High-frequency circuit and semiconductor device
Patent Information
- Application Number
- JP2023517405
- Authority / Receiving Office
- JP · JP
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2022-11-07
- Filing Date
- 2022-11-07
- Publication Date
- 2024-10-09
- Estimated Expiration
- 2042-11-07
AI Technical Summary
Thinning the substrate of microwave and millimeter wave circuits to reduce size leads to issues such as conductive resin creeping onto the chip surface, potential short-circuiting, and reduced wire bond strength, making high-yield mounting difficult.
Incorporating convex portions or protrusions along the outer peripheral and/or central portions of the substrate back surface to increase the distance between the bonding material application surface and the substrate top surface, preventing resin creep and facilitating high-yield mounting.
Prevents conductive resin from creeping onto the substrate surface, allowing for miniaturized circuits with stable production and improved mounting yield, while maintaining circuit performance and reducing wafer warping.
Abstract
Description
[Technical Field]
[0001] The present disclosure relates to a high-frequency circuit and a semiconductor device. [Background technology]
[0002] Patent Document 1 discloses a filter having a microstrip line formed thereon. This filter includes a dielectric substrate, a microstrip metal conductor film formed on the front surface of the dielectric substrate, and a back surface metal film formed over the entire back surface of the dielectric substrate. Directly below the microstrip metal conductor film within the dielectric substrate, multiple internal spaces are formed at predetermined intervals along the extension direction of the microstrip metal conductor film. [Prior art documents] [Patent documents]
[0003] [Patent Document 1] Japanese Patent Application Laid-Open No. 2001-320202 Summary of the Invention [Problem to be solved by the invention]
[0004] One way to miniaturize microwave and millimeter-wave circuits is to thin the substrate. For an MMIC that uses microstrip lines for impedance matching, if the substrate is thinned from 100 μm to 50 μm, for example, the width of the microstrip line on the top surface of the chip can be reduced for the same characteristic impedance. This means that the area occupied by the matching circuit can be reduced.
[0005] However, when mounting a chip whose substrate has been thinned from 100 μm to 50 μm using conductive resin, the conductive resin may creep up onto the chip's surface. This can make it difficult to achieve high-yield mounting. Furthermore, the conductive resin creeping up onto the chip's surface can unintentionally short-circuit the pattern, preventing the chip from functioning properly. Furthermore, the conductive resin adhering to the pads can cause problems such as insufficient wire bond strength.
[0006] An object of the present disclosure is to provide a high-frequency circuit and a semiconductor device that can suppress the bonding material from creeping up onto the upper surface of a substrate. [Means for solving the problem]
[0007] A high-frequency circuit according to the present disclosure includes a substrate and a signal line provided on an upper surface of the substrate, and first protrusions are formed along at least two opposing sides of the substrate on an outer periphery of a back surface of the substrate opposite to the upper surface. The first protrusion is formed inside the outermost periphery of the rear surface of the substrate. are. The high-frequency circuit according to the present disclosure comprises: a substrate; and a signal line provided on an upper surface of the substrate, wherein first protrusions are formed along at least two opposing sides of the substrate on an outer periphery of a back surface of the substrate opposite to the upper surface; A second protrusion is formed in the center of the rear surface of the substrate. are. The semiconductor device according to the present disclosure includes: The semiconductor device includes a substrate and a signal line provided on an upper surface of the substrate, and first protrusions are formed along at least two opposing sides of the substrate on the outer periphery of the back surface of the substrate opposite to the upper surface. The device includes a high-frequency circuit, a mounting substrate, and protrusions that are provided on the mounting substrate and fit between the first protrusions of the high-frequency circuit. [Effects of the Invention]
