Accelerator-free, highly tear-resistant synthetic gloves
A bi-layer laminate glove with a chloroprene outer and nitrile inner layer addresses the comfort and resistance issues of existing gloves, providing enhanced durability and grip through metal oxide cross-linking, achieving superior performance in surgical and examination settings.
Patent Information
- Application Number
- JP2024505178
- Authority / Receiving Office
- JP · JP
- Patent Type
- Patents
- Current Assignee / Owner
- Priority Date
- 2021-07-27
- Filing Date
- 2022-07-27
- Publication Date
- 2024-12-09
- Estimated Expiration
- 2042-07-27
AI Technical Summary
Current surgical and examination gloves lack a combination of comfort, chemical resistance, and tear resistance, with nitrile and neoprene gloves being less comfortable than polyisoprene but lacking its chemical resistance, and polyisoprene gloves not being accelerator-free.
A bi-layer laminate glove composed of a chloroprene outer layer and a nitrile inner layer, cross-linked with metal oxides, providing high tear resistance and good grip without accelerators, and designed to be thin and soft for extended wear.
The laminate glove offers superior comfort, tear resistance, and grip, with enhanced durability and chemical resistance, outperforming comparable gloves in mechanical stress tests and chemical exposure scenarios.
Smart Images

Figure 0007596597000002 
Figure 0007596597000003 
Figure 0007596597000004
Abstract
Description
[Technical field]
[0001] This application relates generally to non-supported gloves, such as surgical and examination gloves. [Background technology]
[0002] 2. Description of Related Art During surgery or examination procedures, gloves may be worn for several hours. Therefore, comfort is a high priority, as is integrity and resistance to sterile fluids. Polyisoprene gloves can provide significant comfort and are free of allergy-inducing proteins. However, most are not accelerator-free or exhibit the chemical resistance of nitrile and neoprene gloves. On the other hand, nitrile and neoprene gloves are generally not as comfortable as polyisoprene gloves.
[0003] Making gloves accelerator-free increases comfort by minimizing skin irritation. In addition, designing gloves to have useful elongation-to-break values ensures that the gloves are less likely to tear during stresses induced by manipulating surgical equipment. Furthermore, gloves need to be thin to provide greater proficiency, less likely to tear from stresses applied during sterile donning, soft and comfortable, and have good grip. However, this combination of properties is not available in current nitrile or chloroprene-based gloves.
[0004] In view of the above, the inventors herein provide an accelerator-free, multi-layer (e.g., two-layer) laminate glove having high tear resistance and good grip. Summary of the Invention
[0005] According to an embodiment of the present disclosure substantially as shown and / or described in connection with at least one of the drawings, such a laminate glove and a method for manufacturing the same are disclosed. Various advantages, aspects, and novel features of the present disclosure will become more fully understood from the following description and drawings. The foregoing summary is not intended, and should not be construed, to describe each embodiment or every implementation of the present disclosure. Other and further embodiments of the present disclosure are described below. Furthermore, changes and modifications can be made to the embodiments described herein without departing from the spirit and scope of the present disclosure and without diminishing its attendant advantages.
[0006] In one exemplary embodiment, a two to three layer unsupported glove includes: (A) an outer first layer having a polymer content of 55 wt% or more chloroprene, 0 wt% to up to 45 wt% nitrile, including carboxylated nitrile, and about 5 wt% or less of another polymer; and (B) a second layer having a polymer content of substantially 90 wt% or more nitrile, laminated to the outer layer, the glove having a thickness of 0.16 mm or less (or <0.15 mm, or <0.14 mm, or <0.13 mm) and conforming to ASTM D412:2016(E 2021) of an unaged tensile strength of greater than 17 MPa (or >18 MPa, or >19 MPa) or an aged tensile strength of greater than 23 MPa (or >24 MPa, or >25 MPa), and is accelerator-free, and the glove is (i) packaged so that the inner layer is positioned inside the outer layer, or (ii) folded to facilitate donning of the glove by the user with the inner layer inside the outer layer.
