Method for manufacturing a semiconductor substrate and apparatus for manufacturing, and control device

By employing light interference to control growth conditions in the ELO method, the method addresses yield issues in semiconductor substrate manufacturing, resulting in high-quality, low-defect nitride semiconductor layers.

KR103044624B1Active Publication Date: 2026-11-06KYOCERA CORP
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
KR1020247024650
Authority / Receiving Office
KR · KR
Patent Type
Patents
Current Assignee / Owner
Priority Date
2022-01-27
Filing Date
2023-01-26
Publication Date
2026-11-06
Estimated Expiration
2043-01-26

AI Technical Summary

Technical Problem

Existing methods for manufacturing semiconductor substrates using the ELO method face challenges in controlling the transition timing between longitudinal and transverse growth conditions, leading to decreased manufacturing yield due to scattering in deposition rates, which affects dislocation density and aspect ratio.

Method used

The method employs the use of light with specific wavelengths absorbed by the nitride semiconductor during growth to monitor the growth state and transition conditions, utilizing the interference of reflected light from the semiconductor and mask surfaces to control the growth direction, transitioning from vertical to horizontal growth at optimal times.

Benefits of technology

This approach enhances the manufacturing yield by reducing defects and improving crystallinity of the nitride semiconductor layer, allowing for cost-effective production of thin, wide, and low-defect semiconductor substrates.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 112024079270319-PCT00003_ABST
    Figure 112024079270319-PCT00003_ABST
Patent Text Reader

Abstract

A method for manufacturing a semiconductor substrate, comprising: a process of growing a nitride semiconductor portion (8) from the upper surface of a base substrate (BS) exposed to an opening (KS) of a mask (6); a process of irradiating a mask portion (5) and a nitride semiconductor portion (8) during growth with a first light (L1) having a wavelength absorbed by the nitride semiconductor portion at a growth temperature; a process of receiving a second light (L2) from a semiconductor substrate (10); and a process of transitioning from a first condition of growth conditions of the nitride semiconductor portion (8) to a second condition.
Need to check novelty before this filing date? Find Prior Art

Description

Technology Field

[0001] The present disclosure relates to a method for manufacturing a semiconductor substrate, a manufacturing apparatus, and a control apparatus. Background Technology

[0002] Patent Document 1 discloses a method for forming a GaN-based semiconductor layer on a GaN-based substrate or a heterogeneous substrate (e.g., a sapphire substrate) using the ELO (Epitaxial Lateral Overgrowth) method. Prior art literature

[0003] Japanese Patent Publication No. 2013-251304

[0004] The present disclosure includes a method for manufacturing such a semiconductor substrate comprising: a process of preparing a base substrate and a template substrate having a mask portion and an opening portion located on the base substrate; a process of growing a nitride semiconductor portion from the base substrate exposed to the opening portion; a process of irradiating a semiconductor substrate including the template substrate and the nitride semiconductor portion being grown with a first light having a wavelength absorbed by the nitride semiconductor portion at the growth temperature of the nitride semiconductor portion; a process of receiving a second light from the semiconductor substrate; and a process of performing a growth condition for the nitride semiconductor portion. Brief explanation of the drawing

[0005] FIG. 1 is a cross-sectional view showing the configuration of a semiconductor substrate according to the present embodiment. FIG. 2 is a flowchart illustrating a method for manufacturing a semiconductor substrate according to the present embodiment. FIG. 3 is a cross-sectional view showing a method for manufacturing a semiconductor substrate according to the present embodiment. Figure 4 is a graph showing the temporal change in reflectance and set temperature, which is the ratio of the intensity of the second light to the intensity of the first light. Figure 5 is a graph showing the temporal change in reflectance and relative level, which is the ratio of the intensity of the second light to the intensity of the first light. Figure 6 is a plan view showing an example of a mask. Figure 7 is a cross-sectional view showing an example of the configuration of a base substrate. FIG. 8 is a schematic diagram showing the configuration of a semiconductor substrate manufacturing apparatus according to the present embodiment. FIG. 9 is a cross-sectional view illustrating a method for manufacturing such a semiconductor substrate in Example 1. FIG. 10 is a cross-sectional view illustrating a method for manufacturing such a semiconductor device in Example 2. FIG. 11 is a cross-sectional view showing a method for manufacturing a semiconductor substrate according to the present embodiment. Specific details for implementing the invention

[0006] (Semiconductor substrate)

[0007] FIG. 1 is a cross-sectional view showing the configuration of a semiconductor substrate according to the present embodiment. As shown in FIG. 1, the semiconductor substrate (10) (semiconductor wafer) according to the present embodiment comprises a base substrate (BS), a mask (mask pattern) (6) formed on the base substrate and having an opening (KS) and a mask portion (5), and a nitride semiconductor portion (8) disposed extending from above the base substrate (BS) exposed at the opening (KS) to above the mask portion (5). The mask (5) may be a mask layer, and the nitride semiconductor portion (8) may be a nitride semiconductor layer.

