementing the present disclosure. The contents of the embodiments do not limit the technical scope of the present disclosure, and many design changes such as changes, additions, and deletions of components are possible within the scope of the invention defined in the claims. A new embodiment with a design change has the effects of each of the combined embodiments and modifications. In the above-mentioned embodiments, the contents for which such design changes are possible are emphasized by adding notations such as "in this embodiment" and "in this embodiment", but design changes are permitted even in contents without such notations. In addition, any combination of components included in each embodiment is also valid as an aspect of the present disclosure. The hatching on the cross section of the drawing does not limit the material of the object to which the hatching is added.
[0085] (Variation 1) FIG. 7(A) is a perspective view of the cushioning member 40 according to the first modification. FIG. 7(B) is a front view of the cushioning member 40. The cushioning member 40 according to the embodiment has a two-layer structure of a first layer 42 and a second layer 44, but the number of layers is not particularly limited. For example, the cushioning member 40 according to this modification has a three-layer structure of a first layer 42, a second layer 44, and a third layer 50. The first layer 42, the second layer 44, and the third layer 50 are arranged in this order in the first direction X. The third layer 50 has a third softening portion 52 composed of a through hole penetrating the third layer 50 in the first direction X or a recessed portion recessed in the first direction X. In FIG. 7(A) and FIG. 7(B), the third softening portion 52 composed of a through hole is illustrated. The softening portions are evenly arranged at equal intervals over approximately the entire sheet constituting each layer.
[0086] In the cushioning member 40 according to the embodiment, the first layer 42 and the second layer 44 are perfectly aligned with each other, but the positions of the first softened portion 46 and the second softened portion 48 are shifted. On the other hand, in the cushioning member 40 according to the first modification, the first layer 42, the second layer 44, and the third layer 50 have the same shape, including the arrangement of the softened portions. The first layer 42 and the second layer 44 are arranged such that their outer edges are shifted from each other, so that the first softened portion 46 and the second softened portion 48 are shifted from each other. The second layer 44 and the third layer 50 are arranged such that their outer edges are shifted from each other, so that the second softened portion 48 and the third softened portion 52 are shifted from each other.
[0087] The cushioning member 40 of this modified example can achieve the same effects as the embodiment. Moreover, in this modified example, the first layer 42 to the third softened portion 52 have the same shape, so the manufacturing process for the cushioning member 40 can be further simplified. The first layer 42 and the third layer are also arranged so as to be shifted from each other, and the first softened portion 46 and the third softened portion 52 are shifted from each other. This allows the ease of deformation of the cushioning member 40 to be adjusted more finely.
[0088] (Variation 2) Fig. 8(A) is a perspective view of a cushioning member 40 according to the second modification. Fig. 8(B) is a front view of the cushioning member 40. The first softening portion 46 and the second softening portion 48 of the cushioning member 40 according to the embodiment are circular when viewed from the first direction X, but the shape of each softening portion is not particularly limited. For example, the first softening portion 46 and the second softening portion 48 of the cushioning member 40 according to this modification are substantially rectangular when viewed from the first direction X. In addition, the first layer 42 and the second layer 44 may be polygonal, such as a hexagon.
[0089] (Variation 3) The buffer members 40 may be provided for all combinations of two adjacent power storage devices 10, or may be provided for some combinations. In addition to being provided between the two power storage devices 10, the buffer members 40 may also be provided between the power storage device 10 and the end plate 4. Furthermore, the buffer members 40 may be provided only between the power storage device 10 and the end plate 4.
[0090] (Variation 4) The number of power storage devices 10 included in the power storage module 1 is not particularly limited, and the power storage module 1 only needs to have at least one power storage device 10. The structures of each part of the power storage module 1, including the structures of the end plates 4 and the restraining members 6, are not particularly limited.