[0007] So that the foregoing features of the invention can be understood in detail, a more particular description of the invention briefly summarized above can be understood with reference to embodiments, some of which are illustrated in the accompanying drawings, in which it should be noted, however, that the accompanying drawings illustrate only exemplary embodiments of the invention and are therefore not to be considered as limiting the scope thereof since the invention may admit of other equally effective embodiments. [Brief description of the drawings]
[0008] [Figure 1] 1A and 1B show the mixing of latex. [Diagram 2] FIG. 2 shows the glove forming process. DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0009] For ease of understanding, the same reference numbers have been used, where possible, to indicate comparable elements common to the drawings. The drawings are not drawn to scale and may be simplified for clarity. It is contemplated that elements and features of one embodiment may be beneficially incorporated in other embodiments without further recitation.
[0010] It should be noted at the outset that in the development of any such practical embodiment, numerous implementation-specific decisions must be made to achieve the developer's particular goals, e.g., adherence to system-related and business-related constraints, which will vary from implementation to implementation. Moreover, it will be appreciated that such a development effort may be complex and time-consuming, but would nevertheless be a routine undertaking for those of ordinary skill in the art having the benefit of this disclosure. In addition, the compositions used / disclosed herein may also include several components other than those described herein. In the Summary and in this Detailed Description, each numerical value should be read once as modified by the term "about" (unless already so modified) and then again as not so modified unless otherwise noted.
[0011] The following definitions are provided to aid those skilled in the art in understanding the detailed description.
[0012] As used in the specification and claims, "near" includes "at."
[0013] As used in this specification, the terms "have," "may have," "include," "comprise," "may include," and "may comprise" indicate the presence of the corresponding feature (e.g., value, function, operation, or component) but do not exclude the presence of additional features.
[0014] For purposes herein, an article is "free" or "substantially free" of a material when no accelerator is intentionally added to the ingredients from which the article is made and / or the concentration of the material is less than about 0.01 wt% of the total weight of the article. For example, for purposes herein, a glove is "accelerator-free," also referred to herein as not containing accelerators, when no accelerator is intentionally added to the ingredients from which the article is made and / or the concentration of the accelerator is less than about 0.01 wt% of the total weight of the article.
[0015] For purposes of this specification, accelerator-free refers to non-metallic crosslinkers, e.g., sulfur-based chemical accelerators including dithiocarbamates, thiurams, mercaptobenzothiazoles (MBT), etc. Thus, if the rubber is crosslinked with polyvalent metal ions such as Zn, Ti, Al, and / or the like, the glove may be accelerator-free.
[0016] For purposes of this specification, the term "nitrile" refers to elastomers that include polyacrylonitrile and butadiene moieties, i.e., polyacrylonitrile and butadiene rubber, also referred to herein as nitrile rubber.
[0017] For purposes of this specification, carboxylated nitrile, also referred to as carboxylated nitrile rubber, refers to a terpolymer of butadiene, acrylonitrile, and an unsaturated carboxylic acid or dicarboxylic acid, such as, for example, acrylic acid, methacrylic acid, crotonic acid, maleic acid, fumaric acid, or combinations thereof and / or the like, and the resulting carboxylic acid groups allow for crosslinking of the polymer backbone through the addition of one or more metal additives, sulfur, and the like.
[0018] For purposes herein, all percentages are weight defined (i.e., wt %) based on the total weight of a particular portion or layer of an article, e.g., based on the total weight of the referenced polymer layer.
[0019] In this disclosure, phrases such as "A and / or B," "at least one of A and / or B," and "one or more of A and / or B" refer to cases in which any and all combinations of one or more of the associated listed items may be included. For example, the terms "A and / or B" and "at least one of A or B" may refer to cases in which (1) A is included, (2) B is included, or (3) both A and B are included.
[0020] While the terms "first" and "second" refer to various elements in various embodiments disclosed herein, it is to be understood that these labels do not limit the elements to a particular order, amount, or importance, and that such terms are used only to distinguish one element from another, and do not limit the order and / or priority of the elements. Similarly, such terms are used relative to other terms, and do not convey an absolute position, location, or order. For example, a first element of one embodiment may be referred to as a second element in another embodiment, and similarly, a second element may be referred to as a first element, without departing from the scope of the present disclosure.