[0008] In the high-frequency circuit according to the present disclosure, when the high-frequency circuit is mounted using a bonding material, the first convex portion can increase the distance from the surface on which the bonding material is applied to the upper surface of the substrate, thereby preventing the bonding material from creeping up onto the upper surface of the substrate. [Brief explanation of the drawings]
[0009] [Figure 1] 1 is a cross-sectional view of a high-frequency circuit according to a first embodiment. [Figure 2]3 is a diagram illustrating the configuration of the back side of the high-frequency circuit according to the first embodiment. FIG. [Figure 3] FIG. 2 is a cross-sectional view of a high-frequency circuit according to a first comparative example. [Figure 4] FIG. 10 is a cross-sectional view of a high-frequency circuit according to a second comparative example. [Figure 5] 1 is a perspective view illustrating a configuration of a semiconductor device according to a first embodiment. [Figure 6] 1 is a side view of a semiconductor device according to a first embodiment. [Figure 7] FIG. 2 is a perspective view illustrating the configuration of a wafer according to the first embodiment. [Figure 8] 3 is a diagram illustrating a state of a protrusion of a wafer before dicing according to the first embodiment. FIG. [Figure 9] 5A and 5B are diagrams illustrating a state after dicing of the convex portions of the wafer according to the first embodiment. [Figure 10] FIG. 10 is a cross-sectional view of a high-frequency circuit according to a second embodiment. [Figure 11] 10 is a diagram illustrating the configuration of the back side of the high-frequency circuit according to the second embodiment. FIG. [Figure 12] FIG. 10 is a perspective view illustrating the configuration of a semiconductor device according to a second embodiment. [Figure 13] FIG. 10 is a side view of a semiconductor device according to a second embodiment. [Figure 14] FIG. 10 is a cross-sectional view of a high-frequency circuit according to a third embodiment. [Figure 15] 10 is a diagram illustrating the configuration of the back side of the high-frequency circuit according to the third embodiment. FIG. [Figure 16] FIG. 10 is an enlarged view of a high-frequency circuit according to a fourth embodiment. [Figure 17] FIG. 10 is an enlarged view of a high-frequency circuit according to a fifth embodiment. [Figure 18] FIG. 13 is a diagram illustrating the configuration of the back side of the high-frequency circuit according to the sixth embodiment. [Figure 19] FIG. 20 is a diagram illustrating the configuration of the back side of a high-frequency circuit according to a modified example of the sixth embodiment. [Figure 20] FIG. 13 is a cross-sectional view of a high-frequency circuit according to a seventh embodiment. [Figure 21] FIG. 13 is a diagram illustrating the configuration of the back side of the high-frequency circuit according to the seventh embodiment. DETAILED DESCRIPTION OF THE INVENTION
[0010] High-frequency circuits and semiconductor devices according to the embodiments will be described with reference to the drawings. The same or corresponding components are designated by the same reference numerals, and repeated description may be omitted.
[0011] Embodiment 1 FIG. 1 is a cross-sectional view of a high-frequency circuit 50 according to the first embodiment. FIG. 2 is a diagram illustrating the configuration of the back side of the high-frequency circuit 50 according to the first embodiment. The high-frequency circuit 50 is, for example, a micro / millimeter wave band MMIC (Monolithic Microwave Integrated Circuit) chip. The high-frequency circuit 50 includes a substrate 10 and a signal line 14 provided on an upper surface 11 of the substrate 10. The substrate 10 is, for example, a SiC substrate. The signal line forms, for example, a microstrip line.
[0012] On the outer periphery of the back surface 12 opposite to the top surface 11 of the substrate 10, protrusions 16 are formed along each of two opposing sides of the substrate 10. In other words, the substrate 10 is thinned, leaving only the portions along the two opposing sides that are the circuit periphery. In this embodiment, no protrusions are formed along the other two sides of the outer periphery of the back surface 12 of the substrate 10 other than the two sides on which the protrusions 16 are formed.