[0091] (Variation 5) FIG. 9(A) is a perspective view of a cushioning member 40 according to the fifth modification. FIG. 9(B) is a perspective view of a cross section taken along the line AA in FIG. 9(A). The cushioning member 40 according to this modification has a five-layer structure including a first layer 42, a second layer 44, a third layer 50, a fourth layer 54, and a fifth layer 56, for example. The first layer 42, the second layer 44, the third layer 50, the fourth layer 54, and the fifth layer 56 are arranged in this order in the first direction X. The third layer 50 has a third softened portion 52, and the fourth layer 54 has a fourth softened portion 58. The first softened portion 46 to the fourth softened portion 58 are each formed of a through hole. The fifth layer 56 does not have a softened portion.
[0092] The softened parts of each layer are arranged concentrically. The opening areas of the first softened part 46 to the fourth softened part 58 become gradually smaller in this order. Therefore, the cushioning member 40 is provided with a recess having an inner surface that curves so as to widen as it approaches the first layer 42 side. When the electricity storage device 10 arranged on the first layer 42 side expands, the expanding part of the electricity storage device 10 can be accommodated in this recess. [Explanation of symbols]
[0093] 1 Energy storage module, 10 Energy storage device, 13 Housing, 38 Electrode body, 40 Cushioning member, 42 First layer portion, 42a First sheet, 44 Second layer portion, 44a Second sheet, 46 First softening portion, 48 Second softening portion.
Claims
1. At least one power storage device; a buffer member arranged in a first direction together with the power storage device and receiving a load from the power storage device in the first direction; the buffer member has at least a first layer and a second layer arranged in the first direction, the first layer portion has a first softening portion configured with a through hole penetrating the first layer portion in the first direction or a recessed portion recessed in the first direction, the second layer portion has a second softened portion configured with a through hole penetrating the second layer portion in the first direction or a recessed portion recessed in the first direction, the first softened portion and the second softened portion are at least partially misaligned when viewed from the first direction, The first softening portion includes a plurality of first spaced portions and a plurality of first overlapping portions, the first separated portion is the first softened portion that is entirely shifted with respect to the second softened portion when viewed from the first direction, The first overlapping portion is the first softened portion that is partially shifted from the second softened portion when viewed from the first direction. Energy storage module.
2. the first layer portion has a first remainder which is a portion other than the first softened portion, the second layer portion has a second remainder which is a portion excluding the second softened portion, The cushioning member has a laminated portion where the first remaining portion and the second remaining portion overlap each other. The energy storage module according to claim 1 .
3. a ratio of an area of the laminated portion to a unit area of the buffer member is smaller on a central portion side than on an outer edge side of the buffer member when viewed from the first direction; The power storage module according to claim 2 .
4. The power storage device includes a housing, a pair of output terminals disposed on a first surface of the housing, and an electrode body accommodated in the housing; The housing has a side surface that extends in a direction intersecting with the first direction, a ratio of an area of the laminated portion to a unit area of the cushioning member is smaller on a central portion side of the side surface than on an outer edge portion side of the side surface, as viewed from the first direction; The power storage module according to claim 3 .
5. The power storage device includes a housing, a pair of output terminals disposed on a first surface of the housing, and an electrode body accommodated in the housing; The electrode assembly has a positive electrode and a negative electrode aligned in the first direction, a ratio of an area of the laminated portion to a unit area of the buffer member is smaller on a central portion side than on an outer edge side of the electrode body when viewed from the first direction; The power storage module according to claim 3 .
6. When viewed from the first direction, the first remainder has a smaller area than the second remainder. The power storage module according to claim 2 .
7. a density of the first layer portion is smaller on a central portion side than on an outer edge portion side of the first layer portion when viewed from the first direction; The energy storage module according to claim 1 .
8. At least one of the plurality of first overlapping portions is disposed closer to a center portion of the buffer member than the plurality of first separated portions when viewed from the first direction. The energy storage module according to claim 1 .
9. The power storage device includes a housing, a pair of output terminals disposed on a first surface of the housing, and an electrode body accommodated in the housing; The housing has a side surface that extends in a direction intersecting with the first direction, At least one of the plurality of first overlapping portions is disposed closer to a center portion of the side surface than the plurality of first separated portions when viewed from the first direction. The energy storage module according to claim 1 or 8.