[0021] The embodiments according to the present disclosure relate to multi-layer (e.g., at least two-layer) laminate gloves having a chloroprene polymer outer layer and a nitrile rubber layer laminated to the inside of the chloroprene layer. In embodiments, these gloves have the required combination of properties, including being cured using crosslinking via metal ions, containing no accelerators, being highly tear-resistant, being soft and comfortable to the wearer over time, and having a good grip. In addition, when subjected to a mechanical simulation of the localized tension applied to the wrist of the glove when worn, the laminate gloves are much more resistant to tearing than a nitrile glove of comparable thickness, and even more resistant compared to a comparable chloroprene glove. Thus, applicants have discovered a previously unknown symbiotic relationship between chloroprene and nitrile rubber, which, when combined and arranged according to the embodiments disclosed herein, results in gloves that have superior properties compared to gloves formed from the individual components.
[0022] The first outer layer of the glove, primarily polychloroprene (neoprene), is crosslinked with a metal oxide (e.g., divalent or trivalent), such as zinc oxide, lead oxide, lead tetroxide, etc., as known in the art (see, e.g., Smejda-Krzewicka et al., Polymer Bulletin volume 77, pages 4131-4146 (2020); US 2014 / 0011936). The latex suspension generally includes an antioxidant, such as an oligomeric hindered phenolic antioxidant.
[0023] The second inner layer, which is essentially nitrile (acrylonitrile butadiene), is typically crosslinked with a metal oxide (e.g., divalent or trivalent), such as zinc oxide, titanium oxide, aluminum oxide, etc. See, e.g., US 7,005,478 B2, US 10,954,364 B2, US 10,023,718 B2.
[0024] The layers that are primarily polychloroprene (i.e., contain more than 50 wt% polychloroprene) contain, in polymer content, about 55 wt% or more chloroprene, 0% up to about 45 wt% nitrile, including carboxylated nitrile, and about 5 wt% or less of another polymer. The other polymer can be, for example, natural rubber (NR), synthetic polyisoprene (PI), polyurethane (PU), butyl rubber (IIR or butyl), styrene-butadiene rubber (SBR, e.g., carboxylated), a combination of butyl and fluoroelastomer (FKM, also known as Viton®), or a mixture thereof. In embodiments, these layers have a polymer content of about 98 wt% or more, about 99 wt% or more, or 100 wt% polychloroprene.
[0025] In embodiments, the nitrile comprises about 10 wt% or more, or about 20 wt% or more, or about 30 wt% or more (up to about 45 wt%) of the layer that is primarily polychloroprene. In embodiments, the nitrile comprises about 40 wt% or less, or about 30 wt% or less of the layer that is primarily polychloroprene. (Unless otherwise specified, polymer composition is relative to structural polymer content (e.g., not pigments or rheological agents) and is expressed by weight.)
[0026] The primarily polychloroprene layer can be, for example, about 75 micrometers (about 2.95 mils) to about 120 micrometers (about 4.7 mils) thick, measured in the center of the palm.
[0027] The substantially nitrile layer is about 90 wt% or more nitrile. In embodiments, the substantially nitrile layer is about 95 wt% or more, or about 97 wt% or more, or about 98 wt% or more, or 100 wt% nitrile. The other polymers can be, for example, chloroprene (CR), natural rubber (NR), synthetic polyisoprene (PI), polyurethane (PU), butyl rubber (IIR or butyl), styrene-butadiene rubber (SBR, e.g., carboxylated), combinations of butyl and fluoroelastomers, or mixtures thereof. The degree of carboxylation can be an amount that promotes cure or chemical resistance to a second class of chemicals (e.g., weak acids such as acetic acid, hydrocarbons, heptane, hexane, toluene, or xylene). See US10,154,699B2. One skilled in the art will recognize that the amount of carboxylation can be adjusted to the desired properties. For example, the carboxylation can be at the lower end required for cure or chemical resistance to help provide greater elasticity.
[0028] The glove polymer can be selected to minimize allergens such as those found in gloves containing NR or high amounts of NR.
