Glass Spacer and Hard Disc Drive Device
Patent Information
- Application Number
- LAP839
- Authority / Receiving Office
- LA · LA
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2017-09-29
- Filing Date
- 2018-10-01
- Publication Date
- 2024-11-22
AI Technical Summary
Conventional hard disk drive (HDD) devices face challenges in increasing storage capacity due to limitations in recording density and the generation of fine particles from ring-shaped spacers, which can lead to adhesion issues between magnetic disks and spacers, affecting long-term reliability and ease of separation during maintenance.
A ring-shaped glass spacer with a surface roughness of 1.0 μm or less and an average slope of 0.02 or more is used, along with a metal film on its surface to reduce adhesion and prevent close contact with magnetic disks, enhancing separation and reducing particle generation.
The solution effectively suppresses adhesion between the spacer and magnetic disks, preventing close contact and reducing fine particle generation, thereby improving the long-term reliability and ease of maintenance in HDD devices, especially with multiple disks.
Smart Images

Figure 00000000_0000_ABST 
Figure 00000000_0001_ABST
Abstract
Description
Glass spacer and hard disk drive device
[0001] The present invention relates to a ring-shaped glass spacer provided in contact with a magnetic disk in a magnetic recording hard disk drive, and to a hard disk drive using this glass spacer.
[0002] With the recent rise of cloud computing, many hard disk drives (HDDs) are used in cloud data centers to increase storage capacity. Consequently, there is a demand for larger storage capacities in each HDD compared to conventional models. Conventional HDDs have improved recording density by narrowing the floating distance between the magnetic head and the magnetic disk, or by miniaturizing the magnetic particles on the magnetic disk. However, in recent years, these measures are approaching their physical limits, and therefore cannot adequately meet the demand for larger storage capacities in HDDs. For this reason, increasing the number of magnetic disks installed in an HDD is being considered.
[0003] Incidentally, HDD devices are equipped with ring-shaped magnetic disk spacers between the magnetic disks to hold them apart. These spacers function to ensure that the magnetic disks do not touch each other and are positioned precisely spaced apart. However, since the spacers do come into contact with the magnetic disks, friction caused by relative misalignment between the disks and spacers due to this contact can generate foreign matter such as fine particles from the spacers. In this case, the long-term reliability of the HDD device is easily compromised by the generated fine particles. Therefore, it is desirable to reduce the amount of fine particles generated from the spacers.
[0004] As such a spacer, a glass spacer is known in which the average surface roughness of the portion in contact with the substrate (the main surface of the spacer) is 0.001 to 0.005 μm (Patent Document 1).
[0005] Patent No. 4136268
[0006] In the above-mentioned spacer, the surface roughness of the main surface is small, which can suppress the generation of fine particles. However, reducing the surface roughness of the main surface of the spacer increases the adhesion force between the spacer and the magnetic disk, which may lead to the problems described below.
[0007] When glass spacers and magnetic disks are assembled into an HDD device, their inner holes are alternately inserted into the HDD device's spindle, stacked, and then pressed down from the spindle axis direction to assemble them into the HDD device. The assembled HDD device undergoes inspections such as performance tests. In HDD devices where defects are found during performance tests, the stacked magnetic disks and spacers are sequentially removed from the spindle to remove the defective magnetic disk. At this time, because the spacers and magnetic disks are pressed down strongly in the spindle axis direction and in contact, they may become tightly adhered and impossible to separate. Therefore, it is preferable to minimize the adhesion force between the magnetic disks and spacers as much as possible. In particular, when the number of magnetic disks mounted in an HDD device is large, the number of spacers between the magnetic disks also increases, further increasing the possibility of adhesion between the magnetic disks and spacers. In recent years, in order to improve recording density, the surface roughness of the main surface of magnetic disks has become even smaller, so the above adhesion problem has become even more significant.
[0008] Therefore, the present invention aims to provide a glass spacer and an HDD device that make it less likely for the magnetic disk and spacer to stick together when the magnetic disk and spacer are removed from an HDD device in which the magnetic disk and spacer are assembled.