[0008] The nitride semiconductor part (8) includes a nitride semiconductor as the main material. The nitride semiconductor can be represented, for example, as AlxGayInzN (0≤x≤1; 0≤y≤1; 0≤z≤1; x+y+z=1), and specific examples include GaN-based semiconductor, AlN (aluminum nitride), InAlN (indium aluminum nitride), and InN (indium nitride). A GaN-based semiconductor is a semiconductor containing gallium atoms (Ga) and nitrogen atoms (N), and typical examples include GaN, AlGaN, AlGaInN, and InGaN.

[0009] The nitride semiconductor part (8) may be a doped type (e.g., n-type including a donor) or a non-doped type. A semiconductor substrate means a substrate containing a nitride semiconductor, and the base substrate (BS) may contain a semiconductor other than a nitride semiconductor (e.g., silicon-based semiconductor, SiC, gallium oxide) or a non-semiconductor (sapphire). There is a case where the base substrate (BS) and the mask (6) are included and called a template substrate (TS).

[0010] The nitride semiconductor part (8) can be formed by the ELO (Epitaxial Lateral Overgrowth) method starting from the base substrate (BS) exposed from the opening (KS). The thickness direction of the nitride semiconductor part (8) is the c-axis direction ( <0001> It may be a direction. The opening (KS) has a long shape, and its width direction may be the a-axis direction (<11-20> direction) of the nitride semiconductor part (8). In the semiconductor substrate (10), the direction from the base substrate (BS) to the nitride semiconductor part (8) is "upward." Viewing an object with a line of sight parallel to the normal direction of the semiconductor substrate (10) (including cases of perspective) is sometimes referred to as "viewing in a plane."

[0011] (Method for manufacturing a semiconductor substrate)

[0012] FIG. 2 is a flowchart illustrating a method for manufacturing a semiconductor substrate according to the present embodiment. FIG. 3 is a cross-sectional view illustrating a method for manufacturing a semiconductor substrate according to the present embodiment. FIG. 4 is a graph showing the temporal change of reflectance, which is the ratio of the intensity of the second light to the intensity of the first light, and the set temperature.

[0013] As shown in FIGS. 2 to 4, the method for manufacturing a semiconductor substrate of the present embodiment comprises the steps of: preparing a base substrate (BS) and a template substrate (TS) having a mask (mask pattern) (6) located on the base substrate (BS) and including a mask portion (5) and an opening portion (KS); growing a nitride semiconductor portion (8) from the upper surface (lower layer (4)) of the base substrate (BS) exposed to the opening portion (KS); irradiating a semiconductor substrate (10) including the template substrate (TS) and the nitride semiconductor portion (8) during growth with a first light (L1) having a wavelength absorbed by the nitride semiconductor portion (8) at the growth temperature of the nitride semiconductor portion (8); receiving a second light (L2) from the semiconductor substrate (10); and performing a process of transitioning the growth conditions of the nitride semiconductor portion (8) (transitioning from the first condition to the second condition).

[0014] The first light (L1) of Fig. 3, etc. may be irradiated onto the nitride semiconductor part (8) and the mask part (5). The second light (L2) includes the reflected light of the first light (L1) from the upper surface of the nitride semiconductor part (8) and the reflected light of the first light (L1) from the upper surface of the mask part (5), and the transition from the first condition of growth conditions to the second condition may be initiated using the second light (L2).

[0015] With the thickness direction of the mask portion (5) as the vertical direction and the width direction of the mask portion (5) as the horizontal direction, the first condition may be a condition that prioritizes the vertical growth (growth in the c-axis direction) of the nitride semiconductor portion (8), and the second condition may be a condition that prioritizes the horizontal growth (growth in the a-axis direction) of the nitride semiconductor portion (8). The wavelength of the first light (L1) may be included in the wavelength range of 395 to 415 nm.

[0016] Using the intensity of the second light (L2), the relative level (SL) of the nitride semiconductor part (8) based on the upper surface level (UL) of the mask part (5) may be detected over time, and the implementation of the growth condition may be started at the timing when the relative level (SL) reaches a specified value.

[0017] For example, after the growth of the nitride semiconductor part (8) begins, the growth condition may be transitioned to a second growth condition at a timing (tc) when the relative level (SL) is negative under the first growth condition (a period when the thickness of the nitride semiconductor part (8) is thinner than the mask part (5)) and the relative level (SL) becomes zero. After the transition, growth may be carried out under the second condition. In this case, the specified value becomes 0. Additionally, the transition may be initiated immediately after the timing when the relative level (SL) becomes zero. In this case, the specified value becomes a positive value.

[0018] The reflectance, which is the ratio of the intensity of the second light (L2) to the intensity of the first light (L1), may be acquired over time. In this case, the reflectance may vary periodically (the appearance of fringe). Additionally, the intensity of the second light (L2) (reflected light intensity) may be acquired over time with the intensity of the first light (L1) set to a fixed value, in which case the intensity of the second light (L2) (reflected light intensity) varies periodically.