[0013] The length of one side of the high-frequency circuit 50 is, for example, 5 mm or less. The thickness of the thick portion of the substrate 10 is, for example, 100 μm to 200 μm. The thickness of the thinned portion of the substrate 10 is, for example, 50 μm or less, specifically 10 μm to 50 μm. The width of the protrusion 16 is, for example, about 50 to 200 μm.
[0014] Pads 18 are provided on side surfaces 17 of the substrate 10 corresponding to the two sides on which the protrusions 16 are formed. The pads 18 are DC or RF pads. The rear surface 12 of the substrate 10 is covered with a conductor layer 20 that serves as GND.
[0015] FIG. 3 is a cross-sectional view of a high-frequency circuit 50a according to a first comparative example. FIG. 4 is a cross-sectional view of a high-frequency circuit 50b according to a second comparative example. Using FIGS. 3 and 4, miniaturization of a circuit by thinning the substrate will be described. The thickness of the substrate 10a of the high-frequency circuit 50a is 100 μm. A signal line 14 is provided on the top surface of the substrate 10a. A conductor layer 20 serving as GND is provided on the back surface of the substrate 10a. In contrast, the thickness of the substrate 10b of the high-frequency circuit 50b is 50 μm. A signal line 14 is provided on the top surface of the substrate 10b. A conductor layer 20 serving as GND is provided on the back surface of the substrate 10b.
[0016] If the characteristic impedances of the high-frequency circuits 50a and 50b are the same, the width of the signal line 14 of the high-frequency circuit 50b, which has a thinner substrate 10b, will be smaller, and W1 > W2. For example, low-impedance lines are generally used in the output combining circuit of the final stage of a power amplifier. If the line width of the matching circuit can be reduced while maintaining the same characteristic impedance, the area of the output combining circuit can be reduced. This allows for the overall miniaturization of the MMIC.
[0017] However, when a GaN MMIC chip using a SiC substrate thinned to, for example, 50 μm is mounted with conductive resin, the conductive resin may creep up onto the top surface of the chip. In the high-frequency circuit 50b, the distance from the back surface 12, where the conductive resin is provided, to the top surface 11 is reduced from 100 μm to 50 μm. In this case, when the side of the MMIC chip is held with tweezers or a collet, the tip of the tweezers or collet approaches the surface coated with the conductive resin. As a result, the conductive resin is sucked up, increasing the risk of the conductive resin creeping up onto the pattern provided on the top surface of the substrate 10. This can lead to poor mounting yield and make stable production difficult.
[0018] In contrast, in this embodiment, the protrusions 16 can increase the distance from the surface on which the bonding material, such as conductive resin, is applied to the top surface 11 of the substrate 10. As a result, by gripping the two thicker sides of the substrate 10 when mounting the high-frequency circuit 50, the distance from the tip of the tweezers, collet, or the like to the surface on which the conductive resin is applied can be ensured. This makes it possible to prevent the bonding material from creeping up onto the top surface 11 of the substrate 10 via the tweezers, collet, or the like. As described above, in this embodiment, the substrate 10 can be made thinner, thereby miniaturizing the high-frequency circuit 50, and the high-frequency circuit 50 can be mounted with a high yield.
[0019] In this embodiment, the spread of the conductive resin can be confirmed from the two sides of the substrate 10 where the protrusions 16 are not formed. This makes it possible to visually confirm that the die bonding has been performed reliably. Furthermore, by providing the DC or RF extraction pads 18 on the side surfaces 17 of the substrate 10 instead of on the top surface 11, the MMIC chip can be further miniaturized.
[0020] As another comparative example of this embodiment, there is a method of locally thinning the area directly below the microstrip line to widen the selection range of low-impedance or high-impedance lines. Another method is to fill the area directly below the microstrip line with a material with a different dielectric constant than that of the substrate. In such a configuration, it is conceivable that the signal line will branch into multiple lines, like a T-branch structure or a cross-branch structure, at the area where the characteristic impedance changes, specifically at the boundary between the locally thinned area and the thicker area of the substrate. In such a case, parasitic components are added, which may make it difficult to achieve the desired performance in a terahertz waveband circuit.
