Display panel, display device and method of manufacturing a display panel

The display panel design with a dam and extended film layers in the non-display area addresses the vulnerability of OLEDs to moisture and oxygen, enhancing packaging reliability and extending the display panel's lifespan by increasing crack paths and barrier effectiveness.

KR103044606B1Active Publication Date: 2026-11-06비젼녹스 테크놀로지 인크
View PDF 5 Cites 0 Cited by

Patent Information

Application Number
KR1020247025526
Authority / Receiving Office
KR · KR
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-08-02
Filing Date
2023-01-29
Publication Date
2026-11-06
Estimated Expiration
2043-01-29

AI Technical Summary

Technical Problem

OLED displays are susceptible to corrosion by moisture and oxygen, leading to reduced lifespan due to conventional thin-film packaging technology easily separating or breaking under stress, increasing the risk of water vapor intrusion.

Method used

A display panel design with a dam and first blocking part in the non-display area, extending the film layer beyond the dam's outer contours, and incorporating multiple inorganic and organic layers to enhance packaging reliability by increasing the crack path and reducing the risk of cracks extending to the display area.

Benefits of technology

The design improves packaging reliability by increasing the extension length of film layers, reducing the risk of cracks, and enhancing the barrier effect against moisture and oxygen, thus extending the display panel's lifespan.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 112024082205580-PCT00002_ABST
    Figure 112024082205580-PCT00002_ABST
Patent Text Reader

Abstract

The present application provides a display panel, a display device, and a method for manufacturing a display panel. A display panel comprising a display area and a non-display area located on the periphery of the display area comprises a base, a light-emitting element layer, a first blocking part, a dam, and a packaging module. The light-emitting element layer is installed on one side of the base and is located within the display area, and the dam is installed on the same side of the base and is located in the non-display area, and is located on one side of the display area along a first direction parallel to the plane in which the base is located. The first blocking part is installed on one side of the dam facing away from the base, and the first blocking part comprises a first part and a second part located on one side facing away from the base of the first part, and the second part is installed so as to extend at least partially beyond the first part in the first direction. The packaging module is located on one side facing away from the base of the light-emitting element layer, and at least a portion of the film layer of the packaging module extends across the outer contours of the dam, the first part, and the second part to one side facing away from the display area of ​​the first blocking part.
Need to check novelty before this filing date? Find Prior Art

Description

Technology Field

[0001] This application claims priority to Chinese patent application 202210922544.8, filed on August 2, 2022, with the invention title "Display panel, display device and method of manufacturing a display panel," all contents of said application incorporated herein by reference.

[0002] This application relates to the field of display device technology, and in particular to a display panel, a display device, and a method for manufacturing a display panel. Background Technology

[0003] OLED (Organic Light Emitting Diode) displays are self-emissive displays. Compared to LCD (liquid crystal display), OLED displays do not require a backlight, making them thinner and lighter. Additionally, OLED displays have advantages such as high brightness, low power consumption, a wide viewing angle, fast response speed, and a wide operating temperature range, so they are increasingly being applied in various high-performance display fields.

[0004] However, OLED displays are susceptible to corrosion by moisture and oxygen, which shortens their lifespan; typically, thin-film packaging technology is used to block the intrusion of moisture and oxygen. Nevertheless, conventional thin-film packaging technology easily separates or breaks due to factors such as stress during reliability testing, increasing the risk of water vapor intrusion.

[0005] The embodiments of the present application provide a display panel, a display device, and a method for manufacturing a display panel that can improve packaging reliability.

[0006] In a first aspect, an embodiment of the present application provides a display panel having a display area and a non-display area located on the periphery side of the display area, wherein the display panel comprises a base, a light-emitting element layer, a first blocking part, a dam, and a packaging module; the light-emitting element layer is installed on one side of the base and is located within the display area; the dam is installed on the same side of the base and is located in the non-display area and is located on one side of the display area along a first direction parallel to the plane on which the base is located; the first blocking part is installed on one side facing away from the base of the dam and is located on one side of the display area along the first direction and includes a first part and a second part installed on one side facing away from the base of the first part and installed to extend at least partially beyond the first part in the first direction; the packaging module is located on one side facing away from the base of the light-emitting element layer, and at least a portion of the film layer of the packaging module extends from the first blocking part to the side facing away from the display area across the outer contours of the dam, the first part, and the second part.

[0007] In a second aspect, an embodiment of the present application provides a display device comprising a display panel of the above-described embodiment.

[0008] In a third aspect, an embodiment of the present application provides a method for manufacturing a display panel having a display area and a non-display area located on the periphery of the display area, and the manufacturing method is

[0009] A dam is formed on one side of a base, wherein the dam is located within a non-display area and is located on one side of a display area along a first direction parallel to the plane in which the base is located;

[0010] A predetermined film layer is installed on the same side of the base, and the predetermined film layer is patterned to form a first part and a second part that are in contact with each other, wherein the first part is located on the side facing away from the base of the dam, the second part is located on the side facing away from the base of the first part, and the second part extends at least partially beyond the first part in the first direction;

[0011] Forming at least a portion of the structure of the light-emitting element layer on the same side of the base; and

[0012] A packaging module is formed on one side facing away from the base of the light-emitting element layer, wherein at least a portion of the film layer of the packaging module extends from the first blocking portion to the one side facing away from the display area across the outer contours of the dam, the first portion and the second portion.