10. The power storage device includes a housing, a pair of output terminals disposed on a first surface of the housing, and an electrode body accommodated in the housing; The electrode assembly has a positive electrode and a negative electrode aligned in the first direction, At least one of the plurality of first overlapping portions is disposed closer to a center portion of the electrode body than the plurality of first spaced portions when viewed from the first direction. The energy storage module according to claim 1 , 8 , or 9 .
11. a density of the second layer portion is smaller on a central portion side than on an outer edge portion side of the second layer portion when viewed from the first direction; The energy storage module according to claim 1 , 7 , 8 , 9 , or 10 .
12. At least one power storage device; a buffer member arranged in a first direction together with the power storage device and receiving a load from the power storage device in the first direction; the buffer member has at least a first layer and a second layer arranged in the first direction, the first layer portion has a first softening portion configured with a through hole penetrating the first layer portion in the first direction or a recessed portion recessed in the first direction, the second layer portion has a second softened portion configured with a through hole penetrating the second layer portion in the first direction or a recessed portion recessed in the first direction, the first softened portion and the second softened portion are at least partially misaligned when viewed from the first direction, The second softening portion includes a plurality of second spaced portions and a plurality of second overlapping portions, the second separated portion is the second softened portion that is entirely shifted with respect to the first softened portion when viewed from the first direction, The second overlapping portion is the second softened portion that is partially shifted from the first softened portion when viewed from the first direction. Energy storage module.
13. At least one of the plurality of second overlapping portions is disposed closer to a center portion of the buffer member than the plurality of second spaced portions when viewed from the first direction. The power storage module according to claim 12.
14. The power storage device includes a housing, a pair of output terminals disposed on a first surface of the housing, and an electrode body accommodated in the housing; The housing has a side surface that extends in a direction intersecting with the first direction, At least one of the plurality of second overlapping portions is disposed closer to a center portion of the side surface than the plurality of second separated portions when viewed from the first direction. The energy storage module according to claim 12 or 13.
15. The power storage device includes a housing, a pair of output terminals disposed on a first surface of the housing, and an electrode body accommodated in the housing; The electrode assembly has a positive electrode and a negative electrode aligned in the first direction, At least one of the plurality of second overlapping portions is disposed closer to a center portion of the electrode body than the plurality of second spaced portions when viewed from the first direction. The energy storage module according to any one of claims 12 to 14.
16. A buffer member arranged in a first direction together with at least one power storage device and receiving a load from the power storage device in the first direction, The optical fiber includes at least a first layer portion and a second layer portion arranged in the first direction, the first layer portion has a first softening portion configured with a through hole penetrating the first layer portion in the first direction or a recessed portion recessed in the first direction, the second layer portion has a second softened portion configured with a through hole penetrating the second layer portion in the first direction or a recessed portion recessed in the first direction, the first softened portion and the second softened portion are at least partially misaligned when viewed from the first direction, The first softening portion includes a plurality of first spaced portions and a plurality of first overlapping portions, the first separated portion is the first softened portion that is entirely shifted with respect to the second softened portion when viewed from the first direction, The first overlapping portion is the first softened portion that is partially shifted from the second softened portion when viewed from the first direction. Cushioning material.
17. A method for manufacturing a buffer member that is arranged in a first direction together with at least one power storage device and receives a load from the power storage device in the first direction, comprising: The method includes laminating a first sheet having a first softened portion constituted by a through hole penetrating the first sheet in the thickness direction or a recessed portion recessed in the thickness direction, and a second sheet having a second softened portion constituted by a through hole penetrating the first sheet in the thickness direction or a recessed portion recessed in the thickness direction, such that at least a portion of the first softened portion and the second softened portion are misaligned, The first softening portion includes a plurality of first spaced portions and a plurality of first overlapping portions, the plurality of first separated portions are the first softened portion that is entirely shifted with respect to the second softened portion when viewed from the first direction, The plurality of first overlapping portions are the first softened portions that are partially shifted from the second softened portion when viewed from the first direction. A method for manufacturing a cushioning member.
Citation Information
Patent Citations
Power storage module
JP2015099648A
Power supply module
JP2015185463A
Power storage device
JP2019067665A
Power supply device, vehicle equipped with same, power storage device and separator for power supply device
WO2018207607A1