[0029] The substantially nitrile layer can be, for example, about 50 micrometers (about 2 mils) to about 80 micrometers (about 3.1 mils) thick, measured at the center of the palm.
[0030] In an embodiment, the glove has a thin third layer inside the substantially nitrile layer, such as a polymeric coating layer comprising polyurethane, polyacrylic, polyacrylonitrile, polyisoprene, or a blend or copolymer. This layer can be thinner than the first or second layers, for example, or about 1 to about 20 micrometers thick (about 0.04 to about 0.8 mils), or about 5 to about 15 micrometers thick (about 0.2 to about 0.6 mils), or about 3 micrometers thick to about 5 micrometers thick (about 0.12 to about 0.2 mils).
[0031] The polymer composition optionally contains suitable additives such as pH balancers, fillers, rheology modifiers, etc., to stabilize the polymer composition or to impart desired properties. The polymer composition optionally contains commonly used stabilizers, including but not limited to potassium hydroxide, ammonia, sulfonates, and others known to those skilled in the art. The polymer composition may contain other commonly used ingredients, such as surfactants, antimicrobial agents, fillers / additives to impart various physical and chemical properties, etc., known to those skilled in the art.
[0032] In conjunction with the formation of the glove, a polymeric dispersion is formulated as illustrated in Figures 1A and 1B. In Figure 1A, in process 131, a stabilized CR latex is provided, which may be appropriately adjusted for TSC in step 132. Next, in step 134, NBR latex is added. Other polymers may be added in conjunction with steps 132 or 134 or separately. In step 136, metal oxides, antioxidants, and pigments are added. In step 138, the TSC used for dipping, for example about 18-35 wt%, is established, typically by adding water.
[0033] In FIG. 1B, in process 151, a stabilized NBR latex is provided, which can be appropriately adjusted for TSC in step 152. Then, in step 154, metal oxides and antioxidants are added. Other polymers may be added in conjunction with steps 152 or 154, or separately. In step 156, a pigment is added. In step 158, the TSC used for steeping, for example about 18-35 wt%, is established, typically by adding water.
[0034] The glove forming process 100 is shown in Figure 2. In step 110, the former is heated to an appropriate temperature for dipping. In step 120, the former is dipped into a coagulant and oven dried. In step 130, the former is dipped into polychloroprene latex, optionally a blended latex. In step 140, the former with the CR coating is dried. In step 150, the former is dipped into a latex that is essentially NBR to form a second polymer coating. Step 160 In step 160, the double coated former is dried and pre-leached. In optional step 170, the coating is further coated with another polymer layer (as described above) and cured. In step 180, the coating is post-leached and siliconized. In step 190, the coating, now the glove, is stripped from the former and the glove is packaged and sterilized.
[0035] The gloves of the present invention are unsupported. They may be examination or surgical gloves. As surgical gloves, they may be presented in a sterile package, typically in pairs to the package (e.g., polypropylene-lined packages). The surgical gloves may be unique to right and left gloves to provide a greater fit. Thus, left and right may be labeled using sleeves or separators in the package, or the gloves may be labeled. The surgical gloves may be cuff folded to facilitate the sterile donning procedure.
[0036] While tear strength is important, the repeated pulling process that mimics the pulling on the glove cuff during wear, i.e., tear fixture testing, may be a more important parameter. In embodiments, aged or unaged gloves withstand substantially more such pulling without tearing than nitrile gloves of comparable thickness and tear strength. In embodiments, the glove durability is 350 or more cycles in tear fixture testing, or 400 or more cycles, or 425 or more cycles, or 450 or more cycles.
[0037] In embodiments, the grip of the glove (against the metal of the textured exterior) is about 200 g / f (gram force) or greater, or about 240 g / f or greater, or about 260 g / f or greater, or about 300 g / f or greater. In embodiments, the grip of the glove is up to about 350 g / f. The texturing may be formed, for example, by a raised diamond pattern texture mold as described in WO 2006 / 025843 A1, a surface having a plurality of convex projections or suction cup structures, or a surface with a series of depressions, as described in US 8,522,363 B2, or by the method of US 10,500,797 B2.