[0013] Embodiments of the present application provide a display panel, a display device, and a method for manufacturing a display panel. By adding a first blocking portion to the dam of the display panel, the extension length of at least some film layer in the packaging module is increased. Additionally, since a second portion of the first blocking portion is installed to extend at least partially beyond the first portion in a first direction, the extension length can be further increased because the film layer must be bent and extended at a position corresponding to the second portion. Furthermore, if a crack occurs in some film layer of the packaging module, this design increases the path for the crack to extend to the display area, thereby reducing the risk of the crack extending inward to the display area, improving the reliability of the packaging module, and satisfying the packaging requirements of the display panel. Brief explanation of the drawing

[0014] FIG. 1 is a schematic diagram of the structure of a display panel provided by an embodiment of the present application. FIG. 2 is a schematic diagram of the cross-sectional structure in AA of a display panel provided by an embodiment of the present application. FIG. 3 is a schematic diagram of the cross-sectional structure at BB of a display panel provided by an embodiment of the present application. FIG. 4 is a schematic diagram of the cross-sectional structure of another display panel provided by an embodiment of the present application. Figure 5 is a schematic diagram of the enlarged structure of the Q region of Figure 2. FIG. 6 is a schematic diagram of the cross-sectional structure in AA of another display panel provided by an embodiment of the present application. FIG. 7 is a schematic diagram of the cross-sectional structure in AA of another display panel provided by an embodiment of the present application. Figure 8 is a schematic diagram of the enlarged structure of region P in Figure 7. FIG. 9 is a schematic diagram of the cross-sectional structure in AA of another display panel provided by an embodiment of the present application. FIG. 10 is a schematic diagram of the cross-sectional structure at BB of another display panel provided by an embodiment of the present application. FIG. 11 is a schematic diagram of the structure of a display device provided by an embodiment of the present application. FIG. 12 is a flowchart of a method for manufacturing a display panel provided by an embodiment of the present application. FIGS. 13a to 13d are schematic diagrams of the process structure of a method for manufacturing a display panel provided by an embodiment of the present application. FIG. 14 is a schematic diagram of the process structure of a method for manufacturing a display panel provided by an embodiment of the present application. FIG. 15 is a schematic diagram of the process structure of a method for manufacturing a display panel provided by an embodiment of the present application. FIG. 16 is a schematic diagram of the process structure of a method for manufacturing a display panel provided by an embodiment of the present application. Specific details for implementing the invention

[0015] The following describes in detail the configurations of various aspects of the present application and exemplary embodiments. To clarify the purpose, means of technical solution, and advantages of the present application, the present application is described further below in conjunction with the drawings and specific embodiments. It should be understood that the specific embodiments described herein are intended only to interpret the present application and are not intended to limit the present application. Those skilled in the art may practice without the need for some of these specific details of the present application. The description of the embodiments below is merely intended to provide a better understanding of the present application through examples.

[0016] Organic Light-Emitting Diodes (OLEDs) are current-type organic light-emitting devices that emit light through carrier injection and recombination, and can be used as light-emitting elements in display panels. However, when OLEDs are exposed to moisture and air, their performance deteriorates rapidly, which in turn reduces the reliability and lifespan of the display panel; therefore, effective packaging methods must be used to limit the impact of moisture and oxygen penetration on the OLEDs.

[0017] Generally, a packaging module is installed on a light-emitting element to cover it, thereby preventing the intrusion of moisture and oxygen. However, if the elasticity of some film layers in the packaging module is poor, cracks may occur due to factors such as external forces. If these cracks extend inward to the location of the light-emitting element, the module's barrier effect against moisture and oxygen cannot be secured, making it prone to packaging defects and other problems.

[0018] To solve the above problem, an embodiment of the present application provides a display panel. Referring to FIGS. 1 to 3, the display panel comprises a display area (AA) and a non-display area (NA) located on the periphery of the display area (AA). The display panel includes a base (1), a light-emitting element layer (2), a first blocking part (3), a dam (7), and a packaging module (4). The light-emitting element layer (2) is installed on one side of the base (1) and is also located within the display area (AA). The dam (7) is installed on the same side of the base (1) and is located in the non-display area (NA). The dam (7) is located on one side of the display area (AA) along a first direction (X) parallel to the plane in which the base (1) is located. Specifically, the dam (7) may be installed to surround the display area (AA) once.

[0019] The first blocking part (3) is installed on one side facing away from the base (1) of the dam (7), and the first blocking part (3) includes a first part (31) and a second part (32) located on one side facing away from the base (1) of the first part (31), and the second part (32) is installed so as to extend at least partially beyond the first part (31) in the first direction (X).

[0020] The packaging module (4) is located on one side facing away from the base (1) of the light-emitting element layer (2), and at least a portion of the film layer of the packaging module (4) extends across the outer contours of the dam (7), the first part (31) and the second part (32) to one side facing away from the display area (AA) of the first blocking part (3).

[0021] The display panel is divided into a display area (AA) and a non-display area (NA). The display area (AA) refers to an area having a display function, and the embodiments of the present application do not limit the shape and size of the display area (AA). For example, the display area (AA) may have a rectangular or circular structure. The non-display area (NA) is installed to surround the display area (AA). The non-display area (NA) refers to an area that does not have the function of the display area (AA). Generally, various signal wiring is installed within the non-display area (NA) to be used for driving and to implement various functions.

[0022] The light-emitting element layer (2) is located on one side of the base (1) and includes a plurality of light-emitting units (21) for implementing a display effect. For example, the light-emitting element layer (2) includes a red light-emitting unit for emitting red light, a green light-emitting unit for emitting green light, and a blue light-emitting unit for emitting blue light.

[0023] The packaging module (4) is installed to cover the light-emitting element layer (2) and blocks water vapor from entering the interior of the light-emitting element layer (2). The light-emitting element layer (2) is located within the display area (AA), and a part of the packaging module (4) is located within the display area (AA) to cover the light-emitting element layer (2), while another part is located within the non-display area (NA), thereby reducing the risk of moisture and oxygen penetrating into the display area (AA) through the non-display area (NA) of the display panel. Here, the packaging module (4) may include multiple different film layers, and the embodiments of the present application do not limit the number of film layers and the types of film layers within the packaging module (4).

[0024] The dam (7) is installed in the non-display area (NA) and is installed on the same layer as the light-emitting element layer (2). By installing the dam (7), a portion of the film layer of the packaging module (4) is restricted to one side facing the display area (AA) of the dam (7), and the first blocking part (3) is installed on one side facing away from the base of the dam (7), that is, the first blocking part (3) can also be located within the non-display area (NA). Here, the dam (7) can be formed by stacking various film layers; for example, the dam (7) can be formed by stacking an inorganic layer and a metal layer together.