[0009] One aspect of the present invention is a ring-shaped glass spacer provided in contact with a magnetic disk within a hard disk drive, wherein the surface roughness Ra of the main surface of the glass spacer that contacts the magnetic disk is 1.0 μm or less, and the average gradient RΔa of the main surface obtained using the following formula (1) is 0.02 or more. Here, dzi / dX is expressed by the following equation (2), where ΔX is the data interval [μm] of the surface roughness measurement data, and z i (where i is a natural number) is the i-th measurement data point.
[0010] The surface roughness Ra is preferably 0.5 μm or less. The surface roughness Ra is preferably 0.01 μm or more.
[0011] Preferably, a metal film is formed on at least the main surface of the glass spacer.
[0012] Another aspect of the present invention is a hard disk drive device comprising the glass spacer and the magnetic disk.
[0013] In the hard disk drive device described above, it is preferable that the magnetic disk is a disk on which a magnetic film is formed on a glass substrate. Furthermore, in the hard disk drive device described above, it is preferable that the surface roughness Ra of the main surface of the magnetic disk is 0.3 nm or less.
[0014] The hard disk drive device preferably has eight or more magnetic disks mounted on it.
[0015] With the glass spacer and HDD device described above, when removing the magnetic disk and spacer from the HDD device, it is possible to make it less likely for the magnetic disk and spacer to stick together.
[0016] This is an external perspective view of a magnetic disk spacer according to one embodiment. This is a diagram illustrating the arrangement of the spacer and magnetic disk according to one embodiment. This is a cross-sectional view of a main part illustrating an example of the structure of an HDD device into which the spacer according to one embodiment is incorporated. (a) is a diagram schematically illustrating an example of the uneven shape of the main surface of the spacer according to one embodiment, and (b) is a diagram schematically illustrating an example of the uneven shape of the main surface of a conventional spacer.
[0017] The glass spacer of the present invention will be described in detail below. Figure 1 is an external perspective view of a glass spacer (hereinafter simply referred to as "spacer") 1 according to one embodiment, and Figure 2 is a diagram illustrating the arrangement of the spacer 1 and the magnetic disk 5. Figure 3 is a cross-sectional view of a key part illustrating an example of the structure of an HDD device into which the spacer 1 is incorporated.
[0018] As shown in Figure 2, the spacers 1 are incorporated into the HDD device by stacking the magnetic disks 5 and spacers 1 alternately. As shown in Figure 3, multiple magnetic disks 5 are fitted onto a spindle 14 that rotates connected to a motor 12 via the spacers 1, and are further secured to the spindle 14 by being pressed from above with screws via a top clamp 16, thereby mounting them at predetermined intervals.
[0019] As shown in Figure 2, the spacers 1 and magnetic disks 5 are arranged alternately so that the spacers 1 are located between the two magnetic disks 5, maintaining a predetermined gap between adjacent magnetic disks 5. In the following embodiments, the spacers 1 described are spacers that are provided between the two magnetic disks 5 so as to be in contact with the magnetic disks 5, but the spacers targeted by the present invention also include spacers that are in contact only with the uppermost or lowermost magnetic disk 5.
[0020] As shown in Figure 1, the spacer 1 has a ring shape and comprises an outer circumferential end face 2, an inner circumferential end face 3, and two opposing main surfaces 4. Chamfered surfaces (not shown) may be provided on the surface of the spacer 1 as appropriate. The inner circumferential end face 3 is the surface that contacts the spindle 14 and is a wall surface surrounding a hole with an inner diameter slightly larger than the outer diameter of the spindle 14. The main surfaces 4 are two parallel surfaces that contact the magnetic disk 5. The spacer 1 contacts the main surfaces of the magnetic disk 5 and fixes the magnetic disk 5 by frictional force. For this reason, the surface roughness Ra (arithmetic mean roughness) and average slope RΔa of the main surfaces 4 that contact the magnetic disk 5 are determined as described later.