[0021] For this reason, it is desirable to uniformly thin the central portion of the substrate 10 where the circuit is formed, as in this embodiment. Note that, in FIG. 1 , a portion of the signal line 14 is located directly above the protruding portion 16. If the signal line 14 directly above the protruding portion 16 is a line or pad for applying a DC bias, changes in the characteristic impedance of the signal line 14 generally have little effect on the circuit characteristics. This is because the RF signal component of interest is appropriately processed within the circuit or in a peripheral circuit outside the MMIC. If the signal line 14 directly above the protruding portion 16 is a main line through which the RF signal passes or an RF probe pad, changes in the characteristic impedance, i.e., changes in the distance between the signal line 14 and the GND conductor, may affect the characteristics. Therefore, it may be necessary to understand the effect in advance using electromagnetic field simulations, etc., and then perform appropriate design, such as changing the signal line width. For these reasons, the protruding portion 16 may be located away from the circuit portion, particularly the main line or RF probe pad through which the RF signal passes. Furthermore, the signal line 14 directly above the protrusion 16 may be a line or pad for applying a DC bias.
[0022] Furthermore, by thinning the entire central portion of the substrate 10, the heat dissipation of the transistors can be improved. Furthermore, by thinning the substrate 10, the VH (via hole) diameter can be reduced, making it easier to further miniaturize the circuit. VHs are usually carved by dry etching. Therefore, if the amount of carving, i.e., the substrate thickness, is small, the VH diameter can be reduced.
[0023] FIG. 5 is a perspective view illustrating the configuration of the semiconductor device 100 according to the first embodiment. FIG. 6 is a side view of the semiconductor device 100 according to the first embodiment. FIG. 6 is a view as viewed from direction A in FIG. 5. The semiconductor device 100 includes a high-frequency circuit 50, a mounting substrate 60, and a protrusion 62 provided on the mounting substrate 60. The protrusion 62 is fitted between the convex portions 16 of the high-frequency circuit 50. The protrusion 62 has a shape corresponding to the recess in the rear surface 12 of the substrate 10. An upper surface 63 of the protrusion 62 is a bonding surface with the rear surface 12 of the high-frequency circuit 50, that is, a portion to which a conductive resin is applied. The mounting substrate 60 is also called a die-bond substrate.
[0024] According to the semiconductor device 100 of this embodiment, a large distance can be ensured between the upper surface 63 of the protrusion 62 and the upper surface 11 of the substrate 10 of the high-frequency circuit 50. This makes it possible to prevent the conductive resin from being sucked up by tweezers or the like, and enables high-yield mounting. The height of the protrusion 62 is preferably about 50 μm longer than the dimensions of the recess in the back surface 12 of the high-frequency circuit 50. As a result, most of the conductive resin that protrudes outside the chip will not head toward the tip of the tweezers or the like, but will creep up on the mounting substrate 60 around the protrusion 62. This makes it possible to sufficiently reduce the risk of the conductive resin creeping up onto the upper surface of the chip.
[0025] FIG. 7 is a perspective view illustrating the configuration of a wafer 80 according to the first embodiment. FIG. 7 shows the state before the substrate 10 of this embodiment is separated into chips. The wafer 80 has protrusions 81 and 82, which are thick portions of the wafer 80. The protrusion 81 corresponds to the protrusion 16 of the high-frequency circuit 50. The width of the protrusion 81 is, for example, 100 to 400 μm. The protrusion 82 is a dummy portion provided for the purpose of reinforcing the strength and warping of the wafer 80. The width of the protrusion 82 is, for example, 100 to 400 μm.