[0038] For purposes of this specification, glove grip is determined under dry conditions, i.e., on dry specimens, using an in-house method with an IMADA tribometer.
[0039] For purposes of this specification, the thickness of a glove is measured at the center of the palm and, in embodiments, is about 0.16 mm or less, about 0.15 mm or less, or about 0.14 mm or less, or about 0.13 mm or less. The thickness may be about 0.11 mm or more, or about 0.12 mm or more.
[0040] In embodiments, the glove has an unaged tensile strength of about 17 MPa or more (ASTM D412:2016(E 2021)), or about 18 MPa or more, or about 19 MPa or more. In embodiments, the glove has an unaged tensile strength of about 9 N or more (EN 455-2:2015), or about 9.5 N or more, or about 10 N or more.
[0041] In embodiments, the glove has an aged tensile strength of at least 23 MPa (ASTM D412:2016(E 2021)), or at least 24 MPa, or at least 26 MPa (accelerated aging at 70°C for 7 days). In embodiments, the glove has an aged tensile strength of at least about 9 N (EN 455-2:2015), or at least about 10 N, or at least about 11 N.
[0042] In an embodiment, the gloves have an IPA resistance of at least level 2 (EN 16523-1:2015), which indicates a breakthrough time of at least 30 minutes. The samples are preconditioned at a temperature of 23+ / -2°C for at least 16 hours. The assembled permeation cell is placed in a temperature-controlled room at a similar temperature.
[0043] In embodiments, the elongation at break of the aged and unaged glove is about 650% or greater, or about 700% or greater based on the initial length of the specimen (ASTM D412:2016).
[0044] In embodiments, the tensile stress modulus at 500% of the glove after or before aging is about 7 MPa or less, or about 6 MPa or less, or about 5 MPa or less, or about 4.7 MPa or less (ASTM D412:2016).
[0045] In embodiments, the puncture resistance of the glove before aging is about 65 N / mm or greater, or about 70 N / mm or greater, or about 75 N / mm or greater, as determined according to SNZ AS / NZS 4179:2014.
[0046] In embodiments, the stress retention (i.e., stress relaxation) of the glove before aging is about 42% or greater, or about 45% or greater, or about 48% or greater, as determined according to ASTM D412:2016 (E 2021).
[0047] In embodiments, the tear strength of the glove before aging is greater than or equal to about 16 N / mm, or greater than or equal to about 18 N / mm, or greater than or equal to about 20 N / mm (as determined according to ASTM D624 Type C:2000 (R2020)).
[0048] [Embodiment] The following embodiments are contemplated herein. E1. A non-supportive glove, an outer first layer having a polymer content of at least 55 wt.% chloroprene, 0 wt.% to about 45 wt.% nitrile rubber, and up to about 5 wt.% of another polymer, if another polymer is present; a second layer laminated to the outer layer and including at least about 90 wt. % nitrile rubber in terms of polymer content; the glove has a thickness, as determined at the center of the palm portion of the glove, of about 0.16 mm or less; Approximately 17°C when determined according to ASTM D412:2016(E 2021) M The unsupported glove has a pre-aging tensile strength of 100 Pa or more.
[0049] E2. The unsupported glove of embodiment E1, having a tensile strength of greater than or equal to about 23 MPa, as determined according to ASTM D412:2016 (E 2021), after aging at about 70° C. for 7 days.
[0050] E3. The unsupported glove of embodiment E1 or E2, wherein the nitrile rubber comprises a carboxylated nitrile rubber.
[0051] E4. Non-supportive gloves, A first outer layer having a polymer content of 55 wt% or more of chloroprene, 0 wt% to a maximum of 45 wt% of a nitrile, including a carboxylated nitrile, and about 5 wt% or less of another polymer; and a second layer laminated to the first outer layer, the second layer having a polymer content of substantially 90 wt% or more of nitrile, The glove has a thickness of about 0.16 mm or less and a thickness of about 17 mm or less in accordance with ASTM D412:2016(E 2021). M The unsupported glove has an unaged tensile strength of greater than about 23 MPa when aged for 7 days at about 70° C., and is accelerator-free.