[0021] Here, Ra (arithmetic mean roughness) and Rz (maximum height), which will be described as surface roughness from now on, will conform to JIS B 0601-2001 (ISO 4287-1997). The average slope RΔa will conform to ASME B46-1995. These parameters are calculated from data measured using a stylus-type surface roughness meter, for example. The stylus used will have, for example, a tip radius of curvature of 2 μm and a cone taper angle of 60°. Other measurement and calculation parameters will be, for example, a measurement length of 400 μm, a measurement resolution (pitch: ΔX) of 0.1 μm, a scan speed of 0.1 mm / sec, a low-pass filter cutoff value (Ls) of 2.5 μm, and a high-pass filter cutoff value (Lc) of 80 μm.
[0022] Specifically, the surface roughness Ra of the main surface 4 of the spacer 1 that contacts the magnetic disk 5 is 1.0 μm or less. If the surface roughness Ra exceeds 1.0 μm, since the spacer 1 is made of glass, which is a brittle material, when it comes into contact with the magnetic disk 5, the tips of the protrusions on the surface irregularities of the main surface 4 may break, generating foreign matter such as fine particles from the spacer 1, which reduces the long-term reliability of the HDD device. Therefore, the surface roughness Ra is 1.0 μm or less. In addition, the average gradient RΔa obtained using the following formula (1) of the main surface 4 is 0.02 or more. Here, dzi / dX is expressed by the following equation (2), where ΔX is the data interval [μm] of the surface roughness measurement data, and in the above example, it corresponds to a measurement resolution (pitch) of 0.1 μm, z i (where i is a natural number) is the i-th measurement data point. n is the total number of measurement data points (n > 6). Equation (2) is the formula used in the Savitsky-Goley filter. Note that dz i When i in / dX is 1, 2, 3, (n-2), (n-1), or n, then z is present on the right-hand side of equation (2). -2 , z -1 , z0, z n+1 , z n+2 , z n+3Although they appear, they do not exist as measurement data with a total number of n. In this case, before and after measuring the measurement data with a total number of n, use the preliminary measurement data preliminarily measured as a portion adjacent to the outside of the measurement range, and set the corresponding preliminary measurement data as z -2 z -1 z0, z n+1 z n+2 z n+3 and use them as such.
[0023] Thus, by setting the surface roughness Ra to 1.0 μm or less, the unevenness of the spacer 1 is reduced, thus decreasing the number of fine particles generated. Furthermore, the unevenness of the main surface 4 of the spacer 1 is expected to have the effect of making it less likely for the surface of the magnetic disk 5 to be scratched. From a similar viewpoint, the surface roughness Ra is preferably 0.7 μm or less, and more preferably 0.5 μm or less. On the other hand, the smaller the surface roughness Ra of the main surface 4 of the spacer 1, the greater the adhesion force with the magnetic disk 5. However, if the adhesion force is excessive, it may be difficult to separate the magnetic disk 5 and spacer 1 when removing them from the HDD device. As described above, the assembled HDD device is subjected to inspections such as performance tests. In HDD devices in which defects are found during performance tests, the stacked magnetic disks 5 and spacers 11 are sequentially removed from the spindle 14 in order to remove the defective magnetic disk 5. In this case, if the magnetic disk 5 and the spacer 1 are in close contact, separation of the spacer 1 may fail, or foreign matter may be generated during separation, causing fine particles to adhere to the surface of the magnetic disk 5. Such fine particles can be a factor in reducing the long-term reliability of the HDD device. For this reason, in this embodiment, in order to suppress close contact between the magnetic disk 5 and the spacer 1, the surface roughness Ra is set to 1.0 μm or less, while the average gradient RΔa is set to 0.02 or more. From a similar viewpoint, it is preferable that the average gradient RΔa be 0.05 or more, and more preferably 0.10 or more. There is no upper limit to the average gradient RΔa, but for example, it may be 0.3. If the average gradient RΔa exceeds 0.3, there is a risk of damaging the surface of the magnetic disk 5. When the magnetic disk 5 and the spacer 1 are in close contact, the close-contact magnetic disk 5 and spacer 1 will be separated by strong force, so a part of the surface of the magnetic disk 5 may detach as fine particles. Such fine particles can transfer to the magnetic disk and become a factor in reducing the long-term reliability of the HDD device, so this is undesirable. By setting the surface roughness Ra to 1.0 μm or less and the average gradient RΔa to 0.02 or more, the adhesion between the magnetic disk 5 and the spacer 1 can be suppressed, and thus the number of fine particles generated can also be suppressed.