[0019] FIG. 5 is a graph showing the temporal change of reflectance and relative level, which is the ratio of the intensity of the second light to the intensity of the first light. As shown in FIG. 5, the number of cycles obtained along the time series may correspond to the relative level (SL). The amount of increase in the relative level (SL) per cycle may be a value based on the wavelength of the first light (L1) and the optical characteristics of the mask portion (5) and the nitride semiconductor portion (8). The timing at which a predetermined number of cycles is detected may be the timing (tc) at which the relative level (SL) reaches a specified value (i.e., the timing at which the implementation of the growth condition begins). In this case, the predetermined number may be an integer, but is not limited to an integer.

[0020] In the ELO method, the transition timing from initial growth (e.g., longitudinal growth) to growth with different growth conditions (e.g., transverse growth) is important. When the transition timing is controlled by the deposition time, there was a problem where the manufacturing yield decreased because the transition timing became too fast or too slow due to the deposition rate scattering caused by the aperture width, characteristics of the manufacturing equipment, etc. Manufacturing yield is the rate at which a nitride semiconductor part is manufactured that satisfies suitability conditions regarding, for example, dislocation density (defect density), aspect ratio, etc.

[0021] In this embodiment, by using light of a wavelength absorbed by the nitride semiconductor part (8) at the growth temperature (e.g., 405 nm) and measuring the interference between the reflected light from the surface of the nitride semiconductor part (8) during growth and the reflected light from the mask part (5) as a fringe (shape of the temporal change of physical quantities such as reflectance), the growth state in the height direction (c-axis direction) can be monitored regardless of the internal structure of the base substrate (BS). In addition, when using light of a wavelength that transmits the nitride semiconductor at the growth temperature (e.g., 633 nm, 950 nm), it is affected by the structure of the base substrate, so it becomes difficult to analyze the fringe (extract components that contribute to film thickness detection).

[0022] The inventors discovered that when a nitride semiconductor part (8) (e.g., a GaN crystal) is grown on a template substrate (TS) that includes a mask (6) (mask pattern), a fringe at a wavelength of 405 nm occurs, which is not visible when the nitride semiconductor is grown on a flat substrate that does not include a mask pattern. Since light of a wavelength of 405 nm is absorbed by the nitride semiconductor (e.g., GaN) at the growth temperature of the nitride semiconductor part (8) (high temperature of 1000°C or higher), the fringe is not visible on the flat substrate, but when using a template substrate (TS) that has a mask (6) (e.g., a mask pattern including a silicon nitride film as the mask part (5)), the interference of light reflected from the surface of the nitride semiconductor part (8) and the surface of the mask part (5) can be measured as a fringe.

[0023] The ratio of reflected light intensity to incident light intensity on the upper surface of the nitride semiconductor part (8) (reflectance of the nitride semiconductor part) may be greater than the ratio of reflected light intensity to incident light intensity on the upper surface of the mask part (5) (reflectance of the mask part).

[0024] The absorption coefficient of the first light (L1) at the growth temperature of the nitride semiconductor part (8) may be at least 10 times the absorption coefficient of the first light (L1) at room temperature. The bandgap of the nitride semiconductor part (8) at the growth temperature may be smaller than the bandgap of the nitride semiconductor part (8) at room temperature (3.4 eV in the case of GaN). The wavelength of the first light (L1) may be set according to the bandgap of the nitride semiconductor part (8) at the growth temperature. The first light (L1) may be a laser light.

[0025] The absorption coefficient of the first light (L1) at the growth temperature of the nitride semiconductor part (8) is K [m -1 〕, the thickness of the mask part (5) is set to D [m], and K > 1 / D may be used.

[0026] The nitride semiconductor part (8) includes a GaN-based semiconductor, and the growth conditions include a growth temperature. Regarding the growth temperature, the first temperature, which is the first condition, is preferably a temperature suitable for longitudinal growth, and may be lower than the second temperature, which is the second condition. The growth conditions include a flow rate of a source gas containing gallium, and regarding the flow rate of the source gas, the first flow rate, which is the first condition, may be smaller than the second flow rate, which is the second condition.

[0027] The a-axis direction of the nitride semiconductor part (8) may be the width direction of the mask part (5) or the opening (KS), and the width of the mask part (5) may be 20 [㎛] or more. The ratio of the thickness of the mask part (5) to the width of the opening (KS) may be 3.0 or less.

[0028] FIG. 6 is a plan view showing an example of a mask. An opening (KS) of the mask (6) (mask pattern) has the function of a growth initiation opening that exposes the upper surface of the base substrate to initiate the growth of the nitride semiconductor part (8), and the mask part (5) may have the function of a selective growth mask that grows the nitride semiconductor part (8) in the transverse direction. The opening (KS) is a part (non-forming part) of the mask pattern (6) where the mask part (5) is not present, and it may not be surrounded by the mask part (5).