[0025] Since the dam (7) is located on one side of the display area along the first direction (X), the first blocking part (3) is also likewise located on one side of the display area (AA) along the first direction (X), and, for example, the first direction (X) is perpendicular to the thickness direction (Y) of the display panel. The first blocking part (3) includes a first part (31) and a second part (32), the second part (32) is located on one side facing away from the base (1) of the first part (31), i.e., in the thickness direction (Y), and the second part (32) and the base (1) are each located on both sides of the first part (31).

[0026] The second part (32) is installed so as to extend at least partially beyond the first part (31) in the first direction (X), that is, at least part of the orthographic projection of the second part (32) on the base (1) is located outside the orthographic projection of the first part (31) on the base (1). Here, the second part (32) may be installed so as to extend beyond the first part (31) on one side close to the display area (AA) or on one side away from the display area (AA), and the embodiments of the present application are not limited thereto.

[0027] It should be explained that the orthographic projection of the second part (32) on the base (1) may be installed to completely cover and exceed the first part (31), or the orthographic projection of the second part (32) on the base (1) may overlap only with a part of the structure of the first part (31), and the embodiments of the present application are not limited thereto. Furthermore, the size of the second part (32) in the first direction (X) may be larger than the size of the first part (31) in the first direction (X), or may be equal to or smaller than the size of the first part (31) in the first direction (X).

[0028] At least a portion of the film layer of the packaging module (4) extends across the outer contours of the dam (7), the first portion (31), and the second portion (32) to one side facing away from the light-emitting element layer (2) of the first blocking portion (3). Specifically, at least a portion of the film layer in the packaging module (4) is installed to be located within the display area (AA) and to cover the light-emitting element layer (2). The portion of the film layer extends from the display area (AA) to the non-display area (NA) to reach the dam (7), and then extends along the dam (7) to the position where the first portion (31) in the first blocking portion (3) is located. After that, the film layer first extends in a direction away from the base (1) along the outer contour of the first portion (31) to reach the second portion (32), and then continues to extend along the outer contour of the second portion (32), but the second portion (32) is installed so that it extends at least partially beyond the first portion (31) in the first direction (X), so that the film layer is the second The film layer is extended in a curved manner at a position exceeding the first part (31) in part (32), thereby increasing the extension length in the second part (32) of the film layer. Finally, the film layer reaches one side away from the light-emitting element layer (2) of the first part (31), continues to extend along the outer contour of the first part (31) and the dam (7), and finally leaves the first blocking part (3) and the dam (7).

[0029] An embodiment of the present application increases the extension length of at least some film layers in a packaging module (4) by adding a first blocking portion (3) to the dam (7). Additionally, since the second portion (32) in the first blocking portion (3) is installed to extend at least partially beyond the first portion (31) in the first direction (X), the extension length can be further increased as the film layers must be bent and extended at the corresponding position of the second portion (32). Furthermore, if a crack occurs in some film layers of the packaging module (4), this design increases the path for the crack to extend to the display area (AA), thereby reducing the risk of the crack extending inward to the display area (AA), improving the reliability of the packaging module (4) and satisfying the packaging requirements of the display panel.

[0030] It should be explained that the number of dams (7) is multiple, and multiple dams (7) can be installed in a row. Based on this, in addition to including a first blocking part (3), the display panel may include a second blocking part (5) having the same structure as the first blocking part (3), as shown in FIG. 4, and even more blocking parts. Furthermore, the first blocking part (3) may be located on one side close to the display area of ​​the second blocking part (5), or on one side facing away from the display area of ​​the second blocking part (5), and the embodiments of the present application are not limited to all of these.

[0031] In some embodiments, referring to FIGS. 2, 3 and 5, the second part (32) includes a first protrusion (321), and the orthographic projection of the first protrusion (321) on the base (1) is located outside the orthographic projection of the first part (31) on the base (1). The packaging module (4) includes a first inorganic layer (41), and the first inorganic layer (41) includes a first sub-segment (411) and a second sub-segment (412) connected to each other, the first sub-segment (411) is located on one side facing the base (1) of the second part (32), and the orthographic projection of the first sub-segment (411) on the base (1) is located within the orthographic projection of the first protrusion (321) on the base (1). Here, the thickness of at least some of the first sub-segment (411) is thinner than the thickness of the second sub-segment (412).

[0032] The packaging module (4) includes a first inorganic layer (41), a portion of the first inorganic layer (41) is installed to cover the light-emitting element layer (2) within the display area (AA), and another portion is located within the non-display area (NA). At the location of the first blocking portion (3), the first inorganic layer (41) extends along the outer contour of the first portion (31) and the second portion (32), and extends from one side close to the display area (AA) of the first blocking portion (3) to one side away from the display area (AA) of the first blocking portion (3).

[0033] The first protrusion (321) is structured to extend beyond the first part (31) in the second part (32), and in the first direction (X), the orthographic projection of the first protrusion (321) in the base (1) is located on one side of the orthographic projection of the first part (31) in the base (1), and the first protrusion (321) may be located on one side close to the display area (AA) of the first part (31) or on one side farther away from the display area (AA) of the first part (31). Since the first protrusion (321) is installed to protrude from the first part (31) in the first direction (X), the first protrusion (321) and the first part (31) can together form a second receiving space (A2), where the first sub-segment (411) of the first inorganic layer (41) is located within the second receiving space (A2). In FIG. 5, the second receiving space (A2) is illustrated with a dotted box.

[0034] The second sub-segment (412) is connected to the first sub-segment (411), and the second sub-segment (412) includes two parts, one of which is located on one side facing away from the base (1) in the second part (32), and the orthographic projection of the base (1) of the other part is installed adjacent to the orthographic projection of the base (1) of the second part (32) while being offset from the orthographic projection of the base (1) of the second part (32).