[0026] For example, if the entire wafer is thinned to 50 μm or less, warping may occur, making it impossible to secure the wafer to a stage during characteristic testing in the wafer state. Furthermore, attaching the wafer to tape for wafer dicing may be difficult. Furthermore, if a warped wafer is secured to a flat stage, it may break or crack, resulting in reduced yield. Furthermore, substrate thicknesses are sometimes reduced to 30 μm or less to accommodate higher frequencies, such as those in the terahertz waveband (>100 GHz), and to improve heat dissipation. Achieving this substrate thickness with wafers with a diameter of 4 inches or more is even more difficult due to issues such as conductive resin creeping and wafer warpage, as well as reduced strength, which can lead to cracks during wafer handling.
[0027] In contrast to this, in this embodiment, by providing thick portions in a grid pattern on the wafer 80, it is possible to suppress warpage and a decrease in strength of the wafer 80 even when the wafer 80 is thinned. This makes it possible to suppress a decrease in yield due to wafer breakage, wafer cracks, etc. in processes such as characteristic inspection and dicing.
[0028] Fig. 8 is a diagram illustrating the state of the protrusions 81 of the wafer 80 according to the first embodiment before dicing. Fig. 9 is a diagram illustrating the state of the protrusions 81 of the wafer according to the first embodiment after dicing. During dicing, a dimension equivalent to the width of the dicing blade 90 used to cut the wafer 80 is removed. The width of the protrusions 81 in the wafer state is approximately the sum of the width of two protrusions 16 after dicing and the width of the dicing blade 90.
[0029] As a modification of this embodiment, the substrate 10 may be formed from a material other than SiC. Furthermore, the high-frequency circuit 50 is not limited to an MMIC, but may be a matching circuit, a filter, or the like. The bonding material for bonding the high-frequency circuit 50 to the protrusion 62 is not limited to conductive resin, but may be solder, or the like. Furthermore, as will be described in a later embodiment, the protrusions 16 are not limited to being formed on the two opposing sides of the substrate 10, but may also be formed on other sides. In other words, it is sufficient that the protrusions 16 are formed at least along each of the two opposing sides of the substrate 10.
[0030] The above-described modifications can be applied as appropriate to the high-frequency circuits and semiconductor devices according to the following embodiments. Note that the high-frequency circuits and semiconductor devices according to the following embodiments have many points in common with the first embodiment, so the following description will focus on the differences from the first embodiment.
[0031] Embodiment 2 FIG. 10 is a cross-sectional view of a high-frequency circuit 250 according to the second embodiment. FIG. 11 is a diagram illustrating the configuration of the back surface side of the high-frequency circuit 250 according to the second embodiment. In this embodiment, the location where the convex portion 216 is formed differs from that of the first embodiment. The other configurations are the same as those of the first embodiment. In this embodiment, the convex portion 216 is formed along the four sides of the substrate 210 on the outer periphery of the back surface 12 of the substrate 210. In other words, the annular convex portion 216 is formed on the outer periphery of the substrate 210.
[0032] In this embodiment as well, the protrusions 216 can increase the distance from the surface on which the conductive resin is applied to the upper surface of the substrate. This can prevent the bonding material from creeping up onto the upper surface of the substrate 210. This allows the substrate 210 to be made thinner, thereby miniaturizing the high-frequency circuit 50 and enabling the high-frequency circuit 250 to be mounted with a high yield. In this embodiment, the outer periphery of the substrate 210 is thickened on all four sides, so the spread of the conductive resin can be confirmed by the conductive resin spilling out of the substrate 210. The spilled conductive resin appears on the mounting substrate 60.
[0033] FIG. 12 is a perspective view illustrating the configuration of a semiconductor device 200 according to the second embodiment. FIG. 13 is a side view of the semiconductor device 200 according to the second embodiment. In the semiconductor device 200, convex portions 216 provided along the four sides of the substrate 210 surround the protrusions 62 on the mounting substrate 60. This allows the high-frequency circuit 250 to be positioned, improving the positional accuracy of the mounting. In addition, the chip can be held in one of two directions. Therefore, the effects of this embodiment can be obtained even when the chip holding direction is restricted, such as when the mounting space is narrow.