[0024] Even if the surface roughness Ra of the main surface 4 is the same, the surface irregularities vary considerably. Figure 4(a) schematically illustrates an example of the irregularities of the main surface of a spacer according to one embodiment, and (b) schematically illustrates an example of the irregularities of the main surface of a conventional spacer. Even if the surface roughness Ra is the same, as shown in Figures 4(a) and (b), the average slope RΔa differs depending on whether there are irregularities with short periods or with long periods. The average slope RΔa in an irregularity shape with short periods is larger than the average slope RΔa in an irregularity shape with long periods. Because such irregularities with short periods are present on the main surface 4, the magnetic disk 5 and the spacer 1 do not adhere closely together. The ΔX shown in the above formula (2) that determines the average slope surface RΔa is preferably 0.05 to 0.2 μm, preferably 0.08 to 0.12 μm, and in particular preferably 0.1 μm. It is preferable that ΔX is within the above range and the average slope surface RΔa is 0.02 or greater.
[0025] According to one embodiment, the surface roughness Ra of the spacer 1 is preferably 0.01 μm or more. If the surface roughness Ra is less than 0.01 μm, it is possible to make it difficult to scratch the magnetic disk 5, but when the spindle 14 is rotated, there is a risk that the contact surfaces of the magnetic disk 5 and the spacer 1 will slip and shift. This is due to the effect of the lubricant provided on the surface of the magnetic disk 5. Since the lubricant is a liquid, it moves to fill the gaps in the contact surfaces, making it slippery in the direction parallel to the main surface of the spacer 1 or the magnetic disk 5, and increasing the adhesion force in the direction that separates the magnetic disk 5 and the spacer 1 (i.e., the direction perpendicular to the main surface 4). In particular, the surface of the magnetic disk 5 is usually provided with a lubricant film of about 1 nm thickness. However, if this lubricant film transfers to the surface of the spacer 1 and fills some of the grooves in the uneven shape of the main surface 4 of the spacer 1, the spacer 1 or the magnetic disk 5 may become more slippery from each other in the direction parallel to the main surface of the spacer 1 or the magnetic disk 5, and the adhesion force between the spacer 1 and the magnetic disk 5 may increase further in the direction perpendicular to the main surface 4. This phenomenon is thought to be due to the meniscus force of the lubricant, and it is more likely to occur as the lubricant film thickness increases. Considering the above, the adhesion force between the magnetic disk 5 and the spacer 1 can be reduced by setting the surface roughness Ra to 0.01 μm or more and 1.0 μm or less, and the average slope RΔa to 0.02 or more. In order to more reliably reduce the adhesion force between the magnetic disk 5 and the spacer 1, the surface roughness Ra is preferably 0.05 μm or more, more preferably 0.1 μm or more, and even more preferably 0.3 μm or more.
[0026] According to one embodiment, it is preferable that a metal film is formed on at least the main surface 4 of the spacer 1 that is in contact with the magnetic disk 5. In particular, since the spacer 1 is made of glass and is an insulator, static electricity tends to accumulate on the magnetic disk 5 and the spacer 1. When the magnetic disk 5 and the spacer 1 are charged, foreign matter and fine particles are more easily attracted to them, and the discharge of accumulated static electricity to the magnetic head may damage the recording and playback elements of the magnetic head, which is undesirable. Therefore, in order to remove static electricity and to impart electrical conductivity to the spacer 1, it is preferable to form a conductive metal film on the surface of the spacer 1. The metal film is formed by immersion, vapor deposition, or sputtering methods used in plating treatments such as electroless plating. The components of the metal film can be, for example, chromium, titanium, tantalum, tungsten, alloys containing these metals, or nickel alloys such as NiP (nickel-phosphorus) or NiW (nickel-tungsten). It is preferable that the nickel alloy is non-magnetic.