[0029] As a mask (6), an inorganic film (ZF) (inorganic insulating film) such as a silicon oxide (SiOx) film, a silicon nitride (SiNx) film, a silicon oxynitride (SiON) film, or a titanium nitride (TiNx) film may be used. The opening (KS) may have an elongated shape, and a plurality of openings (KS) may be periodically arranged in the <11-20> direction (a-axis direction) of the nitride semiconductor part (8). The width of the opening (KS) may be approximately 0.2 μm to 20 μm. The smaller the width of the opening (KS), the fewer the number of penetrating dislocations propagating from the opening (KS) to the nitride semiconductor part (8). In addition, peeling of the nitride semiconductor part (8) becomes easier in a subsequent process (described later). A laminated film containing the above materials (for example, at least two of silicon oxide, silicon nitride, and silicon oxynitride) may be used as the mask (6).

[0030] In the mask (6) (mask pattern), a plurality of long inorganic films (ZF), each functioning as a mask portion (5), may be arranged in the <11-20> direction (a-axis direction) of the nitride semiconductor portion (8) with a plurality of gaps (ZN) functioning as openings (KS). In addition to being arranged in the <11-20> direction (a-axis direction), the plurality of long inorganic films (ZF) may also be arranged in the <1-100> direction (m-axis direction).

[0031] FIG. 7 is a cross-sectional view showing an example of the configuration of a base substrate. The base substrate (BS) may have a main substrate (1) which is a heterogeneous substrate with a different lattice constant from the nitride semiconductor part (8). The nitride semiconductor part (8) may include a GaN-based semiconductor, and the heterogeneous main substrate (1) may be a silicon substrate. Examples of heterogeneous substrates include a sapphire (Al2O3) substrate, a silicon carbide (SiC) substrate, etc. The plane direction of the main substrate (1) is, for example, the (111) plane of a silicon substrate, the (0001) plane of a sapphire substrate, the 6H-SiC (0001) plane of a SiC substrate, or the 4H-SiC (0001) plane. These are examples, and any substrate and plane direction capable of growing the nitride semiconductor part (8) by the ELO method may be used.

[0032] A base substrate (BS) may include a main substrate (1) and a lower portion (4) on the main substrate (1), and a nitride semiconductor portion (8) may be grown from the upper surface of the lower portion (4) exposed to an opening (KS). The lower portion (4) may include a GaN-based semiconductor. The lower portion (4) may include at least one of a seed portion and a buffer portion. A GaN-based semiconductor may be used as the seed portion. A GaN-based semiconductor, AlN, SiC, etc. may be used as the buffer portion. The base substrate (BS) may be composed of a self-supporting single-crystal substrate such as GaN or SiC (e.g., a wafer cut from a bulk crystal), and a mask (6) may be placed on the single-crystal substrate.

[0033] (Semiconductor substrate manufacturing device)

[0034] FIG. 8 is a schematic diagram showing the configuration of a semiconductor substrate manufacturing apparatus according to the present embodiment. As shown in FIG. 8, the semiconductor substrate manufacturing apparatus (20) comprises a base substrate (BS), a stage (21) for loading a template substrate (TS) having a mask pattern including a mask portion and an opening located on the base substrate (BS), a raw material supply device (22) for supplying raw materials for growing a nitride semiconductor portion (8) on the template substrate (TS), an optical device (23) for irradiating a semiconductor substrate (10) including the template substrate (TS) and the nitride semiconductor portion being grown with a first light (L1) having a wavelength absorbed by the nitride semiconductor portion (8) at the growth temperature of the nitride semiconductor portion (8) and receiving a second light (L2) from the semiconductor substrate (10), and a control device (24) for controlling the raw material supply device (22) so that the growth condition of the nitride semiconductor portion (8) transitions from a first condition (e.g., a first flow rate) to a second condition (e.g., a second flow rate > a first flow rate). The control device (24) may be capable of at least one of wired communication and wireless communication between the optical device (23).

[0035] A semiconductor substrate manufacturing device (20) may be equipped with a chamber (25) including a stage (SG), a flow channel (27) passing through the chamber (25), and a heating device (26) for heating the chamber (25), and a semiconductor substrate (10) may be placed within the flow channel (27). A control device (22) may use the intensity of a second light (L2) to instruct the heating device (26) to transition from a first condition (first temperature) to a second condition (second temperature > first temperature). An optical device (23) may be located outside the chamber (25). A wind (28) through which the first light (L1) and the second light (L2) pass may be installed in the chamber (25).

[0036] The stage (21) may perform a rotational operation (using the axis in the normal direction of the template substrate (TS) as the axis of rotation). In FIG. 8, the raw material supply device (22) flows the raw material gas in the flow channel (27) in the transverse direction (a direction parallel to the upper surface of the template substrate) under the first and second conditions, thereby exhausting in the transverse direction, but is not limited thereto. The raw material gas may also flow in the longitudinal direction (the normal direction of the template substrate (TS)) under the first and second conditions.

[0037] The control device (24) uses the intensity of the second light (L2) to detect the relative level of the upper surface of the nitride semiconductor part (8) based on the upper surface level (UL) of the mask part (5) over time, and at the timing when the relative level reaches a specified value (see tc in FIG. 5), it may instruct the raw material supply device (22) to transition from a first condition (e.g., first flow rate) to a second condition (e.g., second flow rate > first flow rate), and at this timing, it may instruct the heating device (26) to transition from a first condition (first temperature) to a second condition (second temperature > first temperature).