[0035] The first inorganic layer (41) is generally manufactured through a method such as chemical vapor deposition, and during the manufacturing process of the first inorganic layer (41), the amount of material deposited in the second receiving space (A2) is reduced due to the blocking of the first protrusion (321), so that the thickness of at least a portion of the first sub-segment (411) formed in the second receiving space (A2) becomes thinner than the thickness of the second sub-segment (412). Furthermore, since it is difficult to continuously mold the material located in the second receiving space (A2), the first sub-segment (411) is formed as a plurality of independent parts.

[0036] Furthermore, since the thickness of at least part of the first sub-segment (411) is thin, even a fracture phenomenon may occur, making it more difficult for a crack to extend inward from the first sub-segment (411), so that when a crack occurs in the first inorganic layer (41), the presence of the first sub-segment (411) further increases the difficulty of the crack extending inward to the display area (AA), thereby improving the packaging reliability of the packaging module (4).

[0037] In some embodiments, the first sub-segment (411) comprises a first segment (411a) bonded to the first protrusion (321), a second segment (411b) bonded to the first part (31) and connected to the first segment (411a), and a third segment (411c) connected to the second segment (411b) and installed opposite the first segment (411a) in the thickness direction (Y), and the thickness of at least one of the first segment (411a), the second segment (411b) and the third segment (411c) is thinner than the thickness of the second sub-segment (412).

[0038] The first division segment (411a) and the third division segment (411c) are both connected to the second sub-segment (412), and the second division segment (411b) integrally connects the first division segment (411a) and the third division segment (411c). The second division segment (411b) is installed to be located on one side of the first part (31) in the first direction (X) and bonded with the first part (31). The second division segment (411b) has a first end and a second end in the thickness direction (Y), the first end is located on one side away from the base (1) of the second end, the first division segment (411a) is connected to the first end, and the third division segment (411c) is connected to the second end.

[0039] During the manufacturing process, the reaction gas diffuses into the second receiving space (A2), is adsorbed onto the surface of the structure, such as the first protrusion and the first part (31), and forms the first divided segment (411a), the second divided segment (411b), and the third divided segment (411c) through a chemical reaction. In this process, due to the blockage of the first protrusion, it becomes difficult for the reaction gas to enter the second receiving space (A2), so that the thickness of at least one of the first divided segment (411a), the second divided segment (411b), and the third divided segment (411c) becomes thinner than the thickness of the second sub-segment (412). Optionally, the thicknesses of the first divided segment (411a), the second divided segment (411b), and the third divided segment (411c) are all thinner than the thickness of the second sub-segment (412).

[0040] In some embodiments, referring to FIGS. 1 and FIGS. 6, the packaging module (4) further includes a first organic layer (42) installed on one side facing away from the base (1) of the first inorganic layer (41), and the first organic layer (42) is located on one side facing the display area (AA) of the first blocking part (3).

[0041] Inorganic materials have a relatively strong ability to block moisture and oxygen, but they are prone to breakage due to their poor elasticity; organic materials have a relatively weak ability to block moisture and oxygen, but the presence of organic materials can reduce the risk of the inorganic materials breaking. Accordingly, the embodiment of the present application improves the packaging effect and reliability of the packaging module (4) by adding a first organic layer (42) based on the first inorganic layer (41).

[0042] The first organic layer (42) can be installed to cover the light-emitting element layer (2), and the first organic layer (42) is located on one side facing the display area (AA) of the first blocking part (3) in the first direction (X). Similar to the dam (7), the installation of the first blocking part (3) can serve to limit the first organic layer (42). Thus, the installation of the first blocking part (3) can increase the blocking height at the position corresponding to the dam (7) on the display panel, thereby further reducing the risk of the first organic layer (42) exceeding the dam (7) and lowering the difficulty of manufacturing the packaging module (4).

[0043] It should be explained that due to the presence of the first organic layer (42), the risk of cracking occurring in the packaging module (4) within the display area (AA) is low. However, on one side of the first blocking part (3) away from the display area (AA), the first organic layer (42) is not present in the packaging module (4), so the first inorganic layer (41) at that location is easily cracked by the action of an external force; however, due to the presence of the first blocking part (3), the risk of the crack in that part extending inward toward the display area (AA) is reduced, thereby improving the reliability of the packaging module (4).

[0044] In some embodiments, referring to FIGS. 7 and FIGS. 8, the packaging module (4) further includes a second inorganic layer (43) located on one side facing away from the base (1) of the first organic layer (42), the first sub-segment (411) is surrounded to form a first receiving space (A1), and the second inorganic layer (43) includes a third sub-segment (431) and a fourth sub-segment (432) connected to each other, and the third sub-segment (431) is located within the first receiving space (A1).

[0045] On one side close to the display area (AA) of the first blocking part (3), the first inorganic layer (41) and the second inorganic layer (43) are each located on both sides of the first organic layer (42) in the thickness direction (Y), and by the first inorganic layer (41) and the second inorganic layer (43) completely covering and coating the first organic layer (42), the flow of the first organic layer (42) can be reduced. In addition, the method of installing the organic layer and the inorganic layer in an overlapping manner can improve the packaging effect of the packaging module (4). On the side far from the display area (AA) of the first blocking part (3), the first organic layer (42) is not present, so the first inorganic layer (41) and the second inorganic layer (43) are installed to be bonded together.

[0046] Referring together with FIG. 5, in the manufacturing process, the second inorganic layer (43) is formed by manufacturing after the first inorganic layer (41) is manufactured, and after the manufacturing of the first inorganic layer (41) is completed, the first segment (411a), the second segment (411b), and the third segment (411c) located within the second receiving space (A2) are surrounded together to form the first receiving space (A1). The third sub-segment (431) of the second inorganic layer (43) is formed within the first receiving space (A1), and, for example, the third sub-segment (431) includes a fourth segment (431a) bonded to the first segment (411a), a fifth segment (431b) bonded to the second segment (411b), and a sixth segment (431c) bonded to the third segment (411c).