[0034] In this embodiment, the convex portions 216 are formed along the four sides of the substrate 210. Therefore, both of the convex portions 81 and 82 on the wafer 80 shown in FIG.
[0035] Embodiment 3 FIG. 14 is a cross-sectional view of a high-frequency circuit 350 according to the third embodiment. FIG. 15 is a diagram illustrating the configuration of the back side of the high-frequency circuit 350 according to the third embodiment. This embodiment differs from the second embodiment in that the pads 18 are not provided on the side surfaces of the substrate 210. The other configurations are the same as those of the second embodiment. In such a case, the pads 18 are disposed on the upper surface 11 of the substrate 210. Even if the pads 18 are not provided on the side surfaces 17, the effect of suppressing the creeping up of the resin is maintained.
[0036] In this embodiment, an example has been shown in which pads 18 are not provided on side surfaces 17 of substrate 210 of embodiment 2, but pads 18 do not have to be provided on side surfaces 17 of substrate 10 of embodiment 1.
[0037] Embodiment 4 16 is an enlarged view of a high-frequency circuit 450 according to the fourth embodiment. In the high-frequency circuit 450, an RF pad 418 is provided directly on the protrusion 16, not on the side surface 17 of the substrate 10. The other configurations are the same as those of the first embodiment. This makes it possible to reduce the capacitance between the RF pad 418 and the conductor layer 20, thereby improving the accuracy of on-wafer measurement.
[0038] 16, if the signal line 14 is replaced with a transistor, the RF pad 418 becomes the electrode pad of the transistor. In this case, the performance of the transistor can be improved by reducing the pad capacitance. Pads may be provided both on the side surface 17 of the substrate 10 and directly above the protrusion 16.
[0039] Embodiment 5. 17 is an enlarged view of a high-frequency circuit 550 according to the fifth embodiment. In the high-frequency circuit 550, the protrusion 16 is formed inside the outermost periphery of the rear surface 12 of the substrate 510. In other words, the substrate 510 has a thinned inner recess 522 outside the protrusion 16. The inner recess 522 is the portion indicated by the length L1 in FIG. 17. The other configurations are the same as those of the fourth embodiment.
[0040] According to this embodiment, the substrate 510 can be thinned at the cut portion by dicing. Therefore, dicing can be easily performed. Also, the distance from the tip of the tweezers, collet, etc. to the surface to which the conductive resin is applied can be further increased. Therefore, creeping up of the conductive resin can be further suppressed.
[0041] Embodiment 6 18 is a diagram illustrating the configuration of the back side of a high-frequency circuit 650 according to embodiment 6. In high-frequency circuit 650, a convex portion 624 is further formed in the center of back surface 12 of substrate 610. The other configuration is the same as that of embodiment 1. Convex portion 624 extends from one convex portion 16 to the other convex portion 16, for example, in the center in the longitudinal direction of substrate 610.
[0042] In this embodiment, the effect of suppressing wafer warpage can be enhanced. According to this embodiment, a decrease in chip strength can be suppressed, particularly when the thinned region is large. Furthermore, when the aspect ratio of the length-to-width dimensions of the chip is large, forming a protrusion 624 midway along the long side of the chip can suppress a decrease in chip strength.
[0043] 19 is a diagram illustrating the configuration of the back side of a high-frequency circuit 750 according to a modification of embodiment 6. In high-frequency circuit 750, a convex portion 624 is formed in the center of back surface 12 of substrate 710. In this way, convex portion 624 of this embodiment is not limited to convex portion 16 of embodiment 1, and may be combined with convex portion 216 of embodiment 2.