[0052] E5. The unsupported glove of any one of embodiments E1-E4, wherein the outer first layer comprises, by polymer content, at least about 55 wt.% chloroprene, from 0 wt.% to at least about 45 wt.% nitrile rubber including carboxylated nitrile rubber, and at most about 5 wt.% of another polymer, if present.
[0053] E6. The unsupported glove of any one of embodiments E1-E5, wherein the durability of the glove is greater than or equal to about 350 cycles as determined according to a tear fixture test.
[0054] E7. before The first layer is In terms of polymer content The unsupported glove of any one of embodiments E1-E6, comprising about 20 wt. % or more of nitrile rubber.
[0055] E8. The first layer but Polymer Content In The unsupported glove of any one of embodiments E1-E7, comprising about 30 wt. % or more of nitrile.
[0056] E9. The unsupported glove of any one of embodiments E1-E8, wherein the layer has a thickness of about 0.075 mm to about 0.12 mm.
[0057] E10. The unsupported glove of any one of embodiments E1-E9, wherein the second layer has a thickness of about 0.05 mm to about 0.08 mm.
[0058] E11. The non-supported glove of any one of embodiments E1-E10, comprising a third layer that is thinner than the first and second layers.
[0059] E12. The unsupported glove of any one of embodiments E1-11, wherein the glove has a thickness of about 0.12 mm to about 0.14 mm.
[0060] E13. The non-supported glove of any one of embodiments E1-E12, wherein the glove has a grip of about 200 g / f or greater.
[0061] E14. The second layer but Polymer Content In The unsupported glove of any one of embodiments E1-E13, comprising about 90 wt. % or more of nitrile.
[0062] E15. The unsupported glove of any one of embodiments E1-E14, having an IPA resistance of level 2 or greater.
[0063] E16. The unsupported glove of any one of embodiments E1-E15, having a pre-aged tear strength of about 16 N / mm or greater, as determined according to ASTM D624 Type C:2000(R 2020).
[0064] E17. The non-supported glove of any one of embodiments E1-E16, wherein the puncture resistance before aging is greater than or equal to about 65 N / mm as determined according to SNZ AS / NZS 4179:2014.
[0065] E18. The unsupported glove of any one of embodiments E1-E17, wherein the elongation to break, after or before aging, is about 650% or greater.
[0066] E19. The unsupported glove of any one of embodiments E1-E18, wherein the tensile strength modulus at 500% of aging or before aging is about 7 MPa or less.
[0067] E20. The non-supported glove of any one of embodiments E1-E19, having a stress retention before aging of about 42% or greater, as determined according to ASTM D412:2016 (E 2021).
[0068] E21. The unsupported glove of any one of embodiments E1-E20, wherein the unsupported glove is packaged (i) so that the inner layer is disposed inside the outer layer, or (ii) so that the inner layer is folded to facilitate donning of the unsupported glove by a user so that the inner layer is inside the outer layer.
[0069] E22. The unsupported glove of any one of embodiments E1-E21 having two or more layers.
[0070] E23. The unsupported glove of any one of embodiments E1-E21 having three or more layers.
[0071] E24. A non-supported glove according to any one or combination of the embodiments disclosed herein.
[0072] Specific embodiments in accordance with the methods of the present invention are described in the following examples, which are illustrative only, and not intended to limit the remainder of the disclosure in any way.
[0073] All ranges described herein include the ranges therebetween and may include or exclude the endpoints. Any included ranges are the integer values between (or including one original endpoint), the recited digits or the next lower digit. For example, if the lower range value is 0.2, any included endpoints can be 0.3, 0.4, ... 1.1, 1.2, etc., as well as 1, 2, 3, etc., and if the upper range is 8, any included endpoints can be 7, 6, etc., as well as 7.9, 7.8, etc. One-sided boundaries such as 3 or more similarly include consistent boundaries (or ranges) beginning with the recited digit or the next lower integer value. For example, 3 or more includes 4 or more, or 3.1 or more. If two ranges such as about 1-10 and about 2-5 are listed, a person skilled in the art will recognize that the included ranges of 1-5 and 2-10 are within the scope of the invention.