[0038] The control device (24) may be configured to control at least one of the raw material supply device (22) and the heating device (26) by executing a program stored on, for example, an internal memory, a communication device capable of communication, or an accessible network, and the program and the recording medium in which the program is stored are also included in this embodiment.

[0039] (Example 1)

[0040] FIG. 9 is a cross-sectional view illustrating a method for manufacturing such a semiconductor substrate in Example 1. In FIG. 9, a lower portion (4) containing a nitride semiconductor is formed on a main substrate (1), and a mask pattern (6) containing a plurality of stripe-shaped mask portions (5) is formed on the lower portion (4). The mask portion (5) is made of a silicon nitride film with a film thickness of 100 nm and a width of 52 μm, and the m-axis direction of the nitride semiconductor portion (8) is the length direction. The pitch of the stripes of the mask portion (5) is 55 μm.

[0041] A stripe pattern of resist is formed on a base substrate (BS) on which a nitride semiconductor film is deposited as a lower portion (4) by photolithography technology. Next, a silicon nitride film with a thickness of 100 nm is deposited over the entire surface by sputtering. Next, the silicon nitride film is patterned by a lift-off method and formed into a mask pattern (6) (initial stripe pattern). Next, a nitride semiconductor portion (8) including an initial growth portion (8s) is grown on the mask pattern (6) by organometallic vapor deposition (MOCVD) using trimethylgallium (TMG) and ammonia (NH3) (ELO method).

[0042] In FIG. 9, an initial growth portion (8s) is formed above the lower portion (4) exposed to the opening (KS). The growth condition is set as the first condition. Then, the transition of the growth condition (from the first condition to the second condition) is initiated at a timing just before the edge of the initial growth portion (8s) climbs up the upper surface of the mask portion (5) (at the stage where it is in contact with the upper side of the mask portion (5), relative level (SL)=0), or immediately after it climbs up the upper surface of the mask portion (5) (SL>0). Depending on the semiconductor device, it may be better for the nitride semiconductor portion (8) to be somewhat thicker, and in that case, it is easier to form a thick nitride semiconductor portion (8) by making the initial growth portion (8s) to which the first condition is applied thicker. In that case, the transition from the first condition to the second condition may be initiated at a timing when the relative level (SL) becomes somewhat greater than 0.

[0043] In Example 1, using the film thickness monitoring technology described in the embodiment, the first condition (condition prioritizing longitudinal growth) was set as follows: Growth temperature (set temperature): 1100°C (first temperature), growth pressure: 10 kPa, ammonia flow rate: 7.5 slm, trimethylgallium flow rate: 3 sccm. Additionally, the second condition (condition prioritizing transverse growth) was set as follows: Growth temperature (set temperature): 1175°C (second temperature), growth pressure: 10 kPa, ammonia flow rate: 7.5 slm, trimethylgallium flow rate: 11 sccm.

[0044] The initial growth portion (8s) serves as the starting point for the transverse growth of the nitride semiconductor portion (8). The initial growth layer (8s) can be formed with a thickness of, for example, 30 nm to 1000 nm, 50 nm to 400 nm, or 70 nm to 350 nm. By growing the initial growth portion (8s) in a transverse direction while it protrudes slightly from the mask portion (5), the growth of the nitride semiconductor portion (8) in the c-axis direction (thickness direction) is suppressed, and the nitride semiconductor portion (8) can be grown in the transverse direction at high speed and with high crystallinity, and the consumption of raw materials is reduced. By doing this, a thin, wide, and low-defect nitride semiconductor portion (8) (a crystal of a nitride semiconductor such as GaN) can be formed at a low cost.

[0045] The internal stress of the nitride semiconductor part (8) can be reduced by having a gap (gap) (GP) so that the nitride semiconductor part (8) grown horizontally in the reverse direction from two adjacent openings (KS) does not come into contact (associate) with each other on the mask part (5). By doing so, cracks and defects (dislocations) visible in the nitride semiconductor part (8) can be reduced. This effect is particularly effective when the main substrate (1) is a heterogeneous substrate. The width of the gap (GP) can be 5㎛ or less, 3㎛ or less, or 2㎛ or less.

[0046] Among the nitride semiconductor part (8), the part located on the initial growth part (8s) becomes a dislocation succession part with many penetrating dislocations, and the part (wing part) on the mask part (5) becomes a low-defect part (YS) with a penetrating dislocation density of 1 / 10 or less compared to the dislocation succession part. A penetrating dislocation refers to a part of the nitride semiconductor part (8) in its c-axis direction ( <0001> It is a dislocation (defect) extending in the direction. The penetration dislocation density of the low-defect region (YS) is, for example, 5×10 6 [Pie / cm²] or less. As described below, when an active part (active layer) including a light-emitting part is formed above the nitride semiconductor part (8), the light-emitting part can be positioned above the low-defect part (YS) (so as to overlap the low-defect part (YS) when viewed in a plane).