[0044] Embodiment 7 FIG. 20 is a cross-sectional view of a high-frequency circuit 850 according to the seventh embodiment. FIG. 21 is a diagram illustrating the configuration of the back side of the high-frequency circuit 850 according to the seventh embodiment. In the high-frequency circuit 850, a hole 826 is formed on the back surface 12 of the substrate 810, directly below the edge of the signal line 14. The hole 826 is filled with a metal 828. The other configuration is the same as that of the second embodiment. The hole 826 has a diameter of, for example, 15 μm. The multiple holes 826 are formed at intervals of approximately 35 μm.
[0045] The substrates according to the first to sixth embodiments are sufficiently thinned except for the peripheral portions. Furthermore, in this embodiment, holes 826 are formed directly below the edges of the signal line 14 where the electric field concentrates in the microstrip line, thereby carving out the substrate 810. This further increases the capacitance between the substrate 810 and the signal line 14, allowing the low characteristic impedance line to be used as a matching circuit. For example, for a 100 GHz SiC substrate, a quarter wavelength is approximately 250 μm. In this case, by arranging five pairs, or 10 or fewer holes 826, a matching circuit using a quarter wavelength ultra-low impedance microstrip line can be realized.
[0046] Here, holes 826 filled with metal 828 are arranged, but it is also possible to adjust the characteristic impedance by using holes 826 that are not filled with metal 828. Note that holes 826 may be formed in substrate 10 of embodiment 1, not limited to embodiment 2.
[0047] The technical features described in each embodiment may be used in appropriate combination. [Explanation of symbols]
[0048] 10, 10a, 10b substrate, 11 top surface, 12 back surface, 14 signal line, 16 convex portion, 17 side surface, 18 pad, 20 conductor layer, 50, 50a, 50b high frequency circuit, 60 mounting substrate, 62 protrusion, 63 top surface, 80 wafer, 81, 82 convex portion, 90 dicing blade, 100, 200 semiconductor device, 210 substrate, 216 convex portion, 250 high frequency circuit, 350 high frequency circuit, 418 RF pad, 450 high frequency circuit, 510 substrate, 550 high frequency circuit, 610 substrate, 624 convex portion, 650 high frequency circuit, 710 substrate, 750 high frequency circuit, 810 substrate, 826 hole, 828 metal, 850 high frequency circuit
Claims
1. A substrate; A signal line provided on an upper surface of the substrate; Equipped with a first protrusion is formed along at least two opposing sides of the substrate on an outer periphery of a back surface of the substrate opposite to the top surface, The high-frequency circuit according to claim 1, wherein the first convex portion is formed inside an outermost periphery of the back surface of the substrate.
2. 2. The high-frequency circuit according to claim 1, further comprising pads provided on side surfaces of the substrate corresponding to the two sides.
3. 3. The high-frequency circuit according to claim 1, wherein no protrusions are formed along the outer periphery of the rear surface of the substrate along the other two sides of the substrate other than the two sides.
4. 3. The high frequency circuit according to claim 1, wherein a protrusion is formed along four sides of the substrate on an outer periphery of the rear surface of the substrate.
5. 3. The high frequency circuit according to claim 1, further comprising an RF pad provided directly on the first convex portion.
6. A substrate, A signal line provided on an upper surface of the substrate; Equipped with a first protrusion is formed along at least two opposing sides of the substrate on an outer periphery of a back surface of the substrate opposite to the top surface, A high frequency circuit, comprising: a second protrusion formed in a central portion of the rear surface of the substrate.
7. 3. The high-frequency circuit according to claim 1, wherein a hole is formed on the back surface of the substrate directly below an edge portion of the signal line.
8. 8. The high frequency circuit according to claim 7, wherein the holes are filled with a metal.
9. A high-frequency circuit comprising: a substrate; a signal line provided on an upper surface of the substrate; and a first protrusion formed along at least two opposing sides of the substrate on an outer periphery of a back surface of the substrate opposite the upper surface; A mounting board; a protrusion provided on the mounting board and fitted between the first protrusions of the high frequency circuit; A semiconductor device comprising: