Display apparatus and manufacturing the same

The display device's innovative layer structure with varying film densities and stress properties addresses the issue of internal damage from impacts, maintaining clear images and device functionality.

KR103044996B1Active Publication Date: 2026-11-06SAMSUNG DISPLAY CO LTD
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
KR1020220008522
Authority / Receiving Office
KR · KR
Patent Type
Patents
Current Assignee / Owner
Filing Date
2022-01-20
Publication Date
2026-11-06
Estimated Expiration
2042-01-20

AI Technical Summary

Technical Problem

Display devices, particularly those that are freely deformable, suffer from internal layer damage and pixel malfunction due to external impacts, leading to dead spots and impaired image clarity.

Method used

A display device structure comprising specific layers with varying densities and stress properties, including a substrate, semiconductor layers, and interlayer insulating films with oxide and nitride films, is designed to enhance durability against external impacts.

Benefits of technology

The structure prevents internal layer damage and maintains clear image display after external impacts, ensuring the device's functionality and integrity.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure R1020220008522_ABST
    Figure R1020220008522_ABST
Patent Text Reader

Abstract

The present invention provides a display device for improving impact resistance and reducing a defect rate, comprising: a substrate; a first semiconductor layer disposed on the substrate; a second semiconductor layer disposed on the first semiconductor layer; an interlayer insulating layer disposed on the second semiconductor layer and comprising a plurality of inorganic insulating films; a source electrode or a drain electrode disposed on the interlayer insulating layer and respectively connected to the first semiconductor layer or the second semiconductor layer; and an organic light-emitting element connected to the source electrode or the drain electrode, wherein the plurality of inorganic insulating films comprises at least one oxide film, a first nitride film disposed on the oxide film and having a first density, and a second nitride film disposed on the first nitride film and having a second density lower than the first density.
Need to check novelty before this filing date? Find Prior Art

Description

Technology Field

[0001] The present invention relates to a display device and a method for manufacturing the same, and more specifically, to a display device capable of realizing a clear image even after an external impact has been applied, and a method for manufacturing the same. Background Technology

[0002] Mobile-based electronic devices are being widely used. In addition to small electronic devices such as mobile phones, tablet PCs have recently become widely used as mobile electronic devices.

[0003] Such portable electronic devices include a display device to support various functions and to provide visual information, such as images or videos, to the user. Recently, as other components for driving the display device have become miniaturized, the proportion of the display device within the electronic device is gradually increasing, and structures capable of bending from a flat state to a predetermined angle are also being developed.

[0004] In such cases, if an object falls from the upper surface of the display device on which the image is implemented, some of the layers of the display device may be damaged or broken. The problem to be solved

[0005] When an object falls and collides with the upper surface of a display device, some of the internal layers may be damaged or broken, causing some of the pixels of the display device to malfunction and resulting in dead spots. This problem occurs particularly frequently in display devices that are freely deformable. Embodiments of the present invention provide a display device capable of displaying a clear image even after an external impact has been applied. means of solving the problem

[0006] According to one aspect of the present invention, a display device is provided comprising a substrate, a first semiconductor layer disposed on the substrate, a second semiconductor layer disposed on the first semiconductor layer, an interlayer insulating layer disposed on the second semiconductor layer and comprising a plurality of inorganic insulating films, a source electrode or a drain electrode disposed on the interlayer insulating layer and respectively connected to the first semiconductor layer or the second semiconductor layer, and an organic light-emitting element connected to the source electrode or the drain electrode, wherein the plurality of inorganic insulating films comprises at least one oxide film, a first nitride film disposed on the oxide film and having a first density, and a second nitride film disposed on the first nitride film and having a second density lower than the first density.

[0007] In one embodiment, the hydrogen content of the first nitride film may be lower than the hydrogen content of the second nitride film.

[0008] In one embodiment, the first nitride film may have compressive stress, and the second nitride film may have tensile stress.

[0009] In one embodiment, the thickness of the first nitride film may be smaller than the thickness of the at least one oxide film.

[0010] In one embodiment, the thickness of the first nitride film may be smaller than the thickness of the second nitride film.

[0011] In one embodiment, the thickness of the interlayer insulating layer may be 5500 Å to 7500 Å, and the thickness of the first nitride film may be 400 Å to 600 Å.

[0012] In one embodiment, the plurality of inorganic insulating films further include a third nitride film disposed between the first nitride film and the second nitride film, and the third nitride film may have a third density lower than the first density and higher than the second density.

[0013] In one embodiment, the hydrogen content of the third nitride film may be higher than the hydrogen content of the first nitride film and lower than the hydrogen content of the second nitride film.

[0014] In one embodiment, the display device further comprises a first metal layer disposed on the first semiconductor layer, a second metal layer disposed between the first metal layer and the second semiconductor layer, and a third metal layer disposed between the second semiconductor layer and the interlayer insulating layer, and at least one of the first to third metal layers may have a compressive stress or a tensile stress of 200 MPa or less.

[0015] According to another aspect of the present invention, a method for manufacturing a display device is provided, comprising the steps of forming a first semiconductor layer on a substrate, forming a second semiconductor layer on the first semiconductor layer, and forming an interlayer insulating layer comprising a plurality of inorganic insulating films on the second semiconductor layer, wherein the step of forming the interlayer insulating layer comprises the steps of forming at least one oxide film on the second semiconductor layer, forming a first nitride film having a first density on the at least one oxide film, and forming a second nitride film having a second density lower than the first density on the first nitride film.

[0016] In one embodiment, the hydrogen partial pressure in the chamber during the step of forming the first nitride film may be lower than the hydrogen partial pressure in the chamber during the step of forming the second nitride film.

[0017] In one embodiment, the first nitride film may have a thickness of 400 Å to 600 Å.

[0018] In one embodiment, the interlayer insulating layer may have a thickness of 5500 Å to 7500 Å.

[0019] In one embodiment, the method for manufacturing a display device may further include the step of forming a third nitride film having a third density lower than the first density and higher than the second density between the step of forming the first nitride film and the step of forming the second nitride film.

[0020] In one embodiment, the hydrogen partial pressure in the chamber during the step of forming the third nitride film may be higher than the hydrogen partial pressure in the chamber during the step of forming the first nitride film, and lower than the hydrogen partial pressure in the chamber during the step of forming the second nitride film.

[0021] In one embodiment, the method for manufacturing a display device may further include the step of forming a first metal layer on the first semiconductor layer, the step of forming a second metal layer on the first metal layer, which is disposed between the step of forming the first semiconductor layer and the step of forming the second semiconductor layer, and the step of forming a third metal layer on the second semiconductor layer, which is disposed between the step of forming the second semiconductor layer and the step of forming the interlayer insulating layer.

[0022] In one embodiment, at least one of the first to third metal layers may have a compressive stress or a tensile stress of 200 MPa or less.

[0023] In one embodiment, at least one of the steps of forming the first metal layer, forming the second metal layer, and forming the third metal layer may be formed using a rotary sputtering device having a plurality of cylindrical targets.

[0024] In one embodiment, the plurality of cylindrical targets may be spaced apart with a ground portion in between.

[0025] In one embodiment, the substrate is placed on a stage, and the height difference between the upper surface of the stage measured at the center of the substrate and the upper surface of the interlayer insulating layer measured at the edge of the substrate may be 150 μm or less.

[0026] Other aspects, features, and advantages other than those described above will become clear from the following drawings, claims, and detailed description of the invention.

[0027] These general and specific aspects may be implemented using a system, method, computer program, or any combination of a system, method, or computer program. Effects of the invention

[0028] The display device according to the embodiments of the present invention may not generate dark spots due to external impact.

[0029] The display device according to the embodiments of the present invention can be freely deformed and prevent some internal layers from being damaged or broken during deformation.

[0030] The display device according to the embodiments of the present invention is capable of effectively handling external shocks. Brief explanation of the drawing

[0031] FIG. 1 is a schematic plan view illustrating a display device according to one embodiment of the present invention. FIG. 2 is a cross-sectional view showing a part of a display device according to one embodiment of the present invention. FIG. 3 is a schematic plan view illustrating a display device according to one embodiment of the present invention. FIG. 4 is an equivalent circuit diagram of a pixel circuit for driving a pixel according to one embodiment of the present invention. FIG. 5 is a schematic layout diagram illustrating a pair of pixel circuits of a display device according to one embodiment of the present invention. FIG. 6 is a cross-sectional view schematically illustrating a display device according to one embodiment of the present invention. FIG. 7 is a cross-sectional view schematically illustrating a display device according to another embodiment of the present invention. FIGS. 8 to 10 are cross-sectional views sequentially illustrating a method for manufacturing a display device according to an embodiment of the present invention. FIG. 11 is a schematic diagram illustrating the steps of forming a metal layer according to one embodiment of the present invention. FIG. 12 is a graph illustrating the height of the upper surface of a display device according to a comparative example and embodiments of the present invention. Specific details for implementing the invention

[0032] The present invention is capable of various modifications and may have various embodiments; specific embodiments are illustrated in the drawings and described in detail in the detailed description. The effects and features of the present invention, and the methods for achieving them, will become clear by referring to the embodiments described below in detail together with the drawings. However, the present invention is not limited to the embodiments disclosed below but can be implemented in various forms.

[0033] Hereinafter, embodiments of the present invention will be described in detail with reference to the attached drawings. When describing with reference to the drawings, identical or corresponding components are given the same reference numerals, and redundant descriptions thereof will be omitted.

[0034] In this specification, terms such as first, second, etc. are used not in a limiting sense, but for the purpose of distinguishing one component from another.

[0035] In this specification, singular expressions include plural expressions unless the context clearly indicates otherwise.

[0036] In this specification, terms such as "include" or "have" mean that the features or components described in the specification exist, and do not preclude the possibility that one or more other features or components may be added.

[0037] In this specification, when a part such as a film, region, or component is described as being on or above another part, it includes not only cases where it is immediately above the other part, but also cases where another film, region, or component is interposed therein.

[0038] In this specification, when it is stated that a membrane, region, component, etc. is connected, it includes cases where the membrane, region, or component is directly connected, or / or cases where other membranes, regions, or components are interposed between them to form an indirect connection. For example, when it is stated that a membrane, region, or component, etc. is electrically connected in this specification, it indicates cases where the membrane, region, or component, etc. are directly electrically connected, and / or cases where other membranes, regions, or components are interposed between them to form an indirect electrical connection.

[0039] In this specification, "A and / or B" indicates the case where it is A, B, or both A and B. And, "at least one of A and B" indicates the case where it is A, B, or both A and B.

[0040] In this specification, the x-axis, y-axis, and z-axis are not limited to three axes in an orthogonal coordinate system and may be interpreted in a broader sense that includes them. For example, the x-axis, y-axis, and z-axis may be orthogonal to each other, but they may also refer to different directions that are not orthogonal to each other.

[0041] Where any embodiment in this specification can be implemented differently, a specific process sequence may be performed differently from the order described. For example, two processes described consecutively may be performed substantially simultaneously or proceed in the reverse order of the order described.

[0042] In the drawings, the size of components may be exaggerated or reduced for convenience of explanation. For example, the size and thickness of each component shown in the drawings are depicted arbitrarily for convenience of explanation, so the present invention is not necessarily limited to what is illustrated.

[0043] FIG. 1 is a schematic plan view illustrating a display device according to an embodiment of the present invention. FIG. 2 is a cross-sectional view showing a part of a display device according to an embodiment of the present invention, and FIG. 2 is a cross-sectional view taken along line A-A' of FIG. 1. FIG. 3 is a schematic plan view illustrating a display device according to an embodiment of the present invention.

[0044] Referring to FIGS. 1 to 3, the display device (10) may include a display area (DA) and a peripheral area (NDA). The display area (DA) is an area where pixels (P) are arranged. The display area (DA) can provide an image using light emitted from each pixel (P). The pixels (P) may be connected to signal lines, such as a scan line (SL) extended in the x-direction and a data line (DL) extended in the y-direction. Although not shown in FIG. 1, the pixels (P) may be connected to power lines that transmit DC signals, such as a driving power line and a common power line. The display area (DA) may be covered by a thin film encapsulation layer (400) that overlaps with the substrate (100).

[0045] A pixel (P) may include a pixel circuit electrically connected to the aforementioned signal line and power line, and a display element, such as an organic light emitting diode (OLED), in the pixel circuit. The pixel (P) may emit light, for example, red, green, blue, or white light through the organic light emitting diode.

[0046] The peripheral area (NDA) may include a first scan driver (11), a second scan driver (12), a terminal portion (20), a driving voltage supply line (30), a common voltage supply line (40), and a wiring layer (50). This peripheral area (NDA) may be an area where no pixels are placed.

[0047] The first scan driver (11) and the second scan driver (12) may be placed in the peripheral area (NDA). The first scan driver (11) and the second scan driver (12) may be spaced apart from each other with the display area (DA) in between. The first scan driver (11) and / or the second scan driver (12) may generate and transmit a scan signal to each pixel (P) through a scan line (SL). FIG. 1 illustrates a case where two scan drivers are placed, but the present invention is not limited thereto. In another embodiment, a single scan driver may be placed on one side of the display area (DA).

[0048] The terminal portion (20) may be disposed at one end of the peripheral area (NDA) and includes terminals (21, 22, 23, 24). The terminal portion (20) may be exposed without being covered by an insulating layer and may be connected to a driver IC (13). The driver IC (13) may include a data driver.

[0049] The driving voltage supply line (30) can provide driving voltage to the pixels (P). The driving voltage supply line (30) can be placed in the surrounding area (NDA) adjacent to one side of the display area (DA).

[0050] The common voltage supply line (40) can provide a common voltage to the pixels (P). The common voltage is a voltage applied to the cathode electrode of the organic light-emitting diode, and the common voltage supply line (40) can be placed in the surrounding area (NDA) to partially surround the display area (DA).

[0051] The first wiring (51), the second wiring (52), the third wiring (53), and the fourth wiring (54) are positioned between one end of the display area (DA) and the terminal part (20) and can be extended along the y-direction. The first wiring (51) electrically connects the signal line of the display area (DA) and the terminal part (20), and the second wiring (52) electrically connects the driving voltage supply line (30) and the terminal part (20). The third wiring (53) electrically connects the first scan driver (11) and the second scan driver (12), respectively, to the terminal part (20), and the fourth wiring (54) electrically connects the common voltage supply line (40) and the terminal part (20).

[0052] In FIG. 1, the terminals (21, 22, 23, 24) of the terminal section (20) are described with different reference numbers as the first wiring (51), the second wiring (52), the third wiring (53), and the fourth wiring (54), but each of the terminals (21, 22, 23, 24) can be understood as a part of the first wiring (51), the second wiring (52), the third wiring (53), and the fourth wiring (54). That is, the end portion of the first wiring (51) corresponds to terminal (21), the end portion of the second wiring (52) corresponds to terminal (22), the end portion of the third wiring (53) corresponds to terminal (23), and the end portion of the fourth wiring (54) corresponds to terminal (24).

[0053] A display layer (200) is disposed on a substrate (100). The display layer (200) includes a plurality of pixels. Since each pixel may include a display element and a pixel circuit for operating the display element, the display layer (200) may include a plurality of display elements and pixel circuits connected to each display element.

[0054] The display layer (200) can be shielded by a thin film encapsulation layer (400). The thin film encapsulation layer (400) may include at least one organic encapsulation layer and at least one inorganic encapsulation layer. At least one organic encapsulation layer and at least one inorganic encapsulation layer may be stacked alternately. An input sensing member (TSL) and an optical functional member (OFL) may be disposed on the thin film encapsulation layer (400).

[0055] The input sensing member (TSL) includes various patterns of touch electrodes (TD) for touchscreen functions. The touch electrodes (TD) include first touch electrodes (TD1) connected to each other along a first direction (x direction) and second touch electrodes (TD2) connected to each other along a first direction (y direction) intersecting the first direction.

[0056] Such touch electrodes (TD) may be provided with a transparent electrode material so that light from the light-emitting regions of pixels disposed below the input sensing member (TSL) can be transmitted. Alternatively, the touch electrodes (TD) may be provided in a mesh shape so that light from the light-emitting regions of pixels can be transmitted. In this case, the touch electrodes (TD) are not limited to a transparent electrode material. For example, the touch electrodes (TD) may be a single film or a multilayer film made of a conductive material including aluminum (Al), copper (Cu), and / or titanium (Ti), etc.

[0057] The touch electrode (TD) is connected to a touch wire (TL) for transmitting a signal detected by the touch electrode (TD), and the touch wire (TL) can extend from the top of the thin film encapsulation layer (400) along one side of the thin film encapsulation layer (400) to the surrounding area (NDA).

[0058] The touch wiring (TL) is connected to the touch electrode (TD) of the input sensing member (TSL) of the display area (DA) and can extend from the top of the thin film encapsulation layer (400). The touch wiring (TL) is connected to the touch terminal (25) of the terminal portion (20) and can exchange electrical signals with the input sensing member (TSL).

[0059] The optical function member (OFL) can reduce the reflectivity of light (external light) incident from the outside toward the display device (10) and / or improve the color purity of light emitted from the display device (10).

[0060] In one embodiment, the optical function member (OFL) may include a phase retarder and a polarizer. The phase retarder may be of the film type or liquid crystal coating type and may include a λ / 2 phase retarder and / or a λ / 4 phase retarder. The polarizer may also be of the film type or liquid crystal coating type. The film type may include a stretched synthetic resin film, and the liquid crystal coating type may include liquid crystals arranged in a predetermined arrangement.

[0061] In another embodiment, the optical function member (OFL) may include a black matrix and color filters. The color filters may be arranged considering the color of light emitted from each pixel of the display device (10). Each of the color filters may include a red, green, or blue pigment or dye. Alternatively, each of the color filters may further include quantum dots in addition to the aforementioned pigment or dye. Alternatively, some of the color filters may not include the aforementioned pigment or dye and may include scattering particles such as titanium oxide.

[0062] In another embodiment, the optical function member (OFL) may include a destructive interference structure. The destructive interference structure may include a first reflective layer and a first reflective layer disposed on different layers. The first reflected light and the first reflected light reflected from the first reflective layer and the first reflective layer, respectively, may undergo destructive interference, and accordingly, the external light reflectance may be reduced.

[0063] FIG. 4 is an equivalent circuit diagram of a pixel circuit for driving a pixel according to one embodiment of the present invention.

[0064] The pixel circuit (PC) may include a driving thin-film transistor (T1), a switching thin-film transistor (T2), a compensation thin-film transistor (T3), a first initialization thin-film transistor (T4), an operation control thin-film transistor (T5), a light emission control thin-film transistor (T6), a second initialization thin-film transistor (T7), and a first storage capacitor (Cst) and a second storage capacitor (Cbt). Additionally, the pixel circuit (PC) may be connected to a plurality of signal lines, first and second initialization voltage lines (VL1, VL2) and a driving voltage line (PL). The signal lines may include a data line (DL), a first scan line (SL1), a second scan line (SL2), a previous scan line (SLp), a subsequent scan line (SLn), and a light emission control line (EL). In one embodiment, at least one of the signal lines, the first and second initialization voltage lines (VL1, VL2) and / or the driving voltage line (PL) may be shared among adjacent pixel circuits.

[0065] The driving voltage line (PL) can transmit a first power supply voltage (ELVDD) to the driving thin-film transistor (T1). The first initialization voltage line (VL1) can transmit a first initialization voltage (Vint1) that initializes the driving thin-film transistor (T1) to the pixel circuit (PC). The second initialization voltage line (VL2) can transmit a second initialization voltage (Vint2) that initializes the organic light-emitting diode (OLED) to the pixel circuit (PC).

[0066] In one embodiment, among the driving thin film transistor (T1), switching thin film transistor (T2), compensation thin film transistor (T3), first initialization thin film transistor (T4), operation control thin film transistor (T5), light emission control thin film transistor (T6), and second initialization thin film transistor (T7), the compensation thin film transistor (T3) and the first initialization thin film transistor (T4) are implemented as NMOS (n-channel MOSFET), and the remaining thin film transistors can be implemented as PMOS (p-channel MOSFET).

[0067] The drain region of the driving thin-film transistor (T1) can be electrically connected to the organic light-emitting diode (OLED) via the light-emitting control thin-film transistor (T6). The driving thin-film transistor (T1) can receive a data signal (Dm) according to the switching operation of the switching thin-film transistor (T2) and supply a driving current to the organic light-emitting diode (OLED).

[0068] The switching thin-film transistor (T2) can perform a switching operation in which it is turned on according to the first scan signal (Sn1) received through the first scan line (SL1) and transmits the data signal (Dm) transmitted through the data line (DL) to the source region of the driving thin-film transistor (T1).

[0069] The gate electrode of the compensation thin film transistor (T3) can be connected to the second scan line (SL2). The source region of the compensation thin film transistor (T3) is connected to the drain region of the driving thin film transistor (T1) and can be connected to the pixel electrode of the organic light-emitting diode (OLED) via the light-emitting control thin film transistor (T6). The drain region of the compensation thin film transistor (T3) can be connected together with one electrode of the first storage capacitor (Cst), the source region of the first initialization thin film transistor (T4), and the gate electrode of the driving thin film transistor (T1). The compensation thin film transistor (T3) is turned on according to the second scan signal (Sn2) received through the second scan line (SL2) to connect the gate electrode and the drain region of the driving thin film transistor (T1) to each other, thereby making the driving thin film transistor (T1) diode-connected.

[0070] The gate electrode of the first initialization thin film transistor (T4) can be connected to the previous scan line (SLp). The drain region of the first initialization thin film transistor (T4) can be connected to the first initialization voltage line (VL1). The source region of the first initialization thin film transistor (T4) can be connected together with one electrode of the first storage capacitor (Cst), the drain region of the compensation thin film transistor (T3), and the gate electrode of the driving thin film transistor (T1). The first initialization thin film transistor (T4) can be turned on according to the previous scan signal (Sn-1) received through the previous scan line (SLp) to transmit the first initialization voltage (Vint1) to the gate electrode of the driving thin film transistor (T1) and perform an initialization operation to initialize the voltage of the gate electrode of the driving thin film transistor (T1).

[0071] The gate electrode of the second initialization thin film transistor (T7) can be connected to the scan line (SLn). The source region of the second initialization thin film transistor (T7) can be connected to the pixel electrode of the organic light-emitting diode (OLED). The drain region of the second initialization thin film transistor (T7) can be connected to the second initialization voltage line (VL2). The second initialization thin film transistor (T7) can be turned on according to the scan signal (Sn+1) received through the scan line (SLn) to initialize the pixel electrode of the organic light-emitting diode (OLED).

[0072] The first storage capacitor (Cst) may include a first electrode (CE1) and a second electrode (CE2). The first electrode (CE1) may be connected to the gate electrode of the driving thin-film transistor (T1), and the second electrode (CE2) may be connected to the driving voltage line (PL). The first storage capacitor (Cst) can maintain the voltage applied to the gate electrode of the driving thin-film transistor (T1) by storing and maintaining a voltage corresponding to the difference between the voltages of the driving voltage line (PL) and the gate electrode of the driving thin-film transistor (T1).

[0073] The second storage capacitor (Cbt) may include a third electrode (CE3) and a fourth electrode (CE4). The third electrode (CE3) may be connected to the gate electrode of the first scan line (SL1) and the switching thin-film transistor (T2). The fourth electrode (CE4) may be connected to the gate electrode of the driving thin-film transistor (T1) and the first electrode (CE1) of the first storage capacitor (Cst). The second storage capacitor (Cbt) is a boosting capacitor, and when the first scan signal (Sn1) of the first scan line (SL1) is a voltage that turns off the switching thin-film transistor (T2), it can increase the voltage of the node (N) to reduce the voltage that displays black (black voltage).

[0074] The specific operation of each pixel circuit (PC) according to one embodiment is as follows.

[0075] During the first initialization period, when a previous scan signal (Sn-1) is supplied through the previous scan line (SLp), the first initialization thin film transistor (T4) is turned on in response to the previous scan signal (Sn-1), and the driving thin film transistor (T1) can be initialized by the first initialization voltage (Vint1) supplied from the first initialization voltage line (VL1).

[0076] During the data programming period, when a first scan signal (Sn1) and a second scan signal (Sn2) are supplied through the first scan line (SL1) and the second scan line (SL2), respectively, the switching thin-film transistor (T2) and the compensation thin-film transistor (T3) can be turned on in response to the first scan signal (Sn1) and the second scan signal (Sn2). At this time, the driving thin-film transistor (T1) can be diode-connected by the turned-on compensation thin-film transistor (T3) and forward-biased. Then, a voltage compensated for the threshold voltage (Vth) of the driving thin-film transistor (T1) from the data signal (Dm) supplied from the data line (DL) can be applied to the gate electrode of the driving thin-film transistor (T1). A first power supply voltage (ELVDD) and a compensation voltage are applied to both ends of the first storage capacitor (Cst), and a charge corresponding to the voltage difference between the two ends can be stored in the first storage capacitor (Cst).

[0077] During the light emission period, the operation control thin film transistor (T5) and the light emission control thin film transistor (T6) can be turned on by the light emission control signal (En) supplied from the light emission control line (EL). A driving current is generated according to the voltage difference between the voltage of the gate electrode of the driving thin film transistor (T1) and the first power supply voltage (ELVDD), and the driving current can be supplied to the organic light-emitting diode (OLED) through the light emission control thin film transistor (T6).

[0078] During the second initialization period, when a subsequent scan signal (Sn+1) is supplied through the subsequent scan line (SLn), the second initialization thin film transistor (T7) is turned on in response to the subsequent scan signal (Sn+1), and the organic light-emitting diode (OLED) is initialized by the second initialization voltage (Vint2) supplied from the second initialization voltage line (VL2).

[0079] In one embodiment, at least one of the plurality of thin-film transistors (T1 to T7) may be an oxide-based thin-film transistor comprising an oxide semiconductor, and the remainder may be silicon-based thin-film transistors comprising a silicon semiconductor. Specifically, the driving thin-film transistor (T1), which directly affects the brightness of the display device, is configured as a silicon-based thin-film transistor comprising a silicon semiconductor composed of polycrystalline silicon having high reliability, thereby enabling the implementation of a high-resolution display device.

[0080] Meanwhile, since oxide semiconductors have high carrier mobility and low leakage current, the voltage drop is not significant even when the driving time is long. In other words, since the color change of the image due to the voltage drop is not significant even during low-frequency driving, low-frequency driving is possible. As oxide semiconductors have the advantage of low leakage current, at least one of the compensation thin-film transistor (T3) and the first initialization thin-film transistor (T4) connected to the gate electrode of the driving thin-film transistor (T1) is equipped with an oxide semiconductor to prevent leakage current from flowing to the gate electrode of the driving thin-film transistor (T1) while simultaneously reducing power consumption.

[0081] For convenience of explanation below, the driving thin-film transistor (T1), the switching thin-film transistor (T2), the operation control thin-film transistor (T5), the light emission control thin-film transistor (T6), and the second initialization thin-film transistor (T7) are provided as silicon-based thin-film transistors including silicon semiconductors, and the compensation thin-film transistor (T3) and the first initialization thin-film transistor (T4) are provided as oxide-based thin-film transistors including oxide semiconductors.

[0082] FIG. 5 is a schematic layout diagram illustrating a pair of pixel circuits of a display device according to an embodiment of the present invention. The pixel circuits may be arranged to form rows and columns, and FIG. 5 illustrates a pair of pixel circuits (PCs) arranged in the same row of adjacent columns. The pixel circuit (PC-L) arranged on the left and the pixel circuit (PC-R) arranged on the right shown in FIG. 5 have a left-right symmetrical structure.

[0083] The semiconductor layers of the driving thin-film transistor (T1), the switching thin-film transistor (T2), the compensation thin-film transistor (T3), the first initialization thin-film transistor (T4), the operation control thin-film transistor (T5), the light emission control thin-film transistor (T6), and the second initialization thin-film transistor (T7) include a channel region and source regions and drain regions on both sides of the channel region, wherein the source region and drain region can be understood as the source electrode and drain electrode of the corresponding thin-film transistor. The source region and drain region may be interchanged depending on the properties of the transistor. Hereinafter, the terms source region and drain region are used instead of source electrode or drain electrode.

[0084] Referring to FIG. 5, a driving thin-film transistor (T1), a switching thin-film transistor (T2), an operation control thin-film transistor (T5), a light emission control thin-film transistor (T6), and a second initialization thin-film transistor (T7) may be arranged along the first semiconductor layer (1100), and a compensation thin-film transistor (T3) and a first initialization thin-film transistor (T4) may be arranged along the second semiconductor layer (1400).

[0085] The first semiconductor layer (1100) may be disposed on a substrate (100, FIG. 6) on which a buffer layer (111, FIG. 6) comprising an inorganic insulating material is formed. In one embodiment, the first semiconductor layer (1100) may include low temperature polysilicon (LTPS). Since polysilicon material has high electron mobility (100 cm² / Vs or higher), low power consumption, and excellent reliability, it can be used as a semiconductor layer for a thin-film transistor in a display device. However, the present invention is not limited thereto, and the first semiconductor layer (1100) may be formed of amorphous silicon (a-Si) and / or oxide semiconductor.

[0086] Some regions of the first semiconductor layer (1100) correspond to the semiconductor layers of the driving thin-film transistor (T1), the switching thin-film transistor (T2), the operation control thin-film transistor (T5), the light emission control thin-film transistor (T6), and the second initialization thin-film transistor (T7). In other words, the semiconductor layers of the driving thin-film transistor (T1), the switching thin-film transistor (T2), the operation control thin-film transistor (T5), the light emission control thin-film transistor (T6), and the second initialization thin-film transistor (T7) can be understood as being connected to each other and curved in various shapes.

[0087] The second semiconductor layer (1400) may be disposed on a third gate insulating layer (117, FIG. 6) comprising an inorganic insulating material. In one embodiment, the second semiconductor layer (1400) may include an oxide semiconductor material. The oxide semiconductor material is a Zn oxide-based material and may include Zn oxide, In-Zn oxide, Ga-In-Zn oxide, etc. In one embodiment, the oxide-based semiconductor layer may include an IGZO (In-Ga-Zn-O), ITZO (In-Sn-Zn-O), or IGTZO (In-Ga-Sn-Zn-O) semiconductor containing metals such as indium (In), gallium (Ga), and tin (Sn) in ZnO.

[0088] Some regions of the second semiconductor layer (1400) correspond to the semiconductor layers of the compensation thin-film transistor (T3) and the first initialization thin-film transistor (T4). In other words, the semiconductor layers of the compensation thin-film transistor (T3) and the first initialization thin-film transistor (T4) can be understood as being connected to each other. Since oxide semiconductors have high carrier mobility and low leakage current, the voltage drop is not significant even if the driving time is long. That is, since the color change of the image due to voltage drop is not significant even during low-frequency driving, low-frequency driving is possible. As oxide semiconductors have the advantage of low leakage current, the compensation thin-film transistor (T3) and the first initialization thin-film transistor (T4), which are connected to the gate electrode of the driving thin-film transistor (T1), are equipped with oxide semiconductors to prevent leakage current from flowing to the gate electrode of the driving thin-film transistor (T1) while simultaneously reducing power consumption.

[0089] The driving thin-film transistor (T1) may include a driving semiconductor layer and a first gate electrode (G1). The driving semiconductor layer may include a first channel region (C1), a first source region (S1) and a first drain region (D1) on both sides of the first channel region (C1). The driving semiconductor layer may have a curved shape so that the first channel region (C1) is formed longer than other channel regions (C2 to C7). For example, by having the first channel region (C1) have a shape that is folded multiple times, such as 'S', 'M', 'W', etc., a long channel length can be formed within a narrow space. Since the first channel region (C1) is formed long, the driving range of the gate voltage applied to the first gate electrode (G1) is widened, allowing for more precise control of the gradation of light emitted from the organic light-emitting diode (OLED) and improving display quality. In one embodiment, the first channel region (C1) may be provided in a straight shape rather than a folded shape. The first gate electrode (G1) may be provided in an isolated form so as to overlap with the first channel region (C1).

[0090] The first storage capacitor (Cst) may be arranged to overlap with the driving thin-film transistor (T1). The first storage capacitor (Cst) may include a first electrode (CE1) and a second electrode (CE2). The first gate electrode (G1) may perform the function of a control electrode for the driving thin-film transistor (T1), as well as the function of the first electrode (CE1) of the first storage capacitor (Cst). That is, the first gate electrode (G1) and the first electrode (CE1) may be formed as a single unit. The second electrode (CE2) of the first storage capacitor (Cst) is provided to overlap with the first electrode (CE1) with an insulating layer in between, and in this case, the insulating layer may serve as the dielectric layer of the first storage capacitor (Cst).

[0091] The switching thin-film transistor (T2) may include a switching semiconductor layer and a second gate electrode (G2). The switching semiconductor layer may include a second channel region (C2), a second source region (S2) and a second drain region (D2) on both sides of the second channel region (C2). The second source region (S2) is electrically connected to a data line (DL), and the second drain region (D2) may be connected to a first source region (S1). The second gate electrode (G2) may be provided as part of a first scan line (SL1).

[0092] The operation control thin-film transistor (T5) may include an operation control semiconductor layer and a fifth gate electrode (G5). The operation control semiconductor layer may include a fifth channel region (C5), a fifth source region (S5) and a fifth drain region (D5) on both sides of the fifth channel region (C5). The fifth source region (S5) is electrically connected to a first driving voltage line (PL1), and the fifth drain region (D5) may be connected to the first source region (S1). The fifth gate electrode (G5) may be provided as part of a light emission control line (EL).

[0093] The light-emitting control thin-film transistor (T6) may include a light-emitting control semiconductor layer and a sixth gate electrode (G6). The light-emitting control semiconductor layer may include a sixth channel region (C6), a sixth source region (S6) and a sixth drain region (D6) on both sides of the sixth channel region (C6). The sixth source region (S6) is connected to the first drain region (D1), and the sixth drain region (D6) may be electrically connected to the pixel electrode of an organic light-emitting diode (OLED). The sixth gate electrode (G6) may be provided as part of a light-emitting control line (EL).

[0094] The second initialization thin-film transistor (T7) may include a second initialization semiconductor layer and a seventh gate electrode (G7). The second initialization semiconductor layer may include a seventh channel region (C7), a seventh source region (S7) and a seventh drain region (D7) on both sides of the seventh channel region (C7). The seventh source region (S7) may be electrically connected to the second initialization voltage line (VL2), and the seventh drain region (D7) may be connected to the sixth drain region (D6). The seventh gate electrode (G7) may subsequently be provided as part of the scan line (SLn).

[0095] A second gate insulating layer (117, FIG. 11) is disposed on a driving thin film transistor (T1), a switching thin film transistor (T2), an operation control thin film transistor (T5), a light emission control thin film transistor (T6), and a second initialization thin film transistor (T7) that include a silicon semiconductor, and a compensation thin film transistor (T3) that includes an oxide semiconductor and a first initialization thin film transistor (T4) may be disposed on a third gate insulating layer (117).

[0096] The semiconductor layers of the compensation thin-film transistor (T3) and the first initialization thin-film transistor (T4) may each include a channel region, source regions on both sides of the channel region, and drain regions. In one embodiment, the source region and drain region may be formed by making the oxide semiconductor conductive by controlling the carrier concentration. For example, the source region and drain region of the compensation thin-film transistor (T3) and the first initialization thin-film transistor (T4) may be formed by increasing the carrier concentration in the oxide semiconductor through plasma treatment using a hydrogen (H) series gas, a fluorine (F) series gas, or a combination thereof. The source region and drain region may correspond to the source electrode and drain electrode, respectively. Hereinafter, the terms source region and drain region will be used instead of source electrode or drain electrode.

[0097] The compensation thin-film transistor (T3) may include a compensation semiconductor layer comprising an oxide semiconductor material and a third gate electrode (G3). The compensation semiconductor layer may include a third channel region (C3), and a third source region (S3) and a third drain region (D3) on both sides of the third channel region (C3). The third source region (S3) may be bridge-connected to the first gate electrode (G1) through a node connection line (171). Additionally, the third source region (S3) may be connected to a fourth drain region (D4) disposed in the same layer. The third drain region (D3) may be electrically connected to the driving semiconductor layer (A1) of the driving thin-film transistor (T1) and the light-emitting control semiconductor layer (A6) of the light-emitting control thin-film transistor (T6). The third gate electrode (G3) may be provided as part of the second scan line (SL2).

[0098] The first initialization thin film transistor (T4) may include a first initialization semiconductor layer comprising an oxide semiconductor material and a fourth gate electrode (G4). The first initialization semiconductor layer may include a fourth channel region (C4), a fourth source region (S4) and a fourth drain region (D4) on both sides of the fourth channel region (C4). The fourth source region (S4) may be electrically connected to the first initialization voltage line (VL1), and the fourth drain region (D4) may be bridge-connected to the first gate electrode (G1) through a node connection line (171). The fourth gate electrode (G4) may be provided as part of the previous scan line (SLp).

[0099] A fourth gate insulating layer (119, FIG. 11) may be disposed between the compensation semiconductor layer and the third gate electrode (G3), and between the first initialization semiconductor layer and the fourth gate electrode (G4), so as to correspond to each channel region.

[0100] The third electrode (CE3) of the second storage capacitor (Cbt) is provided as part of the first scan line (SL1) and can be connected to the second gate electrode (G2) of the switching thin-film transistor (T2). The fourth electrode (CE4) of the second storage capacitor (Cbt) is arranged to overlap with the third electrode (CE3) and can be provided as an oxide semiconductor. The fourth electrode (CE4) is provided in the same layer as the compensation semiconductor layer of the compensation thin-film transistor (T3) and the first initialization semiconductor layer of the first initialization thin-film transistor (T4), and may be an area between the compensation semiconductor layer and the first initialization semiconductor layer. Alternatively, the fourth electrode (CE4) may be provided extending from the first initialization semiconductor layer. Alternatively, the fourth electrode (CE4) may be provided extending from the compensation semiconductor layer.

[0101] The node connection line (171) can be electrically connected to the first electrode (CE1) and the compensation semiconductor layer of the compensation thin-film transistor (T3). The second electrode (CE2) is electrically connected to the first driving voltage line (PL1), and the first driving voltage line (PL1) can be electrically connected to the second driving voltage line (PL2). The first driving voltage line (PL1) and the second driving voltage line (PL2) can be extended in the second direction (y direction). The second electrode (CE2) can be extended in the first direction (x direction) to serve to transmit the first power supply voltage (ELVDD) in the first direction (x direction). Accordingly, a plurality of first driving voltage lines (PL1) and second driving voltage lines (PL2) and a plurality of second electrodes (CE2) can form a mesh structure in the display area (DA).

[0102] In one embodiment, some of the wirings may be provided with two conductive layers disposed on different layers. For example, the previous scan line (SLp) may include a lower scan line (143) and an upper scan line (163) disposed on different layers. The lower scan line (143) may be provided with the same material on the same layer as the second electrode (CE2) of the first storage capacitor (Cst). The lower scan line (143) may be disposed to overlap at least partially with the upper scan line (163). Since the lower scan line (143) and the upper scan line (163) correspond to a part of the third gate electrode of the compensation thin film transistor (T3), the compensation thin film transistor (T3) may have a dual gate structure having control electrodes on the upper and lower parts of the semiconductor layer, respectively.

[0103] Additionally, the second scan line (SL2) may include a lower scan line (145) and an upper scan line (165) disposed on different layers. The lower scan line (145) may be provided with the same material on the same layer as the second electrode (CE2) of the first storage capacitor (Cst). The lower scan line (145) may be disposed to overlap at least partially with the upper scan line (165). Since the lower scan line (145) and the upper scan line (165) correspond to a part of the fourth gate electrode (G4) of the first initialization thin film transistor (T4), the first initialization thin film transistor (T4) may have a dual gate structure having control electrodes on the upper and lower parts of the semiconductor layer, respectively.

[0104] The initialization voltage line (VL) may include a first initialization voltage line (VL1) and a second initialization voltage line (VL2) disposed on different layers. The first initialization voltage line (VL1) may be provided with the same material on the same layer as the second electrode (CE2) of the first storage capacitor (Cst). The second initialization voltage line (VL2) may be provided with the same material on the same layer as the first driving voltage line (PL1).

[0105] FIG. 6 is a schematic cross-sectional view illustrating a display device according to one embodiment of the present invention. FIG. 6 corresponds to a cross-sectional view taken along the line BB' of FIG. 5.

[0106] Referring to FIG. 6, the display device (10) may include a substrate (100). The substrate (100) may include a glass material, a ceramic material, a metal material, or a material having flexible or bendable properties. In one embodiment, when the substrate (100) has flexible or bendable properties, the substrate (100) may include a first base layer, a first barrier layer, a second base layer, and a second barrier layer sequentially stacked. The first base layer and the second base layer may be made of a polymer resin having high heat resistance. For example, the first base layer and the second base layer may include one or more materials selected from the group consisting of polyethersulfone, polyacrylate, polyetherimide, polyethylene naphthalate, polyethylene terephthalate, polyphenylene sulfide, polyarylate, polyimide, polycarbonate, cellulose triacetate, cellulose acetate propionate, and polyarylene ethersulfone. In one embodiment, the first base layer and the second base layer may be provided with polyimide.

[0107] A first barrier layer may be disposed between the first base layer and the second base layer. The first barrier layer is disposed on the first base layer and can reduce or block the penetration of foreign matter, moisture, or outside air from below.

[0108] A second barrier layer may be disposed on the second base layer. The second barrier layer is disposed on the second base layer and can reduce or block the penetration of foreign matter, moisture, or outside air from below.

[0109] The first barrier layer and the second barrier layer are silicon nitride (SiN X ), silicon oxide (SiO X ), silicon oxynitride (SiO₂ X N YIt may include inorganic insulating materials such as aluminum oxide (Al2O3), titanium oxide (TiO2), tantalum oxide (Ta2O5), hafnium oxide (HfO2), or zinc oxide (ZnO). In one embodiment, the first barrier layer and the second barrier layer may be provided with the same material. For example, the first barrier layer and the second barrier layer may be silicon oxide (SiO2). X It may be provided as follows. In one embodiment, the first barrier layer and the second barrier layer may be provided with different materials. For example, the first barrier layer and / or the second barrier layer may be omitted.

[0110] A buffer layer (111) may be disposed on the substrate (100). The buffer layer (111) is located on the substrate (100) and can reduce or block the penetration of foreign matter, moisture, or outside air from below, and can provide a flat upper surface. The buffer layer (111) is silicon nitride (SiN X ), silicon oxide (SiO X ), silicon oxynitride (SiO₂ X N Y It may include inorganic insulating materials such as aluminum oxide (Al2O3), titanium oxide (TiO2), tantalum oxide (Ta2O5), hafnium oxide (HfO2), or zinc oxide (ZnO).

[0111] In one embodiment, the buffer layer (111) may be provided with a first buffer layer and a second buffer layer. In one embodiment, the first buffer layer and the second buffer layer may be provided with the same material. In one embodiment, the first buffer layer and the second buffer layer may be provided with different materials.

[0112] A driving thin-film transistor (T1) (e.g., a first thin-film transistor (TFT1)) and a first storage capacitor (Cst) may be disposed on the buffer layer (111). The first thin-film transistor (TFT1) may include a driving semiconductor layer (A1) and a first gate electrode (G1). The first storage capacitor (Cst) may include a first electrode (CE1) and a second electrode (CE2).

[0113] A first semiconductor layer (1100, FIG. 5) including semiconductor layers of a driving thin-film transistor (T1), a switching thin-film transistor (T2), an operation control thin-film transistor (T5), a light emission control thin-film transistor (T6), and a second initialization thin-film transistor (T7) may be disposed on the buffer layer (111), and FIG. 6 illustrates a driving semiconductor layer (A1) of the driving thin-film transistor (T1), which is a part region of the first semiconductor layer (1100).

[0114] In one embodiment, the driving semiconductor layer (A1) is disposed on the buffer layer (111) and may include polysilicon. In one embodiment, the driving semiconductor layer (A1) may include amorphous silicon. The driving semiconductor layer (A1) may include a first channel region (C1) and a first source region (S1) doped with impurities.

[0115] A first gate insulating layer (113) may be provided to cover the driving semiconductor layer (A1). The first gate insulating layer (113) is made of silicon oxide (SiO₂). X ), silicon nitride (SiN X ), silicon oxynitride (SiO₂ X N Y It may include inorganic insulating materials such as aluminum oxide (Al2O3), titanium oxide (TiO2), tantalum oxide (Ta2O5), hafnium oxide (HfO2), or zinc oxide (ZnO). The first gate insulating layer (113) may be a single layer or a multilayer containing the aforementioned inorganic insulating material.

[0116] A first metal layer (1200) including gate electrodes of a driving thin-film transistor (T1), a switching thin-film transistor (T2), an operation control thin-film transistor (T5), a light emission control thin-film transistor (T6), and a second initialization thin-film transistor (T7) may be disposed on the first gate insulating layer (113), and the first gate electrode (G1) of the driving thin-film transistor (T1) is shown in FIG. 6. Additionally, a third electrode (CE3) of a second storage capacitor (Cbt) and a light emission control line (EL, FIG. 5) may be disposed on the first gate insulating layer (113).

[0117] A first metal layer (1200) including a first gate electrode (G1) of a driving thin-film transistor (T1) and a third electrode (CE3) of a second storage capacitor (Cbt) may be disposed on the first gate insulating layer (113). The first gate electrode (G1) may be disposed to overlap with the driving semiconductor layer (A1), and the third electrode (CE3) may be disposed to overlap with a part of the first initialization semiconductor layer (A4). The first metal layer (1200) may include molybdenum (Mo), aluminum (Al), copper (Cu), titanium (Ti), etc., and may be composed of a single layer or multiple layers. In one embodiment, the first metal layer (1200) may be a single layer of molybdenum (Mo).

[0118] The second gate insulating layer (115) may be provided to cover the first metal layer (1200). The second gate insulating layer (115) is silicon oxide (SiO₂). X ), silicon nitride (SiN X ), silicon oxynitride (SiO₂ X N Y It may include inorganic insulating materials such as aluminum oxide (Al2O3), titanium oxide (TiO2), tantalum oxide (Ta2O5), hafnium oxide (HfO2), or zinc oxide (ZnO2). The second gate insulating layer (115) may be a single layer or a multilayer containing the aforementioned inorganic insulating material.

[0119] A second metal layer (1300) may be disposed on the upper portion of the second gate insulating layer (115), comprising a second electrode (CE2) of the first storage capacitor (Cst), a first initialization voltage line (VL1, FIG. 10), a lower scan line (143, FIG. 10) of the previous scan line (SLp, FIG. 10), and a lower scan line (145) of the second scan line (SL2). The second electrode (CE2) of the first storage capacitor (Cst) may overlap with the first gate electrode (G1) of the driving thin-film transistor (T1) disposed below it. The first gate electrode (G1) and the second electrode (CE2) that overlap with the second gate insulating layer (115) in between may form the first storage capacitor (Cst). In one embodiment, the first gate electrode (G1) may be the first electrode (CE1) of the first storage capacitor (Cst). In one embodiment, the first electrode (CE1) of the first storage capacitor (Cst) may be provided as a separate independent component.

[0120] In one embodiment, the second electrode (CE2) may have an opening (SOP). The opening (SOP) is formed by removing a portion of the second electrode (CE2) and may have a closed shape.

[0121] The lower scan line (145) of the second scan line (SL2) can be positioned to overlap at least partially with the upper scan line (165) of the second scan line (SL2).

[0122] The portion overlapping with the first initialization semiconductor layer (A4) in the lower scan line (143) of the previous scan line (SLp) can function as the lower gate electrode (G4a) of the first initialization thin film transistor (T4).

[0123] In one embodiment, the second metal layer (1300) may comprise aluminum (Al), platinum (Pt), palladium (Pd), silver (Ag), magnesium (Mg), gold (Au), nickel (Ni), neodymium (Nd), iridium (Ir), chromium (Cr), calcium (Ca), molybdenum (Mo), titanium (Ti), tungsten (W), and / or copper (Cu), and may be a single layer or a multilayer of the aforementioned materials. For example, the second metal layer (1300) may be provided with molybdenum (Mo).

[0124] The third gate insulating layer (117) may be provided to cover the second electrode (CE2). The third gate insulating layer (117) is silicon oxide (SiO₂). X ), silicon nitride (SiN X ), silicon oxynitride (SiO₂ X N Y It may include inorganic insulating materials such as aluminum oxide (Al2O3), titanium oxide (TiO2), tantalum oxide (Ta2O5), hafnium oxide (HfO2), or zinc oxide (ZnO2). The third gate insulating layer (117) may be a single layer or a multilayer containing the aforementioned inorganic insulating material.

[0125] A first initialization thin film transistor (T4) (e.g., a second thin film transistor (TFT2)) may be disposed on the third gate insulating layer (117). The second thin film transistor (TFT2) may include a first initialization semiconductor layer (A4) and an upper gate electrode (G4b) (e.g., a second gate electrode).

[0126] A second semiconductor layer (1400) may be disposed on the third gate insulating layer (117). The second semiconductor layer (1400) may include a Zn oxide-based material. For example, the second semiconductor layer (1400) may include Zn oxide, In-Zn oxide, Ga-In-Zn oxide, etc. In one embodiment, the oxide-based semiconductor layer may include an IGZO (In-Ga-Zn-O), ITZO (In-Sn-Zn-O), or IGTZO (In-Ga-Sn-Zn-O) semiconductor material containing metals such as indium (In), gallium (Ga), and tin (Sn) in ZnO.

[0127] The second semiconductor layer (1400) may include each channel region, source region, and drain region of the compensation thin film transistor (T3) and the first initialization thin film transistor (T4), and FIG. 6 illustrates the first initialization semiconductor layer (A4) of the first initialization thin film transistor (T4).

[0128] The second semiconductor layer (1400) may include the fourth electrode (CE4) of the second storage capacitor (Cbt), for example, the fourth electrode (CE4) may be provided as part of the first initialization semiconductor layer (A4) of the first initialization thin film transistor (T4). A second gate insulating layer (115) and a third gate insulating layer (117) are disposed between the third electrode (CE3) and the fourth electrode (CE4) of the second storage capacitor (Cbt), and the second gate insulating layer (115) and the third gate insulating layer (117) may function as dielectric layers of the second storage capacitor (Cbt).

[0129] A fourth gate insulating layer (119) may be provided on the second semiconductor layer (1400). The fourth gate insulating layer (119) may include an inorganic material including an oxide or a nitride. For example, the fourth gate insulating layer (119) may be silicon oxide (SiO₂). X ), silicon nitride (SiN X ), silicon oxynitride (SiO₂ X N YIt may include at least one of the following: aluminum oxide (Al2O3), titanium oxide (TiO2), tantalum oxide (Ta2O5), hafnium oxide (HfO2), or zinc oxide (ZnO). In one embodiment, the fourth gate insulating layer (119) is silicon nitride (SiN X It can be provided as ).

[0130] A third metal layer (1500) may be disposed on the fourth gate insulating layer (119), comprising the upper gate electrode (G4b) of the first initialization thin film transistor (T4), the second initialization voltage line (VL2, FIG. 5), the upper scan line (163, FIG. 5) of the previous scan line (SLp, FIG. 5), and the upper scan line (165) of the second scan line (SL2). The third metal layer (1500) may comprise at least one of molybdenum (Mo), copper (Cu), titanium (Ti), etc., and may be composed of a single layer or multiple layers.

[0131] The upper gate electrode (G4b) of the first initialization thin film transistor (T4) may be a portion that overlaps with the second semiconductor layer (1400) at the upper scan line (163) of the previous scan line (SLp). The upper gate electrode (G4b) of the first initialization thin film transistor (T4) overlaps with the lower gate electrode (G4a) of the first initialization thin film transistor (T4), so that the first initialization thin film transistor (T4) may have a dual gate structure having control electrodes on the upper and lower parts of the first initialization semiconductor layer (A4), respectively.

[0132] An interlayer insulating layer (120) may be disposed on the third metal layer (1500). In one embodiment, the interlayer insulating layer (120) may be disposed to cover the upper gate electrode (G4b) of the first initialization thin film transistor (T4), the second initialization voltage line (VL2, FIG. 5), the upper scan line (163, FIG. 5) of the previous scan line (SLp, FIG. 5), and the upper scan line (165) of the second scan line (SL2).

[0133] At least one of the first metal layer (1200), the second metal layer (1300), and the third metal layer (1500) disposed below the interlayer insulation layer (120) may have a compressive stress or a tensile stress of 200 MPa or less. In one embodiment, the first metal layer (1200), the second metal layer (1300), or the third metal layer (1500) may have a compressive stress or a tensile stress of 200 MPa or less. In another embodiment, the first metal layer (1200) and the second metal layer (1300) may have compressive stress or tensile stress of 200 MPa or less, or the first metal layer (1200) and the third metal layer (1500) may have compressive stress or tensile stress of 200 MPa or less, or the second metal layer (1300) and the third metal layer (1500) may have compressive stress or tensile stress of 200 MPa or less. In yet another embodiment, the first metal layer (1200), the second metal layer (1300), and the third metal layer (1500) may have compressive stress or tensile stress of 200 MPa or less.

[0134] In one embodiment, at least one of the first metal layer (1200), the second metal layer (1300), and the third metal layer (1500) may be formed using a rotary type sputtering device. Unlike a planar type sputtering device in which ground voltage is applied only to the edge portion of a planar target, the rotary type sputtering device may have a plurality of cylindrical targets spaced apart with a ground portion to which ground voltage is applied, thereby improving the uniformity of the metal layer formed. Accordingly, the metal layer formed using the rotary type sputtering device may have a compressive stress or a tensile stress of 200 MPa or less, as the density on the center of the substrate (100) and the density on the edge portion are reduced. In one embodiment, the first metal layer (1200), the second metal layer (1300), or the third metal layer (1500) may be formed using a rotary sputtering device. In another embodiment, the first metal layer (1200) and the second metal layer (1300) may be formed using a rotary sputtering device, or the first metal layer (1200) and the third metal layer (1500) may be formed using a rotary sputtering device, or the second metal layer (1300) and the fourth metal layer (1500) may be formed using a rotary sputtering device. In yet another embodiment, the first metal layer (1200), the second metal layer (1300), and the third metal layer (1500) may be formed using a rotary sputtering device.

[0135] In one embodiment, the interlayer insulating layer (120) may include at least one oxide film (121), a first nitride film (123) disposed on the oxide film (121), and a second nitride film (125) disposed on the first nitride film (123).

[0136] The oxide film (121) of the interlayer insulation layer (120) is silicon oxide (SiO₂). XIt may include ). In one embodiment, the thickness (d1) of the oxide film (121) may be about 3000 Å. The oxide film (121) may be positioned to be in direct contact with the third metal layer (1500).

[0137] The first nitride film (123) and the second nitride film (125) are silicon nitride (SiN X It may include ). The thickness (d2) of the first nitride film (123) may be about 500 Å. In one embodiment, the thickness (d2) of the first nitride film (123) may be 400 Å to 600 Å. The thickness (d2) of the first nitride film (123) may be smaller than the thickness (d3) of the second nitride film (125). In one embodiment, the thickness (d3) of the second nitride film (125) may be about 2500 Å. In another embodiment, the thickness (d3) of the second nitride film (125) may be about 3500 Å. In one embodiment, the thickness (d3) of the second nitride film (125) may be about 2300 Å to 3700 Å. The total thickness (Dt) of the interlayer insulation layer (120) may be 5700 Å to 7300 Å.

[0138] The first density of the first nitride film (123) may be higher than the second density of the second nitride film (125). In one embodiment, the hydrogen content of the first nitride film (123) may be lower than the hydrogen content of the second nitride film (125). Accordingly, the first nitride film (123) may have compressive stress, and the second nitride film (125) may have tensile stress. As the thickness (Dt) of the interlayer insulation layer (120) increases, the rigidity of the interlayer insulation layer (120) increases, thereby improving the impact resistance of the display device (10). However, the first nitride film (123) has a high density, which can effectively prevent external air, such as moisture, from penetrating into the second semiconductor layer (1400). However, if the first nitride film (123) becomes thick, the increase in compressive stress may cause the center of the substrate (100) to bulge out more than the edge portion, thereby causing the substrate (100) to bend. Therefore, by forming a second nitride film (125) thickly, which has a second density lower than the first density of the first nitride film (123), the bending of the substrate (100) can be prevented or reduced.

[0139] A fourth metal layer (1600) including a first driving voltage line (PL1) and a node connection line (171) may be disposed on the interlayer insulation layer (120). The fourth metal layer (1600) may be provided with a highly conductive material such as a metal or a conductive oxide. For example, the fourth metal layer (1600) may be composed of a single layer or multiple layers including at least one of aluminum (Al), copper (Cu), and titanium (Ti).

[0140] The first driving voltage line (PL1) can be connected to the second electrode (CE2) of the first storage capacitor (Cst) through a contact hole formed in the third gate insulating layer (117), the fourth gate insulating layer (119), and the interlayer insulating layer (120).

[0141] One end of the node connection line (171) can be connected to the first gate electrode (G1) through a contact hole penetrating the interlayer insulation layer (120), the fourth gate insulation layer (119), the third gate insulation layer (117), and the second gate insulation layer (115). The other end of the node connection line (171) can be connected to the second semiconductor layer (1400), for example, the fourth electrode (CE4) of the second storage capacitor (Cbt) or the first initialization semiconductor layer (A4), through a contact hole penetrating the interlayer insulation layer (120).

[0142] A first flattening layer (131) may be disposed on the fourth metal layer (1600). A fifth metal layer (1700) including a data line (DL) and a second driving voltage line (PL2) may be disposed on the first flattening layer (131). The fifth metal layer (1700) may be provided with a highly conductive material such as a metal or a conductive oxide. For example, the fifth metal layer (1700) may be composed of a single layer or multiple layers including at least one of aluminum (Al), copper (Cu), and titanium (Ti).

[0143] A second flattening layer (133) may be disposed on the fifth metal layer (1700). The second flattening layer (133) may have a flat upper surface so that a pixel electrode (210) disposed thereon can be formed flatly. The first flattening layer (131) and the second flattening layer (133) may include an organic material or an inorganic material and may have a single-layer structure or a multi-layer structure. For example, the first planarization layer (131) and the second planarization layer (133) may include general-purpose polymers such as BCB (Benzocyclobutene), polyimide, HMDSO (Hexamethyldisiloxane), polymethylmethacrylate (PMMA), or polystyrene (PS), polymer derivatives having a phenolic group, acrylic polymers, imide polymers, aryl ether polymers, amide polymers, fluorine polymers, p-xylene polymers, or vinyl alcohol polymers. Meanwhile, the first planarization layer (131) and the second planarization layer (133) may include inorganic insulating materials such as silicon oxide (SiOX), silicon nitride (SiNX), silicon oxynitride (SiOXNY), aluminum oxide (Al2O3), titanium oxide (TiO2), tantalum oxide (Ta2O5), hafnium oxide (HfO2), or zinc oxide (ZnO). In one embodiment, when forming the second flattening layer (133), chemical mechanical polishing may be performed on the upper surface of the layer to provide a flat upper surface after forming the layer.

[0144] An organic light-emitting diode (OLED) including a pixel electrode (210), an intermediate layer (220), and a counter electrode (230) may be disposed on the second flattening layer (133).

[0145] A pixel electrode (210) may be disposed on the second planarization layer (133). The pixel electrode (210) may include a conductive oxide such as indium tin oxide (ITO), indium zinc oxide (IZO), zinc oxide (ZnO), indium oxide (In2O3), indium gallium oxide (IGO), or aluminum zinc oxide (AZO). The pixel electrode (210) may include a reflective film comprising silver (Ag), magnesium (Mg), aluminum (Al), platinum (Pt), palladium (Pd), gold (Au), nickel (Ni), neodymium (Nd), iridium (Ir), chromium (Cr), or a compound thereof. For example, the pixel electrode (210) may have a structure having films formed of ITO, IZO, ZnO, or In2O3 above and below the aforementioned reflective film. In this case, the pixel electrode (210) may have a structure laminated with indium tin oxide (ITO) / silver (Ag) / indium tin oxide (ITO).

[0146] The pixel defining film (135) may be disposed on the second flattening layer (133). The pixel defining film (135) may be disposed on the second flattening layer (133) and may cover the edge of the pixel electrode (210). An opening (135OP) that exposes at least a portion of the pixel electrode (210) may be defined in the pixel defining film (135).

[0147] The pixel defining film (135) can prevent an arc, etc. from occurring at the edge of the pixel electrode (210) by increasing the distance between the edge of the pixel electrode (210) and the counter electrode (230) above the pixel electrode (210). The pixel defining film (135) can be formed by a method such as spin coating using an organic insulating material such as polyimide, polyamide, acrylic resin, benzocyclobutene, HMDSO (hexamethyldisiloxane), and phenolic resin.

[0148] Although not illustrated, a spacer for preventing mask imprinting may be further disposed on the pixel defining film (135). The spacer may be formed integrally with the pixel defining film (135). For example, the spacer and the pixel defining film (135) may be formed simultaneously in the same process using a halftone mask process.

[0149] An intermediate layer (220) may be disposed inside the opening (135OP) of the pixel defining film (135) to correspond to the pixel electrode (210). The intermediate layer (220) may include a light-emitting layer. The light-emitting layer may include a high-molecular-weight organic material or a low-molecular-weight organic material and may emit red, green, blue, or white light.

[0150] In one embodiment, the intermediate layer (220) may further include an organic functional layer disposed on the upper and / or lower portion of the light-emitting layer. The organic functional layer may include a first functional layer and / or a second functional layer. In one embodiment, the first functional layer and / or the second functional layer may be omitted.

[0151] The first functional layer may be disposed below the light-emitting layer. The first functional layer may be a single layer or a multilayer made of organic material. The first functional layer may be a hole transport layer (HTL) having a single-layer structure. Alternatively, the first functional layer may include a hole injection layer (HIL) and a hole transport layer (HTL).

[0152] The second functional layer may be disposed on top of the light-emitting layer. The second functional layer may be a single layer or a multilayer made of organic material. The second functional layer may include an electron transport layer (ETL) and / or an electron injection layer (EIL).

[0153] A counter electrode (230) may be disposed on the intermediate layer (220). The counter electrode (230) may include a conductive material with a low work function. For example, the counter electrode (230) may include a (semi)transparent layer including silver (Ag), magnesium (Mg), aluminum (Al), platinum (Pt), palladium (Pd), gold (Au), nickel (Ni), neodymium (Nd), iridium (Ir), chromium (Cr), lithium (Li), calcium (Ca), or alloys thereof. Alternatively, the counter electrode (230) may further include a layer such as ITO, IZO, ZnO, or In2O3 on the (semi)transparent layer including the aforementioned materials.

[0154] In one embodiment, a capping layer (not shown) containing an organic material may be formed on the counter electrode (230). The capping layer may be a layer provided to protect the counter electrode (230) while simultaneously increasing light extraction efficiency. The capping layer may contain an organic material with a higher refractive index than the counter electrode (230). In one embodiment, the capping layer may be provided with an inorganic material.

[0155] Although not shown in FIG. 6, the display device (10) may include a thin film encapsulation layer (400, FIG. 2) that shields an organic light-emitting diode (OLED). The thin film encapsulation layer (400) may include at least one organic encapsulation layer and at least one inorganic encapsulation layer. At least one organic encapsulation layer and at least one inorganic encapsulation layer may be stacked alternately.

[0156] An input sensing member (TSL) and an optical function member (OFL) may be disposed on the thin film encapsulation layer (400).

[0157] FIG. 7 is a cross-sectional view schematically illustrating a display device according to another embodiment of the present invention.

[0158] The display device (10) of FIG. 7 is similar to the display device (10) shown in FIG. 6, but differs in that a third nitride film (127) is further disposed between the first nitride film (123) and the second nitride film (125) of the interlayer insulation layer (120). Hereinafter, descriptions of components identical or similar to those of the display device (10) shown in FIG. 6 will be omitted, and the description will focus on the interlayer insulation layer (120).

[0159] Referring to FIG. 7, the interlayer insulating layer (120) may be disposed on a third metal layer (1500) comprising the upper gate electrode (G4b) of the first initialization thin film transistor (T4), the second initialization voltage line (VL2, FIG. 5), the upper scan line (163, FIG. 5) of the previous scan line (SLp, FIG. 5), and the upper scan line (165) of the second scan line (SL2).

[0160] In one embodiment, the interlayer insulating layer (120) may include at least one oxide film (121), a first nitride film (123), a second nitride film (125), and a third nitride film (127).

[0161] The oxide film (121) of the interlayer insulating layer (120) may include silicon oxide (SiOX). In one embodiment, the thickness of the oxide film (121) may be about 3000 Å. The oxide film (121) may be positioned to be in direct contact with the third metal layer (1500).

[0162] In one embodiment, a first nitride film (123) may be disposed on an oxide film (121), a third nitride film (127) may be disposed on the first nitride film (123), and a second nitride film (125) may be disposed on the third nitride film (127).

[0163] The first nitride film (123) to the third nitride film (127) are silicon nitride (SiN XIt may include ). The thickness of the first nitride film (123) may be about 500 Å or less. The thickness of the first nitride film (123) may be less than the thickness of the second nitride film (125) and the third nitride film (127). In one embodiment, the thickness of the second nitride film (125) may be about 2500 Å. In another embodiment, the thickness of the second nitride film (125) may be about 3500 Å. In one embodiment, the thickness of the second nitride film (125) may be about 2300 Å to 3700 Å.

[0164] The first density of the first nitride film (123) may be higher than the second density of the second nitride film (125) and the third density of the third nitride film (127). The second density of the second nitride film (125) may be lower than the third density of the third nitride film (127). That is, the first density of the first nitride film (123) closest to the oxide film (121) is the highest, the second density of the second nitride film (125) farthest from the oxide film (121) is the lowest, and the third density of the third nitride film (127) interposed between the first nitride film (123) and the second nitride film (125) may have a value between the first density and the second density.

[0165] In one embodiment, the hydrogen content of the first nitride film (123) may be lower than the hydrogen content of the second nitride film (125) and the hydrogen content of the third nitride film (127). The hydrogen content of the second nitride film (125) may be higher than the hydrogen content of the third nitride film (127). That is, the hydrogen content of the first nitride film (123) closest to the oxide film (121) is the lowest, the hydrogen content of the second nitride film (125) farther from the oxide film (121) is the highest, and the hydrogen content of the third nitride film (127) interposed between the first nitride film (123) and the second nitride film (125) may have a value between the hydrogen content of the first nitride film (123) and the hydrogen content of the second nitride film (125).

[0166] Accordingly, the first nitride film (123) has compressive stress, the second nitride film (125) has tensile stress, and the stress of the third nitride film (127) interposed between the first nitride film (123) and the second nitride film (125) can have a value between the stress of the first nitride film (123) and the stress of the second nitride film (125).

[0167] FIG. 7 illustrates a third nitride film (127) interposed between the first nitride film (123) and the second nitride film (125), but according to other embodiments, one or more nitride films may be disposed between the first nitride film (123) and the second nitride film (125).

[0168] The density of one or more nitride films disposed between the first nitride film (123) and the second nitride film (125) may have a value between the first density of the first nitride film (123) and the second density of the second nitride film (125). In one embodiment, the one or more nitride films disposed between the first nitride film (123) and the second nitride film (125) may have a higher density closer to the first nitride film (123) and a lower density closer to the second nitride film (125).

[0169] Likewise, the hydrogen content of one or more nitride films disposed between the first nitride film (123) and the second nitride film (125) may have a value between the hydrogen content of the first nitride film (123) and the hydrogen content of the second nitride film (125). In one embodiment, one or more nitride films disposed between the first nitride film (123) and the second nitride film (125) may have a lower hydrogen content closer to the first nitride film (123) and a higher hydrogen content closer to the second nitride film (125).

[0170] In this way, by placing a nitride film with a different density or hydrogen content between the first nitride film (123) and the second nitride film (125), a lower stress can be applied toward the upper part of the interlayer insulating layer (120). Accordingly, while increasing the thickness of the interlayer insulating layer (120), bending of the substrate (100) can be prevented or reduced.

[0171] FIGS. 8 to 10 are cross-sectional views sequentially illustrating a method for manufacturing a display device according to an embodiment of the present invention.

[0172] Referring to FIGS. 8 through 10, first, transistors and storage capacitors are formed on a substrate (100). In this regard, FIG. 8 illustrates the formation of a driving thin-film transistor (T1), a first initialization thin-film transistor (T4), a first storage capacitor (Cst), and a second storage capacitor (Cbt). A buffer layer (111) may be formed prior to forming the transistors and storage capacitors on the substrate (100).

[0173] A first semiconductor layer (1100) may be formed on the buffer layer (111). The first semiconductor layer (1100) may include low-temperature polysilicon. A portion of the first semiconductor layer (1100) may correspond to the driving semiconductor layer (A1) of the driving thin-film transistor (T1).

[0174] A first gate insulating layer (113) may be formed on the first semiconductor layer (1100). The first gate insulating layer (113) may be formed to cover the entire substrate (100).

[0175] A first metal layer (1200) may be formed on the first gate insulating layer (113). The first metal layer (1200) may include the first gate electrode (G1) of the driving transistor (T1) and the third electrode (CE3) of the second storage capacitor (Cbt). The first metal layer (1200) may include molybdenum (Mo), aluminum (Al), copper (Cu), titanium (Ti), etc., and may be composed of a single layer or multiple layers. In one embodiment, the first metal layer (1200) may be a single layer of molybdenum (Mo). In one embodiment, the first metal layer (1200) may have compressive stress or tensile stress of 200 MPa or less.

[0176] A second gate insulating layer (115) may be formed on the first metal layer (1200). The second gate insulating layer (115) may be formed to cover the entire substrate (100).

[0177] A second metal layer (1300) may be formed on the second gate insulating layer (115). The second metal layer (1300) may include the second electrode (CE2) of the first storage capacitor (Cst) and the lower scan line (145) of the second scan line (SL2). The second metal layer (1300) may include molybdenum (Mo), aluminum (Al), copper (Cu), titanium (Ti), etc., and may be composed of a single layer or multiple layers. In one embodiment, the first metal layer (1200) may be a single layer of molybdenum (Mo). In one embodiment, the second metal layer (1300) may have compressive stress or tensile stress of 200 MPa or less.

[0178] A third gate insulating layer (117) may be formed on the second metal layer (1300). The third gate insulating layer (117) may be formed to cover the entire substrate (100).

[0179] A second semiconductor layer (1400) may be formed. The second semiconductor layer (1400) may include an oxide semiconductor material. The oxide semiconductor material is a Zn oxide-based material and may include Zn oxide, In-Zn oxide, Ga-In-Zn oxide, etc. In one embodiment, the oxide-based semiconductor layer may include an IGZO (In-Ga-Zn-O), ITZO (In-Sn-Zn-O), or IGTZO (In-Ga-Sn-Zn-O) semiconductor containing metals such as indium (In), gallium (Ga), and tin (Sn) in ZnO. A portion of the second semiconductor layer (1400) may correspond to the first initialization semiconductor layer of the first initialization thin-film transistor (T4).

[0180] A fourth gate insulating layer (119) may be formed on the second semiconductor layer (1400). In one embodiment, the fourth gate insulating layer (119) may be formed to cover the entire substrate (100). In another embodiment, the fourth gate insulating layer (119) may be patterned to correspond to the second initialization voltage line (VL2, FIG. 10), the upper scan line (163, FIG. 10) of the previous scan line (SLp, FIG. 10), and the upper scan line (165) of the second scan line (SL2), respectively, which are positioned on the upper surface of the layer.

[0181] A third metal layer (1500) may be formed on the fourth gate insulating layer (119). The third metal layer (1500) may include the upper gate electrode (G4b) of the first initialization thin film transistor (T4) and the upper scan line (165) of the second scan line (SL2). The third metal layer (1500) may include at least one of molybdenum (Mo), copper (Cu), titanium (Ti), etc., and may be composed of a single layer or multiple layers. In one embodiment, the third metal layer (1500) may have a compressive stress or a tensile stress of 200 MPa or less.

[0182] In one embodiment, any one of the first metal layer (1200), the second metal layer (1300), and the third metal layer (1500) can be formed using a rotary type sputtering device. The metal layer formed using the rotary type sputtering device has improved uniformity, so that after the interlayer insulation layer (120, FIG. 11) is formed, the bending of the substrate (100) caused by stress in the interlayer insulation layer (120) can be prevented or reduced.

[0183] Referring to FIG. 9, an interlayer insulating layer (120) may subsequently be formed on the third metal layer (1500). The interlayer insulating layer (120) may include at least one oxide film and a plurality of nitride films. In this regard, FIG. 9 illustrates that the interlayer insulating layer (120) comprises one oxide film (121), a first nitride film (123), and a second nitride film (125), but the present invention is not limited thereto. In one embodiment, the interlayer insulating layer (120) may further include one or more nitride films disposed between the first nitride film (123) and the second nitride film (125).

[0184] The oxide film (121) is silicon oxide (SiO₂). X It may include ). In one embodiment, the thickness (d1) of the oxide film (121) may be formed to be about 3000 Å.

[0185] A first nitride film (123) and a second nitride film (125) may be sequentially formed on the oxide film (121). The first nitride film (123) and the second nitride film (125) are silicon nitride (SiN X It may include ). In the process of forming the first nitride film (123) and the second nitride film (125), by maintaining the hydrogen partial pressure in the chamber when forming the first nitride film (123) lower than the hydrogen partial pressure in the chamber when forming the second nitride film (125), the first density, which is the density of the first nitride film (123), may be higher than the second density, which is the density of the second nitride film (125). Likewise, the hydrogen content of the first nitride film (123) may be lower than the hydrogen content of the second nitride film (125).

[0186] As described above, one or more nitride films having different densities may be formed between the first nitride film (123) and the second nitride film (125). In one embodiment, the hydrogen partial pressure in the chamber during the process of forming the first nitride film (123) may be increased stepwise from the hydrogen partial pressure in the chamber during the process of forming the second nitride film (125) to form each nitride film continuously.

[0187] The thickness (d2) of the first nitride film (123) may be formed to be about 500 Å. In one embodiment, the thickness (d2) of the first nitride film (123) may be 400 Å to 600 Å. The thickness (d2) of the first nitride film (123) may be formed to be smaller than the thickness (d3) of the second nitride film (125). In one embodiment, the thickness (d3) of the second nitride film (125) may be about 2500 Å. In another embodiment, the thickness (d3) of the second nitride film (125) may be about 3500 Å. In one embodiment, the thickness (d3) of the second nitride film (125) may be about 2300 Å to 3700 Å. The total thickness (Dt) of the interlayer insulation layer (120) may be 5700 Å to 7300 Å.

[0188] In one embodiment, the first nitride film (123) formed in a low-hydrogen atmosphere may have a stress of about -435 MPa, and the second nitride film (125) formed in a high-hydrogen atmosphere may have a stress of about 170 MPa. Accordingly, compressive stress may be applied to the first nitride film (123), and tensile stress may be applied to the second nitride film (125). By forming the second nitride film (125) thickly on the first nitride film (123), the bending of the substrate (100) in which the center of the substrate (100) rises convexly higher than the edge portion due to the interlayer insulating layer (120) can be prevented or reduced.

[0189] Referring to FIG. 10, a fourth metal layer (1600) can be formed on an interlayer insulating layer (120). The fourth metal layer (1600) may include a first driving voltage line (PL1) and a node connecting line (171). The fourth metal layer (1600) may be made of a highly conductive material such as a metal or a conductive oxide. For example, the fourth metal layer (1600) may be composed of a single layer or multiple layers including at least one of aluminum (Al), copper (Cu), and titanium (Ti).

[0190] Before forming the fourth metal layer (1600), contact holes penetrating the interlayer insulating layer (120), the fourth gate insulating layer (119), the third gate insulating layer (117), and the second gate insulating layer (115), and contact holes penetrating the interlayer insulating layer (120), the fourth gate insulating layer (119), the third gate insulating layer (117), the second gate insulating layer (115), and the first gate insulating layer (113) can be formed. To form these contact holes, the substrate (100) can be moved by hydraulic pressure of air. Bending of the substrate (100) can hinder the movement of the substrate (100) using hydraulic pressure of air, which may result in defects in the contact holes. As the interlayer insulating layer (120) is composed of at least one oxide film (121) and a first nitride film (123) and a second nitride film (125) having different densities, the bending of the substrate (100) can be prevented or reduced, and the defects of the contact hole can also be reduced.

[0191] A first flattening layer (131), a fifth metal layer (1700), and a second flattening layer (133) may be sequentially formed on the fourth metal layer (1600). The first flattening layer (131) and the second flattening layer (133) may include organic or inorganic materials and may have a single-layer or multi-layer structure. The second flattening layer (133) may have a flat upper surface so that a pixel electrode (210) disposed thereon can be formed flatly.

[0192] An organic light-emitting diode (OLED) including a pixel electrode (210), an intermediate layer (220), and a counter electrode (230) can be formed on the second flattening layer (133).

[0193] FIG. 11 is a schematic diagram illustrating the steps of forming a metal layer according to one embodiment of the present invention.

[0194] Referring to FIG. 11, in one embodiment, at least one metal layer among the first metal layer (1200, FIG. 6), the second metal layer (1300, FIG. 6) and the third metal layer (1500, FIG. 6) can be formed using a rotary sputtering device (700) as shown in FIG. 11.

[0195] A rotary sputtering device (700) may be equipped with a support member (710) that supports a substrate (100), a plurality of cylindrical targets (720), and a plurality of ground members (730).

[0196] The substrate (100) can be fixed to the support member (710). The support member (710) can prevent the substrate (100) from moving or shaking while the deposition process on the substrate (100) is in progress.

[0197] A plurality of cylindrical targets (720) may be provided and spaced apart from each other. Each cylindrical target (720) may rotate during the deposition process and provide a deposition material on the substrate (100).

[0198] A plurality of grounding sections (730) that are grounded or provide grounding power may be arranged between the cylindrical targets (720). Accordingly, the rotary sputtering device (700) can form a plasma having an improved uniformity distribution across the entire surface of the substrate (100) during the deposition process.

[0199] At least one metal layer among the first metal layer (1200, FIG. 6), the second metal layer (1300, FIG. 6), and the third metal layer (1500, FIG. 6) is formed using a rotary sputtering device (700), thereby reducing the difference in stress applied to a portion formed on the center of the substrate (100) and a portion formed on the edge of the substrate (100). Accordingly, after the interlayer insulating layer (120, FIG. 6) is formed, the bending of the substrate (100) caused by the stress of the interlayer insulating layer (120) can be prevented or reduced.

[0200] FIG. 12 is a graph showing the height difference of the upper surface of a display device according to a comparative example and embodiments of the present invention.

[0201] The comparative example includes an oxide film having an interlayer insulating layer with a thickness of about 3,000 Å and a nitride film having a thickness of 2,000 Å. Example 1 includes an oxide film having an interlayer insulating layer with a thickness of about 3,000 Å, a first nitride film having a thickness of about 500 Å, and a second nitride film having a thickness of about 2,500 Å and a second density greater than the first density of the first nitride film. Example 2 includes an oxide film having an interlayer insulating layer with a thickness of about 3,000 Å, a first nitride film having a thickness of about 500 Å, and a second nitride film having a thickness of about 3,500 Å and a second density greater than the first density of the first nitride film. The first metal layer, the second metal layer, and the third metal layer of the comparative example, Example 1, and Example 2 were each formed using a planar sputtering apparatus.

[0202] Example 3 comprises an oxide film having an interlayer insulating layer with a thickness of about 3000 Å, a first nitride film having a thickness of about 500 Å, and a second nitride film having a thickness of about 2500 Å and a second density greater than the first density of the first nitride film. Example 4 comprises an oxide film having an interlayer insulating layer with a thickness of about 3000 Å, a first nitride film having a thickness of about 500 Å, and a second nitride film having a thickness of about 3500 Å and a second density greater than the first density of the first nitride film. The second metal layer and the third metal layer of Examples 3 and 4 were formed using a rotary sputtering apparatus.

[0203] FIG. 12 shows the Z range value based on the height difference measured at several points from the upper surface of the stage supporting the substrate to the upper surface of the interlayer insulation layer of the display device.

[0204] If the Z range value is 150 μm or more, defects in the contact hole may occur due to bending of the substrate. Referring to Examples 1 and 2, it can be seen that even though the thickness of the interlayer insulation layer increased by about 1000 Å to 2000 Å, the Z range value remained similar or decreased further.

[0205] Referring to Examples 3 and 4, it can be seen that the Z range value is further lowered by controlling the stress of the second metal layer and the third metal layer by forming the second metal layer and the third metal layer with a rotary sputtering device.

[0206] Accordingly, the display device according to the embodiments of the present invention can improve impact resistance by increasing the thickness of the interlayer insulation layer, while also reducing the defect rate caused by bending of the substrate.

[0207] The present invention has been described with reference to the embodiments illustrated in the drawings, but this is merely illustrative, and those skilled in the art will understand that various modifications and equivalent alternative embodiments are possible therefrom. Accordingly, the true technical scope of protection of the present invention should be determined by the technical spirit of the appended claims. Explanation of the symbols

[0208] 10: Display device 100: Substrate 120: Interlayer insulation layer 121: Oxide film 123: First nitride film 125: Second nitride film 1100: First semiconductor layer 1200: First metal layer 1300: Second metal layer 1400: Second semiconductor layer 1500: Third metal layer 1600: Fourth metal layer 1700: 5th metal layer 700: Sputtering device

Claims

Claim 1 A display device comprising: a substrate; a first semiconductor layer disposed on the substrate; a second semiconductor layer disposed on the first semiconductor layer; an interlayer insulating layer disposed on the second semiconductor layer and comprising a plurality of inorganic insulating films; a source electrode or a drain electrode disposed on the interlayer insulating layer and respectively connected to the first semiconductor layer or the second semiconductor layer; and an organic light-emitting element connected to the source electrode or the drain electrode; wherein the plurality of inorganic insulating films comprises at least one oxide film, a first nitride film disposed on the oxide film and having a first density, a second nitride film disposed on the first nitride film and having a second density lower than the first density, and a third nitride film disposed between the first nitride film and the second nitride film, wherein the third nitride film has a third density lower than the first density and higher than the second density. Claim 2 A display device according to claim 1, wherein the hydrogen content of the first nitride film is lower than the hydrogen content of the second nitride film. Claim 3 A display device according to claim 1, wherein the first nitride film has compressive stress and the second nitride film has tensile stress. Claim 4 A display device according to claim 1, wherein the thickness of the first nitride film is smaller than the thickness of the at least one oxide film. Claim 5 A display device according to claim 4, wherein the thickness of the first nitride film is smaller than the thickness of the second nitride film. Claim 6 A display device according to claim 4, wherein the thickness of the interlayer insulating layer is 5500 Å to 7500 Å and the thickness of the first nitride film is 400 Å to 600 Å. Claim 7 delete Claim 8 A display device according to claim 1, wherein the hydrogen content of the third nitride film is higher than the hydrogen content of the first nitride film and lower than the hydrogen content of the second nitride film. Claim 9 A display device according to claim 1, further comprising: a first metal layer disposed on the first semiconductor layer; a second metal layer disposed between the first metal layer and the second semiconductor layer; and a third metal layer disposed between the second semiconductor layer and the interlayer insulating layer, wherein at least one of the first to third metal layers has a compressive stress or a tensile stress of 200 MPa or less. Claim 10 A method for manufacturing a display device, comprising: a step of forming a first semiconductor layer on a substrate; a step of forming a second semiconductor layer on the first semiconductor layer; and a step of forming an interlayer insulating layer comprising a plurality of inorganic insulating films on the second semiconductor layer; wherein the step of forming the interlayer insulating layer comprises: a step of forming at least one oxide film on the second semiconductor layer; a step of forming a first nitride film having a first density on the at least one oxide film; a step of forming a third nitride film having a third density lower than the first density on the first nitride film; and a step of forming a second nitride film having a second density lower than the third density on the third nitride film. Claim 11 A method for manufacturing a display device according to claim 10, wherein the hydrogen partial pressure in the chamber during the step of forming the first nitride film is lower than the hydrogen partial pressure in the chamber during the step of forming the second nitride film. Claim 12 A method for manufacturing a display device according to claim 10, wherein the first nitride film has a thickness of 400 Å to 600 Å. Claim 13 A method for manufacturing a display device according to claim 12, wherein the interlayer insulating layer has a thickness of 5500 Å to 7500 Å. Claim 14 delete Claim 15 A method for manufacturing a display device according to claim 10, wherein in the step of forming the third nitride film, the hydrogen partial pressure in the chamber is higher than the hydrogen partial pressure in the chamber in the step of forming the first nitride film, and lower than the hydrogen partial pressure in the chamber in the step of forming the second nitride film. Claim 16 A method for manufacturing a display device according to claim 10, further comprising: a step of forming a first metal layer on the first semiconductor layer disposed between the step of forming the first semiconductor layer and the step of forming the second semiconductor layer; a step of forming a second metal layer on the first metal layer; and a step of forming a third metal layer on the second semiconductor layer disposed between the step of forming the second semiconductor layer and the step of forming the interlayer insulating layer. Claim 17 A method for manufacturing a display device according to claim 16, wherein at least one of the first to third metal layers has a compressive stress or a tensile stress of 200 MPa or less. Claim 18 A method for manufacturing a display device according to claim 16, wherein at least one of the steps of forming the first metal layer, forming the second metal layer, and forming the third metal layer is formed using a rotary sputtering device having a plurality of cylindrical targets. Claim 19 A method for manufacturing a display device according to claim 18, wherein the plurality of cylindrical targets are spaced apart with a ground portion in between. Claim 20 A method for manufacturing a display device according to claim 10, wherein the substrate is placed on a stage, and the height difference between the upper surface of the stage measured at the center of the substrate and the upper surface of the interlayer insulating layer measured at the edge of the substrate is 150 μm or less.

Citation Information

Patent Citations

  • Sputtering device

    KR1020150113828A

  • Thin film transistor substrate and display apparatus comprising the same

    KR1020200143562A

  • Display device and method of fabricating for display device

    KR1020210117389A

  • Displays With Silicon and Semiconducting-Oxide Top-Gate Thin-Film Transistors

    US20180277614A1