[0047] For the low-defect portion (YS), the ratio of the size W1 in the a-axis direction to the thickness d1 (W1 / d1) can be, for example, 2.0 or more. By using the method of Example 1, W1 / d1 can be 1.5 or more, 2.0 or more, 4.0 or more, 5.0 or more, 7.0 or more, or 10.0 or more. It was found that by making W1 / d1 1.5 or more, the splitting process of the nitride semiconductor portion (8) in the subsequent process (for example, a splitting process in which the cross-section becomes the m-plane) becomes easier. In addition, the internal stress of the nitride semiconductor portion (8) is reduced, and the warping of the semiconductor substrate (10) is reduced.

[0048] The aspect ratio (ratio of size in the X direction to thickness = WL / d1) of the nitride semiconductor part (8) can be 3.5 or more, 5.0 or more, 6.0 or more, 8.0 or more, 10 or more, 15 or more, 20 or more, 30 or more, or 50 or more. Additionally, by using the method of Example 1, the ratio (WL / WK) of the size WL in the X direction of the nitride semiconductor part (8) to the width WK of the opening (KS) can be 3.5 or more, 5.0 or more, 6.0 or more, 8.0 or more, 10 or more, 15 or more, 20 or more, 30 or more, or 50 or more, and the ratio of low defects can be increased. The nitride semiconductor part (8) (including the initial growth part (8s)) shown in FIG. 9 can be a nitride semiconductor crystal (e.g., GaN crystal, AlGaN crystal, InGaN crystal, or InAlGaN crystal).

[0049] (Example 2)

[0050] FIG. 10 is a cross-sectional view illustrating a method for manufacturing such a semiconductor device in Example 2. FIG. 10 includes, after preparing the semiconductor substrate (10) described above, a process of forming a compound semiconductor part (9) and electrodes D1 and D2 on the semiconductor substrate (10); a process of bonding a laminate (EB) including a nitride semiconductor part (8), a compound semiconductor part (9), and electrodes D1 and D2 to a support substrate (SK) via bonding layers H1 and H2; a process of peeling off a base substrate (BS); and a process of reorganizing the support substrate (SK) into a plurality of supports (ST) and forming a semiconductor device (SD) in which the laminate (EB) is maintained on the supports (ST). Before peeling off the base substrate (BS), the mask (6) may be removed by wet etching, etc.

[0051] The nitride semiconductor part (8) may be an n-type semiconductor crystal. The compound semiconductor part (9) may include a GaN-based semiconductor. The compound semiconductor part (9) may include an active part (e.g., an active layer such as a quantum-well structure) and a p-type semiconductor part, and may include an n-type semiconductor part (e.g., a ligros layer, an n-type contact layer) under the active part. When the active part of the compound semiconductor part (9) includes a light-emitting part, the light-emitting part may be placed above the low-defect part (YS) (so as to overlap the low-defect part (YS) when viewed in a plane). By doing this, the light-emitting efficiency can be increased.

[0052] Electrode D1 located above the low-defect portion (YS) may be the anode and electrode D2 may be the cathode. The support substrate (SK) may have a conductive pad in contact with the junction layer H1 and a conductive pad in contact with the junction layer H2. The junction layers H1 and H2 may be formed of solder material. Before, during, or after bonding to the support substrate (SK), the long-shaped laminate (EB) may be divided into multiple parts (by cutting in the short direction), and in this case, the division process may be performed by cleavage (e.g., m-plane cleavage where the cleavage plane is the m-plane) with respect to the nitride semiconductor portion (8) and the compound semiconductor portion (9). When using a semiconductor laser element, an end-face coating (formation of a reflective film) may be performed on the m-plane which is the cleavage plane. In FIG. 10, the laminate (EB) is transferred from the base substrate (BS) to the support substrate (SK), but this is not limited thereto. It may be transferred one or more times using tape or the like from the base substrate (BS).

[0053] The semiconductor device (SD) may function as an LED (light-emitting diode) device or a semiconductor laser device. The support (ST) may be a sub-mount substrate. Example 2 includes an electronic device having the semiconductor device (SD) (e.g., a lighting device, a laser device, a display device, a measuring device, an information processing device, etc.).

[0054] FIG. 11 is a cross-sectional view illustrating a method for manufacturing a semiconductor substrate according to the present embodiment. The method for manufacturing a semiconductor substrate according to the present embodiment comprises the steps of: preparing a template substrate (TS) having a seed region (SA) and a growth inhibition region (YA) on the upper side; growing a nitride semiconductor part (8) from the upper side of the seed region (SA); irradiating a semiconductor substrate (10) including the template substrate (TS) and the nitride semiconductor part (8) being grown with a first light (L1) having a wavelength absorbed by the nitride semiconductor part (8) at the growth temperature of the nitride semiconductor part (8); receiving a second light (L2) from the semiconductor substrate (10); and performing a process of transitioning the growth conditions of the nitride semiconductor part (8) (transitioning from a first condition to a second condition).

[0055] The first light (L1) of FIG. 11 may be irradiated onto the nitride semiconductor part (8) and the growth inhibition region (YA). The second light (L2) includes the reflected light of the first light (L1) from the upper surface of the nitride semiconductor part (8) and the reflected light of the first light (L1) from the growth inhibition region (YA), and the second light (L2) may be used to initiate the transition from the first condition of growth conditions to the second condition.

[0056] With the thickness direction of the template substrate (TS) as the vertical direction and the width direction of the growth inhibition region (YA) as the horizontal direction, the first condition may be a condition that prioritizes the vertical growth (growth in the c-axis direction) of the nitride semiconductor part (8), and the second condition may be a condition that prioritizes the horizontal growth (growth in the a-axis direction) of the nitride semiconductor part (8). The wavelength of the first light (L1) may be included in the wavelength range of 395 to 415 nm.

[0057] Using the intensity of the second light (L2), the relative level (SL) of the nitride semiconductor part (8) based on the level (YL) of the growth inhibition region (YA) may be detected over time, and the implementation of the growth condition may be started at the timing when the relative level (SL) reaches a specified value.

[0058] For example, after the growth of the nitride semiconductor part (8) begins, a period of time may elapse during which the relative level (SL) in the growth condition is less than a specified value in the first condition, and at the timing when the relative level (SL) becomes a specified value (e.g., 10 nm to 500 nm), the transition to the second condition of the growth condition may begin, and after the transition, the growth may be carried out under the second condition.

[0059] The seed region (SA) may be composed of a material in which the nitride semiconductor part (8) grows, and may include, for example, a crystalline material with a small lattice constant gap (with the nitride semiconductor part (8)), such as sapphire, in addition to nitride semiconductors such as GaN-based semiconductors and aluminum nitride. The growth inhibition region (YA) may be composed of a material that inhibits the longitudinal growth (for example, growth in the c-axis direction) of the nitride semiconductor part (8), and may include, for example, amorphous materials such as silicon nitride and silicon oxide, semiconductor materials such as SiC, in addition to polycrystalline materials or metal materials.

[0060] (Supplementary Note)

[0061] The foregoing disclosure is for illustrative and illustrative purposes only and is not intended to be limiting. It should be noted that, based on these illustrative and illustrative examples, many variations will be obvious to those skilled in the art, and therefore these variations are also included in the embodiments. Explanation of the symbols

[0062] 1 main board 4 underlayer 5 Mask section 6 Mask (Mask pattern) 8 Nitride semiconductor part 10 Semiconductor substrate 20 Manufacturing apparatus for semiconductor substrates 22 Raw material supply apparatus 23 Optical device 24 Control device BS base substrate TS template substrate KS opening YS low-defect part