[0047] In some embodiments, at least a portion of the thickness of the third sub-segment (431) is thinner than the thickness of the fourth sub-segment (432).

[0048] Similar to the first sub-segment (411), the reaction gas likewise has difficulty entering the first receiving space (A1), so the amount of material deposited in the first receiving space (A1) is reduced, and the thickness of at least part of the third sub-segment (431) formed in the first receiving space (A1) is thinner than the thickness of the fourth sub-segment (432).

[0049] In an embodiment of the present application, the second part (32) is installed to extend at least partially beyond the first part (31) in the first direction (X), thereby increasing the extension length of the first inorganic layer (41) and the second inorganic layer (43). Furthermore, a first sub-segment (411) with a thin thickness can be formed in the first inorganic layer (41), and a third sub-segment (431) with a relatively thin thickness can be formed in the second inorganic layer (43). Since cracks are unlikely to extend from the first sub-segment (411) and the third sub-segment (431), the risk of cracks occurring in the first inorganic layer (41) and the second inorganic layer (43) in the display area (AA) is reduced, and the packaging reliability of the packaging module (4) is improved.

[0050] In some embodiments, the first protrusion (321) is located on one side facing away from the display area (AA) of the first part (31).

[0051] As can be seen from the above, due to the presence of the first protrusion (321), a first sub-segment (411) and a third sub-segment (431) with a thin thickness can be formed in the first inorganic layer (41) and the second inorganic layer (43), respectively, and the first sub-segment (411) and the third sub-segment (431) increase the difficulty of inward extension of cracks, thereby reducing the risk of cracks extending into the display area (AA).

[0052] Furthermore, an embodiment of the present application installs a first protrusion (321) on one side facing away from the display area (AA) of the first part (31), thereby forming a first sub-segment (411) and a third sub-segment (431) on one side facing away from the display area (AA) of the first part (31), thus implementing a crack blockage on the side facing away from the display area (AA) of the first part (31), thereby further reducing the risk of the crack extending to the display area (AA).

[0053] In some embodiments, referring to FIGS. 1 and FIGS. 9, the second part (32) further includes a second protrusion (322), and the second protrusion (322) is located on one side close to the display area (AA) of the first part (31).

[0054] The first protrusion (321) and the second protrusion (322) are located on both sides of the first part (31) in the first direction (X), that is, the size of the second part (32) in the first direction (X) is larger than the size of the first part (31) in the first direction (X). The design of the second protrusion (322) further increases the extension length of the first inorganic layer (41) and the second inorganic layer (43), and additionally, at the corresponding position of the second protrusion (322) and on one side close to the base (1) of the second protrusion (322), the thickness of the first inorganic layer (41) and the second inorganic layer (43) at partial positions is reduced, thereby providing an additional blocking effect against cracks and improving the reliability of the packaging module (4). Optionally, the first protrusion (321) and the second protrusion (322) are distributed axially.

[0055] In some embodiments, with reference to FIGS. 1, FIGS. 3 and FIGS. 9, the display panel further comprises a pixel defining layer (6), the pixel defining layer (6) comprises a plurality of first openings (61), a plurality of light-emitting layers (211) of the light-emitting element layer (2) are accommodated within the first openings (61), and the pixel defining layer (6) comprises an inorganic material.

[0056] The dam (7) includes a third part (71), and the third part (71) is installed in the same layer with the same material as the pixel definition layer (6) and is installed to be bonded with the first inorganic layer (41).

[0057] In the related technology, the inorganic layer of the packaging module (4) is mainly linked with metal and also linked with an organic film layer. However, due to differences in materials, the adhesion between the inorganic layer of the packaging module (4) and the metal or organic film layer is poor, so the problem of film layer separation is likely to occur due to the influence of external force.

[0058] In an embodiment of the present application, the first opening (61) of the pixel definition layer (6) limits the light-emitting layer (211) of the light-emitting element layer (2). The light-emitting layer (211) is a part of the light-emitting unit (21), and, exemplarily, the light-emitting unit (21) further includes a first electrode located on one side facing away from the base (1) of the light-emitting layer (211) and a second electrode (212) located on one side facing the base (1) of the light-emitting layer (211).

[0059] Inorganic material is included within the pixel definition layer (6), and additionally, the third part (71) of the dam (7) is installed in the same layer with the same material as the pixel definition layer (6). Therefore, the third part (71) can be manufactured in the same process as the pixel definition layer (6), thereby reducing the complexity of the process, and the third part (71) likewise includes inorganic material.

[0060] The third part (71) and the first inorganic layer (41) are both inorganic materials and are installed to bond together. This design can improve the adhesion effect between the dam (7) and the first inorganic layer (41), thereby reducing the risk of the two separating and improving the reliability of the internal structure of the display panel. Optionally, the pixel definition layer (6) comprises at least one of silicon nitride and silicon oxide. Furthermore, the first inorganic layer (41) may comprise at least one of silicon nitride and silicon oxide.

[0061] In some embodiments, referring to FIGS. 9 and FIGS. 10, the display panel further includes a limiting part (9) installed on one side facing away from the base (1) of the pixel definition layer (6) located within the display area (AA), and the limiting part (9) includes a first sub-limiting part (91) and a second sub-limiting part (92) located on one side facing away from the base (1) of the first sub-limiting part (91), the first sub-limiting part (91) is installed on the same layer with the same material as the first part (31), and the second sub-limiting part (92) is installed on the same layer with the same material as the second part (32).

[0062] The limiting part (9) is located on one side facing away from the base (1) of the pixel definition layer (6), and the installation of the limiting part (9) can increase the height of the position of the pixel definition layer (6) of the display panel. When the packaging module (4) packages the light-emitting unit (21), the presence of the limiting part (9) divides at least some of the structure of the packaging module (4) into packaging parts installed independently of each other, thereby preventing water vapor, etc. from spreading between the independent packaging parts and further improving the packaging effect.

[0063] In addition, since the first sub-limiting part (91) is installed on the same layer with the same material as the first part (31), the first sub-limiting part (91) can be manufactured and molded in the same process as the first part (31); and since the second sub-limiting part (92) is installed on the same layer with the same material as the second part (32), the second sub-limiting part (92) can be manufactured and molded in the same process as the second part (32), thereby simplifying the manufacturing process of the display panel and improving manufacturing efficiency.

[0064] In some embodiments, the second sub-limiting portion (92) is installed to extend at least partially beyond the first sub-limiting portion (91) in the first direction (X). The structure of the limiting portion (9) and the structure of the first blocking portion (3) are similar. During the manufacturing process of the packaging module (4), at least some film layers of the packaging module (4) are partitioned by the limiting portion (9) to form a plurality of packaging structures corresponding to the light-emitting unit (21), thereby enabling independent packaging for each light-emitting unit (21) and further enhancing the packaging effect.

[0065] In addition, the presence of the limiting portion (9) can also reduce the risk of leakage current occurring in the horizontal direction of adjacent light-emitting units. Specifically, in the manufacturing process of a display panel, a pixel defining layer (6) is generally formed first, then a limiting portion (9) is formed on the pixel defining layer (6), and then film layers such as a light-emitting layer (211), a hole transport layer (not shown), and an electron transport layer (not shown) are formed between adjacent limiting portions (9). Since the second sub-limiting section (92) of the limiting section (9) is installed to extend at least partially beyond the first sub-limiting section (91) in the first direction (X), the second sub-limiting section (92) is partially suspended in the air relative to the first sub-limiting section (91). Since it is difficult for the light-emitting layer (211), the hole transport layer, and the electron transport layer to rise to the position suspended in the air, a breakage occurs. That is, the presence of the limiting section (9) divides the film layers, such as the light-emitting layer (211), the hole transport layer, and the electron transport layer, into separate structures, thereby reducing the risk of leakage current occurring in the horizontal direction of these film layers.

[0066] In some embodiments, the light-emitting element layer (2) further includes a first electrode layer (8) installed on one side facing away from the base (1) of the light-emitting layer (211), the first electrode layer (8) includes a plurality of first electrodes (81), the limiting portion (9) forms a plurality of second openings (93), the material of the first sub-limiting portion (91) and / or the second sub-limiting portion (92) includes a metal material, and two adjacent first electrodes (81) are connected to each other through the limiting portion (9).

[0067] Since metal materials generally have conductivity, adjacent first electrodes (81) can implement signal transmission through the limiting portion (9). In an embodiment of the present application, a plurality of first electrodes (81) are spaced apart from each other through the limiting portion (9) and also interconnected through the limiting portion (9), that is, the plurality of first electrodes (81) together with the limiting portion (9) form a common electrode for driving the light emission of the light-emitting layer (211).

[0068] In some embodiments, the material of the first sub-limiting part (91) includes a metal material, and the material of the second sub-limiting part (92) includes an inorganic material.

[0069] Since the first sub-limiting portion (91) includes a metal material, the adjacent first electrode (81) can conduct through the first sub-limiting portion (91). Based on this, in the embodiment of the present application, the material of the second sub-limiting portion (92) includes an inorganic material, so the second sub-limiting portion (92) is securely adhered to a part of the inorganic film layer of the packaging module (4), thereby improving the reliability of the packaging.

[0070] In a second embodiment, with reference to FIG. 11, an embodiment of the present application provides a display device comprising a display panel of any one of the aforementioned embodiments.

[0071] It should be explained that the display device provided by the embodiment of the present application has the beneficial effects of the display panel of any one of the aforementioned embodiments; therefore, please refer specifically to the description of the aforementioned display panel, and the embodiment of the present application is not described repeatedly here.

[0072] In a third embodiment, with reference to FIG. 12 and FIG. 13, an embodiment of the present application provides a method for manufacturing a display panel, wherein the display panel comprises a display area (AA) and a non-display area (NA) located on the periphery of the display area (AA), and the manufacturing method comprises the following steps.

[0073] In S100, a dam is formed on one side of the base, wherein the dam is located within the non-display area and is located on one side of the display area along a first direction parallel to the plane where the base is located.

[0074] In S100, referring to FIG. 13a, the dam (7) is installed in the non-display area (NA), and the installation of the dam (7) can isolate a part of the film layer of the packaging module on one side close to the display area (AA) of the dam (7) when manufacturing the packaging module later.

[0075] In S110, a pre-set film layer is installed on the same side of the base, and the pre-set film layer is patterned to form a first part and a second part that are in contact with each other, wherein the first part is located on the side facing away from the base of the dam, the second part is located on the side facing away from the base of the first part, and the second part extends at least partially beyond the first part in the first direction.

[0076] In S110, referring to FIG. 13b, a pre-set film layer (not shown) and a dam (7) are formed on the same side of the base (1), and the pre-set film layer forms a first part (31) and a second part (32). Specifically, the pre-set film layer includes two parts installed in a stacked manner, and the materials of the two parts may be the same or different from each other. Since the second part (32) to be formed by the pre-set film layer must be installed so as to extend beyond the first part (31) in the first direction (X), the pre-set film layer must first be patterned through a process such as etching to form the second part (32) in comparison with the first part (31). Then, the pre-set film layer is patterned through a process such as etching to form the first part (31).

[0077] It should be explained that the second part (32) may be installed so as to exceed the first part (31) on one side close to the display area, and may also be installed so as to exceed the first part (31) on one side away from the display area, and the embodiments of the present application are not limited thereto.

[0078] In S120, at least a portion of the structure of the light-emitting element layer is formed on the same side of the base.

[0079] In S120, with reference to FIG. 13c, a light-emitting element layer (2) is formed within a display area (AA), wherein the light-emitting element layer (2) includes a plurality of light-emitting units (21), and the plurality of light-emitting units (21) include a red light-emitting unit that emits red light, a blue light-emitting unit that emits blue light, and a green light-emitting unit that emits green light, but are not limited thereto.

[0080] It should be explained that the light-emitting element layer (2) includes a multilayer structure, wherein the structure of some film layers may be formed after step S110, and the structure of some film layers may be formed before step S110, and the embodiments of the present application are not limited thereto.

[0081] In S130, a packaging module is formed on one side facing away from the base of the light-emitting element layer, and at least a portion of the film layer of the packaging module extends across the outer contours of the dam, the first part and the second part to one side facing away from the display area of ​​the first blocking part.

[0082] In S130, with reference to FIG. 13d, at least a portion of the film layer of the packaging module (4) is bonded to the dam (7), the first portion (31), and the second portion (32) and extends to one side facing away from the display area of ​​the first blocking portion (3). In this process, the second portion (32) is installed to extend at least partially beyond the first portion (31) in the first direction (X), thereby increasing the extension length corresponding to at least a portion of the film layer of the packaging module (4). Furthermore, if a crack occurs in a portion of the film layer of the packaging module (4), this design increases the path for the crack to extend to the display area, thereby reducing the risk of the crack extending inward to the display area, improving the reliability of the packaging module (4) and satisfying the packaging requirements of the display panel.

[0083] In some embodiments, referring to FIG. 13a and FIG. 14, the dam (7) includes a third part (71), and step S100 includes forming a pixel defining material layer on one side of the base (1) and patterning the pixel defining material layer to form a pixel defining layer (6) and a third part (71), wherein the pixel defining layer (6) includes a plurality of first openings (61) located within a display area (AA).

[0084] A pixel defining material layer (not shown) may form a pixel defining layer (6) and simultaneously form a third part (71) of a dam (7), thereby reducing the manufacturing process. Here, the pixel defining layer (6) is located within a display area (AA), and the first opening (61) of the pixel defining layer (6) limits the light-emitting layer (211) of the light-emitting element layer (2). Furthermore, optionally, the material of the pixel defining material layer includes an inorganic material, that is, the third part (71) includes an inorganic material, and this design is advantageous for enabling the inorganic layer of the packaging module to achieve better adhesion with the dam (7), thereby improving the reliability of the packaging module (4).

[0085] Referring to FIG. 15, step S110 comprises patterning a preset film layer to form a first sub-limiting part (91) and a second sub-limiting part (92) that are in contact with each other, wherein the first sub-limiting part (91) is located on one side facing away from the base (1) of the pixel definition layer (6), and the second sub-limiting part (92) is located on one side facing away from the base (1) of the first sub-limiting part (91), and the first sub-limiting part (91) and the second sub-limiting part (92) together form a plurality of second openings (93).

[0086] The first sub-limiting portion (91) and the second sub-limiting portion (92) are both located within the display area (AA) and restrictively form a plurality of second openings (93) for manufacturing a light-emitting element layer. The second sub-limiting portion (92) is located on one side facing away from the base (1) of the first sub-limiting portion (91), and optionally, the second sub-limiting portion (92) is installed to extend at least partially beyond the first sub-limiting portion (91) in the first direction (X).

[0087] The first sub-limiting part (91) is installed on the same layer with the same material as the first part (31), and the first sub-limiting part (91) and the first part (31) can be manufactured and molded in the same process; the second sub-limiting part (92) is installed on the same layer with the same material as the second part (32), and the second sub-limiting part (92) and the second part (32) can be manufactured and molded in the same process, so the manufacturing process of the display panel can be simplified and manufacturing efficiency can be improved.

[0088] Referring to FIG. 16, the light-emitting element layer (2) includes a plurality of first electrodes (81), and step S120 includes forming the first electrodes (81) within the second opening (93).

[0089] A plurality of second openings (93) can form a plurality of first electrodes (81), and the first sub-limiting portion (91) and the second sub-limiting portion (92) can partition and separate the plurality of first electrodes (81). Optionally, at least one of the first sub-limiting portion (91) and the second sub-limiting portion (92) includes a metal material, that is, at least one of the first sub-limiting portion (91) and the second sub-limiting portion (92) can implement the transmission of an electrical signal. Based on this, the first sub-limiting portion (91) and the second sub-limiting portion (92) can implement mutual conduction between the plurality of first electrodes (81), that is, at least one of the first sub-limiting portion (91) and the second sub-limiting portion (92) can form a common electrode together with the plurality of first electrodes (81).

[0090] It should be explained that after forming the first sub-limiting part (91) and the second sub-limiting part (92), and before forming the first electrode (81), a plurality of functional film layers, such as a hole transport layer, a light-emitting layer (211), and an electron transport layer of the light-emitting unit (21), can be formed sequentially within the first opening (61) and the second opening (93).

[0091] Although embodiments of the present application have been disclosed as described above, the above description is merely for the purpose of aiding understanding of the present application and is not intended to limit the present application. A person skilled in the art to which the present application pertains may modify and change the forms and details of the implementations without departing from the spirit and scope disclosed in the present application, and the scope of protection of the present application shall be based on the scope defined by the appended claims.

Claims

Claim 1 A display panel comprising a display area and a non-display area located on the periphery side of the display area, the display panel comprising: a base; a light-emitting element layer installed on one side of the base and also located in the display area; a dam installed on the same side of the base and located in the non-display area, and located on one side of the display area along a first direction parallel to the plane on which the base is located; a first blocking part installed on one side of the dam facing away from the base, and including a first part and a second part located on the side facing away from the base of the first part and installed to protrude at least partially from the first part in the first direction; a packaging module located on the side facing away from the base of the light-emitting element layer, wherein at least a portion of the film layer of the packaging module extends across the outer contours of the dam, the first part, and the second part to the side facing away from the display area of ​​the first blocking part; and a pixel defining layer comprising a plurality of first openings, wherein the plurality of light-emitting layers of the light-emitting element layer are accommodated within the first openings. A display panel comprising a limiting portion located within the display area and installed on one side facing away from the base of the pixel definition layer, wherein the limiting portion includes a first sub-limiting portion and a second sub-limiting portion located on one side facing away from the base of the first sub-limiting portion, wherein the second sub-limiting portion is installed to protrude at least partially from the first sub-limiting portion in the first direction, and wherein the limiting portion divides at least a part of the structure of the packaging module into packaging portions installed independently of each other. Claim 2 In claim 1, the second part comprises a first protrusion, and the orthographic projection of the first protrusion on the base is located outside the orthographic projection of the first part on the base; the packaging module comprises a first inorganic layer, the first inorganic layer comprises a first sub-segment and a second sub-segment connected to each other, the first sub-segment is located on one side of the second part facing the base, and the orthographic projection of the first sub-segment on the base is located within the orthographic projection of the first protrusion on the base; and a display panel in which at least some of the thickness of the first sub-segment is thinner than the thickness of the second sub-segment. Claim 3 In paragraph 2, the first sub-segment comprises a first segmented segment bonded to the first protrusion, a second segmented segment bonded to the first portion and connected to the first segmented segment, and a third segmented segment connected to the second segmented segment and installed opposite to the first segmented segment in the thickness direction of the base, wherein the thickness of at least one of the first segmented segment, the second segmented segment and the third segmented segment is thinner than the thickness of the second sub-segment. Claim 4 In paragraph 2, the packaging module further comprises a first organic layer installed on one side facing away from the base of the first inorganic layer, and the first organic layer is located on one side facing the display area of ​​the first blocking part, and the packaging module further comprises a second inorganic layer located on one side facing away from the base of the first organic layer; the first sub-segment is surrounded to form a first receiving space, and the second inorganic layer comprises a third sub-segment and a fourth sub-segment connected to each other, the third sub-segment is located within the first receiving space, and at least a portion of the thickness of the third sub-segment is thinner than the thickness of the fourth sub-segment, forming a display panel. Claim 5 In paragraph 2, the first protrusion is located on one side facing away from the display area of ​​the first part, the second part further includes a second protrusion, the second protrusion is located on one side close to the display area of ​​the first part, and the first protrusion and the second protrusion are distributed axially. Claim 6 In paragraph 2, the pixel defining layer comprises an inorganic material; the dam comprises a third part, the third part is installed on the same layer with the same material as the pixel defining layer and is installed to be bonded with the first inorganic layer, the pixel defining layer comprises at least one of silicon nitride and silicon oxide, the first sub-limiting part is installed on the same layer with the same material as the first part, and the second sub-limiting part is installed on the same layer with the same material as the second part, forming a display panel. Claim 7 In claim 6, the light-emitting element layer further comprises a first electrode layer installed on one side facing away from the base of the light-emitting layer, and the first electrode layer comprises a plurality of first electrodes; the material of the first sub-limiting portion and / or the second sub-limiting portion comprises a metal material, and two adjacent first electrodes are connected to each other through the limiting portion, or the material of the first sub-limiting portion comprises a metal material and the material of the second sub-limiting portion comprises an inorganic material, a display panel. Claim 8 A display device comprising a display panel according to any one of claims 1 to 7. Claim 9 A method for manufacturing a display panel having a display area and a non-display area located on the periphery of the display area, wherein a dam is formed on one side of a base, the dam is located within the non-display area and is located on one side of the display area along a first direction parallel to the plane on which the base is located, and a pixel defining material layer is installed on one side of the base, and the pixel defining material layer is patterned to form a pixel defining layer, wherein the pixel defining layer includes a plurality of first openings located within the display area; A pre-set film layer is installed on the same side of the base, and the pre-set film layer is patterned to form a first part and a second part that are in contact with each other, wherein the first part is located on the side facing away from the base of the dam, the second part is located on the side facing away from the base of the first part, and the second part protrudes at least partially from the first part in the first direction, and the same side is the same side as the side where the dam is installed, and the pre-set film layer is patterned to form a first sub-limiting part and a second sub-limiting part that are in contact with each other, wherein the first sub-limiting part is located on the side facing away from the base of the pixel definition layer, the second sub-limiting part is located on the side facing away from the base of the first sub-limiting part, and the second sub-limiting part is installed to protrude at least partially from the first sub-limiting part in the first direction, and the limiting part includes the first sub-limiting part and the second sub-limiting part; and at least a part structure of a light-emitting element layer is formed on the same side of the base.A method for manufacturing a display panel comprising forming a packaging module on one side facing away from the base of the light-emitting element layer, wherein at least a portion of the film layer of the packaging module extends across the outer contours of the dam, the first portion, and the second portion to one side facing away from the display area of ​​the first blocking portion, and wherein the limiting portion divides at least a portion of the structure of the packaging module into packaging portions installed independently of each other. Claim 10 A method for manufacturing a display panel according to claim 9, wherein the dam comprises a third part, and forming the dam on one side of the base comprises patterning the pixel defining material layer to form the pixel defining layer and the third part, and installing a predetermined film layer on the same side of the base and patterning the predetermined film layer comprises the first sub-limiting part and the second sub-limiting part together forming a plurality of second openings; and the light-emitting element layer comprises a plurality of first electrodes, and forming at least a part structure of the light-emitting element layer on the same side of the base comprises forming the first electrode within the second opening. Claim 11 delete Claim 12 delete Claim 13 delete Claim 14 delete Claim 15 delete Claim 16 delete Claim 17 delete Claim 18 delete Claim 19 delete

Citation Information

Patent Citations

  • Display panel and electronic device having the same

    KR1020190094269A

  • Organic light-emitting display device and method of manufacturing the same

    KR1020190096467A

  • Display substrate and its manufacturing method and display device

    KR1020190141224A

  • Organic light emitting display device

    KR1020200044520A

  • Display substrate and method for manufacturing the same, display device

    US20220045300A1