[0027] According to one embodiment, it is also preferable that the metal film be formed on the outer peripheral end face 2 and the inner peripheral end face 3 in addition to the main surface 4. When a metal film is formed on the upper and lower main surfaces 4 of the spacer 1 that contacts the magnetic disk 5, it is sufficient that the metal film be formed on at least one of the outer peripheral end face 2 and the inner peripheral end face 3 so that the metal film on the upper and lower main surfaces 4 can be electrically connected. For example, it may be formed only on the inner peripheral end face 3. This increases electrical conductivity and improves the static electricity removal ability. For the above reasons, it is most preferable to form the metal film over the entire surface of the spacer 1. The thickness of the metal film should be such that it has sufficient electrical conductivity to release the static electricity to the outside, for example, 0.01 to 10 μm. Even when such a metal film is formed on the main surface 4, the numerical range of the surface roughness Ra and average gradient RΔa of the main surface 4 remains within the above range. Note that when the spacer 1 is made of conductive glass, the static electricity charged on the magnetic disk 5 can be directly released to the outside through the spacer 1, so a metal film does not need to be provided.
[0028] Such a spacer 1 is suitable for HDD devices that mount eight or more magnetic disks 5. When eight or more magnetic disks 5 are mounted in an HDD device, rather than the usual six, it becomes necessary to press (clamp) the magnetic disks 5 and spacer 1 more firmly with the top clamp 16, requiring a larger pressing pressure from the top clamp 16. As a result, the adhesion force between the spacer 1 assembled in the HDD device and the magnetic disks 5 increases, making it easier to remove the spacer 1 from the magnetic disks 5 and fail to remove it. However, with spacer 1, even if the pressing pressure increases, the surface roughness Ra and average slope RΔa are limited to the above-mentioned numerical range, so adhesion between the spacer 1 and the magnetic disks 5 is unlikely to occur, and the spacer 1 and magnetic disks 5 can be easily separated. A spacer 1 that can suppress removal failures in this way is suitable. For similar reasons, the spacer 1 of this embodiment is more suitable for use in HDD devices that mount nine or more magnetic disks 5, and even more suitable for use in HDD devices that mount ten or more magnetic disks 5.
[0029] The magnetic disk 5 is preferably a disk on which a magnetic film is formed on an aluminum alloy substrate or a glass substrate. Here, when the surface roughness Ra of the magnetic disk 5 is 0.3 nm or less, adhesion with the spacer 1 is more likely to occur, and when it is 0.2 nm or less, it is particularly likely to occur. However, since the spacer 1 of this embodiment has a high adhesion suppression effect, adhesion can be suitably suppressed regardless of the surface roughness of the magnetic disk 5. That is, the spacer 1 is suitable when used with a magnetic disk 5 with a surface roughness Ra of 0.3 nm or less, and is particularly suitable when used with a magnetic disk 5 with a surface roughness Ra of 0.2 nm or less.
[0030] According to one embodiment, it is preferable that the surface roughness Rz (maximum height) of the outer peripheral end face 2 of the spacer 1 is 1.5 to 20 μm. When the operation of removing the spacer 1 is performed by gripping the outer peripheral end face 2 of the spacer 1 during the rework operation of removing a defective magnetic disk from the assembled HDD device, if the surface roughness Rz (maximum height) is less than 1.5 μm, the spacer 1 may slip off from the gripping jig that grips the outer peripheral end face 2 of the spacer 1. When the surface roughness Rz (maximum height) is greater than 20 μm, the spacer 1 may scrape the surface of the gripping jig and fine foreign matter may be generated.
[0031] The material of the spacer 1 is not particularly limited, and examples thereof include aluminosilicate glass, soda lime glass, soda aluminosilicate glass, aluminoborosilicate glass, borosilicate glass, quartz glass, or crystallized glass. Aluminosilicate glass, for example, contains silicon dioxide (SiO 2 ): 59 to 63% by mass, aluminum oxide (Al 2 O 3 ): 5 to 16% by mass, lithium oxide (Li 2 O): 2 to 10% by mass, sodium oxide (Na 2 O): 2 to 12% by mass, zirconium oxide (ZrO 2 ): 0 to 5% by mass, and the glass can be used. This glass is suitable for the spacer 1 in terms of high rigidity and low thermal expansion coefficient. Soda lime glass, for example, contains SiO 2 : 65 to 75% by mass, Al 2 O 3 : 1 to 6% by mass, CaO: 2 to 7% by mass, Na 2 O: 5 to 17% by mass, ZrO 2Glass containing 0 to 5% by mass can be used. This glass is relatively soft and easy to grind and polish, making it suitable for spacer 1 as it easily improves surface smoothness. The spacer 1, being made of glass, is preferably combined with a magnetic disk 5 in which a magnetic film is formed on a glass substrate. This makes it possible to match the thermal expansion coefficients of spacer 1 and magnetic disk 5 to a similar extent, so that even if temperature changes occur within the HDD device, the difference in thermal expansion due to the temperature change will reduce the displacement and friction caused by changes in the relative position of spacer 1 and magnetic disk 5, thereby suppressing reading errors of recorded signals due to displacement and the generation of fine particles due to friction.
[0032] The glass spacer 1 can be made from any of the following materials: a ring-shaped cut from plate glass manufactured by the float method or down-draw method, molded from molten glass by the press method, or sliced to an appropriate length from a glass tube manufactured by the pipe drawing method. The outer circumferential end face 2, inner circumferential end face 3, and main surface 4 of the thus formed ring-shaped glass are subjected to chamfering or other shaping processes, grinding, polishing, etching, etc., as selected and applied as needed. For grinding the main surface 4, for example, lapping with free abrasive grains or grinding using a planetary gear system with fixed diamond abrasive grains (diamond pads) can be performed. For polishing the main surface 4, for example, polishing using a planetary gear system with a polishing solution containing fine particles of cerium oxide or silicon dioxide can be performed. When using diamond abrasive grains as fixed abrasive grains in the grinding process of the main surface 4, one particle may be used as the fixed abrasive grain, or an aggregate formed by bonding multiple particles with vitrified material may be used as the fixed abrasive grain. In particular, fixed abrasive grains containing diamond have excellent cutting ability against glass, making them suitable for increasing the average gradient RΔa of the surface shape. The fixed abrasive grains are dispersed and fixed in, for example, a resin.
[0033] The average particle size (D50) of the fixed abrasive grains is preferably 5 to 100 μm. Furthermore, when an aggregate formed by bonding multiple particles together with a vitrified material is used as a single fixed abrasive grain, the average particle size (D50) of the above particles is preferably 0.5 to 15 μm, and the average particle size (D50) of the above aggregate is preferably in the range of 5 to 100 μm. The average particle size (D50) refers to the particle size at the point where the cumulative curve reaches 50% when the total volume of the powder aggregate in the particle size distribution measured by the light scattering method is taken as 100%. As the apparatus used for grinding or polishing the above main surface 4, a double-sided grinding apparatus (or polishing apparatus) equipped with upper and lower platens and capable of simultaneously grinding (or polishing) the two main surfaces of the workpiece by planetary gear motion can be used. Furthermore, the surface roughness Ra and average slope RΔa can be adjusted by adjusting, for example, the size of the free abrasive grains and fixed abrasive grains, the pressure of the upper and lower platens (load on the workpiece), the method of changing the pressure (such as changing the pressure in multiple stages), and the processing time for grinding or polishing. For example, when grinding the main surface using a diamond pad, the surface roughness Ra and / or average slope RΔa can be increased by increasing the size of the fixed abrasive grains. Here, when aggregates are used as fixed abrasive grains, the trend differs depending on the size of the aggregate itself as well as the size of the particles contained therein, so the surface roughness Ra and / or average slope RΔa can be adjusted as appropriate. Also, increasing the pressure of the upper and lower platens can increase the surface roughness Ra and / or average slope RΔa. After the above processing, chemical polishing (etching treatment) may be performed using an etching solution containing hydrofluoric acid or silicic acid. The surface roughness Ra and / or average slope RΔa can be changed by adjusting the components of the etching solution, the concentration of the etching solution, the processing time, etc. After the grinding and / or etching treatment, polishing treatment may be performed further. Polishing can reduce the surface roughness Ra and / or average gradient RΔa. Etching may be performed after polishing. By appropriately combining these grinding and polishing methods, a main surface 4 with a desired surface shape can be formed. It is preferable to grind and / or polish the outer peripheral end face 2 and inner peripheral end face 3 of the spacer 1, and then grind and / or polish the main surface 4.
[0034] The dimensions of the spacer 1 may be appropriately changed according to the specifications of the HDD to be installed. For an HDD device of the nominal 3.5-inch type, for example, the outer diameter (the diameter of the outer peripheral end face 2) is 31 to 33 mm, the inner diameter (the diameter of the inner peripheral end face 3) is 25 mm, and the thickness is 1 to 4 mm. The end portions on the inner peripheral side or the outer peripheral side of the main surface 4 may be appropriately chamfered to provide a chamfered surface.
[0035] (Experimental Example) In order to confirm the effect of the spacer 1, spacers with various surface irregularities on the main surface were fabricated (Samples 1 to 30). The fabricated spacers had an inner diameter of 25 mm, an outer diameter of 32 mm, and a thickness of 2 mm. The angle of the chamfered surface was 45 degrees, the radial width of the chamfered surface was 150 μm, and all the specifications of the chamfered surface were the same. First, for a glass material obtained by cutting a plate-shaped glass into a ring shape, the outer peripheral end portion and the inner peripheral end portion were ground using a surface grinder to form an outer peripheral end face, an inner peripheral end face, and a chamfered surface. Next, grinding of the main surface was performed using a planetary gear type double-sided grinding apparatus in which a grinding pad having an aggregate in which diamond fine particles were vitrified and bonded as fixed abrasive grains was attached to upper and lower surface plates. In order to create various forms of surface irregularities on the main surface, the size of the fixed abrasive grains in the grinding pad, the surface plate load, the grinding treatment time, etc. were changed. The surface roughness Rz at the outer peripheral end face and the inner peripheral end face was made uniform at 5 μm, and the surface roughness Ra and the average inclination RΔa at the main surface 4 were changed. After the grinding treatment with the grinding pad having the fixed abrasive grains, if necessary, lapping, polishing treatment, or etching treatment of the main surface with free abrasive grains was appropriately combined and performed.
[0036] (Evaluation of Adhesion) The fabricated spacers were assembled into a test apparatus simulating an HDD device using three magnetic disks and four spacers, as shown in Figure 3. The magnetic disks (with a main surface roughness Ra of 0.2 nm) were then mounted using the top clamp 16, and after being left for 30 minutes, the magnetic disks and spacers were separated again. The magnetic disks used were nominal 3.5-inch magnetic disk glass substrates with an outer diameter of 95 mm, an inner diameter of 25 mm, and a plate thickness of 0.635 mm, on which a magnetic film was deposited, and a lubricant with a thickness of 1 nm was applied to the outermost surface. Specifically, the presence or absence of adhesion (inseparability) was investigated using a vacuum suction jig having a ring-shaped suction part that adsorbs almost the entire main surface of the spacer (when removing the magnetic disk 5, the innermost circumference of the main surface is adsorbed).
[0037] (Evaluation of Lubricant Transfer) To evaluate the possibility of close contact between the magnetic disk and the spacer, the transfer marks of lubricant on the magnetic disk after assembly were evaluated. The magnetic disk used was a nominal 3.5-inch magnetic disk glass substrate with an outer diameter of 95 mm, an inner diameter of 25 mm, and a plate thickness of 0.635 mm, on which a magnetic film was deposited, and a lubricant with a thickness of 1 nm was applied to the outermost surface. Unlike the three magnetic disks and four spacers shown in Figure 3, the fabricated spacers were assembled into a test apparatus simulating an HDD device using eight magnetic disks and nine spacers. After mounting the magnetic disks (surface roughness Ra of 0.2 nm) by pressing them down with a top clamp, the apparatus was left for 60 minutes, and then the magnetic disks and spacers were separated (assembly and separation operations). After the above work, the inner circumferential end face of the main surface of the magnetic disk, the portion that came into contact with the main surface of the spacer, was visually inspected in a dark room using a focusing lamp to check for lubricant transfer marks. Since the lubricant is a liquid, some of the lubricant may transfer to the recesses on the spacer surface due to the influence of meniscus force. Transfer marks indicate unevenness in the film thickness of the lubricant. If transfer occurs, it is undesirable because when the above assembly and separation work is performed two or more times, the transferred lubricant is likely to fill some of the grooves in the uneven shape of the main surface of the spacer, causing adhesion. Lubricant transfer was judged and evaluated based on the following criteria: Level 1: One or fewer magnetic disks with transfer marks, Level 2: Two to three magnetic disks with transfer marks, Level 3: Four or more magnetic disks with transfer marks.