Claims

Claim 1 A method for manufacturing a semiconductor substrate, comprising: a process of preparing a base substrate and a template substrate having a mask portion and an opening located on the base substrate; a process of growing a nitride semiconductor portion from the base substrate exposed to the opening; a process of irradiating a semiconductor substrate including the template substrate and the nitride semiconductor portion being grown with a first light having a wavelength absorbed by the nitride semiconductor portion at the growth temperature of the nitride semiconductor portion; a process of receiving a second light including reflected light from the upper surface of the nitride semiconductor portion of the first light from the semiconductor substrate and reflected light from the upper surface of the mask portion of the first light; and a process of using the second light to transition from a first condition of growth conditions of the nitride semiconductor portion to a second condition. Claim 2 A method for manufacturing a semiconductor substrate according to claim 1, wherein the first light is irradiated onto the nitride semiconductor portion and the mask portion. Claim 3 A method for manufacturing a semiconductor substrate according to claim 1 or 2, wherein the thickness direction of the nitride semiconductor part is the longitudinal direction and the width direction of the nitride semiconductor part is the transverse direction, wherein the first condition is a condition that prioritizes longitudinal growth of the nitride semiconductor part and the second condition is a condition that prioritizes transverse growth of the nitride semiconductor part. Claim 4 A method for manufacturing a semiconductor substrate according to claim 1 or 2, wherein the wavelength of the first light is included in the wavelength range of 395 to 415 nm. Claim 5 A method for manufacturing a semiconductor substrate according to claim 1 or 2, wherein the second light is used to detect the relative level of the upper surface of the nitride semiconductor part based on the upper surface level of the mask part over time series. Claim 6 A method for manufacturing a semiconductor substrate according to claim 5, wherein the implementation of growth conditions is initiated at the timing when the relative level reaches a specified value. Claim 7 A method for manufacturing a semiconductor substrate according to claim 5, wherein the above-mentioned relative level is zero at or after the timing at which the above-mentioned relative level becomes zero. Claim 8 A method for manufacturing a semiconductor substrate according to claim 5, wherein a reflectance, which is the ratio of the intensity of the second light to the intensity of the first light, or a reflected light intensity, which is the intensity of the second light, is obtained over a time series. Claim 9 A method for manufacturing a semiconductor substrate according to claim 8, wherein the reflectance or the reflected light intensity varies periodically. Claim 10 A method for manufacturing a semiconductor substrate according to claim 1 or 2, wherein the template substrate has a mask pattern including the mask portion and the opening. Claim 11 A method for manufacturing a semiconductor substrate according to claim 1 or 2, wherein the nitride semiconductor portion has an absorption coefficient of the first light at the growth temperature that is 10 times or more the absorption coefficient of the first light at room temperature. Claim 12 In claim 10, the absorption coefficient of the first light at the growth temperature of the nitride semiconductor part is K [m -1 〕, a method for manufacturing a semiconductor substrate in which the thickness of the mask portion is D[m] and K>1 / D. Claim 13 A method for manufacturing a semiconductor substrate according to claim 1 or 2, wherein the nitride semiconductor portion comprises a GaN-based semiconductor, the growth condition includes a growth temperature, and regarding the growth temperature, the first temperature of the first condition is lower than the second temperature of the second condition. Claim 14 A method for manufacturing a semiconductor substrate according to claim 1 or 2, wherein the nitride semiconductor portion comprises a GaN-based semiconductor, the growth conditions include a growth pressure, and regarding the growth pressure, the first pressure of the first condition is higher than the second pressure of the second condition. Claim 15 A method for manufacturing a semiconductor substrate according to claim 10, wherein the ratio of reflected light intensity to incident light intensity on the upper surface of the nitride semiconductor part is greater than the ratio of reflected light intensity to incident light intensity on the upper surface of the mask part. Claim 16 A method for manufacturing a semiconductor substrate according to claim 10, wherein the width of the mask portion is 20 [㎛] or more. Claim 17 A method for manufacturing a semiconductor substrate according to claim 10, wherein the ratio of the thickness of the mask portion to the width of the opening is 3.0 or less. Claim 18 A method for manufacturing a semiconductor substrate according to claim 10, wherein in the above mask, a plurality of long inorganic films, each functioning as a mask portion, are arranged in the <11-20> direction of the nitride semiconductor portion with a gap functioning as the opening. Claim 19 A method for manufacturing a semiconductor substrate according to claim 18, wherein the plurality of long inorganic films are arranged in the <11-20> direction and the <1-100> direction of the nitride semiconductor portion. Claim 20 A method for manufacturing a semiconductor substrate according to claim 1 or 2, wherein the base substrate has a silicon substrate and the nitride semiconductor part includes a GaN-based semiconductor. Claim 21 A method for manufacturing a semiconductor substrate according to claim 1 or 2, wherein the nitride semiconductor portion comprises a GaN-based semiconductor, the growth condition includes a flow rate of a source gas containing gallium, and with respect to the flow rate of the source gas, the first flow rate of the first condition is smaller than the second flow rate of the second condition. Claim 22 A semiconductor substrate manufacturing apparatus comprising: a base substrate; a stage for loading a template substrate having a mask portion and an opening located on the base substrate; a raw material supply device for supplying raw materials for growing a nitride semiconductor portion on the template substrate; an optical device for receiving a second light, comprising a wavelength absorbed by the nitride semiconductor portion at the growth temperature of the nitride semiconductor portion, irradiating a semiconductor substrate including the template substrate and the nitride semiconductor portion being grown with a first light, and a reflection of the first light from the upper surface of the nitride semiconductor portion and a reflection of the first light from the upper surface of the mask portion, and a control device for controlling the raw material supply device to transition the growth condition of the nitride semiconductor portion from a first condition to a second condition using the second light. Claim 23 A semiconductor substrate manufacturing apparatus according to claim 22, wherein the control device detects, over time, a relative level of the upper surface of the nitride semiconductor part based on the upper surface level of the mask part based on a reflectance which is the ratio of the intensity of the second light to the intensity of the first light, or the intensity of the second light, and when the relative level reaches a specified value, instructs the raw material supply device to perform the transition. Claim 24 A semiconductor substrate manufacturing apparatus comprising: a base substrate; a stage for placing a template substrate having a mask portion and an opening located on the base substrate; a raw material supply device for supplying raw materials for growing a nitride semiconductor portion on the template substrate; an optical device for receiving a second light, comprising a wavelength absorbed by the nitride semiconductor portion at the growth temperature of the nitride semiconductor portion, irradiating the semiconductor substrate including the template substrate and the nitride semiconductor portion being grown with a first light, and a reflection of the first light from the upper surface of the nitride semiconductor portion and a reflection of the first light from the upper surface of the mask portion, and a control device for controlling the raw material supply device to transition the growth condition of the nitride semiconductor portion from a first condition to a second condition using the second light. Claim 25 A method for manufacturing a semiconductor substrate according to claim 1, wherein the transition from a first condition to a second condition of the growth conditions of the nitride semiconductor part is a process performed based on information regarding the interference between the reflected light from the upper surface of the nitride semiconductor part and the reflected light from the upper surface of the mask part. Claim 26 delete Claim 27 delete

Citation Information

Patent Citations

  • Semiconductor device, its manufacturing method and substrate therefor

    JP2006114829A

  • Nitride semiconductor wafer and method of manufacturing nitride semiconductor wafer

    JP2013147383A

  • Method for growing compound semiconductor

    JP2015109389A

  • Substrate of gallium nitride single crystal and processfor producing the same