[0074] A laminate is a bond, fusion, adhesion, etc. between polymeric layers, or between polymeric and textile layers, such that the laminate is of unitary construction in the anticipated range of use.
[0075] If a sentence states that the subject matter is found in an embodiment, or in a particular embodiment, etc., it is applicable to any embodiment to which the subject matter can logically be applied.
[0076] Glove grip was measured using an IMADA tribometer (IMADA horizontal motorized test stand MH2-500N, IMADA mountable digital force gauge ZT series, and IMADA ForceRecorder Standard (COF Ver.) software version 1.01).
[0077] The principle of this test method is based on the fact that the frictional resistance to the relative motion of two solid bodies is proportional to the force with which the surfaces press together and to the roughness of the surfaces. The force perpendicular or "normal" to the surfaces that affects the frictional resistance is typically called the "normal force" and is expressed as N Identified by The frictional resistance is then measured according to formula (II). f friction =m*N In the formula, m=coefficient of friction (II).
[0078] Also, the friction force is assumed to be proportional to the coefficient of friction. However, the amount of force required to move an object starting from rest is usually greater than the force required for the object to start moving and continue moving at a constant speed. Rougher surfaces experience greater friction compared to smoother surfaces. Thus, higher friction values imply better grip properties for these tested samples.
[0079] [Sample preparation and test method] The specimens used for testing were cut from representative areas of the palm back area of the glove samples and inspected to be free of holes, blisters, creases and other defects.
[0080] One specimen was cut from each glove, with a minimum of seven pieces of each lot sample size required.
[0081] All tests were performed at 20-25°C and 45-55% relative humidity, where specimens were conditioned for at least 24 hours prior to testing.
[0082] The rectangular specimen was clamped onto a flat metal surface, and a diamond-shaped glove was wrapped around a flat metal weight, which was then placed on the rectangular specimen. The wrapped flat metal weight to be judged was then pulled with an IMADA force gauge until it reached the 15mm mark.
[0083] Friction measurements were taken using an IMADA horizontal motorized measuring stand MH2-500N. Data was displayed graphically and analyzed by a transfer system at up to 2000 data points per second.
[0084] Stress retention tests are determined according to ASTM D412:2016(E 2021), which is called stress retention or stress relaxation and indicates the reduction in stress in a material subjected to a constant strain over time. The principle of the test method is that when a constant strain is applied to a rubber specimen, the force required to maintain that strain is not constant but decreases with time. This behavior is called "stress retention" or "stress relaxation".
[0085] The processes that cause stress retention can be physical (e.g., pyrolysis) or chemical in nature, and under all normal conditions, both types of processes occur simultaneously. However, at normal or low temperatures and / or short times, stress retention is dominated by physical processes, whereas at higher temperatures and / or longer times, chemical processes dominate.
[0086] The test method includes the following steps: ○ Test specimens are cut into dumbbell specimen shapes using ASTM D412 Die C. The median thickness is determined and measured from three locations on the dumbbell specimen, which is used to calculate the cross-sectional area. The prepared dumbbell specimens are clamped and stressed to 100% of their initial length using a Shimadzu Universal Testing Machine. The amount of stress required to maintain this elongation is then recorded every minute for 30 minutes. The resulting data is then plotted on a graph along with "average stress versus time" and "average percent of initial stress versus time." o Two dumbbells are tested from the same sample for each log / batch. If the difference between the two dumbbells is more than 10%, another dumbbell from the same sample is tested. The average result is obtained from the triplicate samples. 〇Calculation: The % of initial stress on the specimen is equal to equation (i) below:
number
[0087] The durability of the gloves was measured by a "tear fixture test" using a tear fixture tester, a device known in the art for measuring resistance to tearing during donning of gloves. The tensile fixture tester is configured to simulate donning activity by counting the number of pulls until the glove is torn. It uses a piston (automatic servo drive system) in the tester to pull the clamped portion of the glove that is worn on the former. The glove is clamped or gripped at the cuff area. As the piston is pulled (horizontally away from the cuff), it stretches the glove, simulating donning activity. The piston retracts to its original position and then pulls another cycle. The distance pulled is 150 mm. This cycle is repeated until the glove is torn and the number of tears is recorded.
[0088] The invention described herein is a glove and a method for forming the same. Although certain embodiments have been described above, other implementations and applications are within the scope of the following claims. Although the invention has been described with reference to certain embodiments, it should be understood that these embodiments are merely illustrative of the principles and applications of the invention. It should therefore be understood that numerous modifications can be made to the exemplary embodiments and other configurations can be devised without departing from the spirit and scope of the invention as defined by the following claims. More specifically, those skilled in the art will recognize that any embodiment described herein is described as having sub-features that the skilled artisan would recognize may advantageously have sub-features of alternative embodiments.
[0089] All publications and references cited herein, including but not limited to patents and patent applications, are hereby incorporated by reference to the same extent as if each reference was individually and specifically indicated to be incorporated by reference and was set forth in its entirety herein. Any patent application to which this application claims priority is also incorporated by reference herein in the manner described above for publications and references.
Claims
1. A non-supportive glove, An outer first layer comprising, in terms of polymer content, 55 wt % or more of chloroprene, 0 wt % to 45 wt % or less of a nitrile rubber including a carboxylated nitrile rubber, and 5 wt % or less of another polymer; A second layer laminated to the outer layer and including a nitrile rubber having a polymer content of 90 wt % or more, The glove has a thickness of 0.11 mm or more and 0.16 mm or less, having an unaged tensile strength of 17 MPa or greater and / or an aged tensile strength of 23 MPa or greater, as determined according to ASTM D412:2016 (E 2021), and containing no accelerators; The non-supportive glove.
2. 10. The unsupported glove of claim 1, wherein the unsupported glove is packaged such that (i) an inner layer is disposed inside an outer layer, or (ii) the inner layer is folded inside the outer layer to facilitate donning of the unsupported glove by a user.
3. 2. The unsupported glove of claim 1, wherein the outer first layer comprises, in polymer content, at least 55 wt. % chloroprene, at least 0 wt. % to at most 45 wt. % nitrile rubber including carboxylated nitrile rubber, and at most 5 wt. % of another polymer, if present.
4. 10. The unsupported glove of claim 1, wherein the durability of the glove is greater than or equal to 350 cycles as determined according to a tear fixture test.
5. 10. The unsupported glove of claim 1, wherein the first layer comprises at least 20 wt. % nitrile rubber in terms of polymer content.
6. 10. The unsupported glove of claim 1, wherein the first layer comprises at least 30 wt% nitrile in polymer content.
7. 2. The non-supported glove of claim 1, wherein the first layer has a thickness of between 0.075 mm and 0.12 mm.
8. 10. The non-supported glove of claim 1, wherein the second layer has a thickness of from 0.05 mm to 0.08 mm.
9. 10. The non-supported glove of claim 1, further comprising a third layer that is thinner than the first and second layers, the third layer being disposed inside the second layer.
10. 10. The unsupported glove of claim 1, wherein the glove has a thickness of 0.12 mm to 0.14 mm.
11. 10. The non-supported glove of claim 1, wherein the glove has a grip of 200 g / f or greater.
12. 10. The non-supported glove of claim 1, wherein the second layer comprises at least 90 wt% nitrile in terms of polymer content.
13. 10. The unsupported glove of claim 1, having an IPA resistance of level 2 or greater.
14. 10. The non-supported glove of claim 1, having a tear strength before aging of 16 N / mm or greater as determined according to ASTM D624 Type C:2000 (R 2020).
15. 10. The non-supported glove of claim 1, having a puncture resistance before aging of 65 N / mm or greater as determined according to SNZ AS / NZS 4179:2014.
16. 10. The non-supported glove of claim 1, having an elongation at break of 650% or greater after or before aging.
17. 2. The unsupported glove of claim 1, having a tensile strength modulus of 7 MPa or less at 500% of that before or after aging.
18. 10. The non-supported glove of claim 1, having a stress retention before aging of 42% or greater.
Citation Information
Patent Citations
Elastomeric article
CN111978608A
Softer Blended Nitrile Elastomeric Article
US20220135776A1
A biodegradable elastomeric film composition and method for producing the same
WO2019074354A1