[0038]
[0039] According to samples 1 to 30 in Table 1 above, it can be seen that by setting the surface roughness Ra of the main surface to 1.0 μm or less and the average gradient RΔa to 0.02 or more, the adhesion force is reduced and adhesion is suppressed. Furthermore, from the evaluation results of lubricant transfer, it can be seen that lubricant transfer is reduced by setting the average gradient RΔa to 0.05 or more, and further reduced by setting the average gradient RΔa to 0.10 or more. For this reason, by setting the average gradient RΔa to 0.05 or more, and even 0.10 or more, the possibility of adhesion is unlikely to occur even if the assembly and separation of the magnetic disk and spacer is performed two or more times.
[0040] Furthermore, a uniform metal film with a thickness of 1 μm, specifically a Ni-P alloy metal film (P: 10% by mass, remainder Ni), was formed on the outer peripheral end face 2, inner peripheral end face 3, and main surface 4 of the spacer 1 of sample 7 by electroless plating. The spacer 1 with this metal film formed on it was incorporated into the HDD device 10 shown in Figure 3. At this time, the conductivity between all magnetic disks 5 and spacer 1 and the spindle 14 was confirmed with a tester. In other words, by forming a metal film on the spacer 1, static electricity is less likely to accumulate on the magnetic disks 5 and spacer 1, and effects such as reduced adsorption of foreign matter and fine particles to the magnetic disks 5 and spacer 1 can be obtained. From this, the effects of this embodiment are clear.
[0041] Such a spacer 1 can be manufactured as follows. That is, one embodiment is a method for manufacturing a ring-shaped spacer 1 that is provided in contact with a magnetic disk 5 inside a hard disk drive device. This manufacturing method is characterized by including a grinding process in which the main surface of a ring-shaped glass base plate that will be the basis of the spacer 1 is ground using a planetary gear type double-sided grinding device in which grinding pads of fixed abrasive grains containing diamond microparticles are attached to upper and lower surface plates. According to one embodiment, it is preferable that the fixed abrasive grains include aggregates in which diamond microparticles are bonded together with vitrified material. Through the grinding process of this manufacturing method, the surface roughness Ra of the main surface of the spacer that contacts the magnetic disk can be made 1.0 μm or less, and the average inclination RΔa of the main surface of the spacer can be made 0.02 or more.
[0042] Although the glass spacer and hard disk drive device of the present invention have been described in detail above, the present invention is not limited to the above embodiments and examples, and various improvements and modifications may be made without departing from the spirit of the present invention.
[0043] 1. Glass spacer 2. Outer peripheral end face 3. Inner peripheral end face 4. Main surface 5. Magnetic disk 10. Hard disk drive unit 12. Motor 14. Spindle 16. Top clamp
Claims
1. A ring-shaped glass spacer that is provided in contact with a magnetic disk within a hard disk drive device, characterized in that the surface roughness Ra of the main surface of the glass spacer that contacts the magnetic disk is 1.0 μm or less, and the average slope RΔa of the main surface, obtained using the following formula (1), is 0.02 or more.
2. The glass spacer according to claim 1, wherein the surface roughness Ra is 0.5 μm or less.
3. A glass spacer according to claim 1 or 2, wherein a metal film is formed on at least the main surface of the glass spacer.
4. A hard disk drive device comprising the glass spacer according to any one of claims 1 to 3 and the magnetic disk.
5. The hard disk drive device according to claim 4, wherein the magnetic disk is a disk having a magnetic film formed on a glass substrate.
6. The hard disk drive device according to claim 5, wherein the surface roughness Ra of the main surface of said magnetic disk is 0.3 nm or less.
7. The hard disk drive device according to any one of claims 4 to 6, which is equipped with eight or more magnetic disks.